SFRCP steel skeleton fiber reinforced resin pipe

By adopting a multi-layer structure reinforcement layer design and reverse spiral winding of galvanized steel wire and glass fibers in the pipeline, the problem of reduced pressure bearing capacity of the pipeline is solved, and the stable pressure bearing effect is achieved under high pressure conditions.

CN222122458UActive Publication Date: 2024-12-06CHONGQING XIZHOU PIPE IND CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420335676.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-23
Publication Date
2024-12-06
Estimated Expiration
2034-02-23

AI Technical Summary

Technical Problem

The mesh structures of galvanized steel wire and glass fiber in existing pipes are prone to slip when under pressure, resulting in a reduced pressure bearing capacity.

Method used

Design of reinforcement layer with multi-layer structure, including cured bottom layer, cured interlayer and cured surface layer, galvanized steel wire and glass fibers are reverse spiral to form a mesh structure, and the outer layer is coated with flame retardant antistatic polyethylene material , to stabilize the fiber position.

Benefits of technology

Effectively prevent fiber slippage, improve the pressure bearing capacity of the pipeline under high pressure conditions, and ensure long-term stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222122458U_ABST
    Figure CN222122458U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of transportation pipelines, in particular to an SFRCP steel framework fiber reinforced resin pipe which comprises a pipe body, a reinforcing layer and a wrapping outer layer, the reinforcing layer wraps the outer layer of the pipe body, and the wrapping outer layer wraps the outer layer of the reinforcing layer. The reinforcing layer comprises a curing bottom layer, a curing interlayer, a curing surface layer and reinforcing fibers, the curing bottom layer wraps the outer surface of the pipe body, one kind of reinforcing fibers is wound on the surface of the curing bottom layer, the curing interlayer wraps the outer layer of the reinforcing fibers, the other kind of reinforcing fibers wraps the outer side of the curing interlayer, and the curing surface layer wraps the outer side of the curing interlayer. The outer layer of the reinforced fiber is coated with the curing surface layer, and the outer layer of the curing surface layer is coated with the coating outer layer. The reinforced fibers are not prone to position slippage when the reinforced fibers bear large pressure at the same time, and it is guaranteed that the pressure bearing capacity of the pipeline is stable for a long time.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of transportation pipelines, in particular to a SFRCP steel skeleton fiber reinforced resin pipe. Background Art

[0002] SFRCP, or steel fiber reinforced polyethylene composite pressure pipe, is a composite pipe formed by melting and compounding with polyethylene as the matrix, ultra-fine steel fibers with a strength of 2500Mpa and a diameter of less than 0.4mm, and a mesh skeleton formed by continuous spiral winding on the left and right as the reinforcement, and polyethylene as the outer layer. The pipe is suitable for outdoor underground drainage, reclaimed water, fire water transportation, oil collection and injection, industrial slurry transportation, high-pressure water supply system, etc., where the medium temperature does not exceed 80℃.

[0003] Chinese patent CN103104754B discloses an anti-static flame-retardant steel skeleton fiber-reinforced resin pipe and its preparation process. Its main technical features are: it includes a pipe body, and the pipe body is composed of an impermeable flame-retardant conductive inner lining layer and a pressure-bearing flame-retardant conductive structural layer from the inside to the outside, wherein the impermeable flame-retardant conductive inner lining layer includes glass fibers cured in the inner matrix, and the pressure-bearing flame-retardant conductive structural layer includes an outer matrix synchronously wound with galvanized steel wire coated with epoxy resin on the outer surface and glass fiber direct untwisted roving.

[0004] The mesh skeleton composed of galvanized steel wire and glass fiber steel wire in the existing pipeline is made of several independent steel wires wound onto the pipeline through special molding equipment, and then the solidified components are heated and demolded. Several layers of wire mesh can be repeatedly wound. There is a mesh free state similar to a woven structure between the steel wires, and the actual layers are in direct contact with each other. For pipes with this structure, when the inside of the pipeline is subjected to a certain pressure, the mesh structure steel wires in a free state will slip in position, causing the steel wires in some positions to slip and squeeze together, and forming larger mesh holes without wires in some positions, resulting in a significant reduction in the pressure-bearing capacity of the pipe. Utility Model Content

[0005] The utility model aims to solve the problem in the prior art that when a certain pressure is applied inside a pipe, the free mesh structure steel wires will slip, causing the steel wires to slip and squeeze together at some positions, and forming larger mesh holes without steel wires at some positions, which leads to a significant reduction in the pressure bearing capacity of the pipe. The utility model proposes a SFRCP steel skeleton fiber reinforced resin pipe to solve the problem.

[0006] In order to achieve the above purpose, the utility model adopts the following technical solutions:

[0007] An SFRCP steel skeleton fiber reinforced resin pipe, comprising a pipe body, a reinforcement layer and a coating outer layer, wherein the reinforcement layer is coated on the outer layer of the pipe body, and the coating outer layer is coated on the outer layer of the reinforcement layer;

[0008] The reinforcement layer includes a cured bottom layer, a cured interlayer, a cured surface layer and reinforcing fibers. The cured bottom layer is coated on the outer surface of the tube body, one type of reinforcing fibers is wound on the surface of the cured bottom layer, the cured interlayer is coated on the outer layer of the reinforcing fibers, another type of reinforcing fibers is coated on the outside of the cured interlayer, the cured surface layer is coated on the outer layer of the reinforcing fibers, and the coated outer layer is coated on the outer layer of the cured surface layer.

[0009] Preferably, the reinforcing fibers are epoxy resin galvanized steel wire and glass fiber direct untwisted roving respectively.

[0010] Preferably, the adjacent reinforcing fibers are spirally wound on the tube body in opposite directions, and the winding densities of the reinforcing fibers twice are the same.

[0011] Preferably, the outer coating layer is made of flame-retardant and antistatic polyethylene material.

[0012] Preferably, the cured bottom layer, the cured interlayer and the cured surface layer are flame retardant composite materials.

[0013] Preferably, the epoxy resin galvanized steel wire can be replaced by a steel strip.

[0014] In the utility model, when producing the reinforcement layer, the curing component is first coated on the surface of the pipe body, and then the reinforcing fibers are wound on the surface of the curing component, and then the curing component is cured to form a cured bottom layer, thereby limiting the reinforcing fibers. Then, the curing component is coated on the surface of the reinforcing fibers, and then the reinforcing fibers are wound. After curing, a cured interlayer is formed between the two layers of reinforcing fibers, and the cured interlayer is very thin. After the winding is completed, the curing component is coated on the surface of the reinforcing fibers. The curing component for forming the cured interlayer or the cured surface layer is selected according to actual production needs. Multiple layers can be wound, and the outermost layer forms a cured surface layer. The reinforcing fibers in the reinforcement layer produced by this production method are also distributed in the pipeline in a mesh structure. There is a cured interlayer between the two layers of reinforcing fibers. When subjected to a large pressure at the same time, the reinforcing fibers are not easy to slip in position, thereby ensuring the long-term stability of the pressure bearing capacity of the pipeline. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 This is a schematic diagram of the inner layer structure of a SFRCP steel skeleton fiber reinforced resin pipe proposed in the utility model;

[0016] Figure 2 This is a cross-sectional view of a SFRCP steel skeleton fiber reinforced resin pipe proposed by the utility model;

[0017] Figure 3 for Figure 2 A partial enlarged view of middle A.

[0018] In the figure: 1 tube body, 2 reinforcement layer, 21 cured bottom layer, 22 cured interlayer, 23 cured surface layer, 24 reinforcement fiber, 3 coating outer layer. DETAILED DESCRIPTION

[0019] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all of the embodiments.

[0020] Reference Figure 1-Figure 3 , a SFRCP steel skeleton fiber reinforced resin pipe, comprising a pipe body 1, a reinforcement layer 2 and a coating outer layer 3, wherein the reinforcement layer 2 is coated on the outer layer of the pipe body 1, and the coating outer layer 3 is coated on the outer layer of the reinforcement layer 2;

[0021] The reinforcing layer 2 includes a cured bottom layer 21, a cured interlayer 22, a cured surface layer 23 and reinforcing fibers 24. The cured bottom layer 21 is coated on the outer surface of the tube body 1, one reinforcing fiber 24 is wound on the surface of the cured bottom layer 21, the cured interlayer 22 is coated on the outer layer of the reinforcing fiber 24, another reinforcing fiber 24 is coated on the outside of the cured interlayer 22, the cured surface layer 23 is coated on the outer layer of the reinforcing fiber 24, and the coated outer layer 3 is coated on the outer layer of the cured surface layer 23.

[0022] The reinforcing fibers 24 are epoxy resin galvanized steel wire and glass fiber direct untwisted roving respectively. Due to the epoxy resin coating on the outer surface and its excellent adhesion, the galvanized steel wire and the curing component containing the resin glue are not prone to delamination after curing.

[0023] The adjacent reinforcing fibers 24 are reversely spirally wound on the tube body 1, and the density of the two windings of the reinforcing fibers 24 is the same. After the reverse spiral winding, a mesh structure is formed between the reinforcing fibers.

[0024] The outer coating layer 3 is made of flame-retardant antistatic polyethylene material, which has good properties such as wear resistance, severe cold resistance, good low-temperature toughness, and chemical corrosion resistance.

[0025] The main components of the cured bottom layer 21 , the cured interlayer 22 and the cured surface layer 23 include resin glue, flame retardant and curing agent. The resin glue and the galvanized steel wire of the epoxy resin are not easy to delaminate, thereby ensuring the stability of the reinforcement layer 2 .

[0026] Epoxy resin galvanized steel wire can be replaced by steel strip, which has stronger pressure resistance. When the actual steel wire is not enough to meet the design requirements, epoxy resin galvanized steel strip can be used.

[0027] In the utility model, when the reinforcing layer 2 is produced, the curing component is first coated on the surface of the pipe body 1, and then the reinforcing fibers 24 are wound on the surface of the curing component and the curing component is cured to form a cured bottom layer 21, thereby limiting the reinforcing fibers 24. The curing component is then coated on the surface of the reinforcing fibers 24 and then the reinforcing fibers 24 are wound. After curing, a cured interlayer 22 is formed between the two layers of reinforcing fibers 24. The cured interlayer 22 is very thin. After the winding is completed, the curing component is coated on the surface of the reinforcing fibers 24. The curing component used to form the cured interlayer 22 or the cured surface layer 23 is selected according to actual production needs. Multiple layers can be wound, and the outermost layer forms the cured surface layer 23. The reinforcing fibers 24 in the reinforcing layer 2 produced by this production method are also distributed in the pipeline in a mesh structure. There is a cured interlayer 22 between the two layers of reinforcing fibers. When subjected to a large pressure at the same time, the reinforcing fibers 24 are not easy to slip in position, thereby ensuring the long-term stability of the pressure bearing capacity of the pipeline.

[0028] In general, in view of the technical problem: under the condition that the inside of the pipe is subjected to a certain pressure, the mesh structure steel wires in a free state will produce position slippage, causing the steel wires in some positions to slip and squeeze together, and forming larger mesh holes without steel wires in some positions, resulting in a significant reduction in the pressure-bearing capacity of the pipe; adopting a technical solution: adjusting the manufacturing process of the reinforcing layer 2; because the implementation process of the technical solution is: when producing the reinforcing layer 2, first apply the curing component to the surface of the pipe body 1, then wrap the reinforcing fibers 24 around the surface of the curing component, and then cure the curing component to form a cured bottom layer 21, thereby limiting the reinforcing fibers 24, and then apply the curing component on the surface of the reinforcing fibers 24, and then perform the reinforcing The strong fiber 24 is wound, and after curing, a cured interlayer 22 is formed between the two layers of reinforcing fibers 24. The cured interlayer 22 is very thin. After the winding is completed, a curing component is coated on the surface of the reinforcing fiber 24. The curing component used to form the cured interlayer 22 or the cured surface layer 23 is selected according to actual production needs. Multiple layers can be wound, and the outermost layer forms the cured surface layer 23; this will inevitably solve the technical problem, and the technical effect achieved is: the reinforcing fibers 24 in the reinforcing layer 2 produced by this production method are also distributed in the pipeline in a mesh structure, and there is a cured interlayer 22 between the two layers of reinforcing fibers. When the two layers are subjected to a large pressure at the same time, the reinforcing fibers 24 are not easy to slip, thereby ensuring the long-term stability of the pressure bearing capacity of the pipeline.

[0029] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes within the technical scope disclosed by the present invention according to the technical scheme and the utility model concept of the present invention, which should be covered by the protection scope of the present invention.

Claims

1. A SFRCP steel skeleton fiber reinforced resin pipe, comprising a pipe body (1), a reinforcement layer (2) and a coating outer layer (3), characterized in that: The reinforcing layer (2) is coated on the outer layer of the tube body (1), and the coating outer layer (3) is coated on the outer layer of the reinforcing layer (2); The reinforcing layer (2) comprises a cured bottom layer (21), a cured interlayer (22), a cured surface layer (23) and reinforcing fibers (24); the cured bottom layer (21) is coated on the outer surface of the tube body (1); one type of reinforcing fibers (24) is wound on the surface of the cured bottom layer (21); the cured interlayer (22) is coated on the outer layer of the reinforcing fibers (24); another type of reinforcing fibers (24) is coated on the outer side of the cured interlayer (22); the cured surface layer (23) is coated on the outer layer of the reinforcing fibers (24); and the coated outer layer (3) is coated on the outer layer of the cured surface layer (23).

2. The SFRCP steel skeleton fiber reinforced resin pipe according to claim 1, characterized in that: The reinforcing fibers (24) are respectively made of epoxy resin galvanized steel wire and glass fiber direct untwisted roving.

3. The SFRCP steel skeleton fiber reinforced resin pipe according to claim 1, characterized in that: The adjacent reinforcing fibers (24) are spirally wound on the tube body (1) in opposite directions, and the winding densities of the reinforcing fibers (24) are the same twice.

4. The SFRCP steel skeleton fiber reinforced resin pipe according to claim 1, characterized in that: The outer coating layer (3) is made of flame-retardant antistatic polyethylene material.

5. The SFRCP steel skeleton fiber reinforced resin pipe according to claim 1, characterized in that: The cured bottom layer (21), the cured interlayer (22) and the cured surface layer (23) are flame-retardant composite materials.

6. The SFRCP steel skeleton fiber reinforced resin pipe according to claim 2, characterized in that: The epoxy resin galvanized steel wire can be replaced by steel strip.