Forming method for reducing wrinkles of thermal diaphragm by prolonging length of transition area

By extending the transition zone length and filling the transition zone steps according to the thickness and drop-out ratio, the longitudinal folding problem caused by uneven prepreg thickness in the thermal insulation process is solved, and the profile quality of composite parts is significantly improved.

CN118991079AActive Publication Date: 2024-11-22SHANGHAI AIRCRAFT MFG
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202410998456.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-24
Publication Date
2024-11-22
Estimated Expiration
2044-07-24

AI Technical Summary

Technical Problem

When using the thermal diaphragm process to make composite parts with larger thickness, the uneven thickness of the prepreg blast causes lateral extrusion of the membrane at the transition zone, causing longitudinal folds, and affecting the quality of the part shape.

Method used

通过延长过渡区长度,根据预浸料的厚度和丢层比例补平过渡区阶梯,增大丢层比例,减小隔膜对过渡区的侧向挤压,从而减少或消除褶皱的发生。 Specific steps include placing a non-porous isolation film on the prepreg, vacuum pre-compression, using waste to cut and lay out to extend the transition zone, tight fit, and diaphragm molding in a thermal isolation machine.

Benefits of technology

Effectively reduce or eliminate the folds of the thermal insulation membrane, improve the quality of the part shape, and ensure the stability and quality of the molding process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118991079A_ABST
    Figure CN118991079A_ABST
Patent Text Reader

Abstract

The invention discloses a forming method for reducing wrinkles of a thermal diaphragm by prolonging the length of a transition area, which comprises the following steps of: S1, after automatic tape laying is completed, placing a layer of non-porous isolating membrane on a prepreg blank, and vacuumizing and pre-compacting for about 15 minutes to enable the transition area to be more obvious; s2, according to the thickness of a transition area of the part and the ratio of lost layers, a blanking procedure is manufactured by combining the size of a part blank, and a waste prepreg is used for blanking; s3, according to the thickness of the transition area and the layer loss proportion, waste prepreg is used for being laid on the blank along the transition area, waste is used for being in butt joint with the blank, so that the transition area is prolonged, and the layer loss proportion is increased; s4, vacuumizing and pre-compacting for about 15 minutes, so that the waste material and the prepreg blank are tightly attached, and the waste material and the prepreg blank are separated by using a non-porous isolating membrane; and S5, feeding the compacted prepreg blank into a thermal diaphragm machine for diaphragm separation. According to the method, the steps of the transition area are filled in by using the prepreg according to the thickness and the layer loss ratio, and the layer loss ratio of the transition area is increased, so that lateral extrusion of the diaphragm on the transition area is reduced, the occurrence of wrinkles can be greatly reduced or completely eliminated, and the molded surface quality of the part is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of thermal diaphragm forming technology for aerospace composite materials, and in particular to a forming method for reducing thermal diaphragm wrinkles by extending the length of a transition zone. Background Art

[0002] The hot diaphragm process is to place the prepreg flat plate laid by hand or automatic tape laying process between two layers of diaphragms with higher ductility, and transfer the whole to the hot diaphragm machine. The flat plate is pressed into a preform of complex shape by vacuum negative pressure and infrared heating. It has fast production speed, high molding quality and good stability. It has become an important low-cost manufacturing technology and is widely used in the field of aerospace composite parts manufacturing at home and abroad.

[0003] The hot diaphragm process is used to make thicker composite parts. The diaphragm is covered on the prepreg blank. Due to the uneven thickness of the prepreg blank, the diaphragm will produce lateral extrusion in the transition zone, causing large longitudinal wrinkles on the flat blank in the transition zone, affecting the surface quality of the part. Summary of the invention

[0004] The purpose of the present invention is to overcome the shortcomings of the prior art and provide a molding method for reducing the wrinkles of the thermal diaphragm by extending the length of the transition zone, using prepreg to fill the transition zone steps according to the thickness and layer loss ratio, and by increasing the layer loss ratio of the transition zone, reducing the lateral extrusion of the diaphragm on the transition zone, thereby greatly reducing or completely eliminating the occurrence of wrinkles and improving the surface quality of the part.

[0005] In order to achieve the above object, the technical solution adopted by the present invention is:

[0006] A forming method for reducing heat diaphragm wrinkles by extending the length of the transition zone, comprising the following steps:

[0007] Step S1: After the automatic tape laying is completed, a layer of non-porous isolation film is placed on the prepreg blank, and vacuum pre-compacted for about 15 minutes to make the transition zone more obvious;

[0008] Step S2: According to the thickness of the transition zone of the part and the ratio of the lost layers, the blanking procedure is made in combination with the size of the part blank, and waste / expired prepreg is used for blanking;

[0009] Step S3: according to the thickness of the transition zone and the layer loss ratio, using waste prepreg to lay on the blank along the transition zone, and using the waste to butt with the blank to extend the transition zone and increase the layer loss ratio;

[0010] Step S4: vacuum pre-compacting for about 15 minutes to make the waste material and the prepreg blank fit tightly, and a non-porous isolation film is used to separate the two;

[0011] Step S5: sending the compacted prepreg blank into a hot diaphragm machine for diaphragm.

[0012] Furthermore, specific parameters of the extended transition zone are: the angle between the first line between the upper right end of the first layer of blank and the upper right end of the bottom layer of blank and the horizontal plane / horizontal line is a, the angle between the second line between the upper right end of the first layer of waste and the upper right end of the bottom layer of waste and the horizontal plane / horizontal line is b, b / a=0.05-0.25; the bottom layer of blank has a length L1, and the bottom layer of waste has a length L2, L1 / L2=0.1-0.3.

[0013] Furthermore, the angle b / a=0.14-0.15, and the length L1 / L2=0.18-0.2.

[0014] The present invention provides a molding method for reducing heat diaphragm wrinkles by extending the length of the transition zone, using prepreg to fill the transition zone steps according to the thickness and layer loss ratio, and by increasing the layer loss ratio of the transition zone, reducing the lateral extrusion of the diaphragm on the transition zone, thereby greatly reducing or completely eliminating the occurrence of wrinkles and improving the surface quality of the parts. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 It is a schematic diagram of the force analysis of the cause of the thermal diaphragm wrinkles of the present invention;

[0016] Figure 2 This is a comparative schematic diagram of extending the transition zone of the present invention;

[0017] Figure 3 This is a schematic diagram of the effect before the transition zone is extended in the present invention;

[0018] Figure 4 This is a schematic diagram of the effect of extending the transition zone of the present invention. DETAILED DESCRIPTION

[0019] In order to make the technical solution and advantages of the present invention clearer, the technical solution of the present invention will be further described in detail in detail with reference to the accompanying drawings. It can be understood that the specific embodiments described here are only partial embodiments of the present invention, which are only used to explain the present invention, not to limit the present invention. It should be noted that, for the convenience of description, only the parts / structures related to the present invention are shown in the accompanying drawings, and other related parts can refer to the general design. In the absence of conflict, the embodiments of the present invention and the technical features in the embodiments can be combined with each other to obtain new embodiments.

[0020] Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention. In addition, unless otherwise defined, the technical terms or scientific terms used in the description of the present invention should be the common meanings understood by ordinary technicians in the field to which the present invention belongs.

[0021] The present invention will be further described in detail below in conjunction with the accompanying drawings.

[0022] like Figure 1-4 As shown, a forming method for reducing the wrinkles of a thermal diaphragm by extending the length of a transition zone comprises the following steps:

[0023] Step S1: After the automatic tape laying is completed, a layer of non-porous isolation film is placed on the prepreg blank, and vacuum pre-compacted for about 15 minutes to make the transition zone more obvious;

[0024] Step S2: according to the thickness of the transition zone of the part and the ratio of the lost layers, a blanking procedure is prepared in combination with the size of the part blank, and prepreg (waste / expired prepreg) is used for blanking;

[0025] Step S3: According to the thickness of the transition zone and the layer loss ratio, waste prepreg is used to lay on the blank along the transition zone, and the waste is used to connect with the blank to extend the transition zone and increase the layer loss ratio, such as Figure 2 As shown;

[0026] Step S4: vacuum pre-compacting for about 15 minutes to make the waste material and the prepreg blank fit tightly, and a non-porous isolation film is used to separate the two;

[0027] Step S5: sending the compacted prepreg blank into a hot diaphragm machine for diaphragm.

[0028] Among them, in step S3, the specific parameters of the extended transition zone are: the angle between the first line between the upper right end of the first layer of blank and the upper right end of the bottom layer of blank and the horizontal plane / horizontal line is a, the angle between the second line between the upper right end of the first layer of waste and the upper right end of the bottom layer of waste and the horizontal plane / horizontal line is b, b / a=0.1-0.2, preferably 0.14-0.15; the bottom layer of blank has a length L1, and the bottom layer of waste has a length L2, L1 / L2=0.13-0.23, preferably 0.18-0.19.

[0029] like Figure 1 As shown, the diaphragm will produce lateral extrusion in the transition zone, resulting in large longitudinal wrinkles in the flat blank in the transition zone.

[0030] like Figure 2As shown, prepreg is used to fill the transition zone steps according to the thickness and layer loss ratio. By increasing the layer loss ratio of the transition zone (the specific parameters for extending the transition zone are: b / a=0.1-0.2, preferably 0.14-0.15; L1 / L2=0.13-0.23, preferably 0.18-0.19), the lateral extrusion of the diaphragm on the transition zone is reduced, thereby greatly reducing or completely eliminating the occurrence of wrinkles and improving the surface quality of the parts.

[0031] The present invention provides a molding method for reducing heat diaphragm wrinkles by extending the length of the transition zone, using prepreg to fill the transition zone steps according to the thickness and layer loss ratio, and by increasing the layer loss ratio of the transition zone, reducing the lateral extrusion of the diaphragm on the transition zone, thereby greatly reducing or completely eliminating the occurrence of wrinkles and improving the surface quality of the parts.

[0032] The above-mentioned implementation modes are for explanation of the present invention rather than limitation of the present invention. It can be understood that various changes, modifications, substitutions and variations can be made to these embodiments without departing from the principle and spirit of the present invention. The scope of protection of the present invention is defined by the attached claims and their equivalents.

Claims

1. A forming method for reducing heat diaphragm wrinkles by extending the length of the transition zone, comprising the following steps: Step S1: After the automatic tape laying is completed, a layer of non-porous isolation film is placed on the prepreg blank, and vacuum pre-compacted for about 15 minutes to make the transition zone more obvious; Step S2: According to the thickness of the transition zone of the part and the ratio of the lost layers, the blanking procedure is made in combination with the size of the part blank, and waste / expired prepreg is used for blanking; Step S3: according to the thickness of the transition zone and the layer loss ratio, using waste prepreg to lay on the blank along the transition zone, and using the waste to butt joint with the blank to extend the transition zone and increase the layer loss ratio; Step S4: vacuum pre-compacting for about 15 minutes to make the waste material and the prepreg blank fit tightly, and a non-porous isolation film is used to separate the two; Step S5: sending the compacted prepreg blank into a hot diaphragm machine for diaphragm.

2. A forming method for reducing heat diaphragm wrinkles by extending the length of the transition zone as claimed in claim 1, characterized in that: The specific parameters of the extended transition zone are: the angle between the first connecting line between the upper right end of the first layer of blank and the upper right end of the bottom layer of blank and the horizontal plane / horizontal line is a, the angle between the second connecting line between the upper right end of the first layer of waste and the upper right end of the bottom layer of waste and the horizontal plane / horizontal line is b, b / a=0.05-0.25; the bottom layer of blank has a length L1, and the bottom layer of waste has a length L2, L1 / L2=0.1-0.

3.

3. A forming method for reducing heat diaphragm wrinkles by extending the length of the transition zone as claimed in claim 2, characterized in that: Angle b / a=0.14-0.15, length L1 / L2=0.18-0.2.

Citation Information

Patent Citations

  • Automatic manufacturing tool and process for composite stringer and beam structure workpieces

    CN114986936A

  • Forming method of composite material special-shaped cylindrical structural member

    CN116834327A

  • Flat plate material sheet tape laying method and composite material beam manufacturing method

    CN116945638A

  • Method for producing parts made of thermosetting composite by laying of fibres of preimpregnated material

    WO2014057207A2

  • Fabrication of complex-shaped composite structures

    WO2017127772A1