Production process of tetramethyl piperidone and preparation method of catalyst of tetramethyl piperidone

The catalyst prepared by the composite sol-gel method solves the problems of low catalyst activity and poor stability, and achieves high yield and high purity of tetramethylpiperidinone, thus extending the catalyst's service life.

CN122079869APending Publication Date: 2026-05-26WEIFANG YUANLI NEW MATERIAL CO LTD
0 Cites 0 Cited by

Patent Information

Application Number
CN202512044274.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-12-31
Publication Date
2026-05-26

AI Technical Summary

Technical Problem

In the existing technology, the production process of tetramethylpiperidinone has low catalyst activity, weak binding force between active components and support, poor catalyst stability, poor product yield and purity, and short catalytic life.

Method used

The catalyst was prepared by a composite sol method, which formed a composite sol with components such as aluminum isopropoxide, tetraethyl orthosilicate, cerium nitrate and zirconium nitrate. Combined with the post-treatment of ammonium dihydrogen phosphate and ammonium molybdate, POX bonds were gradually formed during the calcination process to ensure uniform dispersion and porous structure of the active components. Alumina and silica were used as supports to form multi-level channels, which improved the stability and selectivity of the catalyst.

Benefits of technology

The catalyst's stability and lifespan were improved, and the yield and purity of tetramethylpiperidinone were significantly increased. After 1200 hours of continuous operation, the yield was 91.1-92.5% and the purity was 98.34-98.85%.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention provides a production process of tetramethyl piperidone and a preparation method of a catalyst of the tetramethyl piperidone, and belongs to the technical field of tetramethyl piperidone. The preparation method of the catalyst comprises the following steps: preparing composite sol, preparing catalyst precursor powder, post-treating and roasting. The preparation method comprises the following steps: preparing catalyst precursor powder, namely adding cerium nitrate and zirconium nitrate into deionized water, adding tartaric acid, uniformly stirring, adding into the composite sol, controlling the adding rate to be 1.5-2.0 g / min and the pH value to be 8.8-9.2, keeping the temperature at 55-60 DEG C for 4.0 hours after adding, washing, and freeze-drying to obtain the catalyst precursor powder; the tetramethyl piperidone obtained by the production process is high in yield and purity, and the service life of the catalyst is long.
Need to check novelty before this filing date? Find Prior Art