A method for separating and purifying fucoidan

By forming calcium alginate gels during the separation and purification of fucoidan and using crosslinked graphene oxide/ferrous tetraoxide to chelate calcium ions to adsorb proteins, combined with magnetic separation technology, the existing technology is solved The problem of waste of resources and low separation efficiency in the process has achieved efficient and low-cost separation and purification of fucoidan and alginic acid.

CN118440222BActive Publication Date: 2024-11-05SYNGARS TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410907832.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-08
Publication Date
2024-11-05
Estimated Expiration
2044-07-08

AI Technical Summary

Technical Problem

The prior art is difficult to effectively isolate alginic acid during the separation and purification of fucoidan, resulting in waste of resources and difficult to separate proteins from polysaccharides, affecting purification efficiency and purity.

Method used

By forming a calcium alginate gel during the leaching process, and using crosslinked graphene oxide/ferrous tetraoxide chitosan chelates calcium ions, adsorbing proteins, preventing them from contacting graphene oxide directly, and combining with magnetic separation Technology to achieve synchronous separation of fucoidan and alginic acid.

Benefits of technology

The separation efficiency and purification purity of fucoidans are improved, the cost is reduced, the use of acids, bases and organic solvents is reduced, and the integrity of polysaccharides and the efficient utilization of resources is achieved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
  • Figure SMS_3
    Figure SMS_3
Patent Text Reader

Abstract

The invention discloses a method for separating and purifying fucoidan, comprising the following steps: S1, placing kelp powder in hot water for leaching; filtering, and concentrating by rotary evaporation; S2, adding calcium chloride aqueous solution to the concentrated solution obtained by S1 in batches, with an excess of calcium chloride solution; S3, adding graphene oxide / ferroferric oxide cross-linked with chitosan; leaving at room temperature, and adsorbing protein on the graphene oxide / ferroferric oxide cross-linked with chitosan; and the protein adsorption is complete; S4, filtering solids, and the obtained liquid is a fucoidan aqueous solution; S5, adding ethanol to the concentrated solution obtained by S4, precipitating fucoidan, filtering, and drying to obtain purified fucoidan; the invention utilizes excess calcium ions to effectively form chelates through chitosan cross-linked with graphene oxide / ferroferric oxide, and utilizes graphene oxide to actively adsorb proteins while preventing proteins from directly contacting and contaminating graphene oxide, thereby effectively improving the separation efficiency and purification purity of fucoidan.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of separation and purification of fucoidan, and in particular to a method for separation and purification of fucoidan. Background Art

[0002] Fucoidan is a type of sulfated water-soluble intercellular polysaccharide with L-fucose as its characteristic monosaccharide, i.e., a polymer of α-L-fucose-4-sulfate, with a small amount of monosaccharide macromolecules in the structure. The prior art uses hydrochloric acid to extract fucoidan from seaweed, which is a common method. The extraction is carried out at room temperature with a pH value of 2 for 7 hours. After a series of steps such as neutralization, precipitation, dialysis, concentration and freeze-drying, the extract is obtained.

[0003] There are three commonly used separation and purification methods for fucoidan, namely water extraction and alcohol precipitation, water extraction and acid precipitation, and water extraction and acid precipitation enzymatic hydrolysis. Seaweed polysaccharides usually include fucoidan and alginate, both of which are soluble in water. In the prior art, fucoidan or alginate is usually extracted separately, for example, acid extraction and then alcohol extraction are performed to obtain only fucoidan, and alginate is difficult to separate from protein, resulting in a waste of resources as the polysaccharides other than the target are difficult to extract.

[0004] CN116813809A discloses a method for separating and purifying fucoidan and an electric field-membrane separation device. In order to separate protein and fucoidan, a dialysis membrane with a pore size of 18nm to 32nm is used. The voltage is applied for 3 to 6 hours, and only fucoidan can be separated and purified, which easily leads to a waste of alginate resources. Summary of the invention

[0005] The object of the present invention is to provide a method for separating and purifying fucoidan. In the present invention, calcium chloride is added in batches to form calcium alginate gel during the extraction process, and excess calcium ions are effectively used to form chelate by cross-linking chitosan with graphene oxide / ferrous oxide, while graphene oxide is used to actively adsorb proteins while preventing proteins from directly contacting and contaminating graphene oxide, thereby effectively improving the separation efficiency and purification purity of fucoidan.

[0006] In order to solve this technical problem, the technical solution of the present invention is: a method for separating and purifying fucoidan, comprising the following steps:

[0007] S1. extracting the kelp powder in hot water at a solid-liquid ratio of 1 g:20 mL; filtering, and concentrating the filtrate by rotary evaporation to a volume of 40% to 50% of the initial volume;

[0008] S2, adding a 2% by mass calcium chloride aqueous solution to the concentrated solution obtained in S1 in batches until the calcium alginate gel in the concentrated solution contains free calcium ions, that is, the calcium chloride solution is excessive;

[0009] S3, adding graphene oxide / ferroferric oxide cross-linked with chitosan to the material system after S2; leaving at room temperature, the protein is adsorbed on the chitosan cross-linked on the surface of graphene oxide / ferroferric oxide and chelated with the excess calcium ions in step S2;

[0010] S4, filtering the solid, and the obtained liquid is a fucoidan aqueous solution; concentrating to 40% to 50% of the volume of the filtered solution;

[0011] S5. Add ethanol to the concentrated solution obtained in S4 to precipitate fucoidan, filter, and dry to obtain purified fucoidan.

[0012] Preferably, the solid obtained in step S4 is dispersed with deionized water, and the graphene oxide / ferroferric oxide cross-linked with chitosan adsorbed with protein and calcium ions in step S3 is separated from the calcium alginate gel formed in step S2 by magnetic attraction. In the present invention, the graphene oxide / ferroferric oxide cross-linked with chitosan is separated from the calcium alginate gel by magnetic force, and the separation efficiency is high.

[0013] Preferably, the calcium alginate gel is placed in a lactic acid solution to form alginic acid and precipitate to obtain alginic acid. The present invention separates alginate after separating and purifying fucoidan, and the separation is achieved through phase changes, so the separation effect is good.

[0014] The method for preparing graphene oxide / ferrosoferric oxide cross-linked with chitosan preferably comprises the following steps:

[0015] S31, dissolving chitosan in acetic acid solution, adding NaOH solution to adjust the pH value to 5.5 to 6.0, stirring, and obtaining a chitosan solution;

[0016] S32, dispersing graphene oxide / ferroferric oxide in a chitosan solution, performing ultrasonic dispersion, and allowing chitosan to self-assemble on the graphene oxide / ferroferric oxide;

[0017] The mass ratio of graphene oxide / ferroferric oxide composite material to chitosan is 1:(10-20);

[0018] S33, adding glutaraldehyde for cross-linking reaction;

[0019] S34, filtering and washing the obtained precipitate, freeze-drying it, and crushing it to obtain graphene oxide / ferroferric oxide particles cross-linked with chitosan.

[0020] The cross-linking reaction process conditions in step S33 are preferably:

[0021] The reaction was carried out at 40°C to 60°C for 60min to 120min; the mass ratio of glutaraldehyde to chitosan was 0.15:1.

[0022] The method for preparing graphene oxide / ferrosoferric oxide preferably comprises the following steps:

[0023] S321, FeCl 3 6H 2 O and FeCl 2 ·4H 2 O was dissolved in deionized water at a molar ratio of 2:1 and stirred until fully dissolved;

[0024] S322, FeCl 3 6H 2 O and FeCl 2 ·4H 2 O aqueous solution is added to the graphene oxide solution which is stirred at a uniform speed, and stirred until the solution is mixed evenly;

[0025] S323, adding ammonia water dropwise to the mixed solution obtained in S32 with stirring until the pH value of the liquid is adjusted to 8 to 9; crystallizing to obtain graphene oxide / ferrosoferric oxide;

[0026] S324, filtering and separating the graphene oxide / ferroferric oxide, washing, and vacuum drying to obtain a graphene oxide / ferroferric oxide magnetic nanocomposite material;

[0027] Graphene oxide and FeCl 3 6H 2 The mass ratio of O is (6 to 8):1.

[0028] Preferably, during the crystallization process of adding ammonia dropwise, the material system is heated at a temperature of 60°C to 80°C.

[0029] The process parameters of hot water extraction in step S1 are preferably as follows:

[0030] The hot water temperature is 90° C. to 95° C., the extraction time is 3 to 4 hours, and the extraction is performed under ultrasonic conditions.

[0031] The present invention uses a neutral environment for hot extraction, reduces the use of acid and alkali, facilitates separation and purification, and is beneficial to maintaining the integrity of polysaccharide molecules.

[0032] The process conditions for adding calcium chloride solution gel in each batch in step S2 are preferably as follows:

[0033] The gel time is 10 min to 20 min; the gel temperature is 25°C to 50°C.

[0034] Preferably, in step S3, the amount of graphene oxide / ferrosoferric oxide cross-linked with chitosan added relative to the volume of the material solution is 4.0 mg / mL to 6.0 mg / mL.

[0035] By adopting the above technical solution, the beneficial effects of the present invention are:

[0036] The present invention obtains fucoidan, alginic acid and protein by hot water extraction and disperses them in an aqueous solution. After concentration, a 2% by mass calcium chloride aqueous solution is added to the concentrated solution in batches, and the calcium alginate in the concentrated solution is gelled until the obtained concentrated solution has free calcium ions, that is, the calcium chloride solution is excessive; by controlling the excess of sodium chloride, it is ensured that the carboxyl groups of the alginate in the extracted raw sugar form stable ionic bonds with the calcium ions, resulting in cross-linking between molecular chains to form a gel with a three-dimensional network structure; the excess calcium chloride ensures that all the alginate is gelled;

[0037] Subsequently, graphene oxide / ferroferric oxide cross-linked with chitosan is added, and the amino group of chitosan chelates calcium ions under neutral conditions; the chelated calcium ions promote chitosan to form an isolation layer around the graphene oxide, while utilizing the adsorption effect of graphene oxide on proteins, while avoiding the direct attachment of proteins to the surface of graphene oxide, so that the graphene oxide / ferroferric oxide cross-linked with chitosan is convenient for desorption of proteins and calcium ions after magnetic separation, thereby realizing the repeated use of graphene oxide / ferroferric oxide cross-linked with chitosan;

[0038] The present invention separates alginic acid and protein in the raw material from the liquid phase through calcium alginate gel and graphene oxide / ferroferric oxide cross-linked with chitosan, thereby realizing the separation and purification of fucoidan, and then separates the protein from the calcium alginate gel through magnetic attraction. The present invention separates and purifies fucoidan and simultaneously separates and purifies calcium alginate, and the graphene oxide / ferroferric oxide cross-linked with chitosan for protein adsorption can be reused, which reduces the cost in the separation and purification of fucoidan and effectively prevents protein from being directly adsorbed on the surface of graphene oxide, thereby preventing graphene oxide from being contaminated by protein and being difficult to reuse; the chitosan cross-linked with graphene oxide / ferroferric oxide is separated by ammonia. The base and hydroxyl groups form stable coordination bonds with calcium ions and chelate quickly; in the same liquid phase environment, the adsorption of proteins involves more complex interactions, such as hydrogen bonds, van der Waals forces and hydrophobic interactions, and these interactions may take more time to establish. Therefore, the adsorption rate of proteins is slower than the chelation rate of calcium ions. The present invention uses excess calcium ions to ensure the surrounding and protection of the graphene oxide surface in the protein adsorbent, while still maintaining the adsorption trend of graphene oxide on proteins. Therefore, the present invention effectively enriches alginate and protein in fucoidan, and can subsequently achieve stable separation, effectively realizing the separation and purification of polysaccharides and ensuring a high purity;

[0039] The present invention uses a water extraction method, which can reduce the hydrolysis of polysaccharides through a neutral leaching environment to obtain complete polysaccharide molecules. The obtained fucoidan and alginate are quickly and effectively separated and the use of acid, alkali and organic solvents is effectively reduced, thereby reducing production costs and improving production efficiency. DETAILED DESCRIPTION

[0040] In order to further explain the technical solution of the present invention, the present invention is described in detail below through specific embodiments.

[0041] Example 1

[0042] This embodiment discloses a method for separating and purifying fucoidan, comprising the following steps:

[0043] S1. Extract the kelp powder in hot water at a solid-liquid ratio of 1 g:20 mL; filter, and concentrate the filtrate by rotary evaporation to a volume of 40% of the initial volume;

[0044] The process parameters of hot water extraction in step S1 are as follows:

[0045] The hot water temperature was 90°C, the extraction time was 3 hours, and ultrasound was performed in the initial 0.5 h with an ultrasound frequency of 100 kHz.

[0046] S2, adding 2% by mass calcium chloride aqueous solution to the concentrated solution obtained in S1 in three batches until the concentrated solution has free calcium ions, that is, the calcium chloride solution is excessive; the volume of the calcium chloride aqueous solution is equal to that of the concentrated solution;

[0047] The process conditions for adding calcium chloride solution gel in each batch in step S2 are as follows:

[0048] The gel time was 10 min and the gel temperature was 35 °C.

[0049] Filter after each gelation until no more gel is produced in the raw material to confirm that there are free calcium ions in the concentrate;

[0050] S3, adding graphene oxide / ferroferric oxide cross-linked with chitosan to the material system after S2; leaving at room temperature for 2 hours, the graphene oxide / ferroferric oxide cross-linked with chitosan chelates the excess calcium ions in step S2 and adsorbs proteins;

[0051] In step S3, the amount of graphene oxide / ferroferric oxide cross-linked with chitosan added relative to the volume of the material solution is 4.0 mg / mL.

[0052] S4, filtering the solid, and the obtained liquid is a fucoidan aqueous solution; concentrating to 50% of the volume of the filtered solution;

[0053] The solid obtained in S4 is dispersed with deionized water, and the graphene oxide / ferroferric oxide cross-linked with chitosan adsorbed with protein and calcium ions in step S3 is separated from the calcium alginate gel formed in step S2 by magnetic attraction. The present invention effectively separates the solid graphene oxide / ferroferric oxide cross-linked with chitosan as a protein adsorbent from the calcium alginate gel by magnetic attraction, with high separation efficiency and good separation effect.

[0054] S5. Add ethanol to the concentrated solution obtained in S4 to precipitate fucoidan, filter, and dry to obtain purified fucoidan.

[0055] In this embodiment, calcium alginate gel is placed in a lactic acid solution with a pH value of 1.8 to form alginic acid and precipitate to obtain alginic acid. The present invention separates alginic acid after separating and purifying fucoidan, and the separation is achieved through phase change, so the separation effect is good.

[0056] The preparation method of graphene oxide / ferroferric oxide cross-linked with chitosan in this embodiment comprises the following steps:

[0057] S31, dissolving chitosan in acetic acid solution, adding NaOH solution to adjust the pH value to 5.5, stirring, and obtaining a chitosan solution;

[0058] S32, dispersing graphene oxide / ferroferric oxide in a chitosan solution, performing ultrasonic dispersion, and allowing chitosan to self-assemble on the graphene oxide / ferroferric oxide;

[0059] The mass ratio of graphene oxide / ferroferric oxide composite material to chitosan is 1:10;

[0060] S33, adding glutaraldehyde for cross-linking reaction;

[0061] The cross-linking reaction process conditions in step S33 are:

[0062] The reaction was carried out at 40°C for 60 min. The mass ratio of glutaraldehyde to chitosan was 0.15:1.

[0063] S34, filtering and washing the obtained precipitate, freeze-drying it, and crushing it to obtain graphene oxide / ferroferric oxide particles cross-linked with chitosan.

[0064] The preparation method of graphene oxide / ferroferric oxide in this embodiment comprises the following steps:

[0065] S321, FeCl 3 6H 2 O and FeCl 2 ·4H 2 O was dissolved in deionized water at a molar ratio of 2:1 and stirred until fully dissolved;

[0066] S322, FeCl 3 6H 2 O and FeCl 2 ·4H 2 O aqueous solution is added to the graphene oxide solution which is stirred at a uniform speed, and stirred until the solution is mixed evenly;

[0067] S323, adding ammonia water dropwise to the mixed solution obtained in S32 with stirring until the pH value of the liquid is adjusted to 8.0; crystallizing to obtain graphene oxide / ferrosoferric oxide;

[0068] During the crystallization process of adding ammonia, the material system was heated at 60°C.

[0069] S324, filtering and separating the graphene oxide / ferroferric oxide, washing, and vacuum drying to obtain a graphene oxide / ferroferric oxide magnetic nanocomposite material;

[0070] Graphene oxide and FeCl 3 6H 2 The mass ratio of O is 6:1.

[0071] The present invention uses a neutral environment for hot extraction, reduces the use of acid and alkali, facilitates separation and purification, and is beneficial to maintaining the integrity of polysaccharide molecules.

[0072] Example 2

[0073] The main differences between this embodiment and embodiment 1 are shown in Table 1 and Table 2.

[0074] Example 3

[0075] The main differences between this embodiment and embodiment 1 are shown in Table 1 and Table 2.

[0076] Example 4

[0077] The main differences between this embodiment and embodiment 1 are shown in Table 1 and Table 2.

[0078] Example 5

[0079] The main differences between this embodiment and embodiment 1 are shown in Table 1 and Table 2.

[0080] Comparative Example 1

[0081] This comparative example discloses a method for separating and purifying fucoidan, comprising the following steps:

[0082] S1. Preparation of crude fucoidan

[0083] Crush the seaweed, add 8 times the volume of water to the seaweed, microwave at 60°C for 60 min, and filter to obtain a solution; continue to add 5 times the volume of water to the residue, stir for 15 min, repeat 3 times, and collect the filtrate;

[0084] Add activated carbon to the filtrate, stir for 60 minutes, filter, and obtain the filtrate; the amount of activated carbon used is 0.2% of the mass of the seaweed;

[0085] Concentrate, distill the filtrate under reduced pressure to remove water, and obtain a concentrate with a volume of 1 / 5 of the filtrate;

[0086] Add 8 times the volume of ethanol to the concentrate, stir at 5°C for 60 min, and filter to obtain crude fucoidan.

[0087] S2. Separation and purification

[0088] The crude fucoidan was dissolved in water with 10 times the mass of the crude fucoidan, centrifuged, and the supernatant was graded and purified by anion exchange column, eluted with deionized water, 0.05M, 0.1M, 0.2M, 0.3M, 0.5M, 0.6M and 0.8M NaCl solutions in sequence, and the eluate of 0.5M NaCl solution was collected and combined according to the elution curve, concentrated, centrifuged, and the supernatant was dialyzed and freeze-dried to obtain separated and purified fucoidan.

[0089] Comparative Example 2

[0090] The main difference between this comparative example and Example 4 is:

[0091] In step S2, a 2% by mass calcium chloride aqueous solution is added to the concentrated solution obtained in S1 in batches, and the calcium alginate gel in the concentrated solution is separated after it is completely formed; the calcium ion concentration in the extract is determined by titration, and then sodium carbonate is added to precipitate the calcium ions; after confirming that the calcium ions are not free in the extract, a protein adsorbent, namely graphene oxide / ferroferric oxide cross-linked with chitosan, is added.

[0092] Comparative Example 3

[0093] The main difference between this comparative example and Example 4 is:

[0094] In this comparative example, the same amount of graphene oxide / ferrosoferric oxide as that in Example 4 was added as a protein adsorbent.

[0095] Table 1 Process parameters for separation and purification of fucoidan in Examples 1 to 5

[0096]

[0097] Table 2 GO / Fe cross-linked with chitosan prepared in Examples 1 to 5 3 O 4 Process parameters

[0098]

[0099] The purity, yield, protein and calcium ion content of the fucoidan and alginate separated and purified in Examples 1 to 5 and Comparative Examples 1 to 3 are shown in Tables 3 and 4 for specific data.

[0100] Table 3 Performance indicators of fucoidan obtained in Examples 1 to 5 and Comparative Examples 1 to 3

[0101]

[0102] Table 4 Performance indicators of alginic acid obtained in Examples 1 to 5 and Comparative Examples 1 to 3

[0103]

[0104] In the present invention, after separating the graphene oxide / ferroferric oxide cross-linked with chitosan adsorbed with protein from the calcium alginate gel by magnetic attraction, a sodium hydroxide solution with a mass fraction of 10% is added, and the mixture is heated to 80° C. and reacted for 60 minutes to remove the protein adsorbed on the chitosan by static electricity, ester bonds, hydrophobic interactions, etc. After the protein is desorbed, the adsorbent is separated, washed to neutrality, dried, and reused. Examples 1 to 5 and Comparative Examples 2 and 3 are repeated, and the protein content in the obtained fucoidan and alginate is as shown in Table 5.

[0105] Table 5 Effect of repeated use of protein adsorbent on protein content (%) in the product

[0106]

[0107] It can be seen from Tables 3 to 5 that the present invention obtains fucoidan, alginic acid and protein dispersed in an aqueous solution by hot water extraction, and after concentration, a 2% by mass calcium chloride aqueous solution is added to the concentrated solution in batches, and the calcium alginate in the concentrated solution is gelled until the obtained concentrated solution has free calcium ions, that is, the calcium chloride solution is excessive; by controlling the excess of calcium chloride, it is ensured that the carboxyl groups of the alginate in the extracted crude sugar form stable ionic bonds with the calcium ions, resulting in cross-linking between the molecular chains to form a gel with a three-dimensional network structure; the excess calcium chloride ensures that all the alginate is gelled; as in Examples 1 to 5, Subsequently, graphene oxide / ferroferric oxide cross-linked with chitosan is added, and the amino groups and hydroxyl groups of chitosan chelate calcium ions under neutral conditions; the chelated calcium ions cooperate with chitosan to form an isolation layer around the graphene oxide, and while utilizing the adsorption effect of graphene oxide on proteins, the proteins are prevented from directly adhering to the surface of the graphene oxide, so that the graphene oxide / ferroferric oxide cross-linked with chitosan is conveniently separated by magnetic attraction and then desorbed, thereby realizing the repeated use of the graphene oxide / ferroferric oxide cross-linked with chitosan; the present invention uses calcium alginate gel and Graphene oxide / ferroferric oxide separates alginate and protein in the raw material from the liquid phase to achieve separation and purification of fucoidan, and then separates the protein from the calcium alginate gel by magnetic attraction. The present invention separates and purifies fucoidan and calcium alginate simultaneously, and the graphene oxide / ferroferric oxide cross-linked with chitosan for protein adsorption can be reused. Compared with Examples 1 to 5 and Comparative Examples 2 and 3, in Comparative Example 2, since there is no excess calcium ion in the concentrated solution, the graphene oxide / ferroferric oxide cross-linked with chitosan as a protein adsorbent is Polysaccharides fail to chelate calcium ions on the surface of graphene oxide, and graphene oxide is easily directly adsorbed by proteins and difficult to desorb, resulting in incomplete protein adsorption after repeated use. In Comparative Example 3, since graphene oxide / ferroferric oxide is directly adsorbed by proteins during the first use, graphene oxide strongly adsorbs proteins, and the desorption effect of alkali solution is limited, the protein content of fucoidan obtained by secondary use increases. The present invention reduces costs in the separation and purification of fucoidan and effectively prevents proteins from being directly adsorbed on the surface of graphene oxide, thereby avoiding graphene oxide from being contaminated by proteins and being difficult to use again.

[0108] The present invention uses a water extraction method, which can reduce the hydrolysis of polysaccharides through a neutral leaching environment to obtain complete polysaccharide molecules. The obtained fucoidan and alginate are quickly and effectively separated and the use of acid and organic solvents is effectively reduced, thereby reducing production costs and improving production efficiency.

Claims

1. A method for separating and purifying fucoidan, Features: The following steps are involved: S1. extracting the kelp powder in hot water at a solid-liquid ratio of 1 g:20 mL; filtering, and concentrating the filtrate by rotary evaporation to a volume of 40% to 50% of the initial volume; S2, adding a 2% by mass calcium chloride aqueous solution to the concentrated solution obtained in S1 in batches, forming a calcium alginate gel in the concentrated solution until the concentrated solution has free calcium ions, that is, the calcium chloride solution is excessive; S3, adding graphene oxide / ferroferric oxide cross-linked with chitosan to the material system after S2; leaving at room temperature, the graphene oxide / ferroferric oxide cross-linked with chitosan chelates the excess calcium ions in step S2 and adsorbs proteins; In step S3, the amount of graphene oxide / ferroferric oxide cross-linked with chitosan added relative to the volume of the material solution is 4.0 mg / mL to 6.0 mg / mL; The preparation method of graphene oxide / ferroferric oxide cross-linked with chitosan comprises the following steps: S31, dissolving chitosan in acetic acid solution, adding NaOH solution to adjust the pH value to 5.5 to 6.0, stirring, and obtaining a chitosan solution; S32, dispersing graphene oxide / ferroferric oxide in a chitosan solution, performing ultrasonic dispersion, and allowing chitosan to self-assemble on the graphene oxide / ferroferric oxide; The mass ratio of graphene oxide / ferroferric oxide to chitosan is 1:(10-20); S33, adding glutaraldehyde for cross-linking reaction; S34, filtering and washing the obtained precipitate, freeze-drying it, and crushing it to obtain graphene oxide / ferroferric oxide particles cross-linked with chitosan; The preparation method of graphene oxide / ferroferric oxide comprises the following steps: S321, FeCl 3 6H 2 O and FeCl 2 ·4H 2 O was dissolved in deionized water at a molar ratio of 2:1 and stirred until fully dissolved; S322, FeCl 3 6H 2 O and FeCl 2 ·4H 2 O aqueous solution is added to the graphene oxide solution which is stirred at a uniform speed, and stirred until the solution is mixed evenly; S323, adding ammonia water dropwise to the mixed solution obtained in S322 with stirring until the pH value of the liquid is adjusted to 8 to 9; crystallizing to obtain graphene oxide / ferrosoferric oxide; S324, filtering and separating the graphene oxide / ferroferric oxide, washing, and vacuum drying to obtain a graphene oxide / ferroferric oxide magnetic nanocomposite material; S4, filtering the solid, and the resulting liquid is a fucoidan aqueous solution, which is concentrated to 40% to 50% of the volume of the filtered solution; S5. Add ethanol to the concentrated solution obtained in S4 to precipitate fucoidan, filter and dry to obtain purified fucoidan.

2. The separation and purification method according to claim 1, Features: The solid obtained in step S4 is dispersed with deionized water, and the graphene oxide / ferroferric oxide cross-linked with chitosan adsorbed with protein and calcium ions in step S3 is separated from the calcium alginate gel formed in step S2 by magnetic attraction.

3. The separation and purification method according to claim 2, Features: Calcium alginate gel is placed in a lactic acid solution to form alginic acid and precipitate to obtain alginic acid.

4. The separation and purification method according to claim 1, Features: The cross-linking reaction process conditions in step S33 are: The reaction was carried out at 40°C to 60°C for 60min to 120min; the mass ratio of glutaraldehyde to chitosan was 0.15:

1.

5. The separation and purification method according to claim 1, Features: Graphene oxide and FeCl 3 6H 2 The mass ratio of O is (6~8):

1.

6. The separation and purification method according to claim 1, Features: During the crystallization process of adding ammonia, the material system is heated at a temperature of 60°C to 80°C.

7. The separation and purification method according to claim 1, Features: The process parameters of hot water extraction in step S1 are as follows: The hot water temperature is 90° C. to 95° C., the extraction time is 3 to 4 hours, and the extraction is performed under ultrasonic conditions.

8. The separation and purification method according to claim 1, Features: The process conditions for adding calcium chloride solution gel in each batch in step S2 are as follows: The gel time is 10 min to 20 min; the gel temperature is 25°C to 50°C.