Anti-vibration branch pipe of nuclear power plant and processing method thereof

The integrated molding design of the nuclear power plant's vibration-resistant branch pipe solves the problem of weld fatigue at the connection between the small branch pipe and the main pipe, achieving structural optimization and cost reduction, and improving the operational reliability and economy of the nuclear power plant.

CN118977069AActive Publication Date: 2024-11-19YANGJIANG NUCLEAR POWER +1
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411313840.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-19
Publication Date
2024-11-19
Estimated Expiration
2044-09-19

AI Technical Summary

Technical Problem

The welds at the connection between the small branch pipes and the main pipe in nuclear power plants are susceptible to vibration stress fatigue, which can lead to connection failure. Existing technologies cannot effectively solve this problem, and the cost of overhaul and inspection is high.

Method used

A topology optimization method was used to design an integrally formed vibration-resistant branch pipe for nuclear power plants, including a smooth transition between the branch pipe body and the pipe seat. Through heat treatment, deep hole drilling, CNC lathe machining, and quality control, the structural strength and stress distribution were optimized.

Benefits of technology

It eliminates the risk of weld vibration fatigue fracture, simplifies the installation and maintenance process, reduces maintenance costs, and improves the vibration fatigue safety and operational reliability of nuclear power plant branch pipes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118977069A_ABST
    Figure CN118977069A_ABST
Patent Text Reader

Abstract

The invention discloses a nuclear power plant anti-vibration branch pipe and a machining method thereof. The nuclear power plant anti-vibration branch pipe comprises a branch pipe body and a pipe base integrally formed with the branch pipe body. The processing method of the anti-vibration branch pipe of the nuclear power plant is simple in design, convenient to implement in batches and wide in application range, and the anti-vibration branch pipes of different specifications of the nuclear power plant can be processed by adopting the optimal design and the processing method. Due to the fact that the anti-vibration branch pipe of the nuclear power plant is integrally formed, butt welding seams are eliminated, the problem of unit power reduction or shutdown caused by vibration fatigue fracture of the welding seams is thoroughly solved, and the risk of fatigue fracture of the branch pipe due to vibration is greatly reduced. Due to the integral forming design, welding connection is avoided, the field installation process is simplified, the installation efficiency is improved, the number of welding joints is reduced, and the maintenance and overhaul cost is reduced. Therefore, the method has remarkable advantages of improving the vibration fatigue safety of the branch pipe of the nuclear power plant and improving the operation reliability and economical efficiency of the power plant.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of nuclear power plant safety, and in particular to a vibration-resistant branch pipe of a nuclear power plant and a processing method thereof. Background Art

[0002] A large number of small branch pipes (outer diameter less than 50mm) are used in nuclear power plants for pressure measurement, flow measurement, drainage or exhaust. These small branch pipes are usually connected to the main pipe by a pipe socket. One end of the pipe socket is welded to the main pipe, and the other end is welded to the branch pipe, that is, the "main pipe-weld-pipe socket-weld-branch pipe" structure. When the main pipe vibrates, the branch pipe vibrates due to the excitation of the main pipe. Since the outer diameter and wall thickness of the pipe socket are much larger than the branch pipe, its structural strength is high and it is not easy to crack and fail. The connection weld between the pipe socket and the branch pipe is usually the location with the greatest vibration stress, and the connection transition is mostly a right-angle transition, with a large local stress concentration. Therefore, it is a weak area of ​​the entire pipe. If fatigue cracking occurs, it may cause the pipeline system to fail to operate normally, or even cause the unit to shut down.

[0003] To address this problem, existing technologies mainly involve adding integrated brackets to small branch pipes to limit their displacement and performing non-destructive testing on welds during overhaul. However, the following problems exist: (1) When there is a large displacement of the main pipe, an excessively high average stress will be formed at the weld between the pipe seat and the branch pipe, reducing the fatigue resistance of the branch pipe; (2) When the main pipe vibrates at high frequency, the high-frequency vibration is transmitted to the branch pipe through the additional bracket, converting the original single-point excitation into multi-point excitation, and the vibration response is actually worsened; (3) Non-destructive testing of welds during overhaul requires a lot of service cooperation work, such as building scaffolding and removing insulation, which has high economic costs.

[0004] In the prior art, the design of branch pipe seats is often based on experience or simple mechanical calculations, which cannot ensure the optimal performance of the structure. Summary of the invention

[0005] The technical problem to be solved by the present invention is to provide a vibration-resistant branch pipe for a nuclear power plant and a processing method thereof.

[0006] The technical solution adopted by the present invention to solve the technical problem is: a processing method for constructing a vibration-resistant branch pipe of a nuclear power plant, wherein the vibration-resistant branch pipe of the nuclear power plant comprises a branch pipe body and a pipe seat integrally formed with the branch pipe body, and the processing method comprises the following steps:

[0007] S1: Determine the interface size between the pipe seat and the mother pipe, as well as the outer diameter, wall thickness and length parameters of the branch pipe body, use the topology optimization method to make a smooth transition between the pipe seat and the branch pipe body, obtain the optimal structure of the pipe seat, and draw a processing drawing of the vibration-resistant branch pipe of the nuclear power plant;

[0008] S2: heat treating the workpiece for manufacturing the anti-vibration branch pipe of the nuclear power plant;

[0009] S3: performing deep hole drilling on the workpiece after heat treatment;

[0010] S4: performing rough machining on the workpiece after deep hole drilling by using a CNC lathe;

[0011] S5: removing residual stress from the workpiece after rough machining;

[0012] S6: using a CNC lathe to perform finish machining on the workpiece after the residual stress is removed;

[0013] S7: Performing quality control and inspection on the workpiece after processing.

[0014] In some embodiments, the topology optimization method includes:

[0015] S11: According to the interface size between the pipe seat and the mother pipe and the outer diameter, wall thickness and length parameters of the branch pipe body, a finite element model is established, constraints on the size limit of the pipe seat are set, and material structure parameters are defined. The material structure parameters include elastic modulus, Poisson's ratio, structural damping and material density;

[0016] S12: setting a preset bending moment load, carrying out static calculation and modal calculation of the initial model of the pipe socket under the preset bending moment load, and obtaining the structural strength, stress and first-order modal characteristics of the initial model of the pipe socket under the preset bending moment load;

[0017] S13: The variable density method is used to perform topological optimization on the structure of the initial model of the pipe socket, and a preset material retention rate is set to obtain an optimized model of the pipe socket with maximum structural strength, minimum stress and highest first-order modal frequency under a preset bending moment load;

[0018] S14: According to the structural performance and production process requirements of the tube socket, the optimization model is geometrically optimized, and the optimization model is fitted and optimized using a spline curve method to obtain the optimal model of the tube socket.

[0019] In some embodiments, in step S2, the workpiece is a forging, the forging is made of stainless steel, and the heat treatment temperature is 1040°C to 1065°C.

[0020] In some embodiments, step S3 includes:

[0021] S31: Fixing the heat-treated workpiece on a workbench of a drilling machine and clamping it with a fixture;

[0022] S32: setting a suitable rotation speed, feed rate and cutting depth according to the workpiece material and the type of drill bit;

[0023] S33: Start the drilling machine and start deep hole drilling;

[0024] S34: performing chip removal;

[0025] S35: After drilling is completed, use measuring tools to measure and inspect the processed holes of the anti-vibration branch pipes of the nuclear power plant to ensure that their size and position accuracy meet the requirements;

[0026] S36: cleaning the coolant and chips on the surface of the workpiece.

[0027] In some embodiments, step S4 includes:

[0028] S41: Mounting the workpiece on a CNC lathe, ensuring that the workpiece is stable and correctly aligned;

[0029] S42: selecting a suitable first tool according to the material of the workpiece and the requirements of rough machining;

[0030] S43: setting a feed path of the first tool and cutting parameters of the workpiece in a programming system of a CNC lathe;

[0031] S44: adjusting a suitable cutting speed and feed rate according to the material of the workpiece and the performance of the first tool;

[0032] S45: Start the CNC lathe to perform rough machining;

[0033] S46: After the rough machining is completed, check whether there is any residual oxide layer, rust or scratches on the surface of the workpiece. If the rough machining requirements are not met, perform rough machining again;

[0034] S47: cleaning iron filings and oil stains on the surface of the workpiece.

[0035] In some embodiments, in step S5, the heat treatment temperature for removing residual stress from the workpiece after rough machining is 300°C to 350°C.

[0036] In some embodiments, step S6 includes:

[0037] S61: Mounting the workpiece on a CNC lathe;

[0038] S62: Select the appropriate second tool and grinding wheel according to the processing requirements;

[0039] S63: setting a feed path of the second tool and cutting parameters of the workpiece in a programming system of a CNC lathe;

[0040] S64: adjusting a suitable cutting speed and feed rate according to the material of the workpiece and the performance of the second tool;

[0041] S65: Start the CNC lathe for finishing;

[0042] S66: After finishing, the workpiece is measured and inspected using a measuring tool to ensure that the size and shape accuracy meet the requirements. If the finishing requirements are not met, finishing is performed again;

[0043] S67: cleaning the grinding fluid and iron filings on the surface of the workpiece, and performing rust prevention treatment.

[0044] In some embodiments, step S7 includes:

[0045] S71: Dimension and shape accuracy inspection, use measuring tools such as outside micrometer and roundness tester to inspect the dimension and shape accuracy of the finished workpiece to ensure that it meets the design requirements;

[0046] S72: Surface quality inspection, observe whether there are scratches, cracks, rust and other defects on the workpiece surface, and take corresponding measures;

[0047] S73: Handling of unqualified products. Products that fail the inspection will be scrapped to ensure that all processed nuclear power plant anti-vibration branches meet the quality standards.

[0048] In this embodiment, a vibration-resistant branch pipe of a nuclear power plant is also constructed, which includes a branch pipe body and a pipe seat integrally formed with the branch pipe body, and there is a smooth transition between the branch pipe body and the pipe seat.

[0049] In some embodiments, the branch tube body has a diameter of 14 mm to 27 mm, a wall thickness of 2 mm to 4 mm, and a length of 100 mm to 1200 mm;

[0050] The length of the tube seat is 70mm to 80mm, the inner diameter is 8mm to 15mm, and the maximum outer diameter is 40mm to 60mm.

[0051] The implementation of the present invention has the following beneficial effects: the processing method of the vibration-resistant branch pipe of the nuclear power plant is simple in design, easy to implement in batches, and has a wide range of applications. The optimized design and processing method can be used to process the vibration-resistant branch pipes of nuclear power plants of different specifications. Since the vibration-resistant branch pipe of the nuclear power plant adopts an integrated design, compared with the existing "branch seat-butt weld-branch pipe" structure, the butt weld is eliminated, and the unit power reduction or shutdown caused by weld vibration fatigue fracture is completely solved, greatly reducing the risk of branch pipe fatigue fracture due to vibration. The integrated design avoids welding connections, simplifies the on-site installation process, and improves installation efficiency. The integrated design reduces the number of welding joints and reduces maintenance and overhaul costs. Therefore, the present invention has significant advantages in improving the vibration fatigue safety of nuclear power plant branches and improving the reliability and economy of power plant operations. BRIEF DESCRIPTION OF THE DRAWINGS

[0052] In order to more clearly illustrate the technical solution of the present invention, the present invention will be further described below in conjunction with the accompanying drawings and embodiments. It should be understood that the following drawings only show certain embodiments of the present invention and should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without creative work. In the drawings:

[0053] Figure 1 is a schematic structural diagram of a nuclear power plant anti-vibration branch pipe in some embodiments of the present invention;

[0054] Figure 2 It is a schematic flow chart of a method for processing anti-vibration branch pipes of a nuclear power plant in some embodiments of the present invention;

[0055] Figure 3 It is a schematic diagram of a finite element model of a vibration-resistant branch pipe of a nuclear power plant in some embodiments of the present invention. DETAILED DESCRIPTION

[0056] In order to have a clearer understanding of the technical features, purposes and effects of the present invention, the specific embodiments of the present invention are now described in detail with reference to the accompanying drawings. In the following description, it should be understood that the directions or positional relationships indicated by "front", "back", "up", "down", "left", "right", "longitudinal", "horizontal", "vertical", "horizontal", "top", "bottom", "inside", "outside", "head", "tail", etc. are based on the directions or positional relationships shown in the accompanying drawings, are constructed and operated in a specific direction, and are only for the convenience of describing the present technical solution, rather than indicating that the device or element referred to must have a specific direction, and therefore cannot be understood as a limitation to the present invention.

[0057] It should also be noted that, unless otherwise clearly specified and limited, the terms such as "installed", "connected", "connected", "fixed", "set" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral one; it can be a mechanical connection or an electrical connection; it can be directly connected or indirectly connected through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. When an element is referred to as being "on" or "under" another element, the element can be "directly" or "indirectly" located on the other element, or there may be one or more intermediate elements. The terms "first", "second", "third", etc. are only for the convenience of describing the present technical solution, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first", "second", "third", etc. can explicitly or implicitly include one or more of the features. For those of ordinary skill in the art, the specific meanings of the above terms in the present invention can be understood according to the specific circumstances.

[0058] See also Figure 1 , is a vibration-resistant branch pipe for a nuclear power plant in some embodiments of the present invention, which includes a branch pipe body 1 and a pipe seat 2 integrally formed with the branch pipe body 1, and a smooth transition between the branch pipe body 1 and the pipe seat 2. It can be understood that in the old technology, the small branch pipe is connected to the mother pipe, and the vibration of the mother pipe forms an exciting force on the small branch pipe. This exciting force is usually unavoidable, and vibration fatigue cracking is prone to occur at the connecting weld between the pipe seat 2 and the branch pipe body 1. In this embodiment, the branch pipe body 1 and the pipe seat 2 are designed as an integrated structure, and the original weld structure is cancelled. The pipe seat 2 and the branch pipe body 1 adopt an integrated smooth transition, which greatly reduces stress concentration and eliminates the discontinuity of material properties, completely solving the problem of branch pipe vibration fatigue failure, and can also reduce on-site welding work and reduce non-destructive testing of welds after installation and overhaul. At the same time, the bracket layout can be simplified, and the economy is high.

[0059] The branch pipe body 1 has a diameter of 14 mm to 27 mm, a wall thickness of 2 mm to 4 mm, and a length of 100 mm to 1200 mm. The branch pipe body 1 preferably has a diameter of 16 mm, a wall thickness of 3 mm, and a length of 1000 mm. The pipe base 2 has a length of 70 mm to 80 mm, an inner diameter of 8 mm to 15 mm, and a maximum outer diameter of 40 mm to 60 mm. The pipe base 2 preferably has a length of 74 mm, an inner diameter of 10 mm, and a maximum outer diameter of 46 mm.

[0060] In this embodiment, if Figure 2 As shown, a design and processing method for a vibration-resistant branch pipe of a nuclear power plant is also constructed, which includes the steps of:

[0061] S1: Determine the interface size between the pipe seat 2 and the mother pipe, as well as the outer diameter, wall thickness and length parameters of the branch pipe body 1, use the topology optimization method to make a smooth transition between the pipe seat 2 and the branch pipe body 1, obtain the optimal structure of the pipe seat 2, and draw the processing diagram of the vibration-resistant branch pipe of the nuclear power plant;

[0062] S2: Heat treatment of workpieces used to manufacture vibration-resistant branch pipes for nuclear power plants;

[0063] S3: deep hole drilling of the workpiece after heat treatment;

[0064] S4: Rough machining of the workpiece after deep hole drilling is performed using a CNC lathe;

[0065] S5: Remove residual stress from the workpiece after rough machining;

[0066] S6: Use a CNC lathe to perform fine machining on the workpiece after the residual stress is removed;

[0067] S7: Perform quality control and inspection on the workpiece after processing.

[0068] Specifically, in step S1, the topology optimization method includes:

[0069] S11: according to the interface size between the pipe seat 2 and the mother pipe and the outer diameter, wall thickness and length parameters of the branch pipe body 1, a finite element model is established, constraints on the size limit of the pipe seat 2 are set, and material structure parameters are defined, the material structure parameters including elastic modulus, Poisson's ratio, structural damping and material density;

[0070] S12: setting a preset bending moment load, performing static calculation and modal calculation of the initial model of the pipe seat 2 under the preset bending moment load, and obtaining the structural strength, stress and first-order modal characteristics of the initial model of the pipe seat 2 under the preset bending moment load;

[0071] S13: topologically optimizing the structure of the initial model of the pipe base 2 by using a variable density method, setting a preset material retention rate, and obtaining an optimized model of the pipe base 2 with maximum structural strength, minimum stress, and highest first-order modal frequency under a preset bending moment load;

[0072] S14: According to the structural performance and production process requirements of the tube socket 2 , the optimization model is geometrically optimized, and the optimization model is fitted and optimized using a spline curve method to obtain an optimal model of the tube socket 2 .

[0073] like Figure 3As shown, the left side is the initial model of the pipe socket 2, and the right side is the optimal model of the pipe socket 2. It can be understood that the topology optimization method is a mathematical method for optimizing the material distribution in a given area according to given load conditions, constraints and performance indicators. It is a kind of structural optimization. The use of this topology optimization method can obtain the optimal shape of the pipe socket 2 to ensure the mechanical properties of the anti-vibration branch pipe of the nuclear power plant as a whole when in use. Specifically, in step S11, the material can be specifically defined as 316L stainless steel, and the elastic modulus, Poisson's ratio, structural damping and material density corresponding to 316L stainless steel are input. In step S12, the preset bending moment load can be set according to actual production needs. The static calculation and modal calculation are algorithms based on the prior art of finite element software. Through this static calculation and modal calculation, the structural strength, stress and first-order modal characteristics of the initial model of the pipe socket 2 under the preset bending moment load can be obtained. In addition, in step S13, the variable density method topology optimization is a density-based topology optimization method, which optimizes the topological structure by defining any point in the design area as a material or void with different densities. The basic idea is to regard the material density distribution in the initial area as a set of multidimensional data, and then use various mathematical methods and algorithms to process these data to generate the optimal structure. In this embodiment, the preset material retention rate is set to 50%, and the preset material retention rate can be adjusted according to actual conditions. In step S14, the optimization model can be geometrically optimized, and the spline curve method can be used to fit and optimize the optimization model to obtain the optimal model of the tube seat 2, that is, to finally determine the specific size of the tube seat 2 to ensure that the shape transition of the tube seat 2 is smooth, avoid stress concentration, meet the structural performance and production process requirements, and have manufacturability.

[0074] In addition, in step S1, SolidWorks software can be used to draw a processing diagram of the anti-vibration branch pipe of the nuclear power plant.

[0075] In step S2, the workpiece is a forging, which is made of stainless steel and the heat treatment temperature is 1040°C to 1065°C. The anti-vibration branch pipe of the nuclear power plant is made of forgings, which are heat treated and then machined. In this embodiment, 316L stainless steel is used for production, and the heat treatment temperature is preferably set to 1050°C.

[0076] Further, step S3 includes:

[0077] S31: Fix the heat-treated workpiece on the workbench of the drilling machine and clamp it with a fixture to ensure the accurate and stable position of the workpiece. Specific fixtures or auxiliary supports can be used;

[0078] S32: according to the workpiece material and the type of drill bit, set the appropriate speed, feed rate and cutting depth. In this embodiment, the speed is set to 1100, the feed rate is set to 20 mm, and the cutting depth is set to 0.1 mm;

[0079] S33: Start the drilling machine and start deep hole drilling. During the processing, the operator should closely monitor the status of the drill bit and the flow of coolant to ensure the stability of the processing;

[0080] S34: Chip removal. Since the chips generated by deep hole drilling are long and difficult to be discharged naturally, it is necessary to effectively manage the discharge of chips to avoid clogging the drill bit and damaging the workpiece.

[0081] S35: After drilling is completed, use measuring tools to measure and inspect the processed holes of the anti-vibration branch pipe of the nuclear power plant to ensure that its size and position accuracy meet the requirements. The measuring tools can be internal diameter micrometers and depth gauges;

[0082] S36: Clean the coolant and chips on the workpiece surface to ensure the quality of the workpiece.

[0083] In addition, in step S4, the workpiece after deep hole drilling is rough-machined using a CNC lathe, that is, the workpiece is preliminarily machined on the CNC lathe, mainly to remove the oxide layer, rust, scratches, etc. on the surface of the workpiece, laying the foundation for subsequent fine machining. This step S4 includes:

[0084] S41: Install the workpiece on the CNC lathe, ensuring that the workpiece is stable and properly aligned. The workpiece can be mounted on the chuck or fixture of the CNC lathe;

[0085] S42: Select the appropriate first tool according to the material of the workpiece and the requirements of rough machining. Rough machining usually uses a large amount of cutting, so it is necessary to select a tool with good rigidity;

[0086] S43: setting a feed path of the first tool and cutting parameters of the workpiece in a programming system of the CNC lathe, where the cutting parameters may be a preset cutting speed, feed rate, and cutting depth;

[0087] S44: According to the material of the workpiece and the performance of the first tool, the appropriate cutting speed and feed rate are adjusted. A larger cutting depth and feed rate are usually used during rough machining to improve machining efficiency. In step S4, the cutting speed of the CNC lathe is set to S600, the feed rate is 0.12 mm, and the cutting depth is 1 mm.

[0088] S45: Start the CNC lathe and perform rough machining. During the machining process, the operator should closely monitor the cutting process to ensure stable machining and avoid abnormalities;

[0089] S46: After the rough machining is completed, check whether there is any residual oxide layer, rust or scratches on the surface of the workpiece. If it does not meet the rough machining requirements, perform rough machining again;

[0090] S47: Clean the iron filings and oil stains on the surface of the workpiece to prepare for subsequent finishing.

[0091] In step S5, the heat treatment temperature for removing residual stress of the workpiece after rough machining is 300° C. to 350° C. It can be understood that machining residual stress will be formed on the surface of the workpiece after deep hole drilling and rough machining, so the workpiece needs to be heat treated to eliminate the residual stress.

[0092] In step S6, the workpiece is processed with high precision on a CNC lathe to obtain the final size, shape and surface quality required for the workpiece. Step S6 includes:

[0093] S61: Install the workpiece on the CNC lathe to ensure that the workpiece is installed on the lathe with accurate position and firm clamping, and can use the center hole or top support;

[0094] S62: Select the appropriate second tool and grinding wheel according to the processing requirements, specifically, a high-precision turning tool and a fine-grained grinding wheel;

[0095] S63: setting a feed path of the second tool and cutting parameters of the workpiece in the programming system of the CNC lathe. Specifically, inputting or selecting a suitable machining program in the programming system of the CNC lathe. The program should include the feed path of the tool, cutting parameters (such as cutting speed, feed amount, cutting depth), etc.;

[0096] S64: According to the material of the workpiece and the performance of the second tool, adjust the appropriate cutting speed and feed rate, and use a smaller cutting depth and feed rate during finishing to improve machining accuracy;

[0097] S65: Start the CNC lathe and perform fine machining. During the machining process, the operator should closely monitor the cutting process to ensure stable machining and avoid abnormalities;

[0098] S66: After finishing, use measuring tools to measure and inspect the workpiece to ensure that its size and shape accuracy meet the requirements. If it does not meet the finishing requirements, then perform finishing. The measuring tool can be an outside diameter micrometer, roundness meter, etc.

[0099] S67: Clean the grinding fluid and iron chips on the workpiece surface and perform rust prevention treatment.

[0100] Among them, in order to ensure the processing quality, fine processing can be done multiple times.

[0101] In step S6, the cutting speed of the CNC lathe is set to S800, the feed rate is set to 0.1 mm, and the cutting depth is set to 0.3 mm.

[0102] In step S7, in order to ensure the processing quality of the anti-vibration branch pipe of the nuclear power plant, strict quality control needs to be carried out after all processing is completed. This step S7 includes:

[0103] S71: Dimension and shape accuracy inspection, use measuring tools such as outside micrometer and roundness tester to inspect the dimension and shape accuracy of the finished workpiece to ensure that it meets the design requirements;

[0104] S72: Surface quality inspection, observe whether there are scratches, cracks, rust and other defects on the workpiece surface, and take corresponding measures;

[0105] S73: Handling of unqualified products. Products that fail the inspection will be scrapped to ensure that all processed nuclear power plant anti-vibration branches meet the quality standards.

[0106] It can be understood that the processing method of the vibration-resistant branch pipe of the nuclear power plant is simple in design, easy to implement in batches, and has a wide range of applications. For the vibration-resistant branch pipes of nuclear power plants of different specifications, this optimized design and processing method can be used for processing. Since the vibration-resistant branch pipe of the nuclear power plant adopts an integrated design, compared with the existing "branch seat-butt weld-branch pipe" structure, the butt weld is eliminated, and the unit power reduction or shutdown caused by the vibration fatigue fracture of the weld is completely solved, and the risk of fatigue fracture of the branch pipe due to vibration is greatly reduced. The one-piece design avoids welding connections, simplifies the on-site installation process, and improves installation efficiency. The one-piece design reduces the number of welding joints and reduces maintenance and overhaul costs. Therefore, the present invention has significant advantages in improving the vibration fatigue safety of nuclear power plant branches and improving the reliability and economy of power plant operations.

[0107] It can be understood that the above embodiments only express the preferred implementation modes of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the patent scope of the present invention. It should be pointed out that, for ordinary technicians in this field, without departing from the concept of the present invention, the above technical features can be freely combined, and several deformations and improvements can be made, which all belong to the protection scope of the present invention. Therefore, all equivalent changes and modifications made to the scope of the claims of the present invention should belong to the scope covered by the claims of the present invention.

Claims

1. A method for processing a vibration-resistant branch pipe of a nuclear power plant, the vibration-resistant branch pipe of the nuclear power plant comprising a branch pipe body (1) and a pipe seat (2) integrally formed with the branch pipe body (1), characterized in that: Includes steps: S1: determining the interface dimensions between the pipe seat (2) and the mother pipe, and the outer diameter, wall thickness and length parameters of the branch pipe body (1), using a topology optimization method to achieve a smooth transition between the pipe seat (2) and the branch pipe body (1), obtaining the optimal structure of the pipe seat (2), and drawing a processing diagram of the anti-vibration branch pipe of the nuclear power plant; S2: heat treating the workpiece for manufacturing the anti-vibration branch pipe of the nuclear power plant; S3: performing deep hole drilling on the workpiece after heat treatment; S4: performing rough machining on the workpiece after deep hole drilling by using a CNC lathe; S5: removing residual stress from the workpiece after rough machining; S6: using a CNC lathe to perform finish machining on the workpiece after the residual stress is removed; S7: Performing quality control and inspection on the workpiece after processing.

2. The method for processing anti-vibration branch pipes of nuclear power plants according to claim 1, characterized in that: The topology optimization method comprises: S11: according to the interface size between the pipe seat (2) and the mother pipe and the outer diameter, wall thickness and length parameters of the branch pipe body (1), a finite element model is established, constraint conditions on the size limit of the pipe seat (2) are set, and material structure parameters are defined, the material structure parameters including elastic modulus, Poisson's ratio, structural damping and material density; S12: setting a preset bending moment load, carrying out static calculation and modal calculation of the initial model of the pipe seat (2) under the preset bending moment load, and obtaining the structural strength, stress and first-order modal characteristics of the initial model of the pipe seat (2) under the preset bending moment load; S13: topological optimization is performed on the structure of the initial model of the pipe seat (2) using a variable density method, a preset material retention rate is set, and an optimized model of the pipe seat (2) with maximum structural strength, minimum stress and highest first-order modal frequency under a preset bending moment load is obtained; S14: geometrically optimizing the optimization model according to the structural performance and production process requirements of the tube seat (2), and fitting and optimizing the optimization model using a spline curve method to obtain an optimal model of the tube seat (2).

3. The method for processing anti-vibration branch pipes of nuclear power plants according to claim 1, characterized in that: In step S2, the workpiece is a forging, the forging is made of stainless steel, and the heat treatment temperature is 1040°C to 1065°C.

4. The method for processing anti-vibration branch pipes of nuclear power plants according to claim 1, characterized in that: Step S3 includes: S31: Fixing the heat-treated workpiece on a workbench of a drilling machine and clamping it with a fixture; S32: setting a suitable rotation speed, feed rate and cutting depth according to the workpiece material and the type of drill bit; S33: Start the drilling machine and start deep hole drilling; S34: performing chip removal; S35: After drilling is completed, use measuring tools to measure and inspect the processed holes of the anti-vibration branch pipes of the nuclear power plant to ensure that their size and position accuracy meet the requirements; S36: cleaning the coolant and chips on the surface of the workpiece.

5. The method for processing the vibration-resistant branch pipe of a nuclear power plant according to claim 1, characterized in that: Step S4 includes: S41: Mounting the workpiece on a CNC lathe, ensuring that the workpiece is stable and correctly aligned; S42: selecting a suitable first tool according to the material of the workpiece and the requirements of rough machining; S43: setting a feed path of the first tool and cutting parameters of the workpiece in a programming system of a CNC lathe; S44: adjusting a suitable cutting speed and feed rate according to the material of the workpiece and the performance of the first tool; S45: Start the CNC lathe to perform rough machining; S46: After the rough machining is completed, check whether there is any residual oxide layer, rust or scratches on the surface of the workpiece. If the rough machining requirements are not met, perform rough machining again; S47: cleaning iron filings and oil stains on the surface of the workpiece.

6. The method for processing the vibration-resistant branch pipe of a nuclear power plant according to claim 1, characterized in that: In step S5, the heat treatment temperature for removing residual stress of the workpiece after rough machining is 300°C to 350°C.

7. The method for processing the vibration-resistant branch pipe of a nuclear power plant according to claim 1, characterized in that: Step S6 includes: S61: Mounting the workpiece on a CNC lathe; S62: Select the appropriate second tool and grinding wheel according to the processing requirements; S63: setting a feed path of the second tool and cutting parameters of the workpiece in a programming system of a CNC lathe; S64: adjusting a suitable cutting speed and feed rate according to the material of the workpiece and the performance of the second tool; S65: Start the CNC lathe for finishing; S66: After finishing, the workpiece is measured and inspected using a measuring tool to ensure that the size and shape accuracy meet the requirements. If the finishing requirements are not met, finishing is performed again; S67: cleaning the grinding fluid and iron filings on the surface of the workpiece, and performing rust prevention treatment.

8. The method for processing anti-vibration branch pipes of nuclear power plants according to claim 1, characterized in that: Step S7 includes: S71: Dimension and shape accuracy inspection, use measuring tools such as outside micrometer and roundness tester to inspect the dimension and shape accuracy of the finished workpiece to ensure that it meets the design requirements; S72: Surface quality inspection, observe whether there are scratches, cracks, rust and other defects on the workpiece surface, and take corresponding measures; S73: Handling of unqualified products. Products that fail the inspection will be scrapped to ensure that all processed nuclear power plant anti-vibration branches meet the quality standards.

9. A vibration-resistant branch pipe for a nuclear power plant, characterized in that: It comprises a branch pipe body (1) and a pipe seat (2) formed integrally with the branch pipe body (1), and there is a smooth transition between the branch pipe body (1) and the pipe seat (2).

10. The anti-vibration branch pipe for a nuclear power plant according to claim 9, characterized in that: The branch pipe body (1) has a diameter of 14 mm to 27 mm, a wall thickness of 2 mm to 4 mm, and a length of 100 mm to 1200 mm; The tube seat (2) has a length of 70 mm to 80 mm, an inner diameter of 8 mm to 15 mm, and a maximum outer diameter of 40 mm to 60 mm.

Citation Information

Patent Citations

  • Connection method for pipe branching from open pore of main pipeline by using 45 DEG branch pipe base

    CN101737584A

  • Method for machining and extruding branch pipes on bent pipe and punch structure

    CN111659751A

  • Process optimization method for low-frequency vibration auxiliary drilling machining

    CN112685872A

  • Branch pipe adapter for nuclear power main pipeline

    CN118088813A

  • Vibrationproof structure and method for drain pipe joint

    JP2000064379A