Annular silver-plated frame for improving layering of crystal grain adhesive film

By setting slots in the silver-plated area of ​​the ring silver-plated frame, the problem of grain adhesion film and frame layering caused by hollows in the QFN package is solved, the quality and yield of the product are improved, and the normal pressure zone and pins are ensured. Wire.

CN222088587UActive Publication Date: 2024-11-29JIANGSU SILICON INTEGRITY SEMICON TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323529848.7
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-25
Publication Date
2024-11-29
Estimated Expiration
2033-12-25

AI Technical Summary

Technical Problem

In the prior art, the ring silver-plated frame of QFN packaged ring silver-plated frame has a hollow due to the pressure-plated silver-plated area of ​​the grain paste film, which leads to layering of the grain paste film and the frame, causing quality risks and yield losses. How to discharge the hole is an urgent solution. The problem.

Method used

Design an annular silver-plating frame that improves the layering of grain adhesion film. By setting grooves in the silver-plating area, grooves can be achieved through etching or laser technology, with a depth of 1/3 to 1/2 of the thickness of the silver-plating layer. The width is ten to fifteen times the diameter of the ground wire, and is used to discharge the voids generated by the DAF film.

Benefits of technology

It effectively avoids the layering of the grain adhesion film and frame caused by hollowing, ensures the quality and yield of the product, and the design does not affect the grounding and pin wiring of the pressing zone.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222088587U_ABST
    Figure CN222088587U_ABST
Patent Text Reader

Abstract

The utility model provides an annular silver-plated frame for improving layering of a crystal grain adhesive film, and belongs to the technical field of semiconductor packaging, the annular silver-plated frame comprises a group of frame units arranged according to a design rule, each frame unit comprises a frame substrate, and the surface of each frame substrate comprises a chip mounting area and an annular silver-plated area. The chip mounting area is located in the middle of the surface of the frame substrate, and the ring silver plating area is located around the chip mounting area; the annular silver plating area comprises silver plating edges surrounding the periphery of the chip installation area, each silver plating edge is provided with at least one open groove with a set shape and size, and the open grooves can be achieved through an existing etching or laser technology; according to the invention, the open slot is formed in the ring silver plating area, and when the DAF film generates a cavity, the cavity can be discharged from the open slot, so that the layering of the crystal grain pasting film and the frame is prevented from being influenced by the cavity.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of semiconductor packaging, and in particular to a ring-shaped silver-plated frame for improving the delamination of a crystal grain pasting film. Background Art

[0002] As the types and categories of packaged products continue to improve, the number of silver-plated frames used for QFN packages is increasing. However, due to the silver-plated areas on the four sides of the chip of the die attach film (DAF / Die attach film) product, voids will be generated. If the voids cannot be removed, the die attach film and the frame will be delaminated. The delamination of the die attach film and the frame will cause serious quality risks and yield losses. Therefore, how to remove the voids is an urgent problem to be solved. Summary of the invention

[0003] Purpose of the invention: The purpose of the present invention is to provide a ring-plated silver-plated frame for improving the delamination of the grain pasting film, in order to address the deficiency of the prior art in that the grain pasting film and the frame are delaminated due to the presence of voids. The frame is provided with slots to discharge the voids and reduce the occurrence of delamination.

[0004] Technical solution: The present invention discloses a ring-shaped silver-plated frame for improving the delamination of a die-bonding film. The ring-shaped silver-plated frame includes a group of frame units arranged according to design rules. The frame units include a frame substrate. The surface of the frame substrate includes a chip mounting area and a ring-shaped silver-plated area. The chip mounting area is located in the middle of the surface of the frame substrate, and the ring-shaped silver-plated area is located around the chip mounting area.

[0005] The silver-plated ring area includes silver-plated edges surrounding the chip mounting area. Each silver-plated edge is provided with at least one slot of a set shape and size. The slots can be realized by existing etching or laser processes. The slots can be any customized shape, not necessarily rectangular, and the number of slots can be adjusted according to actual product requirements.

[0006] Furthermore, the depth of the groove is 1 / 3 to 1 / 2 of the thickness of the silver layer in the silver-plated ring area, which does not affect the grounding at the pressing area on the frame base island; and since this design only grooves the silver-plated ring area, it does not affect the pin bonding.

[0007] Furthermore, the width of the slot is ten to fifteen times the diameter of the ground wire, and this width leaves enough space for the bottom line of the silver-plated area and deviation.

[0008] Furthermore, a chip is mounted on the chip mounting area, and a die pasting film, namely, a DAF film, is arranged between the chip and the chip mounting area. When voids are generated in the DAF film, the voids can be discharged from the grooves.

[0009] Furthermore, the chip is provided with pressure zones distributed according to design rules.

[0010] Further, the pressing area is connected to the corresponding area through a ground line.

[0011] Furthermore, pins are also included.

[0012] Beneficial effects: Compared with the prior art, the advantages of the present invention are:

[0013] (1) The present invention provides a groove in the ring silver-plated area, and when voids are generated in the DAF film, the voids can be discharged from the groove, thereby preventing the voids from affecting the delamination of the die bonding film and the frame;

[0014] (2) The groove depth of the present invention is 1 / 3 to 1 / 2 of the thickness of the silver-plated layer in the ring silver-plated area, and this thickness does not affect the grounding of the ground wire at the pressing area on the frame base island; and because this design only grooves the ring silver-plated area, it does not affect the pin wiring;

[0015] (3) The slot width of the present invention is ten to fifteen times the diameter of the ground wire, and this width leaves enough space for the bottom line of the silver-plated area and deviation. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 It is a schematic diagram of the structure of the present invention;

[0017] Figure 2 It is a schematic diagram of the slotting structure. DETAILED DESCRIPTION

[0018] The technical solution of the present invention is described in detail below with reference to the accompanying drawings, but the protection scope of the present invention is not limited to the embodiments.

[0019] like Figure 1 A ring-shaped silver-plated frame for improving the delamination of a die bonding film is shown. The ring-shaped silver-plated frame includes a group of frame units arranged according to design rules. The frame units include a frame substrate 1. The surface of the frame substrate 1 includes a chip mounting area and a ring-shaped silver-plated area 6. The chip mounting area is located in the middle of the surface of the frame substrate 1. A chip 4 is mounted on the chip mounting area. A die bonding film 5 is arranged between the chip 4 and the chip mounting area. A pressing area 7 is distributed on the chip 4 according to the design rules. The pressing area 7 is connected to the corresponding area through a ground wire 3; and it also includes a pin 8.

[0020] The silver-plated ring area 6 is located around the chip mounting area. The silver-plated ring area 6 includes a silver-plated edge surrounding the chip mounting area. Three slots 2 of set shapes and sizes are set on each silver-plated edge by etching; Figure 2 As shown, the depth of the slot 2 is 1 / 2 of the thickness of the silver-plated layer of the silver-plated ring area 6, and the width of the slot 2 is ten times the wire diameter of the ground wire.

[0021] When using a die-bonding film on a ring-plated silver frame for chip bonding, bubbles and voids are easily generated on the bonding surface. The bubbles will be eliminated through the post-molding (Molding) and post-molding baking (PMC) processes. The principle is that under high temperature and high pressure environment, when the temperature and pressure increase, the solubility of gas in liquid will increase, and gases such as nitrogen and oxygen in the air will also dissolve in water and other liquids. Most polymer materials contain a certain amount of liquid resin and other liquid solvents. The materials need to be cured by baking (Cure). When heated and pressurized to a certain degree, the liquid will evaporate (outgas), and the gas dissolved in it will be taken away at this time. The gas can be discharged through the slot position of the ring-plated silver area, thereby eliminating the bubbles and voids generated on the bonding surface.

[0022] This embodiment can prevent the problem of reliability failure caused by delamination of the die attach film, and improve the quality and yield of the product; moreover, this design is not limited to the QFN die attach film (DAF / Die attach film) pressure ring silver-plated area chip packaging structure, but is also applicable to chip packaging structures of PDIP / SOT / LQFP / SOP series lead frames, and is also applicable to chip packaging structures using epoxy resin.

[0023] As described above, although the present invention has been shown and described with reference to specific preferred embodiments, it should not be construed as limiting the present invention itself. Various changes in form and details may be made without departing from the spirit and scope of the present invention as defined in the appended claims.

Claims

1. A ring-shaped silver-plated frame for improving the delamination of a die-bonding film, the ring-shaped silver-plated frame comprising a group of frame units arranged according to design rules, characterized in that: The frame unit comprises a frame substrate (1), the surface of the frame substrate (1) comprises a chip mounting area and a ring silver-plated area (6), the chip mounting area is located in the middle of the surface of the frame substrate (1), and the ring silver-plated area (6) is located around the chip mounting area; The silver-plated ring area (6) comprises silver-plated edges surrounding the chip mounting area, and each silver-plated edge is provided with at least one slot (2) of a set shape and size.

2. A ring-shaped silver-plated frame for improving the delamination of a die-bonding film according to claim 1, characterized in that: The depth of the groove (2) is 1 / 3 to 1 / 2 of the thickness of the silver-plated layer of the ring silver-plated area (6).

3. A ring-shaped silver-plated frame for improving the delamination of a die-bonding film according to claim 1 or 2, characterized in that: The width of the slot (2) is ten to fifteen times the diameter of the ground wire.

4. The ring-shaped silver-plated frame for improving the delamination of the die-bonding film according to claim 3, characterized in that: A chip (4) is mounted on the chip mounting area, and a crystal grain adhesive film (5) is provided between the chip (4) and the chip mounting area.

5. The ring-shaped silver-plated frame for improving the delamination of the die-bonding film according to claim 4, characterized in that: The chip (4) is provided with pressure areas (7) distributed according to design rules.

6. The ring-shaped silver-plated frame for improving the delamination of the die-bonding film according to claim 5, characterized in that: The pressing area (7) is connected to a corresponding area via a ground wire (3).

7. A ring-shaped silver-plated frame for improving the delamination of a die-bonding film according to any one of claims 1, 2, 4, 5, and 6, characterized in that: Also included is a pin (8).