Combination design method and system for enclosure material of biosafety cryoelectron microscope chamber

By evaluating environmental characteristics and building a multi-layer material combination solution, the problem of magnetic field shielding and sound insulation materials combination in the design of high-end electron microscope chambers is solved, and effective magnetic field shielding and sound insulation of biosafety cryoelectron microscope chambers is achieved, reducing the design Cost and trial and error risks.

CN118965498APending Publication Date: 2024-11-15CHINA ELECTRONICS SYST ENG NO 2 CONSTR
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410964363.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-18
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

In the design of enclosure materials for high-end electron microscope chambers, the combination design of magnetic field shielding and sound insulation materials has problems of trial and error risks and uncontrollable costs, which is difficult to meet the strict requirements of biosafety cryo-electron microscope chambers.

Method used

By evaluating the environmental characteristics of the electron microscope chamber, a combination sequence and thickness scheme of multi-layer shielding layer materials was constructed, and a biosafety protective layer and magnetic shielding material was combined to calculate a solution that satisfies shielding performance and sound insulation performance, and the material combination was optimized through the evaluation module. , reduce trial and error risks and costs.

Benefits of technology

It realizes effective magnetic field shielding and sound insulation in the biosafe cryo-electron microscope chamber, reduces the risk and cost of design trial and error, and ensures the safe operation of high-end electron microscopes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118965498A_ABST
    Figure CN118965498A_ABST
Patent Text Reader

Abstract

According to the combined design method for the enclosure material of the biosafety cryoelectron microscope chamber, provided by the invention, the shielding effectiveness SE required by the to-be-designed electron microscope chamber is calculated on the basis of an environment magnetic field where the to-be-designed electron microscope chamber is located and indoor magnetic field intensity required by a shielding chamber; obtaining thickness combination schemes of all the metal materials meeting the shielding effectiveness requirement based on SE calculation, and finally judging whether a sound insulation material needs to be added in each thickness combination scheme based on the sound insulation requirement R0 of the electron microscope chamber; the final alternative schemes obtained through calculation of the shielding effectiveness SE and the sound insulation requirement R0 are obtained through calculation according to the actual performance of each material without depending on the individual experience of technicians, and it is ensured that all the final alternative schemes can specifically meet the harsh magnetic shielding and sound insulation requirements of a high-end electron microscope.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of engineering construction technology, and in particular to a method and system for designing enclosure materials for a biosafety cryo-electron microscope room. Background Art

[0002] The use of high-end electron microscopes to observe high-risk and high-hazard bioactive factors is an important foundation and requirement for cutting-edge research in the fields of life sciences and public health safety. However, in urban environments, high-end electron microscopes are susceptible to interference from environmental magnetic fields and noise, which affects imaging accuracy. At this time, it is necessary to use the enclosure materials of the electron microscope room and their combination methods to meet the requirements of biosafety protection, magnetic field shielding, and sound insulation and noise reduction to ensure experimental research using high-end electron microscopes. High-level biosafety laboratories have unique requirements for the surface layer of the enclosure structure. The wall and ceiling materials must be easy to clean and disinfect, corrosion-resistant, dust-free, crack-free, smooth and waterproof, and the surface coating should have antistatic properties. In addition, the coupling relationship between magnetic field shielding and sound insulation and noise reduction must also be effectively addressed in the combination of multi-layer materials.

[0003] However, in current engineering practices, magnetic field shielding materials, sound insulation materials and their thickness are mostly designed based on the engineering experience of designers. This is because there is a multi-objective optimization game relationship between the performance, thickness, cost and structural load-bearing of the enclosure materials of the biosafety cryo-electron microscope room. When designing, it is necessary to ensure that the design results meet the requirements of biosafety protection while specifically meeting the stringent magnetic shielding and sound insulation requirements of high-end electron microscopes, so that the enclosure material combination scheme is more reasonable, economical, safe and durable. This leads to a great risk and cost of trial and error during the design period, depending on the level of ability of the designers themselves. Summary of the invention

[0004] In order to solve the problem of trial and error risk and uncontrollable cost during the design of multi-layer enclosure materials for high-end electron microscope rooms in the prior art, the present invention provides a combination design method for enclosure materials for biosafety cryo-electron microscope rooms, which can assist technicians in completing the design and effectively reduce the trial and error risk and cost during the design period. At the same time, the application also discloses a combination design system for enclosure materials for biosafety cryo-electron microscope rooms.

[0005] The technical solution of the present invention is as follows: a method for designing a combination of enclosure materials for a biosafety cryo-electron microscope room, characterized in that it comprises the following steps:

[0006] S1: Evaluate and test the built environment characteristics based on the specific construction site of the electron microscope room to be designed;

[0007] The environmental characteristics include: high and low frequency distribution of magnetic field, noise source and frequency distribution corresponding to the noise source;

[0008] S2: The combination order of various materials in the multi-layer shielding layer materials required to construct the electron microscope room to be designed;

[0009] The material combination sequence of the multi-layer shielding layer materials is set from outside to inside in sequence as follows: biosafety protection layer a, high-frequency suppression metal material, low-frequency suppression metal material and biosafety protection layer b;

[0010] S3: Calculate the shielding effectiveness SE required for the electron microscope room to be designed based on the environmental magnetic field of the electron microscope room to be designed and the indoor magnetic field strength required by the shielding room;

[0011] S4: constructing a thickness combination scheme of metal materials in the multi-layer shielding layer material;

[0012] The metal material includes: a high-frequency suppression metal material and a low-frequency suppression metal material;

[0013] According to the performance parameters of each metal material included in the multi-layer shielding layer material, calculate the thickness combination scheme of all metal materials that meet the shielding effectiveness SE requirements;

[0014] The solution obtained by combining each of the thickness combination solutions with the biosafety protection layer a and the biosafety protection layer b is recorded as: the alternative solution of the multi-layer shielding layer material;

[0015] S5: construct a sound insulation solution for each of the alternative solutions;

[0016] a1: Confirm the indoor noise level R0 required for the electron microscope room to be designed and the current environmental noise level R1;

[0017] a2: Calculate the total sound insulation performance R achieved by each alternative solution W ;

[0018] a3: Confirm the sound insulation performance R corresponding to each alternative solution w Whether the sound insulation requirements can be met;

[0019] If R1-R W ≤R0, the corresponding alternative plan will not be changed, the alternative plan will be recorded as the final alternative plan, and step S6 will be executed;

[0020] Otherwise, execute step a4;

[0021] a4: adding sound insulation material between the low-frequency suppression metal material and the biosafety protection layer b in each of the alternative solutions, so that the multi-layer shielding material corresponding to the alternative solution meets the noise shielding requirements, and obtaining the final alternative solution; executing step S6;

[0022] S6: Obtain all the final alternative solutions and number them;

[0023] S7: Setting evaluation dimensions and scoring criteria, evaluating and comparing all the final alternatives, and obtaining the optimal design solution corresponding to the electron microscope room to be designed;

[0024] The evaluation dimensions include: material compatibility, material stability, comprehensive construction cost, and structural and space utilization.

[0025] It is further characterized by:

[0026] The shielding effectiveness SE is calculated as follows:

[0027]

[0028] Among them, SE is the shielding effectiveness, E1 is the magnetic field strength of the environment without a shielding room, and E0 is the magnetic field strength required in the shielding room;

[0029] The calculation method of the thickness combination scheme is:

[0030]

[0031] Among them, SE is the shielding effectiveness required for the electron microscope room to be designed, n is the total number of metal materials included in the multi-layer shielding material, i is the i-th metal material, U i is the relative magnetic permeability of the i-th metal material, G i is the conductivity of the ith metal material relative to copper, t i is the thickness of the i-th metal material, f is the frequency of the environmental magnetic field, and r is the distance from the field source to the shield;

[0032] In step a2, the sound insulation performance R corresponding to each of the alternative solutions W Calculation method of

[0033]

[0034] Where n is the total number of materials included in the alternatives, i is the i-th material, fs is the ambient noise frequency; t i is the thickness of the i-th material; ρ i is the density of the i-th material;

[0035] In step a4, the design method of the sound insulation material layer to be added in the final alternative solution specifically includes the following steps:

[0036] b1: Calculate the sound insulation value R that the sound insulation material in the final alternative solution needs to meet;

[0037] R=R1-R0-Rw ;

[0038] Among them, R is the sound insulation of the added sound insulation material; R1 is the current ambient noise level without a shielding body; R0 is the indoor noise level required for the electron microscope room to be designed; R W The total sound insulation achieved for the known alternative solutions;

[0039] b2: Calculate the scheme of the sound insulation material;

[0040]

[0041] Where m is the total number of sound insulation material layers that need to be added; j is the jth non-metallic sound insulation material; ρ j is the density of the jth non-metallic sound insulation material; t i is the thickness of the jth non-metallic sound insulation material; T is the thickness of all air interlayers included in the multi-layer shielding material;

[0042] The implementation methods of various materials in the multi-layer shielding layer material include:

[0043] The biosafety protection layer a is realized based on a corrosion-resistant and easy-to-clean stainless steel surface or a color-coated steel surface metal sandwich panel;

[0044] The high-frequency suppression metal material is realized based on a high-conductivity metal material;

[0045] The low-frequency suppression metal material is realized based on a high magnetic permeability metal material;

[0046] The sound insulation material is realized based on sound insulation and shielding filling materials;

[0047] The biosafety protection layer b is realized based on a corrosion-resistant and easy-to-clean stainless steel surface or a color-coated steel surface metal sandwich panel.

[0048] A biosafety cryo-electron microscope room enclosure material combination design system, characterized in that it includes: a construction module, a magnetic shielding acquisition module, a sound insulation module and an evaluation module;

[0049] The construction module is used to detect the environmental characteristics of the construction site where the electron microscope room to be designed is located, and the combination sequence of metal materials in the multi-layer shielding layer materials required by the electron microscope room to be designed;

[0050] The magnetic shielding acquisition module stores a shielding effectiveness calculation model, reads the data stored in the construction module, and calculates all thickness combination schemes of metal materials that meet the shielding effectiveness SE requirements according to the performance parameters of each metal material included in the multi-layer shielding layer material; each thickness combination scheme is combined with the biosafety protection layer a and the biosafety protection layer b to obtain a solution, which is recorded as: an alternative solution of the multi-layer shielding layer material, and all the calculated alternative solutions are sent to the sound insulation module;

[0051] The sound insulation module stores a sound insulation calculation model, and after reading the data stored in the construction module, the sound insulation performance R is calculated for each of the alternative solutions input by the magnetic shielding acquisition module. w , and determine whether to add sound insulation materials. For the alternative solution that requires the addition of sound insulation materials, the sound insulation materials are set between the low-frequency suppression metal material and the biosafety protection layer b; finally, the final alternative solution that satisfies both the magnetic field strength shielding requirements and the sound shielding requirements is sent to the evaluation module;

[0052] The evaluation module stores preset value dimensions and scoring criteria, and calculates the scores of all the schemes corresponding to the electron microscope room to be designed according to the scores corresponding to all the final alternative schemes.

[0053] It is further characterized by:

[0054] The scoring calculation formula pre-stored in the evaluation module is:

[0055]

[0056] Among them, is the average material fit among the final alternatives, is the average stability score, is the average comprehensive construction cost score of the material. The scores for structure and space utilization were average.

[0057] The present invention provides a method for designing a combination of enclosure materials for a biosafety cryo-electron microscope room, which comprises the following steps: the material combination sequence of the multi-layer shielding layer materials is arranged from outside to inside in order: a biosafety protection layer a, a high-frequency suppression metal material, a low-frequency suppression metal material and a biosafety protection layer b; if sound insulation material is required, the sound insulation material is arranged between the low-frequency suppression metal material and the biosafety protection layer b to ensure that both indoors and outdoors meet the biosafety protection requirements; wherein, the high-frequency suppression metal material is arranged on the outer layer of the low-frequency suppression metal material, which can not only make full use of the magnetic field generated by the high-conductivity material to offset the external high-frequency magnetic field, but also protect the inner layer of the high-permeability metal material from magnetization, thereby improving the performance of the electron microscope room maintenance material and extending the service life; in the present application, based on the electron microscope room to be designed, The shielding effectiveness SE required for the electron microscope room to be designed is calculated based on the ambient magnetic field and the indoor magnetic field strength required by the shielding room. Based on SE, the thickness combination schemes of all metal materials that meet the shielding effectiveness requirements are calculated. Finally, based on the sound insulation requirement R0 of the electron microscope room, it is determined whether sound insulation materials need to be added to each thickness combination scheme. The final alternative scheme calculated by the shielding effectiveness SE and the sound insulation requirement R0 does not need to rely on the individual experience of the technicians, but is obtained after calculation based on the actual performance of each material, ensuring that all the final alternative schemes can specifically meet the demanding magnetic shielding and sound insulation requirements of high-end electron microscopes. Finally, through the preset evaluation dimensions, the trade-off game is involved from factors such as material performance, cost, and structural load-bearing, and a multi-objective optimization best solution is obtained. The technical solution of this application can assist technicians in completing the design and effectively reduce the trial and error risks and costs during the design period. BRIEF DESCRIPTION OF THE DRAWINGS

[0058] Figure 1 A schematic diagram of the system module for the design of the enclosure material combination of the biosafety cryo-EM chamber in this application;

[0059] Figure 2 It is a schematic diagram of the structure of multi-layer shielding layer materials;

[0060] Figure 3 Implementation example 1 for enclosure material combination;

[0061] Figure 4 This is example 2 of implementing the enclosure material combination. DETAILED DESCRIPTION

[0062] Usually, high-end electron microscope rooms with biosafety protection requirements should generally be located on solid ground, and the ceiling should be supported on the main structure of the building by hangers. Biosafety protection requirements are that the wall and ceiling materials should be easy to clean and disinfect, corrosion-resistant, dust-free, crack-free, smooth and waterproof, and the surface coating should have antistatic properties. This application is a technical solution for the design process of multi-layer maintenance materials for this type of electron microscope room. The specific construction methods of the ceiling support structure, floor materials, shielding body grounding, door and window openings, etc. of the electron microscope room are based on existing technologies and are not elaborated in this application.

[0063] like Figure 1-2 As shown, the present invention includes a method for designing a combination of enclosure materials for a biosafety cryo-electron microscope room, which includes the following steps.

[0064] S1: Evaluate and test the built environment characteristics based on the specific construction site of the electron microscope room to be designed;

[0065] Environmental characteristics include: high- and low-frequency distribution of magnetic field, noise sources and frequency distribution corresponding to noise sources. Specific environmental characteristics detection methods are implemented based on existing technologies. When evaluating and detecting the high- and low-frequency distribution of magnetic field in the surrounding built environment, noise sources and their frequency distribution, appropriate advance planning should be carried out, taking into account both high- and low-frequency magnetic fields, and retaining a certain amount of design redundancy to prevent the enclosure structure from failing to meet the shielding requirements due to changes in the magnetic field environment and acoustic environment after new construction or additions.

[0066] S2: The combination order of various materials in the multi-layer shielding layer materials required to construct the electron microscope room to be designed;

[0067] The material combination sequence of the multi-layer shielding layer material is set from the outside to the inside as follows: biosafety protection layer a, high-frequency suppression metal material, low-frequency suppression metal material and biosafety protection layer b.

[0068] Figure 2 This is a combination diagram of the enclosure materials for a high-level biosafety cryo-electron microscope laboratory, where 1. Biosafety protection layer a; 2. High-frequency magnetic shielding layer (high-frequency suppression metal material); 3. Low-frequency magnetic shielding layer (low-frequency suppression metal material); 3. Sound insulation layer; 4. Biosafety protection layer b.

[0069] Due to the protection requirements of biosafety laboratories, the biosafety protection layer has specific corrosion resistance, easy cleaning and airtightness requirements, and must meet the biosafety protection requirements both indoors and outdoors (laboratory corridor part). In terms of the order of high conductivity materials (used to suppress high-frequency magnetic fields) and high magnetic permeability materials (used to suppress low-frequency magnetic fields), the shielding principle of high-frequency magnetic fields is to use the eddy current reverse magnetic field generated in high-conductivity, low-resistivity metal materials to form a counteracting effect on external electromagnetic waves, thereby achieving the shielding effect. Eddy currents will generate heat in conductors, resulting in energy loss. In order to make the generated eddy current reverse magnetic field directly (offset) the high-frequency magnetic field generated by the field source (that is, the magnetic field that needs to be suppressed), it should be set in the outermost layer. The shielding principle of low-frequency magnetic fields is to use high-magnetic permeability materials to form a low magnetic resistance path, change the direction or range of the magnetic lines of force, and make the magnetic lines of force pass through the inside of the material to play an isolation role. In addition, high-conductivity materials are not easy to magnetize, high-magnetic permeability materials are easy to magnetize, and high-frequency magnetic fields are more likely to cause metal materials to be magnetized than low-frequency magnetic fields, so they can also play a protective role for the inner layer of high-magnetic permeability materials. Therefore, placing the high magnetic permeability material on the outside in this application has two technical effects: one is to make full use of the magnetic field generated by the high conductivity material to offset the external high-frequency magnetic field; the other is to protect the inner layer of high magnetic permeability metal material from magnetization (or delay its magnetization).

[0070] At the same time, multi-layer composite metal materials will enhance the reflection loss of electromagnetic waves between materials due to the different wave impedances (Zw values) between materials, thus achieving the effect of shielding the magnetic field. From this perspective, there are two meanings. First, the composite of multi-layer metal materials should be given priority to enhance the magnetic field shielding effect. Second, magnetic field shielding materials should be placed adjacent to each other first. Therefore, this application places high-conductivity metal materials and high-magnetic permeability metal materials adjacent to each other in turn.

[0071] In practical applications, the actual implementation of various materials in the multi-layer shielding layer includes:

[0072] The biosafety protection layer a is realized based on corrosion-resistant and easy-to-clean stainless steel surface or color-coated steel surface metal sandwich panel;

[0073] High frequency suppression metal materials are realized based on high conductivity metal materials;

[0074] Low frequency suppression metal materials are realized based on high magnetic permeability metal materials;

[0075] Sound insulation materials are realized based on sound insulation and shielding filling materials;

[0076] The biosafety protection layer b is realized based on a metal sandwich panel with a corrosion-resistant and easy-to-clean stainless steel surface or a color-coated steel surface.

[0077] Usually, biosafety protection layer a and biosafety protection layer b are 100mm thick or 50mm thick stainless steel or color steel metal sandwich panels, and the core material should be greater than 100kg / m 3 The non-combustible inorganic material with sound insulation function, the inner and outer protective layers can choose sandwich panels with different surface layers according to needs, and the sandwich panels are connected into a whole by seam welding or staggered bonding.

[0078] High conductivity materials include aluminum plates, copper plates, or zinc-plated or silver-plated composite metal materials. The thickness should be based on skin depth and mechanical strength.

[0079] The formula for calculating skin depth is:

[0080] Among them, σ represents skin depth, μ represents magnetic permeability, γ represents conductor conductivity, and f represents the frequency of magnetic field. The seams are welded together to form a whole, and the welds are leak-checked and demagnetized.

[0081] High magnetic permeability materials include low carbon steel plates, silicon steel sheets, pure iron plates, Permalloy and other materials, which are welded together to form a whole, and the welds are leak-checked and demagnetized. High-frequency magnetic shielding metal materials and low-frequency magnetic shielding metal materials are isolated by an insulating layer (PVC, etc.), sprayed insulating paint or insulating support structure. Usually, sound insulation materials include inorganic non-combustible materials such as rock wool, glass wool, polyurethane, cement fiberboard, blocks or concrete.

[0082] In selecting the specific material for the enclosure structure, the designers comprehensively consider factors such as durability, cost and construction, analyze each material one by one, select one or several as alternatives, and then perform subsequent calculations according to the method proposed in this application.

[0083] For example, for the outer protective layer, 100mm thick color steel surface (0.5mm thick on both sides) rock wool sandwich panel is preferred, and the inner protective layer is 100mm thick stainless steel surface (3mm thick on both sides) rock wool sandwich panel, which are welded together into a whole, and the welds are leak-checked and demagnetized.

[0084] S3: Calculate the shielding effectiveness SE required for the electron microscope room to be designed based on the environmental magnetic field of the electron microscope room to be designed and the indoor magnetic field strength required by the shielding room;

[0085] Shielding effectiveness SE is calculated as follows:

[0086]

[0087] Among them, SE is the shielding effectiveness, E1 is the magnetic field strength of the environment without a shielding room, and E0 is the magnetic field strength required in the shielding room.

[0088] S4: Construct a thickness combination scheme of metal materials in multi-layer shielding layer materials;

[0089] Metal materials include: high frequency suppression metal materials and low frequency suppression metal materials;

[0090] According to the performance parameters of each metal material included in the multi-layer shielding layer material, the thickness combination scheme of all metal materials that meet the shielding effectiveness SE requirements is calculated;

[0091] The solution obtained by combining each thickness combination scheme with biosafety protection layer a and biosafety protection layer b is recorded as: alternative scheme of multi-layer shielding layer material.

[0092] The calculation method of thickness combination scheme is:

[0093]

[0094] Among them, SE is the shielding effectiveness required for the electron microscope room to be designed, n is the total number of metal materials included in the multi-layer shielding material, i is the i-th metal material, U i is the relative magnetic permeability of the i-th metal material, G i is the conductivity of the ith metal material relative to copper, t i is the thickness of the i-th metal material, f is the frequency of the environmental magnetic field, r is the distance from the field source to the shielding body, and r is usually a fixed value of ≥1.7m according to the acceptance rules of the electron microscope room.

[0095] The thickness combination scheme calculated in this method covers the thickness of different types of metal materials t i The equation is not about the number of layers of metal plates. Because in practical applications, the thickness of each metal plate that can be used for magnetic shielding is not fixed. Therefore, this method actually calculates the thickness of each metal material. Designers can decide how many layers of material plates to use for each metal material based on the total thickness of each metal material and the thickness of the plate actually supplied by the manufacturer to ensure that the shielding effectiveness requirements of the electron microscope room can be met.

[0096] Related research points out that the combination of metal materials with different wave impedances has better magnetic field shielding performance than a single metal material. Therefore, in this embodiment, the magnetic shielding module uses a combination of copper plate + low-carbon steel plate and a combination of pure aluminum plate + pure iron plate + silicon steel sheet, and the thickness of each layer of metal material is calculated according to the above formula under the given magnetic field shielding requirements.

[0097] S5: Construct the sound insulation plan for each alternative;

[0098] a1, confirm the indoor noise level R0 required for the electron microscope room to be designed and the current environmental noise level R1;

[0099] a2: Calculate the total sound insulation performance R achieved by each alternative solution W ;

[0100] In step a2, the sound insulation performance R corresponding to each alternative solution W Calculation method of

[0101]

[0102] Where n is the total number of materials included in the alternatives, i is the i-th material, fs is the ambient noise frequency; t i is the thickness of the i-th material; ρ i is the density of the ith material.

[0103] For example, the sound insulation module respectively increases the selection of finished rock wool board or polyurethane sound insulation board, and the thickness of the listed non-metallic sound insulation material is calculated according to the above formula under the condition of given noise shielding requirements.

[0104] a3: Confirm the sound insulation performance R corresponding to each alternative solution w Whether the sound insulation requirements can be met;

[0105] If R1-R W ≤R0, the corresponding alternative plan does not make any changes, the alternative plan is recorded as the final alternative plan, and step S6 is executed;

[0106] Otherwise, go to step a4.

[0107] a4: Add sound insulation material between the low-frequency suppression metal material and the biosafety protection layer b in each alternative solution, so that the multi-layer shielding material corresponding to the alternative solution meets the noise shielding requirements, and obtain the final alternative solution; execute step S6.

[0108] The sound insulation material is placed between the low-frequency suppression metal material and the biosafety protection layer b because the sound insulation material is usually denser and heavier. If it is placed outside the above-mentioned high conductivity material, it may squeeze such metal materials (high conductivity materials such as aluminum and copper have low mechanical strength and are generally thinner), causing deformation of the metal material. The thicker the high magnetic permeability material is, the better the shielding effect and the better the material stiffness (such as pure iron plate, silicon steel sheet, etc.). Therefore, the sound insulation material adjacent to the high magnetic permeability material is better than the adjacent high conductivity material in protecting the metal shielding material. In addition, placing the sound insulation material closer to the inside of the electron microscope is more conducive to exerting its sound insulation performance in terms of reliability and protecting the electron microscope use space from noise interference.

[0109] The design method of the sound insulation material layer to be added in the final alternative solution specifically includes the following steps:

[0110] b1: Calculate the sound insulation R that the sound insulation material in the final alternative solution needs to meet;

[0111] R=R1-R0-R w ;

[0112] Among them, R is the sound insulation of the added sound insulation material; R1 is the current ambient noise level without a shielding body; R0 is the indoor noise level required for the electron microscope room to be designed; R W The total sound insulation achieved for the known alternative solutions;

[0113] b2: Calculation scheme of sound insulation material layer;

[0114]

[0115] Where m is the total number of sound insulation material layers that need to be added; j is the jth non-metallic sound insulation material; ρ j is the density of the jth non-metallic sound insulation material; t i is the thickness of the jth non-metallic sound insulation material; T is the thickness of all air interlayers included in the multi-layer shielding material.

[0116] The air sound insulation layer in the multi-layer shielding material can be set as needed. The thickness T of the air layer should be less than or equal to 100mm, and its sound insulation is approximately calculated as 0.1T.

[0117] S6: Obtain all final alternatives, sort them and number them.

[0118] Because the sorting and numbering are for subsequent scoring and evaluation, it is necessary not only to sort and number the final alternatives, but also to sort and number each material in the final alternatives to ensure that each material and each final alternative has a unique number.

[0119] For example: the yth scheme of sound insulation material corresponding to the xth thickness combination scheme.

[0120] S7: Set evaluation dimensions and scoring criteria, evaluate and compare all final alternatives, and obtain the optimal design solution corresponding to the electron microscope room to be designed;

[0121] Evaluation dimensions include: material fit, material stability, comprehensive construction cost, and structural and space utilization.

[0122] In the evaluation module, examples of pre-stored evaluation dimensions and scoring criteria are shown in Table 1 below.

[0123] Table 1: Evaluation dimensions and scoring criteria examples

[0124]

[0125] The purpose of setting the evaluation dimensions in this application is to provide a method to comprehensively consider and quantify the impact of multiple factors, and introduce multiple subjects to fully evaluate the availability, feasibility and other characteristics of each combination scheme listed. Factors such as material performance, cost, and structural load-bearing involve trade-offs and constitute a multi-objective optimization relationship. For example, the magnetic permeability of Permalloy is higher than that of pure iron plate, but its cost is also higher; copper has higher electrical conductivity than aluminum, but its cost is also higher and its durability may be worse.

[0126] The enclosure material combination sequence of this application not only meets the requirements of biosafety protection, but also has the beneficial effects of giving full play to the technical performance of each material layer, improving the durability of the enclosure materials, etc. This application determines the required materials and their thicknesses based on the magnetic field characteristics and noise characteristics of the construction environment according to a proven effective formula. The resulting enclosure material combination scheme is highly adaptable and reduces the risk and cost of trial and error. The evaluation module set up in this application introduces multiple substantial participants in the project construction to enhance the rationality, economy and safety of the multi-layer enclosure material combination design output by this application.

[0127] The present application also includes a system for implementing the above-mentioned biosafety cryo-electron microscope room enclosure material combination design method, which includes: a construction module, a magnetic shielding acquisition module, a sound insulation module and an evaluation module.

[0128] The construction module is used to detect the environmental characteristics of the construction site where the electron microscope room to be designed is located, and the combination sequence of metal materials in the multi-layer shielding layer materials required by the electron microscope room to be designed;

[0129] The shielding effectiveness calculation model is stored in the magnetic shielding acquisition module, and the data stored in the construction module is read. According to the performance parameters of each metal material included in the multi-layer shielding layer material, all thickness combination schemes of metal materials that meet the shielding effectiveness SE requirements are calculated; each thickness combination scheme is combined with the biosafety protection layer a and the biosafety protection layer b to obtain a scheme, which is recorded as: an alternative scheme for the multi-layer shielding layer material, and all the calculated alternative schemes are sent to the sound insulation module;

[0130] The sound insulation module stores the sound insulation calculation model. After reading the data stored in the construction module, the sound insulation performance R is calculated for each alternative scheme passed in by the magnetic shielding acquisition module. w , and determine whether to add sound insulation materials. For the alternative solution that requires the addition of sound insulation materials, the sound insulation materials are set between the low-frequency suppression metal material and the biosafety protection layer b; finally, the final alternative solution that meets both the magnetic field strength shielding requirements and the sound shielding requirements is sent to the evaluation module;

[0131] The evaluation module stores preset value dimensions and scoring criteria, and calculates the scores of all schemes corresponding to the electron microscope room to be designed according to the scores corresponding to all final alternative schemes.

[0132] The score calculation formula stored in the evaluation module is:

[0133]

[0134] Among them, is the average material fit among the final alternatives, is the average stability score, is the average comprehensive construction cost score of the material. The scores for structure and space utilization were average.

[0135] Based on the metal shielding materials and their thicknesses and the non-metallic sound insulation materials and their thicknesses output by the sound insulation module, m alternative solutions are formed accordingly. The m thickness combination solutions are scored in turn according to the given evaluation dimensions and scoring criteria (see Table 1), and the Km value is calculated after scoring.

[0136] The specific evaluation process can be achieved by presetting the scores corresponding to each dimension in the evaluation module of the system, or presetting a trained scoring model based on a machine learning model, using the existing maintenance materials of the electron microscope room and the corresponding scores as historical data for training to obtain a trained scoring model; then inputting the thickness combination scheme calculated based on this method into the trained scoring model, and automatically calculating the scores of each dimension corresponding to each scheme through a preset given program. Finally, the scores of each dimension corresponding to each scheme and the final km value are displayed to the designer.

[0137] However, the construction of a biosafety cryo-EM room is usually a renovation project. The evaluation dimensions in Table 1 cover the owner, biosafety expert, structural engineer, material supplier, and engineering construction party. In the specific implementation, in order to better refer to the opinions of experts from all parties, multiple experts from all parties can be introduced to participate in manual scoring, and the scores of each expert can be input into the evaluation module to automatically calculate the final score to enhance the rationality, economy, and safety of the design. Design based on this method can effectively reduce the trial and error cost and comprehensive construction cost of this type of engineering construction, avoid rework, work delays, and equipment waste, and ensure the safe operation of high-end electron microscopes.

[0138] In the evaluation module, according to the formula Calculate the scores of all final alternatives and compare the Km values. The larger the value, the more reasonable, economical and safe the multi-layer enclosure material solution is under given conditions. is the average material compatibility of the combination (scored by the owner and biosafety experts, reflecting the owner's preference), is the average stability score (scored by material experts), is the average value of the comprehensive construction cost score of the material (including material cost, construction cost and operation and maintenance cost, evaluated and scored by the construction party). It is the average score of structure and space utilization (scored by architects and structural engineers). Each participant is composed of two or more scoring experts, and all scores are limited to the range of 1 to 5 and rounded.

[0139] Figure 3 and Figure 4 The following are two final alternative solutions for cryo-EM room enclosure materials with similar magnetic field shielding effectiveness and sound insulation, which meet the requirements of biosafety protection, obtained after magnetic shielding and sound insulation calculation based on this method. Among them, 11, 100 thick stainless steel rock wool sandwich panel; 12, 50 thick rock wool board (ρ≥100kg / m 3 ); 13, 8mm thick mild steel plate; 14, 2mm thick PVC insulation layer; 15, 1mm thick copper plate; 16, 10mm thick polyurethane sound insulation board (ρ≥100kg / m 3 ); 17, 2mm thick silicon steel sheet; 18, 6mm thick pure iron plate; 19, 2mm thick pure aluminum plate.

[0140] Based on the dimensions and standards given in Table 1, Figure 3 and Figure 4 The Km values ​​of the two final alternatives were calculated after scoring the embodiments, and the results are shown in Table 2.

[0141] Table 2 Scoring examples of different thickness combination schemes

[0142]

[0143] Figure 3 In the embodiment, the enclosure materials are as follows from outside to inside: 100 mm thick stainless steel rock wool sandwich panel, 1 mm thick copper plate, 2 mm thick PVC insulation layer, 8 mm thick low carbon steel plate, 50 mm thick rock wool board (ρ≥100 kg / m 3 ), 100mm thick stainless steel rock wool sandwich panel; Figure 4 In the scheme, the enclosure materials from outside to inside are: 100mm thick stainless steel rock wool sandwich panel, 2mm thick pure aluminum plate, 6mm thick pure iron plate, 2mm thick silicon steel sheet, 10mm thick polyurethane sound insulation board (ρ≥100kg / m 3 ), 100mm thick stainless steel rock wool sandwich panel. Based on Table 2, it can be seen that Figure 4 The scheme scored high, so it is the optimal combination scheme for multi-layer enclosure materials for high-level biosafety cryo-electron microscope rooms obtained using this method.

[0144] The present application provides a method and system for designing a combination of multi-layer enclosure materials for a high-end electron microscope room with biosafety protection requirements. Through a construction module, a magnetic shielding acquisition module, a sound insulation module, and an evaluation module, a reasonable, economical, and safe combination of multi-layer enclosure materials is determined, thereby guiding the engineering construction of such high-end electron microscope rooms, significantly enhancing adaptability to specific construction scenarios, and reducing trial and error costs and comprehensive construction costs, making it easier to promote and apply them in practice.

Claims

1. A method for designing a combination of enclosure materials for a biosafety cryo-electron microscope room, characterized in that: It includes the following steps: S1: Evaluate and test the built environment characteristics based on the specific construction site of the electron microscope room to be designed; The environmental characteristics include: high and low frequency distribution of magnetic field, noise source and frequency distribution corresponding to the noise source; S2: The combination order of various materials in the multi-layer shielding layer materials required to construct the electron microscope room to be designed; The material combination sequence of the multi-layer shielding layer materials is set from outside to inside in sequence as follows: biosafety protection layer a, high-frequency suppression metal material, low-frequency suppression metal material and biosafety protection layer b; S3: Calculate the shielding effectiveness SE required for the electron microscope room to be designed based on the environmental magnetic field of the electron microscope room to be designed and the indoor magnetic field strength required by the shielding room; S4: constructing a thickness combination scheme of metal materials in the multi-layer shielding layer material; The metal material includes: a high-frequency suppression metal material and a low-frequency suppression metal material; According to the performance parameters of each metal material included in the multi-layer shielding layer material, calculate the thickness combination scheme of all metal materials that meet the shielding effectiveness SE requirements; The solution obtained by combining each of the thickness combination solutions with the biosafety protection layer a and the biosafety protection layer b is recorded as: the alternative solution of the multi-layer shielding layer material; S5: construct a sound insulation solution for each of the alternative solutions; a1: Confirm the indoor noise level R0 required for the electron microscope room to be designed and the current environmental noise level R1; a2: Calculate the total sound insulation performance R achieved by each alternative solution W ; a3: Confirm the sound insulation performance R corresponding to each alternative solution w Whether the sound insulation requirements can be met; If R1-R W ≤R0, the corresponding alternative plan will not be changed, the alternative plan will be recorded as the final alternative plan, and step S6 will be executed; Otherwise, execute step a4; a4: adding sound insulation material between the low-frequency suppression metal material and the biosafety protection layer b in each of the alternative solutions, so that the multi-layer shielding material corresponding to the alternative solution meets the noise shielding requirements, and obtaining the final alternative solution; executing step S6; S6: Obtain all the final alternative solutions and number them; S7: Setting evaluation dimensions and scoring criteria, evaluating and comparing all the final alternatives, and obtaining the optimal design solution corresponding to the electron microscope room to be designed; The evaluation dimensions include: material compatibility, material stability, comprehensive construction cost, and structural and space utilization.

2. A method for designing enclosure materials for a biosafety cryo-electron microscope room according to claim 1, characterized in that: The shielding effectiveness SE is calculated as follows: Among them, SE is the shielding effectiveness, E1 is the magnetic field strength of the environment without a shielding room, and E0 is the magnetic field strength required in the shielding room.

3. According to claim 1, a method for designing enclosure materials for a biosafety cryo-electron microscope room, characterized in that: The calculation method of the thickness combination scheme is: Among them, SE is the shielding effectiveness required for the electron microscope room to be designed, n is the total number of metal materials included in the multi-layer shielding material, i is the i-th metal material, U i is the relative magnetic permeability of the i-th metal material, G i is the conductivity of the ith metal material relative to copper, t i is the thickness of the i-th metal material, f is the frequency of the environmental magnetic field, and r is the distance from the field source to the shield.

4. According to claim 1, a method for designing enclosure materials for a biosafety cryo-electron microscope room, characterized in that: In step a2, the sound insulation performance R corresponding to each of the alternative solutions W Calculation method of Where n is the total number of materials included in the alternatives, i is the i-th material, fs is the ambient noise frequency; t i is the thickness of the i-th material; ρ i is the density of the ith material.

5. According to claim 1, a method for designing enclosure materials for a biosafety cryo-electron microscope room, characterized in that: In step a4, the design method of the sound insulation material layer to be added in the final alternative solution specifically includes the following steps: b1: Calculate the sound insulation value R that the sound insulation material in the final alternative solution needs to meet; R=R1-R0-R w ; Among them, R is the sound insulation of the added sound insulation material; R1 is the current ambient noise level without a shielding body; R0 is the indoor noise level required for the electron microscope room to be designed; R W The total sound insulation achieved for the known alternative solutions; b2: Calculate the scheme of the sound insulation material; Where m is the total number of sound insulation material layers that need to be added; j is the jth non-metallic sound insulation material; ρ j is the density of the jth non-metallic sound insulation material; t i is the thickness of the jth non-metallic sound insulation material; T is the thickness of all air interlayers included in the multi-layer shielding material.

6. According to claim 1, a method for designing enclosure materials for a biosafety cryo-EM chamber, characterized in that: The implementation methods of various materials in the multi-layer shielding layer material include: The biosafety protection layer a is realized based on a corrosion-resistant and easy-to-clean stainless steel surface or a color-coated steel surface metal sandwich panel; The high-frequency suppression metal material is realized based on a high-conductivity metal material; The low-frequency suppression metal material is realized based on a high magnetic permeability metal material; The sound insulation material is realized based on sound insulation and shielding filling materials; The biosafety protection layer b is realized based on a corrosion-resistant and easy-to-clean stainless steel surface or a color-coated steel surface metal sandwich panel.

7. A biosafety cryo-electron microscope room enclosure material combination design system, characterized in that: It includes: Construction module, magnetic shielding acquisition module, sound insulation module and evaluation module; The construction module is used to detect the environmental characteristics of the construction site where the electron microscope room to be designed is located, and the combination sequence of metal materials in the multi-layer shielding layer materials required by the electron microscope room to be designed; The magnetic shielding acquisition module stores a shielding effectiveness calculation model, reads the data stored in the construction module, and calculates all thickness combination schemes of metal materials that meet the shielding effectiveness SE requirements according to the performance parameters of each metal material included in the multi-layer shielding layer material; each thickness combination scheme is combined with the biosafety protection layer a and the biosafety protection layer b to obtain a solution, which is recorded as: an alternative solution of the multi-layer shielding layer material, and all the calculated alternative solutions are sent to the sound insulation module; The sound insulation module stores a sound insulation calculation model, and after reading the data stored in the construction module, the sound insulation performance R is calculated for each of the alternative solutions input by the magnetic shielding acquisition module. w , and determine whether to add sound insulation materials. For the alternative solution that requires the addition of sound insulation materials, the sound insulation materials are set between the low-frequency suppression metal material and the biosafety protection layer b; finally, the final alternative solution that satisfies both the magnetic field strength shielding requirements and the sound shielding requirements is sent to the evaluation module; The evaluation module stores preset value dimensions and scoring criteria, and calculates the scores of all the schemes corresponding to the electron microscope room to be designed according to the scores corresponding to all the final alternative schemes.

8. A biosafety cryo-EM chamber enclosure material combination design system according to claim 7, characterized in that: The scoring calculation formula pre-stored in the evaluation module is: Among them, is the average material fit among the final alternatives, is the average stability score, is the average value of the comprehensive construction cost score of the material. The scores for structure and space utilization were average.