Automobile finish paint repairing method
By reasonably setting the paint film coverage and layer-by-layer spraying technology in automotive topcoat repair, the color difference problem of metal paint repair is solved, the repair quality is improved and the cost is reduced, and efficient repair of metal paint and mica paint is achieved.
Patent Information
- Application Number
- CN202411362803.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-27
- Publication Date
- 2024-12-03
AI Technical Summary
Car topcoat repairs of metal paint and mica paint are prone to repair color difference problems, especially when the topcoat is made of metal paint, the color difference problem in the repaired parts is serious, which often leads to "black circles" phenomenon, affecting the appearance quality of the paint surface, and a large area of the whole. Spray treatment increases costs and workload.
When the bottom layer of varnish is wet, spray the subsequent paint film and reasonably set the coverage range of each layer of paint film, including expanding out of the repair position to form multiple polishing areas, spraying isolation varnish, metal paint or pearl paint layer by layer, and covering the light varnish and form a barbed area through an appropriate amount of barbed water to ensure a natural transition of the paint film.
The paint repair quality of metal surfaces and pearl paint surfaces has been significantly improved, and the color difference problem of metal paint repair "black circles" is solved, reducing the repair area, and reducing material costs and workload.
Smart Images

Figure CN119056719A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of surface treatment, in particular to a method for repairing automobile topcoat. Background Art
[0002] The information disclosed in this background technology section is only intended to enhance the understanding of the overall background of the invention, and should not necessarily be regarded as an admission or any form of suggestion that the information constitutes the prior art already known to a person skilled in the art.
[0003] The paint surface of a car includes putty layer, intermediate coating, topcoat and clear coat from inside to outside. During the assembly and operation of the car, it is inevitable that the paint surface will be damaged due to scratches and other reasons, which affects the appearance quality of the paint surface. Therefore, paint repair is required.
[0004] Metallic paint refers to a type of automotive topcoat that has fine metal particles added to the paint base. Fine aluminum particles are added to its paint base. When light hits the aluminum particles, it is reflected through the paint film by the aluminum particles, giving it a glittering effect. Similarly, pearl paint refers to a type of automotive topcoat that has fine mica flakes added to the paint base. Repairs to automotive topcoats made with metallic paint and mica paint are prone to problems such as color difference in the repairs. The repaired area is like a patch, which significantly affects the quality of the paint surface repair. Especially when metallic paint is used as the topcoat, the color difference problem of the repaired area is particularly serious, and often appears at the interface with the underlying dry film coating. Figure 3 The "black circle" shown. In order to ensure the quality of the repair, a large area of spraying is required, which increases the cost of repair materials and the workload. The color difference problem has always been a key problem restricting the quality of metal paint or mica paint repair. Summary of the invention
[0005] In view of the shortcomings of the prior art, the purpose of the present invention is to provide a method for repairing automobile topcoat, in which a subsequent paint film is sprayed while the underlying clear coat is wet, and the coverage range of each layer of paint film is reasonably set so that the paint film transition at the repair position is natural, thereby solving the problem of "black circle" color difference in metal paint repair.
[0006] In order to achieve the above object, the present invention is implemented through the following technical solutions:
[0007] The present invention provides a method for repairing automobile metal topcoat, comprising the following steps:
[0008] S1, after the intermediate coating at the repair position is repaired and leveled, rough grinding is performed within a range of 100 to 200 mm outside the repair position to form a level first grinding area, and fine grinding is performed within a range of 200 to 400 mm outside the repair position to form a second grinding area;
[0009] S2, spraying isolation varnish in the first polishing area to form a first topcoat layer, wherein the first topcoat layer covers the repair position;
[0010] S3, after the first topcoat layer is dry, spraying metallic paint or pearl paint to form a second topcoat layer, the second topcoat layer covers the repair position and is smaller than the first topcoat layer;
[0011] S4, spraying a finishing varnish after the second topcoat layer is dry to form a third topcoat layer, wherein the third topcoat layer covers the second topcoat layer and the first topcoat layer and is smaller than the second polishing area;
[0012] S5. Add 1 to 2 times the volume of bridging water to the clear coat, and spray it from the edge of the third topcoat layer outward, and then use pure bridging water to spray from the edge of the third topcoat layer outward to form a bridging area, which is smaller than the second polishing area.
[0013] Optionally, in S1, the rough grinding method is grinding with 600-800# sandpaper and a pneumatic grinder.
[0014] Optionally, in S1, the rough grinding method is hand grinding with 1200# wet sandpaper.
[0015] Optionally, in S1, the edge of the first polishing area is polished to a depth not exceeding the original vehicle finishing varnish layer.
[0016] Optionally, in S1, the fine grinding method is hand grinding with 2000-2500# wet sandpaper.
[0017] Optionally, in S1, the grinding depth of the fine grinding is to remove the coarse grinding marks, and the grinding depth of the edge is not more than the original vehicle top coat varnish layer.
[0018] Optionally, in S2, the isolation varnish uses 1K varnish, which is prepared in a volume ratio of 1K varnish to thinner of 1:(1-2); 1-2 thin coats are sprayed to form a first topcoat layer with tight coverage.
[0019] Optionally, in S2, the isolation varnish uses 2K varnish; 1 to 2 thin coats are sprayed to form a first topcoat layer with tight coverage.
[0020] Optionally, in S2, the edge of the first topcoat layer overlaps with the original automobile topcoat clear varnish.
[0021] Optionally, in S3, the second topcoat layer covers the exposed area of the intermediate coating at the repair point, and the edge of the second topcoat layer overlaps with the original automobile topcoat layer.
[0022] Optionally, in S4, the third topcoat is 2K clearcoat.
[0023] Optionally, the repair method further comprises step S6, baking, curing and polishing the joint area after the surface is dried.
[0024] The beneficial effects of the present invention are as follows:
[0025] In the repair method of the present invention, a thin layer of wet film isolation varnish is first sprayed on the defect, a moist base layer is formed in the repaired area, and the base varnish is colorless and does not affect the base color of the interface. By clarifying the construction scope of the first topcoat layer, the second topcoat layer, the third topcoat layer, the joint area, the first polishing area and the second polishing area, they are reasonably combined with the different paint films of the original automobile paint surface, which significantly improves the paint repair quality of the metal surface and the pearl paint surface, solves the color difference problem of the "black circle" in the metal paint repair, and significantly reduces the repair area, reducing the cost and workload of large-area spraying materials. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] The accompanying drawings in the specification, which constitute a part of the present invention, are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute improper limitations on the present invention.
[0027] Figure 1 Schematic diagram of the area of each repair area in Example 1.
[0028] Figure 2 Schematic diagram of the depth of each repair area in Example 1.
[0029] Figure 3 This is a physical picture of the “black circle” in the background technology.
[0030] Figure 4 This is a real picture of the paint surface repaired in Example 1.
[0031] Among them, 1. The first polishing area; 2. The second polishing area; 3. The first topcoat layer; 4. The second topcoat layer; 5. The third topcoat layer; 6. The joint area; 7. The repair position; 10. The intermediate coating; 11. The original vehicle topcoat layer; 12. The original vehicle clear coat layer. DETAILED DESCRIPTION
[0032] It should be noted that the following detailed descriptions are exemplary and are intended to provide further explanation of the present invention. Unless otherwise specified, all technical and scientific terms used herein have the same meanings as those commonly understood by those skilled in the art to which the present invention belongs.
[0033] Unless otherwise defined, all professional and scientific terms used herein have the same meanings as those familiar to those skilled in the art. The reagents or raw materials used in the present invention can be purchased through conventional channels. Unless otherwise specified, the reagents or raw materials used in the present invention are used in a conventional manner in the art or in accordance with the product instructions. In addition, any method and material similar to or equivalent to the described content can be applied to the method of the present invention. The preferred implementation methods and materials described in the text are for demonstration purposes only.
[0034] It should be noted that the terms used herein are only for describing specific embodiments and are not intended to limit exemplary embodiments according to the present invention. As used herein, unless the context clearly indicates otherwise, the singular form is also intended to include the plural form. In addition, it should be understood that when the terms "comprising" and / or "including" are used in this specification, it indicates the presence of features, steps, operations, devices, components and / or combinations thereof.
[0035] Example 1
[0036] When the metal paint of a car is damaged due to scratches or other reasons, it needs to be repaired. The preparation process includes: grinding the damaged paint surface to a depth that completely removes the damage marks. At this time, the grinding depth may reach the middle coating or even the putty layer. After the putty layer and the middle coating are smoothed to meet the requirements, the repair position is as follows: Figure 2 As shown, the surface of the intermediate coating 10 is flat after treatment, and the outer sides of the intermediate coating 10 are the exposed edges of the original vehicle topcoat layer 11 and the original vehicle topcoat varnish layer 12, which need to be treated with paint. The steps include:
[0037] S1. After the intermediate coating at the repair position 7 is repaired and leveled, Figure 1 As shown, within a range of 100 to 200 mm outside the repair position 7, coarse grinding is performed by using 600 to 800# sandpaper and a pneumatic grinder to form a flat first grinding area 1, thereby ensuring the quality of the bottom layer grinding treatment in the repair area; within a range of 200 to 400 mm outside the repair position 7, fine grinding is performed by hand grinding with 2000 to 2500# wet sandpaper to form a second grinding area 2, thereby ensuring the quality of the subsequent bottom layer grinding treatment in the joint area; the grinding depth of the edge of the first grinding area 1 is not more than the original vehicle finishing varnish layer 12, thereby achieving a transition in the glossiness of the paint surface in the later stage, and the grinding depth of the fine grinding is to remove the rough grinding marks, and the grinding depth of the edge is also not more than the original vehicle finishing varnish layer 12.
[0038] S2, the isolation varnish adopts 1K varnish (single-component varnish), and is prepared in a volume ratio of 1K varnish to thinner of 1: (1-2) (in this embodiment, the volume ratio of varnish to thinner measured after preparation is 1:1.5), such as Figure 1 As shown, spray the isolation varnish (thinly spray 1-2 times) in the first grinding area 1 to form a first topcoat layer 3, so that a layer of wet bottom is formed at the repair area 7, and the isolation varnish is colorless and does not affect the bottom color of the interface; the first topcoat layer 3 covers the repair position 7, and as shown Figure 2 As shown, the edge of the first topcoat layer 3 overlaps with the original automobile clearcoat layer 12, which better ensures the quality of the isolation clearcoat spraying and lays a good foundation for the metallic paint spraying.
[0039] S3, after the first topcoat layer 3 is dry, a metallic paint is sprayed to form a second topcoat layer 4, such as Figure 1 As shown, the second topcoat layer 4 covers the repair position 7 and is smaller than the first topcoat layer 3 to ensure that the repaired metal paint is isolated and does not directly contact the underlying dry film; the second topcoat layer 4 covers the exposed intermediate coating 10 area of the repair position 7, and as shown Figure 2 As shown, the edge of the second topcoat layer 4 overlaps with the original topcoat layer 11 of the automobile.
[0040] S4. After the second topcoat layer 4 is dry, a finishing varnish is sprayed to form a third topcoat layer 5. The third topcoat layer 5 covers the second topcoat layer 4 and is smaller than the second polishing area 2. The third topcoat layer 5 covers the metallic paint of the second topcoat layer 4 and the isolation varnish of the first topcoat layer 3, thereby truly isolating the metallic paint film at the repair position 7 and completing the repair of the repair position 7.
[0041] S5. Add 1 times the volume of bridging water to the clear coat, and spray it from the edge of the third topcoat layer 5 outward. Then use pure bridging water to spray from the edge of the third topcoat layer 5 outward to form a bridging area 6. The bridging area 6 is smaller than the second polishing area 2 to better ensure the repair quality of the bridging at the interface of the third topcoat layer 5.
[0042] S6, joint area 6 is baked, cured and polished after the surface is dry. The baking and curing temperature and time requirements are consistent with the original metal paint requirements of the car.
[0043] The actual photo of the paint surface after repair is as follows Figure 4 As shown, there is no chromatic aberration or "black circle" problem.
[0044] Example 2
[0045] When the paint surface of the automobile pearl paint needs to be repaired, the repair is performed according to the method of Example 1, except that:
[0046] In S1, the rough grinding method is hand grinding with 1200# wet sandpaper.
[0047] In S2, the isolation varnish adopts 2K varnish (two-component varnish), and a curing agent and a thinner are added according to the formulation requirements of the 2K varnish; 1 to 2 thin sprays are applied to form a first topcoat layer with tight coverage.
[0048] In S3, pearl paint is sprayed after the first topcoat is dry.
[0049] The operation mode and paint surface coverage requirements of other steps are consistent with those of Example 1.
[0050] By adopting the method of embodiment 1 and implementation 2, the scope of the repair area can be limited to the range of 200 to 400 mm (the second polishing area) extending outward from the repair position 7, while the scope of conventional large-area spraying treatment is usually within the entire segmented side or the entire vehicle. Therefore, by adopting the scheme of the present invention, the cost and workload of repair materials can be significantly reduced. Since the wet film edge of the repaired metallic paint is in contact with the dry film of the original vehicle finishing paint layer, the black circle problem at the interface of the edge of the repair paint is easily generated. The metallic paint wet film paint layer is isolated from the original vehicle varnish layer by the isolation varnish wet film layer, and the isolation varnish layer (first topcoat layer 3) wet film layer is in contact with the dry film layer of the original vehicle varnish layer and is transparent. There is no color difference problem between the transparent colors, which can avoid color difference and "black circle" problems and ensure the paint surface quality of the product.
[0051] The above description is only the preferred embodiment of the present application and is not intended to limit the present application. For those skilled in the art, the present application may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present application shall be included in the protection scope of the present application.
Claims
1. A method for repairing automobile topcoat, characterized in that the steps include: S1. After the intermediate coating of the repair point is repaired and leveled, the repair position is roughly ground within a range of 100 to 200 mm outside the repair position to form a flat first grinding area, and finely ground within a range of 200 to 400 mm outside the repair position to form a second grinding area; S2, spraying isolation varnish in the first polishing area to form a first topcoat layer, wherein the first topcoat layer covers the repair position; S3, after the first topcoat layer is dry, spray metallic paint or pearl paint to form a second topcoat layer, the second topcoat layer covers the repair point and is smaller than the first topcoat layer; S4, spraying a finishing varnish after the second topcoat layer is dry to form a third topcoat layer, wherein the third topcoat layer covers the second topcoat layer and the first topcoat layer and is smaller than the second polishing area; S5. Add 1 to 2 times the volume of bridging water to the clear coat, and spray it from the edge of the third topcoat layer outward, and then use pure bridging water to spray from the edge of the third topcoat layer outward to form a bridging area, which is smaller than the second polishing area.
2. The automobile topcoat repair method according to claim 1, characterized in that: In S1, the rough grinding method is grinding with 600-800# sandpaper and a pneumatic grinder; or, the rough grinding method is hand grinding with 1200-1600# wet sandpaper.
3. The automobile topcoat repair method according to claim 1, characterized in that: In S1, the fine grinding method is hand grinding with 2000-2500# wet sandpaper.
4. The automobile topcoat repair method according to claim 1, characterized in that: In S1, the edge of the first polishing area is polished to a depth that does not exceed the original vehicle finishing varnish layer.
5. The automobile topcoat repair method according to claim 1, characterized in that: In S1, the grinding depth of fine grinding is to remove the coarse grinding marks, and the grinding depth of the edge is not more than the original vehicle top coat of varnish.
6. The automobile topcoat repair method according to claim 1, characterized in that: In S2, the isolation varnish uses 1K varnish, which is prepared in a volume ratio of 1K varnish to thinner of 1: (1-2); 1-2 thin sprays are applied to form a first topcoat layer with tight coverage.
7. The automobile topcoat repair method according to claim 1, characterized in that: In S2, 2K varnish is used as the isolation varnish; 1 to 2 thin coats are sprayed to form a first topcoat layer with tight coverage.
8. The automobile topcoat repair method according to claim 1, characterized in that: In S2, the edge of the first topcoat layer overlaps with the original car topcoat clearcoat; In S3, the second topcoat layer covers the exposed area of the intermediate coating at the repair point, and the edge of the second topcoat layer overlaps with the original topcoat layer of the vehicle.
9. The automobile topcoat repair method according to claim 1, characterized in that: In S4, the third topcoat is 2K clearcoat.
10. The automobile topcoat repair method according to claim 1, characterized in that: The repair method also includes step S6, baking, curing and polishing the joint area after the surface is dried.
Citation Information
Patent Citations
Paint surface posthaste photo compensation method
CN101234378A
Workpiece coating repairing method
CN110238009A
Method for repairing automobile paint
CN114871075A
Method of repairing local damaged coating on metal surface
CN1608744A
Low-energy UV automotive refinishing paint, as well as method of application and use thereof
WO2017177674A1
Cited By
Spraying, leveling and repairing method for multi-layer functional coating, application of spraying, leveling and repairing method and repairing product