Manufacturing method of step substrate with cavity
By dissolving the uncured materials of the bonding layer and optimizing process conditions during the chip packaging process, the problem of bonding material overflow is solved, the cavity structure and efficient packaging of the step substrate are realized, and the normal bonding between the chip and the leads is ensured. .
Patent Information
- Application Number
- CN202410941853.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-15
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2044-07-15
AI Technical Summary
During the chip packaging process, the bonding material overflows the glue in the deep groove, resulting in an increase in space occupation or overflow, affecting the effect of chip patch and wire bonding.
By dissolving the bonding material at the bottom of the tank before the bonding layer is cured, combining optimized process conditions such as pressing temperature and pressure, reducing overflow, and forming a cavity structure on the step substrate, ensuring the curing and packaging quality of the bonding layer.
It effectively reduces the amount of glue over the bonding material, avoids the problem of chip being unable to bond with wire due to glue overflow, and improves the reliability and efficiency of packaging.
Smart Images

Figure CN119008419A_ABST
Abstract
Description
Technical Field
[0001] The present application belongs to the field of semiconductor packaging technology, and specifically relates to a method for manufacturing a stepped substrate with a cavity. Background Art
[0002] Among the many packaging structures, there is a chip package that requires a deep groove structure to be made on the substrate surface. The chip is pasted in the cavity formed by the deep groove and wire bonding is performed. However, the space in the deep groove is limited. Figure 1 As shown, the bonding material of the top plate and the bottom plate used for bonding the opening groove is squeezed into the groove during the bonding process, forming overflow glue, which may occupy the deep groove space and cover the electrode in the groove, affecting the chip mounting and lead bonding; in severe cases, the overflow glue fills the deep groove, making the deep groove unusable. Summary of the invention
[0003] Therefore, the technical problem to be solved by the present application is to provide a method for manufacturing a stepped substrate with a cavity, which reduces the overflow of bonding material into the groove by specially optimizing the process conditions, and then removes the overflowed glue at the bottom of the groove by dissolving the bonding material at the bottom of the groove before the bonding layer is cured, thereby avoiding the overflow of glue at the bottom of the groove that makes it impossible to mount the chip and bond the leads.
[0004] In order to solve the above problems, the present application provides a method for manufacturing a step substrate with a cavity, comprising:
[0005] laminating a bonding layer on a substrate;
[0006] Pressing a window plate on the side of the bonding layer facing away from the substrate;
[0007] dissolving the bonding material on the bonding layer at a position relative to the window of the window plate;
[0008] The bonding layer is cured.
[0009] Optionally, the bonding material is a dry model photosensitive resin or a thermosetting resin.
[0010] Optionally, the pressing temperature of the bonding layer and the window plate is lower than the conventional pressing temperature of the bonding layer and the window plate, and the conventional pressing temperature of the bonding layer and the window plate is 60° C. to 80° C.;
[0011] The pressing pressure between the bonding layer and the window plate is greater than the conventional pressing pressure between the bonding layer and the window plate, and the conventional pressing pressure between the bonding layer and the window plate is 0.2MPa to 0.6MPa.
[0012] Optionally, the bonding layer and the window plate are laminated by a vacuum laminator.
[0013] Optionally, when dissolving the bonding material on the bonding layer at a position relative to the window of the window plate, the window of the window plate is arranged to face downward.
[0014] Optionally, the curing temperature of the bonding layer is 150° C. to 250° C., and the curing time of the bonding layer is 30 min to 120 min.
[0015] Optionally, the method further includes:
[0016] Drilling a through hole in the stepped substrate having the cavity along a vertical direction;
[0017] The through holes are metallized to form pads.
[0018] Optionally, the method further includes:
[0019] A solder resist layer is formed on the top and bottom surfaces of the step substrate having the cavity in areas outside the projection of the pad.
[0020] Optionally, the method further includes:
[0021] Pad surface coating.
[0022] Optionally, the method further includes:
[0023] Ball planting on the pad surface.
[0024] Beneficial Effects
[0025] The method for manufacturing a stepped substrate with a cavity provided in an embodiment of the present invention, through an optimized bonding process, can effectively reduce the overflow of glue in the window of the window plate after the window plate is bonded, and before the bonding layer is cured, it can dissolve the uncured bonding material at the bottom of the groove, thereby removing the bonding material and overflowed glue at the bottom of the groove, and avoiding the overflow of glue at the bottom of the groove that makes it impossible to mount the chip and bond the leads. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 A schematic diagram of the structure of a step substrate with a cavity produced by a conventional manufacturing method;
[0027] Figure 2 A flowchart of a method for manufacturing a stepped substrate with a cavity according to an optional embodiment of the present application;
[0028] Figure 3 A flowchart of a method for manufacturing a stepped substrate with a cavity according to another optional embodiment of the present application;
[0029] Figure 4 A schematic diagram of a process for preparing a step substrate with a cavity in the present application;
[0030] Figure 5 A schematic diagram of a process for preparing a step substrate with a cavity in the present application;
[0031] Figure 6A schematic diagram of a process for preparing a step substrate with a cavity in the present application;
[0032] Figure 7 A schematic diagram of a process for preparing a step substrate with a cavity in the present application;
[0033] Figure 8 A schematic diagram of a process for preparing a step substrate with a cavity in the present application;
[0034] Fig. 9 A schematic diagram of a process for preparing a step substrate with a cavity in the present application;
[0035] Fig.10 A schematic diagram of a process for preparing a step substrate with a cavity in the present application;
[0036] Fig.11 A schematic diagram of a process for preparing a stepped substrate with a cavity according to the present application.
[0037] The reference numerals are:
[0038] 1. Substrate; 2. Bonding layer; 3. Window plate; 4. Pad; 5. Solder mask layer. DETAILED DESCRIPTION
[0039] In the description of the present application, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.
[0040] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.
[0041] In this application, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be an indirect connection through an intermediate medium, or it can be the internal communication of two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0042] The preferred embodiments of the present invention are described below in conjunction with the accompanying drawings. It should be understood that the preferred embodiments described herein are only used to illustrate and explain the present invention, and are not used to limit the present invention.
[0043] See also Figures 2 to 11 As shown, according to an embodiment of the present application, a method for manufacturing a stepped substrate with a cavity is provided, by dissolving the uncured bonding material at the bottom of the groove after the window plate 3 is bonded and before the bonding layer 2 is cured, so that the overflowed glue at the bottom of the groove can be removed, thereby preventing the overflowed glue at the bottom of the groove from causing the chip to be unable to be mounted and the wires to be bonded.
[0044] Method for manufacturing a stepped substrate with a cavity:
[0045] First, see Figure 4 As shown, step S1: pressing a bonding layer 2 on a substrate 1.
[0046] The substrate 1 can be a single-layer circuit board or a multi-layer circuit board, which can be selected according to the actual situation, and this embodiment does not make any further limitations. It can be understood that a single-layer circuit board is suitable for simpler electronic devices, such as some small electronic toys; a multi-layer circuit board is suitable for the integration of many functional modules and high-performance chips to achieve complex circuit layout and signal transmission, such as smart phones.
[0047] The bonding layer 2 may be a photosensitive resin sheet. The bonding layer 2 is pressed onto the substrate 1 to play a bonding role, and is used to establish a connection between the substrate 1 and other components to form a stable multi-layer structure, so that the substrate 1 and other components can still maintain a stable connection when subjected to external forces such as vibration and impact.
[0048] Then, see Figure 5 As shown, step S2: pressing the window plate 3 on the side of the bonding layer 2 facing away from the substrate 1.
[0049] The window plate 3 has a through groove penetrating the window plate 3 , and the cross section of the through groove may be cylindrical or rectangular, etc., which is not further limited in this embodiment.
[0050] Specifically, the cavity formed by the through groove is used to install the chip. By providing the through groove, a chip packaging space is formed.
[0051] Among them, as one embodiment, the window board 3 is a double-sided copper-clad board, and the window board 3 protects the chip; as another embodiment, the window board 3 is a circuit board, and the window board 3 not only supports the chip but also has the function of connecting the circuit.
[0052] Specifically, the window plate 3 is located on the side of the bonding layer 2 facing away from the substrate 1 , and the window plate 3 is pressed onto the bonding layer 2 . One side of the bonding layer 2 is used to bond to the substrate 1 , and the other side is used to bond to the window plate 3 .
[0053] Secondly, see Figure 6 As shown, step S3: dissolving the bonding material at the position of the bonding layer 2 relative to the window of the window plate 3.
[0054] The bonding material at the position of the bonding layer 2 relative to the window of the window plate 3 is the bonding material at the bottom of the through groove.
[0055] Among them, dissolving the bonding material at the bottom of the through-groove can, on the one hand, expose the electrode at the bottom of the through-groove, making it easier to bond the chip to the electrode lead; on the other hand, it can create better installation conditions for chip installation, which is beneficial to chip mounting.
[0056] Specifically, the window plate of the step substrate with the cavity is placed with the plate surface downward, and in a developing device, a developing solution or an organic solvent is sprayed from bottom to top toward the bottom of the window groove to dissolve the bonding material at the bottom of the through groove.
[0057] Finally, step S4: curing the bonding layer 2 .
[0058] The bonding layer 2 can be cured by baking, so that the bonding layer 2 is tightly combined with the substrate 1 and the window plate 3 respectively, forming a stepped substrate with a cavity.
[0059] In the above-mentioned embodiments, the bonding material is a dry model photosensitive resin or a thermosetting resin.
[0060] When the bonding material is a dry model photosensitive resin, the bonding layer 2 may be a photosensitive resin sheet; when the bonding material is a thermosetting resin, the bonding layer 2 may be a thermosetting resin sheet.
[0061] Specifically, when the bonding material is a dry model photosensitive resin, the bonding material at the bottom of the through groove can be removed by spraying a water-soluble alkaline solution such as a sodium carbonate solution; when the bonding material is a thermosetting resin, the bonding material at the bottom of the through groove can be removed by spraying an organic solvent such as acetone, ethanol, toluene, and xylene.
[0062] When the bonding material is a thermosetting resin, the thermosetting resin is a pure adhesive resin film that does not contain glass fiber cloth.
[0063] In the above embodiment, the pressing temperature of the bonding layer 2 and the window plate 3 is lower than the conventional pressing temperature of the bonding layer 2 and the window plate 3, and the conventional pressing temperature of the bonding layer 2 and the window plate 3 is 60°C to 80°C; the pressing pressure of the bonding layer 2 and the window plate 3 is higher than the conventional pressing pressure of the bonding layer 2 and the window plate 3, and the conventional pressing pressure of the bonding layer 2 and the window plate 3 is 0.2MPa to 0.6MPa. By setting the pressing temperature of the bonding layer 2 and the window plate 3 lower than the conventional pressing temperature of the bonding layer 2 and the window plate 3, the viscosity of the bonding material can be increased, the fluidity of the bonding material can be reduced, and the amount of glue overflow from the bottom of the through groove can be reduced; at the same time, by setting the pressing pressure of the bonding layer 2 and the window plate 3 higher than the conventional pressing pressure of the bonding layer 2 and the window plate 3, it can be ensured that the bonding layer 2 has good circuit filling performance.
[0064] The pressing temperature of the bonding layer 2 and the window plate 3 may be 10° C. to 20° C. lower than the conventional pressing temperature of the bonding layer 2 and the window plate 3 .
[0065] Specifically, when the conventional pressing temperature of the bonding layer 2 and the window plate 3 is 80°C, the setting value of the pressing temperature of the bonding layer 2 and the window plate 3 can be 60°C to 70°C; when the conventional pressing temperature of the bonding layer 2 and the window plate 3 is 70°C, the setting value of the pressing temperature of the bonding layer 2 and the window plate 3 can be 50°C to 60°C. It should be noted that when the conventional pressing temperature of the bonding layer 2 and the window plate 3 is 60°C, the setting value of the pressing temperature of the bonding layer 2 and the window plate 3 can only be 50°C. If the setting value of the pressing temperature of the bonding layer 2 and the window plate 3 is less than 50°C, the substrate 1 and the window plate 3 cannot be bonded.
[0066] The pressing pressure between the bonding layer 2 and the window plate 3 may be 5% to 15% higher than the conventional pressing pressure between the bonding layer 2 and the window plate 3 .
[0067] Specifically, when the conventional pressing pressure of the bonding layer 2 and the window plate 3 is 0.6MPa, the pressing pressure setting value of the bonding layer 2 and the window plate 3 can be 0.63MPa~0.69MPa; when the conventional pressing pressure of the bonding layer 2 and the window plate 3 is 0.4MPa, the pressing pressure setting value of the bonding layer 2 and the window plate 3 can be 0.42MPa~0.46MPa; when the conventional pressing pressure of the bonding layer 2 and the window plate 3 is 0.2MPa, the pressing pressure setting value of the bonding layer 2 and the window plate 3 can be 0.21MPa~0.23MPa.
[0068] In the above embodiment, the bonding layer 2 and the window plate 3 are pressed together using a vacuum laminator. By using a vacuum laminator to press the bonding layer 2 and the window plate 3 together, bubbles can be avoided in the pressing area, ensuring that the bonding layer 2 can be tightly combined with the substrate 1 and the window plate 3.
[0069] In this embodiment, the substrate 1, the bonding layer 2 and the window plate 3 can be placed in a hollow laminating machine for lamination.
[0070] In the above embodiment, when dissolving the bonding material at the position of the bonding layer 2 relative to the window of the window plate 3, the window of the window plate 3 is set in the downward direction, so that the water-soluble alkaline solution or the organic solvent is sprayed in the upward direction, which can reduce the residence time of the water-soluble alkaline solution or the organic solvent at the bottom of the through groove, and avoid the bonding material outside the bottom area of the through groove from being dissolved.
[0071] The downward direction may be a vertically downward direction.
[0072] In the above embodiment, the curing temperature of the bonding layer 2 is 150° C. to 250° C., and the curing time of the bonding layer 2 is 30 min to 120 min.
[0073] For example, the curing temperature of the bonding layer 2 is 150° C., or 160° C., or 170° C., or 180° C., or 190° C., or 200° C., or 210° C., or 220° C., or 230° C., or 240° C., or 250° C. It can be understood that the curing temperature of the bonding layer 2 can also be other values in addition to the above values, as long as the curing temperature of the bonding layer 2 is 150° C. to 250° C.
[0074] Specifically, in this embodiment, the curing temperature of the bonding layer 2, that is, the baking temperature of the bonding layer 2, is preferably 200°C.
[0075] For example, the curing time of the bonding layer 2 can be 30 minutes, or 40 minutes, or 50 minutes, or 60 minutes, or 70 minutes, or 80 minutes, or 90 minutes, or 100 minutes, or 110 minutes, or 120 minutes. It can be understood that the curing time of the bonding layer 2 can also be other values besides the above values, as long as the curing time of the bonding layer 2 is 30 minutes to 120 minutes.
[0076] Specifically, in this embodiment, the curing time of the bonding layer 2, that is, the baking time of the bonding layer 2, is preferably 60 minutes.
[0077] In some possible implementations provided in this application, see Figure 7 As shown, the method for manufacturing a step substrate having a cavity further includes:
[0078] Step S5: drilling a through hole in the stepped substrate having the cavity along the vertical direction.
[0079] Among them, mechanical drilling can be performed on the stepped substrate with cavities, and then the through-holes can be metallized to form conductive channels between different layers, so that current and signals can be transmitted between different layers. Among them, multiple through-holes can be drilled to provide more path options for the layout of the circuit and optimize the circuit design.
[0080] In some possible implementations provided in this application, see Figure 8 As shown, the method for manufacturing a step substrate having a cavity further includes:
[0081] Step S6: metallizing the through hole to form the pad 4 .
[0082] Among them, through-hole metallization can include de-drilling, which removes resin drilling smears and debris generated on the hole wall during the drilling process. Chemical methods can be used, such as using strong oxidants or plasma treatment; hole wall activation, which makes the hole wall surface active so that metal can be adsorbed later. This step may involve the use of chemicals or plasma treatment to activate the hole wall; chemical copper deposition, which deposits a thin layer of copper on the hole wall by chemical plating. It usually involves a series of chemical reactions to reduce copper ions to metallic copper and attach them to the hole wall; electroplating thickening, based on chemical copper deposition, the thickness of the copper layer is further increased by electroplating to meet the requirements of conductivity and reliability.
[0083] Specifically, after the through-holes are metallized, the lines between different layers of the circuit board can be connected to each other through the through-holes, ensuring the smooth transmission of current and signals, providing a good conductive path, reducing contact resistance and signal loss, and improving the stability and reliability of the circuit. At the same time, the metal filling the through-holes can increase the overall strength of the substrate, enabling it to withstand the stress during subsequent processing and use.
[0084] The through-hole metallization further includes forming a pad 4, and the pad 4 can be used as a pin for circuit connection.
[0085] Specifically, the shape and size of the metal layer can be precisely controlled through processes such as photolithography or etching to form a pad 4 of a specific shape and size.
[0086] In some possible implementations provided in this application, see Fig. 9 As shown, the method for manufacturing a step substrate having a cavity further includes:
[0087] Step S7: making solder resist layers on the top and bottom surfaces of the step substrate having the cavity, and making solder resist openings in the pad 4 area.
[0088] It is understandable that by making the solder resist layer 5 in the area outside the projection of the pad 4 on the top and bottom surfaces of the step substrate with the cavity, it is possible to prevent the solder from spreading in the area where soldering is not required, and avoid short circuits caused by solder connection between adjacent circuits. For example, in a circuit board with high-density wiring, the solder resist layer 5 can accurately limit the flow range of the solder and ensure the independence of each circuit.
[0089] The solder resist layer 5 may be made of liquid solder resist ink and dry film solder resist material.
[0090] In some possible implementations provided in this application, see Fig.10 As shown, the method for manufacturing a step substrate having a cavity further includes:
[0091] Step S8: coating the surface of the pad 4.
[0092] The surface of the pad 4 may be plated with tin or nickel-gold.
[0093] Specifically, by coating the surface of the pad 4, the solder can better adhere to the surface of the pad 4 to form a good solder joint and ensure the welding quality; at the same time, a protective film can be formed on the surface of the pad 4 to prevent it from being oxidized during storage and use, thereby ensuring conductivity during welding.
[0094] In some possible implementations provided in this application, see Fig.11 As shown, the method for manufacturing a step substrate having a cavity further includes:
[0095] Step S9: planting a ball on the surface of the pad 4.
[0096] Among them, the ball can be planted on the surface of the pad 4 by using a template ball planting method, a vacuum ball planting method or a spray ball method.
[0097] Specifically, by planting balls on the surface of the pad 4, more connection points can be achieved in a limited space, which is suitable for highly integrated electronic devices; at the same time, compared with traditional pin connections, ball-type connection points can provide better electrical performance and reduce delays and losses in signal transmission.
[0098] The method for manufacturing a step substrate with a cavity provided in the embodiment of the present application adopts a photosensitive resin sheet or a thermosetting resin sheet as a bonding material between the substrate 1 and the window plate 3. After the window plate 3 is bonded, when the photosensitive resin sheet or the thermosetting resin sheet is not cured, the window of the window plate 3 is turned downward, and a developer or a solvent is sprayed upward to dissolve and remove the uncured photosensitive resin sheet or the thermosetting resin sheet at the bottom of the groove with the developer or the solvent. Since the photosensitive resin sheet or the thermosetting resin sheet covered by the window plate 3 cannot be exposed to the developer or the solvent, the photosensitive resin sheet or the thermosetting resin sheet under the window plate 3 is retained. After the photosensitive resin sheet or the thermosetting resin sheet at the bottom of the through groove is removed, the step substrate from which the photosensitive resin sheet or the thermosetting resin sheet at the bottom of the through groove has been removed is heated to form a permanent bond between the substrate 1 and the window plate 3.
[0099] It is easy for those skilled in the art to understand that the above-mentioned advantageous methods can be freely combined and superimposed without conflict.
[0100] The above are only preferred embodiments of the present application and are not intended to limit the present application. Any modifications, equivalent replacements and improvements made within the spirit and principles of the present application shall be included in the protection scope of the present application. The above are only preferred implementations of the present application. It should be pointed out that for ordinary technicians in this technical field, several improvements and variations can be made without departing from the technical principles of the present application, and these improvements and variations should also be regarded as the protection scope of the present application.
Claims
1. A method for manufacturing a stepped substrate having a cavity, It is characterized in that include: Press-bonding a bonding layer (2) on a substrate (1); Pressing a window plate (3) on the side of the bonding layer (2) facing away from the substrate (1); Dissolving the bonding material on the bonding layer (2) at a position relative to the window of the window plate (3); The bonding layer (2) is cured.
2. The method for manufacturing a stepped substrate having a cavity according to claim 1, It is characterized in that The bonding material is a dry model photosensitive resin or a thermosetting resin.
3. The method for manufacturing a stepped substrate having a cavity according to claim 1, It is characterized in that The pressing temperature of the bonding layer (2) and the window plate (3) is lower than the conventional pressing temperature of the bonding layer (2) and the window plate (3), and the conventional pressing temperature of the bonding layer (2) and the window plate (3) is 60° C. to 80° C.; The pressing pressure between the bonding layer (2) and the window plate (3) is greater than the conventional pressing pressure between the bonding layer (2) and the window plate (3), and the conventional pressing pressure between the bonding layer (2) and the window plate (3) is 0.2 MPa to 0.6 MPa.
4. The method for manufacturing a stepped substrate having a cavity according to claim 1, It is characterized in that The bonding layer (2) and the window plate (3) are pressed together using a vacuum laminating machine.
5. The method for manufacturing a stepped substrate having a cavity according to claim 1, It is characterized in that When dissolving the bonding material at a position on the bonding layer (2) relative to the window of the window plate (3), the window of the window plate (3) is arranged to face downward.
6. The method for manufacturing a stepped substrate having a cavity according to claim 1, It is characterized in that The curing temperature of the bonding layer (2) is 150° C. to 250° C., and the curing time of the bonding layer (2) is 30 min to 120 min.
7. The method for manufacturing a stepped substrate having a cavity according to claim 1, It is characterized in that The method further comprises: Drilling a through hole in the stepped substrate having the cavity along a vertical direction; The through-holes are metallized to form pads (4).
8. The method for manufacturing a stepped substrate having a cavity according to claim 7, It is characterized in that The method further comprises: A solder resist layer (5) is formed on the top and bottom surfaces of a step substrate having a cavity in an area outside the projection of a solder pad (4).
9. The method for manufacturing a stepped substrate having a cavity according to claim 7, It is characterized in that The method further comprises: The pad (4) surface is coated.
10. The method for manufacturing a stepped substrate having a cavity according to claim 7, It is characterized in that The method further comprises: The pad (4) is surface-mounted with a ball.
Citation Information
Patent Citations
Adhesive material film, semiconductor mounting external connecting member, semiconductor device and their production
JP2000256628A
Adhesive film and its use and method for producing semiconductor device
JP2002265888A
Conductive paste composition for filling via hole
JP2007096120A
Multilayer wiring board
JP2009065009A
Method for manufacturing organic el element
JP2021057198A