Protective film structure with bendable touch layer
By setting the composite hardened layer and the finely divided ITO island on the transparent substrate of the folded display screen and connecting it with ductile metal wires, the fragility of the protective layer when folding is solved, the hardness and thickness are improved, ensuring that Display screen stability and operation reliability.
Patent Information
- Application Number
- CN202410707613.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-06-05
- Filing Date
- 2024-06-03
- Publication Date
- 2024-12-06
AI Technical Summary
The protective layer of the existing foldable display screen is fragile when folded, resulting in damage to the touch layer and display screen control circuit, and scratching problems occur when the hardness and thickness are insufficient.
Multiple composite hardening layers are arranged on the transparent substrate that can be folded and bent, and the ITO is subdivided into island states. The island is reconnected using ductile metal wires to form touch electrodes, which improves the flexibility and resistance of the protective film. Scraping ability.
It effectively solves the problem of chipping of the protective layer when folding, while improving hardness and thickness, ensuring the stability and operation reliability of the display screen.
Smart Images

Figure CN119078309A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a protective film structure, and in particular to a protective film structure with a bendable touch layer. Background Art
[0002] Figure 1 A schematic diagram of folding a conventional electronic product 100 ′ with a foldable display screen is shown. The electronic product 100 ′ is, for example, a smart phone with a foldable display screen or an e-book reader with electronic paper. Figure 2 A partial cross-sectional view of the structure of the electronic product 100' with a foldable display screen is shown. As shown in this figure, the electronic product 100' has at least a protective layer 10', a touch layer 20' and a foldable display screen 30' from top to bottom. The protective layer 10' needs to have a certain hardness and thickness to provide anti-scratch function, and the transparency must be greater than 70%; however, this will cause the protective layer 10' to break when the foldable display screen 30' is folded. See Figure 3A and Figure 3B , respectively, to illustrate the problems that occur when the electronic product 100' with a foldable display screen is folded. As shown in these figures, since the protective layer 10' of the foldable display screen in the prior art must have a certain hardness and thickness to resist scratches, when the foldable display screen is folded, the protective layer 10' is not flexible enough, causing the protective layer 10 to break. The touch electrode structure in the touch layer 20' under the protective layer 10' will also break. In addition, folding will also cause the control circuit of the display screen 30' to break, causing the display of the electronic product 100' with a foldable display screen to deteriorate or even cause operation errors. If only the hardness or thickness of the protective layer 10' of the foldable display screen in the prior art is reduced, although the flexibility can be improved, it will cause scratch problems caused by insufficient hardness and thickness. Summary of the invention
[0003] The purpose of the present invention is to solve the above-mentioned problem by setting multiple composite hardened layers on a foldable and flexible transparent substrate to provide a protective film structure that is resistant to bending, folding and scratching, and to divide the ITO into islands, so that it can withstand bending. The finely divided ITO islands are then reconnected with ductile metal wires to form touch electrodes, thus solving the problem that the original touch electrodes cannot be bent.
[0004] To achieve the above-mentioned purpose, the present invention provides a protective film structure with a bendable touch layer, which comprises: a transparent substrate: comprising a first surface and a second surface, wherein the first surface is attached to or faces a protected device, such as a display screen; a composite hardened layer, arranged on the second surface of the substrate facing the user, the composite hardened layer comprising a first hard film layer and a second hard film layer, the first hard film layer being located on the outermost surface of the composite hardened layer; a touch layer being located between the first hard film layer and the second hard film layer, each touch electrode of the touch layer comprising a plurality of island electrodes; the transparent substrate is a polymer material substrate such as transparent PI, PET, or an ultra-thin glass substrate with a thickness not greater than 200µm.
[0005] According to an embodiment of the present invention, the area of each island electrode is not greater than 5 square centimeters, or the area of each island electrode is not greater than 1 square centimeter. When viewed from the projection direction, at least 60 percent of the spacing between adjacent island electrodes is not less than 3µm.
[0006] According to one embodiment of the present invention, a plurality of bridge conductors are further included, each of which is electrically connected to each of the adjacent island electrodes to connect each of the island electrodes into a touch electrode. Each of the bridge conductors is a conductive strip composed of a metal conductor with a wire diameter not greater than 50µm, or a metal connection wire mesh composed of a metal conductor with a wire diameter not greater than 50µm.
[0007] According to an embodiment of the present invention, the area of each of the island electrodes is not less than 0.1 square centimeters.
[0008] According to one embodiment of the present invention, the first hard mask layer is made of silicon nitride material. BRIEF DESCRIPTION OF THE DRAWINGS
[0009] Figure 1 A schematic diagram showing the folding of an electronic product with a foldable display screen in the prior art.
[0010] Figure 2 A partial structural cross-sectional view showing the electronic product with a foldable display screen.
[0011] Figure 3A and 3B Schematic diagrams are provided to respectively illustrate problems that may occur when the electronic product with a foldable display screen is folded.
[0012] Figure 4A FIG. 4 is a cross-sectional view of a composite hardened layer according to an embodiment of the present invention.
[0013] Figure 4B FIG. 4 is a cross-sectional view of a composite hardened layer according to another embodiment of the present invention.
[0014] Figure 4CFIG. 4 is a cross-sectional view of a composite hardened layer according to yet another embodiment of the present invention.
[0015] Figure 4D FIG. 4 is a cross-sectional view of a composite hardened layer according to yet another embodiment of the present invention.
[0016] Figure 5A FIG. 4 is a cross-sectional view of a protective film structure with a composite hardening layer according to an embodiment of the present invention.
[0017] Figure 5B FIG. 4 is a cross-sectional view of a protective film structure with a composite hardening layer according to another embodiment of the present invention.
[0018] Figure 5C FIG. 4 is a cross-sectional view of a protective film structure with a composite hardening layer according to yet another embodiment of the present invention.
[0019] Figure 5D FIG. 4 is a cross-sectional view of a protective film structure with a composite hardening layer according to yet another embodiment of the present invention.
[0020] Figure 5E FIG. 4 is a cross-sectional view of a protective film structure with a composite hardening layer according to yet another embodiment of the present invention.
[0021] Fig. 5F FIG. 4 is a cross-sectional view of a protective film structure with a composite hardening layer according to yet another embodiment of the present invention.
[0022] Figure 6 FIG. 4 is a cross-sectional view of a protective film structure with a composite hardening layer according to yet another embodiment of the present invention.
[0023] Fig. 7A The invention is to illustrate a touch layer structure that can be used with a protective film structure according to an embodiment of the invention.
[0024] Figure 7B To illustrate a touch layer structure that can be used with a protective film structure according to another embodiment of the present invention.
[0025] Figure 7C To illustrate a touch layer structure that can be used with a protective film structure according to another embodiment of the present invention.
[0026] Fig.7D To illustrate a touch layer structure that can be used with a protective film structure according to another embodiment of the present invention.
[0027] Fig. 7E The invention is to illustrate a touch layer structure with island-shaped electrodes according to another embodiment of the invention.
[0028] Fig. 8A FIG. 1 is a top view of an island electrode according to an embodiment of the present invention.
[0029] Figure 8B To illustrate the Fig. 8A A cross-sectional view along the dashed line A.
[0030] Figure 8C To illustrate the Fig. 8A Another cross-sectional view along dotted line A.
[0031] Fig.8D To illustrate the Fig. 8A A cross-sectional view along the dashed line B.
[0032] Fig. 8E To illustrate the Fig. 8A Another cross-sectional view along dotted line B.
[0033] 9A to 9D A schematic diagram for explaining the production of a rough surface on the protective film structure of the present invention.
[0034] FIG. 10A to FIG. 10D A schematic diagram for explaining the production of a rough surface on the protective film structure of the present invention.
[0035] FIG. 11A to FIG. 11E A schematic diagram for explaining the production of a rough surface on the protective film structure of the present invention.
[0036] In the figure: 100': electronic product; 10: protective film structure; 10': protective layer; 20, 20': touch layer; 22: touch electrode layer; 22A: first touch electrode layer; 22B: second touch electrode layer; 22A1, 22A2, 22AN: first touch electrode; 22B1, 22B2, 22Bn: second touch electrodes; CA, CB: island electrodes; BM1, BM2: bridge conductors; 24: insulation layer; 26A: first metal connection layer; 26B: second metal connection layer; 30, 30': display screen; 12, 12A, 12N, 13, 13A, 13B, 13N: first composite hardened layer; 14, 14A, 14N, 15: second composite hardened layer; 121,131,141,151: first dura mater layer; 122,132,142,152: second dura mater layer; 133,153: third dura mater layer; 40: transparent substrate; 41: first surface; 42: second surface; 16: organic tiling layer; 16': middle organic tiling layer; 17: inorganic island block; 18: organic island block; 17A, 17A': hollow island block; 17B, 17B': side wall; 19: inorganic hard film layer; A, B, C1, C2: dotted lines. DETAILED DESCRIPTION
[0037] The present invention is further described below in conjunction with the accompanying drawings and specific embodiments so that those skilled in the art can better understand the present invention and implement it, but the embodiments are not intended to limit the present invention.
[0038] See also Figure 4A , is a cross-sectional view of a composite hardened layer for illustrating an embodiment of the present invention. This composite hardened layer can be used in the protective film structure of the present invention (described later for details). This composite hardened layer is, for example, a first composite hardened layer 12, and includes a first hard film layer 121 and a second hard film layer 122 from top to bottom. The so-called "from top to bottom" mentioned above may be, for example, the usual direction of operation of an electronic product (such as a smart phone) having this composite hardened layer, that is, the user's finger is at the top and the screen of this smart phone is at the bottom. However, the above definition is only an exemplary direction description for illustrating the technical features of the present invention, and is not intended to limit the scope of the present invention. See. Figure 4B , is a cross-sectional view of a composite hardened layer of an embodiment of the present invention, and this composite hardened layer can also be used in the protective film structure of the present invention. This composite hardened layer is, for example, a second composite hardened layer 14, and includes a second hard film layer 142 and a first hard film layer 141 from top to bottom. Figure 4A and Figure 4B In the illustrated embodiment, the first hard film layer 121, 141 may be, for example, a silicon nitride material (SiNx) with a hardness greater than 6H (i.e., a pencil hardness of 6H); and the second hard film layer 122, 142 may be, for example, a silicon oxide material (SiOx) with a hardness greater than 3H (i.e., a pencil hardness of 3H) or an acrylic material with a hardness greater than 1H (i.e., a pencil hardness of 1H). Figure 4A In the first composite hardened layer 12 shown, the hardness difference between two adjacent hard coat materials (i.e., the first hard coat layer 121 and the second hard coat layer 122) is preferably not less than 3H pencil hardness, and the hardness of the first hard coat layer 121 is greater than the hardness of the second hard coat layer 122. Figure 4B In the second composite hardened layer 14 shown, the hardness difference between two adjacent hard coat materials (ie, the first hard coat layer 141 and the second hard coat layer 142 ) is preferably not less than 3H pencil hardness, and the hardness of the first hard coat layer 141 is greater than that of the second hard coat layer 142 .
[0039] See also Figure 4C , is a cross-sectional view of a composite hardened layer of another embodiment of the present invention, which can be used in the protective film structure of the present invention (see below for details). The composite hardened layer is, for example, a first composite hardened layer 13, and includes, from top to bottom, a first hard film layer 131, a third hard film layer 133, and a second hard film layer 132. Figure 4D, is a cross-sectional view of a composite hardened layer of another embodiment of the present invention. The composite hardened layer is, for example, a second composite hardened layer 15, and includes, from top to bottom, a second hard coat layer 152, a third hard coat layer 153, and a first hard coat layer 151. Figure 4C and Figure 4D In the illustrated embodiment, the first hard film layer 131, 151 may be, for example, a silicon nitride material (SiNx) with a hardness greater than 6H (i.e., a pencil hardness of 6H); and the second hard film layer 132, 152 may be, for example, a silicon oxide material (SiOx) with a hardness greater than 3H (i.e., a pencil hardness of 3H). The third hard film layer 133, 153 may be, for example, an acrylic material with a hardness greater than 1H (i.e., a pencil hardness of 1H). In addition, Figure 4C In the first composite hardened layer 13 shown, the hardness difference between two adjacent hard coat materials (i.e., between the first hard coat layer 131 and the third hard coat layer 133, and between the third hard coat layer 133 and the second hard coat layer 132) is preferably not less than 3H in pencil hardness, and the hardness of the first hard coat layer 131 is greater than the hardness of the second hard coat layer 132. Figure 4D In the second composite hardened layer 15 shown, the hardness difference between two adjacent hard coat materials (i.e., between the first hard coat layer 151 and the third hard coat layer 153, and between the third hard coat layer 153 and the second hard coat layer 152) is preferably not less than 3H pencil hardness, and the hardness of the first hard coat layer 151 is greater than the hardness of the second hard coat layer 152. The following description will be combined with other figures to further explain the implementation of the composite hardened layer according to the present invention.
[0040] See also Figure 5A , is a cross-sectional view of a protective film structure 10 with a composite hardened layer according to an embodiment of the present invention. The protective film structure 10 of the present invention may include, for example, a plurality of first composite hardened layers 12 from top to bottom, that is, the first composite hardened layer 12A ... the first composite hardened layer 12N as shown in the figure, and a transparent substrate 40 located under the first composite hardened layer 12N. The transparent substrate 40 includes a first surface 41 and a second surface 42, wherein the first surface 41 is attached to or faces a protected device, such as a display screen (see Figure 6 Folding display screen 30). Figure 5A As shown, at least one set of composite hardened layers (ie, the first composite hardened layer 12A ... the first composite hardened layer 12N) is disposed on the second surface 42 of the transparent substrate 40 facing the user (not shown). Figure 4A Each of the first composite hardened layer 12A ... the first composite hardened layer 12N comprises at least two hard film layers of different materials, namely a first hard film layer 121 and a second hard film layer 122, and the material hardness of the first hard film layer 121 is greater than the material hardness of the second hard film layer 122. Figure 5AIn the illustrated embodiment, the transparent substrate 40 may be a polymer material substrate, such as a transparent PI substrate or a PET substrate; or an ultra-thin glass substrate, and the thickness of the ultra-thin glass substrate is not greater than 200 μm.
[0041] See also Figure 5B , is a cross-sectional view of a protective film structure 10 with a composite hardened layer according to another embodiment of the present invention. The protective film structure 10 of the present invention may include, from top to bottom, a first composite hardened layer 12, a touch layer 20, a second composite hardened layer 14, and a transparent substrate 40. Similarly, the transparent substrate 40 includes a first surface 41 and a second surface 42, wherein the first surface 41 is attached to or faces a protected device, such as a display screen (see Figure 6 At least one set of composite hardened layers (i.e., the first composite hardened layer 12 and the second composite hardened layer 14) is disposed on the second surface 42 of the transparent substrate 40 facing the user (not shown). Figure 4A The first composite hardened layer 12 includes at least two hard coat layers made of different materials, namely a first hard coat layer 121 and a second hard coat layer 122, and the material hardness of the first hard coat layer 121 is greater than the material hardness of the second hard coat layer 122. Figure 4B The second composite hardened layer 14 includes at least two hard film layers made of different materials, namely a first hard film layer 141 and a second hard film layer 142, and the material hardness of the first hard film layer 141 is greater than the material hardness of the second hard film layer 142. Figure 5B In the illustrated embodiment, the transparent substrate 40 may be a polymer material substrate, such as a transparent PI substrate or a PET substrate; or an ultra-thin glass substrate, and the thickness of the ultra-thin glass substrate is not greater than 200 μm.
[0042] See also Figure 5C , is a cross-sectional view of a protective film structure 10 with a composite hardening layer according to another embodiment of the present invention. The structure of this embodiment is similar to Figure 5A , that is, the first surface 41 of the transparent substrate 40 faces a protected device, such as a display screen (see Figure 6 At least one set of composite hardened layers (ie, first composite hardened layers 12A, . . . first composite hardened layers 12N) is disposed on the second surface 42 of the transparent substrate 40 facing the user (not shown). Figure 5C Example and Figure 5A The difference shown is that a touch layer 20 is disposed on the first surface 41 of the transparent substrate 40. Similarly, the transparent substrate 40 can be a polymer material substrate, such as a transparent PI substrate or a PET substrate; or an ultra-thin glass substrate, the thickness of which is not greater than 200 μm.
[0043] See also Figure 5D , is a cross-sectional view of a protective film structure 10 with a composite hardening layer according to another embodiment of the present invention. The structure of this embodiment is similar to Figure 5A , that is, the first surface 41 of the transparent substrate 40 faces a protected device, such as a display screen (see Figure 6 At least one set of composite hardened layers (i.e., first composite hardened layers 13A ... first composite hardened layers 13N) is disposed on the second surface 42 of the transparent substrate 40 facing the user (not shown). Figure 4C Each of the first composite hardened layers 13A ... 13N comprises at least two hard coat layers of different materials, namely a first hard coat layer 131 and a second hard coat layer 132 (with a third hard coat layer 133 sandwiched therebetween), and the material hardness of the first hard coat layer 131 is greater than the material hardness of the second hard coat layer 132. Figure 5D In the illustrated embodiment, the transparent substrate 40 may be a polymer material substrate, such as a transparent PI substrate or a PET substrate; or an ultra-thin glass substrate, and the thickness of the ultra-thin glass substrate is not greater than 200 μm.
[0044] See also Figure 5E , is a cross-sectional view of a protective film structure 10 with a composite hardening layer according to another embodiment of the present invention. The structure of this embodiment is similar to Figure 5B That is, the protective film structure 10 includes, from top to bottom, a first composite hardened layer 13, a touch layer 20, a second composite hardened layer 15, and a transparent substrate 40. Similarly, the transparent substrate 40 includes a first surface 41 and a second surface 42, wherein the first surface 41 is attached to or faces a protected device, such as a display screen (see Figure 6 At least one set of composite hardened layers (i.e., the first composite hardened layer 13 and the second composite hardened layer 15) is disposed on the second surface 42 of the transparent substrate 40 facing the user (not shown). Figure 4C The first composite hardened layer 13 includes at least two hard coat layers of different materials, namely, a first hard coat layer 131 and a second hard coat layer 132 (with a third hard coat layer 133 sandwiched therein), and the material hardness of the first hard coat layer 131 is greater than the material hardness of the second hard coat layer 132. Figure 4D The second composite hardened layer 15 includes at least two hard film layers made of different materials, namely, a first hard film layer 151 and a second hard film layer 152 (with a third hard film layer 153 sandwiched therein), and the material hardness of the first hard film layer 151 is greater than the material hardness of the second hard film layer 152. Figure 5EIn the illustrated embodiment, the transparent substrate 40 may be a polymer material substrate, such as a transparent PI substrate or a PET substrate; or an ultra-thin glass substrate, and the thickness of the ultra-thin glass substrate is not greater than 200 μm.
[0045] See also Fig. 5F , is a cross-sectional view of a protective film structure 10 with a composite hardening layer according to another embodiment of the present invention. The structure of this embodiment is similar to Figure 5E , however, the touch layer 20 includes a plurality of first composite hardened layers 13, such as first composite hardened layers 13A and 13B. In addition, the touch layer 20 includes at least one second composite layer 14 below. The structure of the first composite hardened layer 13 can be seen in Figure 4C , that is, the first composite hardened layer 13 includes a three-layer structure of a first hard coat layer 131, a third hard coat layer 133 and a second hard coat layer 132 from top to bottom; and the material hardness of the first hard coat layer 131 is greater than the material hardness of the second hard coat layer 132. The structure of the second composite layer 14 can be seen in Figure 4B , that is, the second composite hardened layer 14 includes a second hard coat layer 142 and a first hard coat layer 141 from top to bottom; and the material hardness of the first hard coat layer 141 is greater than the material hardness of the second hard coat layer 142. Figure 5E and Fig. 5F It can be seen from the embodiments that the number of material layers included in the composite hardened layer of the present invention is not limited to two layers, but can also be three layers, as long as the material hardness of one hard film layer is greater than the material hardness of another hard film layer.
[0046] See also Figure 6 , is a cross-sectional view of a protective film structure 10 with a composite hardening layer according to another embodiment of the present invention. The structure of this embodiment is similar to Figure 5B , however, there are a plurality of first composite hardened layers 12 on the touch layer 20, namely, the first composite hardened layer 12A ... the first composite hardened layer 12N as shown in the figure; and there are a plurality of second composite hardened layers 14 under the touch layer 20, namely, the second composite hardened layer 14A ... the second composite hardened layer 14N as shown in the figure. Furthermore, although not explicitly shown in the figure, according to the present invention, there may also be a plurality of first composite hardened layers 13 on the touch layer 20, and the structure of each first composite hardened layer 13 is as shown in the figure. Figure 4C Furthermore, there may be a plurality of second composite hardened layers 15 under the touch layer 20, and the structure of each second composite hardened layer 15 is as shown in FIG. Figure 4D Furthermore, Figure 6 In the embodiment, a protected device, such as a foldable display screen 30 , is established on the first surface 41 of the transparent substrate 40 .
[0047] See also Fig. 7A, is a cross-sectional view of the touch layer 20 according to the present invention. The touch electrodes of the prior art are all made of transparent conductive material ITO. Since ITO material is a ceramic material with brittle characteristics, it cannot be bent. In order to solve the problem that the existing technology cannot be used in the application scenario of flexible screens, the present invention divides the touch electrodes made of ITO into islands, so that it can withstand bending, and then uses a ductile metal wire to reconnect the scattered ITO islands to form the original touch electrodes. The detailed description is as follows. As shown in this figure, this touch layer 20 is, for example, a touch electrode for mutual capacitive touch, and includes a first touch electrode layer 22A and a second touch electrode layer 22B separated by an insulating layer 24, wherein each touch electrode layer includes a plurality of touch electrodes. See also Fig.7D , which is a top view of the touch layer 20 according to the present invention. The first touch electrode layer 22A may include strip electrodes arranged in rows (i.e., first touch electrodes 22A1, 22A2, ...), and the second touch electrode layer 22B may include strip electrodes arranged in columns (i.e., second touch electrodes 22B1, 22B2, ...). Please also refer to Fig. 7A and Fig.7D The touch electrodes of the first touch electrode layer 22A and the second touch electrode layer 22B may be separated from each other in the up and down directions and an insulating layer 24 is used as electrical insulation between electrodes of different layers.
[0048] See also Figure 7B , is a cross-sectional view of a touch layer 20 according to an embodiment of the present invention. As shown in this figure, the touch layer 20 is, for example, a touch electrode for mutual capacitive touch, and the transmitting electrode and the receiving electrode are both located on the same touch electrode layer 22. Furthermore, the touch electrode layer 22 has a plurality of touch electrodes (i.e., first touch electrodes) corresponding to the transmitting electrode and electrically connected via the first metal connection layer 26A; the touch electrode layer 22 has a plurality of touch electrodes (i.e., second touch electrodes) corresponding to the receiving electrode and electrically connected via the second metal connection layer 26B. In addition, the first metal connection layer 26A and the second metal connection layer 26B are insulated from each other by an insulating layer 24.
[0049] See also Figure 7C , is a cross-sectional view of a touch layer 20 according to another embodiment of the present invention. Figure 7B However, the first touch electrode layer 22A and the second touch electrode layer 22B for realizing mutual capacitance are located in different layers and separated by an insulating layer 24. Figure 7B , the touch electrodes belonging to the first touch electrode layer 22A are electrically connected via the first metal connection layer 26A; and the touch electrodes belonging to the second touch electrode layer 22B are electrically connected via the second metal connection layer 26B. 7A to 7D The touch electrode of the embodiment is a transparent metal oxide (ITO) electrode.
[0050] See also Fig. 7E , to illustrate the corresponding Fig.7D According to one embodiment of the present invention, each touch electrode 22A1, 22A2 (or 22B1, 22B2) of the touch electrode layer may include a plurality of island electrodes CA (or CB), and the plurality of island electrodes belonging to the same touch electrode are connected by a plurality of bridge conductors BM1 (or BM2) to form a touch electrode. Fig. 7E As shown, a touch electrode of the first touch electrode layer 22A (e.g., a first touch electrode 22A1 extending along the row direction) includes a plurality of island electrodes CA, and the plurality of island electrodes CA belonging to the same touch electrode (e.g., the first touch electrode 22A1) are electrically connected by a plurality of bridge conductors BM1 to collectively form the first touch electrode 22A1. Similarly, a touch electrode of the second touch electrode layer 22B (e.g., a second touch electrode 22B1 extending along the column direction) includes a plurality of island electrodes CB, and the plurality of island electrodes CB belonging to the same touch electrode (e.g., the second touch electrode 22B1) are electrically connected by a plurality of bridge conductors BM2 to collectively form the second touch electrode 22B1.
[0051] Furthermore, see Fig. 7E , the area of each island electrode CA (or CB) is, for example, not greater than 5 square centimeters. According to one embodiment of the present invention, the area of each island electrode is, for example, not greater than 1 square centimeter. According to one embodiment of the present invention, the area of each island electrode is not less than 0.1 square centimeter. The optimal condition is that at least 60 percent of the island electrode area is not greater than 5 square centimeters. Furthermore, for island electrodes not greater than 5 square centimeters, the spacing between at least sixty percent of adjacent island blocks is not less than 3µm when viewed from the projection direction. In addition, the bridging conductor may be, for example, a highly ductile conductor such as a composite layer structure of aluminum or molybdenum-aluminum-molybdenum, an island-shaped transparent conductor, or a conductive strip composed of a metal conductor with a wire diameter not greater than 50µm, or a metal connecting wire mesh composed of a metal conductor with a wire diameter not greater than 50µm.
[0052] See also Fig. 8A and Figure 8B , for a more detailed description of the island electrode according to the present invention. Figure 8B As shown, the corresponding Fig. 8A The cross-sectional view of the dashed line A in FIG. 1 and may correspond to, for example, Figure 5B The embodiment shown, that is, the corresponding screen protection film structure 10 includes a first composite hardened layer 12, a touch layer 20, a second composite hardened layer 14 and a transparent substrate 40 from top to bottom. Figure 8B As shown, see Fig. 7A or Figure 7CThe island electrodes CA corresponding to the touch electrodes of the first touch electrode layer 22A and the island electrodes CB corresponding to the touch electrodes of the second touch electrode layer 22B are separated by the insulating layer 24. Fig.8D , corresponding to Fig. 8A The cross-sectional view of the dashed line B corresponds to Figure 8B For more information, see Figure 8B , the plurality of island electrodes CA corresponding to the first touch electrodes of the first touch electrode layer 22A are electrically connected to each other by the bridge conductor BM1 to form the first touch electrode. Fig.8D The plurality of island electrodes CB of the touch electrodes corresponding to the second touch electrodes 22B are electrically connected to each other via the bridge conductor BM2 to form a second touch electrode.
[0053] See also Fig. 8A and Figure 8C , is another more detailed description of the island electrode according to the present invention. Figure 8C As shown, the corresponding Fig. 8A The cross-sectional view of the dotted line A may correspond to, for example, Figure 5B In the embodiment, the corresponding screen protection film structure 10 includes a first composite hardened layer 12, a touch layer 20, a second composite hardened layer 14 and a transparent substrate 40 from top to bottom. Figure 8B As shown, see Figure 7B , the island electrodes CA corresponding to the touch electrodes of the first touch electrode layer 22A and the island electrodes CB corresponding to the touch electrodes of the second touch electrodes 22B are on the same plane. Fig. 8E , corresponding to Fig. 8A The cross-sectional view of the dotted line B corresponds to Figure 8C For more information, see Figure 8C , the plurality of island electrodes CA corresponding to the first touch electrodes of the first touch electrode layer 22A are electrically connected to each other by the bridge conductor BM1 to form the first touch electrode. Fig. 8E The plurality of island electrodes CB of the touch electrodes corresponding to the second touch electrodes 22B are electrically connected to each other via the bridge conductor BM2 to form a second touch electrode.
[0054] See also 9A to 9DIn addition to forming the touch electrodes with multiple island electrodes as mentioned above, since electronic paper is the mainstream of flexible displays, electronic paper relies on light reflecting the electronic ink of the electronic paper to form an image, which is different from LCD or OLED which uses the screen itself to emit light to form an image. Therefore, the anti-glare requirements on the surface of the protective film are relatively high. The greater the reflection coefficient, the more unfavorable it is for reading. Therefore, the present invention forms rough surfaces of different heights on the surface of the protective film to produce random reflections, thereby reducing the reflection coefficient. In addition, the rough surface can also change the hard coating from a planar structure to a three-dimensional structure. When a foreign object contacts and causes a local collapse, the three-dimensional structure of the hard coating helps to extend the plane and is not easy to crack. When a collapse occurs, the height difference of the rough surface of the hard coating will be reduced, thereby expanding the surface area, so that it can withstand a deeper collapse. The present invention can also form an island-shaped first hard coating layer 151 or an island-shaped third hard coating layer 153 on the substrate 40. Fig.9A As shown, each island-shaped first hard coat layer 151 or third hard coat layer 153 has a length of 5-1000 um and a width of 5-1000 um. Fig. 9C As shown, the protective film structure may include a third hard coat layer 153 and a first hard coat layer 151 from top to bottom; or a first hard coat layer 151 and a third hard coat layer 153 from top to bottom. Fig.9D As shown, the protective film structure may include a second hard coat layer 152, a first hard coat layer 151 and a third hard coat layer 153 from top to bottom; or a second hard coat layer 152, a third hard coat layer 153 and a first hard coat layer 151 from top to bottom. 9A to 9D The specific structures of the first hard coat layer 151, the second hard coat layer 152 and the third hard coat layer 153 can be seen in Figure 4D In other words, the first hard film layer 151 may be, for example, an inorganic material such as silicon nitride (SiNx) and have a hardness greater than 6H (i.e., pencil hardness 6H); and the second hard film layer 152 may be, for example, an inorganic material such as silicon oxide (SiOx) and have a hardness greater than 3H (i.e., pencil hardness 3H). The third hard film layer 153 may be, for example, an organic material such as acrylic or a transparent polymer material and have a hardness greater than 1H (i.e., pencil hardness 1H). Fig.9D The structure can replace Figure 5B , Figure 5E and Fig. 5F The second composite hardened layers 14, 15 are provided to provide anti-scratch and anti-crack protection for the touch layer 20 and the screen.
[0055] See also FIG. 10A to FIG. 10D , is a cross-sectional view illustrating a protective film structure having a composite hardening layer according to another embodiment of the present invention. Fig. 10AAs shown, a plurality of inorganic island blocks 17 (first island block layer) in an island shape may be formed on the transparent substrate 40; the material of the inorganic island block 17 may be, for example, silicon dioxide. An organic paving layer 16 is formed on the inorganic island block 17; the material of the organic paving layer 16 may be, for example, acrylic and the thickness is not less than twice the thickness of the organic island block 17. In addition, a second composite hardened layer 14 and a first composite hardened layer 12 are formed on the organic paving layer 16, respectively. The materials of the first composite hardened layer 12 and the second composite hardened layer 14 may be, for example, Figure 4A and Figure 4B , and related descriptions. In addition, see Fig. 10D Each island-shaped inorganic island block 17 is a polygon, such as a rectangle, and the length m of the rectangle is 5-1000um and the width n is also 5-1000um. In this illustration, the shape of the island block is a rectangle for the convenience of explanation, and the shape of the island block of the present invention is not limited thereto. The shape can be a triangle, a circle, or various polygons.
[0056] In other embodiments of the present invention, the first island block layer may be made of an organic material, such as an acrylic material.
[0057] See later Fig. 10B ,At Fig. 10A A plurality of organic islands 18 (second island layer) may be formed on the obtained structure, and the material thereof may be, for example, acrylic or photosensitive polyimide. Furthermore, an inorganic hard film layer 19 may be formed on the plurality of organic islands 18, and the material thereof may be, for example, silicon nitride material (SiNx), and the thickness thereof may be less than 2 um. Fig. 10C An intermediate organic paving layer 16' may also be formed between the first composite hardening layer 12 and the second composite hardening layer 14, and its material is, for example, acrylic. FIG. 10A to FIG. 10C The first composite hardened layer 12 and the second composite hardened layer 14 may be a multi-layer structure, or may be Figure 4C and Figure 4D The first composite hardened layer 13 and the second composite hardened layer 15 are replaced.
[0058] In other embodiments of the present invention, the second island block layer may be made of an inorganic material, such as silicon dioxide or silicon nitride.
[0059] See also FIG. 11A to FIG. 11E , is a schematic diagram for explaining the production of a rough surface on the protective film structure of the present invention. Fig.11A As shown, a hollow island block 17A may be formed on the transparent substrate 40. Fig. 11B , which is along Fig.11A The cross-sectional view of the dotted line C1. Fig. 11BAs shown, the hollow island block 17A is a recessed portion defined by the side wall (grid structure) 17B. The hollow island block (hollow portion) 17A can be a polygon, such as a rectangle, and the length of the rectangle is 5-1000um and the width is also 5-1000um. In addition, the material of the side wall (grid structure) 17B can be an inorganic material such as silicon dioxide, or an organic material such as acrylic material. In this illustration, the shape of the hollow island block (first hollow island block) 17A is a rectangle just for the convenience of explanation. The shape of the hollow island block 17A of the present invention is not limited to this; its shape can be a triangle, a circle, or various polygons, etc. For complex coordination, see Fig. 11C , Fig.11D and Fig.11E , which are respectively along Fig.11A The cross-sectional view of the dotted lines C1 and C2. Fig. 11C In the embodiment shown, the sidewall (grid structure) 17B of the hollow island block is made of inorganic material, such as silicon dioxide, and at least one inorganic hard film layer 19, such as a silicon nitride hard film layer, is disposed on the hollow island block layer. Fig.11D In another embodiment shown, the side wall (grid structure) 17B of the hollow island block is made of organic material, such as acrylic material, and at least one composite hardened layer is provided on the hollow island block layer, such as a second hard film layer 122 of silicon dioxide superimposed on a first hard film layer 121 of silicon nitride. Fig.11E In the embodiment shown, along Fig.11A The cross-sectional view of the dotted line C2 shows that this embodiment includes two layers of hollow island block layers, wherein the first island block layer is an inorganic material side wall (grid structure) 17B disposed on the surface of the transparent substrate 40 and forming a plurality of hollow island blocks 17A, and a paving layer (e.g., an organic paving layer 16) and other corresponding structures (e.g., Figures 10A-10D The first composite hardened layer 12 and the second composite hardened layer 14, etc., shown in the figure, and a second island block layer is arranged on the upper end of each of the composite hardened layers, preferably a hollow island block (second hollow island block) 17A' composed of a side wall grid structure 17B' of an organic material (such as an acrylic material), and at least one composite hardened layer is arranged on the hollow island block layer, such as a second hard film layer 122 of silicon dioxide superimposed on a first hard film layer 121 of silicon nitride. Among them, it is preferred that the hollow island blocks 17A and the auxiliary hollow island blocks 17A' of different island block layers do not completely overlap in the projection direction. The above-mentioned embodiments 11C, 11D and 11E all use the hollow island block 17A (or / and the hollow island block 17A') to form a rough surface of the hard film layer to enhance the anti-bending and anti-scratch functions of the protective film structure. In the above-mentioned embodiments, the protective film structure with a composite hardened layer of the present invention includes at least two groups of composite hardened layers, such as FIG. 5A to FIG. 5F and Figure 6Furthermore, the protective film structure comprises at least three sets of composite hardened layers, such as Fig. 5F and Figure 6 Each composite hardened layer comprises at least two hard film layers of different materials, such as Figure 4A and Figure 4B The two hard layers shown, or Figure 4C and Figure 4D The three hard coat layers shown. Furthermore, the thickness of each first hard coat layer in each of the above-mentioned composite hardened layers is not greater than 2um, the total thickness of each first hard coat layer of all the composite hardened layers is not greater than 10um, and the total thickness of each first hard coat layer of all the composite hardened layers is not less than 0.3um. Furthermore, the thickness of each second hard coat layer in each of the above-mentioned composite hardened layers is not greater than 5um, the total thickness of each second hard coat layer of all the composite hardened layers is not greater than 15um, and the total thickness of each second hard coat layer of all the composite hardened layers is not less than 0.5um. With the above-mentioned thickness configuration of the first hard coat layer and the second hard coat layer, and designing the material hardness of the first hard coat layer to be greater than the material hardness of the second hard coat layer, the protective film structure with a composite hardened layer of the present invention can be made flexible, scratch-resistant and crack-resistant.
[0060] exist FIG. 8A to FIG. 8D , 9A to 9D , FIG. 10A to FIG. 10D , FIG. 11A to FIG. 11D In the structure shown, by means of an island electrode, an island-shaped first hard coat layer 151 or a third hard coat layer 153, an inorganic island block 17, or a hollow island block 17A, the surface of a hard coat layer of the composite hardened layer can be made concave and convex, and the height difference is not less than 0.1µm; or the roughness of a surface of the protective film structure facing the user is made not less than 0.1µm, so as to increase the hydrophobicity and reduce the reflection coefficient of the electronic products using this protective film structure. In addition, the rough surface can also make the hard coating layer change from a planar structure to a three-dimensional structure. When a local collapse is caused by foreign matter contact, the three-dimensional structure of the hard coating layer helps to extend the plane and is not easy to crack. When collapse occurs, the height difference of the rough surface of the hard coating layer will be reduced, thereby expanding the surface area, so that it can withstand a deeper collapse.
[0061] The above-described embodiments are only preferred embodiments for fully illustrating the present invention, and the protection scope of the present invention is not limited thereto. Equivalent substitutions or changes made by those skilled in the art based on the present invention are within the protection scope of the present invention. The protection scope of the present invention shall be subject to the claims.
Claims
1. A protective film structure with a bendable touch layer, characterized in that: Include: A transparent substrate comprising a first surface and a second surface, wherein the first surface is attached to or faces a display screen; At least one composite hardened layer is disposed on the second surface of the substrate facing the user, each of the at least one composite hardened layer comprises a first hard coat layer and a second hard coat layer, and the first hard coat layer is located on the outermost surface of the composite hardened layer; A touch layer is located between a composite hardening layer and the substrate, and each touch electrode of the touch layer includes a plurality of island electrodes; The transparent substrate is a polymer material substrate, or an ultra-thin glass substrate with a thickness not greater than 200 μm.
2. The protective film structure with a bendable touch layer according to claim 1, characterized in that: The area of each island electrode is no greater than 5 square centimeters.
3. The protective film structure with a bendable touch layer according to claim 2, characterized in that: The area of each island electrode is no greater than 1 square centimeter.
4. The protective film structure with a bendable touch layer according to claim 2, characterized in that: The area of each island electrode is not less than 0.1 square centimeters.
5. The protective film structure with a bendable touch layer according to claim 2, characterized in that: When viewed from the projection direction, the spacing between at least 60 percent of the adjacent island electrodes is not less than 3 μm.
6. The protective film structure with a bendable touch layer according to claim 1, characterized in that: The invention further comprises a plurality of bridge conductors, each of which is electrically connected to each of the adjacent island electrodes to connect each of the island electrodes into a touch electrode.
7. The protective film structure with a bendable touch layer according to claim 6, characterized in that: Each of the bridging conductors is a conductive strip composed of a metal conductor with a wire diameter not greater than 50 μm, or a metal connecting wire mesh composed of a metal conductor with a wire diameter not greater than 50 μm.
8. The protective film structure with a bendable touch layer according to claim 1, wherein: The first hard film layer is made of silicon nitride material.
Citation Information
Cited By
Vane-like wear-resistant ultra-wideband anti-reflection film structure and preparation method thereof
CN121657180A