Battery cells and devices, electric devices, energy storage devices and systems, charging networks
By using graphite with high BET specific surface area and graphite materials with specific interlayer spacing in battery cells, combined with large cross-sectional area electrode terminals and multi-level stepped sealing structure, the sealing failure problem during thermal runaway of battery cells is solved, thereby improving the structural reliability and service life of battery cells.
Patent Information
- Application Number
- CN202511056287.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2025-07-30
- Publication Date
- 2025-11-25
- Estimated Expiration
- 2045-07-30
AI Technical Summary
When a battery cell experiences thermal runaway, the internal pressure increases rapidly, leading to seal failure and affecting the sealing performance of the battery casing structure.
The graphite has a BET specific surface area greater than 2.25 m²/g and an interlayer spacing variation rate of 8.3%≤M≤9.1%. Combined with the fact that the cross-sectional area of the first connection part of the electrode terminal is larger than that of the mounting hole, and with the addition of a sealing ring and a multi-stage stepped structure, the sealing reliability is enhanced.