Fluidized bed material temperature control method and system
By real-time monitoring and analysis of the temperature data of graphite electrode materials in the fluidized bed, determining the drying stage and adjusting the coal burning volume and wind speed, the difficulty in temperature control caused by abnormal particle size and moisture content is solved, and the complete drying of graphite electrode materials is achieved .
Patent Information
- Application Number
- CN202411578810.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-11-07
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2044-11-07
AI Technical Summary
When drying graphite electrode materials in a fluidized bed, abnormal particle size or abnormal moisture content leads to difficulty in temperature control and cannot ensure that the moisture is completely dry.
By obtaining temperature data in real time, determine the preheating, constant speed and speed reduction stages during the drying process, judge the abnormal temperature data, obtain the degree of abnormal particles and moisture, and adjust the coal burning volume and wind speed to control the temperature.
Accurate temperature regulation of graphite electrode materials is achieved, ensuring complete drying of moisture and improving drying efficiency.
Smart Images

Figure CN119063438A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of solid drying, and in particular to a fluidized bed material temperature control method and system. Background Art
[0002] Fluidized bed is an important chemical equipment, which can be used for drying, catalytic reaction and combustion. In the manufacturing process of batteries, graphite electrode materials need to be dried to ensure that the moisture in the graphite electrode materials is fully volatilized. Fluidized bed can efficiently dry the moisture in graphite electrode materials. Therefore, in the existing method, the graphite electrode materials for manufacturing batteries are dried by fluidized bed.
[0003] In the existing method, during the drying process of the graphite electrode material through the fluidized bed, the temperature data of the graphite electrode material in the fluidized bed can be obtained in real time, and then the temperature data of the graphite electrode material can be adjusted in time to completely dry the water in the graphite electrode material. However, in actual situations, abnormal particle size or abnormal water content of the graphite electrode material will cause abnormal temperature of the graphite electrode material in the fluidized bed, which will lead to the inability to timely and accurately adjust the temperature data of the graphite electrode material, and it is impossible to ensure that the water in the graphite electrode material is completely dried. Summary of the invention
[0004] In order to solve the technical problem that the temperature of the graphite electrode material in the fluidized bed is abnormal due to the abnormal particle size or abnormal moisture content of the graphite electrode material, which makes it impossible to timely and accurately adjust the temperature data of the graphite electrode material, making it impossible to ensure that the moisture in the graphite electrode material is completely dried, the purpose of the present invention is to provide a fluidized bed material temperature control method and system, and the technical scheme adopted is as follows: In a first aspect, an embodiment of the present invention provides a method for controlling the temperature of a fluidized bed material, the method comprising the following steps: Obtain the temperature data of graphite electrode materials at each moment during the fluidized bed drying process; According to the change of temperature data, determine the preheating drying stage, constant speed drying stage and speed reduction drying stage in the drying process; According to the difference of temperature data at adjacent moments in the preheating and drying stage, determine whether the temperature data is abnormal; When it is determined that the temperature data is abnormal, the degree of abnormality of the particles of the graphite electrode material in the preheating and drying stage is obtained according to the duration of the preheating and drying stage; the first degree of abnormality of the moisture content of the graphite electrode material in the constant-speed drying stage is obtained according to the duration of the constant-speed drying stage; the second degree of abnormality of the moisture content of the graphite electrode material in the speed-decreasing drying stage is obtained according to the difference in the temperature data at adjacent moments in the speed-decreasing drying stage; According to the abnormal degree of particles, the first abnormal degree of moisture and the second abnormal degree of moisture, the temperature of the graphite electrode material is controlled by adjusting the amount of coal burned and the wind speed of the fluidized bed.
[0005] Furthermore, the method for determining the preheating drying stage, the constant speed drying stage and the speed reduction drying stage in the drying process according to the change of the temperature data is: When the temperature data first appears to be greater than or equal to the standard temperature data of water evaporation of the graphite electrode material, the time corresponding to the corresponding temperature data is taken as the first target time; The time period formed by the initial time and the first target time is used as the preheating and drying stage; When the temperature data first appears and the difference between it and the standard temperature data of water evaporation of the graphite electrode material is greater than the predicted temperature difference threshold, and the difference between the temperature data at the next adjacent moment to the moment corresponding to the corresponding temperature data and the standard temperature data of water evaporation of the graphite electrode material is also greater than the predicted temperature difference threshold, the moment corresponding to the corresponding temperature data is taken as the second target moment; The time period formed by the first target time and the second target time is used as a constant-speed drying stage; The time period formed by the second target time and the current time is used as the speed reduction drying stage.
[0006] Furthermore, the method for determining whether the temperature data is abnormal is: Obtain the difference between the temperature data of each moment and the previous adjacent moment in the preheating and drying stage as the first difference of the corresponding moment; Acquire the number of first differences greater than a preset first difference threshold value in the preheating and drying stage as the first number; When the first number is greater than a preset first number threshold, it is determined that the temperature data is abnormal; When the first number is less than or equal to a preset first number threshold, it is determined that there is no abnormality in the temperature data.
[0007] Furthermore, the method for obtaining the degree of particle abnormality is: The result of normalizing the difference between the duration of the preheating drying stage and the standard preset drying duration is taken as the particle abnormality degree value.
[0008] Furthermore, the method for obtaining the first moisture abnormality degree is: The result of normalizing the difference between the duration of the constant-speed drying stage and the standard constant-speed drying duration is used as the first moisture abnormality degree value.
[0009] Furthermore, the method for obtaining the second moisture abnormality degree is: Obtaining the first difference at each moment in the speed-down drying stage, and taking the number of first differences greater than a preset second difference threshold in the speed-down drying stage as the second number; The ratio of the second quantity to the total quantity of all first differences in the speed-down drying stage is used as the second moisture abnormality degree value.
[0010] Furthermore, the method for controlling the temperature of the graphite electrode material by adjusting the amount of coal burned and the wind speed of the fluidized bed according to the particle abnormality, the first moisture abnormality and the second moisture abnormality is: Obtain an abnormality judgment value according to the particle abnormality value, the first moisture abnormality value, and the second moisture abnormality value; wherein the particle abnormality value is negatively correlated with the abnormality judgment value, and the first moisture abnormality value and the second moisture abnormality value are both positively correlated with the abnormality judgment value; When the abnormal situation judgment value is greater than or equal to the preset abnormal situation judgment threshold, the wind speed of the fluidized bed is kept unchanged; when the temperature data at the current moment is greater than the preset standard temperature data, the coal burning amount of the fluidized bed is reduced according to the first preset step length until the temperature data is less than or equal to the preset standard temperature data, and the coal burning amount is stopped; when the temperature data at the current moment is less than the preset standard temperature data, the coal burning amount of the fluidized bed is increased according to the first preset step length until the temperature data is greater than or equal to the preset standard temperature data, and the coal burning amount is stopped; when the temperature data at the current moment is equal to the preset standard temperature data, the coal burning amount is not adjusted; When the abnormal situation judgment value is less than the preset abnormal situation judgment threshold, the coal burning amount of the fluidized bed is kept unchanged; when the temperature data at the current moment is greater than the preset standard temperature data, the wind speed of the fluidized bed is increased according to the second preset step length until the temperature data is less than or equal to the preset standard temperature data, and the wind speed is stopped from being increased; when the temperature data at the current moment is less than the preset standard temperature data, the wind speed of the fluidized bed is reduced according to the second preset step length until the temperature data is less than or equal to the preset standard temperature data, and the wind speed is stopped from being reduced; when the temperature data at the current moment is equal to the preset standard temperature data, the wind speed is not adjusted.
[0011] Furthermore, the first preset step size is set to 1 kilogram; and the second preset step size is set to 0.1 meters per second.
[0012] Furthermore, the fluidized bed material temperature control method further comprises: When it is determined that there is no abnormality in the temperature data, the temperature of the graphite electrode material is not adjusted.
[0013] In a second aspect, another embodiment of the present invention provides a fluidized bed material temperature control system, the system comprising: a memory, a processor, and a computer program stored in the memory and executable on the processor, and when the processor executes the computer program, the steps of any one of the above methods are implemented.
[0014] The present invention has the following beneficial effects: The present invention first determines the preheating drying stage, the constant speed drying stage and the speed reduction drying stage in the drying process according to the change of temperature data, which is conducive to the subsequent accurate analysis of whether the temperature data is abnormal and the cause of the abnormal temperature data; then, according to the difference of temperature data at adjacent moments in the preheating drying stage, it is accurately judged whether the temperature data is abnormal, and the efficiency of drying the graphite electrode material is improved; when it is judged that the temperature data is abnormal, first, according to the length of the preheating drying stage, the degree of abnormality of the particles of the graphite electrode material in the preheating drying stage is obtained, and the abnormality of the particle size of the graphite electrode material in the preheating drying stage is accurately reflected; then, according to the length of the constant speed drying stage, the constant speed drying stage is obtained. The first moisture abnormality of the graphite electrode material in the drying stage accurately reflects the abnormality of the moisture content of the graphite electrode material in the constant speed drying stage; finally, according to the difference in temperature data at adjacent moments in the speed-decreasing drying stage, the second moisture abnormality of the graphite electrode material in the speed-decreasing drying stage is obtained, accurately reflecting the abnormality of the moisture content of the graphite electrode material in the speed-decreasing drying stage; further, according to the particle abnormality, the first moisture abnormality and the second moisture abnormality, the cause of the abnormal temperature data is accurately determined, and then corresponding measures are taken to adjust the coal burning amount and wind speed of the fluidized bed to reasonably control the temperature of the graphite electrode material, so that the moisture in the graphite electrode material is completely dried accurately and efficiently. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] In order to more clearly illustrate the technical solutions and advantages in the embodiments of the present invention or the prior art, the drawings required for use in the embodiments or the prior art descriptions are briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0016] Figure 1 A schematic flow chart of a method for controlling the temperature of a fluidized bed material provided by an embodiment of the present invention; Figure 2 A flow chart of a method for controlling the temperature of a graphite electrode material by adjusting the amount of coal burned and the wind speed of a fluidized bed provided by an embodiment of the present invention; Figure 3A structural diagram of a fluidized bed material temperature control system provided by one embodiment of the present invention; Figure 4 A schematic diagram of a computer device provided by an embodiment of the present invention. DETAILED DESCRIPTION
[0017] In order to further explain the technical means and effects adopted by the present invention to achieve the predetermined invention purpose, the following is a detailed description of a fluidized bed material temperature control method and system proposed by the present invention, its specific implementation method, structure, characteristics and effects, in combination with the accompanying drawings and preferred embodiments. In the following description, different "one embodiment" or "another embodiment" does not necessarily refer to the same embodiment. In addition, specific features, structures or characteristics in one or more embodiments may be combined in any suitable form.
[0018] Unless defined otherwise, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this invention belongs.
[0019] The specific scheme of a fluidized bed material temperature control method and system provided by the present invention is described in detail below with reference to the accompanying drawings.
[0020] Embodiment 1: The specific scenario of this embodiment is as follows: when the graphite electrode material starts to be dried, the temperature data of the graphite electrode material at each moment in the fluidized bed drying process is obtained in real time in this embodiment, and then the preheating drying stage, the constant speed drying stage and the speed reduction drying stage in the drying process of the graphite electrode material are determined. By analyzing the change of the temperature data in the preheating drying stage, it is determined whether the temperature data is abnormal. When it is determined that the temperature data is abnormal, the possible reasons for the abnormal temperature data in the preheating drying stage, the constant speed drying stage and the speed reduction drying stage are analyzed. Because the cause of the temperature abnormality is continuous, each drying stage in the drying process is analyzed; and then the particle abnormality degree of the graphite electrode material in the preheating drying stage, the first moisture abnormality degree of the graphite electrode material in the constant speed drying stage and the second moisture abnormality degree of the graphite electrode material in the speed reduction drying stage are obtained, and the reasons that may cause the temperature data abnormality in each stage of the drying process are determined. Then, according to the particle abnormality degree, the first moisture abnormality degree and the second moisture abnormality degree, the reason for the temperature abnormality of the graphite electrode material in the fluidized bed drying process is determined, and then corresponding measures are taken to regulate the temperature in the fluidized bed so that the moisture in the graphite electrode material is fully volatilized. It should be noted that, in this embodiment, the temperature data of the graphite electrode material is regulated in real time after the speed reduction drying stage occurs.
[0021] The present invention proposes a fluidized bed material temperature control method, please refer to Figure 1, which shows a schematic flow chart of a fluidized bed material temperature control method provided by an embodiment of the present invention, the method comprising the following steps: Step S1: Obtaining temperature data of the graphite electrode material at each moment during the fluidized bed drying process.
[0022] Specifically, in order to fully dry the water in the graphite electrode material through the fluidized bed, it is necessary to obtain the temperature data of the graphite electrode material at each moment during the fluidized bed drying process, so as to timely control the temperature data of the graphite electrode material so that the water in the graphite electrode material can be fully volatilized. In this embodiment, the temperature data of the graphite electrode material at the center point of the bed cross section in the fluidized bed at each moment during the fluidized bed drying process is obtained by a temperature sensor as the temperature data of the graphite electrode material at each moment during the fluidized bed drying process. In this embodiment, the time interval between two adjacent moments of collecting temperature data is set to 1 second. The implementer can set the time interval between two adjacent moments of collecting temperature data according to actual conditions, which is not limited here.
[0023] Step S2: determining the preheating drying stage, the constant speed drying stage and the speed reduction drying stage in the drying process according to the change of the temperature data.
[0024] Specifically, the temperature change trend of the graphite electrode material in the fluidized bed during the drying process is divided into three stages, namely the preheating and drying stage, the constant speed drying stage and the speed reduction drying stage. Among them, in the preheating and drying stage, the temperature data of the graphite electrode material increases and changes most significantly, while the moisture content in the graphite electrode material does not change much. The heat generated by the coal burned in the fluidized bed is mainly used to preheat the graphite electrode material until the temperature data of the graphite electrode material increases to the standard temperature data of the graphite electrode material moisture evaporation. The moisture in the graphite electrode material begins to evaporate, and at the same time, the temperature data of the graphite electrode material begins to tend to the standard temperature data of the graphite electrode material moisture evaporation. The preheating and drying stage ends and enters the constant speed drying stage. In the constant speed drying stage, the temperature data of the graphite electrode material is dominated by the influence of moisture. Among them, the change of the temperature data of the graphite electrode material affected by the moisture content is mainly manifested in maintaining within the local range of the standard temperature data of the graphite electrode material moisture evaporation, and will not increase significantly. Therefore, when the difference between the temperature data of the graphite electrode material and the standard temperature data of the graphite electrode material moisture evaporation reaches a certain degree, the constant speed drying stage ends and enters the speed reduction drying stage. Therefore, this embodiment determines the preheating drying stage, the constant speed drying stage and the speed reduction drying stage in the drying process according to the change of the temperature data.
[0025] Preferably, in a manner that can be implemented in this embodiment, the method for determining the preheating drying stage, the constant speed drying stage and the speed reduction drying stage in the drying process is: when the temperature data first appears to be greater than or equal to the standard temperature data of water evaporation of the graphite electrode material, it indicates that the preheating drying stage is over and the constant speed drying stage begins. Then, this embodiment uses the time corresponding to the corresponding temperature data as the first target time, and then uses the time period formed by the initial time and the first target time as the preheating drying stage; wherein the initial time is the time when the temperature data of the graphite electrode material is first obtained; When the difference between the temperature data and the standard temperature data of the water evaporation of the graphite electrode material is smaller, the graphite electrode material is more likely to be in the constant speed drying stage; when the difference between the temperature data and the standard temperature data of the water evaporation of the graphite electrode material is larger, the graphite electrode material is more likely to be in the speed reduction drying stage, and then the predicted temperature difference threshold is set to 5 degrees Celsius in this embodiment. When the temperature data first appears to have a difference with the standard temperature data of the water evaporation of the graphite electrode material greater than the predicted temperature difference threshold, it indicates that the constant speed drying stage is over; but considering that the temperature data has slight fluctuations, in order to avoid the time corresponding to the temperature data that is accidentally or abnormally greater than the standard temperature data of the water evaporation of the graphite electrode material being mistaken as the end time of the constant speed drying stage, therefore, in this embodiment, when the temperature data first appears to have a difference with the standard temperature data of the water evaporation of the graphite electrode material greater than the predicted temperature difference threshold, and the difference between the temperature data at the next adjacent time corresponding to the time corresponding to the corresponding temperature data and the standard temperature data of the water evaporation of the graphite electrode material is also greater than the predicted temperature difference threshold, the time corresponding to the corresponding temperature data is taken as the second target time, that is, the end time of the constant speed drying stage, and then the time period formed by the first target time and the second target time is taken as the constant speed drying stage; Finally, the time period formed by the second target moment and the current moment is used as the speed-down drying stage. After entering the speed-down drying stage, this embodiment begins to regulate the temperature data of the graphite electrode material in real time to ensure that the moisture in the graphite electrode material is fully volatilized.
[0026] It should be noted that the temperature data at the time moments commonly included in two adjacent drying stages are divided into the drying stage that is located later in the drying process. For example, if the end moment of the preheating drying stage and the start moment of the constant-speed drying stage are the same moment, the temperature data at the end moment of the preheating drying stage is deleted, and the temperature data at the start moment of the constant-speed drying stage is retained.
[0027] Step S3: judging whether the temperature data is abnormal according to the difference between the temperature data at adjacent moments in the preheating and drying stage.
[0028] Specifically, when the graphite electrode material is dried by a fluidized bed, the temperature data of the graphite electrode material will change abnormally due to the abnormality of the graphite electrode material itself, wherein the abnormality of the graphite electrode material itself includes two situations: abnormal particle size of the graphite electrode material and abnormal moisture content. Because the drying of the graphite electrode material is a continuous process, if the temperature data in the preheating and drying stage is abnormal, then each subsequent stage of the drying process may have temperature abnormalities. It is known that the purpose of the preheating and drying stage is to preheat the graphite electrode material. Under normal circumstances, the temperature data of the graphite electrode material in the preheating and drying stage varies within a slight fluctuation range. In order to analyze whether the temperature data is abnormal, this embodiment determines whether the temperature data is abnormal based on the difference in temperature data at adjacent moments in the preheating and drying stage.
[0029] Preferably, in a method that can be implemented in this embodiment, the method for determining whether the temperature data is abnormal is: obtaining the absolute value of the difference between the temperature data of each moment in the preheating and drying stage and the previous adjacent moment as the first difference of the corresponding moment; it should be noted that there is no previous adjacent moment at the initial moment of the preheating and drying stage, so the first difference at the initial moment of the preheating and drying stage is not obtained. When the first difference is larger and the number of large first differences is larger, it means that the temperature data of the graphite electrode material in the preheating and drying stage is more likely to be abnormal, which indirectly indicates that the graphite electrode material itself is more likely to be abnormal, and then the temperature data of the graphite electrode material in the entire drying process is more likely to be abnormal. In this embodiment, the preset first difference threshold is set to 10 degrees Celsius. The implementer can set the size of the preset first difference threshold according to the actual situation, which is not limited here. The number of first differences greater than the preset first difference threshold in the preheating and drying stage is obtained as the first number; when the first number is larger, it means that the temperature data of the graphite electrode material in the preheating and drying stage is more likely to be abnormal. In this embodiment, the preset first number threshold is set to 3. The implementer can set the size of the preset first number threshold according to the actual situation, which is not limited here. When the first number is greater than the preset first number threshold, it is judged that the temperature data is abnormal, and the temperature data of the graphite electrode material is further analyzed to determine the cause of the abnormality of the graphite electrode material itself, so that corresponding measures can be taken subsequently to regulate the temperature data of the graphite electrode material to improve the efficiency and integrity of the graphite electrode material in fully volatilizing water; when the first number is less than or equal to the preset first number threshold, it is judged that the temperature data is not abnormal, and the temperature data of the graphite electrode material is not regulated.
[0030] Step S4: When it is determined that the temperature data is abnormal, the degree of particle abnormality of the graphite electrode material in the preheating and drying stage is obtained according to the duration of the preheating and drying stage; the first degree of moisture abnormality of the graphite electrode material in the constant speed drying stage is obtained according to the duration of the constant speed drying stage; and the second degree of moisture abnormality of the graphite electrode material in the speed reduction drying stage is obtained according to the difference in temperature data at adjacent moments in the speed reduction drying stage.
[0031] Specifically, when it is determined that the temperature data is abnormal, the duration of the preheating and drying stage and the constant-speed drying stage is analyzed. Under normal circumstances, the duration of the preheating and drying stage and the constant-speed drying stage of the graphite electrode material are fixed, that is, the preheating and drying stage corresponds to a standard preset drying time, and the constant-speed drying stage corresponds to a standard constant-speed drying time. The greater the difference between the obtained duration of the preheating and drying stage and the standard preset drying time, the greater the possibility that the particle size of the graphite electrode material is abnormal; the greater the difference between the obtained duration of the constant-speed drying stage and the standard constant-speed drying time, the more abnormal the moisture content of the graphite electrode material. In the deceleration drying stage, the surface of the graphite electrode material gradually dries up, and the temperature data of the graphite electrode material increases with the increase of drying time. Under normal circumstances, the difference in temperature data at two adjacent moments fluctuates within a specified range. If the moisture content of the graphite electrode material is abnormal, the difference in temperature data at adjacent moments of the graphite electrode material will exceed the specified range. Furthermore, this embodiment obtains the degree of particle abnormality of the graphite electrode material in the preheating and drying stage according to the duration of the preheating and drying stage; obtains the first degree of moisture abnormality of the graphite electrode material in the constant rate drying stage according to the duration of the constant rate drying stage; and obtains the second degree of moisture abnormality of the graphite electrode material in the speed reduction drying stage according to the difference in temperature data between each moment in the speed reduction drying stage and its adjacent moments.
[0032] Preferably, in a method that can be implemented in this embodiment, the method for obtaining the degree of particle abnormality is: the result of normalizing the absolute value of the difference between the duration of the preheating and drying stage and the standard preset drying time is used as the value of the degree of particle abnormality. Among them, this embodiment normalizes the absolute value of the difference between the duration of the preheating and drying stage and the standard preset drying time by the norm normalization function. The larger the value of the degree of particle abnormality, the more abnormal the particle size of the graphite electrode material.
[0033] Preferably, in a method that can be implemented in this embodiment, the method for obtaining the first moisture abnormality degree is: the result of normalizing the absolute value of the difference between the duration of the constant speed drying stage and the standard constant speed drying duration is used as the first moisture abnormality degree value. Among them, this embodiment normalizes the absolute value of the difference between the duration of the constant speed drying stage and the standard constant speed drying duration by the norm normalization function. The larger the first moisture abnormality degree value, the more abnormal the moisture content of the graphite electrode material.
[0034] Preferably, in a method that can be implemented in this embodiment, the method for obtaining the second moisture abnormality is: obtaining the first difference at each moment in the deceleration drying stage. In this embodiment, the preset second difference threshold is set to 5 degrees Celsius. The implementer can set the size of the preset second difference threshold according to the actual situation, which is not limited here. The number of first differences greater than the preset second difference threshold in the deceleration drying stage is obtained as the second number; the larger the second number, the more abnormal the moisture content of the graphite electrode material. In order to determine the abnormal moisture content of the graphite electrode material reflected in the deceleration drying stage, the ratio of the second number to the total number of all first differences in the deceleration drying stage is used as the second moisture abnormality value. The larger the second moisture abnormality value, the more abnormal the moisture content of the graphite electrode material. It should be noted that in order to better observe the abnormal moisture content of the graphite electrode material in the deceleration drying stage, this embodiment starts to obtain the second moisture abnormality value after 30 seconds in the deceleration drying stage, and at the same time, the temperature data of the graphite electrode material is adjusted in real time after 30 seconds in the deceleration drying stage.
[0035] Step S5: According to the abnormal degree of particles, the first abnormal degree of moisture and the second abnormal degree of moisture, the amount of coal burned and the wind speed of the fluidized bed are adjusted to control the temperature of the graphite electrode material.
[0036] Specifically, the greater the degree of particle abnormality in the preheating and drying stage, it indirectly indicates that the degree of moisture abnormality of the graphite electrode material in the preheating and drying stage is smaller; the greater the first degree of moisture abnormality in the constant speed drying stage and the second degree of moisture abnormality in the speed reduction drying stage, it indirectly indicates that the degree of moisture abnormality of the graphite electrode material in the constant speed drying stage and the speed reduction drying stage is greater; therefore, this embodiment determines the cause of the abnormality in the temperature data of the graphite electrode material according to the degree of particle abnormality, the first degree of moisture abnormality and the second degree of moisture abnormality, and then adjusts the coal burning amount and wind speed of the fluidized bed according to the cause of the abnormality in the temperature data to control the temperature of the graphite electrode material.
[0037] Preferably, in one possible implementation of this embodiment, the method for adjusting the amount of coal burned and the wind speed of the fluidized bed to control the temperature of the graphite electrode material can be found in Figure 2 , which shows a flow chart of a method provided in this embodiment for adjusting the amount of coal burned and the wind speed of the fluidized bed to control the temperature of the graphite electrode material, comprising the following steps: Step S201: Obtain an abnormal situation judgment value according to the particle abnormality value, the first moisture abnormality value and the second moisture abnormality value.
[0038] It is known that when the particle abnormality value is smaller, the first moisture abnormality value is larger, and the second moisture abnormality value is larger, it is more likely that the cause of the abnormal temperature data is caused by the abnormal moisture content of the graphite electrode material; on the contrary, when the particle abnormality value is larger, the first moisture abnormality value is smaller, and the second moisture abnormality value is smaller, it is more likely that the cause of the abnormal temperature data is caused by the abnormal particle size of the graphite electrode material. Therefore, this embodiment obtains the abnormal situation judgment value according to the particle abnormality value, the first moisture abnormality value, and the second moisture abnormality value, wherein the particle abnormality value is negatively correlated with the abnormal situation judgment value, and the first moisture abnormality value and the second moisture abnormality value are both positively correlated with the abnormal situation judgment value. The larger the abnormal situation judgment value, the more likely that the cause of the abnormal temperature data of the graphite electrode material is caused by the abnormal moisture content of the graphite electrode material; the smaller the abnormal situation judgment value, the more likely that the cause of the abnormal temperature data of the graphite electrode material is caused by the abnormal particle size of the graphite electrode material. Among them, the calculation formula of the abnormal situation judgment value is: ; In the formula, y is the abnormality judgment value; l is the particle abnormality degree value; is the first moisture abnormality value; is the second moisture anomaly value; norm is the normalization function.
[0039] Step S202: Based on the abnormal situation judgment value, the coal burning amount and wind speed of the fluidized bed are adjusted to control the temperature of the graphite electrode material.
[0040] It is known that the larger the abnormal situation judgment value is, the more likely it is that the abnormal temperature data of the graphite electrode material is caused by the abnormal moisture content of the graphite electrode material; the smaller the abnormal situation judgment value is, the more likely it is that the abnormal temperature data of the graphite electrode material is caused by the abnormal particle size of the graphite electrode material; therefore, this embodiment sets the preset abnormal situation judgment threshold to 0.6, and the implementer can set the size of the preset abnormal situation judgment threshold according to actual conditions, and it is not limited here.
[0041] When the abnormal situation judgment value is greater than or equal to the preset abnormal situation judgment threshold, it is determined that the reason for the abnormal temperature data of the graphite electrode material is caused by the abnormal moisture content of the graphite electrode material. In order to effectively reduce the degree of abnormal temperature data of the graphite electrode material caused by the abnormal moisture content of the graphite electrode material, this embodiment keeps the wind speed of the fluidized bed unchanged. When the temperature data at the current moment is greater than the preset standard temperature data, it means that the temperature data of the graphite electrode material at this time has increased abnormally. In order to reduce the temperature data of the graphite electrode material, the amount of coal burned in the fluidized bed is reduced according to the first preset step length, the heat in the fluidized bed is reduced, and the temperature data of the graphite electrode material is reduced until the temperature data is less than or equal to the preset standard temperature data, and the reduction of coal burning is stopped. Among them, the preset standard temperature data can be set according to the actual situation, without limitation. In this embodiment, it is set to 90 degrees Celsius; When the temperature data at the current moment is less than the preset standard temperature data, it indicates that the temperature data of the graphite electrode material is abnormally reduced. In order to increase the temperature data of the graphite electrode material, the amount of coal burned in the fluidized bed is increased according to the first preset step length until the temperature data is greater than or equal to the preset standard temperature data, and then the increase in the amount of coal burned is stopped; When the temperature data at the current moment is equal to the preset standard temperature data, it means that the abnormal moisture content of the graphite electrode material has a relatively small influence on the temperature data of the graphite electrode material during the drying process, which can be ignored, and then the coal burning amount of the fluidized bed is not adjusted.
[0042] When the abnormal situation judgment value is less than the preset abnormal situation judgment threshold, it is determined that the reason for the abnormal temperature data of the graphite electrode material is caused by the abnormal particle size of the graphite electrode material. In order to effectively reduce the degree of abnormal temperature data of the graphite electrode material caused by the abnormal particle size of the graphite electrode material, this embodiment keeps the coal burning amount of the fluidized bed unchanged. When the temperature data at the current moment is greater than the preset standard temperature data, the temperature data of the graphite electrode material increases abnormally at this time. In order to reduce the temperature data of the graphite electrode material, the wind speed of the fluidized bed is increased according to the second preset step length until the temperature data is less than or equal to the preset standard temperature data, and the wind speed is stopped from increasing. When the temperature data at the current moment is less than the preset standard temperature data, the temperature data of the graphite electrode material decreases abnormally. In order to increase the temperature data of the graphite electrode material, the wind speed of the fluidized bed is reduced according to the second preset step length until the temperature data is less than or equal to the preset standard temperature data, and the wind speed is stopped from being reduced. When the temperature data at the current moment is equal to the preset standard temperature data, it means that the abnormal particle size of the graphite electrode material has a relatively small influence on the temperature data of the graphite electrode material during the drying process, which can be ignored, and the wind speed of the fluidized bed is not adjusted.
[0043] In this embodiment, the first preset step length is set to 1 kilogram, and the second preset step length is set to 0.1 meters per second. The implementer can set the size of the first preset step length and the second preset step length according to actual conditions, and no limitation is made here.
[0044] At this point, the temperature data of the graphite electrode material is accurately adjusted so that the moisture in the graphite electrode material is fully volatilized, and the problem of substandard quality caused by moisture in the graphite electrode material can be effectively avoided during the battery manufacturing process.
[0045] In summary, this embodiment obtains the temperature data of the graphite electrode material during the fluidized bed drying process, and determines whether the temperature data is abnormal according to the difference in temperature data at adjacent moments in the preheating and drying stage; when the temperature data is abnormal, the particle abnormality is obtained according to the duration of the preheating and drying stage, the first moisture abnormality is obtained according to the duration of the constant speed drying stage, and the second moisture abnormality is obtained according to the difference in temperature data at adjacent moments in the speed reduction drying stage, and then the temperature is controlled according to the particle abnormality, the first moisture abnormality and the second moisture abnormality. The present invention determines the cause of the abnormal temperature data by obtaining the particle abnormality, the first moisture abnormality and the second moisture abnormality, and then takes corresponding measures to regulate the temperature of the graphite electrode material, so that the graphite electrode material is effectively dried.
[0046] Embodiment 2: The present invention also proposes a fluidized bed material temperature control system, please refer to Figure 3 , which shows a structural diagram of a fluidized bed material temperature control system provided by an embodiment of the present invention, the system includes: a data acquisition module 10, a drying stage division module 20, a temperature data abnormality judgment module 30, an abnormality analysis module 40 and a temperature control module 50.
[0047] The data acquisition module 10 is used to acquire the temperature data of the graphite electrode material at each moment during the fluidized bed drying process.
[0048] The drying stage division module 20 is used to determine the preheating drying stage, the constant speed drying stage and the speed reduction drying stage in the drying process according to the change of the temperature data.
[0049] The temperature data abnormality judgment module 30 is used to judge whether the temperature data is abnormal according to the difference of the temperature data at adjacent moments in the preheating and drying stage.
[0050] The abnormality analysis module 40 is used to obtain the degree of particle abnormality of the graphite electrode material in the preheating and drying stage according to the duration of the preheating and drying stage when it is determined that the temperature data is abnormal; obtain the first degree of moisture abnormality of the graphite electrode material in the constant speed drying stage according to the duration of the constant speed drying stage; and obtain the second degree of moisture abnormality of the graphite electrode material in the speed reduction drying stage according to the difference in temperature data at adjacent moments in the speed reduction drying stage.
[0051] The temperature control module 50 is used to adjust the coal burning amount and wind speed of the fluidized bed to control the temperature of the graphite electrode material according to the particle abnormality degree, the first moisture abnormality degree and the second moisture abnormality degree.
[0052] It should be noted that: the system provided in the above embodiment is only illustrated by the division of the above functional modules. In actual applications, the above functions can be assigned to different functional modules as needed, that is, the internal structure of the computer device is divided into different functional modules to complete all or part of the functions described above. In addition, a fluidized bed material temperature control system and a fluidized bed material temperature control method embodiment provided in the above embodiment belong to the same concept. The specific implementation process is detailed in the method embodiment and will not be repeated here.
[0053] Embodiment 3: The present invention also proposes a fluidized bed material temperature control device, which includes a memory and a processor, wherein the memory stores an executable program code, and the processor is used to call and execute the executable program code to execute a fluidized bed material temperature control method provided in an embodiment of the present application. The device can be a chip, a component or a module, and the chip may include a connected processor and a memory; wherein the memory is used to store instructions, and when the processor calls and executes the instructions, the chip can execute a fluidized bed material temperature control method provided in the above embodiment.
[0054] In addition, the present application embodiment also protects a computer device, see Figure 4 The computer device includes a memory 401, a processor 402, and a computer program 403 stored in the memory 401 and running on the processor 402, wherein when the processor 402 executes the computer program 403, the computer device can execute any one of the fluidized bed material temperature control methods introduced above.
[0055] Embodiment 4: This embodiment also provides a computer-readable storage medium, in which a computer program code is stored. When the computer program code is run on a computer, the computer executes the above-mentioned related method steps to implement a fluidized bed material temperature control method provided in the above embodiment.
[0056] Embodiment 5: This embodiment further provides a computer program product. When the computer program product is run on a computer, the computer is enabled to execute the above-mentioned related steps to implement a fluidized bed material temperature control method provided in the above embodiment.
[0057] Among them, the device, computer-readable storage medium, computer program product or chip provided in this embodiment is used to execute the corresponding method provided above. Therefore, the beneficial effects that can be achieved can refer to the beneficial effects in the corresponding method provided above, and will not be repeated here.
[0058] It should be noted that the sequence of the above embodiments of the present invention is only for description and does not represent the advantages and disadvantages of the embodiments. The processes depicted in the accompanying drawings do not necessarily require the specific order or continuous order shown to achieve the desired results. In some embodiments, multitasking and parallel processing are also possible or may be advantageous.
[0059] The various embodiments in this specification are described in a progressive manner, and the same or similar parts between the various embodiments can be referenced to each other, and each embodiment focuses on the differences from other embodiments.
Claims
1. A method for controlling the temperature of fluidized bed materials, It is characterized in that The method comprises the following steps: Obtain the temperature data of graphite electrode materials at each moment during the fluidized bed drying process; According to the change of temperature data, determine the preheating drying stage, constant speed drying stage and speed reduction drying stage in the drying process; According to the difference of temperature data at adjacent moments in the preheating and drying stage, determine whether the temperature data is abnormal; When it is determined that the temperature data is abnormal, the degree of abnormality of the particles of the graphite electrode material in the preheating and drying stage is obtained according to the duration of the preheating and drying stage; the first degree of abnormality of the moisture content of the graphite electrode material in the constant-speed drying stage is obtained according to the duration of the constant-speed drying stage; the second degree of abnormality of the moisture content of the graphite electrode material in the speed-decreasing drying stage is obtained according to the difference in temperature data at adjacent moments in the speed-decreasing drying stage; According to the degree of particle abnormality, the first degree of moisture abnormality and the second degree of moisture abnormality, the temperature of the graphite electrode material is controlled by adjusting the amount of coal burned and the wind speed of the fluidized bed.
2. A method for controlling the temperature of a fluidized bed material according to claim 1, It is characterized in that The method for determining the preheating drying stage, the constant speed drying stage and the speed reduction drying stage in the drying process according to the change of the temperature data is as follows: When the temperature data first appears to be greater than or equal to the standard temperature data of water evaporation of the graphite electrode material, the time corresponding to the corresponding temperature data is taken as the first target time; The time period formed by the initial time and the first target time is used as the preheating and drying stage; When the temperature data first appears and the difference between it and the standard temperature data of water evaporation of the graphite electrode material is greater than the predicted temperature difference threshold, and the difference between the temperature data at the next adjacent moment to the moment corresponding to the corresponding temperature data and the standard temperature data of water evaporation of the graphite electrode material is also greater than the predicted temperature difference threshold, the moment corresponding to the corresponding temperature data is taken as the second target moment; The time period formed by the first target time and the second target time is used as a constant-speed drying stage; The time period formed by the second target time and the current time is used as the speed reduction drying stage.
3. A method for controlling the temperature of fluidized bed materials according to claim 1, It is characterized in that The method for determining whether the temperature data is abnormal is: Obtain the difference between the temperature data of each moment and the previous adjacent moment in the preheating and drying stage as the first difference of the corresponding moment; Acquire the number of first differences greater than a preset first difference threshold value in the preheating and drying stage as the first number; When the first number is greater than a preset first number threshold, it is determined that the temperature data is abnormal; When the first number is less than or equal to a preset first number threshold, it is determined that there is no abnormality in the temperature data.
4. A method for controlling the temperature of fluidized bed materials according to claim 1, It is characterized in that The method for obtaining the particle abnormality degree is: The result of normalizing the difference between the duration of the preheating drying stage and the standard preset drying duration is taken as the particle abnormality degree value.
5. A method for controlling the temperature of fluidized bed materials as claimed in claim 1, It is characterized in that The method for obtaining the first moisture abnormality degree is: The result of normalizing the difference between the duration of the constant-speed drying stage and the standard constant-speed drying duration is used as the first moisture abnormality degree value.
6. A method for controlling the temperature of fluidized bed materials as claimed in claim 3, It is characterized in that The method for obtaining the second moisture abnormality degree is: Obtaining the first difference at each moment in the speed-down drying stage, and taking the number of first differences greater than a preset second difference threshold in the speed-down drying stage as the second number; The ratio of the second quantity to the total quantity of all first differences in the speed-down drying stage is used as the second moisture abnormality degree value.
7. A method for controlling the temperature of fluidized bed materials according to claim 1, It is characterized in that The method for controlling the temperature of the graphite electrode material by adjusting the amount of coal burned and the wind speed of the fluidized bed according to the particle abnormality, the first moisture abnormality and the second moisture abnormality is: Obtain an abnormality judgment value according to the particle abnormality value, the first moisture abnormality value, and the second moisture abnormality value; wherein the particle abnormality value is negatively correlated with the abnormality judgment value, and the first moisture abnormality value and the second moisture abnormality value are both positively correlated with the abnormality judgment value; When the abnormal situation judgment value is greater than or equal to the preset abnormal situation judgment threshold, the wind speed of the fluidized bed is kept unchanged; when the temperature data at the current moment is greater than the preset standard temperature data, the coal burning amount of the fluidized bed is reduced according to the first preset step length until the temperature data is less than or equal to the preset standard temperature data, and the coal burning amount is stopped; when the temperature data at the current moment is less than the preset standard temperature data, the coal burning amount of the fluidized bed is increased according to the first preset step length until the temperature data is greater than or equal to the preset standard temperature data, and the coal burning amount is stopped; when the temperature data at the current moment is equal to the preset standard temperature data, the coal burning amount is not adjusted; When the abnormal situation judgment value is less than the preset abnormal situation judgment threshold, the coal burning amount of the fluidized bed is kept unchanged; when the temperature data at the current moment is greater than the preset standard temperature data, the wind speed of the fluidized bed is increased according to the second preset step length until the temperature data is less than or equal to the preset standard temperature data, and the wind speed is stopped from being increased; when the temperature data at the current moment is less than the preset standard temperature data, the wind speed of the fluidized bed is reduced according to the second preset step length until the temperature data is less than or equal to the preset standard temperature data, and the wind speed is stopped from being reduced; when the temperature data at the current moment is equal to the preset standard temperature data, the wind speed is not adjusted.
8. A method for controlling the temperature of fluidized bed materials as claimed in claim 7, It is characterized in that The first preset step length is set to 1 kilogram; the second preset step length is set to 0.1 meters per second.
9. A method for controlling the temperature of fluidized bed materials as claimed in claim 1, It is characterized in that The fluidized bed material temperature control method further comprises: When it is determined that there is no abnormality in the temperature data, the temperature of the graphite electrode material is not adjusted.
10. A fluidized bed material temperature control system, comprising a memory, a processor, and a computer program stored in the memory and executable on the processor, It is characterized in that When executing the computer program, the processor implements the steps of a fluidized bed material temperature control method as described in any one of claims 1 to 9.
Citation Information
Patent Citations
Intelligent optimization control method and system for aluminum oxide roasting furnace
CN116068897A
Drying chamber temperature control system suitable for lactic acid bacteria hot dry method production
CN116974313A
3D printing temperature control system and control method
CN118181771A
Plate heat exchanger unit energy efficiency evaluation method and system
CN118427567A
Desiccation controlling system for fluidized-bed
CN2859406Y
Cited By
Superheated water intelligent control method based on material drying process
CN120609195A
Granulation control method of granulator for producing water dispersible granules
CN120860907A
A granulator control method for producing water dispersible granules
CN120860907B