Industrial fermentation defoaming agent and preparation method thereof
By using terpene olefins and gradient cloud point polyether composites in fermentation defoamers, the problem of defoamers' performance deterioration after high temperature sterilization is solved, and rapid and effective foam control and fermentation efficiency are achieved.
Patent Information
- Application Number
- CN202411288396.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-14
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2044-09-14
AI Technical Summary
Existing fermentation defoamers are prone to demulsification after high temperature sterilization, resulting in a degradation of performance and difficulty in effectively controlling the foam generated during fermentation, affecting the fermentation efficiency and yield.
Using industrial fermentation defoaming agents containing terpene olefins and gradient cloud point polyether composites, a stable emulsion is formed by mixing silicone actives, polyether modified organosiloxanes, emulsifiers and thickeners to ensure that The stability and defoaming properties of defoaming agent under high temperature conditions.
The defoaming agent does not demulsify after high temperature sterilization, and quickly and effectively controls foam during fermentation, improves fermentation efficiency and yield, reduces labor costs and subsequent separation and removal processes.
Smart Images

Figure SMS_1 
Figure SMS_2
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of fermentation defoamers, and in particular to an industrial fermentation defoamer and a preparation method thereof. Background Art
[0002] Bio-fermentation is widely used in the pharmaceutical industry, food industry, energy industry, chemical industry, agriculture and other industries. However, when using bio-fermentation technology, foam problems often occur. These foams may be caused by operation, surrounding environment, stirring and other reasons. The generation of foam will cause a decrease in fermentation yield, overflow pollution of fermentation liquid, and a decrease in working volume. When the fermentation product is an anionic surfactant, the foam produced during the fermentation process is more stable.
[0003] Fermentation is divided into aerobic fermentation and anaerobic fermentation. Defoamers are used in both aerobic and anaerobic fermentation processes to eliminate foam. Aerobic fermentation produces a large amount of foam, which requires the defoamer to have a certain ability to break foam. In addition, in some processes of aerobic fermentation, some foam needs to remain. At this time, the defoamer needs to have the ability to control foam. The anaerobic fermentation process has high requirements for the defoamer to suppress foam, and the defoamer needs to suppress foam for a long time at a low addition amount. Whether it is aerobic or anaerobic fermentation, the defoamer will be disinfected and sterilized before using the defoamer. After the defoamer is disinfected and sterilized at high temperature, many emulsion-type defoamers will demulsify and their performance will decrease. In the fermentation production process, if a defoamer with demulsification is used, a large amount of sticky substances will be produced on the kettle wall, or sediment will be produced at the bottom of the kettle, and the performance will also decrease. Adding excessive thickening stabilizer to the defoamer will cause the emulsion viscosity to be too large and the dispersibility to be poor, which is not conducive to the rapid defoaming of the defoamer.
[0004] Chinese patent CN113750577B points out that polyether-modified silicone, polyether-modified heptamethyl trisiloxane, and solvents, and their compound performs well in rhamnolipid surfactants and has a good defoaming effect. However, they have almost no effect in real fermentation liquids and consume a huge amount of money. The ingredients in rhamnolipid fermentation liquid are complex, resulting in many factors that cause foam changes. Ethanol, isopropanol, and n-butanol cannot break bubbles in the system, and small molecule alcohols have a certain antibacterial effect, which affects the final yield.
[0005] Chinese patent CN113750577B states that only silicone paste, polyether, emulsifier, glycerol fatty acid ester and other materials are used to prepare defoamers, but it does not clearly state the stability of the defoamer under high temperature. The patent uses conventional emulsifiers to emulsify the defoamer, which has a certain risk of high temperature demulsification.
[0006] Therefore, there is a need for an industrial fermentation defoamer with good demulsification inhibition and defoaming performance. Summary of the invention
[0007] In view of this, the purpose of the present application is to provide an industrial fermentation defoamer and a preparation method thereof, which can inhibit the demulsification of the product during the sterilization process of the front end of industrial fermentation, and maintain the stable performance of the product before and after sterilization. The defoamer is compounded with different polyether turbidity point precipitates and matched with polyether modified organosiloxane to complement the emulsion emulsifier, thereby ensuring that the silicone active substance does not precipitate.
[0008] In order to achieve or at least partially achieve the above objectives, the present application provides the following technical solutions:
[0009] In the first aspect, the present application provides an industrial fermentation defoamer, comprising the following components in parts by weight: 5 to 10 parts of an organosilicon active substance, 3 to 7 parts of a polyether-modified organosiloxane, 30 to 40 parts of a polyether compound, 1 to 3 parts of an emulsifier, 1 to 3 parts of a thickener, and 37 to 60 parts of deionized water;
[0010] The organosilicon active material includes hydroxy silicone oil, hydrogen silicone oil, terpene olefin, vinyl silicone oil, MQ silicone resin, silicon dioxide, and a catalyst;
[0011] The polyether compound comprises at least one of fatty alcohol polyether, propylene glycol polyether, glycerol polyether and pentaerythritol polyether.
[0012] In a second aspect, the present application provides a method for preparing the aforementioned industrial fermentation defoamer, comprising the following steps:
[0013] Step 1: Mix the organosilicon active material, polyether-modified organosiloxane and emulsifier, stir and heat to 50-80° C. to obtain a first mixed solution;
[0014] Step 2: adding water and a thickener to the first mixed solution in sequence, then adjusting the pH value to 7, and repeating the above operation 2 to 3 times to obtain a second mixed solution;
[0015] Step 3: Keep the temperature of the second mixed solution at 50-80° C., add the polyether compound and mix, and naturally cool to room temperature to obtain the defoaming agent for industrial fermentation.
[0016] The present application provides an industrial fermentation defoamer and a preparation method thereof, which have at least the following beneficial effects:
[0017] 1. Compared with the prior art, the industrial fermentation defoamer provided in the present application has excellent defoaming ability, and only a small amount is needed to effectively control the foam generated during the fermentation process, the defoaming speed is fast, and the occurrence of demulsification of the defoamer is inhibited.
[0018] 2. The raw materials used for the industrial fermentation defoamer provided in this application are mild. Due to the small amount added, it will be decomposed into carbon source components of the culture medium by the fermentation bacteria in the later stage of fermentation. After use, there is no need for additional defoamer separation and removal steps, which improves fermentation efficiency and reduces labor costs.
[0019] 3. The preparation method of the industrial fermentation defoamer provided in this application is simple to operate, the raw materials are readily available, and it is suitable for large-scale production. DETAILED DESCRIPTION
[0020] In order to make the purpose, technical solution and advantages of the present application more clearly understood, the present application is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present application and are not used to limit the present application.
[0021] In the present application text, the term "terpene olefins" refers to olefin compounds whose molecular formula is an integer multiple of isoprene, and the general formula is n(C5H8). "Terpene olefins" are a class of natural hydrocarbons widely present in plants, which can be obtained from many plants, especially conifers; they are the main components of resins and turpentine derived from resins. Studies have found that a large number of terpene olefin compounds are also extracted from marine organisms. There are many types of "terpene olefins", which can be roughly divided into hemiterpenes (n=1, C5H8, meta-isoprene), monoterpenes (n=2, C 10 H 16 , such as pinene, limonene, myrcene, camphene), sesquiterpenes (n = 3, C 15 H 24 , such as gingerene), diterpenes (n=4, C 20 H 32 , such as camphorene) and polyterpenes (n=6, C 30 H 48 , such as squalene).
[0022] In the text of this application, the terms "first", "second" and the like are used to distinguish between identical or similar items with substantially the same functions and effects. This is only for the purpose of clearly describing the technical solutions of the embodiments of this application, and shall not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features.
[0023] In the present application, the term "normal temperature" refers to room temperature or general temperature, and the temperature range is 15 to 25°C.
[0024] In the text of this application, the term "cloud point" refers to cloud point, a characteristic constant of nonionic surfactants, which is affected by the molecular structure of surfactants and coexisting substances. The aqueous solution of surfactants will become turbid as the temperature rises, and the surfactant changes from completely dissolved to partially dissolved, and the temperature at the time of its transition is the cloud point temperature. Cloud point (CP) is the temperature at which the uniform micellar solution of nonionic surfactant (NS) undergoes phase separation, which is a very important physical parameter. The liquid sample is cooled to the critical temperature at which turbidity begins to appear under standard conditions. In the text of this application, the liquid sample refers to a polyether compound, including one or more combinations of fatty alcohol polyethers, propylene glycol polyethers, glycerol polyethers, and pentaerythritol polyethers. The cloud point of the polyether compound refers to the temperature at which the polyether solution begins to become turbid, which is due to the intensification of the motion of polyether molecules as the temperature rises, resulting in the weakening of the interaction force between molecules, thereby making the solution turbid. In the text of this application, the cloud point test method is not clearly defined, and it should be understood that it uses existing public technology to test the cloud point.
[0025] In view of the problems existing in the prior art, the present application embodiment has improved the existing fermentation defoamer composition components to obtain a new type of industrial fermentation defoamer, the defoamer component adds an organosilicon active containing terpene substances, some terpene substances have hydrophilic groups, increase hydrophilicity, and plant-based terpene substances, which will make the degradation rate of the compound faster. At the same time, the industrial fermentation defoamer also introduces a polyether compound, which is composed of at least one polyether with different cloud points or multiple polyethers with different cloud points among fatty alcohol polyether, propylene glycol polyether, glycerol polyether, and pentaerythritol polyether. Its polyether compound is composed of three polyethers with different cloud points of 5-20°C polyether, 21-30°C polyether, and 31-50°C polyether. The above three polyethers with different cloud points are 1-5 parts, 60-68 parts, and 27-39 parts by mass. During the high-temperature sterilization process, the industrial fermentation defoamer containing the above polyether compound supplements the defoamer emulsifier due to the precipitation of the combined polyether, and the precipitate is evenly dispersed in the emulsion, increasing the viscosity. During the high-temperature sterilization process, the emulsion will become more delicate by stirring, thereby achieving a better defoaming effect.
[0026] Based on this, an embodiment of the present application provides an industrial fermentation defoamer, comprising the following components in parts by weight: 5 to 10 parts of silicone active material, 3 to 7 parts of polyether-modified organosiloxane, 30 to 40 parts of polyether compound, 1 to 3 parts of emulsifier, 1 to 3 parts of thickener, and 37 to 60 parts of deionized water; the silicone active material includes hydroxy silicone oil, hydrogen-containing silicone oil, terpene olefins, vinyl silicone oil, MQ silicone resin, silica, and a catalyst; the polyether compound includes at least one of fatty alcohol polyether, propylene glycol polyether, glycerol polyether, and pentaerythritol polyether.
[0027] In the embodiment of the present application, the hydrogen-containing silicone oil, terpene olefins, vinyl silicone oil, hydroxy silicone oil, and MQ silicone resin are the reaction components of the silicone active material, and silicon dioxide is the foam-breaking particles in the silicone active material. The reaction components, foam-breaking particles, and catalysts together constitute the defoamer active material. In certain embodiments, the molar ratio of hydrogen-containing silicone oil, terpene olefins, vinyl silicone oil, and hydroxy silicone oil in the reaction components of the silicone active material is 1: 0.1-0.3: 0.4-0.6: 0.2-0.4. In certain preferred embodiments, the molar ratio of hydrogen-containing silicone oil, terpene olefins, vinyl silicone oil, and hydroxy silicone oil in the reaction components of the silicone active material is 1: 0.2: 0.5: 0.3.
[0028] In some embodiments, the hydrogen-containing silicone oil is end-side hydrogen silicone oil, and its hydrogen content is 0.1% to 1%.
[0029] In certain preferred embodiments, the terpene olefin is sesquiterpene. In certain more preferred embodiments, the terpene olefin is gingerene.
[0030] In some embodiments, the vinyl silicone oil is at least one of single-terminal vinyl silicone oil, double-terminal vinyl silicone oil, and end-side vinyl silicone oil. In some preferred embodiments, the vinyl silicone oil is double-terminal vinyl silicone oil, and its vinyl content is 0.1% to 0.5%.
[0031] In some embodiments, the hydroxy silicone oil is at least one of monohydroxy silicone oil and dihydroxy silicone oil, and the number of D-type chain segments is 10 to 1000. In some preferred embodiments, the hydroxy silicone oil is dihydroxy silicone oil.
[0032] In certain embodiments, the M / Q value of the MQ silicone resin is 0.6-0.8:1, and the mass proportion of the MQ silicone resin in the reaction components is 1%-10%, preferably 1%-5%.
[0033] In some embodiments, the hydrophobic value of the silicon dioxide is 30% to 70%, and the mass ratio of the silicon dioxide to the reaction component is 1 to 10: 100. In some preferred embodiments, the mass ratio of the silicon dioxide to the reaction component is 1 to 5:100.
[0034] In certain embodiments, the catalyst is selected from at least one of a platinum-alcohol complex, a platinum-olefin complex, a platinum-alkoxide complex, a platinum-ether complex, a platinum-ketone complex, a chloroplatinic acid isopropanol solution and a platinum-vinyl complex, and the catalyst is used to catalyze the polymerization reaction of the reaction components.
[0035] In certain preferred embodiments, the catalyst is chloroplatinic acid isopropanol solution.
[0036] In certain embodiments, the amount of the catalyst used is 5-10 ppm based on the total mass of the reaction components, calculated as platinum content.
[0037] In some embodiments, the preparation method of the organosilicon active material includes: mixing hydrogen-containing silicone oil, terpene olefins, and MQ silicone resin, adding a catalyst for the first time to heat up, keeping the temperature at 100-150°C for 30 minutes, and then cooling to room temperature; then adding end-chain vinyl silicone oil, adding a catalyst for the second time, the amount added is 2 to 6 times that of the first time, and heating up to 100-150°C for a second time to react; finally, adding hydroxyl silicone oil and silicon dioxide, stirring evenly, heating to 120°C, keeping the temperature for 4 hours, and then cooling to room temperature to obtain an organosilicon active material; the catalyst is selected from at least one of a platinum-alcohol complex, a platinum-olefin complex, a platinum-alkoxide complex, a platinum-ether complex, a platinum-ketone complex, a chloroplatinic acid isopropanol solution, and a platinum-vinyl complex.
[0038] In the embodiment of the present application, the polyether-modified organosiloxane is a complex formed by reacting polyorganohydrogensiloxane and unsaturated polyether under alkaline catalyst conditions.
[0039] In certain embodiments, the polyorganohydrogen siloxane has the following general structure: (CH3)3SiO[Si(CH3)2O] m (SiHCH3O) n Si(CH3)3, wherein m is an integer from 0 to 150, and n is an integer from 1 to 150.
[0040] In certain embodiments, the unsaturated polyether has the general formula HO(EO) p (PO) q OH, wherein p is an integer from 1 to 10, and q is an integer from 2 to 10.
[0041] In certain embodiments, the molar ratio of the organic hydrogen-containing siloxane to the unsaturated polyether is 1:1-2.
[0042] In some embodiments, the alkaline catalyst is selected from at least one of sodium hydroxide, potassium hydroxide, potassium silanolate, sodium silanolate, sodium methoxide, sodium ethoxide, potassium methoxide, potassium ethoxide, β-hydroxyethyl trimethylamine, and tetramethyl ammonium hydroxide. In some preferred embodiments, the alkaline catalyst is potassium hydroxide, and its amount is 5 to 10 ppm of the total mass of the polyether-modified organosiloxane.
[0043] In certain embodiments, the method for preparing the polyether-modified organosiloxane comprises: mixing polyorganohydrogensiloxane, unsaturated polyether, and alkaline catalyst to obtain a mixed solution, then heating the mixed solution to 120-200° C. for 30 min, and then cooling to room temperature.
[0044] In certain embodiments, the polyether compound is composed of one or more polyethers selected from fatty alcohol polyether, propylene glycol polyether, glycerol polyether, and pentaerythritol polyether. The polyether compound is composed of polyethers with three cloud points, namely, a first polyether, a second polyether, and a third polyether. The cloud point range of the first polyether is 5 to 20°C, the cloud point range of the second polyether is 21 to 30°C, and the cloud point range of the third polyether is 31 to 50°C; the mass ratio of the first polyether, the second polyether, and the third polyether is 1 to 5:60 to 68:27 to 39.
[0045] In the embodiments of the present application, the main function of the emulsifier is to reduce the interfacial tension between the organosilicon active substance and water, so that the organosilicon active substance can be dispersed stably in water for a long time. The emulsifier used in the embodiments of the present application includes nonionic surfactants, anionic surfactants, cationic surfactants, and amphoteric surfactants. In some preferred embodiments, nonionic surfactants are selected as emulsifiers.
[0046] In certain embodiments, the nonionic surfactant is a carbon chain emulsifier, including at least one of sorbitan monostearate (S-60), sorbitan monooleate (S-80), sorbitan tristearate (S-65), sorbitan monostearate (S-60), sorbitan monooleate polyoxyethylene ether ester (T-80), sorbitan tristearate polyoxyethylene ether ester (T-65), fatty alcohol polyoxyethylene ether, castor oil polyoxyethylene ether, alkylphenol polyoxyethylene ether, and glyceryl monostearate.
[0047] In the embodiments of the present application, the thickener is used to enhance the stability of the emulsion. The thickener is divided into natural thickeners and synthetic thickeners. The thickener includes at least one of polyvinyl alcohol (PVA), sodium carboxymethyl cellulose, methyl cellulose, hydroxyethyl cellulose, guar gum, xanthan gum, nonionic polyurethane, and alkali-soluble acrylate. In certain preferred embodiments, the thickener is alkali-soluble acrylate.
[0048] In the process of industrial fermentation, the fermentation liquid usually contains inorganic salts or trace elements. Therefore, in the embodiment of the present application, deionized water is used as a component of the industrial fermentation defoamer to minimize the impact on the fermentation liquid.
[0049] Based on this, an embodiment of the present application also provides a method for preparing the aforementioned industrial fermentation defoamer, comprising: a first step: mixing an organosilicon active, a polyether-modified organosiloxane, and an emulsifier, stirring and heating to 50-80°C; obtaining a first mixed solution; a second step: adding water and a thickener to the first mixed solution in sequence, and then adjusting the pH value to 7, repeating the above operation 2-3 times to obtain a second mixed solution; a third step: maintaining the temperature of the second mixed solution at 50-80°C, adding a polyether compound for mixing, and naturally cooling to room temperature to obtain the defoamer for industrial fermentation.
[0050] The technical solution of the present application and the technical effects achieved are described in detail below through more specific embodiments.
[0051] Example 1
[0052] This embodiment provides a method for preparing an industrial fermentation defoamer, comprising the following steps:
[0053] (1) Preparing an organosilicon active material, the specific method is as follows: firstly weighing reaction components, including 1 mol of hydrogen-containing silicone oil with a hydrogen content of 0.1%, 0.2 mol of gingerol, 0.5 mol of terminal vinyl silicone oil and 0.3 mol of hydroxy silicone oil (the number of D-type chain segments is 350); weighing MQ silicone resin (M / Q value is 0.7), the mass of which is 1% of the reaction components; weighing silicon dioxide, the mass of which is 1% of the reaction components; mixing the weighed hydrogen-containing silicone oil, gingerol and MQ silicone resin; Combine, add chloroplatinic acid isopropanol solution (1ppm of the total mass of the reaction components) for the first time to increase the temperature, keep the temperature for 30 minutes when the temperature reaches 100°C, and then cool to room temperature; add terminal vinyl silicone oil and add chloroplatinic acid isopropanol solution (4ppm of the total mass of the reaction components) for the second time, and heat it for the second time to 150°C for reaction; add hydroxy silicone oil and silicon dioxide, mix well, increase the temperature to 120°C, keep the temperature for 4 hours, and then cool to room temperature to obtain silicone active material X1;
[0054] (2) Preparation of polyether-modified organosiloxane: weigh 0.1 mol of polyorganohydrogen-containing siloxane, the chemical formula of which is (CH3)3SiO[Si(CH3)2O] 50 (SiHCH3O) 50 Si(CH3)3; weigh 0.15 mol of unsaturated polyether, whose chemical formula is HO(EO)5(PO)5OH; add potassium hydroxide (whose mass is 5 ppm of the total mass of polyorganohydrogensiloxane, unsaturated polyether and potassium hydroxide), raise the temperature to 120°C, and keep it warm for 30 minutes to obtain polyether-modified organosiloxane Y1;
[0055] (3) 5 g of organosilicon active material X1, 3 g of polyether-modified organosiloxane Y1, 0.5 g of sorbitan monooleate (S-80), and 0.5 g of sorbitan monooleate polyoxyethylene ether ester (T-80) were added to a beaker, stirred and heated to 50° C., 12 g of deionized water was added for emulsification, 0.5 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7, and stirred for 10 min; 12 g of water was added for emulsification, 0.5 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7; 12 g of water was added for emulsification, 0.5 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7;
[0056] (4) maintaining the mixed solution obtained in step (3) at a temperature of 80°C, adding 30 g of a polyether compound, wherein the polyether compound comprises a first polyether, a second polyether, and a third polyether, wherein the first polyether is a fatty alcohol polyether, having a turbidity point of 5°C and a mass of 0.3 g, the second polyether is a propylene glycol polyether, having a turbidity point of 21°C and a mass of 18 g, and the third polyether is a glycerol polyether, having a turbidity point of 50°C and a mass of 11.7 g; and cooling the mixture to room temperature to obtain a defoaming agent Z1 for industrial fermentation.
[0057] Example 2
[0058] This embodiment provides a method for preparing an industrial fermentation defoamer, comprising the following steps:
[0059] (1) Preparing an organosilicon active material, the specific method is as follows: firstly weighing reaction components, including 1 mol of hydrogen-containing silicone oil with a hydrogen content of 0.1%, 0.1 mol of gingerol, 0.4 mol of terminal vinyl silicone oil and 0.2 mol of hydroxy silicone oil (the number of D-type chain segments is 10); weighing MQ silicone resin (M / Q value is 0.6), the mass of which is 3% of the reaction components; weighing silicon dioxide, the mass of which is 3% of the reaction components; mixing the weighed hydrogen-containing silicone oil, gingerol and MQ silicone resin; Combine, add chloroplatinic acid isopropanol solution (2ppm of the total mass of the reaction components) for the first time to increase the temperature, keep the temperature for 30 minutes when the temperature reaches 120°C, and then cool to room temperature; add terminal vinyl silicone oil and add chloroplatinic acid isopropanol solution (8ppm of the total mass of the reaction components) for the second time, heat it for the second time, and heat it to 100°C for reaction; add hydroxy silicone oil and silicon dioxide, mix well, increase the temperature to 120°C, keep the temperature for 4 hours, and then cool to room temperature to obtain silicone active material X2;
[0060] (2) Preparation of polyether-modified organosiloxane: weigh 0.1 mol of polyorganohydrogen-containing siloxane, the chemical formula of which is (CH3)3SiO[Si(CH3)2O] 150 (SiHCH3O) 150 Si(CH3)3; weigh 0.1 mol of unsaturated polyether, whose chemical formula is HO(EO) 10(PO) 10 OH; adding potassium hydroxide (whose mass is 10 ppm of the total mass of the polyorganohydrogensiloxane, the unsaturated polyether and potassium hydroxide), heating to 200° C., and keeping the temperature for 30 min to obtain the polyether-modified organosiloxane Y2;
[0061] (3) 8 g of organosilicon active material X2, 5 g of polyether-modified organosiloxane Y2, 0.5 g of sorbitan monooleate (S-80), and 1 g of sorbitan monooleate polyoxyethylene ether ester (T-80) were added to a beaker, stirred and heated to 60° C., 15 g of deionized water was added for emulsification, 0.33 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7, and stirred for 10 min; 15 g of water was added for emulsification, 0.33 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7; 15 g of water was added for emulsification, 0.33 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7;
[0062] (4) The mixed solution obtained in step (3) is maintained at a temperature of 50°C, and 35 g of a polyether compound is added, wherein the polyether compound comprises a first polyether, a second polyether, and a third polyether, wherein the first polyether is a fatty alcohol polyether, having a turbidity point of 20°C and a mass of 1.4 g, the second polyether is a glycerol polyether, having a turbidity point of 30°C and a mass of 23.1 g, and the third polyether is a pentaerythritol polyether, having a turbidity point of 31°C and a mass of 10.9 g; and the mixture is cooled to room temperature to obtain a defoaming agent Z2 for industrial fermentation.
[0063] Example 3
[0064] This embodiment provides a method for preparing an industrial fermentation defoamer, comprising the following steps:
[0065] (1) Preparing an organosilicon active material, the specific method is as follows: firstly weighing reaction components, including 1 mol of hydrogen-containing silicone oil with a hydrogen content of 0.1%, 0.3 mol of gingerol, 0.6 mol of terminal vinyl silicone oil and 0.4 mol of hydroxy silicone oil (the number of D-type chain segments is 1000); weighing MQ silicone resin (M / Q value is 0.8), the mass of which is 5% of the reaction components; weighing silicon dioxide, the mass of which is 5% of the reaction components; mixing the weighed hydrogen-containing silicone oil, gingerol and MQ silicone resin; Combine, add chloroplatinic acid isopropanol solution (1.5ppm of the total mass of the reaction components) for the first time to increase the temperature, keep the temperature for 30min when the temperature reaches 150°C, and then cool to room temperature; add terminal vinyl silicone oil and add chloroplatinic acid isopropanol solution (6ppm of the total mass of the reaction components) for the second time, heat it for the second time, and heat it to 120°C for reaction; add hydroxy silicone oil and silicon dioxide, mix well, heat it to 120°C, keep it for 4h, and then cool it to room temperature to obtain silicone active material X3;
[0066] (2) preparing a polyether-modified organosiloxane, specifically, weighing 0.1 mol of polyorganohydrogensiloxane, whose chemical formula is SiHCH3OSi(CH3)3; weighing 0.2 mol of unsaturated polyether, whose chemical formula is HO(EO)(PO)2OH; adding potassium hydroxide (whose mass is 8 ppm of the total mass of polyorganohydrogensiloxane, unsaturated polyether and potassium hydroxide), heating to 150°C, and keeping the temperature for 30 minutes, thereby obtaining polyether-modified organosiloxane Y3;
[0067] (3) 10 g of organosilicon active material X3, 7 g of polyether-modified organosiloxane Y3, 1.5 g of sorbitan monooleate (S-80), and 1.5 g of sorbitan monooleate polyoxyethylene ether ester (T-80) were added to a beaker, stirred and heated to 60° C., 20 g of deionized water was added for emulsification, 0.5 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7, and stirred for 10 min; 20 g of water was added for emulsification, 0.5 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7; 20 g of water was added for emulsification, 0.5 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7;
[0068] (4) The mixed solution obtained in step (3) is maintained at a temperature of 70°C, and 40 g of a polyether compound is added, wherein the polyether compound comprises a first polyether, a second polyether, and a third polyether, wherein the first polyether is a glycerol polyether having a turbidity point of 15°C and a mass of 2 g, the second polyether is a glycerol polyether having a turbidity point of 23°C and a mass of 27.2 g, and the third polyether is a glycerol polyether having a turbidity point of 35°C and a mass of 10.8 g; and the mixture is cooled to room temperature to obtain a defoaming agent Z3 for industrial fermentation.
[0069] Example 4
[0070] This embodiment provides a method for preparing an industrial fermentation defoamer, comprising the following steps:
[0071] (1) Preparing an organosilicon active material, the specific method is as follows: firstly weighing reaction components, including 1 mol of hydrogen-containing silicone oil with a hydrogen content of 0.1%, 0.2 mol of gingerol, 0.5 mol of terminal vinyl silicone oil and 0.3 mol of hydroxy silicone oil (the number of D-type chain segments is 400); weighing MQ silicone resin (M / Q value is 0.8), the mass of which is 6% of the reaction components; weighing silicon dioxide, the mass of which is 3% of the reaction components; mixing the weighed hydrogen-containing silicone oil, gingerol and MQ silicone resin; Combine, add chloroplatinic acid isopropanol solution (1ppm of the total mass of the reaction components) for the first time to increase the temperature, keep the temperature for 30 minutes, and then cool to room temperature; add terminal vinyl silicone oil and add chloroplatinic acid isopropanol solution (4ppm of the total mass of the reaction components) for the second time, heat it for the second time, and heat it to 100°C for reaction; add hydroxy silicone oil and silicon dioxide, mix well, heat it to 120°C, keep it for 4 hours, and then cool it to room temperature to obtain silicone active material X4;
[0072] (2) Preparation of polyether-modified organosiloxane: weigh 0.1 mol of polyorganohydrogen-containing siloxane, the chemical formula of which is (CH3)3SiO[Si(CH3)2O] 50 (SiHCH3O) 100 Si(CH3)3; weigh 0.1 mol of unsaturated polyether, whose chemical formula is HO(EO)5(PO)5OH; add potassium hydroxide (whose mass is 6 ppm of the total mass of polyorganohydrogensiloxane, unsaturated polyether and potassium hydroxide), raise the temperature to 120°C, and keep it warm for 30 minutes to obtain polyether-modified organosiloxane Y4;
[0073] (3) 6 g of organosilicon active material X4, 4 g of polyether-modified organosiloxane Y4, 1 g of sorbitan monooleate (S-80), and 1.5 g of sorbitan monooleate polyoxyethylene ether ester (T-80) were added to a beaker, stirred and heated to 60° C., 13 g of deionized water was added for emulsification, 0.5 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7, and stirred for 10 min; 14 g of water was added for emulsification, 0.5 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7; 15 g of water was added for emulsification, 1 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7;
[0074] (4) The mixed solution obtained in step (3) is maintained at a temperature of 60°C, and 35 g of a polyether compound is added, wherein the polyether compound comprises a first polyether, a second polyether, and a third polyether, wherein the first polyether is propylene glycol polyether, having a turbidity point of 18°C and a mass of 1.4 g, the second polyether is glycerol polyether, having a turbidity point of 25°C and a mass of 23.1 g, and the third polyether is pentaerythritol polyether, having a turbidity point of 40°C and a mass of 10.5 g; and the mixture is cooled to room temperature to obtain defoaming agent Z4 for industrial fermentation.
[0075] Comparative Example 1
[0076] This comparative example provides a method for preparing an industrial fermentation defoamer, comprising the following steps:
[0077] (1) Preparing an organosilicon active material, the specific method is as follows: first weighing the reaction components, including 1 mol of hydrogen-containing silicone oil with a hydrogen content of 0.1%, 0.5 mol of terminal vinyl silicone oil and 0.3 mol of hydroxy silicone oil (the number of D-type chain segments is 350); weighing MQ silicone resin (M / Q value is 0.7), the mass of which is 1% of the reaction components; weighing silicon dioxide, the mass of which is 1% of the reaction components; mixing the weighed hydrogen-containing silicone oil, gingerol and MQ silicone resin, adding chloroplatinic acid isopropanol solution (1 ppm of the total mass of the reaction components) for the first time to increase the temperature, and when the temperature reaches 100° C., keeping the temperature for 30 minutes, and then cooling to room temperature; adding terminal vinyl silicone oil and adding chloroplatinic acid isopropanol solution (4 ppm of the total mass of the reaction components) for the second time, heating for the second time, and heating to 150° C. for reaction; adding hydroxy silicone oil and silicon dioxide, mixing evenly, heating to 120° C., keeping the temperature for 4 hours, and then cooling to room temperature, to obtain an organosilicon active material X5;
[0078] (2) Preparation of polyether-modified organosiloxane: weigh 0.1 mol of polyorganohydrogen-containing siloxane, the chemical formula of which is (CH3)3SiO[Si(CH3)2O] 50 (SiHCH3O) 50 Si(CH3)3; weigh 0.15 mol of unsaturated polyether, whose chemical formula is HO(EO)5(PO)5OH; add potassium hydroxide (whose mass is 5 ppm of the total mass of polyorganohydrogensiloxane, unsaturated polyether and potassium hydroxide), raise the temperature to 120°C, and keep it warm for 30 minutes to obtain polyether-modified organosiloxane Y5;
[0079] (3) 5 g of organosilicon active material X5, 3 g of polyether-modified organosiloxane Y5, 0.5 g of sorbitan monooleate (S-80), and 0.5 g of sorbitan monooleate polyoxyethylene ether ester (T-80) were added to a beaker, stirred and heated to 50° C., 12 g of deionized water was added for emulsification, 0.5 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7, and stirred for 10 min; 12 g of water was added for emulsification, 0.5 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7; 12 g of water was added for emulsification, 0.5 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7;
[0080] (4) The mixed solution obtained in step (3) is maintained at a temperature of 80°C, and 30 g of a polyether compound is added, wherein the polyether compound comprises a first polyether, a second polyether, and a third polyether, wherein the first polyether is a fatty alcohol polyether, having a turbidity point of 5°C and a mass of 0.3 g, the second polyether is a propylene glycol polyether, having a turbidity point of 21°C and a mass of 18 g, and the third polyether is a glycerol polyether, having a turbidity point of 50°C and a mass of 11.7 g; and the mixture is cooled to room temperature to obtain the defoaming agent Z5 for industrial fermentation.
[0081] Comparative Example 2
[0082] This comparative example provides a method for preparing an industrial fermentation defoamer, comprising the following steps:
[0083] (1) Preparing an organosilicon active material, the specific method is as follows: firstly weighing reaction components, including 1 mol of hydrogen-containing silicone oil with a hydrogen content of 0.1%, 0.2 mol of gingerol, 0.5 mol of terminal vinyl silicone oil and 0.3 mol of hydroxy silicone oil (the number of D-type chain segments is 350); weighing MQ silicone resin (M / Q value is 0.7), the mass of which is 1% of the reaction components; weighing silicon dioxide, the mass of which is 1% of the reaction components; mixing the weighed hydrogen-containing silicone oil, gingerol and MQ silicone resin; Combine, add chloroplatinic acid isopropanol solution (1ppm of the total mass of the reaction components) for the first time to increase the temperature, keep the temperature for 30 minutes when the temperature reaches 100°C, and then cool to room temperature; add terminal vinyl silicone oil and add chloroplatinic acid isopropanol solution (4ppm of the total mass of the reaction components) for the second time, and heat it for the second time to 150°C for reaction; add hydroxyl silicone oil and silicon dioxide, mix well, increase the temperature to 120°C, keep the temperature for 4 hours, and then cool to room temperature to obtain silicone active material X6;
[0084] (2) Preparation of polyether-modified organosiloxane: weigh 0.1 mol of polyorganohydrogen-containing siloxane, the chemical formula of which is (CH3)3SiO[Si(CH3)2O] 50 (SiHCH3O) 50 Si(CH3)3; weigh 0.15 mol of unsaturated polyether, whose chemical formula is HO(EO)5(PO)5OH; add potassium hydroxide (whose mass is 5 ppm of the total mass of polyorganohydrogensiloxane, unsaturated polyether and potassium hydroxide), raise the temperature to 120°C, and keep it warm for 30 minutes to obtain polyether-modified organosiloxane Y6;
[0085] (3) 5 g of organosilicon active material X6, 3 g of polyether-modified organosiloxane Y6, 0.5 g of sorbitan monooleate (S-80), and 0.5 g of sorbitan monooleate polyoxyethylene ether ester (T-80) were added to a beaker, stirred and heated to 50° C., 12 g of deionized water was added for emulsification, 0.5 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7, and stirred for 10 min; 12 g of water was added for emulsification, 0.5 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7; 12 g of water was added for emulsification, 0.5 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7;
[0086] (4) The mixed solution obtained in step (3) is cooled to room temperature to obtain the defoaming agent Z6 for industrial fermentation.
[0087] Comparative Example 3
[0088] This comparative example provides a method for preparing an industrial fermentation defoamer, comprising the following steps:
[0089] (1) Preparing an organosilicon active material, the specific method is as follows: first weighing the reaction components, including 1 mol of hydrogen-containing silicone oil with a hydrogen content of 0.1%, 0.5 mol of terminal vinyl silicone oil and 0.3 mol of hydroxy silicone oil (the number of D-type chain segments is 350); weighing MQ silicone resin (M / Q value is 0.7), the mass of which is 1% of the reaction components; weighing silicon dioxide, the mass of which is 1% of the reaction components; mixing the weighed hydrogen-containing silicone oil, gingerol and MQ silicone resin, adding chloroplatinic acid isopropanol solution (1 ppm of the total mass of the reaction components) for the first time to increase the temperature, and when the temperature reaches 100° C., keeping the temperature for 30 minutes, and then cooling to room temperature; adding terminal vinyl silicone oil and adding chloroplatinic acid isopropanol solution (4 ppm of the total mass of the reaction components) for the second time, heating for the second time, and heating to 150° C. for reaction; adding hydroxy silicone oil and silicon dioxide, mixing evenly, heating to 120° C., keeping the temperature for 4 hours, and then cooling to room temperature, to obtain an organosilicon active material X7;
[0090] (2) Preparation of polyether-modified organosiloxane: weigh 0.1 mol of polyorganohydrogen-containing siloxane, the chemical formula of which is (CH3)3SiO[Si(CH3)2O] 50 (SiHCH3O) 50 Si(CH3)3; weigh 0.15 mol of unsaturated polyether, whose chemical formula is HO(EO)5(PO)5OH; add potassium hydroxide (whose mass is 5 ppm of the total mass of polyorganohydrogensiloxane, unsaturated polyether and potassium hydroxide), raise the temperature to 120°C, and keep it warm for 30 minutes to obtain polyether-modified organosiloxane Y7;
[0091] (3) 5 g of organosilicon active material X7, 3 g of polyether-modified organosiloxane Y7, 0.5 g of sorbitan monooleate (S-80), and 0.5 g of sorbitan monooleate polyoxyethylene ether ester (T-80) were added to a beaker, stirred and heated to 50° C., 12 g of deionized water was added for emulsification, 0.5 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7, and stirred for 10 min; 12 g of water was added for emulsification, 0.5 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7; 12 g of water was added for emulsification, 0.5 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7;
[0092] (4) The mixed solution obtained in step (3) is cooled to room temperature to obtain the defoaming agent Z7 for industrial fermentation.
[0093] Comparative Example 4
[0094] This comparative example provides a method for preparing an industrial fermentation defoamer, comprising the following steps:
[0095] (1) Preparing an organosilicon active material, the specific method is as follows: firstly weighing reaction components, including 1 mol of hydrogen-containing silicone oil with a hydrogen content of 0.1%, 0.2 mol of gingerol, 0.5 mol of terminal vinyl silicone oil and 0.3 mol of hydroxy silicone oil (the number of D-type chain segments is 350); weighing MQ silicone resin (M / Q value is 0.7), the mass of which is 1% of the reaction components; weighing silicon dioxide, the mass of which is 1% of the reaction components; mixing the weighed hydrogen-containing silicone oil, gingerol and MQ silicone resin; Combine, add chloroplatinic acid isopropanol solution (1ppm of the total mass of the reaction components) for the first time to increase the temperature, keep the temperature for 30 minutes when the temperature reaches 100°C, and then cool to room temperature; add terminal vinyl silicone oil and add chloroplatinic acid isopropanol solution (4ppm of the total mass of the reaction components) for the second time, and heat it for the second time to 150°C for reaction; add hydroxyl silicone oil and silicon dioxide, mix well, increase the temperature to 120°C, keep the temperature for 4 hours, and then cool to room temperature to obtain silicone active material X8;
[0096] (2) Preparation of polyether-modified organosiloxane: weigh 0.1 mol of polyorganohydrogen-containing siloxane, the chemical formula of which is (CH3)3SiO[Si(CH3)2O] 50 (SiHCH3O) 50 Si(CH3)3; weigh 0.15 mol of unsaturated polyether, whose chemical formula is HO(EO)5(PO)5OH; add potassium hydroxide (whose mass is 5 ppm of the total mass of polyorganohydrogensiloxane, unsaturated polyether and potassium hydroxide), raise the temperature to 120°C, and keep it warm for 30 minutes to obtain polyether-modified organosiloxane Y8;
[0097] (3) 5 g of organosilicon active material X8, 3 g of polyether-modified organosiloxane Y8, 0.5 g of sorbitan monooleate (S-80), and 0.5 g of sorbitan monooleate polyoxyethylene ether ester (T-80) were added to a beaker, stirred and heated to 50° C., 12 g of deionized water was added for emulsification, 0.5 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7, and stirred for 10 min; 12 g of water was added for emulsification, 0.5 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7; 12 g of water was added for emulsification, 0.5 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7;
[0098] (4) The mixed solution obtained in step (3) was kept at 80°C, 30 g of fatty alcohol polyether was added, and the cloud point was 5°C; the mixture was cooled to room temperature to obtain the defoaming agent Z8 for industrial fermentation.
[0099] Comparative Example 5
[0100] This comparative example provides a method for preparing an industrial fermentation defoamer, comprising the following steps:
[0101] (1) Preparing an organosilicon active material, the specific method is as follows: firstly weighing reaction components, including 1 mol of hydrogen-containing silicone oil with a hydrogen content of 0.1%, 0.2 mol of gingerol, 0.5 mol of terminal vinyl silicone oil and 0.3 mol of hydroxy silicone oil (the number of D-type chain segments is 350); weighing MQ silicone resin (M / Q value is 0.7), the mass of which is 1% of the reaction components; weighing silicon dioxide, the mass of which is 1% of the reaction components; mixing the weighed hydrogen-containing silicone oil, gingerol and MQ silicone resin; Combine, add chloroplatinic acid isopropanol solution (1ppm of the total mass of the reaction components) for the first time to increase the temperature, keep the temperature for 30 minutes when the temperature reaches 100°C, and then cool to room temperature; add terminal vinyl silicone oil and add chloroplatinic acid isopropanol solution (4ppm of the total mass of the reaction components) for the second time, and heat it for the second time to 150°C for reaction; add hydroxy silicone oil and silicon dioxide, mix well, increase the temperature to 120°C, keep the temperature for 4 hours, and then cool to room temperature to obtain silicone active material X9;
[0102] (2) Preparation of polyether-modified organosiloxane: weigh 0.1 mol of polyorganohydrogen-containing siloxane, the chemical formula of which is (CH3)3SiO[Si(CH3)2O] 50 (SiHCH3O) 50 Si(CH3)3; weigh 0.15 mol of unsaturated polyether, whose chemical formula is HO(EO)5(PO)5OH; add potassium hydroxide (whose mass is 5 ppm of the total mass of polyorganohydrogensiloxane, unsaturated polyether and potassium hydroxide), raise the temperature to 120°C, and keep it warm for 30 minutes to obtain polyether-modified organosiloxane Y9;
[0103] (3) 5 g of organosilicon active material X9, 3 g of polyether-modified organosiloxane Y9, 0.5 g of sorbitan monooleate (S-80), and 0.5 g of sorbitan monooleate polyoxyethylene ether ester (T-80) were added to a beaker, stirred and heated to 50° C., 12 g of deionized water was added for emulsification, 0.5 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7, and stirred for 10 min; 12 g of water was added for emulsification, 0.5 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7; 12 g of water was added for emulsification, 0.5 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7;
[0104] (4) The mixed solution obtained in step (3) was kept at 80°C, 30 g of propylene glycol polyether was added, and the cloud point was 21°C; the mixture was cooled to room temperature to obtain the defoaming agent Z9 for industrial fermentation.
[0105] Comparative Example 6
[0106] This comparative example provides a method for preparing an industrial fermentation defoamer, comprising the following steps:
[0107] (1) Preparing an organosilicon active material, the specific method is as follows: firstly weighing reaction components, including 1 mol of hydrogen-containing silicone oil with a hydrogen content of 0.1%, 0.2 mol of gingerol, 0.5 mol of terminal vinyl silicone oil and 0.3 mol of hydroxy silicone oil (the number of D-type chain segments is 350); weighing MQ silicone resin (M / Q value is 0.7), the mass of which is 1% of the reaction components; weighing silicon dioxide, the mass of which is 1% of the reaction components; and mixing the weighed hydrogen-containing silicone oil, gingerol and MQ silicone resin. Mix, add chloroplatinic acid isopropanol solution (1ppm of the total mass of the reaction components) for the first time to heat up, keep warm for 30min, and then cool to room temperature; add terminal vinyl silicone oil and add chloroplatinic acid isopropanol solution (4ppm of the total mass of the reaction components) for the second time, heat up for the second time, heat to 150℃ for reaction; add hydroxy silicone oil and silicon dioxide, mix well, heat up to 120℃, keep warm for 4h, and then cool to room temperature to obtain organic silicon active material X 10 ;
[0108] (2) Preparation of polyether-modified organosiloxane: weigh 0.1 mol of polyorganohydrogen-containing siloxane, the chemical formula of which is (CH3)3SiO[Si(CH3)2O] 50 (SiHCH3O) 50 Si(CH3)3; weigh 0.15 mol of unsaturated polyether, whose chemical formula is HO(EO)5(PO)5OH; add potassium hydroxide (whose mass is 5 ppm of the total mass of polyorganohydrogensiloxane, unsaturated polyether and potassium hydroxide), raise the temperature to 120°C, and keep it warm for 30 minutes to obtain polyether-modified organosiloxane Y 10 ;
[0109] (3) Take 5g of organic silicon active substance X 10 , 3g polyether modified organosiloxane Y 10 , 0.5 g of sorbitan monooleate (S-80) and 0.5 g of sorbitan monooleate polyoxyethylene ether ester (T-80) were added to a beaker, stirred and heated to 50°C, 12 g of deionized water was added for emulsification, 0.5 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7, and stirred for 10 min; 12 g of water was continued for emulsification, 0.5 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7; 12 g of water was emulsified, 0.5 g of alkali-soluble acrylate was added, and the pH value was adjusted to 7;
[0110] (4) The mixed solution obtained in step (3) was kept at 80°C, 30 g of pentaerythritol polyether was added, and the turbidity point was 50°C; the mixture was cooled to room temperature to obtain the defoamer Z for industrial fermentation. 10 .
[0111] The defoaming ability of the industrial fermentation defoamers prepared in Examples 1 to 4 and Comparative Examples 1 to 6 was tested, and the specific method was as follows:
[0112] (1) High temperature resistance test: 100 g of defoamer was added to a sterilization autoclave, the autoclave was heated to 120°C, kept warm for 4 h, then cooled to room temperature, 5% of the defoamer was taken out and dispersed in water to see if there was any floating oil.
[0113] (2) Post-sterilization performance measurement: 1 g of the sterilized defoamer was taken out and added to a 300 ml sample bottle. 100 g of 1% sodium dodecylbenzene sulfonate solution was added to the sample bottle. After the bottle was filled, an HVS-10M vertical oscillator was used to oscillate at 450 rpm / min for 30 min, and the defoaming time was recorded.
[0114] Industrial fermentation defoamers Z1 to Z2 prepared in Examples 1 to 4 and Comparative Examples 1 to 6 10 The main difference parameters in the preparation process and the final defoaming effect comparison results are shown in Table 1 below.
[0115] Table 1
[0116]
[0117]
[0118] According to the results in Table 1, it can be seen that the industrial fermentation defoamers Z1-Z4 prepared in Examples 1-4 have the best defoaming effect, that is, no oil floating occurs after high-temperature sterilization. At the same time, the defoaming speed is relatively fast, and the defoaming time is less than 30 seconds. The reason for the above results is that the industrial fermentation defoamers prepared in the examples all introduce terpene olefins and polyether compounds with gradient cloud points, wherein the terpene olefin substances (such as gingerol) have hydrophilic groups, which can increase hydrophilicity and accelerate the degradation rate of the compound, thereby achieving a fast defoaming rate. The reason for artificially setting the cloud point gradient of the polyether compound is that during high-temperature sterilization in the fermentation industry, the temperature will rise from room temperature to 120-130°C, and it is necessary to have the effect of maintaining the stability of the emulsion at different temperature sections from room temperature to 120-130°C. This polyether compound with a gradient cloud point forms an optimal hydrophilic-lipophilic balance (HLB), which is of great help in maintaining the stability of the emulsion, avoiding the demulsification of the defoamer after high-temperature sterilization, resulting in oil floating, and the defoamer with only a single cloud point range of polyether compounds cannot achieve this effect.
[0119] The industrial fermentation defoamers Z5 and Z7 prepared in Comparative Examples 1 and 3 have a longer defoaming time because they do not contain terpene olefin components. At the same time, Z7 does not have a polyether compound with a gradient cloud point. After high-temperature sterilization, oil floating occurs. 10 Polyether compounds without polyethers or with only a single cloud point cannot form the best hydrophilic-lipophilic balance (HLB) and maintain the stability of the defoamer. Therefore, after high-temperature sterilization, oil will float. 10 The defoaming time is also higher than that of the industrial fermentation defoamers Z1 to Z4 prepared in the examples.
[0120] In summary, the industrial fermentation defoamer provided in the embodiments of the present application can achieve the optimal defoaming effect on the fermentation broth only when it contains both terpene olefins and a polyether compound with a gradient cloud point.
[0121] The present application is described in detail above. Specific examples are used in this article to illustrate the principles and implementation methods of the present application. The description of the above embodiments is only used to help understand the present application and its core ideas. It should be pointed out that for ordinary technicians in this technical field, without departing from the principles of the present application, several improvements and modifications can be made to the present application, and these improvements and modifications also fall within the scope of protection of the claims of the present application.
Claims
1. An industrial fermentation defoamer, characterized in that: The invention comprises the following components in parts by weight: 5-10 parts of organic silicon active material, 3-7 parts of polyether modified organic silicon oxane, 30-40 parts of polyether compound, 1-3 parts of emulsifier, 1-3 parts of thickener and 37-60 parts of deionized water; the organic silicon active material comprises hydroxy silicone oil, hydrogen silicone oil, terpene olefin, vinyl silicone oil, MQ silicone resin, silicon dioxide and catalyst; the polyether compound comprises at least one of fatty alcohol polyether, propylene glycol polyether, glycerol polyether and pentaerythritol polyether.
2. The industrial fermentation defoamer according to claim 1, characterized in that The hydrogen-containing silicone oil, terpene olefins, vinyl silicone oil, hydroxy silicone oil and MQ silicone resin are reaction components of the organosilicon active material, and the molar ratio of the hydrogen-containing silicone oil, terpene olefins, vinyl silicone oil and hydroxy silicone oil in the reaction components of the organosilicon active material is 1:0.1-0.3:0.4-0.6:0.2-0.
4.
3. The industrial fermentation defoamer according to claim 1, characterized in that The terpene olefin is sesquiterpene.
4. The industrial fermentation defoamer according to claim 1, characterized in that The catalyst is selected from at least one of a platinum-alcohol complex, a platinum-olefin complex, a platinum-alkoxide complex, a platinum-ether complex, a platinum-ketone complex, a chloroplatinic acid isopropanol solution and a platinum-vinyl complex.
5. The industrial fermentation defoamer according to claim 1, characterized in that The preparation method of the organic silicon active material comprises: mixing hydrogen-containing silicone oil, terpene olefins and MQ silicone resin, heating the mixture under the condition of adding a catalyst for the first time, keeping the temperature at 100-150° C. for 30 minutes, and then cooling the mixture to room temperature; then adding end-chain vinyl silicone oil, adding a catalyst for the second time in an amount four times that of the first time, heating the mixture to 100-150° C. for a second time to react; finally adding hydroxy silicone oil and silicon dioxide, stirring the mixture evenly, heating the mixture to 120° C., keeping the temperature for 4 hours, and then cooling the mixture to room temperature to obtain the organic silicon active material; the catalyst is selected from at least one of a platinum-alcohol complex, a platinum-olefin complex, a platinum-alkoxide complex, a platinum-ether complex, a platinum-ketone complex, a chloroplatinic acid isopropanol solution and a platinum-vinyl complex.
6. The industrial fermentation defoamer according to claim 1, characterized in that The polyether-modified organosiloxane is a complex formed by the reaction of polyorganohydrogensiloxane and unsaturated polyether under alkaline catalyst conditions; the general structural formula of the polyorganohydrogensiloxane is as follows: (CH3)3SiO[Si(CH3)2O] m (SiHCH3O) n Si(CH3)3, wherein m is an integer of 0 to 150, and n is an integer of 1 to 150; the general structural formula of the unsaturated polyether is HO(EO) p (PO) q OH, wherein p is an integer of 1 to 10, and q is an integer of 2 to 10; the molar ratio of the organic hydrogen-containing siloxane to the unsaturated polyether is 1:1 to 2.
7. The industrial fermentation defoamer according to claim 6, characterized in that The alkaline catalyst is selected from at least one of sodium hydroxide, potassium hydroxide, potassium silanolate, sodium silanolate, sodium methoxide, sodium ethoxide, potassium methoxide, potassium ethoxide, β-hydroxyethyltrimethylamine, and tetramethylammonium hydroxide.
8. The industrial fermentation defoamer according to claim 1, characterized in that The polyether compound is composed of three types of polyethers with different cloud points, namely a first polyether, a second polyether and a third polyether, wherein the cloud point range of the first polyether is 5 to 20°C, the cloud point range of the second polyether is 21 to 30°C, and the cloud point range of the third polyether is 31 to 50°C; the mass ratio of the first polyether, the second polyether and the third polyether is 1 to 5:60 to 68:27 to 39.
9. The industrial fermentation defoamer according to claim 1, characterized in that The emulsifier includes at least one of sorbitan monostearate, sorbitan monooleate, sorbitan tristearate, sorbitan monostearate, sorbitan monooleate polyoxyethylene ether ester, sorbitan tristearate polyoxyethylene ether ester, fatty alcohol polyoxyethylene ether, castor oil polyoxyethylene ether, alkylphenol polyoxyethylene ether, and glyceryl monostearate; the thickener includes at least one of polyvinyl alcohol, sodium carboxymethyl cellulose, methyl cellulose, hydroxyethyl cellulose, guar gum, xanthan gum, nonionic polyurethane, and alkali-soluble acrylate.
10. The method for preparing the industrial fermentation defoamer according to any one of claims 1 to 9, characterized in that: The following steps are involved: Step 1: Mix the organosilicon active material, polyether-modified organosiloxane and emulsifier, stir and heat to 50-80° C. to obtain a first mixed solution; Step 2: adding water and a thickener to the first mixed solution in sequence, then adjusting the pH value to 7, and repeating the above operation 2 to 3 times to obtain a second mixed solution; Step 3: maintaining the temperature of the second mixed solution at 50-80° C., adding the polyether compound and mixing, and naturally cooling to room temperature to obtain the defoaming agent for industrial fermentation.
Citation Information
Patent Citations
Environment-friendly plastic-replacing glazing oil and application thereof in paper product packaging
CN114592381A
Organosilicon modified terpene resin and its application
CN1306059A
Biodiesel-based emulsion defoamer and method for making the same
US20160107103A1
Organosilicon composite emulsion defoamer for papermaking industry, and preparation method therefor
WO2021203556A1
Cited By
Defoaming agent for fermentation and preparation method thereof
CN119701421A
Tween 85 and low-cloud-point fatty alcohol polyether compounded slag wastewater defoaming agent and preparation method thereof
CN119896885A
Efficient emulsion defoaming agent as well as preparation method and application thereof
CN121155182A