Preparation method of negative electrode slurry and negative electrode slurry

By adjusting the process flow and adopting static mixing technology, the blue-blue problem caused by the long coexistence of SBR and CMC in the negative electrode slurry of lithium battery is solved, and the uniformity and adhesion of the slurry are improved, achieving a more efficient preparation process.

CN118970051AActive Publication Date: 2024-11-15XIAOGAN CORNEX NEW ENERGY INNOVATION TECHNOLOGY CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202411136194.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-19
Publication Date
2024-11-15
Estimated Expiration
2044-08-19

AI Technical Summary

Technical Problem

In the existing lithium battery negative electrode slurry preparation method, the long coexistence of SBR and CMC leads to the slurry blue phenomenon, affecting the electrode performance, and the traditional stirring method easily leads to uneven dispersion of SBR and the depressing force.

Method used

By adjusting the process flow, CMC and SBR are added in batches, and static mixing technology is adopted to reduce the coexistence time between SBR and CMC, and static mixing is used to reduce shear force and ensure the uniformity and adhesion of the slurry.

Benefits of technology

It effectively improves the uniformity and adhesion of the slurry, reduces the blue bleaching phenomenon, shortens the preparation time, improves the production efficiency, and enhances the stability and adhesion of the slurry.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure FT_1
    Figure FT_1
  • Figure FT_2
    Figure FT_2
  • Figure FT_3
    Figure FT_3
Patent Text Reader

Abstract

The invention relates to the technical field of lithium batteries, in particular to a preparation method of negative electrode paste and the negative electrode paste, and the preparation method of the negative electrode paste comprises the following steps: dry-mixing a negative electrode active material, a conductive agent and part of CMC in proportion, stirring and dispersing; adding deionized water, kneading and scraping; adding the residual CMC, kneading and scraping; adding deionized water, stirring and dispersing to obtain a mixture; carrying out defoaming treatment on the mixture; and adding the SBR according to the proportion, and uniformly mixing to obtain the negative electrode slurry. The preparation method provided by the invention has the advantage of reducing the coexistence time of mutually exclusive SBR and CMC, and the negative electrode slurry prepared by the preparation method has better uniformity and stronger binding power as the bluing phenomenon of the negative electrode slurry is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of lithium batteries, and in particular to a method for preparing negative electrode slurry and the negative electrode slurry. Background Art

[0002] In the lithium battery industry, lithium-ion battery electrode slurry usually includes electrode active materials, conductive agents and binders. Among them, the use of binders can significantly enhance the adhesion between electrode materials and current collectors and improve the processing performance of slurry. The most commonly used binder choices are CMC (carboxymethyl cellulose) and SBR (polystyrene butadiene copolymer).

[0003] Since the comprehensive performance of lithium batteries is directly affected by the slurry characteristics, optimizing the slurry preparation process is crucial to improving the performance of the battery. At present, many patents for the preparation of negative electrode slurry using CMC and SBR as binders have been reported.

[0004] For example, the invention patent with publication number CN117317222A reported a lithium battery negative electrode slurry and its preparation method, the preparation method comprising mixing graphite, a conductive agent and a first binder (including CMC), adding deionized water to prepare a first slurry; adding a second binder (including CMC) and deionized water to the first slurry to prepare a second slurry; then, under stirring conditions, adding an organic solvent and SBR in sequence, stirring evenly, cooling and defoaming, to obtain the lithium battery negative electrode slurry. For another example, the invention patent with publication number CN118039904A reported a lithium ion battery negative electrode slurry and its homogenization process, the homogenization process adopts an aqueous system combined with a wet process, including a negative electrode slurry (including CMC) and a dry blend, and then mixing and dispersing the negative electrode slurry and the dry blend in steps, adding SBR to the mixed slurry, stirring and dispersing at a low speed, and vacuuming to remove bubbles to obtain the target slurry.

[0005] Since SBR contains negatively charged carboxyl groups and is mutually exclusive with the carboxyl groups on the surface of CMC, when the two coexist for a long time, the SBR particles float up, causing the slurry to "bleach blue", that is, the solid components in the slurry are unevenly distributed, resulting in inconsistent color of the coating layer. In the above-mentioned slurry preparation process, the process flow is to first add SBR and disperse it at a low speed, and then prepare the required negative electrode slurry through defoaming treatment. Taking the slurry parameter test time into account, the coexistence time of SBR and CMC is about 1.5h, which is very easy to bleach blue. This blue-bleached slurry will cause uneven concentration distribution of SBR and reduced adhesion after coating, and then stick to the roller during rolling, affecting battery performance. Summary of the invention

[0006] In order to solve the above problems, the present invention provides a method for preparing a negative electrode slurry and a negative electrode slurry. The preparation method has the advantage of reducing the coexistence time of mutually exclusive SBR and CMC. The blue bleaching phenomenon of the negative electrode slurry prepared by the preparation method is improved, so that it has better uniformity and stronger bonding force.

[0007] To achieve the above-mentioned purpose, the present invention is implemented by the following technical solutions: In a first aspect, the present invention provides a method for preparing a negative electrode slurry, comprising the following steps: S1. Dry mix the negative electrode active material, conductive agent and part of CMC in proportion and stir and disperse; S2. Add deionized water, knead and scrape; S3. Add the remaining CMC, knead and scrape; S4. Add deionized water, stir and disperse to obtain a mixture; S5. Defoaming the mixture; S6. Add SBR in proportion and mix evenly to obtain the negative electrode slurry.

[0008] In conventional negative electrode slurry preparation methods, the long-term coexistence of SBR and CMC can easily cause the slurry to bleach blue. The present invention improves the slurry bleaching blue by adjusting the production process to reduce the coexistence time of SBR and CMC, two mutually exclusive substances. Secondly, the present invention adds CMC in batches, first adding part of CMC to initially form a stable colloidal system, so that the graphite particles are initially wetted and dispersed, and then adding the remaining CMC, which can more effectively wrap and stabilize each particle on the basis of better dispersion and avoid agglomeration.

[0009] Preferably, in step S1, part of the negative electrode active material, the conductive agent, part of the CMC, and the remaining negative electrode active material are added in order according to proportions for dry mixing.

[0010] By adding graphite in batches, the distribution of particles during the mixing process can be better controlled to ensure the uniformity of the slurry.

[0011] Preferably, in order to construct a preliminary colloidal system, a smaller amount of CMC is preferably added. Specifically, in step S1, 25% to 35% of the total amount by mass of CMC is added.

[0012] Preferably, in step S1, the revolution speed is 5-15 rpm and the rotation speed is 750-950 rpm.

[0013] Preferably, in step S2, the material is scraped after kneading at a revolution speed of 5-15 rpm for 8-15 minutes.

[0014] Preferably, in step S3, the material is scraped after kneading at a revolution speed of 5-15 rpm for 45-75 min.

[0015] Preferably, the step S4 further comprises the following steps: S4.1. Add deionized water and disperse at a speed of 5-15 rpm and 1200-1400 rpm for 60-80 min; S4.2 Add deionized water and disperse at a speed of 5-15 rpm and 800-1000 rpm for 20-40 min; The mass of the deionized water added in step S4.1 is greater than the mass of the deionized water added in step S4.2.

[0016] By adding water in stages, the slurry can achieve ideal fluidity and stability. First, add a large amount of deionized water to achieve initial dispersion of the slurry and form a more uniform slurry base. After the initial dispersion of the slurry is completed, adjust the stirring speed to avoid excessive shear force causing damage to the material.

[0017] Preferably, in step S5, the defoaming treatment includes stirring defoaming and / or vacuum defoaming.

[0018] Preferably, in step S5, the stirring and defoaming conditions are stirring and defoaming at a speed of 5-15 rpm and 400-600 rpm for 30 minutes.

[0019] Preferably, in step S6, SBR is added to the defoaming mixture under static mixing conditions.

[0020] Since SBR is a polymer material, when using traditional stirring methods, too high a shear speed will break up the SBR, resulting in low slurry viscosity, poor stability, and a reduced slurry storage period; too low a stirring speed will cause uneven dispersion of SBR in the slurry system, severe slurry bleaching, and further lead to roller sticking during the coating, roller pressing and slitting processes.

[0021] The static mixing does not rely on dynamic stirring blades, but promotes material mixing through static elements. Preferably, in step S6, SBR is added to the defoamed mixture through a pipeline mixer.

[0022] The pipeline mixer uses static elements (such as spiral blades, baffles, etc.) fixed in the pipeline to change the flow path of the fluid and achieve mixing through the kinetic energy of the fluid itself. This method can achieve mixing with lower shear force, reducing the risk of excessive shearing of polymer materials such as SBR, thereby maintaining the appropriate viscosity and stability of the slurry. In addition, under the traditional stirring and mixing method, it takes 15 to 30 minutes to disperse SBR. The rapid mixing ability of the pipeline mixer can complete the dispersion of SBR in a short time, shortening the preparation time while reducing the possibility of long-term contact between SBR and other components in the slurry.

[0023] Preferably, during the preparation of the negative electrode slurry, the reaction temperature is maintained at no higher than 80°C.

[0024] Preferably, the negative electrode slurry comprises the following components in parts by mass: 90~98 parts of negative electrode active material, 0.5~1 parts of conductive agent, 0.3~0.7 parts of CMC, 1.2~2.4 parts of SBR.

[0025] Preferably, the negative electrode active material includes graphite.

[0026] Preferably, the conductive agent includes SP.

[0027] In a second aspect, the present invention further provides a negative electrode slurry prepared according to the above preparation method.

[0028] The beneficial effects of the present invention are: 1. In this application, by adjusting the production process, the coexistence time of SBR and CMC, two mutually exclusive substances, is reduced, the blue bleaching of the slurry is improved, and the uniformity and adhesion of the negative electrode slurry are thereby improved.

[0029] 2. In the present application, a static mixing method is adopted, which can provide a uniform dispersion environment under the condition of relatively low shear force, further improve the blue bleaching phenomenon of the slurry, and save about 15 to 30 minutes in the preparation of each can of slurry, which helps to improve production efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] Figure 1 A schematic diagram of a slurry state of an embodiment of the present invention; Figure 2 It is a schematic diagram of the slurry state of the comparative example of the present invention; Figure 3 It is a box plot of the bonding force of the embodiments of the present invention and the comparative examples. DETAILED DESCRIPTION

[0031] The present invention is further described below in conjunction with the accompanying drawings and specific embodiments of the specification. Those of ordinary skill in the art will be able to implement the present invention based on these descriptions. In addition, the embodiments of the present invention involved in the following description are generally only embodiments of a part of the present invention, rather than all embodiments. Therefore, based on the embodiments of the present invention, all other embodiments obtained by those of ordinary skill in the art without making creative work should fall within the scope of protection of the present invention.

[0032] The raw materials used in the following examples are all conventional chemicals purchased from the market. Example

[0033] The method for preparing the negative electrode slurry of the present invention comprises the following steps: S1. Weigh the materials according to the ratio of artificial graphite: SP: CMC: SBR of 97: 0.7: 0.5: 1.8. Add 50% of the total amount by mass of graphite, SP, 30% of the total amount by mass of CMC, and 50% of the total amount by mass of graphite into the mixer in turn, and disperse them at a speed of 14 rpm and 850 rpm for 30 minutes, and control the temperature not higher than 80°C.

[0034] S2. Add 40% of the total amount by mass of deionized water, control the temperature not higher than 80 ° C, the revolution speed is 14rpm and knead for 10min before scraping; S3. Add 70% of the total amount by mass of CMC, knead at a revolution speed of 14rpm for 60min and scrape; S4. Add 40% of the total amount of deionized water by mass, disperse at a speed of 14 rpm and 1300 rpm for 70 min, and control the temperature not higher than 80 ° C and the vacuum not higher than -90 Kpa; S5. Add 20% of the total amount of deionized water by mass, disperse at a speed of 14 rpm and 900 rpm for 30 min, and control the temperature not higher than 80 ° C and the vacuum degree not higher than -90 Kpa; S6. Stir and defoam at a speed of 14 rpm and 500 rpm for 30 min; S7. Set the SBR flow rate according to the slurry transfer flow rate and add SBR through the pipeline mixer.

[0035] Comparative Example S1. Weigh the materials according to the ratio of artificial graphite: SP: CMC: SBR of 97: 0.7: 0.5: 1.8. Add 50% of the total amount by mass of graphite, SP, 30% of the total amount by mass of CMC, and 50% of the total amount by mass of graphite into the mixer in turn, and disperse them at a speed of 14 rpm and 850 rpm for 30 minutes, and control the temperature not higher than 80°C.

[0036] S2. Add 40% of the total amount by mass of deionized water, control the temperature not higher than 80 ° C, the revolution speed is 14rpm and knead for 10min and then scrape the material; S3. Add 70% of the total amount by mass of CMC, knead at a revolution speed of 14rpm for 60min and scrape; S4. Add 40% of the total amount of deionized water by mass, disperse at a speed of 14 rpm and 1300 rpm for 70 min, and control the temperature not higher than 80 ° C and the vacuum not higher than -90 Kpa; S5. Add 20% of the total amount of deionized water by mass, disperse at a speed of 14 rpm and 900 rpm for 30 min, and control the temperature not higher than 80 ° C and the vacuum degree not higher than -90 Kpa; S6. After adding SBR, disperse at a speed of 14 rpm and 900 rpm for 25 minutes, and control the temperature not higher than 80°C and the vacuum degree not higher than -90Kpa; S7. Stir and defoam at a speed of 14 rpm and 500 rpm for 30 min.

[0037] Depend on Figure 1 and Figure 2 It can be seen that the blue bleaching area of ​​the embodiment is about 1.5cm 2 The blue bleaching area of ​​the comparative example is about 3.2cm 2 Compared with the comparative example, the blue bleaching area of ​​the negative electrode slurry in the embodiment is significantly reduced, and the blue bleaching phenomenon is significantly improved, which directly reflects that the dispersion of SBR in the slurry is more uniform.

[0038] The slurries obtained in the examples and comparative examples were made into pole pieces and rolled, and 62 groups of samples were taken respectively, and their bonding strength was tested to obtain the following Figure 3 Box plot of the bonding force shown. Figure 3 It can be seen that the bonding force of the embodiment is significantly improved compared with the comparative example, with the improvement being about 25%.

Claims

1. A method for preparing a negative electrode slurry, characterized in that: The steps include: S1. Dry mix the negative electrode active material, conductive agent and part of CMC in proportion and stir and disperse; S2. Add deionized water, knead and scrape; S3. Add the remaining CMC, knead and scrape; S4. Add deionized water, stir and disperse to obtain a mixture; S5. Defoaming the mixture; S6. Add SBR in proportion and mix evenly to obtain the negative electrode slurry.

2. The method for preparing negative electrode slurry according to claim 1, characterized in that: In the step S1, part of the negative electrode active material, the conductive agent, part of the CMC, and the remaining negative electrode active material are added in order according to proportion and dry mixed.

3. The method for preparing negative electrode slurry according to claim 1, characterized in that: In the step S1, CMC is added in a total amount of 25% to 35% by mass.

4. The method for preparing negative electrode slurry according to claim 1, characterized in that: The step S4 further comprises the following steps: S4.

1. Add deionized water and disperse at a speed of 5-15 rpm and 1200-1400 rpm for 60-80 min; S4.2 Add deionized water and disperse at a speed of 5-15 rpm and 800-1000 rpm for 20-40 min; The mass of the deionized water added in step S4.1 is greater than the mass of the deionized water added in step S4.

2.

5. The method for preparing negative electrode slurry according to claim 1, characterized in that: In the step S5, the defoaming treatment method includes stirring defoaming and / or vacuum defoaming.

6. The method for preparing negative electrode slurry according to claim 1, characterized in that: In the step S6, SBR is added to the defoamed mixture under static mixing conditions.

7. The method for preparing negative electrode slurry according to claim 1, characterized in that: The negative electrode slurry comprises the following components in parts by mass: 90~98 parts of negative electrode active material, 0.5~1 parts of conductive agent, 0.3~0.7 parts of CMC, 1.2~2.4 parts of SBR.

8. The method for preparing negative electrode slurry according to claim 1, characterized in that: The negative electrode active material includes graphite.

9. The method for preparing negative electrode slurry according to claim 1, characterized in that: The conductive agent includes SP.

10. A negative electrode slurry, characterized in that , Prepared according to the preparation method according to any one of claims 1 to 9.

Citation Information

Patent Citations

  • Preparation method of lithium ion power battery cathode

    CN106848205A

  • Method for preparing lithium ion battery negative electrode slurry

    CN107749460A

  • Lithium ion battery silicon-based negative electrode adhesive and preparation method of negative electrode piece with same

    CN107959027A

  • Negative electrode composite thickening agent, negative electrode pole piece and preparation method

    CN112382757A

  • Lithium ion battery negative electrode slurry and homogenizing process thereof

    CN118039904A