Electrode sheets, electrode assemblies, battery cells, batteries and electrical devices

By setting expansion elements in the thinner areas of the active material layer on the electrode, the lithium plating problem during long-cycle operation of the battery is solved, improving the cycle performance of the battery and saving material costs.

CN117941088BActive Publication Date: 2026-11-10CONTEMPORARY AMPEREX TECHNOLOGY CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202280061125.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-07-29
Publication Date
2026-11-10
Estimated Expiration
2042-07-29

AI Technical Summary

Technical Problem

In existing battery technologies, lithium plating is prone to occur on electrodes during long-term cycling, causing metal ions to accumulate in the thinner areas of the active material layer, which affects battery performance.

Method used

An expansion element is placed in the area where the active material layer of the electrode is thin. The expansion element expands when it comes into contact with the electrolyte to reduce the distance between the positive and negative electrodes, suppress the polarization loss of metal ion transfer, and prevent lithium plating.

Benefits of technology

By incorporating expansion components, lithium plating on the electrodes can be effectively suppressed, improving the battery's cycle performance and saving material costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117941088B_ABST
    Figure CN117941088B_ABST
Patent Text Reader

Abstract

This application provides an electrode sheet, an electrode assembly, a battery cell, a battery, and an electrical device. The electrode sheet includes: a current collector, which includes a tab, a first region, and a second region sequentially disposed along a first direction; an expansion member disposed in at least a portion of the first region adjacent to the second region, configured to expand after being immersed in electrolyte; the first and second regions are coated with active material layers, wherein the thickness of the active material layer corresponding to the first region is less than the thickness of the active material layer corresponding to the second region; the expansion member is disposed between the active material layer and the first region. The technical solution provided by this application can suppress lithium plating of the electrode sheet during long-term cycling, thereby improving the cycle performance of the battery.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of battery technology, and in particular to an electrode sheet, electrode assembly, battery cell, battery, and electrical device. Background Technology

[0002] With increasing environmental pollution, the new energy industry is attracting more and more attention. Within the new energy industry, battery technology is a crucial factor in its development.

[0003] In the development of battery technology, how to improve battery performance is a problem that urgently needs to be solved. Summary of the Invention

[0004] In view of the above problems, embodiments of this application provide an electrode sheet, an electrode assembly, a battery cell, a battery, and an electrical device, which can improve the cycle performance of the battery.

[0005] In a first aspect, an electrode is provided, comprising: a current collector, the current collector including a tab, a first region, and a second region sequentially disposed along a first direction; an expansion member disposed in at least a portion of the first region adjacent to the second region, the expansion member being configured to expand upon immersion in an electrolyte; the first region and the second region being coated with an active material layer, wherein the thickness of the active material layer corresponding to the first region is less than the thickness of the active material layer corresponding to the second region; and the expansion member being disposed between the active material layer and the first region.

[0006] In this embodiment, the electrode includes a current collector and an expansion member. Further, the current collector includes a tab and a first region and a second region coated with an active material layer. The thickness of the active material layer coated on the first region is less than that coated on the second region, which prevents edge bursting and active material layer detachment during cold pressing. However, the different thicknesses of the active material layers result in different metal ion transport distances, leading to metal ion accumulation in the thinner active material layer areas during long-term battery cycling, causing lithium plating. By providing an expansion member in at least a portion of the first region adjacent to the second region, which expands upon contact with the electrolyte, the lithium plating problem that easily occurs in the thinner active material layer areas of the electrode during long-term cycling can be solved. By providing a thinner active material layer in the first region, active material detachment during electrode fabrication can be prevented. Simultaneously, by providing an expansion member that expands upon contact with the electrolyte between the portion of the first region adjacent to the second region and the corresponding active material in the first region, lithium plating during long-term cycling can be prevented, thereby improving the battery's cycle performance.

[0007] In one possible implementation, the first region includes a first sub-region and a second sub-region, the second sub-region being adjacent to the second region, and the expansion member being disposed in the second sub-region.

[0008] In this embodiment, the current collector includes a tab, a first region, and a second region disposed along a first direction; further, the first region includes a first sub-region and a second sub-region, with the second sub-region adjacent to the second region. That is, the current collector includes a tab, a first sub-region, a second sub-region, and a second region disposed along a first direction. By providing an expansion member on the second sub-region, which has a thinner active material layer and is adjacent to the second region, the lithium plating problem of the electrode during long-cycle processing can be solved, thereby improving the cycle performance of the battery; and by providing the expansion member only on the second sub-region, rather than the entire first region, the function of the expansion member in suppressing lithium plating of the electrode can be utilized while also saving material costs.

[0009] In one possible implementation, the thickness of the active material layer corresponding to the first region gradually increases along a first direction.

[0010] In this embodiment, along the first direction, the first region is closer to the tab than the second region. Appropriately thinning the active material layer in the first region, specifically reducing the thickness of the active material layer near the tab, prevents edge bursting of the electrode during manufacturing. The thickness of the active material layer corresponding to the first region gradually increases along the first direction, meaning the active material layer is thinnest in the region closest to the tab. This maximizes the prevention of active material shedding from the electrode, improving electrode performance and consequently, battery performance.

[0011] In one possible implementation, along the first direction, the thickness change rate of the active material layer corresponding to the first sub-region is greater than the thickness change rate of the active material layer corresponding to the second sub-region.

[0012] In this embodiment, to suppress lithium plating on the electrode, an expansion member is provided in a first region near the electrode tab. The expansion member can be provided only in a second sub-region adjacent to the second region. This allows the expansion member to suppress lithium plating on the electrode, improving battery cycle performance, and also saves material costs, avoiding unnecessary material waste. Furthermore, compared to the second sub-region, the first sub-region is closer to the edge of the electrode. In a battery, the first sub-region on the electrode is generally the portion extending beyond the other electrode, and its function is to allow metal ions in the battery to intercalate into the other electrode. By making the thickness change rate of the active material layer corresponding to the first sub-region greater than that corresponding to the second sub-region, it is ensured that metal ions can intercalate into the other electrode, thereby ensuring the normal function of the battery.

[0013] In one possible implementation, the thickness variation trend of the expansion member is opposite to the thickness variation trend of the active material layer corresponding to the second sub-region.

[0014] In this embodiment, the thickness of the active material layer corresponding to the first region gradually increases along the first direction. That is, the active material layer is thinner in the region closer to the electrode and thicker in the region farther away from the electrode. To suppress lithium plating on the electrode and improve the cycle performance of the battery, an expansion member is provided in part of the first region. The first region with the expansion member has a thicker thickness than the first region without the expansion member, which reduces the polarization loss of metal ion transfer and thus suppresses the accumulation of metal ions. By making the thickness change trend of the expansion member opposite to that of the active material layer corresponding to the second sub-region, that is, the thickness of the expansion member becomes thinner and thinner along the first direction, while the thickness of the active material layer corresponding to the second sub-region becomes thicker and thicker, the first region with the expansion member is kept at a relatively stable thickness overall, thereby suppressing the accumulation of metal ions in the first region during long-term cycling and improving the cycle performance of the battery.

[0015] In one possible implementation, the sum of the thickness of the expanded member after expansion and the thickness of the active material layer corresponding to the expanded member is equal to the thickness of the active material layer corresponding to the second region.

[0016] In this embodiment, because the thickness of the active material coated on the first and second regions of the same electrode is different, the polarization loss of metal ion transfer is increased. This causes metal ions to accumulate in the thinner first region during long-term battery cycling, resulting in lithium plating. By providing an expansion member in part of the first region, the thickness of the expansion member after expansion in the electrolyte is made equal to the thickness of the active material layer corresponding to the expansion member, which is equal to the thickness of the active material layer corresponding to the second region. In other words, the thickness of the first and second regions coated with the active material layer is kept consistent during battery operation. This can suppress the accumulation of metal ions at the electrode edge and solve the problem of lithium plating on the electrode. In one possible implementation, the liquid absorption rate of the material of the expansion member is 20%-100%.

[0017] In this embodiment, to suppress lithium plating on the electrode during long-cycle operation, an expansion member is provided on the portion of the first region adjacent to the second region. Using a material with a liquid absorption rate of 20%-100% for the expansion member results in good expansion performance.

[0018] In one possible implementation, the swelling rate of the material of the expander is 10%-300%.

[0019] In this embodiment, to suppress lithium plating on the electrode during long-cycle operation, an expansion element is provided on the portion of the first region adjacent to the second region. A material with a swelling ratio of 10%-300% is used as the expansion element, resulting in good expansion performance.

[0020] In one possible implementation, the swelling rate of the material of the expansion member is 50%-200%.

[0021] In the embodiments of this application, when the expansion component is prepared using a material with a swelling rate of 50%-200%, the expansion component has relatively stable expansion performance.

[0022] In one possible implementation, the main material of the expansion member is at least one of the following: oriented polystyrene, thermoplastic polyurethane, ethylene-vinyl acetate copolymer, silicone film, and styrene resin.

[0023] In this embodiment, oriented polystyrene, thermoplastic polyurethane, ethylene-vinyl acetate copolymer, silicone film, and styrene resin are all commonly used materials that are easy to obtain and have good expansion effects. Using at least one of these materials as raw materials to prepare the expanded parts ensures good expansion performance while reducing manufacturing costs, which is beneficial for its widespread application in production.

[0024] In one possible implementation, the size of the expansion member is 10-15 mm in the first direction.

[0025] In this embodiment, the size of the expansion component is maintained at 10-15mm, which can ensure the normal function of the expansion component and avoid occupying too much area of ​​the current collector, thereby ensuring the energy density of the battery.

[0026] In one possible implementation, the size of the second sub-region is 10-15 mm in the first direction.

[0027] In this embodiment, the first region includes a first sub-region and a second sub-region. The expansion member can be disposed on the entire first region or only on the second sub-region. In the first direction, the size of the second sub-region is set to 10-15mm to leave sufficient space for the installation of the expansion member.

[0028] In one possible implementation, the thickness difference between the active material layer corresponding to the first region and the active material layer corresponding to the second region is 1-20 μm.

[0029] In this embodiment, in the first direction, the first region is closer to the electrode tab than the second region, making the thickness of the active material layer corresponding to the first region smaller than that corresponding to the second region. This can prevent edge bursting and active material layer detachment during electrode manufacturing. However, simply reducing the thickness of the active material layer corresponding to the first region can also affect the energy density of the battery. By maintaining the thickness difference between the active material layer corresponding to the first region and the active material layer corresponding to the second region at 1-20 μm, both active material layer detachment from the electrode and battery energy density can be guaranteed.

[0030] In one possible implementation, the thickness of the expansion element is 1-20 μm.

[0031] In this embodiment, after the expanded element is immersed in the electrolyte, its expanded thickness and the thickness of its corresponding active material layer are equal to the thickness of the active material layer corresponding to the second region. If the expanded thickness of the expanded element is too high, it will still have an adverse effect on battery performance. By maintaining the thickness of the expanded element at 1-20 μm, the effect of the expanded element in suppressing lithium plating on the electrode can be optimized.

[0032] In one possible implementation, the thickness of the active material layer corresponding to the first sub-region is 0-50 μm.

[0033] In this embodiment, because the positions of the other electrode in the battery corresponding to the first sub-region and the second sub-region are different, an expansion member may not be provided on the first sub-region. Furthermore, compared to the second sub-region, the thickness change rate of the active material layer corresponding to the first sub-region is greater than the thickness difference of the active material layer corresponding to the second sub-region. That is, the active material layer thickness of the first region is thinner than that of the second region, and the active material layer thickness corresponding to the first sub-region is even thinner within the first region. By maintaining the thickness of the active material layer corresponding to the first sub-region at 0-50 μm, a larger thickness difference in the active material layer between it and the second region is achieved, thus maximizing the protection against active material layer detachment during electrode fabrication.

[0034] In one possible implementation, the thickness of the active material layer corresponding to the second sub-region is 20-80 μm.

[0035] In this embodiment, on the one hand, the active material layer corresponding to the second sub-region still has a thickness difference with the second region, which can continue to prevent the electrode edge from bursting; on the other hand, an expansion member can be provided on the second sub-region to suppress lithium plating on the electrode and improve the cycle performance of the battery. By making the thickness of the active material layer corresponding to the second sub-region between 20-80μm, the second sub-region can both prevent the electrode edge from bursting and suppress lithium plating on the electrode, thereby improving the cycle performance of the battery.

[0036] In a second aspect, an electrode assembly is provided, including the electrode sheet in any of the above embodiments.

[0037] Thirdly, a battery cell is provided, comprising: the electrode assembly in the above embodiments; a housing having an opening for receiving the electrode assembly; and an end cap for closing the opening.

[0038] Fourthly, a battery is provided, comprising a plurality of battery cells as described in the above embodiments.

[0039] Fifthly, an electrical device is provided, including the battery in the above embodiments, the battery being used to provide electrical energy. Attached Figure Description

[0040] To more clearly illustrate the technical solutions of the embodiments of this application, the drawings used in the embodiments of this application will be briefly introduced below. Obviously, the drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on the drawings without creative effort.

[0041] Figure 1 This is a schematic diagram of the structure of a vehicle according to an embodiment of this application; Figure 2 This is an exploded structural diagram of a battery according to an embodiment of this application; Figure 3 This is a schematic diagram of a battery cell according to an embodiment of this application; Figure 4 This is a schematic diagram of the structure of an electrode sheet according to an embodiment of this application; Figure 5 This is a schematic diagram of different regions of the current collector according to an embodiment of this application; Figure 6 This is a schematic diagram of the structure of an electrode sheet according to another embodiment of this application; Explanation of reference numerals in the attached figures: Vehicle 1, Battery 2, Battery cell 3; Controller 11, motor 12, housing 20, electrode assembly 31, outer shell 32, electrode terminal 33, connecting component 34, pressure relief mechanism 35, electrode plate 40, current collector 41, expansion component 42; First housing 201, second housing 202, accommodating space 203, housing 321, positive electrode terminal 331, negative electrode terminal 332, end cap 361, first region 411, second region 412, electrode tab 413; First sub-region 4111, second sub-region 4112, first direction X. Detailed Implementation

[0042] The embodiments of the technical solution of this application will now be described in detail with reference to the accompanying drawings. These embodiments are only used to more clearly illustrate the technical solution of this application and are therefore merely examples, and should not be used to limit the scope of protection of this application.

[0043] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this application pertains; the terminology used herein is for the purpose of describing particular embodiments only and is not intended to limit the application; the terms “comprising” and “having”, and any variations thereof, in the specification, claims, and foregoing description of the drawings are intended to cover non-exclusive inclusion.

[0044] In the description of the embodiments of this application, technical terms such as "first" and "second" are used only to distinguish different objects and should not be construed as indicating or implying relative importance or implicitly specifying the number, specific order, or primary and secondary relationship of the indicated technical features. In the description of the embodiments of this application, "multiple" means two or more, unless otherwise explicitly defined.

[0045] In this document, the term "embodiment" means that a particular feature, structure, or characteristic described in connection with an embodiment may be included in at least one embodiment of this application. The appearance of this phrase in various places throughout the specification does not necessarily refer to the same embodiment, nor is it a separate or alternative embodiment mutually exclusive with other embodiments. It will be explicitly and implicitly understood by those skilled in the art that the embodiments described herein can be combined with other embodiments.

[0046] In the description of the embodiments in this application, the term "and / or" is merely a description of the relationship between related objects, indicating that three relationships can exist. For example, A and / or B can represent: A existing alone, A and B existing simultaneously, and B existing alone. Additionally, the character " / " in this document generally indicates that the preceding and following related objects have an "or" relationship.

[0047] In the description of the embodiments of this application, the term "multiple" refers to two or more (including two), similarly, "multiple sets" refers to two or more (including two sets), and "multiple pieces" refers to two or more (including two pieces).

[0048] In the description of the embodiments of this application, the technical terms "center," "longitudinal," "lateral," "length," "width," "thickness," "upper," "lower," "front," "rear," "left," "right," "vertical," "horizontal," "top," "bottom," "inner," "outer," "clockwise," "counterclockwise," "axial," "radial," and "circumferential" indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are only for the convenience of describing the embodiments of this application and simplifying the description, and are not intended to indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on the embodiments of this application.

[0049] In the description of the embodiments of this application, unless otherwise expressly specified and limited, technical terms such as "installation," "connection," "joining," and "fixing" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral part; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; they can refer to the internal communication of two components or the interaction between two components. For those skilled in the art, the specific meaning of the above terms in the embodiments of this application can be understood according to the specific circumstances.

[0050] In this application, the battery cell may include lithium metal secondary batteries, sodium metal batteries, or magnesium metal batteries, etc., and the embodiments of this application are not limited to this. The battery cell may be cylindrical, flat, or other shapes, and the embodiments of this application are not limited to this either. Battery cells are generally divided into three types according to their packaging method: cylindrical battery cells, square battery cells, and pouch battery cells, and the embodiments of this application are not limited to this either. For ease of explanation, the following embodiments use lithium metal batteries as an example for illustration.

[0051] The battery mentioned in the embodiments of this application refers to a single physical module comprising one or more battery cells to provide higher voltage and capacity. For example, the battery mentioned in this application may include a battery module or a battery pack. A battery generally includes a housing for encapsulating one or more battery cells. The housing prevents liquids or other foreign matter from affecting the charging or discharging of the battery cells.

[0052] In existing batteries, the positive and negative electrode sheets have active material thinning zones after coating with active materials. These zones are designed to prevent edge bursting and active material layer detachment during electrode fabrication. However, the presence of these thinning zones also leads to lithium plating, where metal ions accumulate at the edges of the thinning zones during long-term cycling. To alleviate lithium plating, two main technical approaches are currently employed: (1) increasing the cell balance (CB) value of the electrode, which is the ratio of the unit area capacity of the negative electrode active material to the unit area capacity of the positive electrode active material layer; and (2) directly creating local protrusions on the current collector corresponding to the thinning zone.

[0053] However, in practical applications, neither of the above two methods is ideal. Because both the positive and negative electrode edges have thinned active material areas, the distance between them increases, increasing polarization loss in metal ion transfer, and lithium plating still occurs during long-term cycling. Furthermore, while directly creating protrusions on the current collector can alleviate lithium plating to some extent, excessively high protrusions can lead to edge bursting and decarburization during electrode fabrication; conversely, excessively low protrusions are ineffective, and the significant distance between the thinned active material areas of the positive and negative electrodes still results in lithium plating.

[0054] In view of the above problems, this application provides an electrode with an expansion element. After the expansion element is wetted by the electrolyte, it can reduce the distance between the positive and negative electrodes, reduce the polarization loss of metal ion transfer, thereby suppressing lithium deposition on the electrode and improving the cycle performance of the battery.

[0055] The electrode sheets described in the embodiments of this application are applicable to electrode assemblies, battery cells, batteries, and electrical devices.

[0056] Electrical equipment can include vehicles, mobile phones, portable devices, laptops, ships, spacecraft, electric toys, and power tools, etc. Vehicles can be gasoline-powered cars, natural gas-powered cars, or new energy vehicles; new energy vehicles can be pure electric vehicles, hybrid electric vehicles, or range-extended electric vehicles, etc. Spacecraft include airplanes, rockets, space shuttles, and spacecraft, etc. Electric toys include stationary or mobile electric toys, such as game consoles, electric car toys, electric ship toys, and electric airplane toys, etc. Power tools include metal cutting power tools, grinding power tools, assembly power tools, and railway power tools, such as electric drills, electric grinders, electric wrenches, electric screwdrivers, electric hammers, impact drills, concrete vibrators, and electric planers, etc. This application does not impose any special limitations on the above-mentioned electrical devices.

[0057] For ease of explanation, the following embodiments will use a vehicle as an example of an electrical device.

[0058] Figure 1 This is a schematic diagram of the structure of a vehicle 1 provided in an embodiment of this application. Figure 1 As shown, a battery 2 is installed inside the vehicle 1. The battery 2 can be located at the bottom, front, or rear of the vehicle 1. The battery 2 can be used to power the vehicle 1; for example, the battery 2 can serve as the operating power source for the vehicle 1.

[0059] The vehicle 1 may also include a controller 11 and a motor 12. The controller 11 is used to control the battery 2 to supply power to the motor 12, for example, for the power needs of the vehicle 1 during startup, navigation and driving.

[0060] In some embodiments of this application, the battery 2 can not only serve as the operating power source for the vehicle 1, but also as the driving power source for the vehicle 1, replacing or partially replacing fuel or natural gas to provide driving power for the vehicle 1.

[0061] Figure 2 This is an exploded schematic diagram of battery 2 provided in one embodiment of this application. Figure 2 As shown, battery 2 includes a housing 20 and a battery cell 3, with the battery cell 3 housed within the housing 20.

[0062] The housing 20 is used to accommodate the battery cell 3. The housing 20 can have various structures. In some embodiments, the housing 20 may include a first housing portion 201 and a second housing portion 202, which overlap each other, and together define a receiving space 203 for accommodating the battery cell 3. The second housing portion 202 may be a hollow structure with one end open, and the first housing portion 201 may be a plate-like structure, with the first housing portion 201 covering the open side of the second housing portion 202 to form a housing 20 with the receiving space 203; the first housing portion 201 and the second housing portion 202 may also both be hollow structures with one side open, with the open side of the first housing portion 201 covering the open side of the second housing portion 202 to form a housing 20 with the receiving space 203. Of course, the first box section 201 and the second box section 202 can be of various shapes, such as cylinders, cuboids, etc.

[0063] To improve the sealing performance after the first housing part 201 and the second housing part 202 are connected, a sealing element, such as sealant or sealing ring, can also be provided between the first housing part 201 and the second housing part 202.

[0064] Assuming that the first box part 201 covers the top of the second box part 202, the first box part 201 can also be called the upper box cover, and the second box part 202 can also be called the lower box.

[0065] In battery 2, there are multiple battery cells 3. These multiple battery cells 3 can be connected in series, parallel, or in a mixed configuration. A mixed configuration means that multiple battery cells 3 are connected in both series and parallel connections. Multiple battery cells 3 can be directly connected in series, parallel, or in a mixed configuration and then housed within the housing 20. Alternatively, multiple battery cells 3 can first be connected in series, parallel, or in a mixed configuration to form a battery module (not shown in the figure), and then these battery modules can be connected in series, parallel, or in a mixed configuration to form a whole, which is then housed within the housing 20. The multiple battery cells 3 within a battery module can be electrically connected through a busbar component to achieve parallel, series, or mixed connections.

[0066] like Figure 3 The diagram shown is a structural schematic of a battery cell 3 according to an embodiment of this application. The battery cell 3 includes one or more electrode assemblies 31, a housing 321, and an end cap 361. The housing 321 and the end cap 361 form a casing or battery box 32. The walls of the housing 321 and the end cap 361 are both referred to as the walls of the battery cell 3. For a cuboid battery cell 3, the walls of the housing 321 include a bottom wall and four side walls. The shape of the housing 321 depends on the shape of the assembled one or more electrode assemblies 31. For example, the housing 321 can be a hollow cuboid, cube, or cylinder, and one face of the housing 321 has an opening so that one or more electrode assemblies 31 can be placed inside the housing 321. For example, when the housing 321 is a hollow cuboid or cube, one plane of the housing 321 is an open face, that is, this plane does not have a wall, allowing communication between the inside and outside of the housing 321. When the housing 321 can be a hollow cylinder, the end face of the housing 321 is an open face, that is, the end face does not have a wall, allowing the inside and outside of the housing 321 to communicate. The end cap 361 covers the opening and is connected to the housing 321 to form a closed cavity for placing the electrode assembly 31. The housing 321 is filled with an electrolyte, such as an electrolyte solution.

[0067] The battery cell 3 may also include two electrode terminals 33, which can be disposed on the end cover 361. The end cover 361 is typically flat, and the two electrode terminals 33 are fixed to the flat surface of the end cover 361. The two electrode terminals 33 are a positive electrode terminal 331 and a negative electrode terminal 332, respectively. Each electrode terminal 33 is provided with a corresponding connecting member 34, or a current collector 34, which is located between the end cover 316 and the electrode assembly 31, and is used to electrically connect the electrode assembly 31 and the electrode terminal 33.

[0068] In this battery cell 3, depending on actual usage requirements, the electrode assembly 31 can be configured as a single unit or multiple units, such as... Figure 3 As shown, the battery cell 3 contains four independent electrode assemblies 31.

[0069] Figure 4 This is a schematic diagram of the structure of an electrode sheet according to an embodiment of this application. Figure 5 This is a schematic diagram of different regions of the current collector according to an embodiment of this application. For example... Figure 4 and Figure 5 As shown, the electrode 40 includes: a current collector 41, which includes a tab 413, a first region 411, and a second region 412 arranged sequentially along a first direction X; an expansion member 42, disposed in at least a portion of the first region 411 adjacent to the second region 412, the expansion member 42 being configured to expand after being wetted by an electrolyte; the first region 411 and the second region 412 are coated with an active material layer, wherein the active material layer corresponding to the first region 411 is less than the thickness of the active material layer corresponding to the second region 412; the expansion member 42 is disposed between the active material layer and the first region 411.

[0070] In this embodiment, the expansion member 42 being disposed between the active material layer and the first region 411 means that when the first region 411 is not coated with active material, the expansion member 42 is first disposed on the first region 411, and then the active material is coated on the expansion member 42. That is, along the thickness direction of the electrode 40, the expansion member 42 is disposed between the active material layer and the first region 411.

[0071] The electrode 40 includes a current collector 41 and an expansion member 42. Further, the current collector 41 includes a tab 413 and a first region 411 and a second region 412 coated with an active material layer. The thickness of the active material layer coated on the first region 411 is smaller than that coated on the second region 412, which can prevent the electrode 40 from cracking or the active material layer from falling off during cold pressing.

[0072] However, when problems such as edge bursting during the preparation of the electrode 40 are solved by setting a first region 411 and a second region 412 with different active material layer thicknesses, the difference in the thickness of the active material layer coated on the first region 411 and the second region 412 will cause different metal ion transport distances. During long-term cycling of the battery 2, metal ions will accumulate in the region with the thinner active material layer, causing lithium plating. Therefore, an expansion member 42 is provided in at least a portion of the first region 411 adjacent to the second region 412. The expansion member 42 expands when it comes into contact with the electrolyte, which can solve the lithium plating problem that easily occurs in the first region 411 of the electrode 40 with a thinner active material layer during long-term cycling of the battery 2.

[0073] In the above scheme, by setting a first region 411 with a thinner active material layer, the active material of the electrode 40 can be prevented from falling off during the preparation process; at the same time, by setting an expansion member 42 that can expand when exposed to electrolyte between the first region 411 and the active material corresponding to the first region 411 adjacent to the second region 412, the electrode 40 can be prevented from lithium plating during long-term cycling, thereby improving the cycle performance of the battery 2.

[0074] In some embodiments, the first region 411 includes a first sub-region 4111 and a second sub-region 4112, the second sub-region 4112 being adjacent to the second region 412, and the expansion member 42 being disposed in the second sub-region 4112.

[0075] The current collector 41 includes a tab 413, a first region 411, and a second region 412 disposed along a first direction X; further, the first region 411 includes a first sub-region 4111 and a second sub-region 4112, and the second sub-region 4112 is adjacent to the second region 412. That is, the current collector 41 includes a tab 413, a first sub-region 4111, a second sub-region 4112, and a second region 412 disposed along a first direction X.

[0076] In the above solution, by setting the expansion member 42 in the second sub-region 4112, which has a thinner active material layer and is adjacent to the second region 412, the lithium plating problem of the electrode 40 during long cycle can be solved, thereby improving the cycle performance of the battery 2; and by setting the expansion member 42 only in the second sub-region 4112 rather than in the entire first region 411, the material cost can be saved while the expansion member 42 suppresses lithium plating of the electrode 40.

[0077] In some embodiments, along the first direction X, the thickness of the active material layer corresponding to the first region 411 gradually increases.

[0078] Along the first direction X, the first region 411 is closer to the tab 413 than the second region 412. Appropriately thinning the active material layer on the first region 411, that is, thinning the active material layer on the first region 411 that is closer to the tab 413, can prevent the electrode 40 from bursting during the preparation process.

[0079] In the above scheme, by making the thickness of the active material layer corresponding to the first region 411 gradually increase along the first direction X, that is, the thickness of the active material layer corresponding to the region away from the tab 413 is the thinnest, this can prevent the active material on the electrode 40 from falling off to the greatest extent, improve the performance of the electrode 40, and thus improve the performance of the battery 2.

[0080] In some embodiments, along the first direction X, the thickness change rate of the active material layer corresponding to the first sub-region 4111 is greater than the thickness change rate of the active material layer corresponding to the second sub-region 4112.

[0081] To suppress lithium plating on the electrode 40, an expansion member 42 is provided on the first region 411 near the tab. The expansion member 42 can be provided only on the second sub-region 4112 adjacent to the second region 412. This allows the expansion member 42 to suppress lithium plating on the electrode 40, improving the cycle performance of the battery 2, while also saving material costs and avoiding unnecessary material waste. Furthermore, compared to the second sub-region 4112, the first sub-region 4111 is closer to the edge of the tab 40. In the battery 2, the first sub-region 4111 on the electrode 40 is generally the portion extending beyond the other electrode 40, and its function is to allow metal ions in the battery 2 to intercalate into the other electrode 40.

[0082] In the above scheme, by making the thickness change rate of the active material layer corresponding to the first sub-region 4111 greater than the thickness change rate of the active material layer corresponding to the second sub-region 4112, it can be ensured that metal ions can be embedded into the other electrode, thereby ensuring the normal function of the battery 2.

[0083] In some embodiments, the thickness variation trend of the expansion member 42 is opposite to the thickness variation trend of the active material layer corresponding to the second sub-region 4112.

[0084] Along the first direction X, the thickness of the active material layer corresponding to the first region 411 gradually increases. That is, the active material layer corresponding to the region of the first region 411 closer to the tab 413 is thinner, and the active material layer corresponding to the region farther away from the tab 413 is thicker. In order to suppress the lithium plating problem of the electrode 40 and improve the cycle performance of the battery 2, an expansion member 42 is provided on a portion of the first region 411. The first region 411 with the expansion member 42 has a slightly increased thickness compared to the first region 411 without the expansion member 42, which reduces the polarization loss of metal ion transfer and thus suppresses the accumulation of metal ions.

[0085] In the above scheme, by making the thickness variation trend of the expansion member 42 opposite to the thickness variation trend of the active material layer corresponding to the second region 412, that is, along the first direction X, the thickness of the expansion member 42 becomes thinner and thinner, while the thickness of the active material layer corresponding to the second sub-region 4112 becomes thicker and thicker. This keeps the thickness of the first region 411, where the expansion member 42 is provided, relatively stable overall, thereby suppressing the accumulation of metal ions on the first region 411 during long-term cycling and improving the cycle performance of the battery 2.

[0086] Figure 6 This is a schematic diagram of the structure of an electrode sheet according to another embodiment of this application. Figure 6 As shown, the sum of the thickness of the expanded member 42 after expansion and the thickness of the active material layer corresponding to the expanded member 42 is equal to the thickness of the active material layer corresponding to the second region 412.

[0087] Because the thickness of the active material layer coated on the first region 411 and the second region 412 in the same electrode 40 is different, the polarization loss of metal ion transfer is increased. This causes metal ions to accumulate in the thinner first region 411 during long-term cycling of the battery 2, resulting in lithium plating. An expansion member 42 is provided on the first region 411. After the expansion member 42 is wetted by the electrolyte, the difference in overall thickness between the first region 411 and the corresponding active material layer thickness in the second region 412 is reduced, effectively mitigating the lithium plating problem.

[0088] In the above solution, by setting an expansion member 42 in a portion of the first region 411, the sum of the thickness of the expansion member 42 after it expands in the electrolyte and the thickness of the active material layer corresponding to the expansion member 42 is equal to the thickness of the active material layer corresponding to the second region 412. In other words, the first region 411 and the second region 412 coated with the active material layer maintain the same thickness during battery operation. This can effectively suppress the accumulation of metal ions at the edge of the electrode 40 and solve the lithium plating problem of the electrode 40.

[0089] In some embodiments, the liquid absorption rate of the material of the expansion member 42 is 20%-100%.

[0090] In this embodiment of the application, unless otherwise specified, the thickness of the expansion member 42 is the same as the thickness before expansion.

[0091] The absorption rate here is the mass of absorbed organic solvent / the mass of the material itself, that is, the mass of organic solvent absorbed by the expansion member 42 / the mass of the expansion member 42. In the embodiments of this application, the organic solvent can be an organic solvent such as carbonate, or other commonly used electrolyte organic solvents; this application does not limit this.

[0092] In this embodiment, the specific thickness of the expander 42 needs to be calculated based on the specific application. For example, when using an expander 42 with a liquid absorption rate of 50%, the thickness of the active material layer corresponding to the first sub-region is 50 μm, and the thickness of the active material layer corresponding to the second region 412 is 100 μm, then the thickness of the expander 42 is 25 μm. The above is only a simple description of how the thickness of the expander 42 should be set. In practical applications, the thickness variation of the active material layer corresponding to the second sub-region 4112 or the first region 411 should be taken into account.

[0093] In the above scheme, in order to suppress lithium plating on the electrode 40 during long-cycle operation, an expansion member 42 is provided on the first region 411 adjacent to the second region 412. When the expansion member 42 is made of a material with a liquid absorption rate of 20%-100%, the expansion effect of the expansion member 42 is better.

[0094] In some embodiments, the swelling rate of the material of the expansion element is 10%-300%.

[0095] Swelling is the phenomenon of a polymer expanding in volume in a solvent. For example, ion exchange resins are hydrophilic polymers; when dry ion exchange resins are immersed in water, their volume often increases, a phenomenon known as swelling. In the embodiments of this application, the swelling rate of the expanding element 42 is the increase in volume due to swelling divided by the original volume of the expanding element 42.

[0096] In the above scheme, in order to suppress lithium plating on the electrode 40 during long-cycle operation, an expansion member 42 is provided on the first region 411 adjacent to the second region 412. The expansion member 42 is made of a material with a swelling ratio of 10%-300%, and the expansion effect of the expansion member 42 is good.

[0097] In some embodiments, the swelling rate of the material of the expander 42 is 50%-200%.

[0098] When the swelling ratio of the expansion component 42 is too large or too small, the thickness of the expansion component 42 may be too high or too low after expansion, and the expansion component 42 may not be able to play a role in inhibiting lithium plating.

[0099] In the above scheme, when the expansion component 42 is prepared using a material with a swelling rate of 50%-200%, the expansion component 42 has relatively stable expansion performance.

[0100] In some embodiments, the main material of the expansion member 42 is at least one of the following: oriented polystyrene, thermoplastic polyurethane, ethylene-vinyl acetate copolymer, silicone film, and styrene resin.

[0101] In the embodiments of this application, the above examples are merely illustrative. The expansion member 42 can also be prepared from other materials with liquid absorption rate or swelling rate within the range. This application does not impose any limitations on the material of the expansion member 42.

[0102] Oriented polystyrene is a new type of skin packaging material that meets environmental protection requirements. It has high strength, high rigidity, stable shape, and high shrinkage and liquid absorption rates.

[0103] Thermoplastic polyurethane, ethylene-vinyl acetate copolymer, silicone film, and styrene resin are all commonly used polymers and are widely applied in various industries.

[0104] In the above scheme, oriented polystyrene, thermoplastic polyurethane, ethylene-vinyl acetate copolymer, silicone film, and styrene resin are all commonly used materials, easy to obtain, have good water-swelling effect, and are environmentally friendly. Using at least one of these materials as raw materials to prepare the expandable part 42 ensures good expansion performance while reducing manufacturing costs, which is beneficial for its widespread application in production.

[0105] In some embodiments, the size of the expansion member 42 is 10-15 mm.

[0106] In the above scheme, the size of the expansion component 42 is maintained at 10-15mm, which can ensure the normal function of the expansion component 42 and also avoid occupying too much area of ​​the current collector 41, thereby ensuring the energy density of the battery 2.

[0107] In some embodiments, the size of the second sub-region 4112 in the first direction X is 10-15 mm.

[0108] In the above scheme, the first region 411 includes a first sub-region 4111 and a second sub-region 4112. The expansion member 42 can be disposed on the entire first region 411 or only on the second sub-region 4112. In the first direction X, the size of the second sub-region 4112 is set to 10-15mm to leave sufficient space for the installation of the expansion member 42.

[0109] In some embodiments, the thickness difference between the active material layer corresponding to the first region 411 and the active material layer corresponding to the second region 412 is 1-20 μm.

[0110] In the first direction X, the first region 411 is closer to the tab 413 than the second region 412, making the thickness of the active material layer corresponding to the first region 411 smaller than that of the active material layer corresponding to the second region 412. This can prevent the electrode 40 from cracking or the active material layer from falling off during the manufacturing process. However, simply reducing the active material layer corresponding to the first region 411 will also affect the energy density of the battery 2.

[0111] In the above scheme, by maintaining the thickness difference between the active material layer corresponding to the first region 411 and the active material layer corresponding to the second region 412 at 1-20μm, it is possible to prevent the active material layer on the electrode 40 from falling off and to ensure the energy density of the battery 2.

[0112] In some embodiments, the thickness of the expansion member 42 is 1-20 μm.

[0113] After the expansion element 42 is immersed in the electrolyte, the sum of its expanded thickness and the thickness of its corresponding active material layer is equal to the thickness of the active material layer corresponding to the second region 412. If the expanded thickness of the expansion element 42 is too high, it will still have an adverse effect on the performance of the battery 2.

[0114] In the above scheme, by maintaining the thickness difference between the active material layer corresponding to the first region 411 and the active material layer corresponding to the second region 412 at 1-20μm, it is possible to prevent the active material layer on the electrode 40 from falling off and to ensure the energy density of the battery 2.

[0115] In some embodiments, the thickness of the active material layer corresponding to the first sub-region 4111 is 0-50 μm.

[0116] Because the positions of the other electrode 40 in the battery 2 corresponding to the first sub-region 4111 and the second sub-region 4112 are different, the expansion member 42 does not need to be provided on the first sub-region 4111. In addition, compared with the second sub-region 4112, the thickness change rate of the active material layer corresponding to the first sub-region 4111 is greater than the thickness difference of the active material corresponding to the second sub-region 4112. That is, the active material layer thickness of the first region 411 is thinner than that of the second region 412, and the active material layer thickness corresponding to the first sub-region 4111 in the first region 411 is even thinner.

[0117] In the above scheme, by maintaining the thickness of the active material layer corresponding to the first sub-region 4111 at 0-50μm, a large difference in active material layer thickness is formed with the second region 412. This can ensure to the greatest extent that the active material layer of the electrode 40 will not fall off during the preparation process.

[0118] In some embodiments, the thickness of the active material layer corresponding to the second sub-region 4112 is 20-80 μm.

[0119] On the one hand, the active material layer corresponding to the second sub-region 4112 still has a thickness difference with the second region 412, which can continue to prevent the edge of the electrode 40 from bursting; on the other hand, an expansion member 42 can be provided on the second sub-region 4112 to suppress lithium plating of the electrode 40 and improve the cycle performance of the battery 2.

[0120] This application also provides an electrode assembly 31. The electrode assembly 31 includes the electrode 40 in any of the above embodiments.

[0121] This application also provides a battery cell 3. The battery cell 3 includes an electrode assembly 31; a housing 321 having an opening for accommodating the electrode assembly 31; and an end cap 361 of the foregoing embodiments, the end cap 361 closing the opening.

[0122] This application also provides a battery 2, which includes the battery cell 3 in the foregoing embodiments.

[0123] This application also provides an electrical device, including the battery 2 of the aforementioned embodiment, which is used to provide electrical energy.

[0124] Although this application has been described with reference to preferred embodiments, various modifications can be made thereto and components can be replaced with equivalents without departing from the scope of this application. In particular, the technical features mentioned in the various embodiments can be combined in any manner, provided there is no structural conflict. This application is not limited to the specific embodiments disclosed herein, but includes all technical solutions falling within the scope of the claims.

Claims

1. An electrode sheet, characterized in that, include: A current collector, comprising a tab, a first region, and a second region arranged sequentially along a first direction; An expansion member is disposed in at least a portion of the first region adjacent to the second region, and the expansion member is configured to expand along the thickness direction of the electrode after being wetted with electrolyte; The first region and the second region are coated with an active material layer, wherein the thickness of the active material layer corresponding to the first region is less than the thickness of the active material layer corresponding to the second region; Along the thickness direction of the electrode sheet, the expansion member is disposed between the active material layer and the first region; The sum of the thickness of the expanded member after expansion and the thickness of the active material layer disposed at the location of the expanded member is equal to the thickness of the active material layer corresponding to the second region.

2. The electrode sheet according to claim 1, characterized in that, The first region includes a first sub-region and a second sub-region, the second sub-region being adjacent to the second region, and the expansion member being disposed in the second sub-region.

3. The electrode sheet according to claim 2, characterized in that, Along the first direction, the thickness of the active material layer corresponding to the first region gradually increases.

4. The electrode sheet according to claim 3, characterized in that, Along the first direction, the thickness change rate of the active material layer corresponding to the first sub-region is greater than the thickness change rate of the active material layer corresponding to the second sub-region.

5. The electrode sheet according to claim 3, characterized in that, Along the first direction, the thickness variation trend of the expansion member is opposite to the thickness variation trend of the active material layer corresponding to the second sub-region.

6. The electrode sheet according to any one of claims 1 to 5, characterized in that, The liquid absorption rate of the material of the expansion component is 20%-100%.

7. The electrode sheet according to any one of claims 1 to 5, characterized in that, The swelling rate of the material of the expansion component is 10%-300%.

8. The electrode sheet according to claim 7, characterized in that, The swelling rate of the material of the expansion component is 50%-200%.

9. The electrode sheet according to claim 6, characterized in that, The main material of the expansion component is at least one of the following: oriented polystyrene, thermoplastic polyurethane, ethylene-vinyl acetate copolymer, silicone film, and styrene resin.

10. The electrode sheet according to any one of claims 1 to 5, characterized in that, In the first direction, the size of the expansion member is 10-15 mm.

11. The electrode sheet according to any one of claims 2 to 5, characterized in that, In the first direction, the size of the second sub-region is 10-15 mm.

12. The electrode sheet according to any one of claims 2 to 5, characterized in that, In the first direction, the size of the first sub-region is 0.5-1.5 mm.

13. The electrode sheet according to any one of claims 1 to 5, characterized in that, The thickness difference between the active material layer corresponding to the first region and the active material layer corresponding to the second region is 1-20 μm.

14. The electrode sheet according to any one of claims 1 to 5, characterized in that, The thickness of the expansion element is 1-20 μm.

15. The electrode sheet according to any one of claims 2 to 5, characterized in that, The thickness of the active material layer corresponding to the first sub-region is 0-50 μm.

16. The electrode sheet according to any one of claims 2 to 5, characterized in that, The thickness of the active material layer corresponding to the second sub-region is 20-80 μm.

17. An electrode assembly, characterized in that, include: The electrode as described in any one of claims 1 to 16.

18. A single battery cell, characterized in that, include: The electrode assembly as described in claim 17; The housing has an opening for accommodating the electrode assembly; as well as End cap, used to close the opening.

19. A battery, characterized in that, include Multiple battery cells as described in claim 18.

20. An electrical appliance, characterized in that, include: The battery of claim 19 is used to provide electrical energy.

Citation Information

Patent Citations

  • Electrode plate and electrochemical device comprising same

    CN109841794A

  • Positive plate, lithium ion battery and preparation method of positive plate

    CN113140697A

  • Battery and electronic equipment

    CN114447408A