High-specific-heat-capacity phase change heat absorption medium and preparation method thereof
Through the combination of polymer water-absorbing resin and water, a high specific heat capacity phase change heat absorption medium is formed, which solves the problems of small specific heat capacity and low cost performance in the prior art, and achieves higher heat absorption and energy storage effects and wider application scenarios. At the same time, it reduces the cost and production difficulty.
Patent Information
- Application Number
- CN202411319665.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-20
- Publication Date
- 2024-12-03
AI Technical Summary
The existing phase change heat absorption media have a small specific heat capacity, a low phase change temperature and a high cost, resulting in a low cost performance in the field of special thermal protection.
High specific heat capacity phase change heat absorption medium is prepared by polymer water absorption resin and water, and the gel-like polymer is formed by absorbing water expansion of polymer water absorption resin, with a water content greater than 90%, and a mildew-proof agent and dispersant are added to improve specific heat capacity and stability. .
It significantly improves the specific heat capacity and phase change temperature of phase change heat absorption medium, avoids the growth of mold, reduces production cost and time, and provides a wider range of application scenarios and higher heat absorption and energy storage effects.
Smart Images

Figure CN119060697A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of phase change materials, and in particular to a high specific heat capacity phase change heat absorbing medium and a preparation method thereof. Background Art
[0002] Phase change heat absorbing medium (PCM) is used to absorb heat transferred from the outside, and begins to change phase when the accumulated heat reaches the phase change temperature. The medium changes from solid to liquid, solid to gas, or liquid to gas. After absorbing heat, the physical form changes, and the medium temperature remains unchanged. Specific heat and phase change physical changes are used to ensure that the surface temperature change of the object protected by the medium lags behind the external environment. Commonly used phase change heat absorbing media include inorganic PCM, organic PCM and composite PCM. Inorganic PCM mainly includes crystalline hydrated salts, molten salts, metals or alloys; organic PCM includes paraffin, acetic acid and other organic matter; composite phase change combines the advantages of both. All three types of PCM have the problems of small specific heat capacity, low phase change temperature, high cost, and low cost-effectiveness in the field of special thermal protection.
[0003] Therefore, it is necessary to provide a high specific heat capacity phase change heat absorbing medium and a preparation method thereof to solve the problems mentioned in the above background technology. Summary of the invention
[0004] To achieve the above object, the present invention provides the following technical solution: a phase-change heat-absorbing medium with high specific heat capacity, wherein the phase-change heat-absorbing medium comprises a polymer water-absorbing resin and water;
[0005] The phase-change heat-absorbing medium is a gel polymer obtained by swelling with a high molecular weight water-absorbing resin;
[0006] The water content of the phase-change heat-absorbing medium is greater than 90%.
[0007] Further, preferably, based on the mass of the phase-change heat absorbing medium, the amount of the polymer water-absorbing resin is 1 to 2% of the mass of the phase-change heat absorbing medium;
[0008] Preferably, the polymer water-absorbent resin powder has a water absorption multiple of not less than 300 times and a particle size of 100 to 120 meshes;
[0009] Further preferably, the polymer water-absorbing resin powder is selected from at least one of polyacrylic acids, polyvinyl alcohols, polyoxyalkylenes, hydroxymethylated starch and hydroxymethylated cellulose.
[0010] Furthermore, preferably, the raw material of the phase change heat absorbing medium also includes a mildew preventer and / or a dispersant;
[0011] The mildew preventer is selected from at least one of 1,2-benzisothiazolin-3-one and isothiazolinone;
[0012] The dispersant is selected from at least one of propylene glycol and glycerol.
[0013] Further, preferably, based on the mass of the phase change endothermic medium, the amount of the dispersant is 2.9% to 8% of the mass of the phase change endothermic medium, and the amount of the mildew inhibitor is 0.1% to 0.2% of the mass of the phase change endothermic medium.
[0014] Furthermore, preferably, the high specific heat capacity phase change heat absorbing medium comprises: 90-96 parts of pure water, 1-2 parts of polymer water-absorbing resin powder, 2.9-8 parts of dispersant, and 0.1-0.2 parts of mildewproofing agent.
[0015] Furthermore, preferably, the specific heat capacity of the phase-change heat absorbing medium is greater than 3.5 kJ / kg·°C.
[0016] A method for preparing a high specific heat capacity phase change heat absorbing medium comprises at least the following steps:
[0017] The polymer water-absorbing resin powder is placed in water to obtain a mixture, the mixture is stirred in the same direction until all the polymer water-absorbing resin powder absorbs water and swells, and the mixture is allowed to stand for reaction to obtain a high specific heat capacity phase change heat absorption medium.
[0018] Furthermore, preferably, the method further comprises:
[0019] The mixture also includes a dispersant and / or a preservative.
[0020] Further, preferably, the method comprises:
[0021] Step 1: adding polymer water-absorbing resin powder into the dispersant to obtain a suspension;
[0022] Step 2: adding the mildew inhibitor into the suspension and stirring to obtain a mixed solution;
[0023] Step 3: adding water to the mixed solution and stirring until all the polymer water-absorbent resin powder absorbs water and swells to obtain an intermediate;
[0024] Step 4: allowing the intermediate to react in a closed space to obtain a high specific heat capacity phase change heat absorbing medium.
[0025] Furthermore, preferably, the addition requirement of the mildew inhibitor is: adjusting the pH value of the mixed solution to 6-7.
[0026] Further, as a preferred embodiment, it is characterized in that when the polymer water-absorbing resin powder is mixed with water, the temperature of the water is 60°C ± 1°C;
[0027] The static reaction time is 20 to 60 minutes.
[0028] Compared with the prior art, the present invention provides a method for preparing a phase-change heat-absorbing medium with high specific heat capacity, which has the following beneficial effects:
[0029] 1. The phase change heat absorption medium of the present invention has a specific heat capacity 0.5 to 1 times greater than that of the PCM phase change heat absorption medium, a higher phase change temperature (greater than 100°C), better heat absorption and energy storage effect, and a wider range of application scenarios.
[0030] 2. Compared with the phase-change heat-absorbing material using pure water, the phase-change heat-absorbing medium of the present invention avoids the growth of mold, and at the same time, the polymer water-absorbing resin can be used to lock the moisture, which is not easy to evaporate and diffuse at normal temperature and pressure; at the same time, the dispersant (glycerol) is used to form a layer of water-locking and moisturizing film on the surface of the water polymer after water absorption, which further reduces the volatilization and diffusion of moisture.
[0031] 3. Compared with PCM phase-change heat-absorbing medium, the raw materials used in the phase-change heat-absorbing medium of the present invention are common chemical materials, which have a wide range of sources and low procurement costs. The preparation method of the phase-change heat-absorbing medium of the present invention is simple, the preparation time is short, no special production tools are required, the investment cost is low, and the cost performance is higher. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] Figure 1 The figure is a flow chart of manufacturing the high specific heat capacity phase change heat absorbing medium of the present invention; DETAILED DESCRIPTION
[0033] See also Figure 1 , the present invention provides a phase-change heat-absorbing medium with high specific heat capacity, the raw materials of which include a polymer water-absorbing resin and water;
[0034] The phase-change heat-absorbing medium is a gel polymer obtained by swelling with a high molecular weight water-absorbing resin;
[0035] The water content of the phase-change heat-absorbing medium is greater than 90%.
[0036] Specifically, the water is pure water (distilled water) and meets the third-level water standard specified in the national standard GB / T6682 for water used in analytical laboratories.
[0037] Furthermore, based on the mass of the phase-change heat-absorbing medium, the amount of the polymer water-absorbing resin is 1 to 2% of the mass of the phase-change heat-absorbing medium;
[0038] Preferably, the polymer water-absorbent resin powder has a water absorption multiple of not less than 300 times and a particle size of 100 to 120 meshes;
[0039] More preferably, the polymer water-absorbing resin powder is selected from at least one of polyacrylic acid, polyvinyl alcohol, polyoxyalkylene, hydroxymethylated starch and hydroxymethylated cellulose, preferably a single component or a mixed component of a polyacrylic acid salt polymer water-absorbing resin powder.
[0040] Preferably, the polymer water-absorbent resin powder does not dissolve at a temperature below 140°C. After absorbing water, the polymer water-absorbent resin powder generates a resin gel. The higher dissolution temperature allows the resin gel to use hydrophilic molecules to decompose internal water molecules and diffuse out at high temperatures, causing the internal structure to collapse and thermally crack, thereby achieving a phase change process of releasing water vapor. Among them, the polymer water-absorbent resin powder selects a higher melting temperature to ensure that the resin gel after absorbing water can still lock water at high temperatures, thereby increasing the high-temperature specific heat capacity.
[0041] Furthermore, the raw materials of the phase change heat absorbing medium also include a mildew preventer and / or a dispersant;
[0042] The mildew preventer is selected from at least one of 1,2-benzisothiazolin-3-one and isothiazolinone;
[0043] It needs to be explained that since the water absorption performance and water absorption rate of polymer resin are greatly affected by pH, it is necessary to add pH adjuster to increase the reaction speed of production. Polymer water-absorbing resin powder is organic matter, and it is inevitable to contact bacteria during the production process. After a long time, a large number of bacteria will breed and multiply. The breeding products will affect the pH of the solution, and the generated enzymes may cause the polymer water-absorbing resin to dissolve, which will affect the water polymer. Therefore, it is necessary to add antifungal agents to kill and inhibit bacterial reproduction and production.
[0044] Commonly used fungicides include 1,2-benzisothiazolin-3-one (BIT mildew preventer) and isothiazolinone (kasson). The pH value of BIT fungicides is greater than 8, which is weakly alkaline, and the pH value of kasson fungicides is less than 6, which is weakly acidic. Whether to use one or a mixture of the two depends on the pH value of the polymer water-absorbing resin powder and the pH value of the solution. The preferred polyacrylic acid salt polymer water-absorbing resin is a weakly acidic substance. It is recommended to use BIT fungicides to adjust the pH value of the mixed solution to obtain a better water absorption rate and water absorption amount.
[0045] Considering the solubility of the solution in pure water and the effect of locking water and moisturizing, the dispersant is selected from at least one of propylene glycol and glycerol (glycerin), and the amount of the dispersant is 3 to 5 times the mass of the polymer water-absorbing resin powder to ensure that the polymer water-absorbing resin powder is evenly dispersed. Among them, propylene glycol and glycerol (glycerin) are mostly used for locking water and moisturizing in cosmetics, with wide applications, low prices and high solubility.
[0046] Furthermore, based on the mass of the phase-change heat absorbing medium, the amount of the dispersant is 2.9% to 8% of the mass of the phase-change heat absorbing medium, and the amount of the mildew inhibitor is 0.1% to 0.2% of the mass of the phase-change heat absorbing medium.
[0047] Preferably, the high specific heat capacity phase change heat absorbing medium comprises, by mass, 90 to 96 parts of pure water, 1 to 2 parts of polymer water-absorbing resin powder, 2.9 to 8 parts of dispersant, and 0.1 to 0.2 parts of mildewproofing agent.
[0048] Furthermore, the specific heat capacity of the phase-change heat absorbing medium is greater than 3.5 kJ / kg·°C.
[0049] Among them, the high specific heat capacity of the high specific heat capacity phase change heat absorption medium is achieved by relying on the high mass proportion of water in the water polymer. The higher the content of the polymer water-absorbing resin, the greater the volume change of the obtained phase change heat absorption medium, and the lower the specific heat capacity. The preferred water content is greater than 90%, and the specific heat capacity of the obtained phase change heat absorption medium is greater than 3.5kJ / kg·℃. The volume of the obtained heat absorption medium and the volume of the solution will not be significantly different, and the low-temperature expansion rate is similar to that of water. The temperature characteristics of water should be referred to when using it.
[0050] A method for preparing a high specific heat capacity phase change heat absorbing medium comprises at least the following steps:
[0051] The polymer water-absorbing resin powder is placed in water to obtain a mixture, the mixture is stirred in the same direction until all the polymer water-absorbing resin powder absorbs water and swells, and the mixture is allowed to stand for reaction to obtain a high specific heat capacity phase change heat absorption medium.
[0052] Furthermore, the mixture also includes a dispersant and / or a preservative.
[0053] Furthermore, the method comprises:
[0054] Step 1: adding polymer water-absorbing resin powder into the dispersant to obtain a suspension;
[0055] Step 2: adding the mildew inhibitor into the suspension and stirring to obtain a mixed solution;
[0056] Step 3: adding water to the mixed solution and stirring until all the polymer water-absorbent resin powder absorbs water and swells to obtain an intermediate;
[0057] Step 4: allowing the intermediate to react in a closed space to obtain a high specific heat capacity phase change heat absorbing medium.
[0058] Furthermore, the requirement for adding the mildew inhibitor is: adjusting the pH value of the mixed solution to 6-7.
[0059] It should be explained that a single polymer water-absorbent resin powder can obtain a phase-change heat-absorbing medium in pure water, but the polymer water-absorbent resin powder has different appearances under different acid-base conditions. In an acidic environment, the polymer water-absorbent resin powder is more likely to swell, and the water absorption rate and water absorption amount will increase, while under alkaline conditions, it is completely the opposite. When the polymer water-absorbent resin powder is in a neutral environment, the water absorption rate and water absorption amount are usually in the best state. At the same time, the chemical stability of the polymer water-absorbent resin powder will also change under different acid-base conditions. Specifically, in an acidic environment, the stability of the polymer water-absorbent resin powder will decrease, and in an alkaline environment, it will increase. The specific acidity and alkalinity should be selected according to the use environment and the pH value of the polymer water-absorbent resin powder. The water polymer formed by the polymer water-absorbent resin powder when it meets water may adhere to each other, affecting the water absorption rate and water absorption effect. Therefore, the polymer water-absorbent resin powder should be avoided from agglomerating during use, and a dispersant should be used to make the polymer water-absorbent resin powder evenly distributed in the solution to prevent the gel adhesion after water absorption from affecting the use effect.
[0060] Specifically, by adding a mildew preventer to the polymer water-absorbent resin powder and adjusting the pH value of the solution to 6-7 using the mildew preventer, the polymer water-absorbent resin powder can obtain a faster water absorption rate under a suitable pH environment. At the same time, the mildew preventer can make the obtained high specific heat capacity phase change heat absorption medium have an anti-mildew effect, thereby improving its use stability; and by adding a dispersant to the polymer water-absorbent resin powder, the polymer water-absorbent powder is evenly distributed in the solution, preventing the gel (high specific heat capacity phase change heat absorption medium) after water absorption from sticking and affecting the use effect, and at the same time, improving the anti-volatilization and water retention capacity of the phase change heat absorption medium.
[0061] Furthermore, when the polymer water-absorbing resin powder is mixed with water, the temperature of the water is 60°C±1°C, which increases the solubility of the bactericide and dispersant in pure water; and the static reaction time is 20 to 60 minutes.
[0062] It should be explained that, in addition to having a large number of hydrophilic groups that form hydrogen bonds with water molecules to produce adsorption, the cross-linked polymer structure of the resin can also enhance the adsorption of water molecules. At the same time, during the water absorption process, the high ion concentration inside the resin will balance the internal and external osmotic pressures under the penetration of water molecules. In this process, water molecules will also be adsorbed into the resin grid to form a gel-like water polymer. The holes and gaps inside the resin can also absorb some water molecules. The above water absorption mechanism requires a certain amount of time to reach a state equilibrium to ensure that the resulting heat absorption medium has stable characteristics. The standing time can be adjusted according to actual needs (specifically refer to the ultraviolet irradiation method to accelerate the water absorption and stability of polyacrylates).
[0063] What is described above is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.
Claims
1. A high specific heat capacity phase change heat absorbing medium, characterized in that: The raw materials of the phase-change heat-absorbing medium include polymer water-absorbing resin and water; The phase-change heat-absorbing medium is a gel polymer obtained by swelling with a high molecular weight water-absorbing resin; The water content of the phase-change heat-absorbing medium is greater than 90%.
2. A high specific heat capacity phase change heat absorbing medium according to claim 1, characterized in that: Based on the mass of the phase-change heat-absorbing medium, the amount of the polymer water-absorbing resin is 1 to 2% of the mass of the phase-change heat-absorbing medium; Preferably, the polymer water-absorbent resin powder has a water absorption multiple of not less than 300 times and a particle size of 100 to 120 meshes; Further preferably, the polymer water-absorbing resin powder is selected from at least one of polyacrylic acids, polyvinyl alcohols, polyoxyalkylenes, hydroxymethylated starch and hydroxymethylated cellulose.
3. The high specific heat capacity phase change heat absorbing medium according to claim 1, characterized in that: The raw materials of the phase change heat absorbing medium also include mildew inhibitor and / or dispersant; The mildew preventer is selected from at least one of 1,2-benzisothiazolin-3-one and isothiazolinone; The dispersant is selected from at least one of propylene glycol and glycerol.
4. The high specific heat capacity phase change heat absorbing medium according to claim 1, characterized in that: Based on the mass of the phase-change heat absorbing medium, the amount of the dispersant is 2.9% to 8% of the mass of the phase-change heat absorbing medium, and the amount of the mildew inhibitor is 0.1% to 0.2% of the mass of the phase-change heat absorbing medium.
5. The high specific heat capacity phase change heat absorbing medium according to claim 1, characterized in that: The specific heat capacity of the phase-change heat absorbing medium is greater than 3.5 kJ / kg·°C.
6. A method for preparing a phase-change heat-absorbing medium with high specific heat capacity, characterized in that: The method comprises at least the following steps: The polymer water-absorbent resin powder is placed in water to obtain a mixture, the mixture is stirred in the same direction until all the polymer water-absorbent resin powder absorbs water and swells, and the mixture is allowed to stand for reaction to obtain a high specific heat capacity phase change heat absorption medium.
7. The method for preparing a phase-change heat absorbing medium with high specific heat capacity according to claim 6, characterized in that: The method further comprises: The mixture also includes a dispersant and / or a preservative.
8. The method for preparing a phase-change heat absorbing medium with high specific heat capacity according to claim 7, characterized in that: The method comprises: Step 1: adding polymer water-absorbing resin powder into the dispersant to obtain a suspension; Step 2: adding the mildew inhibitor into the suspension and stirring to obtain a mixed solution; Step 3: adding water to the mixed solution and stirring until all the polymer water-absorbent resin powder absorbs water and swells to obtain an intermediate; Step 4: allowing the intermediate to react in a closed space to obtain a high specific heat capacity phase change heat absorbing medium.
9. The method for preparing a phase-change heat absorbing medium with high specific heat capacity according to claim 8, characterized in that: The requirement for adding the mildew inhibitor is: adjusting the pH value of the mixed solution to 6-7.
10. A method for preparing a phase-change heat absorbing medium with high specific heat capacity according to any one of claims 6 to 8, characterized in that: When the polymer water-absorbing resin powder is mixed with water, the temperature of the water is 60°C ± 1°C; The static reaction time is 20 to 60 minutes.