A nitrogen-heterocyclic carbene ruthenium complex coordinated by σ-π chelation mode, its preparation method and application
By preparing nitrogen heterocyclic carbene ruthenium complexes coordinated in a σ-π chelate mode, the dependence of existing photocatalysts on photosensitizers and inert gases in the catalytic reaction of norbornene was solved, and stable catalysis of norbornene to form polynorbornene under red light was achieved, with the advantages of high conversion rate and low cost.
Patent Information
- Application Number
- CN202611322568.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-28
- Publication Date
- 2026-11-17
AI Technical Summary
Existing photocatalysts require photosensitizers or high-energy light sources to catalyze the ring-opening metathesis polymerization of norbornene, and are unstable in air and cannot work effectively under inert gas protection.
A nitrogen-heterocyclic carbene ruthenium complex coordinated in a σ-π chelate mode was developed and prepared by reacting it with a p-cymene ruthenium complex under red light to form a catalytically active nitrogen-heterocyclic carbene ruthenium complex capable of catalyzing the ring-opening metathesis polymerization of norbornene in an air atmosphere.
The method achieves the catalytic formation of polynorbornene under red light without the need for photosensitizers and inert gas protection. It features stable catalytic activity, simple operation, low cost, and high conversion rate.
Smart Images

Figure CN123106777A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of organometallic catalysis technology, and in particular to a nitrogen heterocyclic carbene ruthenium complex coordinated in a σ-π chelate mode, its preparation method, and its application. Background Technology
[0002] The literature [J. Am. Chem. Soc. 2009, 131, 2038-2039.] reports a ruthenium catalyst containing an easily leaving acetylacetone ligand that can catalyze ring-closure metathesis (RCM) and ring-opening metathesis polymerization (ROMP) in the presence of a photoacid generator and under ultraviolet light irradiation, thus promoting the development of photocatalytic olefin metathesis reactions.
[0003] The literature [ACS Catal. 2020, 10, 2033-2038.] reports two Grubbs-type ruthenium catalysts coordinated with phosphite ligands, and tests their blue light catalytic activity for RCM and ROMP. The wavelength of the photocatalytic ROMP was pushed into the blue light region, but due to the presence of the alkylene carbene structure in the Grubbs-type catalyst, it requires inert gas protection during catalysis.
[0004] The literature [J. Am. Chem. Soc. 2019, 141, 6791-6796.] reports a blue-light-controlled olefin metathesis catalyst of Grubbs-type bisNHC ruthenium complex, achieving blue-light-controlled RCM. However, it is entirely dependent on photosensitizers, and also suffers from poor water and oxygen tolerance of the catalytically active species due to the presence of alkylene carbenes, thus requiring inert gas protection during catalysis.
[0005] The literature [Nature Chemistry. 2026, 18, 51-60.] reports an infrared light-controlled ROMP method, pioneering a substrate-centered light-controlled system. However, the activation of this system depends on the photothermal effect generated by the absorption of infrared light by the gold bipyramid encapsulated in silica. Furthermore, the substrate is limited to norbornadiene and its derivatives, and the catalysis still uses the Grubbs series catalysts, which have poor tolerance to water and oxygen.
[0006] The aforementioned literature reports that achieving ROMP for photocatalytic norbornene has problems such as requiring photosensitizers or other additives, requiring higher-energy blue or ultraviolet light, or being unable to be carried out without inert gas protection. Summary of the Invention
[0007] In view of this, the purpose of this invention is to provide a nitrogen-containing heterocyclic carbene ruthenium complex coordinated in a σ-π chelate mode, its preparation method, and its applications. The nitrogen-containing heterocyclic carbene ruthenium complex coordinated in a σ-π chelate mode provided by this invention can achieve ring-opening metathesis polymerization of norbornene to form polynorbornene under red light without the aid of additives or inert gas protection.
[0008] To achieve the above-mentioned objectives, the present invention provides the following technical solution: This invention provides a nitrogen heterocyclic carbene ruthenium complex coordinated in a σ-π chelate mode, having the structure shown in Formula 1: Formula 1.
[0009] This invention also provides a method for preparing nitrogen heterocyclic carbene ruthenium complexes coordinated in the σ-π chelate mode as described in the above technical solution, comprising the following steps: The p-cymene ruthenium complex with the structure shown in Formula 2 was mixed with an organic solvent and reacted under red light irradiation to obtain the nitrogen heterocyclic carbene ruthenium complex coordinated in the σ-π chelate mode. Equation 2.
[0010] Preferably, the wavelength of the red light is 640~680nm.
[0011] Preferably, the reaction temperature is 10~30℃ and the time is 12~24h; the reaction is carried out under stirring conditions.
[0012] Preferably, after the reaction is completed, the process further includes: subjecting the obtained reaction solution to a first rotary evaporation to obtain a viscous substance; mixing the viscous substance with ethanol and subjecting it to a second rotary evaporation to obtain a rotary evaporation system; performing solid-liquid separation on the rotary evaporation system to obtain a solid and a liquid, respectively; and washing the solid with ice-cold ethanol to obtain the nitrogen heterocyclic carbene ruthenium complex coordinated in the σ-π chelate mode.
[0013] This invention also provides the application of the nitrogen heterocyclic carbene ruthenium complexes coordinated in the σ-π chelate mode described above, or the nitrogen heterocyclic carbene ruthenium complexes prepared by the preparation method described above, in catalytic ring-opening metathesis polymerization reactions.
[0014] This invention also provides a method for preparing polynorbornene, comprising the following steps: Norbornene, a catalyst, and an aprotic solvent were mixed and subjected to a ring-opening metathesis polymerization reaction under red light irradiation to obtain the polynorbornene. The catalyst is a nitrogen heterocyclic carbene ruthenium complex coordinated in a σ-π chelate mode as described in the above technical solution, or a nitrogen heterocyclic carbene ruthenium complex coordinated in a σ-π chelate mode prepared by the preparation method described in the above technical solution.
[0015] Preferably, the molar ratio of norbornene to catalyst is 1:0.0005~0.02.
[0016] Preferably, the wavelength of the red light is 620~680nm; the temperature of the ring-opening metathesis polymerization reaction is 10~30℃, and the time is 6~24h; the ring-opening metathesis polymerization reaction is carried out under stirring conditions.
[0017] Preferably, after the ring-opening metathesis polymerization reaction, the method further includes: quenching the ring-opening metathesis polymerization reaction to obtain a quenching system; and purifying the quenching system by column chromatography to obtain the polynorbornene. The eluent used in the column chromatography purification was dichloromethane.
[0018] This invention provides a nitrogen heterocyclic carbene ruthenium complex coordinated in a σ-π chelation mode.
[0019] The σ-π chelate-coordinated nitrogen heterocyclic carbene ruthenium complex provided by this invention contains an asymmetric nitrogen heterocyclic carbene and has catalytic activity. It can exist stably at room temperature and in solid conditions and can catalyze the ring-opening metathesis polymerization of norbornene (NB) to form polynorbornene under 620~680nm red light irradiation and air atmosphere without the need for additional photosensitizers, making it a good red light catalyst; its catalytic activity is weak in the absence of light irradiation. Attached Figure Description
[0020] Figure 1 The 1H NMR spectrum of the bright red solid obtained in Example 1; Figure 2 The carbon NMR spectrum of the bright red solid obtained in Example 1; Figure 3 ESI of the bright red solid obtained in Example 1 + Mass spectrum; Figure 4 The UV-Vis absorption spectrum of the bright red solid obtained in Example 1 is shown below. Figure 5 This is a coordination environment diagram of the nitrogen heterocyclic carbene ruthenium complex coordinated in the σ-π chelation mode obtained in Example 1; Figure 6 The crystal structure diagram of the nitrogen heterocyclic carbene ruthenium complex coordinated in the σ-π chelate mode obtained in Example 1 is shown. Figure 7 The image shows the 1H NMR spectrum of the quenched ring-opening metathesis polymerization reaction solution obtained in Example 1. Detailed Implementation
[0021] If certain terms are used in this specification to refer to specific substances or methods, those skilled in the art will understand that different regions may use different names to refer to the same substance or method. This specification does not use differences in name as a way to distinguish substances or methods. The term "comprising" as used throughout this specification is an open-ended term and should be interpreted as "comprising but not limited to". "Probably" means that within an acceptable margin of error, those skilled in the art can solve the technical problem and substantially achieve the technical effect within a certain margin of error. The following descriptions in this specification are preferred embodiments for carrying out this application; however, these descriptions are for the purpose of illustrating the general principles of this application and are not intended to limit the scope of this application.
[0022] It should also be noted that the terms "comprising," "including," or any other variations thereof are intended to cover non-exclusive inclusion, such that a product or system comprising a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such a product or system. Without further limitation, an element defined by the phrase "comprising one..." does not exclude the presence of other identical elements in the product or system that includes said element.
[0023] This invention provides a nitrogen heterocyclic carbene ruthenium complex (NHC-Ru, Ru2) coordinated in a σ-π chelate mode, having the structure shown in Formula 1: Formula 1.
[0024] In this invention, when the nitrogen heterocyclic carbene ruthenium complex coordinated in the σ-π chelate mode is denoted as NHC-Ru, NHC represents nitrogen heterocyclic carbene and Ru represents ruthenium.
[0025] The σ-π chelate-coordinated nitrogen heterocyclic carbene ruthenium complex provided by this invention contains an asymmetric nitrogen heterocyclic carbene and exhibits catalytic activity. It is stable at room temperature and under solid conditions and can catalyze the ring-opening metathesis polymerization of norbornene (NB) to form polynorbornene under 620-680 nm red light irradiation, air atmosphere, or inert atmosphere without the need for additional photosensitizers, making it an excellent red light catalyst. Its catalytic activity is weak in the absence of light. In particular, it can catalyze the ring-opening metathesis polymerization of norbornene (NB) to form polynorbornene under low-energy 620-680 nm red light irradiation and air atmosphere without the need for additional photosensitizers, making its catalytic conditions milder than other catalysts.
[0026] This invention also provides a method for preparing nitrogen heterocyclic carbene ruthenium complexes coordinated in the σ-π chelate mode as described in the above technical solution, comprising the following steps: The p-cymene ruthenium complex with the structure shown in Formula 2 was mixed with an organic solvent and reacted under red light irradiation to obtain the nitrogen heterocyclic carbene ruthenium complex coordinated in the σ-π chelate mode. Equation 2.
[0027] Unless otherwise specified, the raw materials used in this invention are preferably commercially available products.
[0028] In this invention, the p-cymene ruthenium complex (denoted as Ru1) with the structure shown in Formula 2 is preferably prepared according to the preparation method disclosed in Chinese Patent Publication No. CN122234112A, which will not be repeated here.
[0029] In this invention, the organic solvent is preferably an aprotic solvent, which preferably includes one or more of dichloromethane, chloroform and acetonitrile, and more preferably dichloromethane.
[0030] In this invention, the preferred ratio of the p-cymene ruthenium complex to the organic solvent is 0.0506 g: 4~10 mL, and more preferably 0.0506 g: 5 mL.
[0031] In this invention, the wavelength of the red light is preferably 640~680nm, and more preferably 640nm, 650nm, 660nm, 670nm or 680nm.
[0032] In this invention, the reaction temperature is preferably 10~30℃, more preferably 25℃; in a specific embodiment of this invention, the reaction temperature is preferably room temperature, i.e., neither additional heating nor additional cooling is required; the reaction time is preferably 12~24h, specifically preferably 24h; the reaction is preferably carried out under stirring. In this invention, the reaction is preferably carried out under a protective atmosphere, preferably argon.
[0033] After the reaction is completed, the present invention preferably further includes: subjecting the obtained reaction solution to a first rotary evaporation to obtain a viscous substance; mixing the viscous substance with ethanol and subjecting it to a second rotary evaporation to obtain a rotary evaporation system; performing solid-liquid separation on the rotary evaporation system to obtain a solid and a liquid respectively; washing the solid with ice-cold ethanol to obtain the nitrogen heterocyclic carbene ruthenium complex coordinated in the σ-π chelate mode. The present invention does not specifically limit the operation of the first rotary evaporation, as long as most of the organic solvent can be removed. The present invention does not specifically limit the operation of the second rotary evaporation, as long as all the organic solvent can be removed. In the present invention, the solid-liquid separation method is preferably filtration. In the present invention, the temperature of the ice-cold ethanol is preferably -5~5℃. The present invention preferably further includes: evaporating the liquid obtained from the solid-liquid separation and then recycling it as the cymene ruthenium complex to improve the yield; the recycling is preferably 2~4 times, more preferably 3 times.
[0034] The reaction formula for preparing nitrogen heterocyclic carbene ruthenium complexes coordinated in a σ-π chelate mode according to the present invention is as follows: .
[0035] This invention also provides the application of the nitrogen heterocyclic carbene ruthenium complexes coordinated in the σ-π chelate mode described in the above-described technical solutions, or the nitrogen heterocyclic carbene ruthenium complexes prepared by the preparation method described in the above-described technical solutions, in catalytic ring-opening metathesis polymerization reactions.
[0036] This invention provides a method for preparing polynorbornene, comprising the following steps: Norbornene, a catalyst, and an aprotic solvent were mixed and subjected to a ring-opening metathesis polymerization reaction under red light irradiation to obtain the polynorbornene. The catalyst is a nitrogen heterocyclic carbene ruthenium complex coordinated in a σ-π chelate mode as described in the above technical solution, or a nitrogen heterocyclic carbene ruthenium complex coordinated in a σ-π chelate mode prepared by the preparation method described in the above technical solution.
[0037] In this invention, the molar ratio of norbornene to catalyst is preferably 1:0.0005~0.02, and more preferably 1:0.0005, 1:0.001, 1:0.005, 1:0.01, 1:0.015 or 1:0.02.
[0038] In this invention, the aprotic solvent preferably includes one or more of tetrahydrofuran, toluene, dichloromethane and 1,2-dichloroethane, and more preferably dichloromethane.
[0039] In this invention, the preferred ratio of norbornene to aprotic solvent is 0.1177g:4~10mL, and more preferably 0.1177g:5mL.
[0040] In this invention, the wavelength of the red light is preferably 620-680 nm, specifically preferably 620 nm, 630 nm, 640 nm, 650 nm, 660 nm, 670 nm, or 680 nm; the temperature of the ring-opening metathesis polymerization reaction is preferably 10-30°C, more preferably 25°C; in a specific embodiment of this invention, the temperature of the ring-opening metathesis polymerization reaction is preferably room temperature, i.e., no additional heating or cooling is required; the time is preferably 6-24 h, specifically preferably 12 h; the ring-opening metathesis polymerization reaction is preferably carried out under stirring conditions. In this invention, the ring-opening metathesis polymerization reaction is preferably carried out in an air atmosphere; the ring-opening metathesis polymerization reaction is preferably carried out without the use of a photosensitizer. In this invention, the ring-opening metathesis polymerization reaction is considered complete when the system becomes a dark orange-yellow gel.
[0041] In this invention, the atmosphere for the ring-opening metathesis polymerization reaction is preferably an inert atmosphere or an air atmosphere, and more preferably an air atmosphere.
[0042] Following the ring-opening metathesis polymerization reaction, the present invention preferably further includes: quenching the ring-opening metathesis polymerization reaction to obtain a quenching system; and purifying the quenching system by column chromatography to obtain the polynorbornene.
[0043] In this invention, the quencher used to quench the ring-opening metathesis polymerization reaction preferably includes ethyl vinyl ether; the quenching time for the ring-opening metathesis polymerization reaction is preferably 10 min. In this invention, the eluent for column chromatography purification is preferably dichloromethane.
[0044] In this invention, the reaction formula for preparing polynorbornene is as follows: .
[0045] The σ-π chelate-coordinated nitrogen heterocyclic carbene ruthenium complex provided by this invention has the advantages of red light open-circuit catalytic ring-opening metathesis polymerization of olefins to prepare polynorbornene, with low catalyst dosage, no need for additional photosensitizer, simple operation, high conversion rate and low cost.
[0046] The following detailed description, in conjunction with embodiments, illustrates the σ-π chelate-mode coordinated nitrogen heterocyclic carbene ruthenium complexes provided by the present invention, their preparation methods, and applications. However, these descriptions should not be construed as limiting the scope of protection of the present invention.
[0047] Example 1 A method for preparing a nitrogen heterocyclic carbene ruthenium complex (denoted as Ru2) coordinated in a σ-π chelate mode is as follows: Under argon protection, 0.0506 g of Ru1 and 5 mL of dichloromethane were added to a 10 mL Schlenk tube. The mixture was stirred at room temperature and irradiated with 640 nm light for 24 h. The mixture was then evaporated under reduced pressure until a small amount of solvent remained. 20 mL of anhydrous ethanol was added, and the DCM was evaporated to dryness. The mixture was filtered to obtain a solid and a filtrate, respectively. The solid was washed with ice-cold anhydrous ethanol to obtain 0.0166 g of a bright red solid, with a yield of 44.62%.
[0048] The obtained bright red solid was characterized as follows: Figure 1 The following is the 1H NMR spectrum of the obtained bright red solid. Specific information is as follows: 1 ¹H NMR (500 MHz, CDCl₃): 2.19 ppm (s, 6H), 3.83 ppm (s, 3H), 4.66 ppm (s, 2H), 4.93 ppm (s, 2H), 5.51 ppm (s, 1H), 6.83 ppm (d, J=2 Hz, 1H), 6.96 ppm (d, J=2Hz, 1H). The 7.26 ppm peak represents the chloroform solvent peak.
[0049] Figure 2 The following is the carbon NMR spectrum of the obtained bright red solid. Specific information is as follows: 13 C10 NMR (500 MHz, CDCl3): 18.83 ppm, 37.93 ppm, 53.15 ppm, 74.24 ppm, 77.22 ppm, 87.82 ppm, 100.07 ppm, 112.10 ppm, 117.88 ppm, 124.29 ppm, 170.91 ppm. Among them, 76.76 ppm, 77.02 ppm, and 77.27 ppm are chloroform solvent peaks.
[0050] Figure 3 ESI of the obtained bright red solid + Mass spectrum, from Figure 3 It can be seen that the peak at 337 m / z is the peak generated by the dissociation of a chlorine ligand of the catalyst.
[0051] Figure 4 The UV-Vis absorption spectrum of the obtained bright red solid is shown below. The solvent is dichloromethane with a concentration of 10. -3 mol / L, from Figure 4 It can be seen that the maximum absorption peak is located at 415 nm.
[0052] Figure 5 Coordination environment diagram of the nitrogen heterocyclic carbene ruthenium complexes coordinated in the obtained σ-π chelation mode. Figure 6Crystal structure diagram of nitrogen heterocyclic carbene ruthenium complexes coordinated in σ-π chelate mode, from Figure 5 and Figure 6 It can be seen that the trimethylbenzene-like structures on the flanking sides of the NHC ligand have undergone η-interaction with the Ru center. 6 Coordination.
[0053] The above spectral data show that the obtained bright red solid is consistent with the structure of the nitrogen heterocyclic carbene ruthenium complex (NHC-Ru, Ru2) coordinated by the σ-π chelate mode provided by this invention.
[0054] Application Example 1 The preparation of polynorbornene involves the following steps: In an air atmosphere, 0.1177 g (1.25 mmol) of norbornene, 0.0047 g (0.0125 mmol) of a nitrogen-containing heterocyclic carbene ruthenium complex Ru2 coordinated in a σ-π chelate mode, and 5 mL of dichloromethane were added to a 10 mL Schlenk tube. The mixture was irradiated with 640 nm red light and stirred for 12 h until the reaction system turned into a dark orange-yellow gel. Two drops of ethyl vinyl ether were added to the system and stirred for 10 min to quench the reaction, yielding a quenched ring-opening metathesis polymerization reaction solution. Then, 1 mmol of mesitylene was added to the reaction solution as an internal standard, and samples were taken for 1H NMR spectroscopy to calculate the conversion rate. The 1H NMR data are shown below. Figure 7 As shown, Figure 7 The 1H NMR spectrum of the reaction solution is shown below. Figure 7 The proton spectrum shown indicates a conversion rate of 76.8%.
[0055] The process for red-light ROMP catalysts using nitrogen heterocyclic carbene ruthenium complexes coordinated by the σ-π chelation mode provided by this invention is stable and feasible, with high yield and high purity.
[0056] The above description is only a preferred embodiment of the present invention. It should be noted that for those skilled in the art, several improvements and modifications can be made without departing from the principle of the present invention, and these improvements and modifications should also be considered within the scope of protection of the present invention.
Claims
1. A nitrogen-heterocyclic carbene ruthenium complex coordinated in a σ-π chelate mode, characterized in that, It has the structure shown in Equation 1: Formula 1.
2. The method for preparing the nitrogen heterocyclic carbene ruthenium complex coordinated in the σ-π chelate mode as described in claim 1, characterized in that, Includes the following steps: The p-cymene ruthenium complex with the structure shown in Formula 2 was mixed with an organic solvent and reacted under red light irradiation to obtain the nitrogen heterocyclic carbene ruthenium complex coordinated in the σ-π chelate mode. Equation 2.
3. The preparation method according to claim 2, characterized in that, The wavelength of the red light is 640~680nm.
4. The preparation method according to claim 2 or 3, characterized in that, The reaction is carried out at a temperature of 10~30℃ for 12~24h; the reaction is carried out under stirring conditions.
5. The preparation method according to claim 2, characterized in that, After the reaction is completed, the process further includes: subjecting the obtained reaction solution to a first rotary evaporation to obtain a viscous substance; mixing the viscous substance with ethanol and subjecting it to a second rotary evaporation to obtain a rotary evaporation system; performing solid-liquid separation on the rotary evaporation system to obtain a solid and a liquid, respectively; and washing the solid with ice-cold ethanol to obtain the nitrogen heterocyclic carbene ruthenium complex coordinated in the σ-π chelate mode.
6. The application of the nitrogen heterocyclic carbene ruthenium complex coordinated in a σ-π chelate mode as described in claim 1, or the nitrogen heterocyclic carbene ruthenium complex prepared by the preparation method described in any one of claims 2 to 5, in catalytic ring-opening metathesis polymerization.
7. A method for preparing polynorbornene, characterized in that, Includes the following steps: Norbornene, a catalyst, and an aprotic solvent were mixed and subjected to a ring-opening metathesis polymerization reaction under red light irradiation to obtain the polynorbornene. The catalyst is the nitrogen heterocyclic carbene ruthenium complex coordinated in a σ-π chelate mode as described in claim 1, or the nitrogen heterocyclic carbene ruthenium complex prepared by the preparation method described in any one of claims 2 to 5.
8. The preparation method according to claim 7, characterized in that, The molar ratio of norbornene to catalyst is 1:0.0005~0.
02.
9. The preparation method according to claim 7, characterized in that, The wavelength of the red light is 620~680nm; the temperature of the ring-opening metathesis polymerization reaction is 10~30℃, and the time is 6~24h; the ring-opening metathesis polymerization reaction is carried out under stirring conditions.
10. The preparation method according to claim 7 or 9, characterized in that, Following the ring-opening metathesis polymerization reaction, the process further includes: quenching the ring-opening metathesis polymerization reaction to obtain a quenching system; and purifying the quenching system by column chromatography to obtain the polynorbornene. The eluent used in the column chromatography purification was dichloromethane.
Citation Information
Patent Citations
P-cymene ruthenium complex, preparation method and application thereof, and method for preparing polymer through ring-opening metathesis polymerization reaction of olefin
CN122234112A