Packaging substrate and its manufacturing method

By designing step-shaped oblique side surfaces and multi-layer structures on the packaging substrate, the problem of difficult to judge solder spot performance and solder foot oxidation in the prior art is solved, and the visibility evaluation of solder performance and the improvement of solder stability is achieved.

CN111199948BActive Publication Date: 2024-11-26ASE SHANGHAI +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202010144124.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-03-04
Publication Date
2024-11-26
Estimated Expiration
2040-03-04

AI Technical Summary

Technical Problem

The existing grille array packaging technology is difficult to judge the performance of solder points from the appearance, and the cross-section of the solder foot is easily oxidized, which affects the operability and stability of the packaging product.

Method used

A package substrate is designed, which includes a line top layer, a line bottom layer, a first insulating layer and a stepped oblique side surface, a conductive top layer, a conductive bottom layer, an oxidation anti-layer, and a side conductive layer and a lateral oxidation anti-layer through a combination of these layers The structure improves solder visibility and prevents oxidation.

Benefits of technology

It realizes an effective evaluation of the solder performance of the packaging substrate, improves the contact area and stability of the solder, reduces the oxidation of the solder cutting surface, and improves the operability and stability of the packaging products.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN111199948B_ABST
    Figure CN111199948B_ABST
Patent Text Reader

Abstract

The embodiments of the present application relate to a packaging substrate and a manufacturing method thereof. According to one embodiment of the packaging substrate, it includes: a top layer of a circuit; a bottom layer of a circuit; a first insulating layer, which is located between the top layer of the circuit and the bottom layer of the circuit; and at least one stepped oblique side surface, the stepped oblique side surface having a first stepped oblique side surface extending from the top layer of the circuit to the first insulating layer and a second stepped oblique side surface extending from the first insulating layer to the bottom layer of the circuit. The packaging substrate and the manufacturing method thereof provided by the embodiments of the present application can effectively evaluate the soldering performance of the packaging substrate from the appearance.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] Embodiments of the present application generally relate to the field of semiconductors, and more specifically, to a packaging substrate and a method for manufacturing the same. Background Art

[0002] Land grid array (LGA) packaging technology is a "leap-forward technological revolution" in the field of semiconductor packaging technology, mainly because it uses metal contact packaging to replace the previous pin-shaped pins. However, it is generally difficult to judge whether the performance of the solder joints, especially the solder joints at the bottom, is good from the appearance of the land grid array package product. In addition, the solder pins on the side of the LGA package are only cut off at the connection of the package unit during the production process to expose the solder pin cut surface. Accordingly, due to the small solder pin cut surface, it is difficult to adhere enough solder during welding. Moreover, the exposed solder pin cut surface is prone to oxidation after a period of time, which will make it more difficult to tin the solder pin cut surface, thereby affecting the operability and stability of the packaged product during application.

[0003] Therefore, the existing grid array packaging substrate needs to be further improved. Summary of the invention

[0004] One of the purposes of the embodiments of the present application is to provide a packaging substrate and a manufacturing method thereof, which can effectively evaluate the soldering performance of the packaging substrate from the appearance.

[0005] One embodiment of the present application provides a packaging substrate, which includes: a circuit top layer; a circuit bottom layer; a first insulating layer, which is located between the circuit top layer and the circuit bottom layer; and at least one stepped inclined side surface, the stepped inclined side surface having a first stepped inclined side surface extending from the circuit top layer to the first insulating layer and a second stepped inclined side surface extending from the first insulating layer to the circuit bottom layer.

[0006] According to another embodiment of the present application, the first insulating layer has a core layer. The circuit top layer further includes a conductive top layer, and an anti-oxidation top layer is provided above the conductive top layer. The packaging substrate further includes a side conductive layer, which extends from the conductive top layer along the at least one stepped oblique side surface to the circuit bottom layer, and a side anti-oxidation layer, which is located above the side conductive layer and extends from the anti-oxidation top layer. The packaging substrate further includes an anti-oxidation bottom layer covering the circuit bottom layer, and the anti-oxidation bottom layer extends from the side anti-oxidation layer.

[0007] According to another embodiment of the present application, the circuit bottom layer further includes a conductive bottom layer, and an anti-oxidation bottom layer is provided below the conductive bottom layer. The conductive top layer, the side conductive layer and the conductive bottom layer are copper layers, and the anti-oxidation top layer, the side anti-oxidation layer and the anti-oxidation bottom layer are nickel-gold layers. The side surface of the anti-oxidation top layer is also inclined and stepped.

[0008] Another embodiment of the present application further provides a packaging substrate material-strip, which includes the above-mentioned packaging substrate.

[0009] Another embodiment of the present application also provides a method for manufacturing a packaging substrate, which includes: providing a packaging substrate material strip having a plurality of packaging substrate units, each packaging substrate unit including: a circuit top layer; a circuit bottom layer; and a first insulating layer, which has a core layer and is located between the circuit top layer and the circuit bottom layer; drilling a hole from the upper surface of the circuit top layer downward to a portion of the first insulating layer to form a first groove, the first groove having a first stepped oblique side extending from the circuit top layer to the first insulating layer; and drilling a hole from the bottom of the first groove to the circuit bottom layer to form a second groove, the second groove having a second stepped oblique side extending from the first insulating layer to the circuit bottom layer; and dividing the plurality of packaging substrate units to form separate packaging substrates.

[0010] According to another embodiment of the present application, the top layer of the circuit has a conductive top layer, and the above method includes forming an anti-oxidation top layer located above the conductive top layer, and further includes forming a side conductive layer, which extends from the conductive top layer along the first step inclined side surface and the second step inclined side surface to the bottom layer of the circuit; and forming a side anti-oxidation layer, which is located above the side conductive layer and extends from the anti-oxidation top layer.

[0011] According to another embodiment of the present application, the method further includes forming an anti-oxidation bottom layer covering the circuit bottom layer, wherein the anti-oxidation bottom layer extends from the side anti-oxidation layer.

[0012] According to another embodiment of the present application, the circuit bottom layer includes a conductive bottom layer, and the method further includes forming an anti-oxidation bottom layer below the conductive bottom layer.

[0013] Compared with the prior art, the packaging substrate provided in the embodiment of the present application has solder visibility, so that it is possible to effectively judge whether the solderability of the packaging substrate is good, and at the same time, the cut surface of the packaging substrate is not easily oxidized. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] The following will briefly describe the drawings necessary for describing the embodiments of the present application or the prior art to facilitate the description of the embodiments of the present application. Obviously, the drawings described below are only some of the embodiments in the present application. For those skilled in the art, without the need for creative work, drawings of other embodiments can still be obtained based on the structures illustrated in these drawings.

[0015] FIG. 1 is a cross-sectional view of a package substrate 100 according to some embodiments of the present application.

[0016] 2A-2G are diagrams showing a method for manufacturing a package substrate 100 according to some embodiments of the present application.

[0017] FIG. 3 is a top view and a cross-sectional view of a package substrate strip 110 composed of a package substrate 100 array according to some embodiments of the present application. DETAILED DESCRIPTION

[0018] In order to better understand the spirit of the embodiments of the present application, some preferred embodiments of the present application are further described below.

[0019] The embodiments of the present application will be described in detail below. In the full text of the present application specification, the same or similar components and components with the same or similar functions are represented by similar reference numerals. The embodiments of the accompanying drawings described herein are illustrative, graphical, and are used to provide a basic understanding of the present application. The embodiments of the present application should not be interpreted as limiting the present application.

[0020] As used herein, the terms "substantially," "substantially," "essentially," and "about" are used to describe and illustrate small variations. When used in conjunction with an event or circumstance, the terms may refer to instances where the event or circumstance occurred exactly as well as instances where the event or circumstance occurred very approximately. For example, when used in conjunction with a numerical value, the terms may refer to a range of variation less than or equal to ±10% of the numerical value, such as less than or equal to ±5%, less than or equal to ±4%, less than or equal to ±3%, less than or equal to ±2%, less than or equal to ±1%, less than or equal to ±0.5%, less than or equal to ±0.1%, or less than or equal to ±0.05%. For example, two values ​​may be considered “substantially” the same if the difference between them is less than or equal to ±10% of the average of the values ​​(e.g., less than or equal to ±5%, less than or equal to ±4%, less than or equal to ±3%, less than or equal to ±2%, less than or equal to ±1%, less than or equal to ±0.5%, less than or equal to ±0.1%, or less than or equal to ±0.05%).

[0021] In this specification, unless otherwise specified or limited, relative terms such as "central", "longitudinal", "lateral", "front", "rear", "right", "left", "inner", "outer", "lower", "higher", "horizontal", "vertical", "above", "below", "above", "below", "top", "bottom" and their derivative terms (such as "horizontally", "downwardly", "upwardly", etc.) should be interpreted as referring to the directions described in the discussion or depicted in the drawings. These relative terms are only used for convenience of description and do not require that the present application be constructed or operated in a specific direction.

[0022] In addition, sometimes amounts, ratios and other numerical values ​​are presented in range format herein. It should be understood that such range format is for convenience and brevity, and should be flexibly understood to include not only the numerical values ​​explicitly specified as range limits, but also all individual numerical values ​​or sub-ranges encompassed within the range, as if each numerical value and sub-range were explicitly specified.

[0023] Furthermore, for ease of description, “first”, “second”, “third”, etc. may be used herein to distinguish different components in one figure or a series of figures. “First”, “second”, “third”, etc. are not intended to describe the corresponding components.

[0024] FIG1 is a cross-sectional view of a package substrate 100 according to some embodiments of the present application. The package substrate 100 includes a circuit top layer 10, a circuit bottom layer 12, and an insulating layer 14 located between the circuit top layer 10 and the circuit bottom layer 12. The insulating layer 14 may be a core layer. In addition, the package substrate 100 also includes at least one stepped oblique side surface 102 to facilitate the tinning of the side of the package substrate 100, and the soldering condition of the package substrate 100 can be well judged according to the solder points. In actual production, a number of package substrates 100 can be processed and transported together on a package substrate strip (not shown), thereby improving production efficiency.

[0025] According to some embodiments of the present application, the stepped oblique side surface 102 can be divided into two sections, as shown in FIG1 , the first section is a first stepped oblique side surface 102a extending from the top layer 10 of the circuit to the insulating layer 14, and the second section is a second stepped oblique side surface 102b extending from the insulating layer 14 to the bottom layer 12 of the circuit. The two-section sloped design side surface of the package substrate 100 makes the package tinning effect better, and the smaller the angle between the first stepped oblique side surface 102a and the second stepped oblique side surface 102b and the surface of the bottom layer 12 of the circuit, the better the tinning effect of the side surface of the package substrate 100.

[0026] According to some embodiments of the present application, as shown in FIG1 , the circuit top layer 10 may include a conductive top layer 10a, which may be used for circuit connection between devices on the package substrate. For example, the conductive top layer 10a may be located on a resin layer 210b of the circuit top layer 10, such as a semi-cured resin PP (prepreg) layer. The thickness of the conductive top layer 10a is about 10-20 microns. The package substrate 100 may also include an anti-oxidation top layer 10b located above the conductive top layer 10a. The anti-oxidation top layer 20b may be used to protect the electronic circuit on the conductive top layer 10a.

[0027] The conductive top layer 10a and the anti-oxidation top layer 10b thereon can extend along the stepped oblique side surface 102 toward the circuit bottom layer 12, respectively, to form a side conductive layer 112 and a side anti-oxidation layer 114 located above the side conductive layer 112. According to some embodiments of the present application, the thickness of the side conductive layer 112 can be about 10-20 microns.

[0028] According to some embodiments of the present application, the circuit bottom layer 12 may include a conductive bottom layer 12a, which can also be used for circuit connection between devices on the package substrate 100. Similarly, the conductive bottom layer 12a can be located below the resin layer 220b. According to some embodiments of the present application, the package substrate 100 may also include an anti-oxidation bottom layer 115 covering the circuit bottom layer 12. The anti-oxidation bottom layer 115 may extend from the side anti-oxidation layer 114.

[0029] According to some embodiments of the present application, the packaging substrate 100 may further include another anti-oxidation bottom layer 12 b located below the conductive bottom layer.

[0030] According to some embodiments of the present application, the conductive top layer 10a, the side conductive layer 112 and the conductive bottom layer 12a are metal layers, such as copper layers, and the anti-oxidation top layer 10b, the side anti-oxidation layer 114, the anti-oxidation bottom layer 12b and another anti-oxidation bottom layer 115 are also metal layers, such as nickel-gold layers.

[0031] According to some embodiments of the present application, the side surface 102c of the anti-oxidation top layer 10b is also stepped.

[0032] 2A to 2F illustrate a method of manufacturing a packaging substrate 100 according to some embodiments of the present application.

[0033] 2A , a package substrate (e.g., LBGA package substrate) strip having a plurality of package substrate units is provided, each package substrate unit 200 comprising: a circuit top layer 210, a circuit bottom layer 220, and an insulating layer 214 located between the circuit top layer 210 and the circuit bottom layer 220. The thickness of the circuit top layer 210 and the circuit bottom layer 220 is about 35-55 microns, and the thickness of the insulating layer 214 is about 55-65 microns, and the insulating layer may be a BT resin substrate material. The circuit top layer 210 may include a conductive top layer 210a, and the circuit bottom layer 220 may include a conductive bottom layer 220a. The conductive top layer 210a and the conductive bottom layer 220a may be made of a metal material, such as copper. The thickness and shape of the conductive top layer 210a and the conductive bottom layer 220a may vary with the process during the production process, for example, they may be about 12 microns initially, and their thickness may be reduced to about 3 microns through an etching process. Similarly, those skilled in the art should understand that in the semiconductor manufacturing process, other layer structures may also be affected in a similar manner, and the existence of the structures and the relationship between them cannot be denied.

[0034] Referring to FIG. 2B , the circuit top layer 210 at an opening on the conductive top layer 210a and a portion of the insulating layer below the circuit top layer 210 are removed downward to expose a portion of the surface of the insulating layer 214, and a first groove 201 is formed at the same time. The size of the first groove 201 can be controlled by controlling the thickness and process of the conductive top layer 210a. For example, according to some embodiments of the present application, the upper opening width of the first groove 201 can be about 550 microns. The number and position of the first groove 201 can be determined as needed and are not described in detail here. In some embodiments, other grooves, such as grooves for forming through holes, can also be formed on the packaging substrate 100.

[0035] According to some embodiments of the present application, the first groove 201 can be formed by laser drilling and mechanical drilling, so that the first groove 201 has a first oblique side surface 201a extending from the circuit top layer 210 to the insulating layer 214. The stepped (or multi-stage) side surface design can have a better soldering effect. For example, in the embodiment shown in FIG. 2B, the first oblique side surface 201a can be composed of two sections of oblique side surfaces. Similarly, the shape and size of the first oblique side surface 201a can also be controlled by controlling the thickness and process of the conductive top layer 210a.

[0036] 2C , the insulating layer at the bottom of the first groove 201 and a portion of the circuit bottom layer under the insulating layer 214 are removed downward from the bottom of the first groove 201 to form a second groove 202 .

[0037] According to some embodiments of the present application, the second groove 202 can be formed into an inverted trapezoidal structure by laser drilling or other processes, wherein the conductive bottom layer 220a can be used as an etching stop layer. This can expose part of the conductive bottom layer of the circuit bottom layer 220, thereby achieving precise control of the depth of the second groove 202. The second groove 202 has a second oblique side surface 201b extending from the insulating layer 214 to the bottom of the second groove 202. According to some embodiments of the present application, the bottom width of the second groove 202 is about 240-260 microns.

[0038] According to some embodiments of the present application, the sum of the depths of the first groove 201 and the second groove 202 may be approximately 110-130 microns, such as 120um. The sum of the depths may be further improved through structural design and process, such as using a laser method to increase the design space. On the other hand, the bottom copper in the circuit bottom layer 220 may help control the sum of the depths, thereby achieving depth consistency control. One or more conductive layers may be formed at corresponding positions on the package substrate where the grooves have been formed as required.

[0039] For example, referring to FIG. 2D , a first conductive layer 212 may be formed, which may extend along the first side surface 201a of the first groove 201 and the second oblique side surface 201b of the second groove 202 to the bottom of the second groove 202, so that the first conductive layer 212 has a stepped oblique side surface, thereby forming the side conductive layer 112 of the substrate unit 200. The first conductive layer 212 may be a copper layer with a thickness of about 1 micron, and may be formed by, for example, but not limited to, a chemical method. The first conductive layer 212 may also be formed on the upper surface of the conductive top layer 210a and the lower surface of the conductive bottom layer 220a, respectively, to further thicken the conductive top layer 210a and the conductive bottom layer 220a, or to cover the bottom of the second groove 202. The first conductive layer 212 may be prepared for the subsequent formation of a circuit layer.

[0040] Referring to FIG. 2E, the corresponding circuit can be obtained by laminating the upper and lower surfaces of the substrate 200 with a polymer layer, exposing and developing the patterned polymer layer, and then removing the polymer layer. In some embodiments, the corresponding grooves can be filled as needed, such as the grooves used to fill the through holes to form through holes. In some embodiments, the thickness of the copper layer in the first groove 201 and / or the second groove 202 can also be adjusted as needed. For example, in one example, the second conductive layer 216 can be formed on the upper and lower surfaces of the substrate 200 and the oblique sides of the first groove 201 and the second groove 202 by, for example, but not limited to, electroplating. The second conductive layer 216 can cover the first conductive layer 212 and its stepped oblique side, and can fill the corresponding grooves as needed. The second conductive layer 216 can be formed into a copper layer with a thickness of about 22-28 microns, for example, about 25 microns.

[0041] The thickness of the corresponding position of the second conductive layer 216 on the stepped oblique side surface of the first conductive layer 212 can be adjusted as needed later, for example, by laminating, exposing and developing the polymer layer again, patterning the polymer layer, etching the exposed second conductive layer, reducing the thickness of the second conductive layer 216 on the oblique sidewalls and bottom of the first groove 201 and the second groove 202 to about 10 microns, and then removing the polymer layer. The thickness of the conductive top layer 210a and the conductive bottom layer 220a of the substrate unit 200 can be further increased by the second conductive layer 216.

[0042] After the above-mentioned exemplary processing, such as forming the first conductive layer 212 and the second conductive layer 216, and operations based on the first conductive layer 212 and the second conductive layer 216, the required appropriate conductive top layer, side conductive layer and conductive bottom layer can be obtained, such as the conductive top layer 10a, side conductive layer 112 and conductive bottom layer 12a in Figure 1.

[0043] According to some embodiments of the present application, when etching the second conductive layer 216 , the conductive top layer 210a above the circuit top layer may be formed with a stepped slanted side surface, such as the side surface 201c of the conductive top layer 210a in FIG. 2F .

[0044] An anti-oxidation layer may be formed above the circuit layer to prevent oxidation of the circuit layer and provide good conductive properties.

[0045] For example, referring to FIG. 2G , an anti-oxidation layer 218 is formed on the second conductive layer 216 of the substrate unit 200 according to the position requirements to protect the conductive layer below from being oxidized and enhance the electrical transmission performance of the circuit. For example, an anti-oxidation top layer 10b, a side anti-oxidation layer 114, and an anti-oxidation bottom layer 12b may be formed above the conductive top layer 210, above the side conductive layer 112, and below the conductive bottom layer 220a of the substrate unit 200, respectively. In some embodiments, the anti-oxidation bottom layer 218 may cover the conductive layer at the bottom of the second groove 202, for example, another anti-oxidation bottom layer 115 as shown in FIG. 1 . The anti-oxidation layer may be, for example, but not limited to, a nickel-gold layer. As shown in FIG. 2G , since the conductive top layer 210a above the circuit top layer forms a stepped oblique side surface, such as the side 201c of the conductive top layer 210a in FIG. 2F (as shown in FIG. 2F ), the anti-oxidation layer located thereon may also form an inclined stepped oblique side surface 102c. Finally, the package substrate strip obtained by the above processing method can be cut to obtain a top view of a package substrate strip 110 composed of a package substrate 100 array and a cross-sectional view of a corresponding sawing area (A and A′) as shown in FIG. 3 .

[0046] Referring to Figure 3, the stepped oblique side structure of the packaging substrate 100 makes the cutting (saw) area (A and A') designed to be a stepped semi-hole structure. When soldering, the soldering condition of the entire product including the bottom and side soldering conditions can be observed through the side soldering condition, thereby effectively judging whether the side soldering condition of the packaging substrate 100 is good. At the same time, the soldering area can be increased, thereby improving the firmness and stability of the product.

[0047] The packaging substrate structural design proposed in the present invention enables the quality of the packaging solder on the substrate to be confirmed by observing the solder creeping on the side, while increasing the contact area of ​​the solder on the finished substrate during the packaging process and improving the soldering yield. The multi-stage climbing design effectively improves the soldering effect. Through appropriate process selection, the size of the oblique side of the substrate can be effectively controlled, and uniform control can be achieved.

[0048] The technical content and technical features of this application have been disclosed as above, but those skilled in the art may still make various substitutions and modifications based on the teachings and disclosures of this application without departing from the spirit of this application. Therefore, the protection scope of this application should not be limited to the contents disclosed in the embodiments, but should include various substitutions and modifications that do not depart from this application, and are covered by the claims of this patent application.

Claims

1. A packaging substrate, comprising: A circuit top layer, the circuit top layer further comprising a conductive top layer, an anti-oxidation top layer being disposed above the conductive top layer; Line bottom layer; A first insulating layer, which is located between the top layer of the circuit and the bottom layer of the circuit; At least one stepped oblique side surface, the stepped oblique side surface having a first stepped oblique side surface extending from the top layer of the circuit to the first insulating layer and a second stepped oblique side surface extending from the first insulating layer to the bottom layer of the circuit, wherein the first stepped oblique side surface and the second stepped oblique side surface are inclined in substantially the same direction, an angle between the first stepped oblique side surface and the bottom layer of the circuit is different from an angle between the second stepped oblique side surface and the bottom layer of the circuit, and a connecting surface between the first stepped oblique side surface and the second stepped oblique side surface has an angle with both of them; and A side conductive layer extends from the conductive top layer along the at least one stepped inclined side surface to the circuit bottom layer; and a side anti-oxidation layer is located above the side conductive layer and extends from the anti-oxidation top layer. The package substrate according to claim 1 , wherein the first insulating layer has a core layer. 3 . The packaging substrate according to claim 1 , further comprising an anti-oxidation bottom layer covering the circuit bottom layer, wherein the anti-oxidation bottom layer extends from the side anti-oxidation layer. 4 . The packaging substrate according to claim 1 , wherein the circuit bottom layer further comprises a conductive bottom layer, and an anti-oxidation bottom layer is disposed below the conductive bottom layer. The package substrate according to claim 4 , wherein the conductive top layer, the side conductive layer and the conductive bottom layer are copper layers. 6 . The packaging substrate according to claim 3 , wherein the anti-oxidation top layer, the side anti-oxidation layer and the anti-oxidation bottom layer are nickel-gold layers. 7 . The packaging substrate according to claim 1 , wherein a side surface of the anti-oxidation top layer is also in an inclined step shape.

8. A packaging substrate strip, comprising the packaging substrate according to any one of claims 1 to 7.

9. A method for manufacturing a packaging substrate, comprising: A packaging substrate strip having a plurality of packaging substrate units is provided, each of the packaging substrate units comprising: A circuit top layer, the circuit top layer further comprising a conductive top layer, an anti-oxidation top layer being disposed above the conductive top layer; Line bottom layer; and A first insulating layer, which is located between the top line and the bottom line; A first groove is formed by drilling a hole downward from the upper surface of the top layer of the circuit to a portion of the first insulating layer, wherein the first groove has a first stepped oblique side surface extending from the top layer of the circuit to the first insulating layer; and A second groove is formed by drilling a hole from the bottom of the first groove to the bottom layer of the circuit, wherein the second groove has a second stepped oblique side surface extending from the first insulating layer to the bottom layer of the circuit, wherein the first stepped oblique side surface and the second stepped oblique side surface are inclined in substantially the same direction, an angle between the first stepped oblique side surface and the bottom layer of the circuit is different from an angle between the second stepped oblique side surface and the bottom layer of the circuit, and a connecting surface between the first stepped oblique side surface and the second stepped oblique side surface has an angle with both of them; Dividing a plurality of package substrate units based on a cutting area to form separate package substrates, wherein the first step oblique side surface and the second step oblique side surface enable the cutting area to be designed into a step shape of a half-hole structure; as well as A side conductive layer is formed, which extends from the conductive top layer along the first step inclined side surface and the second step inclined side surface to the circuit bottom layer; and a side anti-oxidation layer is formed, which is located above the side conductive layer and extends from the anti-oxidation top layer. 10 . The method for manufacturing a package substrate according to claim 9 , further comprising forming an anti-oxidation bottom layer covering the circuit bottom layer, wherein the anti-oxidation bottom layer extends from the side anti-oxidation layer. 11 . The method for manufacturing a package substrate according to claim 9 , wherein the circuit bottom layer comprises a conductive bottom layer, and the method further comprises forming an anti-oxidation bottom layer under the conductive bottom layer. 12 . The method for manufacturing a package substrate according to claim 9 , wherein a side surface of the anti-oxidation top layer is also in an inclined step shape. 13 . The method for manufacturing a package substrate according to claim 9 , wherein the first insulating layer has a core layer. 14 . The method for manufacturing a package substrate according to claim 11 , wherein the conductive top layer, the side conductive layer and the conductive bottom layer are copper layers. 15 . The method for manufacturing a package substrate according to claim 10 , wherein the anti-oxidation top layer, the side anti-oxidation layer and the anti-oxidation bottom layer are nickel-gold layers.