Flexible photoelectrochemical sensor for instantly detecting content of uric acid in sweat and preparation method of flexible photoelectrochemical sensor
Through flexible photoelectrochemical sensors combined with microfluidic control technology and photoelectrochemical sensing technology, uric acid oxidase and nanomaterials are used to perform photoelectrochemical reactions, solving the problems of poor non-invasiveness and low sensitivity of existing uric acid detection methods, and realizing non-invasive and instant , accurate uric acid testing is suitable for the self-test needs of a variety of uric acid-related diseases.
Patent Information
- Application Number
- CN202411160679.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-22
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2044-08-22
AI Technical Summary
The existing uric acid detection methods have problems such as poor non-invasiveness, low sensitivity, complex operation and equipment dependence, which are difficult to meet the needs of immediate and accurate detection of uric acid, especially in patients with gout, cardiovascular disease, hyperuricemia and liver and renal dysfunction. Self-test requirements.
Using flexible photoelectrochemical sensors, combined with microfluidic control technology and photoelectrochemical sensing technology, the electroosmosis electrode pair and photoelectrochemical sensing three electrodes are derived through sweat, and materials such as uric acid oxidase, zinc sulfide nanosheets and redox graphene are used to perform. Photoelectrochemical reactions enable high sensitivity detection of uric acid in sweat.
It realizes non-invasive, instant and accurate uric acid detection, reduces the lower limit of detection, avoids the infection risk brought by acupuncture sampling, simplifies operation, and is suitable for in-place POCT applications.
Smart Images

Figure CN119044277A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a flexible photoelectrochemical sensor for instant detection of uric acid content in sweat and a preparation method thereof, belonging to the frontier cross-manufacturing technology field of flexible electronics and medical devices. Background Art
[0002] As the final product of purine metabolism in the human body, uric acid is of great significance for the clinical diagnosis and treatment of various diseases. When the human body's uric acid metabolism is abnormal, sodium urate and uric acid crystals are easily formed in the synovium of the joints or the kidneys, causing gout or urinary stones. Excessive uric acid levels in the blood can also have an adverse effect on kidney function, thereby inducing serious diseases such as myocardial infarction, hyperuricemia and type II diabetes. When the uric acid level in the blood is too low, the risk of suffering from diseases such as liver necrosis and hepatolenticular degeneration will be greatly increased. Therefore, rapid and accurate uric acid content determination is crucial for the precise diagnosis and treatment of various diseases and public health inspections.
[0003] The "gold standard" for human uric acid detection is the concentration of uric acid in the blood. The blood uric acid concentration of adult males should be between 150 and 420 μmol / L; the blood uric acid concentration of adult females should be between 89 and 360 μmol / L. The method commonly used in clinical practice to determine the blood uric acid content is the uricase-peroxidase coupling method. This method first requires a sufficient blood sample to be tested from the patient, and then the uric acid is decomposed into allantoin and hydrogen peroxide by urate oxidase. The generated hydrogen peroxide, under the catalytic action of catalase, can condense 3.5-dichlorodihydroxybenzenesulfonic acid and 4-aminoantipyrine into red quinone compounds. The red compound shows obvious absorption characteristics for 520nm light waves. Therefore, by measuring the absorbance value of the compound, the uric acid concentration of the blood to be tested can be calculated. This method is suitable for manual and automatic biochemical analysis and can meet the needs of routine clinical analysis. However, this method still has shortcomings such as poor peroxidase specificity, susceptibility to interference from reducing substances, invasive blood sampling process, need for additional optical equipment assistance, and long waiting time for testing, which limits its application in human uric acid point-of-care testing (POCT). In addition, drawing on portable blood glucose meters, domestic and foreign medical POCT equipment research and development companies represented by Sino Biotechnology have developed a variety of home-use blood uric acid testers, which to a certain extent meet the POCT needs of patients' uric acid levels. However, these uric acid testing devices still require a needle to pierce the fingertips to take blood samples, and long-term use can easily cause infection in patients (especially those with diabetes and liver and kidney dysfunction). In addition, the results of a single test are easily affected by the sampling method, resulting in large reading deviations and low test credibility.
[0004] Therefore, there is an urgent need for a non-invasive, highly sensitive, and easy-to-operate POCT method for uric acid content to help patients with gout, cardiovascular disease, hyperuricemia, type II diabetes, liver and kidney dysfunction and other diseases to conduct real-time, accurate, and rapid self-testing of their own uric acid levels.
[0005] The sweat secreted by human skin contains a variety of biological molecules such as glucose, lactic acid, uric acid, ions and amino acids, which can reflect the health status of the human body. Compared with other body fluids such as blood, interstitial fluid, and tears, sweat sampling is simpler, the sampling process is non-invasive, and the discomfort caused is low. Therefore, flexible microfluidic sensors for sweat detection have received widespread attention. However, the low concentration of uric acid in sweat (no more than 35.7μmol / L) puts higher requirements on the uric acid sensing ability of the sensitive unit in the flexible microfluidic sensor. Therefore, it is urgent to develop a highly sensitive and low detection limit sweat uric acid content POCT flexible microfluidic sensor, so as to comprehensively promote the practical application of sweat uric acid content in clinical diagnosis and treatment, related patient health monitoring, etc. Summary of the invention
[0006] In order to solve the problem of high sensitivity and on-site POCT of uric acid content in patient's sweat secretion, the present invention combines microfluidic technology, photoelectrochemical sensing technology and flexible electronic technology to propose a flexible photoelectrochemical sensor for POCT of uric acid content in sweat and its preparation method. The sensor can realize the electro-osmotic extraction of sweat in human skin glands, the efficient collection of exuded sweat and the photoelectrochemical detection of uric acid concentration, thereby meeting the high sensitivity, low detection limit and on-site POCT detection requirements of uric acid content in patient's sweat.
[0007] The present invention is achieved through the following technical solutions.
[0008] In one aspect of the present invention, a flexible photoelectrochemical sensor for instant detection of uric acid content in sweat is provided, comprising a medical double-sided adhesive layer, a sweat extraction electro-osmotic electrode pair, a photoelectrochemical sensing three-electrode, a polyimide PI substrate, a photoelectrochemical sensitive material, a sweat collection microchannel and a flexible packaging layer, which are sequentially distributed from bottom to top;
[0009] The medical double-sided adhesive layer is provided with a sweat collection through-hole array and two upper and lower electroosmotic electrode through-grooves;
[0010] The sweat extraction electroosmotic electrode pair comprises a pair of electroosmotic anodes and electroosmotic cathodes, wherein the electroosmotic anodes and the electroosmotic cathodes are respectively overlapped with the upper and lower electroosmotic electrode slots;
[0011] The three electrodes of photoelectrochemical sensing include counter electrode, working electrode and reference electrode;
[0012] A sweat collecting through hole array is provided on the polyimide PI substrate, and the sweat collecting through hole array corresponds to the sweat collecting through hole array on the medical double-sided adhesive layer;
[0013] The sweat collection microchannel is provided with a plurality of channel inlets and a channel outlet respectively connected with each through hole of the sweat collection through hole array;
[0014] The flexible packaging layer is provided with a sweat discharge hole corresponding to the flow channel outlet;
[0015] The sweat in the skin sweat glands is non-invasively extracted through the sweat extraction electro-osmosis electrode, and the sweat is transported to the photoelectrochemical sensing three electrodes through the sweat collection microchannel. The photoelectrochemical reaction is carried out by the contact between the sweat and the photoelectrochemical sensitive material to realize the detection of uric acid content in sweat.
[0016] Preferably, the upper and lower electroosmotic electrode slots are arranged from bottom to top, and the sweat collection hole array is located below the lower electroosmotic electrode slot.
[0017] Preferably, the electro-osmosis anode and the electro-osmosis cathode of the sweat-extracting electro-osmosis electrode pair are arranged in a pair of sickle shapes facing each other, and the length of the curved hook arc section of the electro-osmosis anode is smaller than that of the electro-osmosis cathode arc section.
[0018] Preferably, the working electrode is located in the middle of the three photoelectrochemical sensing electrodes and is a straight line segment; the counter electrode and the reference electrode are located on both sides of the three photoelectrochemical sensing electrodes and are symmetrical bow shapes; after superposition, the periphery of the three photoelectrochemical sensing electrodes is located within the sickle-shaped electrode frame of the sweat extraction electroosmosis electrode pair.
[0019] Preferably, the sweat collection microchannel includes a circular flow channel, the circular flow channel is connected to multiple flow channel inlets, each inlet of the multiple flow channels is respectively connected to each through hole of the sweat collection through hole array, and is connected to a flow channel outlet on the circular flow channel; the counter electrode, working electrode and reference electrode of the photoelectrochemical sensor three electrodes are located in the circular flow channel frame.
[0020] Another aspect of the present invention provides a method for preparing the flexible photoelectrochemical sensor for instant detection of uric acid content in sweat, comprising the following steps:
[0021] Step 1, polyimide PI substrate sweat extraction electroosmosis electrode to substrate electrode and lead wire:
[0022] Print sweat-extracting electroosmotic electrodes to base electrodes and lead patterns on one side of the polyimide PI film;
[0023] Step 2, base electrode and leads of polyimide PI substrate photoelectrochemical sensing three electrodes:
[0024] Print the substrate electrode and lead pattern of the photoelectrochemical sensing three electrodes on the other side of the polyimide PI substrate;
[0025] Step 3, modification of the carbon layer on the counter electrode and working electrode in the photoelectrochemical sensing three-electrode:
[0026] Positioning and printing the counter electrode and the working electrode on the polyimide PI substrate surface printed with the base electrode and lead pattern of the photoelectrochemical sensing three electrodes, heating and curing, and obtaining the carbon layer-modified counter electrode and working electrode in the photoelectrochemical sensing three electrodes;
[0027] Step 4, modification of the gold nanofilm on the working electrode and chlorination of the reference electrode in the photoelectrochemical sensing three-electrode:
[0028] Gold nanoparticles are deposited on the surface of the working electrode in the photoelectrochemical sensing three-electrode by electrodeposition in a chloroauric acid / sulfuric acid mixed electrolyte, and then rinsed and dried to obtain a working electrode with a gold nanofilm modified on the surface;
[0029] The reference electrode is chlorinated and modified by cyclic voltammetry in a potassium chloride / hydrochloric acid mixed electrolyte, and then rinsed and dried to obtain a silver / silver chloride reference electrode;
[0030] Step 5, synthesis of photoelectrochemical sensitive materials and functional modification of the working electrode surface:
[0031] Zinc sulfide nanosheets, redox graphene and bismuth vanadate nanorods were synthesized by hydrothermal and sol-gel methods and dispersed in a solvent;
[0032] Add zinc sulfide nanosheets, redox graphene and bismuth vanadate nanorod dispersions to the surface of the working electrode modified with gold nanofilm obtained in step 4, add urate oxidase solution to it after natural drying, and then drip Nafion after drying again, and obtain the working electrode modified with photoelectrochemical sensitive material after curing;
[0033] Step 6, forming a sweat collection through-hole array on a polyimide PI substrate:
[0034] The polyimide PI substrate where the photoelectrochemical sensing three electrodes modified with the photoelectrochemical sensitive material obtained in step 5 are located is subjected to laser cyclic cutting and laser etching to obtain a sweat collection through-hole array structure on the polyimide PI substrate;
[0035] Step 7, forming the sweat collection through hole array and the electroosmotic electrode through groove on the medical double-sided adhesive layer:
[0036] The medical double-sided adhesive layer is sandwiched between two pieces of oily paper, and the medical double-sided adhesive layer with the oily paper is subjected to laser circular cutting and laser etching to obtain a sweat collection through-hole array and an electroosmotic electrode through-groove structure on the medical double-sided adhesive layer;
[0037] Step 8, bonding between the polyimide PI substrate and the medical double-sided adhesive layer:
[0038] Tear off the oily paper attached to one side of the medical double-sided adhesive layer obtained in step 7, and stick it on the sweat extraction electroosmosis electrode pair substrate electrode and lead covering surface of the structure prepared in step 6, and align it with the sweat collection through hole array on the double-sided adhesive, the sweat extraction electroosmosis electrode pair substrate electrode and the electroosmosis electrode through groove to obtain a bonded polyimide PI substrate and medical double-sided adhesive layer;
[0039] Step 9, the electro-osmosis anode and cathode of the sweat extraction electro-osmosis electrode pair are formed by coating with glue:
[0040] An agarose aqueous solution is prepared, carbachol and sodium chloride are added to two agarose aqueous solutions respectively and stirred evenly to form an anode and a cathode colloidal solution, and the solutions are cooled and added to the electroosmotic electrode slots respectively to obtain an electroosmotic anode and a cathode of a sweat extraction electroosmotic electrode pair;
[0041] Step 10: Processing and molding of sweat collection microchannels:
[0042] The glass plate covered with waterproof double-sided tape was laser cut and laser etched to obtain the sweat collection microchannel;
[0043] Step 11: Lamination between the sweat collection microchannel and the polyimide PI substrate:
[0044] Tear off the oily paper on one side of the sweat collection microfluidic channel, and attach it to the back side of the structure obtained in step 9, align the inlet of the sweat collection microfluidic channel of the double-sided adhesive layer with the sweat collection through-hole array of the structure obtained in step 6, and obtain the attached sweat collection microfluidic channel and the polyimide PI substrate;
[0045] Step 12, forming the sweat discharge holes on the flexible packaging layer:
[0046] Prepare a PDMS mixed solution, and spin-coat the PDMS mixed solution on a clean glass sheet;
[0047] The air bubbles are removed by vacuum filtration, and the PDMS film is cured by constant temperature heating to obtain a glass sheet covered with a flexible encapsulation layer;
[0048] The glass sheet covered with the PDMS film is subjected to laser cyclic cutting and laser etching to obtain the sweat discharge hole structure on the flexible encapsulation layer;
[0049] Step 13, top packaging of flexible photoelectrochemical sensor for POCT of sweat uric acid content:
[0050] Tear off the oily paper on the other side of the sweat collection microchannel structure obtained in step 11, and stick it firmly to the flexible packaging layer. Align the sweat discharge holes on the flexible packaging layer with the outlet of the sweat collection microchannel to obtain a top-encapsulated flexible photoelectrochemical sensor for POCT of sweat uric acid content.
[0051] Preferably, in steps 1 and 2, the pass spacing of the printing process is set to 0.1-0.3 mm, the feed rate to 70-200 mm / min, and the fluidity to 0.5-1.5 mm; the polyimide PI substrate after the dispensing printing is placed on a 50-80°C hot plate, heated and cured, and then cooled to room temperature.
[0052] Preferably, in step 3, the dispensing machine feed rate is set to 100-300 mm / min and the fluidity is set to 0.3-0.8 mm; the polyimide PI substrate after positioning printing is placed on a hot plate at 80-100° C., heated and cured, and then cooled to room temperature.
[0053] Preferably, in step 4, sulfuric acid, chloroauric acid and water are mixed uniformly in a mass ratio of (98-295): (0.17-1.36): 1000 to obtain an electrolyte, and gold nanoparticles are deposited on the surface of the working electrode at a constant current of 0.2-0.6 A in the chloroauric acid / sulfuric acid mixed electrolyte for 400-800 s;
[0054] Potassium chloride, hydrochloric acid and water were mixed evenly in a mass ratio of (3.7-15):(0.70-2.8):1000 to obtain an electrolyte, and the reference electrode was chlorinated by cyclic voltammetry with a scanning range of -0.15-1.05 V, a scanning rate of 25-100 mV / s, and a scanning number of 5-10 times. The electrode was rinsed and dried to obtain a silver / silver chloride reference electrode.
[0055] Preferably, in step 5, the preparation of the working electrode modified with the photoelectrochemical sensitive material comprises:
[0056] a. Prepare precursor solution:
[0057] Zinc acetate, thiourea, water and ethylenediamine were uniformly mixed in a mass ratio of (9.–37):(8–30):(200–250):(0.67–0.72) to obtain a precursor solution;
[0058] b. Preparation of zinc sulfide nanosheets / redox graphene composite powder:
[0059] Add redox graphene to the precursor solution in a mass ratio of (30–50):(3–10) and heat at 120–150°C for 10–16 hours;
[0060] c. Preparation of bismuth vanadate nanorod powder:
[0061] Bismuth nitrate pentahydrate, polyvinyl pyrrolidone, water and nitric acid are mixed uniformly according to a mass ratio of (3-6): (0.5-3.0): 20: (2.5-7.5) to obtain solution A; ammonium vanadate, water and sodium hydroxide are mixed and dissolved uniformly according to a mass ratio of (1-2): (10-30): (1.6-4.8) to obtain solution B; solution B is added dropwise to solution A under stirring conditions, and the pH is adjusted to 7.0; the mixed solution is heated at 160-200°C for 18-24 hours; the reaction product is centrifuged, washed and dried to obtain bismuth vanadate nanorod powder;
[0062] d. The zinc sulfide nanosheet / redox graphene composite material and bismuth vanadate nanorod powder were mixed with pineneol in a mass ratio of (0.03–0.10):(0.09–0.36) to form two suspensions;
[0063] Dropping a zinc sulfide nanosheet / redox graphene suspension onto the surface of the working electrode, allowing it to dry naturally, then dropping a bismuth vanadate nanorod powder suspension onto it, and drying it again to obtain a working electrode surface modified with zinc sulfide nanosheets, redox graphene, and bismuth vanadate nanorods;
[0064] The urate oxidase solution was dripped onto the surface of the working electrode, left to dry at 4°C, and then dripped with Nafion. After solidification, a working electrode modified with a photoelectrochemical sensitive material was obtained.
[0065] Preferably, in steps 7, 10 and 12, laser cutting cycles are performed 5-20 times according to the designed structural contour at a power of 5-10 W and a cutting speed of 1000-2000 mm / min.
[0066] Preferably, in step 9, the electro-osmosis anode and cathode of the sweat-extracting electro-osmosis electrode pair are formed by coating with glue:
[0067] 2-5% w / w agarose is mixed in deionized water, heated at 200-250°C to prepare a gel solution, cooled to 150-170°C, and 0.8-1.2% w / w carbachol and 0.8-1.2% w / w sodium chloride are added to two portions of the gel solution, respectively, to form anode and cathode colloid solutions.
[0068] The present invention adopts the above technical solution, which has the following beneficial effects:
[0069] 1. The sensor of the present invention is equipped with a pair of sweat extraction electro-osmotic electrodes, which can realize the non-invasive extraction of sweat in the sweat glands of human skin, and is helpful for the real-time detection of uric acid content in the body of patients using this sensor.
[0070] 2. The sensor is equipped with a sweat collection microchannel, which can realize the efficient and automatic collection of sweat to be tested by electroosmosis, avoiding the infection risk brought by the fingertip blood sample used in conventional home uric acid testers and the inaccurate test results caused by irregular sampling.
[0071] 3. The working electrodes in the sensitive unit area of the sensor are modified with carbon layer, Au nanoparticles, zinc sulfide nanosheets, redox graphene, bismuth vanadate nanorods and urate oxidase, respectively. The sensor can utilize the specific photoelectrochemical reaction between urate oxidase, zinc sulfide nanosheets, redox graphene, bismuth vanadate nanorods and uric acid molecules in sweat to convert low uric acid concentrations into strong photoelectrochemical signals, thereby achieving highly sensitive, on-site POCT detection of uric acid content in sweat. BRIEF DESCRIPTION OF THE DRAWINGS
[0072] The drawings described herein are used to provide a further understanding of the present invention, constitute a part of the present application, and do not constitute an improper limitation of the present invention. In the drawings:
[0073] Figure 1 This is a schematic diagram of the structure explosion of a flexible photoelectrochemical sensor for POCT of human uric acid content;
[0074] Figure 2 This is the working principle diagram of the flexible photoelectrochemical sensor;
[0075] Figure 3 This is a process flow chart for the preparation of flexible photoelectrochemical sensors. DETAILED DESCRIPTION
[0076] The present invention will be described in detail below in conjunction with the accompanying drawings and specific embodiments. The exemplary embodiments and descriptions of the present invention are used to explain the present invention but are not intended to limit the present invention.
[0077] like Figure 1 and 2 As shown, an embodiment of the present invention provides a flexible photoelectrochemical sensor 1 for POCT of uric acid content in sweat, which includes, from bottom to top, a medical double-sided adhesive layer 2, a sweat extraction electro-osmosis electrode pair 3, a photoelectrochemical sensing three-electrode 4, a polyimide PI substrate 5, a photoelectrochemical sensitive material 6, a sweat collection microchannel 7 and a flexible packaging layer 8.
[0078] The medical double-sided adhesive layer 2 is provided with a sweat collection through hole array a and first and second electroosmotic electrode through slots b and c. The first and second electroosmotic electrode through slots b and c are arranged from bottom to top, and the sweat collection through hole array a is located below the first electroosmotic electrode through slot b.
[0079] The sweat extraction electroosmosis electrode pair 3 is a pair of electrodes arranged in a sickle shape facing each other, wherein the tops of the sickle hooks are the electroosmosis anode e and the electroosmosis cathode d, respectively; the electroosmosis anode e overlaps with the first electroosmosis electrode slot b, the electroosmosis cathode d overlaps with the second electroosmosis electrode slot c, and the length of the arc segment of the sickle hook of the electroosmosis anode e is smaller than that of the arc segment of the electroosmosis cathode d.
[0080] The photoelectrochemical sensing three electrodes 4 include a counter electrode g, a working electrode i and a reference electrode h, wherein the working electrode i is located in the middle of the photoelectrochemical sensing three electrodes and is a straight line segment; the counter electrode g and the reference electrode h are located on both sides of the photoelectrochemical sensing three electrodes and are symmetrically arched. After being superimposed, the periphery of the photoelectrochemical sensing three electrodes 4 is located within the sickle-shaped electrode frame of the sweat extraction electroosmotic electrode pair 3.
[0081] A sweat collecting through hole array f is provided on the polyimide PI substrate 5 , and the sweat collecting through hole array f corresponds to the sweat collecting through hole array a provided on the medical double-sided adhesive layer 2 .
[0082] The sweat collection microchannel 7 includes a circular channel, and the circular channel is connected to multiple channel inlets j, each of which is connected to each through hole of the sweat collection through hole array f, and is connected to a channel outlet k on the circular channel. The counter electrode, working electrode and reference electrode of the photoelectrochemical sensor are located in the circular channel enclosure.
[0083] The flexible packaging layer 8 is provided with a sweat discharge hole 1, which corresponds to the flow channel outlet k.
[0084] In this embodiment, the medical double-sided adhesive layer 2 is made of 3M9917 produced by 3M Company, which has the characteristics of being breathable, anti-allergic, waterproof and sweat-proof, and having long-lasting adhesion, and can ensure that the sensor is permanently attached to the skin.
[0085] The polyimide PI substrate 5 uses a high temperature resistant insulating PI film with a thickness of 12.5 μm produced by Kapton Company, which can meet the flexibility requirements of the sensor.
[0086] The sweat collection microchannel 7 uses 3M9448A double-sided tape from 3M Company. The tape has the characteristics of being waterproof and highly sticky, and can meet the requirements of microchannel sealing and preventing liquid leakage during the sweat collection process.
[0087] The flexible encapsulation layer 8 uses Dow Corning's DC184 PDMS high-transparency elastomer to ensure that visible light can effectively irradiate the photoelectrochemical functional material and realize the photoelectrochemical reaction of uric acid on the working electrode.
[0088] The working principle of this sensor is shown in Figure 2, the sensor 1 is attached to the human skin n as a whole, positive electricity is applied to the electro-osmotic anode e, and negative electricity is applied to the electro-osmotic cathode d; the sweat in the sweat gland m on the skin n is extracted by using the electro-osmotic principle. The extracted sweat enters the entrance j of the sweat collection microchannel through the sweat collection through hole array a, f, and then flows to the photoelectrochemical sensing three electrodes 4 where the counter electrode g, the working electrode i and the reference electrode h are located under the action of capillary force. With the continuous accumulation in the collection microchannel 7, the sweat eventually reaches the channel outlet k, and is discharged from the entire device through the sweat discharge hole l on the flexible packaging layer 8. When the sweat flows through the counter electrode g, the working electrode i and the reference electrode h, the sweat is fully in contact with the photoelectrochemical sensitive material 6. At this time, the photoelectrochemical sensitive material 6 is illuminated to promote the photoelectrochemical reaction between uric acid in the sweat and the photoelectrochemical sensitive material 6, and then the uric acid concentration in the sweat is successfully converted into a photoelectrochemical current signal in the photoelectrochemical sensitive material 6, thereby realizing highly sensitive, on-site POCT detection of uric acid content in sweat.
[0089] like Figure 3 As shown, the present invention further provides a method for preparing a flexible photoelectrochemical sensor for POCT of sweat uric acid content, comprising the following steps:
[0090] Step 1: Polyimide PI substrate (one side) sweat extraction electroosmosis electrode to substrate electrode and lead forming
[0091] Lay the polyimide PI film flat on the clean dispensing printer workbench ( Figure 3 a) and fix the four corners of the film;
[0092] Based on the conductive silver paste, the base electrode and lead pattern of the sweat-derived electro-osmotic electrode were printed using a dispensing machine according to the designed sweat-derived electro-osmotic electrode. The printing process was set to pass the spacing of 0.1-0.3mm, the feed rate of 70-200mm / min, and the fluidity of 0.5-1.5mm to achieve the patterning of the sweat-derived electro-osmotic electrode on one side of the polyimide PI substrate to the base electrode and the lead ( Figure 3 b);
[0093] The polyimide PI substrate after the dispensing printing is placed on a 50-80°C hot plate, heated and cured, and then cooled to room temperature to obtain a sweat extraction electro-osmosis electrode on one side of the polyimide PI substrate to a substrate electrode and a lead structure.
[0094] Step 2: Forming the base electrode and lead wires of the polyimide PI substrate (the other side) photoelectrochemical sensing three electrodes
[0095] Turn over the structure obtained in step 1, lay it flat on a clean dispensing printer workbench, and fix the four corners. Be careful not to damage the sweat-extracting electroosmotic electrode to the base electrode and the lead structure on the back during the process;
[0096] Based on the conductive silver paste, the dispensing machine is used to print the substrate electrode and lead pattern of the designed photoelectrochemical sensing three electrodes. The printing process is set to pass the spacing of 0.1-0.3mm, the feed rate of 70-200mm / min, and the fluidity of 0.5-1.5mm to achieve the patterning of the substrate electrode and lead of the photoelectrochemical sensing three electrodes ( Figure 3 c);
[0097] The polyimide PI substrate after the dispensing printing is placed on a 50-80°C hot plate, heated and cured, and then cooled to room temperature to obtain the base electrode and lead structure of the photoelectrochemical sensing three electrodes on the other side of the polyimide PI substrate.
[0098] Step 3: Carbon layer modification on the counter electrode and working electrode in the photoelectrochemical sensing three-electrode
[0099] Use the positioning printing function of the dispensing machine to select and position the counter electrode and working electrode regions in the photoelectrochemical sensing three electrodes obtained in step 2;
[0100] Based on the conductive carbon paste, a dispensing machine is used to print according to the designed counter electrode and working electrode structure patterns, and the dispensing machine feed rate is set to 100-300mm / min and the fluidity is set to 0.3-0.8mm to achieve selective modification of the conductive carbon paste on the counter electrode and working electrode;
[0101] The polyimide PI substrate after positioning printing was placed on a hot plate at 80-100°C, heated and cured, and then cooled to room temperature to obtain the carbon layer-modified counter electrode and working electrode ( Figure 3 d).
[0102] Step 4: modification of the gold nanofilm on the working electrode and chlorination of the reference electrode in the photoelectrochemical sensing three-electrode
[0103] Using an electrochemical workstation, a commercial counter electrode and a reference electrode, sulfuric acid, chloroauric acid and water were evenly mixed in a mass ratio of (98–295):(0.17–1.36):1000 to obtain an electrolyte. Gold nanoparticles were deposited on the surface of the working electrode by constant current electrodeposition in the chloroauric acid / sulfuric acid mixed electrolyte, wherein the deposition current was 0.2-0.6A and the deposition time was 400-800s, thereby achieving the deposition of gold nanoparticles on the surface of the working electrode in the photoelectrochemical sensing three-electrode. The electrode was then rinsed with deionized water and blown dry to obtain a working electrode modified with a gold nanofilm on the surface.
[0104] Using an electrochemical workstation, a commercial counter electrode and a reference electrode, the reference electrode was chlorinated by cyclic voltammetry in a potassium chloride / hydrochloric acid mixed electrolyte. Potassium chloride, hydrochloric acid and water were evenly mixed in a mass ratio of (3.7–15):(0.70–2.8):1000 to obtain an electrolyte. The reference electrode was chlorinated by cyclic voltammetry with a scanning range of -0.15-1.05V, a scanning rate of 25-100mV / s, and a scanning number of 5-10 times. The electrode was then rinsed with deionized water and dried to obtain a silver / silver chloride reference electrode ( Figure 3 e).
[0105] Step 5: Synthesis of photoelectrochemical sensitive materials and functional modification of the working electrode surface
[0106] Synthesize zinc sulfide nanosheets, redox graphene and bismuth vanadate nanorods by hydrothermal and sol-gel methods, and redisperse them in a specific solvent for use;
[0107] Preparation of ZnS nanosheets, redox graphene and bismuth vanadate nanorod dispersions:
[0108] 51) Prepare precursor solution:
[0109] Zinc acetate, thiourea, water and ethylenediamine were uniformly mixed in a mass ratio of (9–367):(8–30):(200–250):(0.67–0.72) to obtain a precursor solution.
[0110] 52) Preparation of zinc sulfide nanosheets / redox graphene composite powder
[0111] 3–10 mg of redox graphene was added to 30–50 mL of the precursor solution, and then placed in a Teflon autoclave and heated to 120–150 ° C and maintained for 10–16 hours. After heating, the product was cleaned and dried in a vacuum. ZnS nanosheets / redox graphene composite powder was obtained.
[0112] 53) Preparation of bismuth vanadate nanorod powder
[0113] Bismuth nitrate pentahydrate, polyvinyl pyrrolidone, water and nitric acid are mixed evenly in a mass ratio of (3–6): (0.5–3.0): 20: (2.5–7.5) to obtain solution A. Ammonium vanadate, water and sodium hydroxide are mixed and dissolved evenly in a mass ratio of (1–2): (10–30): (1.6–4.8) to obtain solution B. Solution B is added dropwise to solution A under stirring conditions, and the pH is adjusted to 7.0 with nitric acid solution or ammonia water. The prepared mixed solution is transferred to a high-temperature reactor, heated to 160–200°C and reacted for 18–24 hours. The reaction product is then centrifuged, washed, and dried to obtain bismuth vanadate nanorod powder;
[0114] 54) Modification of functional materials on the working electrode surface
[0115] Zinc sulfide nanosheets / redox graphene composites and bismuth vanadate nanorod powders were mixed with pineneol in a mass ratio of (0.03–0.10):(0.09–0.36) to form two suspensions.
[0116] Add zinc sulfide nanosheets, redox graphene and bismuth vanadate nanorod dispersions dropwise onto the surface of the working electrode in the photoelectrochemical sensing three electrodes obtained in step 4;
[0117] A zinc sulfide nanosheet / redox graphene suspension is dropped on the surface of the working electrode, and after natural drying, a bismuth vanadate nanorod powder suspension is added, and after drying again, a working electrode surface modified with zinc sulfide nanosheets, redox graphene and bismuth vanadate nanorods is obtained.
[0118] Prepare 0.5-2 mg / mL urate oxidase solution, take 5-10 μL and drop it on the surface of the working electrode, and place it in a 4°C refrigerator to dry, then drop 5-15 μL Nafion, and after solidification, obtain a working electrode modified with photoelectrochemical sensitive materials ( Figure 3 f).
[0119] Step 6: Formation of sweat collection through-hole array on polyimide PI substrate
[0120] The structure obtained in step 5 was placed under a UV femtosecond laser, and 5–20 cycles of cutting were performed according to the designed structure contour at a power of 5–10 W and a cutting speed of 1000–2000 mm / min. Laser etching was performed to obtain a sweat collection through-hole array structure on a polyimide PI substrate ( Figure 3 g);
[0121] Step 7: Forming the sweat collection through hole array and the electroosmotic electrode through slot on the medical double-sided adhesive layer. Figure 3 h) Sandwiched between two pieces of oily paper to protect its adhesiveness;
[0122] The medical double-sided adhesive layer with oily paper was placed under a femtosecond laser, and 5-20 cycles of cutting were performed according to the designed structure contour at a power of 5-10W and a cutting speed of 1000-2000mm / min. Laser etching was performed to obtain the sweat collection through-hole array and the electroosmotic electrode through-groove structure on the medical double-sided adhesive layer ( Figure 3 i).
[0123] Step 8: Bonding of polyimide PI substrate and medical double-sided adhesive layer
[0124] Tear off the oily paper on one side of the medical double-sided adhesive layer obtained in step 7, and paste it on the base electrode and lead covering surface of the sweat extraction electroosmosis electrode pair structure prepared in step 6. During the pasting process, attention should be paid to the alignment between the base and the sweat collection through-hole array on the double-sided adhesive, and between the base electrode of the sweat extraction electroosmosis electrode pair and the electroosmosis electrode through-groove ( Figure 3 j), to obtain a bonded polyimide PI substrate and a medical double-sided adhesive layer ( Figure 3 k).
[0125] Step 9: Forming the electro-osmotic anode and cathode of the sweat-extracting electro-osmotic electrode pair by coating
[0126] The agarose aqueous solution is prepared by heating and stirring. 2-5% w / w agarose is mixed into deionized water, and the mixture is heated to 200-250°C with constant stirring until the gel solvent is evenly mixed. The gel solvent is cooled to 150-170°C, and 0.8-1.2% w / w carbachol and 0.8-1.2% w / w sodium chloride are added to the two solvents to form anode and cathode colloidal solutions. Then, carbachol and sodium chloride are added to the two agarose aqueous solutions and stirred evenly. After the solutions are cooled, they are poured into the electroosmotic electrode channels to obtain the electroosmotic anode and cathode of the sweat extraction electroosmotic electrode pair ( Figure 3 l).
[0127] Step 10: Processing and molding of sweat collection microchannels
[0128] Put the waterproof double-sided tape with oily paper on both sides ( Figure 3 m) Fix flatly on a clean glass plate;
[0129] The glass plate covered with waterproof double-sided tape was placed under a femtosecond laser and cut 5–20 times according to the designed structure contour at a power of 5–10 W and a cutting speed of 1000–2000 mm / min. The sweat collection microchannel was obtained by laser etching ( Figure 3 n).
[0130] Step 11: Lamination between the sweat collection microchannel and the polyimide PI substrate
[0131] Tear off the oily paper on one side of the sweat collection microfluidic channel and attach it to the back side of the structure obtained in step 9. During the attaching process, attention should be paid to the alignment between the inlet of the double-sided adhesive layer and the sweat collection through-hole array of the structure obtained in step 6, so as to obtain the attached sweat collection microfluidic channel and the polyimide PI substrate ( Figure 3 o).
[0132] Step 12: Forming the sweat discharge holes on the flexible packaging layer
[0133] A mixed solution of PDMS glue A and B was prepared in a mass ratio of 10:1, and the PDMS mixed solution was spin-coated on a clean glass slide; then the glass slide coated with PDMS was placed on a glue spreader and rotated at a low speed of 200-600 r / min and a high speed of 800-1500 r / min for 10-15 and 20-40 s, respectively.
[0134] The air bubbles were removed by vacuum filtration, and the PDMS film was cured by constant temperature heating at 90-120°C for 1-1.5 h to obtain a film with a flexible encapsulation layer ( Figure 3 p) glass;
[0135] The glass sheet covered with the PDMS film encapsulation layer was placed under a femtosecond laser and cut 5–20 times according to the designed structure contour at a power of 5–10 W and a cutting speed of 1000–2000 mm / min. The sweat discharge pore structure on the flexible encapsulation layer was obtained by laser etching ( Figure 3 q).
[0136] Step 13: Top encapsulation of flexible photoelectrochemical sensor for POCT of sweat uric acid content
[0137] The oily paper on the other side of the sweat collection microchannel structure obtained in S11 was torn off and firmly adhered to the flexible packaging layer. During the pasting process, care should be taken to ensure that there are no bubbles on the bonding surface to prevent leakage during the use of the device. In addition, attention should be paid to the alignment between the sweat discharge hole on the flexible packaging layer and the outlet of the sweat collection microchannel. Finally, a flexible photoelectrochemical sensor for POCT of sweat uric acid content encapsulated on the top was obtained ( Figure 3 r).
[0138] The preparation method of the flexible photoelectrochemical sensor for POCT of uric acid content in sweat of the present invention is further described in detail below through specific examples.
[0139] Example 1
[0140] S1, polyimide PI substrate (one side) sweat extraction electroosmosis electrode to substrate electrode and lead forming
[0141] 11) Cut a 8cm×6cm polyimide PI film, lay it flat on a clean dispensing printer workbench and fix the four corners;
[0142] 12) Using the VOLTERA V-One dispensing machine and its dedicated conductive silver paste, select the printing mode as simple printing, and set the pass spacing of the printing process to 0.1 mm, the feed rate to 100 mm / min, and the fluidity to 1.0 mm to achieve patterned printing of the sweat-derived electro-osmotic electrode to the base electrode and the lead wire;
[0143] 13) The polyimide PI substrate with the sweat extraction electroosmosis electrode pair base electrode and lead pattern is placed on a 60°C hot plate and heated until the conductive silver paste solidifies and cools to room temperature to obtain the sweat extraction electroosmosis electrode pair base electrode and lead structure.
[0144] S2, polyimide substrate (the other side) substrate electrode and lead forming of the photoelectrochemical sensing three electrodes
[0145] 21) Turn over the polyimide PI substrate and lay it flat on a clean dispensing printer workbench, fix the four corners of the film, and be careful not to damage the sweat-extracting electro-osmotic electrode on the back to the substrate electrode and the lead structure during the process;
[0146] 22) Using the VOLTERA V-One dispensing machine and its dedicated conductive silver paste, select the printing mode as simple printing, and set the pass spacing of the printing process to 0.1 mm, the feed rate to 100 mm / min, and the fluidity to 1.0 mm to achieve patterned printing of the base electrode and lead wires of the three-electrode photoelectrochemical sensor;
[0147] 23) The polyimide PI substrate is placed on a 60° C. hot plate and heated until the conductive silver paste is completely cured, thereby obtaining a base electrode and lead structure of the photoelectrochemical sensing three electrodes on the other side of the polyimide PI substrate.
[0148] S3, Carbon layer modification on the counter electrode and working electrode in the three-electrode photoelectrochemical sensor
[0149] 31) Using the VOLTERA V-One dispensing machine, select the printing mode as positioning printing to achieve the selection and positioning of the counter electrode and working electrode areas;
[0150] 32) Based on the CH-8 carbon paste of Shijo Company, the dispensing machine feed rate was set to 200 mm / min and the fluidity to 0.6 mm to achieve selective modification of the conductive carbon paste on the counter electrode and the working electrode;
[0151] 33) The polyimide PI substrate is placed on a 90° C. hot plate and heated until the carbon slurry solidifies, and then cooled to room temperature to obtain a carbon layer-modified counter electrode and a working electrode in the photoelectrochemical sensing three-electrode.
[0152] S4, Gold nanofilm modification on the working electrode and chlorination of the reference electrode in the photoelectrochemical sensing three-electrode
[0153] 41) Using Shanghai Chenhua's CHI-660E electrochemical workstation, commercial platinum wire counter electrode and silver / silver chloride reference electrode, sulfuric acid, chloroauric acid and water were evenly mixed in a mass ratio of 195:1.36:1000 to obtain an electrolyte, in which gold nanoparticles were deposited on the surface of the working electrode by a constant current method, wherein the deposition current was 0.5 A and the deposition time was 600 s, and then rinsed with deionized water and blown dry to obtain a working electrode with a surface modified with a gold nanofilm.
[0154] 42) Using Shanghai Chenhua's CHI-660E electrochemical workstation, commercial platinum wire counter electrode and silver / silver chloride reference electrode, potassium chloride, hydrochloric acid and water were evenly mixed in a mass ratio of 10.6:0.70:1000 to obtain an electrolyte, in which the reference electrode was chlorinated by cyclic voltammetry with a scan range of -0.15-1.05 V, a scan rate of 50 mV / s, and 5 scans. The electrode was then rinsed with deionized water and dried to obtain a silver / silver chloride reference electrode.
[0155] S5. Synthesis of photoelectrochemical sensitive materials and functional modification of working electrode surface
[0156] 51) Prepare precursor solution:
[0157] Zinc acetate, thiourea, water and ethylenediamine were uniformly mixed in a mass ratio of 27:8:220:0.68 to obtain a precursor solution.
[0158] 52) Preparation of zinc sulfide nanosheets / redox graphene composite powder
[0159] 10 mg of redox graphene was added to 40 mL of the precursor solution, and then placed in a Teflon autoclave and heated to 120°C for 12 hours. After the heating was completed, the product was cleaned and dried in a vacuum to obtain a zinc sulfide nanosheet / redox graphene composite material powder.
[0160] 53) Preparation of bismuth vanadate nanorod powder
[0161] Bismuth nitrate pentahydrate, polyvinyl pyrrolidone, water and nitric acid are mixed evenly in a mass ratio of 5:3.0:20:4.5 to obtain solution A. Ammonium vanadate, water and sodium hydroxide are mixed and dissolved evenly in a mass ratio of 1:20:3.2 to obtain solution B. Solution B is added dropwise to solution A under stirring conditions, and the pH is adjusted to 7.0 with nitric acid solution or ammonia water. The prepared mixed solution is transferred to a high-temperature reactor, heated to 200°C and reacted for 18 hours. The reaction product is then centrifuged, washed, and dried to obtain bismuth vanadate nanorod powder;
[0162] 54) Modification of functional materials on the working electrode surface
[0163] The zinc sulfide nanosheet / redox graphene composite material and bismuth vanadate nanorod powder were mixed with pineneol at a mass ratio of 0.06:0.26 to form two suspensions. 7 μL of the zinc sulfide nanosheet / redox graphene suspension was dropped on the working electrode surface, and after natural drying, 7 μL of bismuth vanadate nanorod powder suspension was added, and after drying again, the working electrode surface modified with zinc sulfide nanosheets, redox graphene and bismuth vanadate nanorods was obtained.
[0164] Prepare 1 mg / mL urate oxidase solution, take 5 μL and drop it on the surface of the working electrode, and place it in a 4°C refrigerator to dry, then drop 10 μL Nafion, and after solidification, obtain a working electrode modified with photoelectrochemical sensitive materials.
[0165] S6, Formation of sweat collection through-hole arrays on polyimide PI substrate
[0166] The structure obtained in step S5 was placed under an ultraviolet femtosecond laser, and 20 cycles of cutting were performed according to the designed structure contour at a power of 10 W and a cutting speed of 1000 mm / min to obtain a sweat collection through-hole array structure on a polyimide PI substrate.
[0167] S7, Forming of sweat collection through hole array and electroosmotic electrode through slot on medical double-sided adhesive layer
[0168] 71) Sandwich the medical double-sided adhesive layer between two pieces of oily paper to protect its adhesiveness, and fix it flatly on a clean glass plate;
[0169] 72) Place the glass plate with the medical double-sided adhesive layer under a femtosecond laser, perform 10 cycles of cutting and laser etching according to the designed structural contour at a power of 8 W and a cutting speed of 1500 mm / min to obtain a sweat collection through-hole array and an electroosmotic electrode through-groove structure on the medical double-sided adhesive layer.
[0170] S8, bonding between polyimide PI substrate and medical double-sided adhesive layer
[0171] Tear off the oily paper on one side of the medical double-sided adhesive layer, and stick it to the sweat extraction electroosmosis electrode pair on the polyimide PI substrate and the lead covering surface. During the pasting process, attention should be paid to the alignment between the substrate and the sweat collection through-hole array on the double-sided adhesive, and between the substrate electrode of the sweat extraction electroosmosis electrode pair and the electroosmosis electrode through-groove, so as to obtain a bonded polyimide PI substrate and medical double-sided adhesive layer.
[0172] S9, electroosmotic anode and cathode coating and forming of sweat extraction electroosmotic electrode pair
[0173] 3% w / w agarose was mixed into deionized water, and the mixture was heated to 200°C with constant stirring until the gel solvent was evenly mixed. The gel solvent was cooled to 170°C, and 1.0% w / w carbachol and 1.0% w / w sodium chloride were added to the two solvents respectively to form anode and cathode colloidal solutions. The above solutions were added into the electroosmotic electrode slot, and after cooling, the electroosmotic anode and cathode of the sweat extraction electroosmotic electrode pair were obtained.
[0174] S10, Processing and molding of sweat collection microchannels
[0175] 101) Fix the waterproof double-sided tape with oily paper on both sides flatly on the clean glass plate;
[0176] 102) The glass plate covered with waterproof double-sided tape was placed under a femtosecond laser, and 10 cycles of cutting and laser etching were performed according to the designed structural contour at a power of 8 W and a cutting speed of 1500 mm / min to obtain a sweat collection microchannel.
[0177] S11, bonding between the sweat collection microchannel and the polyimide PI substrate
[0178] Tear off the oily paper on one side of the waterproof double-sided adhesive channel wall and stick it to the back side of the polyimide PI substrate. During the sticking process, attention should be paid to the alignment between the channel inlet of the double-sided adhesive layer and the sweat collection through-hole array of the structure obtained in step 6 to obtain a stuck sweat collection microchannel and polyimide PI substrate.
[0179] S12, Forming of sweat discharge holes on the flexible packaging layer
[0180] 121) Prepare a mixed solution of PDMS glue A and B at a mass ratio of 10:1, stir thoroughly with a glass rod for 3-8 min, take a glass slide of size 8 cm × 6 cm, clean and blow dry, evenly apply an appropriate amount of PDMS mixed material on the glass slide, and then place the PDMS-coated glass slide on a glue spreader and rotate at a low speed of 400 r / min and a high speed of 1000 r / min for 12 s and 30 s, respectively.
[0181] 122) The glass slide coated with PDMS is taken out from the glue roller and placed in a vacuum filter to remove bubbles in the PDMS film; after the extraction is completed, it is placed on a constant temperature heating table and heated at 100° C. for 1 hour to solidify the PDMS film to obtain a glass slide covered with a flexible encapsulation layer;
[0182] 123) A glass sheet covered with a PDMS encapsulation layer was placed under a femtosecond laser, and 10 cycles of cutting and laser etching were performed according to the designed structural contour at a power of 8 W and a cutting speed of 1500 mm / min to obtain a sweat discharge pore structure on the flexible encapsulation layer.
[0183] S13, Top packaging of flexible photoelectrochemical sensor for POCT of sweat uric acid content
[0184] Tear off the oily paper on the other side of the sweat collection microchannel and stick it firmly to the flexible packaging layer. During the pasting process, care should be taken to ensure that there are no bubbles on the bonding surface to avoid leakage during the use of the device. In addition, attention should be paid to the alignment between the sweat discharge holes on the PDMS packaging layer and the outlet of the double-sided tape channel, and finally a flexible photoelectrochemical sensor for POCT of sweat uric acid content with top encapsulation was obtained.
[0185] Example 2
[0186] S1, polyimide PI substrate (one side) sweat extraction electroosmosis electrode to substrate electrode and lead forming
[0187] 11) Cut a 8cm×6cm polyimide PI film, lay it flat on a clean dispensing printer workbench and fix the four corners;
[0188] 12) Using the VOLTERA V-One dispensing machine and its dedicated conductive silver paste, the printing mode was selected as simple printing, and the pass spacing of the printing process was set to 0.3 mm, the feed rate to 70 mm / min, and the fluidity to 1.5 mm, to achieve patterned printing of the sweat-derived electro-osmotic electrode to the base electrode and the lead wire;
[0189] 13) The polyimide PI substrate with the sweat extraction electroosmosis electrode pair base electrode and lead pattern is placed on a 50°C hot plate and heated until the conductive silver paste solidifies and cools to room temperature to obtain the sweat extraction electroosmosis electrode pair base electrode and lead structure.
[0190] S2, polyimide substrate (the other side) substrate electrode and lead forming of the photoelectrochemical sensing three electrodes
[0191] 21) Turn over the polyimide PI substrate and lay it flat on a clean dispensing printer workbench, fix the four corners of the film, and be careful not to damage the sweat-extracting electro-osmotic electrode on the back to the substrate electrode and the lead structure during the process;
[0192] 22) Using the VOLTERA V-One dispensing machine and its dedicated conductive silver paste, select the printing mode as simple printing, and set the pass spacing of the printing process to 0.3mm, the feed rate to 70mm / min, and the fluidity to 1.5mm to achieve patterned printing of the base electrode and lead of the three-electrode photoelectrochemical sensor;
[0193] 23) The polyimide PI substrate is placed on a 50° C. hot plate and heated until the conductive silver paste is completely solidified, thereby obtaining a base electrode and lead structure of the photoelectrochemical sensing three electrodes on the other side of the polyimide PI substrate.
[0194] S3, Carbon layer modification on the counter electrode and working electrode in the three-electrode photoelectrochemical sensor
[0195] 31) Using the VOLTERA V-One dispensing machine, select the printing mode as positioning printing to achieve the selection and positioning of the counter electrode and working electrode areas;
[0196] 32) Based on the CH-8 carbon paste of Shijo Company, the dispensing machine feed rate was set to 100 mm / min and the fluidity to 0.8 mm to achieve selective modification of the conductive carbon paste on the counter electrode and the working electrode;
[0197] 33) The polyimide PI substrate is placed on a hot plate at 100° C. and heated until the carbon slurry is solidified, and then cooled to room temperature to obtain a carbon layer-modified counter electrode and a working electrode in the photoelectrochemical sensing three-electrode.
[0198] S4, Gold nanofilm modification on the working electrode and chlorination of the reference electrode in the photoelectrochemical sensing three-electrode
[0199] 41) Using Shanghai Chenhua's CHI-660E electrochemical workstation, commercial platinum wire counter electrode and silver / silver chloride reference electrode, sulfuric acid, chloroauric acid and water were evenly mixed in a mass ratio of 98:0.86:1000 to obtain an electrolyte, in which gold nanoparticles were deposited on the surface of the working electrode by a constant current method, wherein the deposition current was 0.2 A and the deposition time was 800 s, and then rinsed with deionized water and blown dry to obtain a working electrode with a surface modified with a gold nanofilm.
[0200] 42) Using Shanghai Chenhua's CHI-660E electrochemical workstation, commercial platinum wire counter electrode and silver / silver chloride reference electrode, potassium chloride, hydrochloric acid and water were evenly mixed in a mass ratio of 3.73:1.75:1000 to obtain an electrolyte, in which the reference electrode was chlorinated by cyclic voltammetry with a scan range of -0.15-1.05 V, a scan rate of 100 mV / s, and 8 scans. The electrode was then rinsed with deionized water and dried to obtain a silver / silver chloride reference electrode.
[0201] S5. Synthesis of photoelectrochemical sensitive materials and functional modification of working electrode surface
[0202] 51) Prepare precursor solution:
[0203] Zinc acetate, thiourea, water and ethylenediamine were uniformly mixed in a mass ratio of 37:30:250:0.67 to obtain a precursor solution.
[0204] 52) Preparation of zinc sulfide nanosheets / redox graphene composite powder
[0205] 3 mg of redox graphene was added to 30 mL of the precursor solution, and then placed in a Teflon autoclave and heated to 150°C for 10 hours. After the heating was completed, the product was cleaned and dried in a vacuum to obtain zinc sulfide nanosheets / redox graphene composite material powder.
[0206] 53) Preparation of bismuth vanadate nanorod powder
[0207] Bismuth nitrate pentahydrate, polyvinyl pyrrolidone, water and nitric acid are mixed evenly in a mass ratio of 6:2.2:20:7.5 to obtain solution A. Ammonium vanadate, water and sodium hydroxide are mixed and dissolved evenly in a mass ratio of 1.5:10:4.8 to obtain solution B. Solution B is added dropwise to solution A under stirring conditions, and the pH is adjusted to 7.0 with nitric acid solution or ammonia water. The prepared mixed solution is transferred to a high-temperature reactor, heated to 180°C for reaction for 20 hours. The reaction product is then centrifuged, washed, and dried to obtain bismuth vanadate nanorod powder;
[0208] 54) Modification of functional materials on the working electrode surface
[0209] The zinc sulfide nanosheet / redox graphene composite material and bismuth vanadate nanorod powder were mixed with pineneol at a mass ratio of 0.03:0.09 to form two suspensions. 10 μL of the zinc sulfide nanosheet / redox graphene suspension was dropped on the working electrode surface, and after natural drying, 10 μL of bismuth vanadate nanorod powder suspension was added, and after drying again, the working electrode surface modified with zinc sulfide nanosheets, redox graphene and bismuth vanadate nanorods was obtained.
[0210] Prepare 2 mg / mL urate oxidase solution, take 10 μL and drop it on the surface of the working electrode, and place it in a 4°C refrigerator to dry, then drop 5 μL Nafion, and after solidification, obtain a working electrode modified with photoelectrochemical sensitive materials.
[0211] S6, Formation of sweat collection through-hole arrays on polyimide PI substrate
[0212] The structure obtained in step S5 was placed under an ultraviolet femtosecond laser, and 10 cycles of cutting were performed according to the designed structure contour at a power of 8 W and a cutting speed of 1500 mm / min to obtain a sweat collection through-hole array structure on a polyimide PI substrate.
[0213] S7, Forming of sweat collection through hole array and electroosmotic electrode through slot on medical double-sided adhesive layer
[0214] 71) Sandwich the medical double-sided adhesive layer between two pieces of oily paper to protect its adhesiveness, and fix it flatly on a clean glass plate;
[0215] 72) Place the glass plate with the medical double-sided adhesive layer under a femtosecond laser, perform 5 cycles of cutting and laser etching according to the designed structural contour at a power of 10 W and a cutting speed of 1000 mm / min to obtain a sweat collection through-hole array and an electroosmotic electrode through-groove structure on the medical double-sided adhesive layer.
[0216] S8, bonding between polyimide PI substrate and medical double-sided adhesive layer
[0217] Tear off the oily paper on one side of the medical double-sided adhesive layer, and stick it to the sweat extraction electroosmosis electrode pair on the polyimide PI substrate and the lead covering surface. During the pasting process, attention should be paid to the alignment between the substrate and the sweat collection through-hole array on the double-sided adhesive, and between the substrate electrode of the sweat extraction electroosmosis electrode pair and the electroosmosis electrode through-groove, so as to obtain a bonded polyimide PI substrate and medical double-sided adhesive layer.
[0218] S9, electroosmotic anode and cathode coating and forming of sweat extraction electroosmotic electrode pair
[0219] 2% w / w agarose was mixed into deionized water, and the mixture was heated to 220°C with constant stirring until the gel solvent was evenly mixed. The gel solvent was cooled to 160°C, and 0.8% w / w carbachol and 0.8% w / w sodium chloride were added to the two solvents respectively to form anode and cathode colloidal solutions. The above solutions were added into the electroosmotic electrode slot, and after cooling, the electroosmotic anode and cathode of the sweat extraction electroosmotic electrode pair were obtained.
[0220] S10, Processing and molding of sweat collection microchannels
[0221] 102) Fix the waterproof double-sided tape with oily paper on both sides flatly on the clean glass plate;
[0222] 102) The glass plate covered with waterproof double-sided tape was placed under a femtosecond laser, and 5 cycles of cutting and laser etching were performed according to the designed structural contour at a power of 10 W and a cutting speed of 1000 mm / min to obtain a sweat collection microchannel.
[0223] S11, bonding between the sweat collection microchannel and the polyimide PI substrate
[0224] Tear off the oily paper on one side of the waterproof double-sided adhesive channel wall and stick it to the back side of the polyimide PI substrate. During the sticking process, attention should be paid to the alignment between the channel inlet of the double-sided adhesive layer and the sweat collection through-hole array of the structure obtained in step 6 to obtain a stuck sweat collection microchannel and polyimide PI substrate.
[0225] S12, Forming of sweat discharge holes on the flexible packaging layer
[0226] 121) Prepare a mixed solution of PDMS glue A and B at a mass ratio of 10:1, stir thoroughly with a glass rod for 3-8 min, take a glass slide of size 8 cm × 6 cm, clean and blow dry, evenly apply an appropriate amount of PDMS mixed material on the glass slide, and then place the glass slide coated with PDMS on a glue spreader and rotate at a low speed of 600 r / min and a high speed of 1500 r / min for 10 s and 20 s respectively.
[0227] 122) The glass slide coated with PDMS was taken out from the glue machine and placed in a vacuum filter to remove bubbles in the PDMS film; after the extraction, it was placed on a constant temperature heating table and heated at 90° C. for 1.5 h to solidify the PDMS film, thereby obtaining a glass slide covered with a flexible encapsulation layer;
[0228] 123) The glass sheet covered with the PDMS encapsulation layer was placed under a femtosecond laser, and 5 cycles of cutting and laser etching were performed according to the designed structure contour at a power of 10 W and a cutting speed of 1000 mm / min to obtain the sweat discharge pore structure on the flexible encapsulation layer.
[0229] S13, Top packaging of flexible photoelectrochemical sensor for POCT of sweat uric acid content
[0230] Tear off the oily paper on the other side of the sweat collection microchannel and stick it firmly to the flexible packaging layer. During the pasting process, care should be taken to ensure that there are no bubbles on the bonding surface to avoid leakage during the use of the device. In addition, attention should be paid to the alignment between the sweat discharge holes on the PDMS packaging layer and the outlet of the double-sided tape channel, and finally a flexible photoelectrochemical sensor for POCT of sweat uric acid content with top encapsulation was obtained.
[0231] Example 3
[0232] S1, polyimide PI substrate (one side) sweat extraction electroosmosis electrode to substrate electrode and lead forming
[0233] 11) Cut a 8cm×6cm polyimide PI film, lay it flat on a clean dispensing printer workbench and fix the four corners;
[0234] 12) Using the VOLTERA V-One dispensing machine and its dedicated conductive silver paste, the printing mode was selected as simple printing, and the pass spacing of the printing process was set to 0.2 mm, the feed rate to 200 mm / min, and the fluidity to 0.5 mm, to achieve patterned printing of the sweat-derived electro-osmotic electrode to the base electrode and the lead wire;
[0235] 13) The polyimide PI substrate with the sweat extraction electroosmosis electrode pair base electrode and lead pattern is placed on a hot plate at 80°C and heated until the conductive silver paste solidifies and cools to room temperature to obtain the sweat extraction electroosmosis electrode pair base electrode and lead structure.
[0236] S2, polyimide substrate (the other side) substrate electrode and lead forming of the photoelectrochemical sensing three electrodes
[0237] 21) Turn over the polyimide PI substrate and lay it flat on a clean dispensing printer workbench, fix the four corners of the film, and be careful not to damage the sweat-extracting electro-osmotic electrode on the back to the substrate electrode and the lead structure during the process;
[0238] 22) Using the VOLTERA V-One dispensing machine and its dedicated conductive silver paste, select the printing mode as simple printing, and set the pass spacing of the printing process to 0.2mm, the feed rate to 200mm / min, and the fluidity to 0.5mm to achieve patterned printing of the base electrode and lead of the three electrodes of the photoelectrochemical sensor;
[0239] 23) The polyimide PI substrate is placed on a hot plate at 80° C. and heated until the conductive silver paste is completely cured, thereby obtaining a base electrode and lead structure of the photoelectrochemical sensing three electrodes on the other side of the polyimide PI substrate.
[0240] S3, Carbon layer modification on the counter electrode and working electrode in the three-electrode photoelectrochemical sensor
[0241] 31) Using the VOLTERA V-One dispensing machine, select the printing mode as positioning printing to achieve the selection and positioning of the counter electrode and working electrode areas;
[0242] 32) Based on the CH-8 carbon paste of Shijo Company, the dispensing machine feed rate was set to 300 mm / min and the fluidity to 0.3 mm to achieve selective modification of the conductive carbon paste on the counter electrode and the working electrode;
[0243] 33) The polyimide PI substrate is placed on a hot plate at 80°C and heated until the carbon slurry solidifies, and then cooled to room temperature to obtain a carbon layer-modified counter electrode and a working electrode in the photoelectrochemical sensing three-electrode.
[0244] S4, Gold nanofilm modification on the working electrode and chlorination of the reference electrode in the photoelectrochemical sensing three-electrode
[0245] 41) Using Shanghai Chenhua's CHI-660E electrochemical workstation, commercial platinum wire counter electrode and silver / silver chloride reference electrode, sulfuric acid, chloroauric acid and water were evenly mixed in a mass ratio of 294:0.17:1000 to obtain an electrolyte, in which gold nanoparticles were deposited on the surface of the working electrode by a constant current method, wherein the deposition current was 0.6 A and the deposition time was 400 s, and then rinsed with deionized water and blown dry to obtain a working electrode with a surface modified with a gold nanofilm.
[0246] 42) Using Shanghai Chenhua's CHI-660E electrochemical workstation, commercial platinum wire counter electrode and silver / silver chloride reference electrode, potassium chloride, hydrochloric acid and water were evenly mixed in a mass ratio of 15:28:1000 to obtain an electrolyte, in which the reference electrode was chlorinated by cyclic voltammetry with a scan range of -0.15-1.05 V, a scan rate of 25 mV / s, and 5 scans. The electrode was then rinsed with deionized water and dried to obtain a silver / silver chloride reference electrode.
[0247] S5. Synthesis of photoelectrochemical sensitive materials and functional modification of working electrode surface
[0248] 51) Prepare precursor solution:
[0249] Zinc acetate, thiourea, water and ethylenediamine were uniformly mixed in a mass ratio of 9:18:200:0.72 to obtain a precursor solution.
[0250] 52) Preparation of zinc sulfide nanosheets / redox graphene composite powder
[0251] 8 mg of redox graphene was added to 50 mL of the precursor solution, and then placed in a Teflon autoclave and heated to 140°C for 16 hours. After the heating was completed, the product was cleaned and dried in a vacuum to obtain zinc sulfide nanosheets / redox graphene composite material powder.
[0252] 53) Preparation of bismuth vanadate nanorod powder
[0253] Bismuth nitrate pentahydrate, polyvinyl pyrrolidone, water and nitric acid are mixed evenly in a mass ratio of 3:0.5:20:2.5 to obtain solution A. Ammonium vanadate, water and sodium hydroxide are mixed and dissolved evenly in a mass ratio of 2:30:1.6 to obtain solution B. Solution B is added dropwise to solution A under stirring conditions, and the pH is adjusted to 7.0 with nitric acid solution or ammonia water. The prepared mixed solution is transferred to a high-temperature reactor, heated to 160°C for reaction for 24 hours. The reaction product is then centrifuged, washed, and dried to obtain bismuth vanadate nanorod powder;
[0254] 54) Modification of functional materials on the working electrode surface
[0255] The zinc sulfide nanosheet / redox graphene composite material and bismuth vanadate nanorod powder were mixed with pineneol at a mass ratio of 0.10:0.36 to form two suspensions. 5 μL of the zinc sulfide nanosheet / redox graphene suspension was dropped on the working electrode surface, and after natural drying, 5 μL of bismuth vanadate nanorod powder suspension was added, and after drying again, the working electrode surface modified with zinc sulfide nanosheets, redox graphene and bismuth vanadate nanorods was obtained.
[0256] A 0.5 mg / mL urate oxidase solution was prepared, 8 μL was dripped on the surface of the working electrode, and placed in a 4°C refrigerator to dry, and then 15 μL of Nafion was dripped on. After solidification, a working electrode modified with a photoelectrochemical sensitive material was obtained.
[0257] S6, Formation of sweat collection through-hole arrays on polyimide PI substrate
[0258] The structure obtained in step S5 was placed under an ultraviolet femtosecond laser, and 5 cycles of cutting were performed according to the designed structure contour at a power of 5 W and a cutting speed of 2000 mm / min to obtain a sweat collection through-hole array structure on a polyimide PI substrate.
[0259] S7, Forming of sweat collection through hole array and electroosmotic electrode through slot on medical double-sided adhesive layer
[0260] 71) Sandwich the medical double-sided adhesive layer between two pieces of oily paper to protect its adhesiveness, and fix it flatly on a clean glass plate;
[0261] 72) The glass plate with the medical double-sided adhesive layer is placed under a femtosecond laser, and 20 cycles of cutting are performed according to the designed structural contour at a power of 5 W and a cutting speed of 2000 mm / min, and laser etching is performed to obtain a sweat collection through-hole array and an electroosmotic electrode through-groove structure on the medical double-sided adhesive layer.
[0262] S8, bonding between polyimide PI substrate and medical double-sided adhesive layer
[0263] Tear off the oily paper on one side of the medical double-sided adhesive layer, and stick it to the sweat extraction electroosmosis electrode pair on the polyimide PI substrate and the lead covering surface. During the pasting process, attention should be paid to the alignment between the substrate and the sweat collection through-hole array on the double-sided adhesive, and between the substrate electrode of the sweat extraction electroosmosis electrode pair and the electroosmosis electrode through-groove, so as to obtain a bonded polyimide PI substrate and medical double-sided adhesive layer.
[0264] S9, electroosmotic anode and cathode coating and forming of sweat extraction electroosmotic electrode pair
[0265] 5% w / w agarose was mixed into deionized water, and the mixture was heated to 250°C with constant stirring until the gel solvent was evenly mixed. The gel solvent was cooled to 150°C, and 1.2% w / w carbachol and 1.2% w / w sodium chloride were added to two portions of the gel solvent respectively to form anode and cathode colloidal solutions. The colloidal solution was added into the electroosmotic electrode slot, and after cooling, the electroosmotic anode and cathode of the sweat extraction electroosmotic electrode pair were obtained.
[0266] S10, Processing and molding of sweat collection microchannels
[0267] 103) Fix the waterproof double-sided tape with oily paper on both sides flatly on the clean glass plate;
[0268] 102) The glass plate covered with waterproof double-sided tape was placed under a femtosecond laser, and 20 cycles of cutting and laser etching were performed according to the designed structural contour at a power of 5 W and a cutting speed of 2000 mm / min to obtain a sweat collection microchannel.
[0269] S11, bonding between the sweat collection microchannel and the polyimide PI substrate
[0270] Tear off the oily paper on one side of the waterproof double-sided adhesive channel wall and stick it to the back side of the polyimide PI substrate. During the sticking process, attention should be paid to the alignment between the channel inlet of the double-sided adhesive layer and the sweat collection through-hole array of the structure obtained in step 6 to obtain a stuck sweat collection microchannel and polyimide PI substrate.
[0271] S12, Forming of sweat discharge holes on the flexible packaging layer
[0272] 121) Prepare a mixed solution of PDMS glue A and B at a mass ratio of 10:1, stir thoroughly with a glass rod for 3-8 min, take a glass slide of 8 cm × 6 cm, clean and blow dry, evenly apply an appropriate amount of PDMS mixed material on the glass slide, and then place the PDMS-coated glass slide on a glue spreader and rotate at a low speed of 200 r / min and a high speed of 800 r / min for 15 s and 40 s, respectively.
[0273] 122) The glass slide coated with PDMS is taken out from the coating machine and placed in a vacuum filter to remove bubbles in the PDMS film; after the extraction is completed, it is placed on a constant temperature heating table and heated at 120° C. for 1 hour to solidify the PDMS film to obtain a glass slide covered with a flexible encapsulation layer;
[0274] 123) A glass sheet covered with a PDMS encapsulation layer was placed under a femtosecond laser, and 20 cycles of cutting and laser etching were performed according to the designed structural contour at a power of 5 W and a cutting speed of 2000 mm / min to obtain a sweat discharge pore structure on the flexible encapsulation layer.
[0275] S13, Top packaging of flexible photoelectrochemical sensor for POCT of sweat uric acid content
[0276] Tear off the oily paper on the other side of the sweat collection microchannel and stick it firmly to the flexible packaging layer. During the pasting process, care should be taken to ensure that there are no bubbles on the bonding surface to avoid leakage during the use of the device. In addition, attention should be paid to the alignment between the sweat discharge holes on the PDMS packaging layer and the outlet of the double-sided tape channel, and finally a flexible photoelectrochemical sensor for POCT of sweat uric acid content with top encapsulation was obtained.
[0277] From the above examples, it can be seen that the flexible photoelectric chemical sensor of the present invention detects the uric acid content in sweat (no more than 35.7 μmol / L) with high detection sensitivity, which can reach 200 μA·mM -1 cm -2 above.
[0278] In addition, compared with conventional clinical blood uricase detection methods, the present invention does not require high-end detection equipment, is not restricted by time and location, and does not require professional technicians to operate. It can better detect changes in uric acid content in patients' sweat in real time online, and provides new strategies and technical guarantees for continuous monitoring of uric acid-related diseases, customization of personalized diagnosis and treatment plans for patients, remote early warning for critically ill patients, home treatment of chronic diseases, research on the pathogenesis of multiple diseases, analysis of the action mechanism of specific drugs, and development of new drugs.
[0279] The present invention also provides a method for preparing a flexible photoelectrochemical sensor for POCT of sweat uric acid content, which involves multiple core manufacturing technologies such as multi-scale laser precision machining, microchannel design and preparation technology, gel electrode preparation, 3D dispensing printing, electrochemical modification, hydrothermal synthesis, and electrochemical deposition. It provides a technical solution for the construction and optimization of flexible microfluidic sensor devices of the same type of biochemical markers.
[0280] The present invention is not limited to the above-mentioned embodiments. On the basis of the technical solution disclosed in the present invention, technicians in this field can make some substitutions and deformations to some technical features therein according to the disclosed technical content without creative labor, and these substitutions and deformations are all within the protection scope of the present invention.
Claims
1. A flexible photoelectrochemical sensor for real-time detection of uric acid content in sweat, characterized in that: It includes a medical double-sided adhesive layer, a sweat extraction electro-osmotic electrode pair, a photoelectrochemical sensing three-electrode, a polyimide PI substrate, a photoelectrochemical sensitive material, a sweat collection microchannel and a flexible packaging layer which are sequentially distributed from bottom to top; The medical double-sided adhesive layer is provided with a sweat collection through-hole array and two upper and lower electroosmotic electrode through-grooves; The sweat extraction electroosmotic electrode pair comprises a pair of electroosmotic anodes and electroosmotic cathodes, wherein the electroosmotic anodes and the electroosmotic cathodes are respectively overlapped with the upper and lower electroosmotic electrode slots; The three electrodes of photoelectrochemical sensing include counter electrode, working electrode and reference electrode; A sweat collecting through hole array is provided on the polyimide PI substrate, and the sweat collecting through hole array corresponds to the sweat collecting through hole array on the medical double-sided adhesive layer; The sweat collection microchannel is provided with a plurality of channel inlets and a channel outlet respectively connected with each through hole of the sweat collection through hole array; The flexible packaging layer is provided with a sweat discharge hole corresponding to the flow channel outlet; The sweat in the skin sweat glands is non-invasively extracted through the sweat extraction electro-osmosis electrode, and the sweat is transported to the photoelectrochemical sensing three electrodes through the sweat collection microchannel. The photoelectrochemical reaction is carried out by the contact between the sweat and the photoelectrochemical sensitive material to realize the detection of uric acid content in sweat.
2. The flexible photoelectrochemical sensor for real-time detection of uric acid content in sweat according to claim 1, characterized in that: The upper and lower electroosmotic electrode slots are arranged from bottom to top, and the sweat collection through hole array is located below the lower electroosmotic electrode slot.
3. The flexible photoelectrochemical sensor for real-time detection of uric acid content in sweat according to claim 1, characterized in that: The electro-osmosis anode and the electro-osmosis cathode of the sweat extraction electro-osmosis electrode pair are arranged in a pair of sickle shapes facing each other, and the length of the curved hook arc section of the electro-osmosis anode is smaller than that of the electro-osmosis cathode arc section.
4. The flexible photoelectrochemical sensor for real-time detection of uric acid content in sweat according to claim 1, characterized in that: The working electrode is located in the middle of the three photoelectrochemical sensors and is a straight line segment; the counter electrode and the reference electrode are located on both sides of the three photoelectrochemical sensors and are symmetrically arched; after superposition, the periphery of the three photoelectrochemical sensors is located within the sickle-shaped electrode frame of the sweat extraction electroosmosis electrode pair.
5. The flexible photoelectrochemical sensor for real-time detection of uric acid content in sweat according to claim 1, characterized in that: The sweat collection microchannel includes a circular channel, which is connected to multiple channel inlets, each of which is connected to each through hole of the sweat collection through hole array, and is connected to a channel outlet on the circular channel; the counter electrode, working electrode and reference electrode of the three-electrode photoelectrochemical sensor are located in the circular channel frame.
6. A method for preparing a flexible photoelectrochemical sensor for real-time detection of uric acid content in sweat as claimed in any one of claims 1 to 5, characterized in that: The steps include: Step 1, polyimide PI substrate sweat extraction electroosmosis electrode to substrate electrode and lead wire: Print sweat-extracting electroosmotic electrodes to base electrodes and lead patterns on one side of the polyimide PI film; Step 2, base electrode and leads of polyimide PI substrate photoelectrochemical sensing three electrodes: Print the substrate electrode and lead pattern of the photoelectrochemical sensing three electrodes on the other side of the polyimide PI substrate; Step 3, modification of the carbon layer on the counter electrode and working electrode in the photoelectrochemical sensing three-electrode: Positioning and printing the counter electrode and the working electrode on the polyimide PI substrate surface printed with the base electrode and lead pattern of the photoelectrochemical sensing three electrodes, heating and curing, and obtaining the carbon layer-modified counter electrode and working electrode in the photoelectrochemical sensing three electrodes; Step 4, modification of the gold nanofilm on the working electrode and chlorination of the reference electrode in the photoelectrochemical sensing three-electrode: Gold nanoparticles are deposited on the surface of the working electrode in the photoelectrochemical sensing three-electrode by electrodeposition in a chloroauric acid / sulfuric acid mixed electrolyte, and then rinsed and dried to obtain a working electrode with a gold nanofilm modified on the surface; The reference electrode is chlorinated and modified by cyclic voltammetry in a potassium chloride / hydrochloric acid mixed electrolyte, and then rinsed and dried to obtain a silver / silver chloride reference electrode; Step 5, synthesis of photoelectrochemical sensitive materials and functional modification of the working electrode surface: Zinc sulfide nanosheets, redox graphene and bismuth vanadate nanorods were synthesized by hydrothermal and sol-gel methods and dispersed in a solvent; Add zinc sulfide nanosheets, redox graphene and bismuth vanadate nanorod dispersions to the surface of the working electrode modified with gold nanofilm obtained in step 4, add urate oxidase solution to it after natural drying, and then drip Nafion after drying again, and obtain the working electrode modified with photoelectrochemical sensitive material after curing; Step 6, forming a sweat collection through-hole array on a polyimide PI substrate: The polyimide PI substrate where the photoelectrochemical sensing three electrodes modified with the photoelectrochemical sensitive material obtained in step 5 are located is subjected to laser cyclic cutting and laser etching to obtain a sweat collection through-hole array structure on the polyimide PI substrate; Step 7, forming the sweat collection through hole array and the electroosmotic electrode through groove on the medical double-sided adhesive layer: The medical double-sided adhesive layer is sandwiched between two pieces of oily paper, and the medical double-sided adhesive layer with the oily paper is subjected to laser circular cutting and laser etching to obtain a sweat collection through-hole array and an electroosmotic electrode through-groove structure on the medical double-sided adhesive layer; Step 8, bonding between the polyimide PI substrate and the medical double-sided adhesive layer: Tear off the oily paper attached to one side of the medical double-sided adhesive layer obtained in step 7, and stick it on the sweat extraction electroosmosis electrode pair substrate electrode and lead covering surface of the structure prepared in step 6, and align it with the sweat collection through hole array on the double-sided adhesive, the sweat extraction electroosmosis electrode pair substrate electrode and the electroosmosis electrode through groove to obtain a bonded polyimide PI substrate and medical double-sided adhesive layer; Step 9, the electro-osmosis anode and cathode of the sweat extraction electro-osmosis electrode pair are formed by coating with glue: An agarose aqueous solution is prepared, carbachol and sodium chloride are added to two agarose aqueous solutions respectively and stirred evenly to form an anode and a cathode colloidal solution, and the solutions are cooled and added to the electroosmotic electrode slots respectively to obtain an electroosmotic anode and a cathode of a sweat extraction electroosmotic electrode pair; Step 10: Processing and molding of sweat collection microchannels: The glass plate covered with waterproof double-sided tape was laser cut and laser etched to obtain the sweat collection microchannel; Step 11: Lamination between the sweat collection microchannel and the polyimide PI substrate: Tear off the oily paper on one side of the sweat collection microfluidic channel, and attach it to the back side of the structure obtained in step 9, align the inlet of the sweat collection microfluidic channel of the double-sided adhesive layer with the sweat collection through-hole array of the structure obtained in step 6, and obtain the attached sweat collection microfluidic channel and the polyimide PI substrate; Step 12, forming the sweat discharge holes on the flexible packaging layer: Prepare a PDMS mixed solution, and spin-coat the PDMS mixed solution on a clean glass sheet; The air bubbles are removed by vacuum filtration, and the PDMS film is cured by constant temperature heating to obtain a glass sheet covered with a flexible encapsulation layer; The glass sheet covered with the PDMS film is subjected to laser cyclic cutting and laser etching to obtain the sweat discharge hole structure on the flexible encapsulation layer; Step 13, top packaging of flexible photoelectrochemical sensor for POCT of sweat uric acid content: Tear off the oily paper on the other side of the sweat collection microchannel structure obtained in step 11, and stick it firmly to the flexible packaging layer. Align the sweat discharge holes on the flexible packaging layer with the outlet of the sweat collection microchannel to obtain a top-encapsulated flexible photoelectrochemical sensor for POCT of sweat uric acid content.
7. The method for preparing a flexible photoelectrochemical sensor for real-time detection of uric acid content in sweat according to claim 6, characterized in that: In steps 1 and 2, the printing process is set to have a pass spacing of 0.1-0.3 mm, a feed rate of 70-200 mm / min, and a fluidity of 0.5-1.5 mm; the polyimide PI substrate after the dispensing printing is placed on a hot plate at 50-80° C., heated and cured, and then cooled to room temperature; In step 3, set the dispensing machine feed rate to 100-300 mm / min and the fluidity to 0.3-0.8 mm; place the polyimide PI substrate that has completed positioning printing on a hot plate at 80-100°C, heat and cure, and then cool to room temperature.
8. The method for preparing a flexible photoelectrochemical sensor for real-time detection of uric acid content in sweat according to claim 6, characterized in that: In step 4, sulfuric acid, chloroauric acid and water are mixed uniformly in a mass ratio of (98–295):(0.17–1.36):1000 to obtain an electrolyte, and gold nanoparticles are deposited on the surface of the working electrode at a constant current of 0.2-0.6 A in the chloroauric acid / sulfuric acid mixed electrolyte for 400-800 s; Potassium chloride, hydrochloric acid and water were mixed evenly in a mass ratio of (3.7-15):(0.70-2.8):1000 to obtain an electrolyte, and the reference electrode was chlorinated by cyclic voltammetry with a scanning range of -0.15-1.05 V, a scanning rate of 25-100 mV / s, and a scanning number of 5-10 times. The electrode was rinsed and dried to obtain a silver / silver chloride reference electrode.
9. The method for preparing a flexible photoelectrochemical sensor for real-time detection of uric acid content in sweat according to claim 6, characterized in that: In step 5, the preparation of the working electrode modified with the photoelectrochemical sensitive material includes: a. Prepare precursor solution: Zinc acetate, thiourea, water and ethylenediamine were uniformly mixed in a mass ratio of (9.–37):(8–30):(200–250):(0.67–0.72) to obtain a precursor solution; b. Preparation of zinc sulfide nanosheets / redox graphene composite powder: Add redox graphene to the precursor solution in a mass ratio of (30–50):(3–10) and heat at 120–150°C for 10–16 hours; c. Preparation of bismuth vanadate nanorod powder: Bismuth nitrate pentahydrate, polyvinyl pyrrolidone, water and nitric acid are mixed uniformly according to a mass ratio of (3-6): (0.5-3.0): 20: (2.5-7.5) to obtain solution A; ammonium vanadate, water and sodium hydroxide are mixed and dissolved uniformly according to a mass ratio of (1-2): (10-30): (1.6-4.8) to obtain solution B; solution B is added dropwise to solution A under stirring conditions, and the pH is adjusted to 7.0; the mixed solution is heated at 160-200°C for 18-24 hours; the reaction product is centrifuged, washed and dried to obtain bismuth vanadate nanorod powder; d. The zinc sulfide nanosheet / redox graphene composite material and bismuth vanadate nanorod powder were mixed with pineneol in a mass ratio of (0.03–0.10):(0.09–0.36) to form two suspensions; Dropping a zinc sulfide nanosheet / redox graphene suspension onto the surface of the working electrode, allowing it to dry naturally, then dropping a bismuth vanadate nanorod powder suspension onto it, and drying it again to obtain a working electrode surface modified with zinc sulfide nanosheets, redox graphene, and bismuth vanadate nanorods; The urate oxidase solution was dripped onto the surface of the working electrode, left to dry at 4°C, and then dripped with Nafion. After solidification, a working electrode modified with a photoelectrochemical sensitive material was obtained.
10. The method for preparing a flexible photoelectrochemical sensor for real-time detection of uric acid content in sweat according to claim 6, characterized in that: In steps 7, 10, and 12, laser cutting is performed 5–20 times according to the designed structural contour at a power of 5–10 W and a cutting speed of 1000–2000 mm / min; In step 9, the electro-osmotic anode and cathode of the sweat-extracting electro-osmotic electrode pair are formed by coating with glue: 2-5% w / w agarose is mixed in deionized water, heated at 200-250°C to prepare a gel solution, cooled to 150-170°C, and 0.8-1.2% w / w carbachol and 0.8-1.2% w / w sodium chloride are added to two portions of the gel solution, respectively, to form anode and cathode colloid solutions.
Citation Information
Patent Citations
Structure of detection microsensor and detecting method thereof
CN110455887A
Electrochemical method for detecting uric acid and urate oxidase and application thereof
CN111879836A
PEDOT: PSS hydrogel modified electrode and preparation method and application thereof
CN113466304A
Uric acid sensor and preparation method and application thereof
CN115616053A
High-sensitivity and high-selectivity sweat collection and detection electrochemical sensor and preparation method thereof
CN116337964A
Cited By
Microstructure electrode flexible electrochemical sensor
CN120436628A