A surface mounted thick film fuse structure and manufacturing method thereof
By improving the current path structure of the surface-mount thick-film fuse to multiple parallel circuits and adding a heat insulation layer on the lower surface of the fuse element, the problems of low rated voltage and arcing are solved, realizing a fuse design with high rated voltage and low arcing, which is suitable for aerospace, aviation, electronics, shipbuilding and other fields.
Patent Information
- Application Number
- CN202210177941.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-02-25
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2042-02-25
AI Technical Summary
Existing surface-mount thick-film fuses have low rated voltages, and the arcing problem becomes more severe as the circuit power supply voltage increases.
The single current path is improved into a multi-channel series and parallel current path, a grid-type thick film structure is adopted, and a heat insulation layer is set on the lower surface of the fuse to improve the uniform distribution of energy during melting.
The rated voltage of the fuse has been increased, the generation of electric arc has been reduced, and the miniaturization and high reliability of the equipment have been maintained, making it suitable for mass production.
Smart Images

Figure CN114464509B_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the field of electronic components, and further relates to the field of film fuses, and in particular, to a surface-mount thick film fuse structure and a manufacturing method thereof. Background Art
[0002] Among electronic components, a fuse is a component that is connected in series in an electronic circuit for overcurrent protection. When the circuit current exceeds the specified value and lasts for a certain period of time, the fuse element itself generates more heat than the heat dissipated and the temperature of the fuse element reaches its melting point, causing the fuse element to melt, thereby achieving the purpose of overcurrent protection.
[0003] Surface mount thick film fuses are widely used in aerospace, aviation, electronics, shipbuilding and other fields due to their small size, stable electrical performance, high reliability and suitability for direct soldering and installation on PCB boards. Figure 1 As shown, it is an "I"-shaped single fuse structure. The fuse body is usually wide at both ends and narrow in the middle. The energy during melting is mainly concentrated in the narrowest area in the middle, generating a larger arc. Therefore, the rated voltage of surface-mount thick film fuses is usually low. As the circuit power supply voltage continues to increase, the rated voltage of thick film fuses must be increased accordingly, thereby further generating a larger arc.
[0004] In view of this, the present invention is proposed. Summary of the invention
[0005] The technical problem to be solved by the present invention is to solve the contradiction between increasing the rated voltage and reducing the arc in the prior art.
[0006] The inventive concept of the present invention is to improve the single current path of the existing surface-mount thick film fuse into a multi-channel series-parallel current path, which is realized by using a "grid" thick film on the thick film plane structure, and a heat insulation layer structure is provided on the lower surface of the fuse body, such as Figure 2 , Figure 3 As shown. For a fuse with a "grid" type graphic fuse link, the energy generated during melting is evenly distributed, thereby improving the arc suppression performance of the fuse and further increasing the rated voltage of the fuse.
[0007] To this end, the present invention provides a surface mount thick film fuse structure, such as Figure 2 , Figure 3 The invention comprises: a substrate substrate 1, a back electrode 2, a surface electrode 3, a heat insulating layer 4, a fuse layer 5, an encapsulating layer 6, a terminal electrode 7, a fuse body 8, a fuse isolation through hole 9, and a fuse 10.
[0008] The material of the substrate base plate 1 is a high temperature resistant insulating material, such as ceramic, glass, etc.
[0009] The back electrodes 2 are located at two ends of the back side of the substrate 1 .
[0010] The surface electrodes 3 are located at two ends of the surface of the substrate substrate 1 .
[0011] The heat insulation layer 4 is located on the surface of the substrate substrate 1 , and two ends of the heat insulation layer 4 are connected to the surface electrodes 3 at two ends of the surface of the substrate substrate 1 .
[0012] The fuse layer 5 is located on the surface of the heat insulating layer 4 , and two ends of the fuse layer 5 are connected to the surface electrodes 3 at two ends of the surface of the substrate substrate 1 .
[0013] The encapsulation layer 6 is located on the surface of the fuse layer 5, and two ends of the encapsulation layer 6 overlap with the surface electrodes 3 at two ends of the surface of the substrate substrate 1; the material of the encapsulation layer 6 is glass material.
[0014] The terminal electrode 7 covers the back electrode 2 , the surface electrode 3 and both ends of the substrate substrate 1 .
[0015] The fuse isolation through hole 9 passes through the fuse body 8. The shape, number, size and arrangement of the isolation through holes 9 are set according to the specific performance of the fuse, and can be circular, grooved or other shapes.
[0016] The fuse 10 is the end portion of the fuse body between the isolation through holes 9 and is a film-shaped fuse.
[0017] The manufacturing method of the surface-mount thick film fuse structure includes the following manufacturing process:
[0018] (1) Printing and sintering the surface electrode and the back electrode on the surface and back of the substrate respectively. The main components of the surface electrode and the back electrode are silver palladium, wherein the palladium content is 1% to 35%.
[0019] (2) Printing and sintering a heat-insulating layer on the surface of the substrate substrate on which the electrode has been prepared, wherein the main component of the heat-insulating layer is silicon dioxide.
[0020] (3) Printing and sintering a fuse layer on the surface of the prepared thermal insulation layer, wherein the main component of the fuse is a precious metal such as gold, silver, etc.
[0021] (4) Printing and sintering an encapsulation layer on the surface of the prepared fuse.
[0022] The heat insulation layer can be prepared by thick film screen printing, and the fired film thickness of the heat insulation layer is 10 μm to 100 μm.
[0023] The firing temperature of the heat insulation layer is greater than or equal to the firing temperature of the fuse layer.
[0024] The plane pattern of the fuse layer is a grid type, such as Figure 3As shown, it is composed of multiple fuses connected in series and parallel.
[0025] The fuse layer can be printed by thick film screen printing, and the fired film thickness of the fuse layer is 1 μm to 50 μm.
[0026] The firing temperature of the fuse layer is greater than or equal to the firing temperature or the curing temperature of the encapsulation layer.
[0027] Compared with the prior art, the present invention has the following beneficial effects:
[0028] (1) The rated voltage of surface mount thick film fuses can be greatly improved.
[0029] (2) As the circuit power supply voltage continues to increase, the arc can be controlled to a very small level, solving the contradiction of increasing the rated voltage and causing the arc to increase accordingly.
[0030] (3) Because it is an integrated process, it has a small size and high reliability.
[0031] (4) Suitable for batch and large-scale production, with high quality consistency, high yield and low cost.
[0032] The invention is widely used in the field of miniaturized surface-mount fuses with high operating voltage and low arc and high reliability. BRIEF DESCRIPTION OF THE DRAWINGS
[0033] Figure 1 It is a schematic diagram of the planar structure of the fuse link of an existing fuse.
[0034] Figure 2 It is a schematic diagram of the longitudinal structure of the fuse of the present invention.
[0035] Figure 3 It is a schematic diagram of the planar structure of the fuse layer of the present invention.
[0036] In the figure: 1 is a substrate substrate, 2 is a back electrode, 3 is a surface electrode, 4 is a heat insulating layer, 5 is a fuse layer, 6 is an encapsulation layer, 7 is a terminal electrode, 8 is a fuse body, 9 is a fuse isolation through hole, and 10 is a fuse. DETAILED DESCRIPTION
[0037] Combination Figure 2 , Figure 3 The specific implementation methods of the technical solution of the present invention are as follows:
[0038] (1) Material preparation: Select a ceramic substrate as the base substrate, and use a dicing machine to draw the split lines (i.e., the grooves for splitting a single fuse chip) on the ceramic substrate according to the arrangement and layout size of the fuse.
[0039] (2) Screen printing the surface electrode and the back electrode on the surface of the scribed ceramic substrate. The main components of the surface electrode and the back electrode are silver palladium, wherein the palladium content is 1% to 35%.
[0040] (3) A thermal insulation layer is prepared on the surface of the ceramic substrate on which the electrode has been prepared. The thermal insulation layer is mainly composed of silicon dioxide. The sintering temperature of the thermal insulation layer is 850°C ± 30°C. The sintering film thickness of the thermal insulation layer is 10 μm to 100 μm.
[0041] (4) Screen printing a fuse layer on the surface of the prepared thermal insulation layer. The main component of the fuse is gold or silver. The plane structure of the fuse layer is as follows: Figure 2 As shown, it has a grid structure, which is composed of 4 rows of fuses connected in series, each row of fuses is composed of 3 fuses connected in parallel, the firing film thickness of the fuse body is 1μm~50μm, and the firing temperature of the fuse body is 850℃±30℃.
[0042] (5) A glass encapsulation layer is printed on the surface of the prepared fuse, wherein the main component of the encapsulation layer is glass, the fired film thickness of the encapsulation layer is 5 μm to 50 μm, and the firing temperature of the encapsulation layer is 600°C ± 30°C.
[0043] (6) Printing a logo on the surface of the prepared encapsulation layer to facilitate subsequent screening of the product.
[0044] (7) For the product with printed logo, the first strip splitting is performed along the middle line of adjacent electrodes, and then the end surface of the strip product is silver coated. The main component of the silver coating paste is silver palladium, the palladium solder is 1% to 30%, the silver coating depth is 0.1mm to 2mm, and the silver coating firing temperature is 600℃±30℃.
[0045] (8) The silver-coated strip product is subjected to secondary granular cracking.
[0046] (9) The granular products of the secondary split are electroplated, first with nickel, then with lead or tin-lead, with the thickness of the nickel layer being ≥3μm.
[0047] Finally, it should be noted that the above embodiments are merely examples for the purpose of clear explanation. The present invention includes but is not limited to the above embodiments. It is not necessary and impossible to list all implementation methods exhaustively. For ordinary technicians in the relevant field, other different forms of changes or modifications can be made based on the above description. All implementation methods that meet the requirements of the present invention belong to the protection scope of the present invention.
Claims
1. A method for manufacturing a surface-mount thick film fuse structure, characterized in that: The surface-mount thick film fuse structure comprises: a substrate substrate, a back electrode, a surface electrode, a heat insulation layer, a fuse layer, an encapsulation layer, a terminal electrode, a fuse body, a fuse isolation through hole, and a fuse; The material of the substrate base sheet is a high temperature resistant insulating material; The back electrodes are located at two ends of the back side of the substrate; The surface electrodes are located at both ends of the surface of the substrate; The heat insulation layer is located on the surface of the substrate substrate, and two ends of the heat insulation layer are connected to the surface electrodes at two ends of the surface of the substrate substrate; The fuse layer is located on the surface of the heat insulation layer, and two ends of the fuse layer are connected to the surface electrodes at two ends of the substrate substrate surface; The plane structure of the fuse layer is a grid structure, which is composed of a plurality of fuses connected in series and in parallel; The encapsulation layer is located on the surface of the fuse layer, and the two ends of the encapsulation layer overlap with the surface electrodes at the two ends of the substrate substrate surface; The terminal electrodes cover the back electrode, the surface electrode and both ends of the substrate; The fuse isolation through hole is circular or slot-shaped and penetrates the fuse body. The shape, number, size and arrangement of the isolation through hole are set according to the specific performance of the fuse; The fuse is the end portion of the fuse body between the isolation through holes; The manufacturing method of the surface mount thick film fuse structure is as follows: The thermal insulation layer is prepared by thick film screen printing, and the fuse layer is prepared by thick film screen printing; (1) Material preparation: The substrate is a ceramic substrate. The cleavage line is drawn on the ceramic substrate according to the arrangement and layout size of the fuse using a scriber. The surface electrode and back electrode materials are made of silver-palladium slurry containing 1% to 35% palladium. The insulation layer material is made of silicon dioxide slurry. The fuse material is made of gold slurry or silver slurry. The encapsulation layer material is made of glass slurry. The end silver coating material is made of silver-palladium slurry containing 1% to 30% palladium. (2) Screen printing the surface electrode and the back electrode on the surface of the scribed ceramic substrate; (3) preparing a thermal insulation layer on the surface of the ceramic substrate on which the electrode has been prepared, the sintering temperature of the thermal insulation layer is 850°C ± 30°C, and the sintering film thickness of the thermal insulation layer is 10 μm to 100 μm; (4) Screen printing a fuse layer on the surface of the prepared thermal insulation layer, the fired film thickness of the fuse is 1 μm to 50 μm, and the firing temperature of the fuse is 850°C ± 30°C; (5) Printing an encapsulation layer on the surface of the prepared fuse link, the fired film thickness of the encapsulation layer is 5 μm to 50 μm, and the firing temperature of the encapsulation layer is 600°C ± 30°C; (6) Printing product logo on the surface of the prepared encapsulation layer; (7) For the product with printed logo, the first strip splitting is performed along the middle line of adjacent electrodes, and then the end surface of the strip product is silver coated. The silver coating depth is 0.1mm~2mm, and the silver coating firing temperature is 600℃±30℃; (8) Performing secondary granular splitting on the silver-coated strip product; (9) The granular products of the secondary split are electroplated, first with nickel, then with lead or tin-lead, with the thickness of the nickel layer being ≥3μm.
2. A method for manufacturing a surface mount thick film fuse structure as claimed in claim 1, characterized in that: The material of the substrate is ceramic or glass.
3. The method for manufacturing a surface mount thick film fuse structure according to claim 1, characterized in that: The material of the encapsulation layer is glass material.
4. The method for manufacturing a surface mount thick film fuse structure according to claim 1, characterized in that: The grid structure is formed by four rows of fuses connected in series, and each row of fuses is formed by three fuses connected in parallel.
5. The method for manufacturing a surface mount thick film fuse structure according to claim 1, characterized in that: The fuse is a film fuse.