Low-pressure casting method for valve type steel castings

Through low-pressure casting method and composite anti-gravity filling and riser gravity filling technology, the problems of flow rate control difficulties and poor product quality in traditional gravity casting processes are solved, the yield and quality of valve cast steel parts are improved, and the production rate and quality of valve cast steel parts are reduced. Production cost.

CN119035504APending Publication Date: 2024-11-29Liupanshan Laboratory
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202411112923.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-14
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

Traditional gravity casting technology has problems such as difficulty in flow velocity and flow state control, limited filling power, poor product quality, low yield rate, and large subsidies for castings and difficulty in cleaning in valve casting steel parts.

Method used

The low-pressure casting method is adopted to control the casting and solidification process of liquid steel including straight runners, horizontal runners, inner runners and risers by performing composite anti-gravity filling and gravity retraction in low-pressure equipment. The chamber uses compressed gas to press metal hydraulics into the cast cavity and ensure solidification during the pressure-keeping stage.

Benefits of technology

It improves the yield rate of valve cast steel parts, reduces grinding workload, reduces metal liquid losses, improves product quality and production efficiency, and avoids the defects of the coiled gas slag inclusion and shrinkage holes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119035504A_ABST
    Figure CN119035504A_ABST
Patent Text Reader

Abstract

The low-pressure casting method comprises the steps that 1, a sand mold is prepared, specifically, the sand mold containing a casting mold cavity of a sprue, a cross gate, ingates, a valve casting mold and a riser is prepared, one end of the sprue is a pouring opening, the other end of the sprue is communicated with the middle of the cross gate, the two ends of the cross gate are communicated with one ends of the two ingates respectively, and the other ends of the two ingates are communicated with the other ends of the valve casting mold; the other ends of the two ingates are respectively communicated with two sides of the bottom end of the valve casting mold; the lower end of the riser is communicated with the top end of the valve casting mold; step 2, preheating a sand mold; and (3) smelting and pouring are conducted, specifically, molten metal is pressed into a casting mold cavity through a liquid rising pipe via a pouring opening of a sprue for pouring. According to the process, casting is conducted in an anti-gravity mold filling and dead head gravity feeding mode, the problems that the number of dead heads of castings is large, the dead heads are large, the castings are difficult to clean and the yield of the castings is low are solved, meanwhile, the defects of gas entrapment, slag inclusion, shrinkage porosity and shrinkage cavities of the castings are overcome, the production cost is reduced, and meanwhile the product quality is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of valve steel castings, and more particularly to a low-pressure casting method for valve steel castings. Background Art

[0002] Valve castings are a type of valve used to control the flow of media in pipelines. They are mainly used in industry, power and other fields. At present, the casting process of valve castings (such as butterfly valves) is all gravity casting. Figure 1 and Figure 2 As shown in the figure, gravity casting mainly has the following problems: First, the melt flow is achieved by gravity, and the flow rate and flow state are difficult to control, which is easy to produce casting defects such as air entrapment and oxide inclusions; second, the filling power is limited, and thin-walled castings cannot be formed; third, gravity risers are often used to achieve shrinkage compensation, and the shrinkage compensation pressure and distance are limited, the product quality is poor, and it is difficult to meet the production requirements of high-quality complex castings; fourth, the casting risers are heavily compensated and large, the castings are difficult to clean, and the casting yield rate is less than 50%, and the production cost is high.

[0003] Low-pressure casting has the advantages of controllable filling speed, smooth flow, less air inclusions, strong filling and shrinkage compensation capabilities, and the produced castings have the advantages of good intrinsic quality and high mechanical properties. Therefore, it is necessary to study a low-pressure casting method for valve-type steel castings to solve the above problems. Summary of the invention

[0004] In view of this, the purpose of the present invention is to solve the shortcomings of the traditional gravity casting process and provide a low-pressure casting device and casting method for valve-type steel castings, which not only make the cast valve products of excellent quality and stable performance, but also improve the process yield, reduce the loss of molten metal, reduce the workload of grinding steel castings, and improve production efficiency.

[0005] In order to achieve the above object, the present invention adopts the following technical solution:

[0006] A low-pressure casting method for valve-type steel castings comprises the following steps:

[0007] Step 1, sand mold preparation: prepare a sand mold containing a sprue, a cross runner, an ingode, a valve mold, and a riser, wherein one end of the sprue is a pouring port, and the other end is connected to the middle of the cross runner, the two ends of the cross runner are respectively connected to one end of the two ingodes, the other ends of the two ingodes are respectively connected to the two sides of the bottom end of the valve mold, and the lower end of the riser is connected to the top end of the valve mold;

[0008] Step 2, preheating the sand mold: preheat the sand mold to 130-150°C, keep warm for half an hour, and ensure that the sand mold is dry;

[0009] Step 3: Melting and pouring: melt qualified molten steel according to the specific material of the valve, control the pouring temperature of the molten steel to be 1530±10℃, put the sand mold into the sand box, and put the sand box into the low-pressure equipment furnace body, and inject compressed gas into the sealed low-pressure equipment furnace body. Under the action of gas pressure, the molten metal is pressed into the casting cavity through the rising pipe and the pouring port of the sprue. The process includes three stages: the liquid rising stage, the filling stage and the pressure holding stage. In the liquid rising stage, the molten steel rises steadily in the rising pipe, the liquid rising pressure reaches 50KPa, and the liquid rising time is 10-15S; in the filling stage, the molten steel fills the casting cavity in 3-5S, and the filling pressure reaches 65KPa; in the pressure holding stage, the pressure holding time needs to be 120S to ensure that the molten steel in the cavity solidifies under a higher pressure;

[0010] Step 4: Take out the cast sand mold from the furnace body of the low-pressure equipment, then remove the remaining sand around the mold, and cut off the sprue, runner, inner gate, and riser to obtain a valve casting with no shrinkage cavities or shrinkage inside.

[0011] Through the above technical scheme, it can be known that compared with the prior art, the present invention discloses a low-pressure casting method for valve-type steel castings. Considering that the steel liquid needs to flow smoothly and quickly, a flat pouring scheme for valve castings is selected, and an open pouring system is selected for the pouring system. The flow enters from the lower part of the straight runner, and the heat node is concentrated at the intersection of the valve casting mold and the bosses on both sides. A riser is placed on the top for shrinkage compensation, and the process yield rate reaches more than 70%. Therefore, the low-pressure casting process design of valve steel castings is a composite anti-gravity filling and riser gravity shrinkage compensation method for casting. Compared with the traditional gravity casting process, the riser is greatly reduced and the compensation under the riser can be removed. On the one hand, the process yield rate of the casting is improved and the workload of casting grinding is reduced. On the other hand, the low-pressure casting metal liquid flows in from the bottom, and the flow rate is stable, which solves the defects of air entrapment and slag inclusion. At the same time, the pouring system compensates the casting, and the shrinkage and shrinkage defects of the casting are reduced, the yield rate is greatly improved, and the quality of the casting is improved.

[0012] Furthermore, the sand mold includes a bottom core, a middle core, and a cover core that are buckled together, the bottom core is formed with the straight runner and the cross runner, the middle core is formed with the inner runner and the valve mold, and the cover core is formed with the riser.

[0013] The beneficial effect of adopting the above technical solution is: by using multiple sand cores for casting, multiple castings can be produced through one casting, that is, the straight runner, cross runner, inner runner, valve mold, and riser can be cast at one time, thereby improving the production efficiency of castings.

[0014] Furthermore, the bottom core and the middle core are both provided with anti-fire grooves along the parting surface.

[0015] The beneficial effect of adopting the above technical solution is that it can prevent fire from occurring during the casting process.

[0016] Furthermore, the middle core and the bottom end surface of the cover core are both provided with a snap-fitting protrusion adapted to snap-fit ​​with the anti-fire escape groove.

[0017] The beneficial effect of adopting the above technical solution is that when assembling the bottom core, the middle core and the cover core, the snap-in protrusion can be snap-fitted with the anti-fire groove, which plays a role in quickly positioning adjacent cores, improving the core assembly accuracy, and avoiding misalignment of adjacent cores.

[0018] Furthermore, hanging handles are provided on both outer side walls of the bottom core, the middle core and the cover core.

[0019] The beneficial effects of adopting the above technical solution are: the hanging handle is used for the transportation, flow coating and core assembly of sand cores.

[0020] Furthermore, screw holes are provided around the bottom core, the middle core and the cover core for fastening by screws after the core assembly is completed.

[0021] The beneficial effect of adopting the above technical solution is that it is easy to assemble and disassemble the bottom core, the middle core and the cover core.

[0022] Furthermore, a chill is placed in the middle core and is in contact with the valve casting mold.

[0023] The beneficial effects of adopting the above technical solution are: placing chillers at appropriate positions of the casting can improve the shrinkage feeding channel, eliminate local thermal stress, prevent cracks, improve the internal quality grade of the casting, and provide high-quality castings. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the provided drawings without paying creative work.

[0025] Figure 1 The present invention provides a schematic diagram of gravity casting of existing valve steel castings.

[0026] Figure 2 The present invention provides a schematic diagram of providing a riser subsidy in gravity casting of existing valve-type steel castings.

[0027] Figure 3 The present invention provides a schematic diagram of the three-dimensional structure of a sand mold used in a low-pressure casting method for a valve type steel casting.

[0028] Figure 4The present invention provides a schematic top view of the structure of a sand mold used in a low-pressure casting method for a valve-type steel casting.

[0029] Figure 5 for Figure 4 Schematic cross-sectional view of the middle section AA.

[0030] Figure 6 This is a schematic diagram of a first-perspective decomposition structure of a sand mold used in a low-pressure casting method for a valve-type steel casting provided by the present invention.

[0031] Figure 7 This is a schematic diagram from a second perspective of the decomposed structure of a sand mold used in a low-pressure casting method for a valve-type steel casting provided by the present invention.

[0032] Figure 8 It is a schematic diagram of the casting mold obtained after sand casting, which contains a sprue, a runner, an ingates, a valve mold, and a riser. DETAILED DESCRIPTION

[0033] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0034] The embodiment of the present invention discloses a low-pressure casting method for valve-type steel castings, comprising the following steps:

[0035] Step 1, sand mold preparation: prepare a sand mold 9 having a casting cavity including a sprue 4, a runner 5, an ingates 6, a valve mold 7, and a riser 8, wherein one end of the sprue 4 is a pouring port 41, and the other end is connected to the middle of the runner 5, both ends of the runner 5 are respectively connected to one end of two ingates 6, and the other ends of the two ingates 6 are respectively connected to both sides of the bottom end of the valve mold 7, and the lower end of the riser 8 is connected to the top end of the valve mold 7;

[0036] Step 2, preheating the sand mold 9: apply a layer of refractory coating for cast steel on the inner surface of the sand core of the sand mold 9, and preheat the sand mold 9 to 130-150°C for half an hour to ensure that the sand mold 9 is dry;

[0037] Step 3: Melting and pouring: melt qualified molten steel according to the specific material of the valve, control the pouring temperature of the molten steel to be 1530±10℃, put the sand mold 9 into the sand box, and put the sand box into the low-pressure equipment furnace body, and inject compressed gas into the sealed low-pressure equipment furnace body. Under the action of gas pressure, the molten metal is pressed into the casting mold cavity through the rising pipe and the pouring port 41 of the sprue 4. The process includes three stages: the liquid rising stage, the filling stage and the pressure holding stage. In the liquid rising stage, the molten steel rises steadily in the rising pipe, the liquid rising pressure reaches 50KPa, and the liquid rising time is 10-15S; in the filling stage, the molten steel fills the casting mold cavity in 3-5S, and the filling pressure reaches 65KPa; in the pressure holding stage, the pressure holding time needs to be 120S to ensure that the molten steel in the mold cavity solidifies under a higher pressure;

[0038] Step 4: Take out the cast sand mold 9 from the furnace body of the low-pressure equipment, then remove the remaining sand around the mold, and cut off the sprue 4, the runner 5, the ingates 6, and the riser 8 to obtain a valve steel casting without shrinkage cavities and shrinkage inside.

[0039] The sand mold 9 includes a bottom core 91 , a middle core 92 , and a cover core 93 which are buckled up and down. The bottom core 91 is formed with a sprue 4 and a runner 5 , the middle core 92 is formed with an inner runner 6 and a valve mold 7 , and the cover core 93 is formed with a riser 8 .

[0040] The bottom core 91 and the middle core 92 are both provided with anti-fire grooves 10 along the parting surface.

[0041] The bottom end surfaces of the middle core 92 and the cover core 93 are both provided with a snap-fitting protrusion 11 which is adapted to snap-fit ​​with the anti-fire escape groove 10 .

[0042] Hanging handles 12 are provided on both outer side walls of the bottom core 91 , the middle core 92 and the cover core 93 .

[0043] Screw holes 13 are provided around the bottom core 91, the middle core 92 and the cover core 93 for fastening by screws after the core assembly is completed.

[0044] Therefore, in step 3, the bottom core 91, the middle core 92, and the cover core 93 are assembled in sequence, the screws around are tightened, and the sand box is put on the outside of the assembled core package to ensure a spacing of 80-100mm. Then, resin sand is poured in to fill it tightly, and then it is placed in the furnace body of the low-pressure equipment for molten steel pouring.

[0045] A chill 14 in contact with the valve mold 7 is placed in the inner cavity of the middle core 92 .

[0046] The present invention designs stackable three-dimensional models of a bottom core 91, an intermediate core 92, and a cover core 93 in a three-dimensional software. After the three-dimensional model design of the sand mold is completed, the three-dimensional model is imported into a 3D printer, and the sand consumption of each sand mold is set to 20-30 mm in the 3D printer. The sand molds of the bottom core 91, the intermediate core 92, and the cover core 93 are printed out by the 3D printer, and the printed bottom core 91, the intermediate core 92, and the cover core 93 are stacked and cast. That is, through one casting, a plurality of castings with a straight runner 4, a cross runner 5, an inner runner 6, a valve casting mold 7, and a riser 8 can be produced, thereby improving the casting production efficiency.

[0047] The present invention designs a new low-pressure casting process method for valve steel castings, relies on anti-gravity low-pressure pouring and riser weight compensation to simultaneously cast and compensate for the shrinkage of the castings, effectively solves the problems of excessive riser subsidies, large risers, difficult cleaning of castings and low casting yield, and avoids the generation of air entrapment, slag inclusion, shrinkage and shrinkage cavity defects in castings, reduces production costs and improves product quality.

[0048] In this specification, each embodiment is described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the embodiments can be referred to each other. For the device disclosed in the embodiment, since it corresponds to the method disclosed in the embodiment, the description is relatively simple, and the relevant parts can be referred to the method part.

[0049] The above description of the disclosed embodiments enables one skilled in the art to implement or use the present invention. Various modifications to these embodiments will be apparent to one skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but rather to the widest scope consistent with the principles and novel features disclosed herein.

Claims

1. A low-pressure casting method for valve-type steel castings, characterized in that: include: Follow these steps: Step 1, sand mold preparation: prepare a sand mold (9) having a casting cavity including a sprue (4), a runner (5), an ingode (6), a valve mold (7), and a riser (8), wherein one end of the sprue (4) is a pouring port (41), and the other end is connected to the middle of the runner (5), the two ends of the runner (5) are respectively connected to one end of the two ingodes (6), the other ends of the two ingodes (6) are respectively connected to the two sides of the bottom end of the valve mold (7), and the lower end of the riser (8) is connected to the top end of the valve mold (7); Step 2, preheating the sand mold (9): preheating the sand mold (9) to 130-150° C., keeping the temperature for half an hour, and ensuring that the sand mold (9) is dry; Step 3: Melting and pouring: melt qualified molten steel according to the specific material of the valve, control the pouring temperature of the molten steel to be 1530±10℃, put the sand mold (9) into a sand box, and put the sand box into the low-pressure equipment furnace body, inject compressed gas into the sealed low-pressure equipment furnace body, and under the action of gas pressure, press the molten metal into the casting mold cavity through the rising pipe and the pouring port (41) of the sprue (4). The process includes three stages: a liquid rising stage, a filling stage and a pressure holding stage. In the liquid rising stage, the molten steel rises steadily in the rising pipe, the liquid rising pressure reaches 50KPa, and the liquid rising time is 10-15S; in the filling stage, the molten steel fills the casting mold cavity in 3-5S, and the filling pressure reaches 65KPa; in the pressure holding stage, the pressure holding time needs to be 120S to ensure that the molten steel in the mold cavity solidifies under a higher pressure; Step 4: Take out the cast sand mold (9) from the furnace body of the low-pressure equipment, remove the remaining sand around the mold, and cut off the sprue (4), runner (5), ingates (6), and risers (8) to obtain a valve steel casting without shrinkage cavities and shrinkage inside.

2. A low-pressure casting method for valve steel castings according to claim 1, characterized in that: The sand mold (9) comprises a bottom core (91), an intermediate core (92), and a cover core (93) which are buckled together. The bottom core (91) is formed with the sprue (4) and the runner (5), the intermediate core (92) is formed with an inner runner (6) and the valve casting (7), and the cover core (93) is formed with the riser (8).

3. A low-pressure casting method for valve steel castings according to claim 2, characterized in that: The bottom core (91) and the middle core (92) are both provided with anti-fire grooves (10) along the parting surface.

4. A low-pressure casting method for valve steel castings according to claim 3, characterized in that: The bottom end surfaces of the middle core (92) and the cover core (93) are both provided with a clamping protrusion (11) adapted to be clamped with the anti-fire escape groove (10).

5. The low-pressure casting method for valve steel castings according to claim 2, characterized in that: Hanging handles (12) are provided on both outer side walls of the bottom core (91), the middle core (92) and the cover core (93).

6. A low-pressure casting method for valve steel castings according to claim 2, characterized in that: Screw holes (13) are provided around the bottom core (91), the middle core (92) and the cover core (93) for fastening by screws after the core assembly is completed.

7. A low-pressure casting method for valve steel castings according to claim 2, characterized in that: A chill (14) in contact with the valve casting mold (7) is placed in the middle core (92).

Citation Information

Cited By

  • Pouring system and pouring method for low-pressure casting

    CN119703011A

  • A low pressure casting gating system and method

    CN119703011B