Method for homogenizing the magnetic field profile of a superconducting magnet system, in particular by feedback from a measured magnetic field profile - Patents.com

By adjusting heating and cooling powers based on magnetic field feedback, the method homogenizes the superconducting magnet system's magnetic field profile efficiently and cost-effectively, overcoming the limitations of existing temperature-dependent methods.

JP7557510B2Active Publication Date: 2024-09-27BRUKER SWITZERLAND AG
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2022170722
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-11-09
Filing Date
2022-10-25
Publication Date
2024-09-27
Estimated Expiration
2042-10-25

AI Technical Summary

Technical Problem

Existing methods for homogenizing the magnetic field profile of superconducting magnet systems are complex, costly, and limited by hardware design, requiring temperature sensors that occupy valuable space and increase system complexity.

Method used

A method that adjusts the heating and/or cooling power of bulk sub-magnets without measuring their temperature, using feedback from magnetic field profile measurements to achieve a uniform magnetic field, allowing for simple and cost-effective homogenization.

Benefits of technology

This approach achieves high magnetic field homogeneity within the sample volume by redistributing current without temperature sensors, maintaining a compact design and reducing costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007557510000002
    Figure 0007557510000002
  • Figure 0007557510000008
    Figure 0007557510000008
  • Figure 0007557510000001
    Figure 0007557510000001
Patent Text Reader

Abstract

To provide a method for homogenizing a magnetic field profile of a superconductor magnet system in a simple and inexpensive manner.SOLUTION: The invention provides a method for homogenizing a magnetic field profile of a superconductor magnet system. In the method, for changing initial currents into final currents, temperatures of multiple bulk sub-magnets (upper bulk sub-magnet, middle bulk sub-magnet, lower bulk sub-magnet) are chosen by controlling a heating power and / or a cooling power at the bulk sub-magnets without measuring the temperatures of the bulk sub-magnets, where for at least a part of the bulk sub-magnets, the heating powers are set at least temporarily different from each other and / or the cooling powers are set at least temporarily different from each other.SELECTED DRAWING: Figure 6
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for homogenizing a magnetic field profile of a superconducting magnet system, The superconducting magnet system is a cryostat having a room temperature bore; a superconducting bulk magnet housed within a cryostat and positioned coaxially with a room temperature bore; - a cryogenic cooling system adapted to cool a superconducting bulk magnet; Equipped with The superconducting bulk magnet comprises at least N axially stacked bulk sub-magnets, where N≧3; In an initial state, the bulk sub-magnets carry respective initial currents having relative proportions according to an initial distribution scheme; The method includes a post-correction step of changing the initial current to a final current having a relative proportion according to a final distribution scheme different from the initial distribution scheme; The magnetic field profile of the superconducting bulk magnet based on the final current is more uniform than the magnetic field profile based on the initial current; The cryogenic cooling system is adapted to control the temperature of each bulk sub-magnet separately; To change the initial current to the final current, the temperatures of at least some of the bulk sub-magnets are selected to be at least temporarily different from each other, so that - for a first portion of the bulk sub-magnet, the bulk sub-magnet in this first portion is at least approximately magnetically saturated, in particular at least 99% relative magnetic saturation, - for the second portion of the bulk sub-magnet, the bulk sub-magnet in this second portion is far from magnetic saturation, in particular has a maximum relative magnetic saturation of 95%. [Background technology]

[0002] Such a method is known from published European patent application no. 20174683.1.

[0003] A superconductor is a material capable of carrying electric current with virtually no ohmic losses. Superconductors are used, for example, for the generation of high-strength magnetic fields, in particular for nuclear magnetic resonance (NMR). However, the superconducting state is reached at a critical temperature T crit Because temperatures are expected to be less than 1000 K, the superconductors must be exposed to extremely low temperatures, and therefore are typically placed in a cryostat for thermal insulation.

[0004] A common superconductor application is superconducting wire, such as superconducting wire in tape or wire form. The superconducting wire may be used as is (e.g., for current transport) or after being wound into a desired configuration, such as a coil. In particular, superconducting coils for high magnetic field applications are usually made from superconducting wire wound into a solenoid shape.

[0005] However, superconducting bulk magnets are also known. In this case, the supercurrent circulates inside a piece or stack of superconductor, with the superconducting bulk magnet generally being in the shape of a closed ring. Such structures are simple and cheap to manufacture and are often made from high temperature superconductor (=HTS) materials.

[0006] The superconducting bulk magnet may be loaded by a procedure called "field cooling" as described, for example, in U.S. Patent Application No. 7,859,374 B2. In this procedure, the superconducting bulk magnet is Electrical Excitation Magnet excitation The magnet is placed inside the bore and then heated to a temperature T bulk But still T crit While exceeding excitation The magnet is turned on to generate a magnetic field. The superconducting bulk magnet then crit It is then cooled to below T bulk T crit While maintaining it below excitation The magnet is turned off and by this means a current is induced in the superconducting bulk magnet, which results in a magnetic flux being maintained in the superconducting bulk magnet. In other words, the superconducting bulk magnet traps a magnetic field within it. The superconducting bulk magnet is then: excitation It may be removed from the magnet and transported to a location where the trapping magnetic field can be used.

[0007] In many applications, such as the NMR applications mentioned above, it is desirable to have a high degree of uniformity in the magnetic field, however the magnetic field of a superconducting bulk magnet that is magnetized via a field cooling process and brought into its superconducting bore typically has a relatively low uniformity.

[0008] European Patent Application No. 3492941A1 proposes a bulk magnet structure consisting of several axially stacked ring-shaped bulk bodies of the same outer diameter and different radial thickness. The central bulk body has the smallest radial thickness. Planar rings made of metal with high thermal conductivity are arranged between the bulk bodies. The bulk magnet structure is magnetized by magnetic field cooling in the basic magnetization step. Excited Then, in a first temperature adjustment step, the temperature of the bulk magnetic structure is increased to improve the uniformity of the magnetic field distribution, and the central bulk body is brought into a fully magnetized state, and in a second temperature adjustment step, the temperature of the bulk magnetic structure is decreased.

[0009] Although this procedure allows some redistribution of the currents in the bulk magnetic structure for field homogenization, the achievable current distribution is limited by the radial thickness distribution of the ring-shaped bulk body, i.e., by the hardware design, and thus compensation of field inhomogeneities due to manufacturing tolerances is rather limited.

[0010] In European Patent Application No. 20174683.1, several methods are proposed for homogenizing a superconducting magnet system and the magnetic field profile of the superconducting magnet system. The superconducting magnet system comprises a cryostat, a superconducting bulk magnet with a number of bulk sub-magnets, and a cryogenic cooling system. The cryogenic cooling system is adapted to separately control the temperature of each bulk sub-magnet and comprises a temperature sensor in each bulk sub-magnet and an adjustment unit for adjusting the heating and / or cooling power in each bulk sub-magnet. In one method, it is proposed to correct an initial not very homogeneous magnetic field carried by the superconducting bulk magnet. For this purpose, at least temporarily, a first part of the bulk sub-magnet is brought at least close to magnetic saturation by increasing the temperature, and a second part of the bulk sub-magnet is brought farther away from magnetic saturation. In this way, some drift may start in the first part, while the second part remains stable, which allows the magnetic field contributions of the different bulk sub-magnets to be adjusted in order to increase the homogeneity of the magnetic field. During the execution of the method, the magnetic field profile is repeatedly measured. An example is presented in Figure 22 of said European Patent Application showing, among other parameters, the temperature of the different bulk sub-magnets as a function of time. The workflow description in Figure 27 of said European Patent Application describes the execution of said method on the above mentioned superconducting magnet system equipped with a temperature sensor for each bulk sub-magnet.

[0011] Such a temperature sensor in the bulk sub-magnet would make the superconducting magnet system or its cryogenic cooling system more complex and therefore more expensive. Furthermore, the temperature sensor would be required to measure the temperature inside the superconductor cryostat and excitation Magnet excitation This requires some additional space in the limited space inside the bore, which can reduce system performance for a given system size and therefore reduce cost efficiency.

[0012] Post-published European Patent Application No. 21169465.8 further discloses a method for magnetic field cooling of a superconducting magnet system comprising a plurality of bulk sub-magnets, in which the bulk sub-magnets are cooled by a pre-calculated excitation The current is gradually cooled according to the step pattern. excitation will be done. [Prior art documents] [Patent documents]

[0013] [Patent Document 1] European Patent Application No. 20174683.1 [Patent Document 2] U.S. Patent Application No. 7,859,374B2 [Patent Document 3] European Patent Application No. 3492941A1 [Patent Document 4] European Patent Application No. 21169465.8 Summary of the Invention [Problem to be solved by the invention]

[0014] It is an object of the present invention to provide a way by which the magnetic field profile of a superconducting magnet system can be homogenized in a simple and inexpensive manner. [Means for solving the problem]

[0015] According to the invention, the above object is achieved by the method introduced at the beginning, characterized in that in order to change the initial current to a final current, the temperature of the bulk sub-magnet is selected by controlling the heating power and / or cooling power in the bulk sub-magnet without measuring the temperature of the bulk sub-magnet, and for at least some of the bulk sub-magnets, the heating powers are set to be at least temporarily different from each other and / or the cooling powers are set to be at least temporarily different from each other.

[0016] The present invention proposes to change the initial current to the final current by modifying the heating and / or cooling power of the bulk sub-magnets without knowing the exact temperature of each bulk sub-magnet. The temperature check of the individual bulk sub-magnets is completely omitted, simplifying the homogenization of the magnetic field in the post-correction step. This means that the method of the present invention can be performed on a superconducting magnet system without temperature sensors for the individual bulk sub-magnets. The design of the superconducting magnet system can be kept simple and its cost can be kept low compared to superconducting magnet systems including such temperature sensors.

[0017] To carry out the method of the invention, typically an initial trapped magnetic field profile is determined (measured) based on the initial current carried by the bulk sub-magnets. Then, regions of the initial trapped magnetic field profile that need to be corrected to improve the magnetic field homogeneity, i.e. regions that exhibit a locally higher than desired trapped magnetic field compared to other regions, are identified, and further, corresponding bulk sub-magnets ("first part of the bulk sub-magnets") that are responsible for the locally higher than desired trapped magnetic field and therefore require a current reduction in the initial trapped magnetic field profile are identified. Following this, the temperature of the bulk sub-magnets ("second part of the bulk sub-magnets") that do not require a current reduction is set / changed such that the respective bulk sub-magnets are significantly away from magnetic saturation. The temperature of the first part of the bulk sub-magnets is set / changed such that the respective bulk sub-magnets are at least approximately magnetically saturated. This is done by setting / changing the heating and / or cooling powers in the individual bulk sub-magnets (e.g. with an increase in the heating power of the heater element for the first part of the bulk sub-magnets or an increase in the cooling power of the adjustable thermal impedance for the second part of the bulk sub-magnets).

[0018] When the first part of the bulk sub-magnets is at least approximately magnetically saturated, the bulk sub-magnets of the first part show a significant gradual loss of their current ("drift"), and the energy of this bulk sub-magnet of the first part slowly dissipates, weakening the contribution of the bulk sub-magnets of the first part to the magnetic field profile. Due to coupling, part of the magnetic flux (and the respective current) may be taken over by other (non-saturated) bulk sub-magnets of the second part. The drift in the bulk sub-magnets of the first part is used to slowly adjust the magnetic field profile, in particular to homogenize it. It is noted that this drift may be of different strength in different bulk sub-magnets of the first part and / or may be set to last for different lengths in different bulk sub-magnets of the first part. In particular, each bulk sub-magnet may be individually shifted between the first part and the second part (typically from the first part to the second part) during the post-correction step.

[0019] To identify the strength of the drift and / or to monitor the change of the magnetic field profile, the measurement of the captured magnetic field profile is usually performed periodically, in particular periodically or continuously, during the post-correction step. Then, for example, when there is no drift or the drift is too low, the heating and / or cooling power for the bulk sub-magnet of the first part may be adjusted. This adjustment is performed without knowing the exact temperature of the bulk sub-magnet.

[0020] When the desired magnetic field profile is reached, the heating and / or cooling powers in the (last remaining) bulk sub-magnets of the first part are changed so that the respective bulk sub-magnets are far away from magnetic saturation. Just before the desired magnetic field profile is reached, it is also possible to gradually change the heating and / or cooling powers here, in particular to change them separately for each bulk sub-magnet of the first part. In this way, the drift can be adjusted (i.e. weakened / slowed down) so that the correction of the magnetic field profile towards the end of the post-correction step can be performed more accurately, resulting in a higher final magnetic field homogeneity. In particular, the risk of introducing inhomogeneities in the magnetic field profile by making the contribution of one or more bulk sub-magnets of the first part very weak can be reduced.

[0021] Thus, according to the invention, the heating and / or cooling powers in the individual bulk sub-magnets may be adapted using feedback from repeated measurements of the magnetic field profile of the superconducting magnet system within the sample volume, and particularly high magnetic field homogeneity can be achieved.

[0022] By individual control of the heating and / or cooling powers, the bulk sub-magnets may be freely selected to weaken their respective magnetic field contributions. Typically, only one bulk sub-magnet or two bulk sub-magnets are at least approximately magnetically saturated at a time. The allocation of bulk sub-magnets to the first or second part in the post-correction step may be changed over time, and such allocation may be made multiple times for individual bulk sub-magnets, if necessary.

[0023] This method makes it possible to establish a magnetic field with very high homogeneity within the sample volume of a superconducting magnet system, is easy to implement and works without knowing its temperature.

[0024] Preferred Variants of the Invention In a preferred variant of the method of the present invention, the superconducting magnet system is designed without a thermal sensor for measuring the temperature of the bulk sub-magnet. Since the method of the present invention works normally without measuring the temperature of the bulk sub-magnet, it is not necessary to equip each bulk sub-magnet in the superconducting magnet system with a thermal sensor. However, it is noted that usually there is one thermal sensor in the (common) cooling stage ("cooling plate"). The complexity of the superconducting magnet system is kept low, the superconducting magnet system can have a compact design, and the overall cost can be reduced.

[0025] In another preferred variant, in the first part the heating power in the bulk sub-magnets is selected to be at least temporarily higher compared to the second part and / or in the first part the cooling power in the bulk sub-magnets is selected to be at least temporarily lower compared to the second part. This is an easy way to bring the bulk sub-magnets of the first part closer to magnetic saturation, especially when the bulk sub-magnets are of equal type (especially the same size and material). A drift is then initiated in the first part of the bulk sub-magnets, whereby the magnetic field contribution of the bulk sub-magnets of the first part can be adjusted.

[0026] A variant is also preferred in which, during the post-correction step, the intermediate magnetic field profile of the superconducting magnet system is repeatedly measured until the desired magnetic field profile based on the final currents is obtained, and between measurements the heating and / or cooling powers of at least some of the bulk sub-magnets are changed and / or a certain time is waited. By repeated measurements of the magnetic field profile it is possible to know about the current state, in particular the drift state, of the bulk sub-magnets without knowing their temperature. Furthermore, the progress of the method of the invention can be monitored. It is also possible to react quickly to unexpected changes in the course of the method of the invention. By repetition of this variant a particularly high homogeneity of the final magnetic field can be achieved.

[0027] In a preferred further development of this variant, from at least one measured intermediate magnetic field profile, a contribution to said magnetic field profile is reduced, in the following also referred to as an intermediate magnetic field profile, in order to increase the magnetic field homogeneity. excitation Once one or more bulk sub-magnets, called bulk sub-magnets (6a-6c), have been identified, excitation To reduce the contribution of the bulk sub-magnets, one or more of the respective overshoots are excitation Regarding bulk sub magnets, excitation The cooling power is selected to be smaller and / or the heating power is selected to be larger compared to the bulk sub-magnets that are not bulk sub-magnets. This is a simple way to homogenize the magnetic field profile. The contribution of each of the axially stacked bulk sub-magnets to the magnetic field profile is strongest at its own axial position and weaker away from its own axial position. In general, to adjust the magnetic field profile in the sample volume in the central region (z=0), one or more central bulk sub-magnets are adjusted in terms of heating / cooling power, and to adjust the magnetic field profile in the sample volume in the side region (z>0 or z=0), one or more side bulk sub-magnets on each side are adjusted in terms of heating / cooling power.

[0028] In another preferred further development, excitation For at least a portion of the bulk sub-magnets, excitation Regarding bulk sub magnets, excitationThe amount by which the cooling power is selected to be smaller and / or the heating power is selected to be larger compared to the non-bulk sub-magnets is reduced over time in the final phase of reducing the contribution of each bulk sub-magnet to the magnetic field profile, in particular the reduction in said amount depends on how much the contribution of each bulk sub-magnet to the magnetic field profile remains to be reduced, as identified in one or more further measurements of the intermediate magnetic field profile. In this way, the final adjustment of the magnetic field profile can be performed carefully and accurately. The original inhomogeneities can be accurately eliminated and the introduction of new inhomogeneities can be minimized. The overall loss of magnetic field due to the post-correction step can be minimized.

[0029] At least one time after changing the heating and / or cooling power in at least some of the bulk sub-magnets, a first period of time is waited, and then at least a first measurement of an intermediate magnetic field profile is performed; - a second period of time is waited; a second measurement of the intermediate magnetic field profile is performed; determining a current drift characteristic of the intermediate magnetic field profile from at least the first and second measurements; Based on the identified current drift characteristics, a next change in heating and / or cooling power in at least some of the bulk sub-magnets and / or a next time to wait is determined. A further development is also preferred, characterized in that: the first time period for waiting can ensure that possible relaxation processes resulting from a redistribution of currents in the bulk sub-magnet (caused by a change in heating and / or cooling powers) are completed; in the second time period, a linear drift occurs without such relaxation processes; the second time period for waiting can ensure that a detectable current change occurs, which facilitates identifying the drift characteristics; the identification of the drift characteristics can be performed particularly accurately, providing reliable data for the correction of the intermediate magnetic field profile; during the first and second time periods, all heating and cooling powers should be kept constant in order to prevent the occurrence of new relaxation processes and thus to receive useful and consistent data for the correction of the magnetic field.

[0030] a cryostat having a room temperature bore; a superconducting bulk magnet housed within a cryostat and positioned coaxially with a room temperature bore; - a cryogenic cooling system adapted to cool a superconducting bulk magnet; A superconducting magnet system comprising: The superconducting bulk magnet is a bulk magnet having at least N axially stacked bulk magnets, where N≧3. A magnet is provided. a bulk sub-magnet is substantially ring-shaped and disposed coaxially with the room temperature bore; An intermediate body is disposed between each two axially adjacent bulk sub-magnets; an intermediate body having a substantially ring shape and disposed coaxially with the room temperature bore; The bulk sub-magnet is supported on the intermediate body, The intermediate body is made of a non-metallic insulating material having a specific thermal conductivity smaller than that of the material of the bulk sub-magnet; a cryogenic cooling system adapted to separately control the temperature of each bulk sub-magnet; for each bulk sub-magnet there is a regulating unit for regulating the heating and / or cooling power in the respective bulk sub-magnet; The superconducting magnet system is constructed without a thermal sensor for measuring the temperature of the bulk sub-magnet. Also within the scope of the present invention is a superconducting magnet system, characterized in that: The superconducting magnet system of the present invention allows deliberate setting of the temperature of each bulk sub-magnet of the superconducting bulk system. This then results in: excitation Magnetic Guidance excitation This allows subsequent deliberate magnetic saturation (or near-complete saturation) of one or more bulk sub-magnets and thus targeted redistribution of currents in the bulk sub-magnets. As a result, the superconducting magnet system of the present invention allows highly accurate reshaping of the magnetic field generated by the superconducting bulk magnets, in particular to achieve high magnetic field homogeneity.

[0031] The currents in the bulk sub-magnets may be set separately, and the individual setting of the currents can generally be performed with any magnet hardware. The present invention does not require a specially shaped bulk superconducting magnet or bulk sub-magnet, respectively, and can use particularly simple, cheap and compact magnet designs. In particular, the superconducting magnet system of the present invention works well with hardware designs that induce a magnetic field gradient when a default (basic) current distribution on the bulk sub-magnet, such as an axially short superconducting bulk magnet, is applied.

[0032] The present invention provides a method for simulating the induction of a superconducting bulk magnet by inducing drift in one or more selected bulk sub-magnets until a desired magnetic field profile is achieved. excitation A fine setting of the current can be applied later and the magnetic field profile may be monitored for this purpose during the fine setting.

[0033] By placing an intermediate body made of a non-metallic insulating material between the bulk sub-magnets, it is possible to thermally decouple adjacent bulk sub-magnets to a large extent and to establish a stable temperature difference between the bulk sub-magnets, large or small as required. In this way, the saturation of the magnetization of the bulk sub-magnets (or the corresponding current in the bulk sub-magnets) may be set very accurately. The insulating material is usually a plastic material or a composite material containing plastic.

[0034] There are no temperature sensors for the bulk sub-magnets since there is no need to check the individual temperatures of the bulk sub-magnets for homogenization. The absence of temperature sensors allows the superconducting magnet system to be less complicated and therefore less expensive. The absence of the need to provide additional space occupied by temperature sensors increases system performance for a given system size and therefore improves cost efficiency.

[0035] The conditioning units are used to establish the desired heating and / or cooling powers separately in each bulk sub-magnet. The conditioning units are usually controlled by an electronic control unit. Typical conditioning units include adjustable heater elements and / or adjustable thermal impedances, in particular coupled to a common cooling stage.

[0036] The main superconducting bulk magnet or each bulk sub-magnet is generally made from a high temperature superconducting material, for example of the ReBCO type (Re: rare earth element, in particular Eu, Y or Gd), or of the BSCCO type, or of the MgB2 type or of a pnictide.

[0037] A superconducting bulk magnet has a central (axial) bore, also called the superconducting bore, that is substantially cylindrical (cylinder jacket) shaped, and comprises a number of axially stacked bulk sub-magnets. The bulk sub-magnets are each generally in the shape of a closed ring to allow for a sustained circular current. The current in the bulk sub-magnet induces a magnetic field substantially along the axis of the central bore (the "z-axis"). The bulk sub-magnets may each be of the "classical type", i.e. an integral ring grown from the melt. Alternatively, the bulk sub-magnets may each include multiple axial and / or radial layers, in particular may be made from multiple stacked ring elements, and / or may include a circumferential superconducting coating on the surface of one or more tubular carriers. Typically, a superconducting bulk magnet comprises 3-7 bulk sub-magnets, the temperature of which may be controlled separately.

[0038] A preferred embodiment of the superconducting magnet system comprises: for each bulk sub-magnet, there is a heater element thermally connected to the respective bulk sub-magnet; In particular, the heater elements are controlled by an adjustment unit, the adjustment unit being configured to set variable heating powers of the heater elements to respective bulk sub-magnets; In particular, the heater element is an electric heater element. The heater elements are useful in precisely and directly controlling the temperature of the bulk sub-magnets, since they rapidly and precisely introduce individual heating power to the bulk sub-magnets. Electric heater elements may be constructed particularly compactly and are relatively inexpensive.

[0039] Another preferred embodiment is The cryogenic cooling system comprises a common cooling stage for all bulk sub-magnets; and for each bulk sub-magnet, there is a thermal connection from the common cooling stage to the respective bulk sub-magnet; In particular, the thermal connection includes a thermal switch controlled by the regulating unit. This is a simple and compact way to provide cooling power to the bulk sub-magnets, in particular at least approximately equal cooling power to each bulk sub-magnet. The common cooling stage is thermally coupled to the cryocooler, which simplifies the design. A thermal switch allows to temporarily shut off the cooling power, in particular during the post-correction step. It is noted that in each bulk sub-magnet a constant cooling power is often combined with a variable heating power.

[0040] In a preferred further development, the thermal connection comprises a variable thermal impedance controlled by a regulating unit, which is configured to set a variable cooling power at the respective bulk sub-magnet. In this way, it is also possible to precisely and directly control the temperature of the bulk sub-magnet.

[0041] In an advantageous embodiment, the superconducting magnet system further comprises a magnetic field sensor device for measuring the magnetic field profile in the sample volume of the room temperature bore. By knowing the magnetic field, it is possible to determine the influence of the currents of the different bulk sub-magnets on the magnetic field profile. Based on this information, the bulk sub-magnets can be heated or cooled so that the magnetic field profile is adjusted, in particular homogenized.

[0042] A preferred further development provides that the magnetic field sensor device comprises at least one sensor arranged on a moving stage, whereby the at least one sensor can be moved in the sample volume in order to determine the magnetic field profile in the sample volume by repeated readout of the at least one sensor at different positions in the sample volume. Such a sensor ("single sensor") can be easily realized. By using a moving stage, the at least one sensor can scan the sample volume. The density of the measurement positions can be flexibly selected. The sensor device may comprise an off-axis sensor and / or an on-axis sensor. In the case of an off-axis sensor, the moving stage can also realize an azimuthal movement of the off-axis sensor.

[0043] An alternative preferred further development provides that the magnetic field sensor device comprises a sensor arrangement distributed in the sample volume, the arrangement including at least N, preferably at least 2*N, sensors for determining the magnetic field profile in the sample volume by parallel readout of the sensors in the arrangement fixed in a predetermined position. The sensor arrangement allows a particularly fast (instantaneous) acquisition of the magnetic field profile, which can be performed continuously if necessary. The number of sensors in the sensor arrangement can be increased to increase the accuracy of the measurement of the magnetic field profile. The sensors are usually provided off-axis or both on-axis and off-axis.

[0044] In a preferred embodiment, the superconducting magnet system further comprises an electronic control unit for automatically homogenizing the magnetic field profile in the room temperature bore, the electronic control unit being adapted to automatically homogenize the magnetic field profile of the superconducting bulk magnet according to the method of the present invention described above, the electronic control unit repeatedly receiving the measured intermediate magnetic field profile measured with the magnetic field sensor device, and based on the intermediate measurements, without receiving or evaluating temperature data of the bulk sub-magnet, the electronic control unit automatically controls the heating and / or cooling power in the bulk sub-magnet. The method of the present invention is well suited for automatic implementation and is rather simple. In particular, there is no need to process any temperature data. The implementation of the electronic control unit is very comfortable for the user. The availability of the superconducting magnet system can be improved.

[0045] Furthermore, it is within the scope of the present invention to use the above-described superconducting magnet system of the present invention in the above-described method of the present invention. In this way, it is possible to homogenize the magnetic field in a simple and inexpensive manner.

[0046] Further advantages can be derived from the description and the enclosed drawings. The features described above and below can be used in accordance with the invention, individually or collectively, in any combination. The described embodiments should not be understood as an exhaustive enumeration, but rather have exemplary features for the explanation of the invention.

[0047] The invention is illustrated in the drawings. [Brief description of the drawings]

[0048] [Figure 1] FIG. 2 is a schematic diagram of a first embodiment of a superconducting magnet system of the present invention having a single on-axis magnetic field sensor, a thermal switch, and a heater for carrying out the method according to the present invention. [Diagram 2] FIG. 2 is a schematic diagram of a second embodiment of a superconducting magnet system of the invention in which a magnetic field sensor, a non-variable thermal impedance and a heater are arranged for carrying out the method according to the invention. [Diagram 3] FIG. 4 is a schematic diagram of a third embodiment of a superconducting magnet system of the present invention having a single off-axis magnetic field sensor and a variable thermal impedance for carrying out the method according to the present invention. [Figure 4] FIG. 11 is a schematic diagram of a fourth embodiment of a superconducting magnet system of the present invention having a single off-axis magnetic field sensor and a thermal switch for carrying out the method according to the present invention. [Diagram 5] FIG. 4 shows a schematic schedule of the excitation current, the current in the bulk sub-magnet, the overall cooling and heating power in the bulk sub-magnet for a variant of the method of the invention. [Figure 6] FIG. 6 is a close-up view of the bulk sub-magnet current and heating power in the bulk sub-magnet for the schematic time schedule of FIG. 5, as well as the local magnetic flux density at three positions along the magnetic axis. [Figure 7] 7 is a schematic diagram of a magnetic field profile obtained at three time points during the variant of the method of the invention shown in FIGS. 5 and 6; FIG. [Figure 8]FIG. 4 is a schematic diagram of the overall excitation procedure according to the method of the invention in an exemplary variant. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0049] The superconducting magnet system of the present invention Figure 1 shows an example. excitation Magnet 3 excitation a first embodiment of a superconducting magnet system 2 of the present invention disposed partially within a bore 3a; excitation The device 1 is shown in a schematic diagram.

[0050] excitation The magnet 3 may be of the superconducting or normal conducting type; excitation Flowing through magnet 3 excitation The current is, excitation It may be configured with a magnet control unit (not shown in detail). excitation Magnet 3 guides superconducting magnet system 2 excitation For the purpose of excitation A magnetic flux (or magnetic field) may be generated within bore 3a. The generated magnetic flux is generally oriented parallel to central axis A.

[0051] The superconducting magnet system 2 comprises a cryostat 4, the interior of which is maintained in vacuum for thermal insulation. Inside the cryostat 4, a superconducting bulk magnet 5 is housed, which here comprises three bulk sub-magnets 6a, 6b, 6c. The bulk sub-magnets 6a-6c are generally in the shape of closed rings and are axially stacked and arranged coaxially with respect to a central axis A of the superconducting magnet system 2, which results in a radially central, axially extending free space inside the superconducting bulk magnet 5, called the superconducting bore 7. The bulk sub-magnets 6a-6c are made of a high-temperature superconducting material, such as YBCO. The individual bulk sub-magnets 6a-6c are here each formed by a single ring of bulk material. It is also possible (not shown) to combine several ring-shaped sheets of bulk material to form the individual bulk sub-magnets 6a-6c. The axis A is also called the z-axis.

[0052] Axial-wise between adjacent bulk sub-magnets 6a-6c, substantially ring-shaped washer-like intermediate bodies 8a, 8b, here made of polyimide material, are arranged to thermally insulate the bulk sub-magnets 6a-6c from one another. A further intermediate body 8c of polyimide material is arranged between the bottom bulk sub-magnet 6c and a common cooling stage 9 ("cold stage") for the bulk sub-magnets 6a-6c. The bulk sub-magnets 6a-6c rest on the intermediate bodies 8a, 8b and the further intermediate body 8c.

[0053] In the illustrated example, the bulk sub-magnets 6a-6c all have the same outer and inner diameters. Furthermore, in the illustrated example, the intermediate bodies 8a, 8b and the further intermediate body 8c have a larger outer diameter and the same inner diameter as the bulk sub-magnets 6a-6c. It is also possible that the intermediate bodies 8a, 8b and the further intermediate body 8c have the same outer and inner diameters as the bulk sub-magnets 6a-6c (not shown).

[0054] The room temperature bore 7 a of the cryostat 4 leads into the superconducting bore 7 . excitation Magnet 3 or excitation The bore 3a, the superconducting bulk magnet 5 or its superconducting bore 7 and the room temperature bore 7a are arranged coaxially. In the magnetic centre of the superconducting bore 7 and within the room temperature bore 7a is arranged a sample volume 10 in which a sample may be placed that is exposed to the magnetic flux generated by the superconducting magnet system 2.

[0055] To measure and determine the magnetic field profile within a sample volume 10 of the room temperature bore 7a, a magnetic field sensor device 11 is used, here consisting of one sensor 11a ("single sensor") attached via a straight connector 12a to a translation stage 12. The sensor 11a is positioned on-axis with respect to the central axis A and can be moved vertically by the translation stage 12 within the sample volume 10. In this way, the axial gradient of the magnetic field profile, and thus the axial non-uniformity of the magnetic field profile, can be measured in a relatively simple manner.

[0056] The superconducting magnet system 2 further comprises a cryogenic cooling system 13 for cooling the superconducting bulk magnet 5. According to the invention, the temperature of each bulk sub-magnet 6a-6c may be separately adjusted by controlling the heating and / or cooling power in the respective bulk sub-magnet 6a-6c. For this purpose, here, each bulk sub-magnet 6a-6c is connected to an electric heater element 15a, 15b, 15c and a thermal switch 16a, 16b, 16c. Furthermore, the electric heater elements 15a-15c and the thermal switches 16a-16c are connected to an adjustment unit 14 (connections shown by dotted lines), which are here integrated in an electronic control unit 18. Via the adjustment unit 14, it is possible to set a variable heating power in the heater elements 15a-15c and, since the thermal switches 16a-16c can be opened or closed, it is possible to set a cooling power. The heating power of the electric heater elements 15a-15c may be variably adjusted by setting the current intensity. The cooling power reaching the bulk sub-magnets 6a-6c via the thermal switches 16a-16c may be regulated, ie switched off or on, by opening or closing the respective thermal switch 16a-16c, respectively.

[0057] Each heater element 15a-15c is thermally coupled to one of the bulk sub-magnets 6a-6c. Each bulk sub-magnet 6a-6c is thermally coupled to a common cooling stage 9 via thermal connections 17a, 17b, 17c, which here include thermal switches 16a-16c. In the illustrated setup, the thermal switches 16a-16c are all open, so that no cooling power is supplied to the bulk sub-magnets 6a-6c. The common cooling stage 9 is excitation During procedure and normal operation, the bulk sub-magnets 6a-6c are at cryogenic temperatures, typically much lower than the critical temperature of the material.

[0058] For cooling the common cooling stage 9 during normal operation, in the illustrated example the cryostat 4 is permanently equipped with a first cryocooler 19 having its first cryocooler cold stage 19a inside the cryostat 4, where the cryocooler cold stage 19a of the first cryocooler 19 is connected to the common cooling stage 9 via a thermal cryocooler impedance 20.

[0059] excitation During the procedure, the operation of the first cryocooler 19 is excitation It may be impaired by the strong stray magnetic field arising from the magnets 3 and should not be used in that case. Therefore, in the example shown, the cryostat 4 further comprises a port 21 and a supply line 22 for conducting an external cooling fluid from the port 21 to the common cooling stage 9 and back. excitation During the procedure, the port 21 is temporarily connected to an external second cryocooler 23, the second cryocooler cold stage 23a of which is located within a separate auxiliary cryostat 24. Inside the auxiliary cryostat 24, an auxiliary supply line 25 is provided to carry cooling fluid from the cryocooler cold stage 23a of the second cryocooler 23 back to the port 21. Furthermore, during normal operation: excitation This may require less cooling power compared to the conventional procedure and therefore excitation It should be noted that the use of the second cryocooler 23 during the procedure allows the use of the smaller first cryocooler 19 for normal operation.

[0060] When in a particular bulk sub-magnet 6a-6c the heating powers (if any) of the heater elements 15a-15c, the cooling powers (if any) of the common cooling stage 9 via the thermal switches 16a-16c, and further heating or cooling powers via other heat conduction paths (such as blackbody radiation or residual heat conduction through the intermediate bodies 8a, 8b and further intermediate body 8c) are in equilibrium, the bulk sub-magnets 6a-6c maintain a stable temperature (equilibrium temperature). By changing the heating powers of the heater elements 15a-15c and / or the cooling powers via the thermal switches 16a-16c, different equilibrium states may be set. Thereby, different equilibrium temperatures may be obtained, even if their temperature values ​​are not known. It is noted that the bulk sub-magnets 6a-6c are not equipped with thermal sensors for monitoring the temperature of each bulk sub-magnet 6a-6c.

[0061] The magnetic field sensor device 11, the heater elements 15a-15c, and the thermal switches 16a-16c are connected to an electronic control unit 18. The magnetic field sensor device 11 measures the magnetic field profile, which helps to determine the non-uniformity of the magnetic field profile and to monitor the progress of correction of the magnetic field profile. The electronic control unit 18 controls the magnetic field of the superconducting bulk magnet 5. excitation During and after the correction of the magnetic field profile of the superconducting bulk magnet 5, in particular in the post-correction step, the heating power of the heater elements 15a-15c and the thermal switches 16a-16c and thereby the temperature (in particular the equilibrium temperature) of the bulk sub-magnets 6a-6c are controlled. In order to correct the magnetic field profile, the individual bulk sub-magnets 6a-6c may be put in a drift state for some time. Whether a particular bulk sub-magnet 6a-6c is in a suitable drift state for improving the magnetic field homogeneity can best be observed by monitoring the magnetic field profile as a function of time. It is noted that knowing the current temperature of a particular bulk sub-magnet 6a-6c is not required for this purpose.

[0062] It should be noted that the following Figures 2-4 show a modified version of the superconducting magnet system 2 of Figure 1. For this reason, only the differences in features with respect to the embodiment of Figure 1 are described below. It should be noted that in the embodiment shown in Figures 2-4, the second cryocooler 23 is still part of the superconducting magnet system 2, but is not shown for simplicity. However, it is also possible to use a superconducting magnet system 2 having only the first cryocooler 19 and no second cryocooler 23, in which case the first cryocooler 19 is excitation The operation of the first cryocooler 19 is not impaired since it can be shielded against the strong magnetic field (stray magnetic field) arising from the magnet 3. All further superconducting magnet systems 2 presented below have in common that no thermal sensors are used to measure the temperature of the bulk sub-magnets 6a-6c.

[0063] FIG. 2 shows, by way of example, a superconducting magnet system including a second embodiment of the superconducting magnet system 2 of the present invention. excitation The apparatus 1 is shown in a schematic diagram. In comparison to Fig. 1, a different type of magnetic field sensor device 11 is used, in which the thermal switches are replaced by non-variable ("fixed") thermal impedances 26a, 26b, 26c.

[0064] To measure and determine the magnetic field profile in the sample volume 10 of the room temperature bore 7a, a magnetic field sensor device 11 is used, here consisting of an arrangement 11b of sensors 11a ("sensors") mounted on a stationary stage 27. The arrangement 11b of sensors 11a comprises here six sensors 11a. Three sensors 11a' are arranged on-axis with respect to the central axis A and three sensors 11a'' are arranged off-axis with respect to the central axis A. In this way, the on-axis and off-axis gradients of the magnetic field profile and thus the on-axis and off-axis inhomogeneity of the magnetic field profile can be measured simultaneously and directly. The arrangement 11b of sensors 11a is here fixed. In the arrangement 11b of sensors 11a, Hall sensors may be used.

[0065] In the illustrated example, each electric heater element 15a-15c is connected to an adjustment unit 14. The adjustment unit 14 can variably adjust only the heating power in each bulk sub-magnet 6a-6c. Each bulk sub-magnet 6a-6c is thermally coupled to a common cooling stage 9 via thermal connections 17a-17c, which here include non-variable thermal impedances 26a-26c. This ensures that cooling power is constantly supplied to the bulk sub-magnets 6a-6c when the common cooling stage 9 is at a low temperature.

[0066] FIG. 3 shows, by way of example, a superconducting magnet system including a third embodiment of the superconducting magnet system 2 of the present invention. excitation The apparatus 1 is shown in a schematic diagram. Compared to Fig. 1, the magnetic field sensor device 11 is slightly modified, the thermal switches are replaced by variable thermal impedances 28a, 28b, 28c and the heater elements are removed.

[0067] To measure and identify the magnetic field profile in the sample volume 10 of the room temperature bore 7a, a magnetic field sensor device 11 is used, here consisting of a sensor 11a attached to a moving stage 12 via a tilted connector 12b. The sensor 11a is arranged off-axis with respect to the central axis A and can be moved parallel to the central axis A by the moving stage 12 along it in the sample volume 10. Furthermore, the sensor 11a can be rotated around the central axis A. Typically, the sensor 11a is a high-reproducibility sensor. Different positions are scanned along it in the sample volume 10. Then, by means of spherical harmonic analysis, the on-axis and off-axis gradients are calculated. In this way, the on-axis and off-axis magnetic field profiles, as well as the on-axis and off-axis inhomogeneities of the magnetic field profile due to them, can be identified with only one sensor 11a.

[0068] In the illustrated example, each of the variable thermal impedances 28a-28c is connected to an adjustment unit 14. The adjustment unit 14 can variably adjust only the cooling power in each of the bulk sub-magnets 6a-6c. Each of the bulk sub-magnets 6a-6c is thermally coupled to a common cooling stage 9 via thermal connections 17a-17c, which here include the variable thermal impedances 28a-28c.

[0069] FIG. 4 shows, by way of example, a superconducting magnet system including a fourth embodiment of the superconducting magnet system 2 of the present invention. excitation 1 shows a schematic diagram of the device 1. Compared to Fig. 3, the variable thermal impedance is replaced by thermal switches 16a-16c.

[0070] In the illustrated example, each thermal switch 16a-16c is connected to an adjustment unit 14. The adjustment unit 14 can adjust the cooling power in each bulk sub-magnet 6a-6c by simply switching between no cooling power and maximum cooling power from the common cooling stage 9. Each bulk sub-magnet 6a-6c is thermally coupled to the common cooling stage 9 via thermal connections 17a-17c, which here include thermal switches 16a-16c. In a typical operating method of this embodiment, first the thermal switches 16a-16c are closed and the bulk sub-magnets 6a-6c are cooled with maximum cooling power, excitation The current is then decreased. The magnetic field profile is then measured. excitationThe bulk sub-magnets 6a-6c are identified. The respective thermal switches 16a-16c are opened. The temperature of each bulk sub-magnet 6a-6c rises somewhat when no (direct) cooling power is applied, and each bulk sub-magnet 6a-6c drifts. When the uniformity of the magnetic field profile, or the contribution of each bulk sub-magnet to the magnetic field profile, is as desired, the respective thermal switch 16a-16c is closed and maximum cooling power is applied to each bulk sub-magnet 6a-6c, where the drift stops. It should be noted that in general, the thermal switches 16a-16c of different bulk sub-magnets 6a-6c must be closed at different times. Alternatively, the cooling power may be effectively variably adjusted by rapidly changing between open and closed states in the thermal switches 16a-16c of each bulk sub-magnet 6a-6c during the post-correction step, and adjusting the ratio of the duration of the open and closed scenes.

[0071] Method of the invention for homogenizing a magnetic field profile The present invention is used to homogenize the magnetic field profile of a superconducting magnet system after an initial magnetic field cooling step has been applied (for the initial magnetic field cooling step, see European Patent Application No. 20174683.1, the entire contents of which are incorporated herein by reference). The use of the method of the present invention is illustrated in Figs. 5 and 6 as an example for the superconducting magnet system shown in Fig. 2 (i.e. a superconducting magnet system comprising three bulk sub-magnets, a heater, a non-variable thermal impedance and a magnetic field sensor device). It should be noted that the method of the present invention may also be used with other superconducting magnet systems. In general, during the course of the method of the present invention applying the post-correction step, the current strengths of the individual bulk sub-magnets only change slightly, so that the final currents usually deviate from the initial currents by no more than 10%, often no more than 5% each.

[0072] Figure 5 shows the relationship between the time t and the temperature as a function of the time t plotted on the right. excitationIt shows the current I charger (top diagram), an overview of the individual currents in the bulk sub-magnets ("I bulks", second diagram from the top), the total cooling power ("P cool", penultimate diagram) and the heating power applied to the individual bulk sub-magnets ("P heat", last diagram). The focus of Figure 5 is mainly on the initial field cooling step, in other words the step before the post-correction step takes place.

[0073] In the time interval A to B, excitation The magnet has a current of about 125A (amperes). excitation As the current I rises, the bulk sub-magnets reach their critical temperature T crit Since the temperature exceeds excitation After the waiting interval B-C, the cooling power P cool in the bulk sub magnets is increased from 0% to 100% in the interval C-D by bringing down the common cooling stage to its operating temperature (applying a second cryocooler). In the same interval C-D, the heating power in all bulk sub magnets is increased from 0 W (Watts) to 2 W. As a result, the temperature of the bulk sub magnets increases by T crit It drops to less than

[0074] In the initial magnetic cooling step in the time interval D~E, excitation The current I charger is reduced to zero inducing an initial current of about 240-260 kA in the bulk sub magnet according to the initial distribution scheme. The bulk sub magnet is now in an initial state. The initial current in the initial state generates a magnetic field profile in the sample volume of the superconducting magnet system. To increase the uniformity of the magnetic field profile in the sample volume inside the room temperature bore, a post-correction step is then performed. The post-correction step adjusts the initial current, thereby adjusting the magnetic field profile based on the initial current.

[0075] Figure 6 has as its focus the post-correction step 50. Shown as a function of time t plotted on the right are the magnifications of the current in the bulk sub-magnets of Figure 5 ("I bulks", top diagram), the magnifications of the magnetic flux density generated by the bulk sub-magnets as a whole (B pos ", middle diagram, at three positions on the z-axis (axis A), namely the middle position in the centre of the sample volume (indicating the contribution of the middle bulk sub-magnet), the upper position (indicating the contribution of the upper bulk sub-magnet) and the lower position (indicating the contribution of the lower bulk sub-magnet) ("B pos ", middle diagram, compare also Figure 7). z ), as well as the magnification of the heating power applied to the bulk sub magnet in Fig. 5 ("P heat ", last diagram). The solid line refers to the upper bulk sub magnet (compare bulk sub magnet 6a in Fig. 2) i.e. the upper position, the dashed line refers to the middle bulk sub magnet (compare bulk sub magnet 6b in Fig. 2) i.e. the middle position, and the small dashed line refers to the lower bulk sub magnet (compare bulk sub magnet 6c in Fig. 2) i.e. the lower position.

[0076] At time E excitation After switching off the magnets, the current in the upper bulk sub-magnet is at about 260 kA, the current in the middle bulk sub-magnet is at about 242.5 kA and the current in the lower bulk sub-magnet is at about 245 kA. Also at time point E, the magnetic field profile in (and near) the sample volume is measured. Now, after waiting for a relaxation time in the time interval E-F, the magnetic field profile is measured again to ensure that the relaxation of the initial magnetic field cooling step is complete. The magnetic flux density in the upper position is about 6.1350 T (Tesla) and in the middle position is about 6.1345 T. The magnetic flux density in the lower position is about 6.1340 T. Since the correction of the magnetic field profile by the post-correction step reduces, among other things, the magnetic flux density contribution of the individual bulk sub-magnets, the bulk sub-magnet or the position with the smallest magnetic flux density is selected as the preliminary reference value. In this case, the magnetic flux density in the lower position, which is about 6.1340 T, is selected as the preliminary reference value. Compared to this value, the magnetic flux density at the upper and middle positions is too large. The upper and middle bulk sub-magnets are overheated. excitationBulk sub-magnets and their contribution to the magnetic field profile should be reduced in order to increase the uniformity of the magnetic field profile.

[0077] The heating power of each bulk sub magnet is set differently in order to correct the magnetic field profile based on the initial current at time F and to start the desired redistribution of the current in the bulk sub magnet. The heating power of the lower bulk sub magnet is reduced from 2 W to 0 W, since the magnetic flux density in the lower position is already as desired (or at least should not decrease). In this way, the temperature of the lower bulk sub magnet is further reduced and the lower bulk sub magnet is safely far away from magnetic saturation. This prevents a gradual loss of its current (drift) and its contribution to the magnetic field profile is not wasted. The lower bulk sub magnet is assigned to the second part of the bulk sub magnet, which is far away from magnetic saturation. In contrast, the middle bulk sub magnet and the upper bulk sub magnet should lose some current to reduce their contribution to the magnetic field profile. For this purpose, they must be at least approximately magnetically saturated for some time, and they are selected as the first part of the bulk sub magnet that is at least approximately magnetically saturated. Over excitation The heating power of the intermediate bulk sub-magnet increases from 2W to 4W because the magnetic flux density at the intermediate position is larger than desired. excitation The heating power of the assembled upper bulk sub-magnet increases from 2W to 5W because the magnetic flux density at the upper position is even larger than that at the middle position.

[0078] As the heating power in the upper and middle bulk sub magnets increases, the temperature in both bulk sub magnets increases and reaches a certain value (or new equilibrium temperature). This temperature increase reduces their superconducting current carrying capacity so that they are close to or even at magnetic saturation, as is the case here. After time F, the current in the upper bulk sub magnet decreases from about 260 kA to 258.5 kA, now at time G, and the current in the middle bulk sub magnet decreases from about 242.5 kA to 241.5 kA, now at time G. The lower bulk sub magnet then takes over part of the magnetic flux and the corresponding current, its current increases from about 245 kA to 247.5 kA, and the magnetic flux density in the lower position increases to about 6.1342 T (representing the new reference value of the magnetic flux density). It should be noted here that the redistribution of current due to temperature changes in the time interval F to G is not in fact instantaneous and, as a result, arrives somewhat beyond the point in time F at which said redistribution can be considered a mitigation effect.

[0079] After the first change in heating power (at time F), a first time period is waited between times F and G to allow relaxation to complete. Starting at time G, a first measurement of the intermediate magnetic field profile is performed. Then, a second time period is waited between times G and H, after which, at time H, a second measurement of the intermediate magnetic field profile is performed. From these measurements, the current drift characteristics for the bulk sub magnet can be identified. Note that the first time period (wait time) ensures that the subsequent quasi-linear drift can be directly observed in the bulk sub magnet over the second time period.

[0080] Here, the intermediate bulk sub-magnet exhibits a relatively high drift since it is at or very close to its magnetic saturation (above 99% of magnetic saturation). Heating power is maintained since the current drift characteristics in this case are as desired.

[0081] Over the further course of the drift of the intermediate bulk sub-magnet, the magnetic field profile is repeatedly measured (here between time points H to N). At time point K, the current of the intermediate bulk sub-magnet is about 236 kA and the magnetic flux density at the intermediate position approaches the desired magnetic flux density. The heating power is reduced from 4 W to 3.5 W (at time point K), slowing down the drift and allowing precise adjustment of the contribution of the intermediate bulk sub-magnet to the magnetic field profile during the homogenization process. As can be seen from FIG. 6, the drift is slower after time point K than before time point K. Again, the current drift characteristics may be determined as described above (not described in detail) and then the heating power is maintained such that the current drift characteristics in this case (between K and M) are desired.

[0082] The contribution of the intermediate bulk sub magnet to the magnetic field profile continues further but decreases more slowly in the final phase (now the time interval K~M). At time M the magnetic flux density at the intermediate position has reached the desired magnetic flux density (i.e. the reference value). The current in the intermediate bulk sub magnet is now about 235 kA. The heating power is reduced from 3.5 W to 0 W. The temperature of the intermediate bulk sub magnet decreases to a point where the intermediate bulk sub magnet is far away from magnetic saturation and the drift is negligible. The intermediate bulk sub magnet from time M onwards is far away from magnetic saturation and therefore belongs to the second part of the bulk sub magnet.

[0083] From the measurements of the intermediate magnetic field profile at time points G and H, the current drift characteristics involving the upper bulk sub magnet can be identified. Here, the magnetic flux density at the upper position, and therefore the upper bulk sub magnet, shows a moderate drift in the time interval G to H. If this drift were maintained, the total processing time would be about 5000 minutes, and not about 3000 minutes (as intended). Therefore, the heating power in the upper bulk sub magnet increases from 5 W to 5.5 W at time point H, since the current drift characteristics in this case are not required to accelerate the drift. It is noted that the current in the upper bulk sub magnet shows a very small drop from about 258.2 kA to 258.0 kA between time points H and I. Since this current drop is very small, it does not noticeably affect the currents in the intermediate and lower bulk sub magnets in this case.

[0084] After the second change in the heating power (time H), a further first time interval between time H and I is waited to allow the relaxation to complete. At time I, a further first measurement of the intermediate magnetic field profile is performed. Then, a further second time period between time I and time J is waited, after which, at time J, a further second measurement of the intermediate magnetic field profile is performed. From these measurements, the current drift characteristics are again determined. Now, the magnetic flux density at the upper position, and therefore the upper bulk sub-magnet, is at or very close to its magnetic saturation (more than 99% of magnetic saturation) and therefore shows a relatively high drift. The heating power is maintained, since the current drift characteristics in this case are now the one desired.

[0085] Over the course of the drift, the magnetic field profile is repeatedly measured (here between time points J and N). At time point L, the current in the upper bulk sub magnet is about 250 kA and the magnetic flux density at that position approaches the desired magnetic flux density. The heating power is reduced from 5.5 W to 5 W in the upper bulk sub magnet (at time point L), slowing down the drift and allowing precise adjustment of the upper bulk sub magnet's contribution to the magnetic field profile during the homogenization process. Again, the current drift characteristics may be determined as described above (not described in detail). Then, the heating power in the upper bulk sub magnet is further reduced (at time point M) from 5 W to 4.5 W to further slow down the drift.

[0086] The contribution of the upper bulk sub magnet to the magnetic field profile continues, but decreases more slowly in the final phase (now time interval M~N). At time N, the flux density at the upper position approaches the desired flux density (i.e. the reference value) and the current in the upper bulk sub magnet is about 247.5 kA. The heating power is reduced from 4.5 W to 0 W. The temperature of the upper bulk sub magnet decreases to a point where the upper bulk sub magnet is far away from magnetic saturation and drift is negligible.

[0087] The time interval E to O during which the current I bulks in the bulk sub-magnet is changed, in particular fine-tuned by drift, is called the post-correction step 50. During this post-correction step 50, the bulk sub-magnet current I bulks in an initial state with low field homogeneity ("initial current" at time point E) changes to a bulk sub-magnet current I bulks in a final state with high field homogeneity ("final current" at time point N). Typically, the homogeneity in the sample volume during the post-correction step can be increased by a factor of 3 or more, often by a factor of 5 or more, preferably by a factor of 10 or more, most preferably by a factor of 20 or more. At time point O, a final measurement of the magnetic field profile is performed to check whether the post-correction step 50 was successful.

[0088] Figure 7 shows the time evolution of the magnetic field profile near the magnetic center at z=0. The magnetic flux density B is plotted at the top and the position on the z axis is plotted to the right. The time points E (dotted line), K (dashed line), and N (solid line) in Figure 6 are indicated. Also shown are the top, middle, and bottom positions where the magnetic flux density was measured in Figure 5.

[0089] At time point E, the magnetic field profile shows significant inhomogeneity between -15mm and +15mm (here representing the elongation of the sample volume) and B varies between about 6.1340 and 6.1350 Tesla, corresponding to about 163 ppm. The magnetic field profile shows a significant maximum at +15mm near the upper position and also a significantly higher B at the middle position compared to the lower position, i.e., the magnetic field contribution of the upper bulk sub-magnet is quite large and the magnetic field contribution of the middle bulk sub-magnet is somewhat larger.

[0090] Over the course of the drift between points E and N, the uniformity gradually increases as the relative contributions of the upper and middle bulk sub magnets decrease. The final state magnetic field distribution at point N, between -15 mm and +15 mm, now has a non-uniformity of less than 25 ppm.

[0091] FIG. 8 illustrates a method for homogenizing a magnetic field profile in an exemplary embodiment of the present invention for a superconducting magnet system, particularly for the superconducting magnet system of the present invention (e.g., as shown in FIG. 1 ). excitation A schematic flow diagram of the procedure is shown.

[0092] excitation Steps 100 to 105 of the procedure are described in detail in European Patent Application No. 20174683.1, so that the first part of the schematic flow diagram is described here only briefly. The contents of European Patent Application No. 2017468.1 are accordingly incorporated by reference. After start 100, the procedure first comprises an initial magnetic field cooling step 101. During the process: excitation Magnet excitation The current is T crit The bulk magnet rises above the T critCooled to below excitation The main current in the basic distribution system is excitation A magnetic field profile is then induced in the bulk sub-magnets of the bulk magnet according to the intrinsic properties of the magnet and the superconducting magnet system. The resulting magnetic field profile is then mapped (102) and evaluated in step 103.

[0093] If the magnetic field profile is not acceptable in terms of its uniformity within the sample volume, a thermal reset (104) is performed, i.e. the superconducting bulk magnet is discharged and warmed again above its critical temperature. excitation Using the knowledge of the heterogeneity obtained in step (here step 101), a preliminary excitation An optimized field cooling step (105) is then performed. The field profile is then again mapped (102) and evaluated (103). If the captured field profile is still not acceptable, another thermal reset (104) and A separate optimized magnetic field cooling step 105 may be included.

[0094] If the magnetic field profile is acceptable, thermal drift shimming (106), i.e. homogenization using a post-correction step according to the method of the invention, is initiated. For this purpose, parts of the bulk sub-magnets are identified whose contribution to the magnetic field profile is reduced in order to improve the magnetic field homogeneity. Then, each bulk sub-magnet is at least brought close to magnetic saturation, thus increasing the heating power and / or decreasing the cooling power, thus increasing the temperature in each bulk sub-magnet. In this way, a respective drift may be initiated in each bulk sub-magnet, thus decreasing its contribution to the magnetic field profile. The magnetic field profile is iteratively mapped (107) and evaluated for convergence (i.e. the drift characteristics are such that the method of the invention results in the desired homogenous magnetic field profile and can be carried out in a reasonable time frame, for example in a time frame of 3000 minutes) (108).

[0095] If the magnetic field profile does not converge quickly enough towards the desired magnetic field profile (especially taking into account the desired uniformity), the heating power is slightly increased and / or the cooling power is slightly decreased (109) in one or more bulk sub-magnets, thereby increasing the drift in particular in these bulk sub-magnets. If necessary, the initial too fast drift in the individual bulk sub-magnets may be reduced by decreasing the heating power or increasing the cooling power in step 109. The mapping of the magnetic field profile continues (107), the evaluation of the convergence is repeated (108), and, if necessary, a further modification step (109) of modifying the temperature distribution in the bulk sub-magnets may also be included. It is noted that in all these steps, no measurement of the temperature of the bulk sub-magnets is necessary, since knowledge of the temperature of the bulk sub-magnets is not necessary for the magnetic field profile adjustment. It is sufficient to periodically measure the magnetic field profile and observe the changes in the magnetic field profile and identify the drift characteristics of the bulk sub-magnets in particular.

[0096] If the magnetic field profile converges fast enough, the heating and / or cooling power levels in each bulk sub-magnet are kept. The magnetic field profile is again iteratively mapped (110). Then, it is evaluated (111) whether the magnetic field quality of the magnetic field profile is close to the final magnetic field quality (desired magnetic field quality). A typical criterion for identifying whether the magnetic field profile is close to the final magnetic field quality ("closed") may be a residual deviation (RD) of the magnetic flux density (at a particular position) from the final magnetic flux density (at that position) being less than or equal to a limit value, preferably compared to the original deviation (OD) of the magnetic flux density (at that position) from the final magnetic flux density (at that position) at the start of the post-correction step. Typically, the limit value is selected as a relative limit value RLM of the ratio RD / OD, preferably RLM≦25%, more preferably 5%≦RLM≦20%. It should be noted that the final magnetic flux density at that position generally corresponds to a reference value that is the minimum magnetic field density in the magnetic field profile (for all positions in the sample volume) after the last heating power increase or cooling power decrease.

[0097] If the magnetic field profile is not close to the final magnetic field quality, the current drift is allowed to continue for a small waiting time 112. Mapping of the magnetic field profile continues 110 and the evaluation of whether the magnetic field profile is close to the final magnetic field quality is repeated 111. If necessary, mapping of the magnetic field profile is performed 112.

[0098] If the magnetic field profile is close to the final magnetic field quality, the heating power is decreased and / or the cooling power is increased (113) in order to slow down the drift of the magnetic field profile. It should be noted that this may be done separately for the different bulk sub magnets. In this step 113, it may be checked whether the new drift characteristics are as desired, and if not, the heating power is further decreased and / or the cooling power is increased. The mapping of the magnetic field profile continues (114) and waits until the desired magnetic field profile is reached. Once the desired magnetic field quality is reached, the heating is stopped and / or the cooling power is increased to a maximum (115), so that no significant drift occurs anymore and the procedure is finally terminated (116). The entire method was performed without measuring the exact temperature in the bulk sub magnets. [Explanation of symbols]

[0099] 1. Superconductivity excitation Device 2. Superconducting magnet system 3 excitation magnet 3a excitation Boa 4. Cryostat 5. Superconducting bulk magnets 6a, 6b, 6c Bulk Sub Magnets 7 Superconducting bore 7a Room temperature bore 8a,8b intermediate 8c Further intermediates 9 Common cooling stage 10 Sample Volume 11 Magnetic field sensor device 11a, 11a', 11a'' (magnetic field sensor device) sensor 11b (Sensor) Placement 12 Moving stage 12a Straight Connector 12b Angled Connector 13 Cryogenic Cooling System 14 Adjustment unit 15a, 15b, 15c Electric heater elements 16a, 16b, 16c Thermal switches 17a, 17b, 17c Thermal connections 18 Electronic Control Unit 19 The first cryocooler 19a First cryocooler cold stage 20 Thermal Cryocooler Impedance 21 Port 22 Supply Line 23 Second Cryocooler 23a Second cryocooler cold stage 24 Separate auxiliary cryostat 25 Auxiliary Supply Line 26a, 26b, 26c Non-variable thermal impedance 27 Stationary Stage 28a, 28b, 28c Variable Thermal Impedance 50 Post-correction steps 100 start 101 Initial magnetic field cooling 102 Mapping the magnetic field profile 103 Evaluation of magnetic field profile 104 Heat Reset 105 Optimized Magnetic Cooling 106 Start thermal drift shimming 107 Continuous mapping of magnetic field profile 108 Convergence Assessment 109 Adjusting Heating and / or Cooling Power 110Continuous mapping of magnetic field profile 111 Evaluate whether the field quality is close to the final field quality 112 Waiting Time 113 Decreased heating power and / or increased cooling power 114 Wait until final field quality is achieved 115 Stop heating and maximum cooling 116 End A (central axis of a superconducting magnet system)

Claims

1. A method for homogenizing a magnetic field profile of a superconducting magnet system (2), comprising: The superconducting magnet system (2) comprises: a cryostat (4) having a room temperature bore (7a); a superconducting bulk magnet (5) housed within the cryostat (4) and arranged coaxially with the room temperature bore (7a); a cryogenic cooling system (13) adapted to cool said superconducting bulk magnet (5); Equipped with The superconducting bulk magnet (5) comprises at least N axially stacked bulk sub-magnets (6a-6c), where N>3; In an initial state, the bulk sub-magnets (6a-6c) carry respective initial currents having relative proportions according to an initial distribution scheme; The method includes a post-correction step (50) of modifying the initial currents to final currents having relative proportions according to a final distribution scheme different from the initial distribution scheme, a magnetic field profile of the superconducting bulk magnet (5) based on the final current is more uniform than a magnetic field profile based on the initial current; said cryogenic cooling system (13) being adapted to separately control the temperature of each bulk sub-magnet (6a-6c); To change the initial current to the final current, the temperatures of at least some of the bulk sub-magnets (6a-6c) are selected to be at least temporarily different from each other, so that for a first portion of the bulk sub-magnets (6a-6c), the bulk sub-magnets (6a-6c) in this first portion are at least approximately magnetically saturated, in particular at least 99% relative magnetic saturation, for a second portion of said bulk sub-magnets (6a-6c), said bulk sub-magnets (6a-6c) in this second portion are far from magnetic saturation, in particular at most 95% relative magnetic saturation, the temperature of the bulk sub-magnets (6a-6c) is selected by controlling a heating power and / or a cooling power in the bulk sub-magnets without measuring the temperature of the bulk sub-magnets in order to change the initial current to the final current, and the heating powers are set at least temporarily different from one another and / or the cooling powers are set at least temporarily different from one another for at least the part of the bulk sub-magnets (6a-6c); During the post-correction step (50), an intermediate magnetic field profile of the superconducting magnet system (2) is repeatedly measured (107, 110) until a desired magnetic field profile based on the final currents is obtained, and between measurements, the heating and / or cooling powers of at least some of the bulk sub-magnets (6a-6c) are changed (109, 113, 115) and / or a certain time is waited (114). The method comprising:

2. The method according to claim 1, characterized in that the superconducting magnet system (2) is designed without a thermal sensor for measuring the temperature of the bulk sub-magnets (6a-6c).

3. 3. The method according to claim 1 or 2, characterized in that in the first part, the heating power in the bulk sub-magnets (6a-6c) is selected to be at least temporarily higher compared to the second part and / or in that in the first part, the cooling power in the bulk sub-magnets (6a-6c) is selected to be at least temporarily lower compared to the second part.

4. 3. The method according to claim 1 or 2, characterized in that if from at least one measured intermediate magnetic field profile one or more bulk sub-magnets (6a-6c), hereinafter referred to as over-excited bulk sub-magnets (6a-6c), are identified (108), which have a reduced contribution to the magnetic field profile in order to increase magnetic field homogeneity, then for a time period after the measurement of the intermediate magnetic field profile (107), the cooling power is selected to be smaller and / or the heating power is selected to be larger (109) for one or more respective over-excited bulk sub-magnets (6a-6c) in order to reduce the contribution of the over-excited bulk sub-magnets (6a-6c) in comparison to a bulk sub-magnet (6a-6c) that is not over-excited.

5. 5. The method according to claim 4, characterized in that for at least a portion of the over-excited bulk sub-magnets (6a-6c), the amount by which the cooling power is selected to be smaller and / or the heating power is selected to be larger for each over-excited bulk sub-magnet (6a-6c) compared to a bulk sub-magnet (6a-6c) that is not over-excited is reduced over time (113) in a final phase reducing the contribution of each bulk sub-magnet (6a-6c) to the magnetic field profile.

6. At least one occasion after changing (109) the heating and / or cooling power in at least some of the bulk sub-magnets (6a-6c), a first period of time is waited, then at least A first measurement of the intermediate magnetic field profile is taken (107, 110); A second period of time is waited; A second measurement of the intermediate magnetic field profile is taken (107, 110); determining a current drift characteristic of the intermediate magnetic field profile from at least the first and second measurements; Based on the identified current drift characteristics, a next change in the heating and / or cooling power in at least some of the bulk sub-magnets (6a-6c) and / or a next time to wait is determined (108, 111).

3. The method according to claim 1 or 2.

7. a cryostat (4) having a room temperature bore (7a); a superconducting bulk magnet (5) housed within the cryostat (4) and arranged coaxially with the room temperature bore (7a); a cryogenic cooling system (13) adapted to cool said superconducting bulk magnet (5); A superconducting magnet system (2) comprising: the superconducting bulk magnet (5) comprises at least N axially stacked bulk sub-magnets (6a-6c), where N>3; the bulk sub-magnets (6a-6c) are substantially ring-shaped and arranged coaxially with the room temperature bore (7a); Between each two axially adjacent bulk sub-magnets (6a-6c), an intermediate body (8a, 8b) is disposed; said intermediate body (8a, 8b) being substantially ring-shaped and arranged coaxially with said room temperature bore (7a); The bulk sub-magnets (6a to 6c) are supported by the intermediate bodies (8a, 8b); said intermediate bodies (8a, 8b) are made of a non-metallic insulating material having a specific thermal conductivity smaller than that of the material of said bulk sub-magnets (6a-6c); said cryogenic cooling system (13) being adapted to separately control the temperature of each bulk sub-magnet (6a-6c); for each bulk sub-magnet (6a-6c) there is present a regulating unit (14) for regulating the heating and / or cooling power in said respective bulk sub-magnet (6a-6c), the superconducting magnet system (2) further comprising a magnetic field sensor device (11) for measuring a magnetic field profile within a sample volume (10) of the room temperature bore (7a); The superconducting magnet system (2) is configured without a thermal sensor for measuring the temperature of the bulk sub-magnets (6a-6c). A superconducting magnet system (2).

8. for each bulk sub-magnet (6a-6c), there is a heater element (15a-15c) thermally connected to said respective bulk sub-magnet (6a-6c); In particular, said heater elements (15a-15c) are controlled by said regulating unit (14), said regulating unit (14) being configured to set variable heating powers of said heater elements (15a-15c) to said respective bulk sub-magnets (6a-6c), In particular, said heater elements (15a to 15c) are electric heater elements (15a to 15c).

8. A superconducting magnet system (2) according to claim 7, characterized in that

9. said cryogenic cooling system (13) comprising a common cooling stage (9) for all bulk sub-magnets (6a-6c); and for each bulk sub-magnet (6a-6c) there is a thermal connection (17a-17c) from said common cooling stage (9) to said respective bulk sub-magnet (6a-6c), In particular, said thermal connections (17a-17c) include thermal switches (16a-16c) controlled by said regulating unit (14).

9. A superconducting magnet system (2) according to claim 7 or 8, characterized in that

10. 10. The superconducting magnet system (2) according to claim 9, characterized in that the thermal connections (17a-17c) include variable thermal impedances (28a-28c) controlled by the adjustment unit (14), the adjustment unit (14) being configured to set variable cooling powers in the respective bulk sub-magnets (6a-6c).

11. 9. The superconducting magnet system (2) according to claim 7 or 8, characterized in that the magnetic field sensor device (11) comprises at least one sensor (11a, 11a', 11a'') arranged on a moving stage (12), whereby the at least one sensor (11a, 11a', 11a'') can be moved within the sample volume (10) in order to determine the magnetic field profile within the sample volume (10) by repeated readout of the at least one sensor (11a, 11a', 11a'') at different positions within the sample volume (10).

12. the magnetic field sensor device (11) comprises an arrangement (11b) of sensors (11a, 11a', 11a'') distributed in the sample volume (10), for determining the magnetic field profile in the sample volume (10) by parallel readout of the sensors (11a, 11a', 11a'') in the arrangement (11b) fixed in a predetermined position, Superconducting magnet system (2) according to claim 7 or 8, characterized in that said arrangement (11b) comprises at least N sensors (11a, 11a', 11a'').

13. The superconducting magnet system (2) further comprises an electronic control unit (18) for automatically homogenizing the magnetic field profile in the room temperature bore (7a), the electronic control unit (18) being adjusted for automatically homogenizing the magnetic field profile of the superconducting bulk magnets (6a-6c) according to the method of claim 1 or 2, the electronic control unit (18) repeatedly receiving a measured intermediate magnetic field profile measured by the magnetic field sensor device (11), and the electronic control unit (18) automatically controls the heating and / or cooling powers in the bulk sub-magnets (6a-6c) based on the measured intermediate magnetic field profile without receiving or evaluating temperature data of the bulk sub-magnets (6a-6c).

14. Use of a superconducting magnet system (2) according to claim 7 or 8 in a method according to claim 1 or 2.

Citation Information

Patent Citations

  • Bulk magnet structure, magnet system for NMR using said bulk magnet structure, and magnetization method for bulk magnet structure

    EP3492941A1

  • Superconducting magnet system, with individual temperature control of axially stacked bulk sub-magnets

    EP3910651B1

  • Method for charging a superconductor magnet system, with sequential cooling of superconductor bulk sub-magnets

    EP4080527B1

  • Magnetic field generator and nuclear magnetic resonance unit

    JP2007129158A

  • Method for magnetizing superconductor bulk magnet, with generating auxiliary magnetic field in superconductor bore