Thin brightness enhancement board with high adaptability

By adding adhesive and separator on thinned light-enhancing plates and cutting the main body on grid paper, the problems of low adaptability and easy damage to the existing thinned light-enhancing plates are solved, and the adaptability is improved Coordination and service life.

CN222167365UActive Publication Date: 2024-12-13REGENCY OPTICS ELECTRON CORP
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202420756626.4
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-04-12
Publication Date
2024-12-13
Estimated Expiration
2034-04-12

AI Technical Summary

Technical Problem

The existing thin-shaped light-enhancing plates have low adaptability and are difficult to adapt to a variety of lamps of different specifications. The adhesive material is easily adhered to the cutting tool during installation, affecting the service life.

Method used

A thin-shaped light-enhancing plate including a main body, an adhesive and a separator film is designed. The thickness of the adhesive is one quarter of the main body thickness. The thickness of the separator film is the same as that of the adhesive. The separator film is arranged as a PVA coated high-barrier composite film, and Draw the drawing on the grid paper and scratch it to cut the body to avoid the adhesive being exposed to the air.

Benefits of technology

The adaptability of the thinned-shaped light-enhancing plate is improved, making it easier to install, and extends its service life, avoiding adhesives to the cutting tool, enhancing operation convenience and safety.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222167365U_ABST
    Figure CN222167365U_ABST
Patent Text Reader

Abstract

The utility model discloses a thin brightness enhancement board with higher adaptability, which relates to the technical field of brightness enhancement boards, and comprises a main body, one surface of the main body is provided with a triangular prism, the lower side surface of the main body is a smooth surface, the horizontal surface of the main body is coated with an adhesive, and the thickness of the adhesive is one fourth of the thickness of the main body. A separation film is arranged at the end, away from the main body, of the other side of the adhesive, and the thickness of the separation film is the same as that of the adhesive. Compared with an existing common thinned brightness enhancement plate, the thinned brightness enhancement plate with the high adaptation degree has the advantages that before the main body is used, a drawing is drawn on the grid paper firstly, and then the separation film is engraved along the drawing through the sheet-shaped object with the high hardness, so that the thinned brightness enhancement plate with the high adaptation degree is obtained; in this way, the grid paper can be damaged, an operator can more directly observe whether scratches deviate or not, along with scratching, the adhesive can be extruded towards the two sides through the PVA coating high-barrier plastic film, and finally the main body can be cut according to the scratches.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of brightness enhancement plates, in particular to a thin brightness enhancement plate with high adaptability. Background Art

[0002] Liquid crystal display screens are widely used in electronic products such as personal digital assistants, notebook computers, digital cameras, mobile phones, and LCD TVs. Since the liquid crystal display screen itself does not emit light, it needs the help of a backlight module to produce display functions.

[0003] For example, the application number is 201120311780.3. The brightness enhancement sheet of the utility model at least includes: a substrate, a brightness enhancement layer and an inorganic layer. The inorganic layer is arranged between the substrate and the brightness enhancement layer. The inorganic layer can make the substrate and the brightness enhancement layer firmly bonded and not separated, and the refractive index of the brightness enhancement sheet can be greater than 1.6. However, the adaptability of the thin brightness enhancement sheet is low, and it is not convenient to adapt to a variety of lamps of different specifications. Chloroprene, polyvinyl alcohol high barrier composite film

[0004] Therefore, in view of this, the existing structural deficiencies are studied and improved, and a thin light-enhancing plate with a higher adaptability is proposed. Utility Model Content

[0005] The purpose of the utility model is to provide a thin light-enhancing plate with high adaptability to solve the problems raised in the above-mentioned background technology.

[0006] To achieve the above-mentioned purpose, the utility model provides the following technical solutions: a thin light-enhancing plate with high adaptability, comprising a main body, one side of the main body is provided with a triangular prism, and the lower side surface of the main body is set as a smooth surface, an adhesive is coated on the horizontal surface of the main body, and the thickness of the adhesive is set to one-fourth of the thickness of the main body, a separating film is provided on the other side of the adhesive at the end away from the main body, and the thickness of the separating film is the same as the thickness of the adhesive, and the area of ​​the separating film is the same as the area of ​​the main body.

[0007] Preferably, when the adhesive is applied, it is first applied to the smooth surface of the main body, and then the separation film is covered on the adhesive after it is spread flat on the main body.

[0008] Preferably, the adhesive is chloroprene rubber, and the adhesive is specifically set to be anionic chloroprene rubber, and the model of the adhesive is SNL-A.

[0009] Preferably, the separator membrane is configured as an upper and lower part, the side of the separator membrane close to the adhesive is a PVA-coated high-barrier plastic film, and the material of the separator membrane is specifically configured as a polyvinyl alcohol high-barrier composite film, the upper part of the separator membrane is configured as grid paper, and the polyvinyl alcohol high-barrier composite film needs to be coated on the grid paper during preparation of the separator membrane.

[0010] Compared with the prior art, the beneficial effects of the utility model are:

[0011] 1. The utility model is provided with a main body, an adhesive and a separating film. Before using the main body, it is first necessary to draw a drawing on a grid paper according to specific installation requirements, and then the separating film is scratched along the drawing by a ruler, a knife back or other sheet-like objects with high hardness, so that the grid paper can be damaged so that the operator can more directly observe whether the scratch is offset, and as the scratching is carried out, the adhesive can be squeezed to both sides through the PVA-coated high-barrier plastic film, and finally the main body can be cut according to the scratch, and the separating film can be peeled off during installation, and the main body can be pasted at the specified position. BRIEF DESCRIPTION OF THE DRAWINGS

[0012] Figure 1 It is a schematic diagram of the overall three-dimensional structure of the utility model;

[0013] Figure 2 This is a schematic diagram of the bottom structure of the main body of the utility model;

[0014] Figure 3 For this utility model Figure 2 Enlarged structural diagram at A in the middle.

[0015] In the figure: 1. main body; 2. adhesive; 3. separator. DETAILED DESCRIPTION

[0016] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0017] like Figure 1-Figure 3As shown, a thin light-enhancing plate with high adaptability includes a main body 1, characterized in that a triangular prism is provided on one side of the main body 1, and the lower side of the main body 1 is set to a smooth surface, an adhesive 2 is coated on the horizontal surface of the main body 1, and the thickness of the adhesive 2 is set to one-fourth of the thickness of the main body 1, and a separation film 3 is provided on the other side of the adhesive 2 at the end away from the main body 1, and the thickness of the separation film 3 is the same as the thickness of the adhesive 2, and the area of ​​the separation film 3 is the same as the area of ​​the main body 1. When the adhesive 2 is applied, it is first applied to the smooth surface of the main body 1, and after it is laid flat on the main body 1, the separation film 3 is covered on the adhesive 2, the adhesive 2 is chloroprene rubber, and the adhesive 2 is specifically set to anionic chloroprene rubber, the model of the adhesive 2 is SNL-511A, and the separation film 3 is set to an upper and lower part, and the separation film 3 is close to the main body 1. The side close to the adhesive 2 is a PVA coated high-barrier plastic film, and the material of the separating film 3 is specifically set to a polyvinyl alcohol high-barrier composite film, the upper half of the separating film 3 is set to a grid paper, and the separating film 3 needs to be coated with the polyvinyl alcohol high-barrier composite film on the grid paper during preparation. Before using the main body 1, it is first necessary to draw a drawing on the grid paper according to specific installation requirements, and then use a ruler, a knife back or other sheet with a higher hardness to scratch the separating film 3 along the drawing. In this way, the grid paper can be damaged so that the operator can more directly observe whether the scratch is offset, and as the scratching is carried out, the adhesive 2 can be squeezed to both sides through the PVA coated high-barrier plastic film, and finally the main body 1 can be cut according to the scratch, and the separating film 3 can be peeled off during installation, and the main body 1 can be pasted at the specified position.

[0018] Furthermore, the separation film 3 squeezes the adhesive 2 toward both sides, which can prevent the adhesive 2 from adhering to the cutting knife during cutting, and can also press down one side of the separation film 3 to prevent the remaining adhesive 2 from being directly exposed to the air, thereby extending the service life of the device.

[0019] Furthermore, a grid paper is provided on one side of the separation film 3 to assist in drawing and improve the convenience of drawing.

[0020] Furthermore, the material of the separation film 3 near the adhesive 2 is set to be a polyvinyl alcohol high-barrier composite film because the material has good ductility and toughness, which can prevent the separation film 3 from rupturing prematurely when scratching.

[0021] Furthermore, the material of the adhesive 2 is set to chloroprene rubber because the material has physical and mechanical properties, and has the advantages of oil resistance, heat resistance, flame resistance, sunlight resistance, ozone resistance, acid and alkali resistance, and chemical reagent resistance, thereby ensuring the adhesion effect while extending the service life of the device.

[0022] Working principle: When using this thin and highly adaptable light-enhancing board, first, before using the main body 1, you need to draw a drawing on the grid paper according to the specific installation requirements, and then use a ruler, knife back or other sheet-like objects with high hardness to scratch the separation film 3 along the drawing, so that the grid paper can be damaged so that the operator can more directly observe whether the scratch is offset, and as the scratch is made, the adhesive 2 can be squeezed to both sides through the PVA-coated high-barrier plastic film, and finally the main body 1 can be cut according to the scratch, and the separation film 3 can be peeled off during installation, and the main body 1 can be pasted in the specified position. This is the working principle of this thin and highly adaptable light-enhancing board.

Claims

1. A thin light-enhancing plate with high adaptability, comprising a main body (1), characterized in that: A triangular prism is provided on one side of the main body (1), and the lower side of the main body (1) is set to be a smooth surface. An adhesive (2) is coated on the horizontal surface of the main body (1), and the thickness of the adhesive (2) is set to be one quarter of the thickness of the main body (1). A separation film (3) is provided on the other side of the adhesive (2) at the end away from the main body (1), and the thickness of the separation film (3) is the same as the thickness of the adhesive (2). The area of ​​the separation film (3) is the same as the area of ​​the main body (1).

2. A thin light-enhancing plate with high adaptability according to claim 1, characterized in that: When the adhesive (2) is applied, it is first applied to the smooth surface of the main body (1), and after it is spread flat on the main body (1), the separation film (3) is covered on the adhesive (2).

3. A thin light-enhancing plate with high adaptability according to claim 2, characterized in that: The separator (3) is configured as an upper and lower part, the side of the separator (3) close to the adhesive (2) is a PVA-coated high-barrier plastic film, and the material of the separator (3) is specifically configured as a polyvinyl alcohol high-barrier composite film, the upper part of the separator (3) is configured as grid paper, and when the separator (3) is prepared, the polyvinyl alcohol high-barrier composite film needs to be coated on the grid paper.