Glass spontaneous explosion defect detection method
Through photoelastic detection and internal impurity scanning, the risk of self-destruction of glass in high-rise buildings is identified, and the problem of self-destruction of tempered glass is solved, and the rapid and effective risk assessment and prevention measures are achieved, ensuring the safety and image of the building.
Patent Information
- Application Number
- CN202411080750.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-08
- Publication Date
- 2024-11-15
AI Technical Summary
Due to its own characteristics, tempered glass in high-rise buildings has hidden dangers of self-explosion. Frequent extreme weather causes the detection of self-explosion of glass to become urgent, and an effective detection method is needed to ensure personnel safety and building image.
The surface stress detection of glass is carried out by photoelastic method, combined with curtain wall glass software modeling analysis and internal impurity scanning, and the surface stress high area is calibrated through a polarizer full disk scanning, determine the glass stress state, and scan the internal impurity for abnormal parts to determine the impurity type and size, identify the risk of self-destruction.
Quickly find areas with high stress values, identify the risk of glass self-destruction, replace glass if necessary, eliminate self-destruction risks in advance, improve building safety and credibility, and are suitable for projects with urgent construction periods.
Smart Images

Figure CN118962092A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of glass defect detection, and in particular to a glass self-explosion defect detection method. Background Art
[0002] Curtain walls are widely used in modern buildings, such as high-rise buildings, commercial buildings, urban complexes, public buildings, etc. Among curtain walls, especially high-rise buildings, glass curtain walls account for a high proportion. For safety reasons, tempered glass is widely used. However, due to its own characteristics, tempered glass inevitably has the risk of self-explosion. Considering that the current increasingly warming global climate leads to more frequent extreme weather, it is particularly necessary to check for the hidden dangers of glass self-explosion, which can ensure the safety of personnel and prevent property losses. Especially for high-rise commercial buildings and public places, glass self-explosion accidents will leave people with an impression of unsafety and affect the image and reputation of the building. Summary of the invention
[0003] The present invention can conduct inspections on hidden dangers of self-explosion of glass, discover and deal with problems in a timely manner, improve the image and reputation of the building, and enhance the trust of users and the public in the building.
[0004] To solve the above problems, the technical solution adopted by the present invention is as follows: The present invention is a method for detecting glass self-explosion defects, comprising the following steps:
[0005] Step 1: Photoelastic glass surface stress detection, using a polarizing filter to scan the entire glass and calibrate the area with high surface stress;
[0006] Step 2: Use software modeling to analyze the curtain wall glass to determine the stress state of the glass and compare the consistency with the results of the above-mentioned on-site inspection;
[0007] Step 3: For the parts where the two obviously do not match, it is considered that the local stress state is abnormal, and the equipment is used to perform internal impurity scanning for the location of the stress abnormality;
[0008] Step 4: If no impurities are detected, only the surface stress distribution is judged to be abnormal. If impurities are detected, their size is measured and the type of impurity is determined. If the impurity type is nickel sulfide, if the diameter is between 0.04-0.65 microns, it can be judged as a high risk of self-explosion. If the diameter is below 0.04 microns, it is judged to be a glass with a special risk of self-explosion.
[0009] The beneficial effects achieved by the present invention using the above structure are as follows:
[0010] 1. Perform photoelastic testing on curtain wall glass to determine the surface stress distribution, perform internal impurity scans on areas where the surface stress is significantly greater than the surrounding area, analyze the impurities found, determine the size of the impurities, and divide the self-explosion risk. Through inspection, find glass with high self-explosion risk, evaluate it, and replace the glass if necessary to eliminate the risk of self-explosion in advance.
[0011] 2. On-site inspection is simple and easy, and the initial surface stress screening is fast. It can quickly find areas with high stress values and lay the foundation for the subsequent impurity scanning. Based on the results of the internal impurity scanning, the risk of glass self-explosion can be identified, which has certain practical significance for projects with tight construction schedules. BRIEF DESCRIPTION OF THE DRAWINGS
[0012] Figure 1 A physical picture of unknown impurities in a method for detecting self-explosion defects in glass proposed by the present invention;
[0013] Figure 2 A physical picture of yellow nickel sulfide in a method for detecting glass self-explosion defects proposed by the present invention;
[0014] Figure 3 A physical picture of bubbles in a glass self-explosion defect detection method proposed by the present invention;
[0015] Figure 4 This is a glass scanning diagram of a glass self-explosion defect detection method proposed by the present invention. DETAILED DESCRIPTION
[0016] like Figure 1 to Figure 4 As shown, the present invention is a method for detecting glass self-explosion defects. Specific embodiment 1
[0018] The present invention is a method for detecting glass self-explosion defects, comprising the following steps:
[0019] Step 1: Photoelastic glass surface stress detection, using a polarizing filter to scan the entire glass and calibrate the area with high surface stress;
[0020] Step 2: Use software modeling to analyze the curtain wall glass to determine the stress state of the glass and compare the consistency with the results of the above-mentioned on-site inspection;
[0021] Step 3: For the parts where the two obviously do not match, it is considered that the local stress state is abnormal, and the equipment is used to perform internal impurity scanning for the location of the stress abnormality;
[0022] Step 4: If no impurities are scanned, it is only judged that the surface stress distribution is abnormal. If impurities are scanned, their size is measured and the impurity type is determined. If the impurity type is nickel sulfide, if the diameter is between 0.04 microns, it can be judged as a high risk of self-explosion. If the diameter is 0.01 microns, it is judged as a glass with a special risk of self-explosion. Specific embodiment 2
[0024] The present invention is a method for detecting glass self-explosion defects, comprising the following steps:
[0025] Step 1: Photoelastic glass surface stress detection, using a polarizing filter to scan the entire glass and calibrate the area with high surface stress;
[0026] Step 2: Use software modeling to analyze the curtain wall glass to determine the stress state of the glass and compare the consistency with the results of the above-mentioned on-site inspection;
[0027] Step 3: For the parts where the two obviously do not match, it is considered that the local stress state is abnormal, and the equipment is used to perform internal impurity scanning for the location of the stress abnormality;
[0028] Step 4: If no impurities are scanned, it is only judged that the surface stress distribution is abnormal. If impurities are scanned, their size is measured and the impurity type is determined. If the impurity type is nickel sulfide, if the diameter is between 0.65 microns, it can be judged as a high risk of self-explosion. If the diameter is 0.02 microns, it is judged as a glass with a special risk of self-explosion. Specific embodiment 3
[0030] The present invention is a method for detecting glass self-explosion defects, comprising the following steps:
[0031] Step 1: Photoelastic glass surface stress detection, using a polarizing filter to scan the entire glass and calibrate the area with high surface stress;
[0032] Step 2: Use software modeling to analyze the curtain wall glass to determine the stress state of the glass and compare the consistency with the results of the above-mentioned on-site inspection;
[0033] Step 3: For the parts where the two obviously do not match, it is considered that the local stress state is abnormal, and the equipment is used to perform internal impurity scanning for the location of the stress abnormality;
[0034] Step 4: If no impurities are scanned, it is only judged that the surface stress distribution is abnormal. If impurities are scanned, their size is measured and the impurity type is determined. If the impurity type is nickel sulfide, if the diameter is between 0.35 microns, it can be judged as a high risk of self-explosion. If the diameter is 0.03 microns, it is judged as a glass with a special risk of self-explosion.
[0035] It should be understood that although this specification is described in terms of implementation methods, not every implementation method contains only one independent technical solution. This narrative method of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment may also be appropriately combined to form other implementation methods that can be understood by those skilled in the art.
Claims
1. A method for detecting glass self-explosion defects, Features: The steps include: Step 1: Photoelastic glass surface stress detection, using a polarizing filter to scan the entire glass and calibrate the area with high surface stress; Step 2: Use software modeling to analyze the curtain wall glass to determine the stress state of the glass and compare the consistency with the results of the above-mentioned on-site inspection; Step 3: For the parts where the two obviously do not match, it is considered that the local stress state is abnormal, and the equipment is used to perform internal impurity scanning for the location of the stress abnormality; Step 4: If no impurities are detected, only the surface stress distribution is judged to be abnormal. If impurities are detected, their size is measured and the type of impurity is determined. If the impurity type is nickel sulfide, if the diameter is between 0.04-0.65 microns, it can be judged as a high risk of self-explosion. If the diameter is below 0.04 microns, it is judged to be a glass with a special risk of self-explosion.