Ultra-high holding force longitudinal groove pattern elastic machine belt and preparation method thereof
By designing the longitudinal groove pattern layer on the elastic machine belt and combining with specific process flow, the problems of insufficient bend and grip strength of the existing elastic machine belt are solved, the product pass rate and production efficiency are improved, and the processing cost is reduced .
Patent Information
- Application Number
- CN202111480409.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-12-06
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2041-12-06
AI Technical Summary
In high-end equipment applications, existing elastic machine belts have problems such as bending and warping, insufficient grip strength and high processing difficulty, resulting in high product unqualification rate, slippage and dust pollution.
Design an ultra-high grip longitudinal groove pattern elastic machine belt, including a bottom transmission layer, main body tension layer, surface conveying layer and groove pattern layer, and form a longitudinal groove pattern layer through a special mold, combining composite, cutting and The tooth joint process improves the friction coefficient and reduces production costs.
The problem of insufficient bend and warping edges and grip strength is completely solved, the product qualification rate and production efficiency are improved, the processing cost is reduced, and the need for edge grinding and chamfering is avoided.
Smart Images

Figure CN114013918B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of machine belts, and in particular to an ultra-high holding force longitudinal groove pattern elastic machine belt and a preparation method thereof. Background Art
[0002] Existing elastic machine belts, whether imported or domestic, have obvious defects and deficiencies in the application of high-end equipment, especially photovoltaic solar energy equipment: (1) Due to product structure and manufacturing process, elastic machine belts at home and abroad have the common problem of bending and curling, which will cause a high rate of unqualified conveyed products due to belt marks; (2) Due to material formulation, the surface friction coefficient of elastic machine belts is generally around 0.5-1.0, so when conveying products, they often slip due to insufficient gripping force, resulting in symptoms such as inaccurate positioning and scratches on the products; (3) In order to solve the problem of belt marks caused by bending, domestic suppliers often adopt the method of post-processing edge grinding or chamfering of elastic machine belts. However, because elastic machine belts are elastomers, they are difficult to process, have low efficiency and poor precision, so there is a high processing cost and the belt marks cannot be effectively avoided. In addition, there is dust pollution and harm to the occupational health of workers. Summary of the invention
[0003] In order to overcome the deficiencies of the prior art solutions, the present invention provides an ultra-high holding force longitudinal groove pattern elastic machine belt and a preparation method thereof, which can effectively solve the problems raised by the background technology.
[0004] The technical solution adopted by the present invention to solve its technical problem is:
[0005] An ultra-high holding force longitudinal groove pattern elastic machine belt, comprising an elastic machine belt body, the elastic machine belt body comprising a bottom transmission layer, the upper end surface of the bottom transmission layer is provided with a first bridging connection layer, the upper end surface of the first bridging connection layer is provided with a main tensile layer, the upper end surface of the main tensile layer is provided with a second bridging connection layer, the upper end surface of the second bridging connection layer is provided with a surface conveying layer, the upper end surface of the surface conveying layer is provided with a groove pattern layer, and the groove pattern layer is longitudinally distributed on the conveying layer.
[0006] As a further explanation, the first bridging connecting layer and the second bridging connecting layer have the same structure, and both the first bridging connecting layer and the second bridging connecting layer are polyurethane resin adhesive coatings, and the thickness of the first bridging connecting layer and the second bridging connecting layer is 0.05 mm.
[0007] As a further explanation, the bottom transmission layer, the first bridging connection layer, the main tensile layer, the second bridging connection and the surface transport layer are of the same width.
[0008] As a further explanation, the bottom transmission layer, the first bridging connection layer, the main tensile layer, the second bridging connection and the surface transport layer are all connected by bonding.
[0009] As a further explanation, the bottom transmission layer is a PUR antistatic or conductive elastomer bottom layer, the main tensile layer is a TPU elastomer tensile skeleton layer, and the surface transport layer is a thermoplastic high grip polymer layer.
[0010] As a further explanation, the thickness of the surface conveying layer and the groove pattern layer is 0.7-1.0 mm, the thickness of the main tensile layer is 0.15-0.35 mm, and the thickness of the bottom transmission layer is 0.05 mm.
[0011] As a further illustration, a method for preparing an ultra-high holding force longitudinal groove pattern elastic machine belt comprises the following steps:
[0012] Step S1: Ingredients: Generally, the elastic machine belt ingredients are composed of a bottom transmission layer, a first bridging connection layer, a main tensile layer, a second bridging connection layer, a surface conveying layer and a groove pattern layer, wherein the total thickness of the elastic machine belt is 1.0-1.5mm, the thickness of the surface conveying layer and the groove pattern layer is 0.7-1.0mm, the thickness of the main tensile layer is 0.15-0.35mm, the thickness of the bottom transmission layer is 0.05mm, and the thickness of the first bridging connection layer and the second bridging connection layer are both 0.05mm.
[0013] Step S2: Compounding: When compounding the continuous line, the elastic machine belt must be kept in a tensioned state, and the surface of the elastic machine belt must be kept clean and flat. When compounding to the last car or stopping in the middle, it must be fully cooled, and then depressurized and relaxed.
[0014] Step S3: cutting: cutting includes straight edge, cutting and toothing;
[0015] Straight edge: Using the opposite side of the composite as a reference, carefully trim the reference edge of the elastic machine belt.
[0016] Cutting: Cut according to the reference edge and size. Generally, the width tolerance is ±0.2mm and the length tolerance is ±5mm. The belt can be shortened by 3% to 8% according to the customized length.
[0017] Teeth punching: Use a high-precision automatic tooth punching machine to punch out the following tooth-shaped interfaces using different cutting dies according to the different sizes of the elastic machine belt.
[0018] Step S4: Tooth connection: First check whether the tooth interface has any missing or broken edges, then clean the joint, butt-joint and place it flat on the heat press heating template, place pads of the same thickness as the elastic machine belt on both sides of the joint, and then pad the surface of the joint with a silicone embossed pad of the same pattern. Pay attention to the precise alignment of the tooth mouth and ensure the straightness. After the joint is off the machine, clean and organize the joint to ensure that the joint is neat and beautiful.
[0019] Step S5: Inspection and warehousing: The product logo, model, size, manufacturer name and production date are sprayed on the belt, which is inspected by the inspector and then packaged and put into storage.
[0020] As further elaboration, when the thickness of the elastic machine belt in step S1 is 1.0mm, the thickness of the surface conveying layer and the groove pattern layer is 0.7mm, the thickness of the main tensile layer is 0.15mm, the thickness of the bottom transmission layer is 0.05mm, and the thickness of the first bridging connection layer and the second bridging connection layer are both 0.05mm; when the thickness of the elastic machine belt is 1.2mm, the thickness of the surface conveying layer and the groove pattern layer is 0.8mm, the thickness of the main tensile layer is 0.25mm, the thickness of the bottom transmission layer is 0.05mm, and the thickness of the first bridging connection layer and the second bridging connection layer are both 0.05mm; when the thickness of the elastic machine belt is 1.5mm, the thickness of the surface conveying layer and the groove pattern layer is 1.0mm, the thickness of the main tensile layer is 0.35mm, the thickness of the bottom transmission layer is 0.05mm, and the thickness of the first bridging connection layer and the second bridging connection layer are both 0.05mm.
[0021] As further elaboration, when the total thickness of the elastic machine belt made in step S2 is 1.0 mm, the set temperature is 150-160°C, the speed of the composite line is 0.7 M / min, the pressure of the No. 1 drum sulfur machine is 6 MPa, and the pressure of the No. 2 drum sulfur machine is 4 MPa; when the total thickness of the elastic machine belt is 1.2 mm, the set temperature is 150-160°C, the speed of the composite line is 0.6 M / min, the pressure of the No. 1 drum sulfur machine is 7 MPa, and the pressure of the No. 2 drum sulfur machine is 5 MPa; when the total thickness of the elastic machine belt is 1.5 mm, the set temperature is 170-180°C, the speed of the composite line is 0.5 M / min, the pressure of the No. 1 drum sulfur machine is 8 MPa, and the pressure of the No. 2 drum sulfur machine is 6 MPa.
[0022] As a further explanation, the tooth connection type in step S4 is tooth connection type, the hot pressing temperature is 160-180°C, the insulation time is 2-3min, the set pressure is 2-3MPa, and the off-machine temperature is below 40°C.
[0023] Compared with the prior art, the present invention has the following beneficial effects:
[0024] The present embodiment provides an ultra-high holding force longitudinal groove pattern elastic machine belt and a preparation method thereof. A special mold is used to make the conveying surface of the elastic machine belt into the shape of a longitudinal groove pattern layer, which completely solves the problem of belt marks caused by bending and warping of the elastic machine belt, and improves the product qualification rate; and through the coordination between the steps of compounding, cutting, tooth connection and inspection and warehousing, the bottom transmission layer, the first bridge connection layer, the main body tension layer, the second bridge connection, the surface conveying layer and the groove pattern layer can be made into an ultra-high holding force longitudinal groove pattern elastic machine belt, which can increase the surface friction coefficient of the elastic machine belt to greater than 1.8, thereby improving the conveying holding force, completely solving the problem of slippage of the elastic machine belt conveyed products, ensuring that the product conveying can be accurately positioned and improving production efficiency; and the novel structural design and improved formula process of the elastic machine belt make the groove pattern layer elastic machine belt solve all the defects of the existing elastic machine belt once and for all without edge grinding and chamfering, thereby greatly reducing the production cost. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] Figure 1 It is a structural schematic diagram of the present invention;
[0026] Figure 2 It is a process flow chart of the present invention.
[0027] Numbers in the figure: 1- bottom transmission layer; 2- main tension layer; 3- surface transport layer; 4- first bridge connection layer; 5- second bridge connection layer; 6- groove pattern layer. DETAILED DESCRIPTION
[0028] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0029] like Figure 1-2As shown, the present embodiment provides an ultra-high holding force longitudinal groove pattern layer elastic machine belt, comprising an elastic machine belt body, the elastic machine belt body comprising a bottom transmission layer 1, the upper end surface of the bottom transmission layer 1 is provided with a first bridging connection layer 4, the upper end surface of the first bridging connection layer 4 is provided with a main tensile layer 2, the upper end surface of the main tensile layer 2 is provided with a second bridging connection layer 5, the upper end surface of the second bridging connection layer 5 is provided with a surface conveying layer 3, the upper end surface of the surface conveying layer 3 is provided with a groove pattern layer 6, the groove pattern layer 6 is longitudinally distributed on the conveying layer, the thickness of the surface conveying layer 3 and the groove pattern layer 6 is 0.7-1.0mm, by providing the groove pattern layer 6 on the surface conveying layer 3, and the groove pattern is longitudinally distributed on the surface conveying layer 3, the problem of belt marks caused by bending and warping of the elastic machine belt can be completely solved, and the product qualification rate is improved.
[0030] In this embodiment, the widths of the bottom transmission layer 1, the first bridging connection layer 4, the main tensile layer 2, the second bridging connection and the surface conveying layer 3 are consistent, and the bottom transmission layer 1, the first bridging connection layer 4, the main tensile layer 2, the second bridging connection and the surface conveying layer 3 are all connected by bonding. Through the cooperation between the bottom transmission layer 1, the first bridging connection layer 4, the main tensile layer 2, the second bridging connection and the surface conveying layer 3, the surface friction coefficient of the elastic machine belt can be increased to greater than 1.8, thereby improving the conveying gripping force, completely solving the problem of slippage of the elastic machine belt conveying products, ensuring that the product conveying can be accurately positioned and improving production efficiency.
[0031] In this embodiment, the first bridging connecting layer 4 and the second bridging connecting layer 5 have the same structure, and both the first bridging connecting layer 4 and the second bridging connecting layer 5 are polyurethane resin adhesive coatings, and the thickness of the first bridging connecting layer 4 and the second bridging connecting layer 5 is 0.05 mm.
[0032] In this embodiment, the bottom transmission layer 1 is a PUR antistatic or conductive elastomer bottom layer, and the thickness of the bottom transmission layer 1 is 0.05mm. Since the bottom transmission layer 1 is a PUR antistatic or conductive elastomer bottom layer, the PUR antistatic or conductive elastomer has high wear resistance and high conductivity; the main tensile layer 2 is a TPU elastomer tensile skeleton layer, and the thickness of the main tensile layer 2 is 0.15-0.35mm. Since the main tensile layer 2 is a TPU elastomer tensile skeleton layer, the TPU elastomer tensile skeleton layer is environmentally friendly, non-toxic, recyclable and decomposable, and has high resilience and good weather resistance; the surface transport layer 3 is a thermoplastic high-grip polymer layer. Since the surface transport layer 3 is a thermoplastic high-grip polymer layer, the thermoplastic high-grip polymer has super high grip, and is not easy to bend or warp.
[0033] A method for preparing an ultra-high holding force longitudinal groove pattern elastic machine belt comprises the following steps:
[0034] Step S1: ingredients: In general, the elastic machine belt ingredients are composed of a bottom transmission layer 1, a first bridging connection layer 4, a main tensile layer 2, a second bridging connection layer 5, a surface conveying layer 3 and a groove pattern layer 6, wherein the total thickness of the elastic machine belt is 1.0-1.5 mm, the thickness of the surface conveying layer 3 and the groove pattern layer 6 is 0.7-1.0 mm, the thickness of the main tensile layer 2 is 0.15-0.35 mm, the thickness of the bottom transmission layer 1 is 0.05 mm, and the thickness of the first bridging connection layer 4 and the second bridging connection layer 5 are both 0.05 mm; when the thickness of the elastic machine belt is 1.0 mm, wherein the surface conveying layer 3 and the groove pattern layer 6 are ... surface conveying layer 3 and the groove pattern layer 6 are 0.7-1.0 mm, the thickness of the surface conveying layer 3 and the groove pattern layer 6 are 0.7-1.0 mm, the thickness of the surface conveying layer 3 and the groove pattern layer 6 are 0.7-1.0 mm, the thickness of the surface conveying layer 3 and the groove pattern layer 6 are 0.7-1.0 mm, the thickness of the surface conveying layer 3 and the groove pattern layer 6 are 0.7-1.0 mm, the thickness of the surface conveying layer 3 and the groove pattern layer 6 are 0.7-1.0 mm, the thickness The thickness of the groove pattern layer 6 is 0.7mm, the thickness of the main tensile layer 2 is 0.15mm, the thickness of the bottom transmission layer 1 is 0.05mm, and the thickness of the first bridging connection layer 4 and the second bridging connection layer 5 are both 0.05mm; when the thickness of the elastic machine belt is 1.2mm, the thickness of the surface conveying layer 3 and the groove pattern layer 6 is 0.8mm, the thickness of the main tensile layer 2 is 0.25mm, the thickness of the bottom transmission layer 1 is 0.05mm, and the thickness of the first bridging connection layer 4 and the second bridging connection layer 5 are both 0.05mm; when the thickness of the elastic machine belt is 1.5mm, the thickness of the surface conveying layer 3 and the groove pattern layer 6 is 1.0mm, the thickness of the main tensile layer 2 is 0.35mm, the thickness of the bottom transmission layer 1 is 0.05mm, and the thickness of the first bridging connection layer 4 and the second bridging connection layer 5 are both 0.05mm.
[0035]
[0036]
[0037] Step S2: Compounding: When compounding the continuous line, the elastic machine belt must be kept in a tensioned state, and the surface of the elastic machine belt must be kept clean and flat. When compounding to the last car or stopping midway, it must be fully cooled, and then the pressure is released and relaxed. When the total thickness of the elastic machine belt is 1.0mm, the set temperature is 150-160℃, the speed of the compounding line is 0.7M / min, the pressure of the No. 1 drum sulfur machine is 6MPa, and the pressure of the No. 2 drum sulfur machine is 4MPa; when the total thickness of the elastic machine belt is 1.2mm, the set temperature is 150-160℃, the speed of the compounding line is 0.6M / min, the pressure of the No. 1 drum sulfur machine is 7MPa, and the pressure of the No. 2 drum sulfur machine is 5MPa; when the total thickness of the elastic machine belt is 1.5mm, the set temperature is 170-180℃, the speed of the compounding line is 0.5M / min, the pressure of the No. 1 drum sulfur machine is 8MPa, and the pressure of the No. 2 drum sulfur machine is 6MPa.
[0038] Step S3: cutting: cutting includes straight edge, cutting and toothing;
[0039] Straight edge: Using the opposite side of the composite as a reference, carefully trim the reference edge of the elastic machine belt.
[0040] Cutting: Cut according to the reference edge and size. Generally, the width tolerance is ±0.2mm and the length tolerance is ±5mm. The belt can be shortened by 3% to 8% according to the customized length.
[0041]
[0042] Teeth punching: Use a high-precision automatic tooth punching machine to punch out the following tooth-shaped interfaces using different cutting dies according to the different sizes of the elastic machine belt.
[0043] Step S4: Tooth connection: first check whether the toothed interface has any missing points or broken edges, then clean the joint, plug it in and place it flat on the hot press heating template, place pads of the same thickness as the elastic machine belt on both sides of the joint, and then pad the surface of the joint with silicone embossed pads of the same pattern. Pay attention to the precise alignment of the teeth and ensure the straightness. After the joint is removed from the machine, clean and organize the joint to ensure that it is neat and beautiful. The tooth connection type is tooth connection type, the hot pressing temperature is 160-180℃, the insulation time is 2-3min, the set pressure is 2-3MPa, and the temperature off the machine is below 40℃.
[0044]
[0045] Step S5: Inspection and warehousing: The product logo, model, size, manufacturer name and production date are sprayed on the belt, which is inspected by the inspector and then packaged and put into storage.
[0046] In summary, the present embodiment provides an ultra-high holding force longitudinal groove pattern elastic machine belt and a preparation method thereof, which makes the conveying surface of the elastic machine belt into the shape of a longitudinal groove pattern layer 6 through a special mold, completely solves the problem of belt marks caused by bending and warping of the elastic machine belt, and improves the product qualification rate; and through the coordination between the steps of compounding, cutting, tooth connection and inspection and warehousing, the bottom transmission layer 1, the first bridge connection layer 4, the main tensile layer 2, the second bridge connection, the surface conveying layer 3 and the groove pattern layer 6 can be made into an ultra-high holding force longitudinal groove pattern elastic machine belt, which can increase the surface friction coefficient of the elastic machine belt to greater than 1.8, thereby improving the conveying holding force, completely solving the problem of slippage of the elastic machine belt conveying products, ensuring that the product conveying can be accurately positioned and improving production efficiency; and the novel structural design and improved formula process of the elastic machine belt make the groove pattern layer 6 elastic machine belt solve all the defects of the existing elastic machine belt once and for all without edge grinding and chamfering, thereby greatly reducing the production cost.
[0047] It will be apparent to those skilled in the art that the invention is not limited to the details of the exemplary embodiments described above and that the invention can be implemented in other specific forms without departing from the spirit or essential features of the invention. Therefore, the embodiments should be considered exemplary and non-limiting in all respects, and the scope of the invention is defined by the appended claims rather than the foregoing description, and it is intended that all variations falling within the meaning and scope of the equivalent elements of the claims be included in the invention. Any reference numeral in a claim should not be considered as limiting the claim to which it relates.
Claims
1. An ultra-high holding force longitudinal groove pattern elastic machine belt, characterized in that: The elastic machine belt body includes a bottom transmission layer, a first bridging connection layer is arranged on the upper end surface of the bottom transmission layer, a main tensile layer is arranged on the upper end surface of the first bridging connection layer, a second bridging connection layer is arranged on the upper end surface of the main tensile layer, a surface conveying layer is arranged on the upper end surface of the second bridging connection layer, a groove pattern layer is arranged on the upper end surface of the surface conveying layer, and the groove pattern layer is longitudinally distributed on the conveying layer. A method for preparing an ultra-high holding force longitudinal groove pattern elastic machine belt comprises the following steps: Step S1: ingredients: generally, the elastic machine belt ingredients are composed of a bottom transmission layer, a first bridging connection layer, a main tensile layer, a second bridging connection layer, a surface conveying layer and a groove pattern layer, wherein the total thickness of the elastic machine belt is 1.0-1.5 mm, the thickness of the surface conveying layer and the groove pattern layer is 0.7-1.0 mm, the thickness of the main tensile layer is 0.15-0.35 mm, the thickness of the bottom transmission layer is 0.05 mm, the thickness of the first bridging connection layer and the second bridging connection layer are both 0.05 mm, Step S2: Compounding: When compounding the continuous line, the elastic machine belt must be kept in a tensioned state, and the surface of the elastic machine belt must be kept clean and flat. When compounding to the last car or stopping in the middle, it must be fully cooled, and then the pressure is released and relaxed. Step S3: Cutting: Cutting includes straight edge, cutting and toothing. Straight edge: Using the composite opposite alignment side as the reference, carefully trim the reference edge of the elastic machine belt. Cutting: Cut according to the reference edge and size. Generally, the width tolerance is ±0.2mm and the length tolerance is ±5mm. The length of the belt can be shortened by 3% to 8% according to the customized belt length. Teeth punching: Use a high-precision automatic tooth punching machine to punch out the following tooth-shaped interfaces according to the different sizes of the elastic machine belt using different cutting dies. Step S4: Tooth connection: First check whether the tooth interface has any missing or broken edges, then clean the joint, butt-joint and place it flat on the heat press heating template, place pads of the same thickness as the elastic machine belt on both sides of the joint, and then pad the surface of the joint with silicone embossed pads of the same pattern. Pay attention to the precise alignment of the teeth and ensure the straightness. After the joint is off the machine, clean and arrange the joint to ensure that the joint is neat and beautiful. Step S5: Inspection and storage: Print the product logo, model, size, manufacturer name and production date on the belt, which will be inspected by the inspector before being packaged and stored. When the thickness of the elastic machine belt in step S1 is 1.0mm, the thickness of the surface conveying layer and the groove pattern layer is 0.7mm, the thickness of the main tensile layer is 0.15mm, the thickness of the bottom transmission layer is 0.05mm, and the thickness of the first bridging connection layer and the second bridging connection layer are both 0.05mm; when the thickness of the elastic machine belt is 1.2mm, the thickness of the surface conveying layer and the groove pattern layer is 0.8mm, the thickness of the main tensile layer is 0.25mm, the thickness of the bottom transmission layer is 0.05mm, and the thickness of the first bridging connection layer and the second bridging connection layer are both 0.05mm; when the thickness of the elastic machine belt is 1.5mm, the thickness of the surface conveying layer and the groove pattern layer is 1.0mm, the thickness of the main tensile layer is 0.35mm, the thickness of the bottom transmission layer is 0.05mm, and the thickness of the first bridging connection layer and the second bridging connection layer are both 0.05mm, When the total thickness of the elastic machine belt made in step S2 is 1.0mm, the set temperature is 150-160℃, the speed of the composite line is 0.7M / min, the pressure of the No. 1 drum sulfur machine is 6MPa, and the pressure of the No. 2 drum sulfur machine is 4MPa; when the total thickness of the elastic machine belt is 1.2mm, the set temperature is 150-160℃, the speed of the composite line is 0.6M / min, the pressure of the No. 1 drum sulfur machine is 7MPa, and the pressure of the No. 2 drum sulfur machine is 5MPa; when the total thickness of the elastic machine belt is 1.5mm, the set temperature is 170-180℃, the speed of the composite line is 0.5M / min, the pressure of the No. 1 drum sulfur machine is 8MPa, and the pressure of the No. 2 drum sulfur machine is 6MPa, The tooth connection type in step S4 is tooth connection type, the hot pressing temperature is 160-180°C, the heat preservation time is 2-3min, the set pressure is 2-3MPa, and the off-machine temperature is below 40°C.
2. The ultra-high holding force longitudinal groove pattern elastic machine belt according to claim 1, characterized in that: The first bridging connection layer and the second bridging connection layer have the same structure, and both the first bridging connection layer and the second bridging connection layer are polyurethane resin adhesive coatings.
3. The ultra-high holding force longitudinal groove pattern elastic machine belt according to claim 1, characterized in that: The bottom transmission layer, the first bridging connection layer, the main tensile layer, the second bridging connection layer and the surface conveying layer have the same width.
4. The ultra-high holding force longitudinal groove pattern elastic machine belt according to claim 1, characterized in that: The bottom transmission layer, the first bridging connection layer, the main tensile layer, the second bridging connection layer and the surface conveying layer are all connected by bonding.
5. The ultra-high holding force longitudinal groove pattern elastic machine belt according to claim 1, characterized in that: The bottom transmission layer is a PUR antistatic or conductive elastomer bottom layer, the main tensile layer is a TPU elastomer tensile skeleton layer, and the surface transport layer is a thermoplastic high-grip polymer layer.