Security element having liquid crystal layer forming visual object
By applying a first embossed paint layer of multi-region orientation structure and a reinforced reflective coating on the carrier film, combined with the uniform orientation of the liquid crystal material, the problem that existing liquid crystal materials are difficult to achieve high resolution and high cost during the manufacturing process is solved. , achieving efficient anti-counterfeiting protection and visual effects.
Patent Information
- Application Number
- CN202410560940.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-05-08
- Filing Date
- 2024-05-08
- Publication Date
- 2024-11-08
AI Technical Summary
In the manufacturing process of existing liquid crystal materials, it is difficult to achieve high-resolution and low-cost anti-counterfeiting components, and their anti-counterfeiting protection effect is insufficient. In particular, solvent-based liquid crystal paint is easy to level after printing, has poor peeling ability, and has double-sided pressure. Printing may result in undefined visual objects.
By applying a first embossed paint layer and a second embossed paint layer on the carrier film, the first embossed paint layer has a different orientation structure in multiple areas, through which the liquid crystal material is uniformly oriented to form a latent visual object, and at An enhanced reflective coating is applied throughout the surface, and a polarizer is used to make the visual object present a contrasting effect at different angles.
It realizes the anti-counterfeiting protection effect of anti-counterfeiting components without increasing manufacturing costs, and presents different visual objects through different polarizers, enhancing the observer's attention and anti-counterfeiting effect.
Smart Images

Figure CN118915348A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a security element for providing security for valuables, the security element having a visual object layer based on a liquid crystal material, the liquid crystal material being designed and defined for forming a latent visual object, a correspondingly associated production method and a data carrier having such a security element. Background Art
[0002] Data carriers such as value documents or identification documents as well as other valuable items such as brand-name goods are often equipped with security elements for the purpose of anti-counterfeiting, which can verify the authenticity of the data carrier and at the same time serve to prevent unauthorized duplication. Security elements with perspective-dependent or three-dimensional effects play a particular role in authenticity assurance, since such security elements cannot be reproduced even with the latest copying equipment.
[0003] In many cases, special properties of liquid crystal materials are also utilized, in this case in particular the viewing angle-dependent color impression and / or light polarization effects of the liquid crystals.
[0004] Such materials are practically invisible after application to a carrier, but show a clear visual optical effect in a corresponding substrate, for example a reflective printed substrate, and with the aid of a linear or circular polarizer. Only when viewed through a linear or circular polarizer do the coated areas become more or less visible. The impression can also depend to a greater extent on the (angular) position of the polarizer.
[0005] The method used here is based, for example, on providing a nematic liquid crystal layer on a reflective metal layer to ensure good visibility of the polarization effect. WO 2005 / 105475 A1 describes a method in which a nematic liquid crystal material, for example a solvent-based UV-crosslinked liquid crystal lacquer, is printed in a pattern on a carrier film.
[0006] The plastic carrier films used in these methods have, due to their internal structure, a preferential direction (along the travel direction) which is sufficient to orient the liquid crystal material in the desired shape. Plastic films with a surface structure generated during production, such as PET films, are particularly suitable.
[0007] In a subsequent processing step, a UV-curing embossing lacquer layer is then printed over the entire surface of the carrier film and the nematic layer. The desired embossed structure, such as a diffractive structure, is embossed on the embossing lacquer layer, and then a reflective layer is applied, in particular by vapor deposition, for example in the form of a metal layer, in which recesses can be introduced by partial demetallization. Finally, an adhesive medium layer or primer layer is applied to the target substrate, such as paper, and the adhesive layer is applied thereto to the layer composite.
[0008] Viewed from above, the following layer sequence is thus produced: nematic liquid crystal, UV lacquer (with embossed structure), metallization. When viewed without auxiliary components, the layer composite only shows the optically variable diffractive structure, such as a hologram, provided by the embossed structure. If, however, the layer composite is viewed through a circular polarization filter, additional structures appear. Areas with metallization but no nematic liquid crystal layer appear black or at least dark, while areas with nematic liquid crystal have a bright appearance. Horizontal rotation of the circular polarization filter does not lead to a change in contrast.
[0009] Alternatively, these structures can also be made visible through a linear polarization filter (or by viewing the back side, i.e., through a "reverse" circular polarization filter). In this case, the metallized areas without a liquid crystal coating always appear bright. In areas additionally provided with nematic liquid crystal material, a dark impression can be produced by suitable horizontal rotation of the linear polarization filter, which contrasts with the areas without a nematic liquid crystal layer, or the areas have a bright appearance without a clear contrast with the surrounding metallized areas.
[0010] Liquid crystal layers made from solvent-containing formulations are generally difficult to achieve high resolution because relatively thick wet films must be printed, and due to the low viscosity of the formulation, the wet films can exhibit significant leveling or "flow" after printing.
[0011] In order to achieve the best contrast, the nematic liquid crystal layer forms a λ / 4 layer for a predetermined wavelength range. Due to the birefringence of the liquid crystal molecules, a certain layer thickness (on the order of 1 g / m 2 ), and therefore cannot be printed arbitrarily thin. Adding thickeners generally leads to a loss in the quality of the optical properties of the liquid crystal layer.
[0012] Optically anisotropic films in the light path can likewise reduce the achievable contrast, so that the release ability of the carrier film is advantageous. However, particularly thin UV-crosslinked (liquid crystal) layers generally have poor release ability.
[0013] Liquid crystal lacquers based on solvents usually require conditions that promote alignment in order to be able to exert their effect. In other processes, special alignment layers or alignment layers are used for this purpose. In particular, alignment layers are used which consist of linear photopolymers and are exposed to suitable radiation for alignment. Furthermore, the liquid crystal material can also be aligned with the aid of alignment layers, which are provided by finely structured layers or by layers that are oriented by the application of shear forces.
[0014] If, for example, an aligned embossed structure with two different orientations is coated with a nematic liquid crystal material, the resulting regionally different orientation of the liquid crystals makes it possible to make the embossed visual object visible in the form of positive or negative contrast through a linear polarization filter (by rotating the polarization filter). When a circular polarization filter is used, however, the visual object cannot be recognized.
[0015] It is also possible to use, for example, an anti-counterfeiting element with a latent image as described in WO2019 / 068655A1, in which the liquid crystal layer is based on a liquid crystal mixture containing a dichroic dye. The liquid crystal mixture is printed on an embossing lacquer layer provided with an embossing portion, and is embossed and oriented as part of an embossing process. The liquid crystals are oriented independently of each other at two interfaces. This forms, together with the dichroic dye, an anti-counterfeiting feature that displays different independent visual objects on both sides, which become visible by irradiation with linearly polarized light. EP 4129709A1 describes a similar method. However, double-sided embossing may cause uncured material to be rolled out, and thus produce undefined visual objects (or patterns).
[0016] Starting from this, the invention is based on the technical problem of providing a security element of the type mentioned in the introduction which avoids the disadvantages of the prior art, can be produced simply and cost-effectively and which, in addition to being attractive in appearance, also has increased protection against forgery.
[0017] The technical problem is solved by a security element for securing valuables, a data carrier and a method for producing a security element for securing valuables. Developments of the invention are the subject of the dependent claims.
[0018] According to the invention, in a security element of the type described in the invention, it is provided that the security element comprises a first embossing lacquer layer arranged on a carrier film, a partially present visual object layer based on a nematic liquid crystal material and a single-layer or multi-layer second embossing lacquer layer present over the entire surface.
[0019] The first embossing lacquer layer is provided with an embossing which has at least two regions, forming a second latent visual object, which have differently oriented oriented structures.
[0020] The visual object layer is arranged regionally in the form of a first latent visual object directly on the first embossing lacquer layer and overlapping with an area forming a second latent visual object, wherein the liquid crystal material is uniformly oriented in respectively different orientations through the visual object forming area in the form of the second latent visual object, so that the visual object composed of different oriented structures can be identified when observed through a polarizer.
[0021] The second embossing lacquer layer is provided with embossing portions for forming the micro-optical relief structure and the reflection-enhancing coating.
[0022] Layers composed of nematic liquid crystal material have polarization-dependent optical effects which are not perceptible to the naked eye but can be detected by auxiliary means, such as linear or circular polarization filters, and in particular can be made visible to an observer by such auxiliary means.
[0023] In an advantageous configuration, the liquid crystal material is oriented by the first visual object forming region at an angle to the orientation of the liquid crystal material by the second visual object forming region and has a different polarization effect than the first visual object forming region.
[0024] The first embossing lacquer layer is preferably present over the entire surface. The optical object advantageously has no structures that promote alignment of the liquid-crystal material, at least in the region of the optical object layer.
[0025] According to an advantageous embodiment, the surface of the first embossing lacquer layer facing the liquid-crystal material has fine grooves or grids in the region forming the visual object, by which the molecules of the liquid-crystal material are aligned.
[0026] The grooves or grids preferably have a period length of 0.2 μm to 2.0 μm, preferably 0.8 μm to 1.2 μm, and a profile depth of 50 nm to 600 nm, preferably 200 nm to 400 nm.
[0027] In the visible spectrum, the refractive index of the first and / or second embossing lacquer layer is advantageously between the orientation-dependent refractive index of the visual object layer. It is also advantageous if the refractive index of the orientation layer and the second embossing lacquer layer differs by no more than 0.1, in particular by no more than 0.05, in the visible spectrum.
[0028] The alignment structure can also be arranged only in the region of the visual object layer, in particular in register with the visual object layer.
[0029] In an advantageous embodiment, the first latent visual object comprises one or more first image elements, and the second latent visual object comprises a plurality of second image elements, wherein the first and second image elements comprise alphanumeric characters, patterns or codes. The second image elements are advantageously arranged in a grid.
[0030] The micro-optical relief structure is advantageously formed by a diffraction structure, in particular a one-dimensional or two-dimensional periodic diffraction structure, by a matte structure, a subwavelength structure, in particular a subwavelength grating or a moth-eye structure and / or by a non-diffractive microstructure, in particular an arrangement of micromirrors or microlenses.
[0031] The invention also includes a data carrier with a security element of the type described. The data carrier can be in particular a value document, such as a banknote, in particular a paper banknote, a polymer banknote or a film composite banknote, a stock, a bond, a certificate, a gift certificate, a check, a stamp, a tax stamp, a high-end admission ticket, or a certificate, such as a credit card, a bank card, a cash payment card, an authorization card, an identity card or a passport personal information page.
[0032] Finally, the present invention also provides a method for manufacturing the above-mentioned security element, in which
[0033] - applying a first embossing lacquer layer on the carrier film in order to form an orientation layer for achieving a uniform orientation of the liquid crystal material,
[0034] - providing the first embossing lacquer layer with an embossing portion to produce at least two regions with differently oriented oriented structures to form a second latent visual object, and curing the embossing lacquer,
[0035] - applying a visual object layer based on a nematic liquid crystal material in the form of a first latent visual object directly on the first embossing lacquer layer in regions and overlapping with regions forming a second latent visual object, wherein the liquid crystal material is oriented in a different uniform orientation by the orientation structure of the visual object forming region,
[0036] - hardening the liquid crystal material by applying radiation, and
[0037] A single-layer or multi-layer second embossing lacquer layer is applied over the entire surface of the carrier film with the optical object layer, the second embossing lacquer layer having embossing for producing the micro-optical relief structure and subsequently provided with a reflection-increasing coating.
[0038] According to an advantageous embodiment of the method, the first embossing lacquer layer is embossed without pre-curing. Preferably, a further lacquer layer is applied to the carrier film and at least partially cured before the first embossing lacquer layer is applied.
[0039] The liquid crystal material is advantageously dried physically before exposure to radiation. The liquid crystal material is preferably hardened by exposure to ultraviolet radiation.
[0040] Like the second embossing lacquer layer, the first embossing lacquer layer is preferably also applied over the entire surface.
[0041] Furthermore, it is particularly expedient if the second embossing lacquer layer is metallized and, if appropriate, demetallized in regions.
[0042] The first and / or second embossing lacquer layer and / or the optical object layer are particularly advantageously printed.
[0043] In further advantageous embodiments, one or more layers, in particular a primer layer, a thermosetting lacquer layer, a pressure-absorbing layer and / or a protective layer, are also applied to, in particular printed on, the second embossing lacquer layer. BRIEF DESCRIPTION OF THE DRAWINGS
[0044] The present invention is described in more detail below according to embodiments with reference to the accompanying drawings, which also disclose features important to the present invention and do not reflect the actual scale and proportion. These embodiments are for illustration only and should not be considered as limiting. For better understanding, the views in the figures are highly schematic and do not reflect the actual situation. To avoid repetition, the same or corresponding elements in different figures are provided with the same reference numerals and will not be described again. In the drawings:
[0045] Figure 1 A schematic diagram showing a banknote with an embedded security thread and an adhered transfer element,
[0046] Figure 2 A cross-sectional view showing the construction of a security element according to an embodiment of the present invention,
[0047] Figure 3a shows a top view of an embodiment of a security element having a structured alignment layer and a liquid crystal layer applied in the form of a visual object, and Figure 3b A magnified view of the oriented structure is shown,
[0048] Figures 4a to 4d Shows Figure 3a and Figure 3b A top view of the security element, Figure 4a Shown is observation without auxiliary tools, Figure 4b shows observation through a circular polarizer, Figure 4c shows viewing through a linear polarizer in a first position, Figure 4d Viewing through a linear polarizer is shown in a second position rotated relative to the first position. DETAILED DESCRIPTION
[0049] The invention is described here using the example of a security element for banknotes. Figure 1For this purpose, a schematic diagram of a banknote 10 is shown, which is equipped with two security elements 12 and 16 according to an embodiment of the present invention. The first security element forms a security thread 12, which protrudes in a certain window area 14 on the surface of the banknote 10 and is embedded in the interior of the banknote 10 in the area between these window areas. The second security element is composed of an adhesive transfer element 16 of any shape. The transfer element can be present in particular in the form of a patch or a strip, each with or without its own carrier layer. The security element 16 can also be designed in the form of a covering film, which is arranged on the window area or continuous opening of the banknote.
[0050] The following is based on Figure 2 The construction and production of the security element 20 according to the first exemplary embodiment are explained in more detail in FIG.
[0051] The security element 20 is based on a high-quality stretched PET carrier film 22, to which in the present exemplary embodiment a film consisting of a UV-curing lacquer 24 is applied over the entire surface. A UV-curing embossing lacquer 26 is applied over the entire surface of the (partially or completely cured) lacquer layer 24, which is embossed in a so-called "casting" process, preferably without pre-curing.
[0052] The local areas 28A and 28B are respectively provided with an orientation structure 32 on the entire surface. The orientation structure 32 is composed of, for example, a plurality of adjacently arranged parallel grooves, which realize the orientation of the liquid crystal molecules. These grooves have, for example, a period length of 0.2 μm to 2.0 μm and a cross-sectional depth of 200 nm to 600 nm. A smaller cross-sectional depth of, for example, 50 nm is also conceivable. The longitudinal direction of these grooves forms the orientation direction of the orientation structure.
[0053] Depend on Figure 2 , Figure 3a and Figure 3b As can be seen from the view of FIG. 28A, the orientation of the directional structure 32 is different in the local areas 28A and 28B. The local area 28A, for example, has a plurality of parallel grooves arranged vertically, while the local area 28B has a plurality of parallel grooves rotated 45° relative to the vertical direction (in FIG. Figure 3b In the embodiment described, the partial areas 28A are arranged in a grid-like manner in the form of a plurality of repeated image elements (“ 25 ”) in front of a background formed by the partial areas 28B with different alignment orientations (“wallpaper visual object”).
[0054] A thin layer 30 of nematic liquid crystal material is applied in the form of a visual object ("25"), in particular printed, on the orientation structure 32. To increase the sharpness of the edges, it may be advantageous to reduce the weight of the edges or edges of the visual object.
[0055] The visual object applied by means of the liquid crystal material can advantageously have a higher line width. The size of the visual object produced by the liquid crystal material 30 can in particular be selected such that it is significantly larger, preferably a multiple, than the size of the picture element formed by the partial regions 28A of the alignment structure 32 .
[0056] After the application of the liquid crystal layer 30, the nematic liquid crystals are uniformly oriented in the partial regions 28A and 28B corresponding to the dimensions of the oriented structures 32. Thus, the liquid crystal visual object layer 30 has regions corresponding to the partial regions 28A and 28B in which the orientation of the liquid crystals is different. The orientation thus obtained is fixed, if necessary, by crosslinking the liquid crystal layer 30 with ultraviolet radiation after physical drying for removing the solvent.
[0057] A single-layer or multi-layer embossing lacquer structure 34 is applied to the resulting layer sequence. A relief structure 38, such as a holographic structure, a micromirror structure or a subwavelength grating, is embossed into the embossing lacquer structure, and the relief structure 38 is subsequently provided with a reflection-enhancing coating, such as a metal coating 36. Recesses (not shown) can be introduced into the preferably vapor-deposited (e.g., aluminum) metal layer 36 by local demetallization, such as intaglio.
[0058] The grooves can be produced by means of an etching process or a cleaning process. In the case of a cleaning process, soluble cleaning pigments are printed before applying the metal layer, which are washed away together with the substances of the PVD layer deposited thereon after evaporation. In the case of an etching process, the PVD coating process is first carried out, and then the light-resistant coating is printed and structured. The PVD layer is then removed in unprotected locations by an etchant. The remaining light-resistant coating remains on the PVD layer or is removed by using a suitable solvent.
[0059] As an alternative to a metal layer, the relief structure 38 can also be provided with a layer of high refractive index. Examples of suitable materials with high refractive index are CaS, CrO2, ZnS, TiO2 or SiO2. x Likewise, thin-film elements with a color gradient effect can be applied to the relief structure 38 by means of a PVD coating process and optionally provided with recesses. Such thin-film elements are based in particular on viewing angle-dependent interference effects generated by multiple reflections of different sublayers of the element.
[0060] The resulting product can be designed to be heat-bonded directly by means of a primer layer and a heat-bonding lacquer and applied, for example, to a substrate such as paper. The carrier film 22 can be removed after application to the substrate or remain in the structure as a covering film. The latter design is used in particular when applying security elements that should cover continuous openings in the object to be protected from counterfeiting.
[0061] Before applying the thermosetting lacquer, further machine-readable and / or decorative layers can also be applied to the embossing lacquer layer 34, which may be partially demetallized, in particular overlapping the metallization 36. The thermosetting lacquer can also contain machine-readable characteristic materials, such as magnetic, conductive, phosphorescent or fluorescent substances.
[0062] Alternatively, the layer structure can also be further processed into a so-called patch or a single security element. For this purpose, other films, such as a PET film with a relatively low thickness (e.g. 6 μm), can be bonded to the layer structure. A support film can then be bonded to one side of the carrier film 22, which is used for the cutting or punching process that is performed when necessary, and a primer and a hot-pressing adhesive paint can be provided on the surface of the PET film. After pre-cutting or punching out the contour shape and forming the grid (Abgittern), the pre-fabricated single security element (patch) can be applied to the substrate. Patent document WO 2010 / 031543 A1, for example, describes a method for producing such a security element transfer material and a method for transferring a security element from a security element transfer material to a valuable item.
[0063] Figures 4a to 4d 4 shows a top view of a single security element 40 observed without auxiliary devices. When observed without auxiliary devices, the appearance of the security element 40 is an optically variable microstructure with a metallic luster, that is, a shield-shaped relief image 44 ( Figure 4a ).
[0064] When such a security element 40 is observed through a circular polarization filter 42, an image visual object 46 generated by the liquid crystal layer 30 can be seen and appears in the region in the form of bright characters "25" on a dark background ( Figure 4d ). Rotating the polarizing filter does not change the appearance.
[0065] When the security element is viewed through a linear polarizing filter (not shown) (or through a circular polarizing filter viewed from the back, i.e. "inverted"), further visual objects can be seen. In this case, the metal-coated area without liquid crystal layer appears bright, while for a first orientation of the linear polarizing filter in the area of the liquid crystal layer, the observer 48 perceives the local area 28B as dark large image elements 62 (large "25") and the area 28A as a bright visual object in the form of small image elements 64 (small "25") arranged in a grid-like manner ( Figure 4c ).
[0066] When the linear polarization filter is rotated, the relative brightness changes and is reversed in the region of the liquid crystal layer 30 when rotated by 45°, so that the small image element 72 can be seen as a dark visual object, the outline of which is predetermined by the region of the liquid crystal layer. The background corresponding to the partial area 28B appears to have no or less contrast than the regions of the security element 40 that are not provided with the liquid crystal layer 30 and that also appear bright ( Figure 4d ). Here, a small character is used to define a large character.
[0067] A particular advantage of the described embodiment is that it contains different latent visual objects that can be made visible by selecting different polarization filters as auxiliary means. In particular, in addition to "macroscopic", easily recognizable visual objects, very sharp "microscopic" visual objects can also be produced, since the resolution of the polarized visual objects is no longer determined solely by the printing accuracy, but also by the accuracy of the structuring.
[0068] In addition, the present invention provides a more visually attractive image than known liquid crystal based latent security features. If the security element is attractive to the observer, the observer is more likely to pay attention to the security element and the valuables equipped with the security element, thereby producing a greater anti-counterfeiting effect.
[0069] Since different visual objects can be confused due to the different sides of the (circular) polarization filter used to view the security element, the desired visual object can be stylized on the polarization filter used as verification medium on the upper side in each case. In the case of one side of a circular polarization filter that corresponds in effect to a linear polarization filter ("reverse" circular polarization filter) or in the case of a linear polarization filter, two visual objects that can be achieved by rotation can also be stylized.
[0070] For verification purposes, the incident and outgoing light must in principle be polarized, which can be achieved by providing polarization filters. However, other variants are also conceivable. For example, the light source illuminating the observation area can emit polarized light. In this case, the observer can use a polarization filter, for example in the form of polarized glasses, at any position between himself and the verification object.
[0071] The (optically important) working step in producing the security element begins with the first embossing. A visual object consisting of a nematic liquid crystal material 30 is applied, in particular printed, on the resulting orientation structure 32. The orientation structure 32 is filled with nematic liquid crystals in this region (the profile depth of the orientation structure is, for example, 200 nm, the thickness of the nematic liquid crystal layer is, for example, 1 μm). With a suitable choice of the refractive index of the UV embossing lacquer 26, the embossed structure disappears visually.
[0072] In the ideal case, the refractive indices of the adjacent materials are adapted to one another so that no sharp refractive index jumps occur, which would allow the oriented structured visual object to be continuously visible even without auxiliary means. Since the liquid crystal layer has an orientation-dependent refractive index, the UV embossing lacquer 26 is preferably selected such that its refractive index lies between the two orientation-dependent refractive indices of the liquid crystal layer 30.
[0073] Furthermore, if the recognizability of the nematic liquid crystal layer when observing the security element without auxiliary means is undesirable, the alignment quality of the orientation structures 32 in all regions 28A and 28B should be similar.
[0074] In the course of work after the application of the liquid crystal material, a UV embossing lacquer 34 is applied over the entire surface (in the present embodiment in two stages) in order to carry out the actual embossing, for example a hologram or a micro-mirror visual object 44. The nematic liquid crystal layer 30 is thus embedded between the UV lacquer layers. In addition to the nematic visual object, the embossing lacquer layer 34 is also applied directly to the existing embossing 32 or embossing lacquer 26. If the refractive indices are similar (i.e. differ by no more than 0.1, in particular by no more than 0.05 in the visible spectrum), the "aligned" embossing or orientation structure 32 also disappears visually here.
[0075] The liquid crystal layer 30 and the second embossing lacquer structure 34 can have different refractive indices. Ideally, the refractive indices are also adapted to one another in this case, so that no refractive index jumps occur.
[0076] The first impression can be limited to the area where the nematic liquid crystal material should or can be printed (register fluctuation). However, this limitation requires an inkjet printer operation when printing the liquid crystal material, which may lead to an increase in the scrap rate.
[0077] Independently of this, an overprint or nesting process may also be required to prevent the weld seam (embossing tool with aligned visual object and embossing tool with visual object with relief structure) from entering the visual object and causing problems due to accumulation.
[0078] Reference numerals list
[0079] 10 Banknotes
[0080] 12 Transfer element
[0081] 14 Window Area
[0082] 16 Security thread
[0083] 20 Anti-counterfeiting elements
[0084] 22 Carrier film
[0085] 24, 26 Embossed paint
[0086] 28A, 28B local area
[0087] 30 Liquid crystal layer
[0088] 32 Directed Structure
[0089] 34 Embossed paint
[0090] 36 Metallization
[0091] 38 relief structure
[0092] 40 Anti-counterfeiting elements
[0093] 42 Polarizer
[0094] 44 relief images
[0095] 46 Image Visual Objects
[0096] 48 Observer
[0097] 52 Substrate
[0098] 62, 64, 72 image components
Claims
1. An anti-counterfeiting element for providing security for valuables, the anti-counterfeiting element having a visual object layer based on a liquid crystal material, the liquid crystal material being designed and determined to form a latent visual object, characterized in that: the security element comprises a first embossing lacquer layer arranged on a carrier film, a partially present visual object layer based on a nematic liquid crystal material and a second embossing lacquer layer present over the entire surface in a single or multi-layered manner, wherein the first embossing lacquer layer is provided with an embossing portion, the embossing portion having at least two regions forming a second latent visual object, the at least two regions having directional structures with different orientations, wherein the visual object layer is arranged in regions directly on the first embossing lacquer layer in the form of a first latent visual object and overlapping with regions forming a second latent visual object, wherein the liquid crystal material is oriented uniformly in respectively different orientations by the visual object forming regions in the form of the second latent visual object, so that when viewed through a polarizer, visual objects consisting of different orientation structures can be recognized, - and wherein the second embossing lacquer layer is provided with an embossing for forming a micro-optical relief structure and a reflection-enhancing coating.
2. The anti-counterfeiting element according to claim 1, characterized in that: The liquid crystal material is oriented through the first visual object forming area at an angle to the orientation of the liquid crystal material through the second visual object forming area and has a different polarizing effect than the first visual object forming area.
3. The anti-counterfeiting element according to claim 1 or 2, characterized in that: The first embossing lacquer layer is present over the entire surface.
4. The security element according to at least one of claims 1 to 3, characterized in that The surface of the first embossing lacquer layer facing the liquid crystal material has fine grooves or grids in the region of visual object formation, by which the molecules of the liquid crystal material are oriented.
5. The anti-counterfeiting element according to claim 4, characterized in that: The grooves or grids have a period length of 0.2 μm to 2.0 μm, preferably 0.8 μm to 1.2 μm, and a profile depth of 50 nm to 600 nm, preferably 200 nm to 400 nm.
6. The security element according to at least one of claims 1 to 5, characterized in that In the visible spectrum, the refractive index of the first and / or second embossing lacquer layer lies between the orientation-dependent refractive indices of the optical object layers.
7. The security element according to at least one of claims 1 to 6, characterized in that In the visible spectrum, the refractive indices of the orientation layer and the second embossing lacquer layer differ by no more than 0.1, in particular by no more than 0.
05.
8. The security element according to at least one of claims 1 to 7, characterized in that The first latent visual object comprises one or more first image elements and the second latent visual object comprises a plurality of second image elements, wherein the first and second image elements comprise alphanumeric characters, patterns or codes, wherein the second image elements are preferably arranged in a grid.
9. The security element according to at least one of claims 1 to 8, characterized in that The micro-optical relief structure is formed by a diffractive structure, in particular a one-dimensional or two-dimensional periodic diffractive structure, by a matte structure, a subwavelength structure, in particular a subwavelength grating or a moth-eye structure and / or by an arrangement of non-diffractive microstructures, in particular micromirrors or microlenses.
10. A data carrier having a security element according to any one of claims 1 to 9, wherein: The data carrier is in particular a value document or a certificate.
11. A method for manufacturing a security element for providing security for valuables, the security element having a visual object layer consisting of a liquid crystal material designed and determined to form a latent visual object, wherein: In the method - applying a first embossing lacquer layer on the carrier film in order to form an orientation layer for achieving a uniform orientation of the liquid crystal material, - providing the first embossing lacquer layer with an embossing portion to produce at least two regions with differently oriented oriented structures to form a second latent visual object, and curing the embossing lacquer, - applying a visual object layer based on a nematic liquid crystal material in the form of a first latent visual object directly on the first embossing lacquer layer in regions and overlapping with regions forming a second latent visual object, wherein the liquid crystal material is oriented in a different uniform orientation by the orientation structure of the visual object forming region, - hardening the liquid crystal material by applying radiation, and A single-layer or multi-layer second embossing lacquer layer is applied over the entire surface of the carrier film with the optical object layer, the second embossing lacquer layer being provided with embossing for producing the micro-optical relief structure and subsequently provided with a reflection-increasing coating.
12. The method according to claim 11, characterized in that The first embossing lacquer layer is embossed without precuring, wherein a further lacquer layer is preferably applied to the carrier film and at least partially cured before the first embossing lacquer layer is applied.
13. The method according to claim 11 or 12, characterized in that: The liquid crystal material is physically dried before being exposed to radiation.
14. The method according to at least one of claims 11 to 13, characterized in that The first embossing lacquer layer is applied over the entire surface.
15. The method according to at least one of claims 12 to 14, characterized in that The first and / or second embossing lacquer layer and / or optical object layer is printed.
Citation Information
Patent Citations
Semi-finished product, security element, methods of producing them and document of value
EP4129709A1
Sheeting and methods for the production thereof
WO2005105475A1
Security element transfer material with multi-layered carrier
WO2010031543A1
Two-sided transparent window feature with dichroic dyes
WO2019068655A1