High-purity calcium fluoride, and preparation method and application thereof

By strictly controlling the reaction conditions and purification process under an inert atmosphere, high-purity calcium fluoride was prepared, solving the problems of insufficient purity and transmittance in existing technologies, and realizing the preparation of high-purity calcium fluoride suitable for optical devices.

CN122403483APending Publication Date: 2026-07-17HENAN FLUORINE BASED NEW MATERIAL TECH CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
HENAN FLUORINE BASED NEW MATERIAL TECH CO LTD
Filing Date
2026-05-12
Publication Date
2026-07-17

AI Technical Summary

Technical Problem

Existing technologies make it difficult to prepare high-purity, high-transmittance calcium fluoride crystals, especially optical-grade CaF2 single crystals/powders. Impurity elements such as oxygen and metal ions affect their optical properties, and existing methods cannot meet the 4-5N level requirements in terms of purity and transmittance.

Method used

High-purity calcium chloride and potassium fluoride are used as raw materials. The reaction is carried out in an inert atmosphere through dissolution, recrystallization and dropwise addition. The reaction conditions, including temperature, concentration and atmosphere, are strictly controlled. Impurities are removed by multiple filtrations and drying to prepare high-purity calcium fluoride.

Benefits of technology

The high-purity calcium fluoride prepared has a purity of over 99.99%, an oxygen content of less than 200 ppm, and a uniform particle size distribution, meeting the requirements of optical devices. It is also safe to operate and easy to industrialize.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
Patent Text Reader

Abstract

本发明属于无机材料制备技术领域,具体涉及一种高纯氟化钙及其制备方法与应用。本发明中高纯氟化钙的制备过程包括:先将氯化钙原料和氟化钾原料进行提纯后得到纯化氯化钙和纯化氟化钾;再将纯化氯化钙和纯化氟化钾分别溶于高纯水中得到氯化钙溶液和氟化钾溶液;最后将氯化钙溶液加入氟化钾溶液中反应,反应结束后进行固液分离得到氟化钙固体,氟化钙固体经洗涤、吹扫、干燥后得到高纯氟化钙。通过该方法制备得到的高纯氟化钙收率为98%以上,其纯度在99.99%以上,其含氧量在200ppm以下。金属杂质总含量在0.1ppm以下,硫酸根和氯含量小于1ppm,粒径分布D90在2μm以上,满足一般光学器件的使用要求。
Need to check novelty before this filing date? Find Prior Art

Citation Information

Patent Citations

  • Synthesis method of high-purity calcium fluoride raw material

    CN116332216A

  • Ultra-pure calcium fluoride crystal raw material and preparation method thereof

    CN120922904A