A nickel nitrate separation and impurity removal device and impurity removal method

By introducing a machine learning model and an automatic control system into the nickel nitrate separation and impurity removal device, the amount of pH adjuster added is intelligently adjusted to ensure that the extraction reaction conditions are suitable. This solves the problem that the solution acidity is not suitable for the extractant in the existing technology, and improves the impurity removal efficiency and product quality stability.

CN118846581BActive Publication Date: 2024-11-22HUAIHUA HENGAN PETROCHEMICAL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411329524.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-09-24
Publication Date
2024-11-22
Estimated Expiration
2044-09-24

AI Technical Summary

Technical Problem

Existing nickel nitrate separation and impurity removal devices and methods cannot intelligently and adaptively adjust the amount of pH adjuster added, resulting in the solution acidity being unsuitable for the working range of the extractant, affecting the impurity removal effect and product quality stability.

Method used

The extraction process employs an impurity filter, extraction reactor, dosing assembly, and reaction control unit, combined with a machine learning model, to automatically adjust the amount of pH adjuster added. Stirring and heating are used to ensure suitable reaction conditions, and centrifuges and evaporators are used to separate impurities, thus achieving intelligent control of the extraction process.

Benefits of technology

It achieves intelligent adaptive adjustment based on the characteristics of pH adjusters and differences in raw materials, ensuring that the solution acidity is suitable for the working range of the extractant, improving the impurity removal efficiency and product purity, reducing costs, and solving the problems of incomplete impurity removal and unstable product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118846581B_ABST
    Figure CN118846581B_ABST
Patent Text Reader

Abstract

The present invention relates to the technical field of nickel nitrate impurity removal, and in particular to a nickel nitrate separation and impurity removal device and impurity removal method, comprising an impurity filter, which is used to preliminarily filter the initial nickel nitrate solution to be treated to remove insoluble solid impurities; an extraction reactor, which is conductively connected to the liquid outlet of the impurity filter, and the initial nickel nitrate solution is discharged into the extraction reactor after being preliminarily filtered by the impurity filter; and a dosing component, which is arranged on the extraction reactor to automatically add a pH regulator. The present invention realizes intelligent and adaptive adjustment of the addition amount of the pH regulator according to the characteristics of the pH regulator and the difference of the raw materials, ensures the acidity adjustment effect of the solution, makes the acidity of the solution suitable for the working range of the extractant, and ensures the extraction effect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of nickel nitrate impurity removal, and in particular to a nickel nitrate separation and impurity removal device and an impurity removal method. Background Art

[0002] Nickel nitrate is an important chemical raw material, widely used in electroplating, battery manufacturing, catalysts and other fields. However, during the production process, nickel nitrate solution often contains some impurities, which will affect the quality of nickel nitrate products and even its application performance. Therefore, the development of efficient nickel nitrate separation and impurity removal device and production method has important industrial significance.

[0003] The Chinese patent application with publication number CN106865626A discloses a method for removing cobalt impurities from nickel nitrate, which comprises the following specific steps: (1) dissolving the reagent nickel nitrate in water to form a solution, adding reagent-grade sodium hydroxide and sodium hypochlorite solution to generate a trivalent nickel hydroxide precipitate, and washing the trivalent nickel hydroxide precipitate for later use; (2) adding ammonia water and hydrogen peroxide to the industrial nickel nitrate solution, filtering to remove iron impurities, adding the trivalent nickel hydroxide precipitate obtained in step (1), heating and stirring for 30 minutes, and removing the Co in the solution. 2+ Oxidized to Co 3+ , and Co(OH) 3 (3) after separating the precipitate, the solution is concentrated and crystallized to obtain a nickel nitrate product that meets the reagent grade index. The method is easy to operate and can obtain a nickel nitrate product that meets the requirements (cobalt ≤ 0.01%).

[0004] As mentioned in the above application, the existing nickel nitrate separation and impurity removal devices and impurity removal methods generally adopt the extraction method. However, before extraction, the acidity of the solution needs to be adjusted to a range suitable for the working range of the extractant. Due to the differences in the concentration and pH value of the nickel nitrate solution and the characteristics of the pH adjuster, the amount of pH adjuster added is also different. The existing technologies all rely on human experience or a pre-set amount of addition for addition. It is impossible to perform intelligent and adaptive adjustments based on the characteristics of the pH adjuster and the differences in the raw materials, thereby affecting the product impurity removal effect. Summary of the invention

[0005] In order to solve the above problems, the present invention provides a nickel nitrate separation and impurity removal device and impurity removal method.

[0006] The present invention adopts the following technical scheme, a nickel nitrate separation and impurity removal device, comprising:

[0007] An impurity filter, which is used to preliminarily filter the initial nickel nitrate solution to be treated to remove insoluble solid impurities;

[0008] An extraction reactor is connected to the liquid outlet of the impurity filter, and the initial nickel nitrate solution is initially filtered through the impurity filter and then discharged into the extraction reactor;

[0009] A dosing component is provided on the extraction reactor to automatically add a pH regulator;

[0010] A reaction control unit, the reaction control unit comprising:

[0011] A first data acquisition module collects comprehensive parameters of historical initial nickel nitrate solution extraction and impurity removal, wherein the comprehensive parameters include characteristic parameters of the initial nickel nitrate solution and the amount of pH regulator added;

[0012] The first data analysis module trains a machine learning model for predicting the amount of pH regulator to be added based on the collected comprehensive parameters of historical initial nickel nitrate solution extraction and impurity removal, collects the characteristic parameters of the real-time initial nickel nitrate solution, predicts the amount of pH regulator to be added based on the trained machine learning model, and controls the operation of the dosing component based on the predicted amount of pH regulator to be added;

[0013] The second data acquisition module collects the pH value of the nickel nitrate solution after the pH adjuster is added, and records it as the extraction pH value;

[0014] The second data analysis module inputs the collected extraction pH value and characteristic parameters of the initial nickel nitrate solution into a pre-constructed extraction parameter recommendation model to obtain an extraction parameter recommendation set label, thereby obtaining an extraction parameter recommendation set corresponding to the extraction parameter recommendation set label, and controls the working parameters of the extraction reactor based on the control parameters in the extraction parameter recommendation set to extract the nickel nitrate solution.

[0015] As a further description of the above technical solution: it also includes:

[0016] A stirring assembly, which is installed in the extraction reactor and is used to stir and mix the liquid in the extraction reactor;

[0017] The heater is installed in the extraction reactor and is used to heat the solution in the extraction reactor.

[0018] As a further description of the above technical solution: the dosing component includes a storage box, an infusion tube and a flow pump, the storage box is used to store the pH adjuster, the storage box is connected to the extraction reactor through the infusion tube, the flow pump is arranged on the infusion tube, and the flow pump is used to pump the pH adjuster in the storage box into the extraction reactor.

[0019] As a further description of the above technical solution: it also includes: a centrifuge, which is conductively connected to the extraction reactor and is used to separate the extraction agent;

[0020] an evaporator, the evaporator being conductively connected to the extraction reactor;

[0021] A crystallizer is conductively connected to the evaporator.

[0022] As a further description of the above technical solution: the stirring assembly includes a stirring shaft, a stirring motor and a stirring blade, the stirring blade is bolted to the stirring shaft, the stirring motor is bolted to the outer wall of the extraction reactor, and the output shaft of the stirring motor is fixed to the stirring shaft through a coupling.

[0023] As a further description of the above technical solution: the characteristic parameters of the nickel nitrate solution include the nickel nitrate solution adjustment coefficient, the type of pH adjuster, the concentration of the pH adjuster, and the type of impurities in the nickel nitrate solution;

[0024] The parameters affecting the adjustment coefficient of the nickel nitrate solution include the concentration of the nickel nitrate solution, the pH value of the nickel nitrate solution and the total amount of the nickel nitrate solution;

[0025] The expression of the adjustment coefficient of the nickel nitrate solution is:

[0026] ;

[0027] In the formula, is the adjustment coefficient of nickel nitrate solution, is the concentration of nickel nitrate solution, is the pH value of nickel nitrate solution, is the total amount of nickel nitrate solution, , and is the weight factor, , and Both are greater than zero.

[0028] As a further description of the above technical solution: the training method of the machine learning model for predicting the amount of pH regulator added includes:

[0029] Converting the collected characteristic parameters of the initial nickel nitrate solution into a corresponding set of characteristic vectors;

[0030] Each group of feature vectors is used as the input of the machine learning model, and the machine learning model takes the amount of pH adjuster added corresponding to the characteristic parameters of each group of initial nickel nitrate solutions as the output, and takes the amount of pH adjuster added actually corresponding to the characteristic parameters of each group of initial nickel nitrate solutions as the prediction target, and takes minimizing the loss function value of the machine learning model as the training target; training is stopped when the loss function value of the machine learning model is less than or equal to the preset target loss value.

[0031] As a further description of the above technical solution: the recommended set of extraction parameters is:

[0032]

[0033] in, The collection label is The corresponding type of extractant, The collection label is The corresponding amount of extractant is The collection label is The corresponding extraction temperature is The collection label is The corresponding extraction time.

[0034] As a further description of the above technical solution: the training method of the extraction parameter recommendation model includes:

[0035] Set the extraction parameter recommendation set with corresponding numbers in advance;

[0036] The characteristic parameters of the extraction pH value and the initial nickel nitrate solution are converted into a corresponding set of feature vectors, and each set of feature vectors is used as the input of the machine learning model. The machine learning model uses a set of extraction parameter recommendation set numbers corresponding to each set of extraction pH value and the characteristic parameters of the initial nickel nitrate solution as output, and a set of extraction parameter recommendation set numbers actually corresponding to each set of extraction pH value and the characteristic parameters of the initial nickel nitrate solution as a prediction target, and minimizing the loss function value of the machine learning model as a training target; training is stopped when the loss function value of the machine learning model is less than or equal to a preset target loss value.

[0037] A method for separating and removing impurities from nickel nitrate is implemented based on the above-mentioned device for separating and removing impurities from nickel nitrate, comprising the following steps:

[0038] Passing the initial nickel nitrate solution to be treated into an impurity filter for preliminary filtration to remove insoluble solid impurities;

[0039] The filtered nickel nitrate solution is added into the extraction reactor, and a pH regulator is added into the extraction reactor through a dosing component to adjust the acidity of the solution to a range suitable for the working of the extractant;

[0040] Add the extractant into the extraction reactor, and control the operation of the heater and stirring assembly in the extraction reactor to heat and stir the liquid in the extraction reactor to ensure that the reaction is carried out at an appropriate temperature, that the solution and the extractant are fully mixed, and that the reaction efficiency and product quality are improved;

[0041] The extracted solution and the extractant are separated by a centrifuge, the target metal is enriched in the extractant, the extractant enriched with the target metal is introduced into the extraction reactor again, and the target metal is separated from the extractant by adding a stripping agent;

[0042] The stripping liquid is filtered to remove residual impurities, and then concentrated and crystallized through an evaporator and a crystallizer to obtain a high-purity nickel nitrate product.

[0043] Beneficial effects:

[0044] The nickel nitrate separation and impurity removal device provided by the present invention collects the adjustment coefficient of the nickel nitrate solution, the type of pH regulator, the concentration of the pH regulator, and the type of impurities in the nickel nitrate solution, predicts the amount of pH regulator added, and realizes intelligent and adaptive adjustment of the amount of pH regulator added according to the characteristics of the pH regulator and the difference in raw materials, thereby ensuring the acidity adjustment effect of the solution, making the acidity of the solution suitable for the working range of the extractant, and ensuring the extraction effect;

[0045] Furthermore, by inputting the collected extraction pH value and characteristic parameters of the initial nickel nitrate solution into a pre-built extraction parameter recommendation model, an extraction parameter recommendation set label is obtained, thereby obtaining an extraction parameter recommendation set corresponding to the extraction parameter recommendation set label, and controlling the working parameters of the extraction reactor based on the control parameters in the extraction parameter recommendation set, and extracting the nickel nitrate solution, the automatic generation of control parameters to control the operation of the extraction reactor is realized, that is, the intelligent selection of the best type of extractant and amount of extractant, extraction temperature and extraction time is realized, thereby improving the impurity removal efficiency and reducing the cost, and overcoming the defect that the prior art cannot automatically generate control parameters based on the characteristics of the nickel nitrate solution to control the operation of the extraction reactor, resulting in incomplete impurity removal and unstable product quality. BRIEF DESCRIPTION OF THE DRAWINGS

[0046] The present invention will be further explained below in conjunction with the accompanying drawings and embodiments:

[0047] Figure 1 A schematic structural diagram of a nickel nitrate separation and impurity removal device provided in an embodiment of the present invention;

[0048] Figure 2 A schematic diagram of the structure of an extraction reactor provided by an embodiment of the present invention;

[0049] Figure 3 A module connection diagram of a reaction control unit provided in an embodiment of the present invention;

[0050] Figure 4 A flow chart of a method for separating and removing impurities from nickel nitrate provided in an embodiment of the present invention.

[0051] Figure numerals: 1. impurity filter; 2. extraction reactor; 21. dosing component; 211. storage box; 212. infusion tube; 213. flow pump; 22. stirring component; 221. stirring shaft; 222. stirring motor; 223. stirring blade; 23. heater; 24. reaction control unit; 3. centrifuge; 4. evaporator; 5. crystallizer. DETAILED DESCRIPTION

[0052] In order to make the technical means, creative features, objectives and effects of the present invention easy to understand, the present invention is further described below with reference to specific diagrams. It should be noted that the embodiments and features in the embodiments of the present application can be combined with each other without conflict.

[0053] Example 1

[0054] See also Figure 1-Figure 3 The embodiment of the present invention provides a technical solution: a nickel nitrate separation and impurity removal device, comprising:

[0055] The impurity filter 1 is used to preliminarily filter the initial nickel nitrate solution to be treated to remove insoluble solid impurities. It should be noted that the initial nickel nitrate solution is generally obtained by leaching nickel in ore or alloy using nitric acid or other acids, so the initial nickel nitrate solution contains certain impurities.

[0056] The extraction reactor 2 is conductively connected to the liquid outlet of the impurity filter 1 . The initial nickel nitrate solution is initially filtered through the impurity filter 1 and then discharged into the extraction reactor 2 .

[0057] The dosing component 21 is arranged on the extraction reactor 2 for automatically adding a pH adjuster. The dosing component 21 includes a storage box 211, an infusion tube 212 and a flow pump 213. The storage box 211 is used to store the pH adjuster. The storage box 211 is connected to the extraction reactor 2 through the infusion tube 212, and the infusion tube 212 is provided with a flow pump 213 for pumping the pH adjuster in the storage box 211 into the extraction reactor 2.

[0058] The stirring assembly 22 is installed in the extraction reactor 2 and is used to stir and mix the liquid in the extraction reactor 2. The stirring assembly 22 includes a stirring shaft 221, a stirring motor 222 and a stirring blade 223. The stirring blade 223 is bolted to the stirring shaft 221, and the stirring motor 222 is bolted to the outer wall of the extraction reactor 2. The output shaft of the stirring motor 222 is fixedly connected to the stirring shaft 221 through a coupling.

[0059] The heater 23 is installed in the extraction reactor 2 and is used to heat the solution in the extraction reactor 2 .

[0060] A centrifuge 3, which is electrically connected to the extraction reactor 2 and is used for separating the extractant;

[0061] An evaporator 4, which is electrically connected to the extraction reactor 2;

[0062] The crystallizer 5 is electrically connected to the evaporator 4.

[0063] The reaction control unit 24 is used to control the dosage of the nitric acid solution and adjust the pH value of the nickel nitrate solution. The reaction control unit 24 includes:

[0064] The first data acquisition module collects the comprehensive parameters of the historical initial nickel nitrate solution extraction and impurity removal, the comprehensive parameters including the characteristic parameters of the initial nickel nitrate solution and the amount of pH regulator added;

[0065] The characteristic parameters of the nickel nitrate solution include the nickel nitrate solution adjustment coefficient, the type of pH adjuster, the concentration of the pH adjuster, and the type of impurities in the nickel nitrate solution;

[0066] It should be noted that the types of impurities in the nickel nitrate solution can be obtained by chromatographic analysis methods. The types of impurities are detected by the separation behavior of impurities in the solution in the chromatographic column. Commonly used chromatographic analysis methods include:

[0067] Liquid chromatography HPLC: suitable for detecting non-volatile organic impurities and performing separation and analysis through high performance liquid chromatography columns;

[0068] Ion chromatography IC: Suitable for detecting ionic impurities in solutions and performing separation and analysis through ion exchange chromatography columns.

[0069] It should be noted that the type and concentration of the pH adjuster will also affect the pH adjustment process. The types of pH adjusters include hydrochloric acid and nitric acid.

[0070] The parameters that affect the adjustment coefficient of the nickel nitrate solution include the concentration of the nickel nitrate solution, the pH value of the nickel nitrate solution and the total amount of the nickel nitrate solution.

[0071] The expression of the adjustment coefficient of nickel nitrate solution is:

[0072] ;

[0073] In the formula, is the adjustment coefficient of nickel nitrate solution, is the concentration of nickel nitrate solution, is the pH value of nickel nitrate solution, is the total amount of nickel nitrate solution, , and is the weight factor, , and Both are greater than zero.

[0074] It should be noted that a high concentration of nickel nitrate solution requires more pH adjusters to reach the desired pH value. Similarly, the more the total amount of nickel nitrate solution, the more pH adjusters are needed to reach the desired pH value. The higher the pH value of the nickel nitrate solution, the more pH adjusters are needed to reach the desired pH value.

[0075] It should be noted that the size of the weight coefficient is a specific value obtained by quantifying each data to facilitate subsequent comparison. The size of the weight coefficient depends on the number of comprehensive parameters and the preliminary setting of the corresponding weight coefficient for each set of comprehensive parameters by technical personnel in this field.

[0076] The first data analysis module trains a machine learning model for predicting the amount of pH regulator to be added based on the collected historical comprehensive parameters of the initial nickel nitrate solution for extraction and impurity removal, collects the characteristic parameters of the real-time initial nickel nitrate solution, predicts the amount of pH regulator to be added based on the trained machine learning model, and controls the operation of the dosing component 21 based on the predicted amount of pH regulator to be added;

[0077] The training method of the machine learning model for predicting the amount of pH adjuster to be added includes:

[0078] Converting the collected characteristic parameters of the initial nickel nitrate solution into a corresponding set of characteristic vectors;

[0079] Each group of feature vectors is used as the input of the machine learning model. The machine learning model takes the amount of pH adjuster added corresponding to the characteristic parameters of each group of initial nickel nitrate solutions as output, takes the amount of pH adjuster added actually corresponding to the characteristic parameters of each group of initial nickel nitrate solutions as the prediction target, and takes minimizing the loss function value of the machine learning model as the training target; training stops when the loss function value of the machine learning model is less than or equal to the preset target loss value.

[0080] The machine learning model can be one of the models such as support vector machine regression, random forest regression or neural network regression.

[0081] The loss function value of the machine learning model is the mean square error.

[0082] Mean square error is one of the commonly used loss functions. Minimization is used to train the model so that the machine learning model can better fit the data, thereby improving the performance and accuracy of the model.

[0083] In the loss function is the loss function value of the machine learning model, is the feature vector group number; is the number of eigenvector groups; For the predicted The amount of pH regulator added corresponding to the group feature vector, For the The actual amount of pH adjuster added corresponding to the group feature vector.

[0084] In this embodiment, by collecting the adjustment coefficient of the nickel nitrate solution, the type of pH regulator, the concentration of the pH regulator, and the type of impurities in the nickel nitrate solution, the amount of pH regulator added is predicted based on the trained machine learning model that predicts the amount of pH regulator added, and the dosing component 21 is controlled to work based on the predicted amount of pH regulator added, and a specified amount of pH regulator is added to the extraction reactor 2 to adjust the acidity of the solution to a range suitable for the extraction agent to work, thereby achieving precise control of the pH value and improving the purity of the product after impurity removal;

[0085] That is, the amount of pH regulator added is adjusted intelligently and adaptively according to the characteristics of the pH regulator and the differences in raw materials, thereby ensuring the acidity adjustment effect of the solution, making the acidity of the solution suitable for the working range of the extractant, and ensuring the extraction effect.

[0086] Example 2

[0087] See also Figure 1-Figure 3 , this implementation further adds a second data acquisition module and a second data analysis module on the basis of the above embodiment;

[0088] Specifically, the present embodiment is used to solve the problem in the prior art that, during the extraction process of nickel nitrate solution, the extraction control parameters, i.e., the type of extractant, the amount of extractant, the extraction time and the extraction temperature, are generally controlled manually or based on pre-set parameters. That is, the user can only control the operation of the extraction reactor 2 according to the set parameters, and cannot automatically generate control parameters based on the characteristics of the nickel nitrate solution to control the operation of the extraction reactor 2, which leads to the defects of incomplete impurity removal and unstable product quality.

[0089] The second data acquisition module collects the pH value of the nickel nitrate solution after the pH adjuster is added, and records it as the extraction pH value;

[0090] The second data analysis module inputs the collected extraction pH value and characteristic parameters of the initial nickel nitrate solution into a pre-constructed extraction parameter recommendation model to obtain an extraction parameter recommendation set label, thereby obtaining an extraction parameter recommendation set corresponding to the extraction parameter recommendation set label, and controls the working parameters of the extraction reactor 2 based on the control parameters in the extraction parameter recommendation set to extract the nickel nitrate solution.

[0091] The recommended set of extraction parameters is:

[0092]

[0093] in, The collection label is The corresponding type of extractant, The collection label is The corresponding amount of extractant is The collection label is The corresponding extraction temperature is The collection label is The corresponding extraction time.

[0094] The training method of the extraction parameter recommendation model includes:

[0095] Set the extraction parameter recommendation set with corresponding numbers in advance;

[0096] The characteristic parameters of the extraction pH value and the initial nickel nitrate solution are converted into a corresponding set of feature vectors, and each set of feature vectors is used as the input of the machine learning model. The machine learning model uses a set of recommended extraction parameter set numbers corresponding to each set of characteristic parameters of the extraction pH value and the initial nickel nitrate solution as output, and uses a set of recommended extraction parameter set numbers actually corresponding to each set of characteristic parameters of the extraction pH value and the initial nickel nitrate solution as the prediction target, and minimizing the loss function value of the machine learning model as the training target; training is stopped when the loss function value of the machine learning model is less than or equal to the preset target loss value.

[0097] The loss function value of the machine learning model is the mean square error.

[0098] By transforming the loss function: Minimization is used as the goal to train the model so that the machine learning model can better fit the data, thereby improving the performance and accuracy of the model;

[0099] In the loss function is the loss function value of the machine learning model, is the feature vector group number; is the number of eigenvector groups; For the The recommended set number of extraction parameters for group feature vector prediction, For the The recommended set number of extraction parameters that the group feature vector actually corresponds to.

[0100] Other model parameters of the machine learning model, target loss value, optimization algorithm, training set test set validation set ratio, and loss function optimization are all achieved through actual engineering implementation and continuous experimental tuning.

[0101] In this embodiment, the collected extraction pH value and characteristic parameters of the initial nickel nitrate solution are input into a pre-constructed extraction parameter recommendation model to obtain an extraction parameter recommendation set label, thereby obtaining an extraction parameter recommendation set corresponding to the extraction parameter recommendation set label, and controlling the working parameters of the extraction reactor 2 based on the control parameters in the extraction parameter recommendation set, and extracting the nickel nitrate solution, thereby realizing automatic generation of control parameters to control the operation of the extraction reactor 2, that is, realizing intelligent selection of the best type of extractant and amount of extractant, extraction temperature and extraction time, thereby improving impurity removal efficiency and reducing costs, and overcoming the problem that the prior art cannot automatically generate control parameters based on the characteristics of the nickel nitrate solution to control the operation of the extraction reactor 2, resulting in incomplete impurity removal and unstable product quality.

[0102] Example 3

[0103] See also Figure 4 , this embodiment discloses a method for separating and removing impurities from nickel nitrate;

[0104] A method for separating and removing impurities from nickel nitrate is implemented based on a nickel nitrate separation and impurity removal device, comprising the following steps:

[0105] The initial nickel nitrate solution to be treated is passed into the impurity filter 1 for preliminary filtration to remove insoluble solid impurities;

[0106] The filtered nickel nitrate solution is added into the extraction reactor 2, and a pH regulator is added into the extraction reactor 2 through the dosing component 21 to adjust the acidity of the solution to a range suitable for the working of the extractant;

[0107] Adding an extractant into the extraction reactor 2, and controlling the heater 23 and the stirring assembly 22 in the extraction reactor 2 to heat and stir the liquid in the extraction reactor 2, ensuring that the reaction is carried out at a suitable temperature, ensuring that the solution and the extractant are fully mixed, and improving the reaction efficiency and product quality;

[0108] The extracted solution and the extractant are separated by a centrifuge 3, the target metal is enriched in the extractant, and the extractant enriched with the target metal is introduced into the extraction reactor 2 again, and the target metal is separated from the extractant by adding a stripping agent;

[0109] The stripping liquid is filtered to remove residual impurities, and then concentrated and crystallized through an evaporator 4 and a crystallizer 5 to obtain a high-purity nickel nitrate product.

[0110] The basic principles, main features and advantages of the present invention are shown and described above. Those skilled in the art should understand that the present invention is not limited to the above embodiments. The above embodiments and the description in the specification are only to illustrate the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention to be protected. The scope of protection of the present invention is defined by the attached claims and their equivalents.

Claims

1. A nickel nitrate separation and impurity removal device, characterized in that: include: An impurity filter (1) is used to perform preliminary filtration on the initial nickel nitrate solution to remove insoluble solid impurities; An extraction reactor (2) is conductively connected to the liquid outlet of the impurity filter (1); the initial nickel nitrate solution is initially filtered through the impurity filter (1) and then discharged into the extraction reactor (2); A dosing component (21) is arranged on the extraction reactor (2) and performs automatic addition of a pH regulator; A reaction control unit (24), wherein the reaction control unit (24) comprises: A first data acquisition module collects comprehensive parameters of historical initial nickel nitrate solution extraction and impurity removal, wherein the comprehensive parameters include characteristic parameters of the initial nickel nitrate solution and the amount of pH regulator added; A first data analysis module trains a machine learning model for predicting the amount of pH regulator to be added based on the collected historical comprehensive parameters of the initial nickel nitrate solution extraction and impurity removal, collects the real-time characteristic parameters of the initial nickel nitrate solution, predicts the amount of pH regulator to be added based on the trained machine learning model, and controls the operation of the dosing component (21) based on the predicted amount of pH regulator to be added; The second data acquisition module collects the pH value of the nickel nitrate solution after the pH adjuster is added, and records it as the extraction pH value; The second data analysis module inputs the collected extraction pH value and characteristic parameters of the initial nickel nitrate solution into a pre-constructed extraction parameter recommendation model to obtain an extraction parameter recommendation set label, thereby obtaining an extraction parameter recommendation set corresponding to the extraction parameter recommendation set label, and controls the working parameters of the extraction reactor (2) based on the control parameters in the extraction parameter recommendation set to extract the nickel nitrate solution.

2. A nickel nitrate separation and impurity removal device according to claim 1, characterized in that: Also includes: A stirring assembly (22), which is installed in the extraction reactor (2) and is used to stir and mix the liquid in the extraction reactor (2); A heater (23) is installed in the extraction reactor (2) and is used to heat the solution in the extraction reactor (2).

3. A nickel nitrate separation and impurity removal device according to claim 1, characterized in that: The dosing assembly (21) comprises a storage box (211), an infusion tube (212) and a flow pump (213); the storage box (211) is used to store a pH regulator; the storage box (211) is conductively connected to the extraction reactor (2) via the infusion tube (212); the flow pump (213) is arranged on the infusion tube (212); and the flow pump (213) is used to pump the pH regulator in the storage box (211) into the extraction reactor (2).

4. A nickel nitrate separation and impurity removal device according to claim 1, characterized in that: Also includes: a centrifuge (3), the centrifuge (3) being electrically connected to the extraction reactor (2) and used for separating the extraction agent; an evaporator (4), the evaporator (4) being electrically connected to the extraction reactor (2); A crystallizer (5), wherein the crystallizer (5) is conductively connected to the evaporator (4).

5. A nickel nitrate separation and impurity removal device according to claim 2, characterized in that: The stirring assembly (22) comprises a stirring shaft (221), a stirring motor (222) and a stirring blade (223); the stirring blade (223) is bolted to the stirring shaft (221); the stirring motor (222) is bolted to the outer wall of the extraction reactor (2); and the output shaft of the stirring motor (222) is fixedly connected to the stirring shaft (221) via a coupling.

6. A nickel nitrate separation and impurity removal device according to claim 1, characterized in that: The characteristic parameters of the nickel nitrate solution include the nickel nitrate solution adjustment coefficient, the type of pH adjuster, the concentration of the pH adjuster, and the type of impurities in the nickel nitrate solution; The parameters affecting the adjustment coefficient of the nickel nitrate solution include the concentration of the nickel nitrate solution, the pH value of the nickel nitrate solution and the total amount of the nickel nitrate solution; The expression of the adjustment coefficient of the nickel nitrate solution is: ; In the formula, is the adjustment coefficient of nickel nitrate solution, is the concentration of nickel nitrate solution, is the pH value of nickel nitrate solution, is the total amount of nickel nitrate solution, , and is the weight factor, , and Both are greater than zero.

7. A nickel nitrate separation and impurity removal device according to claim 1, characterized in that: The training method of the machine learning model for predicting the amount of pH regulator added includes: Converting the collected characteristic parameters of the initial nickel nitrate solution into a corresponding set of characteristic vectors; Each group of feature vectors is used as the input of the machine learning model, and the machine learning model takes the amount of pH adjuster added corresponding to the characteristic parameters of each group of initial nickel nitrate solutions as the output, and takes the amount of pH adjuster added actually corresponding to the characteristic parameters of each group of initial nickel nitrate solutions as the prediction target, and takes minimizing the loss function value of the machine learning model as the training target; training is stopped when the loss function value of the machine learning model is less than or equal to the preset target loss value.

8. A nickel nitrate separation and impurity removal device according to claim 1, characterized in that: The recommended set of extraction parameters is: ; in, The collection label is The corresponding type of extractant, The collection label is The corresponding amount of extractant is The collection label is The corresponding extraction temperature is The collection label is The corresponding extraction time.

9. A nickel nitrate separation and impurity removal device according to claim 8, characterized in that: The training method of the extraction parameter recommendation model includes: Set the extraction parameter recommendation set with corresponding numbers in advance; The characteristic parameters of the extraction pH value and the initial nickel nitrate solution are converted into a corresponding set of feature vectors, and each set of feature vectors is used as the input of the machine learning model. The machine learning model uses a set of extraction parameter recommendation set numbers corresponding to each set of extraction pH value and the characteristic parameters of the initial nickel nitrate solution as output, and a set of extraction parameter recommendation set numbers actually corresponding to each set of extraction pH value and the characteristic parameters of the initial nickel nitrate solution as a prediction target, and minimizing the loss function value of the machine learning model as a training target; training is stopped when the loss function value of the machine learning model is less than or equal to a preset target loss value.

10. A method for separating and removing impurities from nickel nitrate, based on a device for separating and removing impurities from nickel nitrate as claimed in any one of claims 1 to 4, characterized in that: The following steps are involved: Passing the initial nickel nitrate solution to be treated into an impurity filter (1) for preliminary filtration to remove insoluble solid impurities; The filtered nickel nitrate solution is added into the extraction reactor (2), and a pH regulator is added into the extraction reactor (2) through a dosing component (21) to adjust the acidity of the solution to a range suitable for the working of the extractant; Adding an extractant into the extraction reactor (2), and controlling the operation of the heater (23) and the stirring assembly (22) in the extraction reactor (2) to heat and stir the liquid in the extraction reactor (2), thereby ensuring that the reaction is carried out at a suitable temperature and that the solution and the extractant are fully mixed; The extracted solution and the extractant are separated by a centrifuge (3), the target metal is enriched in the extractant, the extractant enriched with the target metal is introduced into the extraction reactor (2) again, and the target metal is separated from the extractant by adding a stripping agent; The stripping liquid is filtered to remove residual impurities, and then concentrated and crystallized through an evaporator (4) and a crystallizer (5) to obtain a high-purity nickel nitrate product.