Use of 1, 1, 1, 3, 5, 5, 5-heptafluoro-2-pentene in non-aqueous electrolyte solution, non-aqueous electrolyte solution comprising 1, 1, 3, 5, 5, 5-heptafluoro-2-pentene, and secondary battery comprising same
By using HFO-1447, lithium hexafluorophosphate and carbonate solvent in the non-aqueous electrolyte of lithium-ion secondary batteries, the unknown use of HFO-1447 was solved, and the formation of high-quality coating in the secondary battery was achieved, and the battery characteristics were improved. and cycle stability.
Patent Information
- Application Number
- CN202380035496.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-04-28
- Filing Date
- 2023-04-27
- Publication Date
- 2024-12-06
AI Technical Summary
In the prior art, the use of 1,1,1,3,5,5-heptafluoro-2-pentene (HFO-1447) is unknown, especially in non-aqueous electrolytes and secondary batteries. .
HFO-1447 is used in the non-aqueous electrolyte of lithium ion secondary batteries, combining lithium hexafluorophosphate and carbonate solvent to form an electrolyte, and a high-quality coating is formed at the interface between the positive electrode and the negative electrode to improve the battery characteristics.
HFO-1447 forms a high-quality coating in a nonaqueous electrolyte, providing excellent battery characteristics, including high capacity maintenance and cycle stability, and has self-extinguishing and chemical stability, making it suitable as an electrolyte additive.
Smart Images

Figure BDA0005095171310000031 
Figure BDA0005095171310000051 
Figure BDA0005095171310000061
Abstract
Description
Technical Field The present invention relates to use of 1,1,1,3,5,5,5-heptafluoro-2-pentene in a non-aqueous electrolyte, a non-aqueous electrolyte containing 1,1,1,3,5,5,5-heptafluoro-2-pentene, and a secondary battery containing the non-aqueous electrolyte. Background Art 1,1,1,3,5,5,5-heptafluoro-2-pentene (hereinafter sometimes referred to as "HFO-1447") is a known compound such as CAS No. (E)-HFO-1447: 1227064-59-6 and (Z)-HFO-1447: 1227064-60-9, but its use is unknown. Summary of the invention Problem that the invention aims to solve The present invention aims to provide a new use of HFO-1447, in particular a new use of HFO-1447 in a non-aqueous electrolyte; a non-aqueous electrolyte containing HFO-1447 and a secondary battery containing the non-aqueous electrolyte. Solutions for solving problems The present invention provides the following solutions.
[0001] Disclosed is a use of 1,1,1,3,5,5,5-heptafluoro-2-pentene in a non-aqueous electrolyte.
[0002] The use according to [1], wherein the non-aqueous electrolyte is a non-aqueous electrolyte for a secondary battery.
[0003] The use according to [2], wherein the secondary battery is a lithium ion secondary battery.
[0004] The use according to [1], wherein the non-aqueous electrolyte comprises: Electrolytes, 1,1,1,3,5,5,5-heptafluoro-2-pentene, and Non-aqueous organic solvents.
[0005] The use according to [4], wherein the electrolyte is lithium hexafluorophosphate and the non-aqueous organic solvent is a carbonate solvent.
[0006] The use according to any one of [1] to [5], wherein the 1,1,1,3,5,5,5-heptafluoro-2-pentene is (E)-1,1,1,3,5,5,5-heptafluoro-2-pentene, (Z)-1,1,1,3,5,5,5-heptafluoro-2-pentene, or a mixture of (E)-1,1,1,3,5,5,5-heptafluoro-2-pentene and (Z)-1,1,1,3,5,5,5-heptafluoro-2-pentene.
[0007] A non-aqueous electrolyte comprising: Electrolytes, 1,1,1,3,5,5,5-heptafluoro-2-pentene, and Non-aqueous organic solvents.
[0008] The non-aqueous electrolyte solution according to [7], wherein the electrolyte is lithium hexafluorophosphate and the non-aqueous organic solvent is a carbonate solvent.
[0009] The non-aqueous electrolyte according to [7], wherein the 1,1,1,3,5,5,5-heptafluoro-2-pentene is (E)-1,1,1,3,5,5,5-heptafluoro-2-pentene, (Z)-1,1,1,3,5,5,5-heptafluoro-2-pentene, or a mixture of (E)-1,1,1,3,5,5,5-heptafluoro-2-pentene and (Z)-1,1,1,3,5,5,5-heptafluoro-2-pentene.
[0010] A secondary battery comprising the nonaqueous electrolyte solution according to any one of [7] to [9].
[0011] The secondary battery according to
[10] , wherein the secondary battery is a lithium ion secondary battery. Effects of the Invention According to the present invention, a new use of HFO-1447 in a non-aqueous electrolyte, a non-aqueous electrolyte containing HFO-1447, and a secondary battery containing the non-aqueous electrolyte are provided. HFO-1447 forms a high-quality coating at the interface between the positive electrode and the negative electrode, and can provide excellent battery characteristics. BRIEF DESCRIPTION OF THE DRAWINGS Figure 1 is a schematic diagram of a stacked battery used for battery evaluation in Examples. Figure 2 This is a graph showing the transition of the capacity retention rate in the cycle test performed in the battery evaluation of the example. DETAILED DESCRIPTION [effect] 1,1,1,3,5,5,5-heptafluoro-2-pentene (HFO-1447) used in the present invention can be represented by the following formula (1). As described in the examples of this specification, the inventors have newly discovered that HFO-1447 forms a high-quality coating on either or both of the interfaces of the positive and negative electrodes of secondary batteries, which can provide excellent battery characteristics. The usefulness of HFO-1447 was discovered in experiments, and as described below, it is believed that it is due to the chemical structure of HFO-1447. The electrolyte of secondary batteries generally uses a non-aqueous organic solvent, and lithium hexafluorophosphate (LiPF 6) and other fluorine-based electrolytes as electrolytes. HFO-1447 has two trifluoromethyl groups and one fluorine group, so it has a high affinity for fluorine compounds. On the other hand, since it has a basic skeleton of a carbon chain, it also has a high affinity for non-aqueous organic solvents and can be uniformly mixed in the electrolyte. In addition, due to the conjugation of the C=C double bond in the center of the molecule and the electron pair of the fluorine group, the state of polarization can exist stably, so it also has a high affinity for the interface between the positive and negative electrodes and can exist stably between these electrodes. Due to this chemical structural feature, HFO-1447 is considered to be useful as an additive for the electrolyte of secondary batteries. The molecular weight of HFO-1447 is relatively large, at 196, so the boiling points are 52°C for (E)-HFO-1447 and 78°C for (Z)-HFO-1447, and it is a liquid at room temperature and pressure. There are 7 fluorine atoms in the molecule, so it is self-extinguishing. One of the trifluoromethyl groups extending to the outside of the molecule is connected by a methylene group (-CH 2 -) is linked to a rigid C=C double bond, so it has a relatively high degree of freedom, and the external aggressiveness of the reaction reagent to the C=C double bond is moderately restricted. The 2,2,2-trifluoroethyl group bonded to the C=C double bond is affected by the electron-withdrawing property of the trifluoromethyl group at the end, but due to the intervention of the methylene group, it imparts moderate electron-withdrawing property to the C=C double bond compared to the trifluoromethyl group. Therefore, the reactivity of the C=C double bond is moderately restricted. Due to such a chemical structure, the novel compound of the present invention has the following characteristics: it is a liquid at room temperature and pressure, has self-extinguishing properties, can be used in a chemically stable state, and on the other hand, can be recovered as a low molecular weight compound after use by cleaving the C=C double bond. Due to such characteristics, HFO-1447 is considered useful as an additive for electrolytes. [Application of HFO-1447 in non-aqueous electrolyte] As described above, the inventors have newly discovered that HFO-1447 represented by formula (1) of the present invention forms a high-quality coating at the interface between the positive electrode and the negative electrode of a secondary battery, and can provide excellent battery characteristics. In addition, HFO-1447 has the following chemical structural characteristics: it is a liquid at room temperature and pressure, has self-extinguishing properties, can be used in a chemically stable state, and can be recovered as a low-molecular compound after use by cleavage of the C=C double bond. HFO-1447 exists in the geometrical isomers of E-isomer and Z-isomer. In the use of the novel electrolyte of the present invention, any of the E-isomer, the Z-isomer and a mixture of the two can be used. When HFO-1447 is used as an additive for an electrolyte of a secondary battery, it is preferably added to the electrolyte in an amount of 0.005 to 10 wt %, more preferably 0.1 to 7.5 wt %, and most preferably 1 to 5 wt %, based on 100 wt % of the entire electrolyte. As a preferred compounding composition of the electrolyte solution to which HFO-1447 is added, for example, the following composition can be mentioned. (Range of composition of electrolyte) (1) Non-aqueous organic solvent: the remainder As non-aqueous organic solvent, there is no particular limitation, for example, carbonate solvents such as ethylene carbonate and ethyl methyl carbonate, linear carbonate, phosphoric acid ester, cyclic ether, linear ether, lactone compound, linear ester, nitrile compound, amide compound, sulfone compound etc. can be enumerated. Among these organic solvents, from the aspect that is usually used as lithium secondary battery organic solvent, preferred carbonate solvent. (2) Electrolyte: The amount of electrolyte is preferably 0.1 to 2 mol / L, more preferably 0.15 to 1.8 mol / L, and most preferably 0.3 to 1.2 mol / L relative to the volume of the solvent. The electrolyte is not particularly limited, and examples thereof include lithium hexafluorophosphate (LiPF 6 ), lithium boron fluoride (LiBF 4 ), lithium trifluoromethanesulfonate (LiCF 3 SO 3 )、LiBF 3 CF 3 , LiBF 3 C 2 F 5 ,LiC 2 F 5 SO 3 ,LiC 3 F 7 SO 3 ,LiC 4 F 9 SO 3 、LiN(SO 2 F) 2 、LiN(CF 3 SO 2 ) 2 、LiN(C 2 F 5 SO 2 ) 2 、LiN(C 2 F 5 SO 2 ) 2 、LiN(CF 3 SO 2 )(CF 3 CO), LiN(CF 3 SO 2 )(C 2 F 5 SO 2 )、LiC(CF3 SO 2 ) 3 Fluorine electrolytes such as LiPF4 and LiP6 are preferred in terms of improving the safety and stability, conductivity and cycle characteristics of non-aqueous electrolytes. 6 . (3) HFO-1447: When the entire electrolyte solution is taken as 100 wt %, HFO-1447 is preferably added to the electrolyte solution in an amount of 0.005 to 10 wt %, more preferably 0.1 to 7.5 wt %, and most preferably 1 to 5 wt %. (4) Any other additive components (fluoroethyl carbonate (FEC), vinylene carbonate (VC), lithium difluorophosphate, etc.): When the entire electrolyte is set to 100 weight%, they are added to the electrolyte in an amount of 0.005 to 10 weight%, more preferably 0.1 to 7.5 weight%, and most preferably 1 to 5 weight%. Example [Production Example 1] HFO-1447 used for evaluation of battery characteristics was produced by the following production method. (a) SbCl 5 Synthesis of 3-chloro-1,1,1,3,5,5,5-heptafluoropentane (7F) in the presence of a catalyst at low temperature 119.0 g (0.56 mol) of 3-chloro-1,1,1,5,5,5-hexafluoro-2-pentene (HCFO-1446) was added to a 100 ml PFA (perfluoroalkoxyalkane) reactor equipped with a thermometer, a -20°C refrigeration cycle condenser, and an inlet tube. 12.3 g (0.61 mol, 1.1 eq) of anhydrous HF (liquid) was introduced while stirring the reaction liquid at -10°C. Next, SbCl was added 5 4.09 g (13.7 mmol, 2.5 mol%) was added and stirred at 0°C for 48 hours. After stirring for 48 hours, 10 g of water was added under cooling at 0°C to stop the reaction. The reaction solution was transferred to a separatory funnel for separation, and 130.29 g of an organic layer containing 3-chloro-1,1,1,3,5,5,5-heptafluoropentene was quantitatively obtained with a GC purity of 99%. (b) Dehydrochlorination of 3-chloro-1,1,1,3,5,5,5-heptafluoropentane using activated carbon catalyst Synthesis of 5,5,5-heptafluoro-2-pentene For the catalyst tower (φ20.0×400mm) filled with activated carbon pellets (Egret C2X4 / 6-2) as the reactor Figure 1The device was heated at 250°C in the catalyst tower and 150°C in the evaporator, and nitrogen was circulated at 63 SCCM. At the same time, 3-chloro-1,1,1,3,5,5,5-heptafluoropentane (HCFC-457) was supplied at 25.7 ml / h (2.80 mmol / min, 63 SCCM) to make HCFC-457 react with N 2 The flow rate of the mixed gas was 125 SCCM, and the product was collected in a collection tank filled with 300 g of ice water cooled to -2°C. The pump was stopped 47 minutes after the HCFC-457 was supplied, and 23.22 g of the organic layer was recovered from the collection tank after no white smoke was observed in the collection tank. The recovered organic phase was quantified by NMR, and the results showed that no (ND) propadiene compounds and no (ND) HFC-458 were detected. The composition was 40.8% (E)-1,1,1,3,5,5,5-heptafluoro-2-pentene, 57.2% (Z)-1,1,1,3,5,5,5-heptafluoro-2-pentene, and 2.0% HCFC-457. 1,1,1,3,5,5,5-heptafluoro-2-pentene (a mixture of E and Z forms) was obtained with a conversion rate of 98% and a selectivity of >99%. (c)( b) Distillation purification of 1,1,1,3,5,5,5-heptafluoro-2-pentene obtained 150.0 g of a crude liquid with a composition of (E)-HFO-1447 / (Z)-HFO-1447 / propylene compound / HFC-458 / HCFC-457=40.8% / 57.2% / ND / ND / 2.0% was purified by distillation at a reflux ratio of 100 / 1 in a distillation tower of KIRIYAMAPAC (filler: SUS mesh) having 10 theoretical stages. As a result, 55.0 g of (E)-HFO-1447 with a GC purity of >99% was obtained with a yield of 90% (the remaining 10% of the E-form was obtained as a low-purity fraction), and 80.7 g of (Z)-HFO-1447 with a GC purity of >99% was obtained with a yield of 94% (the remaining 6% of the Z-form was obtained as a low-purity fraction). [Battery evaluation] In order to confirm that HFO-1447 has the effect of forming a high-quality coating in a non-aqueous electrolyte, a non-aqueous electrolyte secondary battery using a non-aqueous electrolyte containing HFO-1447 was prepared. Figure 1 Evaluation tests were carried out on the nonaqueous electrolyte secondary battery of the stacked battery shown. <Production steps> [Structure of the battery used] The cross-sectional structure of the laminated battery used in this evaluation test is shown in FIG. Figure 1In the laminated battery, a positive electrode material 1 is applied to a positive electrode collector 2, and a positive electrode tab 3 extending from the positive electrode collector 2 can be electrically connected to a wiring from a measuring device by a fixture, a negative electrode material 5 is applied to a negative electrode collector 6, and a negative electrode tab 7 extending from the negative electrode collector 6 can be electrically connected to a wiring from a measuring device by a fixture, and a separator 4 is arranged between the positive electrode material 1 and the negative electrode material 5. Each component is a flat rectangular shape, and is arranged in layers in the order of the positive electrode collector 2, the positive electrode material 1, the separator 4, the negative electrode material 5, and the negative electrode collector 6, and is contained in a laminated outer package 8. [Battery components used] The positive electrode uses a lithium nickel cobalt manganese oxide (NCM111) electrode coated on an aluminum current collector, and the negative electrode uses an artificial graphite electrode coated on a nickel current collector. The thickness of the positive electrode material (electrode coating part) is 53μm, and the thickness of the negative electrode material is about 56μm. The separator is a polypropylene microporous membrane (manufactured by Celgard; trade name "Celgard#2400") cut into 5cm×6.5cm. The laminated outer package is folded in half to form 11cm×20cm. Figure 1 The stacked battery is made in a structured manner. [Battery Assembly] In the above-mentioned laminated battery, NCM111 is used for the positive electrode and artificial graphite is used for the negative electrode, which are cut into a specified size for use. The tabs for clamping the wide-mouth clamp are welded to each electrode, and a separator is clamped between the positive electrode and the negative electrode, and the laminated battery is placed and dried at 100°C for 1 hour. Then, 0.5 ml of the electrolyte containing HFO-1447 synthesized in Preparation Example 1 is injected into the Ar glove box, and the laminated battery is encapsulated in a vacuum state using a laminator. [Example 1] In a non-aqueous solvent prepared by mixing ethylene carbonate (EC) and ethyl methyl carbonate (EMC) at a volume ratio of EC:EMC=3:7, lithium hexafluorophosphate (LiPF) as an electrolyte was dissolved at a ratio of 1 mol / L. 6 , assuming that the entire electrolyte solution is 100 wt %, 1 wt % of HFO-1447(Z) synthesized and purified in Preparation Example 1 was added to the obtained solution to prepare a non-aqueous electrolyte solution, Figure 1 The stacked battery shown is a non-aqueous electrolyte secondary battery. [Example 2] In a non-aqueous solvent prepared by mixing ethylene carbonate (EC) and ethyl methyl carbonate (EMC) at a volume ratio of EC:EMC=3:7, lithium hexafluorophosphate (LiPF) as an electrolyte was dissolved at a ratio of 1 mol / L. 6In the obtained solution, assuming that the entire electrolyte solution is 100 wt %, 2.5 wt % of HFO-1447 (Z) synthesized and purified in Preparation Example 1 is added to prepare a non-aqueous electrolyte solution, Figure 1 The stacked battery shown is a non-aqueous electrolyte secondary battery. [Example 3] In a non-aqueous solvent prepared by mixing ethylene carbonate (EC) and ethyl methyl carbonate (EMC) at a volume ratio of EC:EMC=3:7, lithium hexafluorophosphate (LiPF) as an electrolyte was dissolved at a ratio of 1 mol / L. 6 In the obtained solution, assuming that the entire electrolyte solution is 100 wt %, 5 wt % of HFO-1447 (Z) synthesized and purified in Preparation Example 1 is added to prepare a non-aqueous electrolyte solution, Figure 1 The stacked battery shown is a non-aqueous electrolyte secondary battery. [Example 4] In a non-aqueous solvent prepared by mixing ethylene carbonate (EC) and ethyl methyl carbonate (EMC) at a volume ratio of EC:EMC=3:7, lithium hexafluorophosphate (LiPF) as an electrolyte was dissolved at a ratio of 1 mol / L. 6 In the obtained solution, assuming that the entire electrolyte solution is 100 wt %, 10 wt % of HFO-1447 (Z) synthesized and purified in Preparation Example 1 is added to prepare a non-aqueous electrolyte solution, Figure 1 The stacked battery shown is a non-aqueous electrolyte secondary battery. [Comparative Example 1] In a non-aqueous solvent prepared by mixing ethylene carbonate (EC) and ethyl methyl carbonate (EMC) at a volume ratio of EC:EMC=3:7, lithium hexafluorophosphate (LiPF) as an electrolyte was dissolved at a ratio of 1 mol / L. 6 And prepare non-aqueous electrolyte, make Figure 1 The non-aqueous electrolyte secondary battery of the stacked battery shown is an example of an electrolyte to which the HFO-1447 synthesized in Production Example 1 is not added. [Measurement method] In order to remove the initial gas, the secondary batteries made using the non-aqueous electrolytes of Examples 1 to 4 and Comparative Example 1 were charged at 60°C at a constant current of 0.2C to 30% of the theoretical capacity and stored for 15 hours. st After charging), the secondary batteries made with the aged non-aqueous electrolytes of Examples 1 to 4 and Comparative Example 1 were placed in an Ar glove box, the ends of the stacked batteries were cut off, exhaust was performed, and vacuum was again drawn with a laminator, and the stacked batteries were packaged in this state. (Exhaust) Next, the secondary batteries made using the non-aqueous electrolytes of Examples 1 to 4 and Comparative Example 1 were charged to 4.2 V at 25°C and 0.2 C constant current, and then charged to 1 / 50 of the theoretical capacity of the active material weight with a charge termination C current of 0.02 C, and then discharged to 2.75 V at a constant current of 0.2 C. (2 nd , 3 rd Charge and discharge) Next, the secondary batteries made using the non-aqueous electrolytes of Examples 1 to 4 and Comparative Example 1 were charged to 4.2V at 25°C and 1C constant current, and then the charge termination C current was set to 0.1C, and the constant voltage was charged to a current value of 1 / 10 of the theoretical capacity of the active material weight, and then discharged to 50% of the theoretical capacity at a constant current of 1C. (4 th Charge and discharge) Then, the secondary batteries made using the non-aqueous electrolytes of the above-mentioned Examples 1 to 4 and Comparative Example 1 were charged to 4.2V at 45°C and 1C constant current, and then the charge termination C current was set to 0.1C, and constant voltage charged to a current value of 1 / 10 of the theoretical capacity of the active material weight, and then discharged to 2.75V at a constant current of 1C. (5 th ~Charge and discharge) In addition, every 100 cycles, the battery was charged at a constant current of 0.2C to 4.2V, and then the charge termination C current was set to 0.1C, and the battery was charged at a constant voltage to a current value of 1 / 10 of the theoretical capacity of the active material weight, and then discharged at a constant current of 1C to 2.75V. Based on the first (5 th ) discharge capacity D 5 , the xth discharge capacity D x (x=105, 205, 305, 405), the capacity retention rate (%) after the xth cycle of the secondary batteries prepared using the nonaqueous electrolyte solutions of Examples 1 to 4 and Comparative Example 1 was calculated by the following formula, and the results are shown in Table 1. Capacity maintenance rate (%) = (D x / D 5 )×100 In addition, the sum of the discharge capacities at the respective cycles up to the 405th cycle is shown in Table 2 as the total discharge capacity. [Table 1] [Table 2] According to Table 1, the capacity retention rate of Examples 1 to 4 in the 105th cycle is higher than that of Comparative Example 1, and the cycle characteristics are excellent. During the period from the 105th cycle to the 405th cycle, the capacity retention rate of each Example and Comparative Example further differs, and it can be seen that 1,1,1,3,5,5,5-heptafluoro-2-pentene (HFO-1447) shown in formula (1) helps to maintain the discharge capacity after long-term cycling. It can be seen that HFO-1447 forms a high-quality film at the interface between the positive electrode and the negative electrode, which can provide excellent battery characteristics. In addition, it can be seen that the capacity retention rate increases as the addition amount of HFO-1447 increases from 1 wt% to 10 wt%. It can also be seen from Table 2 that the total discharge capacity is the highest when the addition amount of HFO-1447 is 2.5 wt%. It can also be seen from these findings that by adjusting the addition amount of HFO-1447, the capacity retention rate and the total discharge capacity can be appropriately controlled. [Examples 5-6] The isomer evaluation of HFO-1447 was carried out at an addition amount of 2.5 wt % at which the total discharge capacity at the 405th cycle was the highest. In a non-aqueous solvent prepared by mixing ethylene carbonate (EC) and ethyl methyl carbonate (EMC) at a volume ratio of EC:EMC=3:7, lithium hexafluorophosphate (LiPF) as an electrolyte was dissolved at a ratio of 1 mol / L. 6 In the obtained solution, for each example, 2.5 wt% of HFO-1447 (E) (Example 5) synthesized and purified in Preparation Example 1 and HFO-1447 (E / Z) (Example 6; an isomer mixture of E and Z, with a molar ratio of E:Z = 4:6) were added to prepare the non-aqueous electrolyte of each example, assuming that the entire electrolyte was 100 wt%. Figure 1 The non-aqueous electrolyte secondary battery of the stacked battery shown. It should be noted that the data of HFO-1447(Z) is compared with the data of Example 2. The capacity retention rate (%) of the secondary batteries prepared using the nonaqueous electrolytes of Examples 5 to 6 after the xth cycle was determined in the same manner as in Example 1, and the results are shown in Table 3. In addition, the total discharge capacity of each cycle up to the 405th cycle is shown in Table 4 as the total discharge capacity. [Table 3] [Table 4] As shown in Table 3, no significant difference was observed in the capacity retention rate according to the isomer ratio of the E-form and the Z-form of HFO-1447. As shown in Table 4, no significant difference was observed in the capacity retention rate according to the isomer ratio of the E-form and the Z-form of HFO-1447, but it was reflected that the capacity retention rate of the Z-form was slightly higher. If the number of cycles increased, the total discharge capacity of HFO-1447 showed a tendency that the Z-form was the highest. It can also be seen that: since the boiling point is 52°C for the E-form and 78°C for the Z-form, the boiling point of the additive can be changed by 26°C even with the same battery characteristics.
Claims
1. Use of 1,1,1,3,5,5,5-heptafluoro-2-pentene in a non-aqueous electrolyte.
2. The use according to claim 1, wherein The non-aqueous electrolyte is a non-aqueous electrolyte for a secondary battery.
3. The use according to claim 2, wherein The secondary battery is a lithium ion secondary battery.
4. The use according to claim 1, wherein The non-aqueous electrolyte comprises: Electrolytes, 1,1,1,3,5,5,5-heptafluoro-2-pentene, and Non-aqueous organic solvents.
5. The use according to claim 4, wherein The electrolyte is lithium hexafluorophosphate, and the non-aqueous organic solvent is a carbonate solvent.
6. The use according to any one of claims 1 to 5, wherein The 1,1,1,3,5,5,5-heptafluoro-2-pentene is (E)-1,1,1,3,5,5,5-heptafluoro-2-pentene, (Z)-1,1,1,3,5,5,5-heptafluoro-2-pentene, or a mixture of (E)-1,1,1,3,5,5,5-heptafluoro-2-pentene and (Z)-1,1,1,3,5,5,5-heptafluoro-2-pentene.
7. A non-aqueous electrolyte comprising: Electrolytes, 1,1,1,3,5,5,5-heptafluoro-2-pentene, and Non-aqueous organic solvents.
8. The non-aqueous electrolyte according to claim 7, wherein The electrolyte is lithium hexafluorophosphate, and the non-aqueous organic solvent is a carbonate solvent.
9. The nonaqueous electrolyte according to claim 7, wherein The 1,1,1,3,5,5,5-heptafluoro-2-pentene is (E)-1,1,1,3,5,5,5-heptafluoro-2-pentene, (Z)-1,1,1,3,5,5,5-heptafluoro-2-pentene, or a mixture of (E)-1,1,1,3,5,5,5-heptafluoro-2-pentene and (Z)-1,1,1,3,5,5,5-heptafluoro-2-pentene. 10 . A secondary battery comprising the nonaqueous electrolyte according to claim 7 .
11. The secondary battery according to claim 10, wherein The secondary battery is a lithium ion secondary battery.