Full-printing 3D micro solid-state aluminum air battery and manufacturing method thereof

Through full printing 3D technology, the aluminum anode and air cathode with quasi-solid hydrogel electrolyte and comb-tooth structures are used to solve the problems of high complexity and difficulty in miniaturization of traditional aluminum-air battery systems, and realize the problem of high complexity and difficulty in miniaturization. Miniaturize the battery and high-efficiency density energy storage.

CN119029422APending Publication Date: 2024-11-26NAT UNIV OF DEFENSE TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411396251.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-08
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

Due to the high system complexity and difficulty in miniaturization, traditional aluminum-air batteries are difficult to achieve the high energy density energy storage requirements of portable and wearable devices.

Method used

The micro solid aluminum air battery is manufactured using full printing 3D technology, using quasi-solid hydrogel electrolyte and comb-tooth structure aluminum anode and air cathode, and stacking electrodes layer by layer through 3D printing technology, and filling the outer frame of the battery Electrolyte realizes a compact structure between the electrode and the battery outer frame.

Benefits of technology

The miniaturization, refinement and rapid production of batteries are achieved, and the complexity of the system is reduced. Through the three-dimensional structure and the use of hydrogel electrolytes, the sufficient oxygen diffusion window is ensured, and it is suitable for the provision of electricity with different needs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119029422A_ABST
    Figure CN119029422A_ABST
Patent Text Reader

Abstract

The invention discloses a full-printing 3D micro solid-state aluminum air battery and a manufacturing method thereof. The solid aluminum air battery comprises a battery outer frame, an air cathode, a quasi-solid hydrogel electrolyte and an aluminum anode, the air cathode and the aluminum anode are both of a comb tooth structure, the tooth space L is larger than the comb width D, and comb teeth of the air cathode and comb teeth of the aluminum anode are arranged in the battery outer frame in a staggered and non-intersecting mode. And the quasi-solid hydrogel electrolyte is filled in gaps between the air cathode and the aluminum anode, between the air cathode and the outer frame of the battery and between the aluminum anode and the outer frame of the battery. The structure is compact and small, the size is millimeter-level, the weight is gram-level, and an array can be formed in a series connection, parallel connection or series-parallel connection mode to provide electric energy for electric appliances with different requirements.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of battery technology, and more specifically, to a fully printed 3D micro solid-state aluminum-air battery and a manufacturing method thereof. Background Art

[0002] With the rapid development of portable and wearable electronic devices, high energy density energy storage devices have received extensive attention. Thanks to its high theoretical energy density and mature anode smelting technology, aluminum-air batteries are considered to be potential competitors for the next generation of energy storage batteries. However, traditional aluminum-air batteries use a sandwich structure and a pump to drive liquid electrolytes for circulation, resulting in high system complexity and difficulty in miniaturization. At this time, innovating its structural design concept and manufacturing method will be able to solve the above problems and achieve the goal of miniaturization.

[0003] At present, the focus at home and abroad is mainly on the development of quasi-solid hydrogel electrolytes to replace traditional liquid electrolytes, and the development of aluminum anodes and air cathodes that are compatible with them. Thanks to the fact that hydrogel electrolytes have a fixed form and do not require a container, the development of solid-state aluminum-air batteries has become possible. However, the current focus of improving the performance of aluminum-air batteries at home and abroad is mainly on the innovation of cathode, anode and electrolyte materials. Therefore, changing the structure of aluminum-air batteries and adopting a new manufacturing method will also be an effective measure to improve their performance and achieve miniaturization. Summary of the invention

[0004] The purpose of the present invention is to provide a fully printed 3D micro solid-state aluminum-air battery and a manufacturing method thereof to overcome the defects of the prior art.

[0005] In order to achieve the above object, the technical solution adopted by the present invention is as follows:

[0006] A fully printed 3D micro solid-state aluminum-air battery comprises an outer battery frame, an air cathode, a quasi-solid hydrogel electrolyte and an aluminum anode, wherein the air cathode and the aluminum anode are both comb-tooth structures and the tooth gap L is greater than the comb width D, the comb teeth of the air cathode and the comb teeth of the aluminum anode are staggered and non-intersectingly arranged in the outer battery frame, and the quasi-solid hydrogel electrolyte is filled in the gaps between the air cathode and the aluminum anode, between the air cathode and the outer battery frame, and between the aluminum anode and the outer battery frame.

[0007] Furthermore, the air cathode and the aluminum anode are stacked layer by layer using 3D printing technology.

[0008] Furthermore, the upper surface of the quasi-solid hydrogel electrolyte is lower than the upper surfaces of the air cathode and the aluminum anode.

[0009] The present invention also provides a method for manufacturing the fully printed 3D micro solid-state aluminum-air battery, comprising the following steps:

[0010] S1. Design the electrode structure to be a comb structure in which the tooth gap L is larger than the comb width D, and the electrode cathode and anode are mirror images of each other;

[0011] S2, adding MnO2, aluminum powder, and electrolyte powder to corresponding binders or aqueous solutions to prepare quasi-solid air cathode ink, aluminum anode ink, and electrolyte ink;

[0012] S3, respectively loading the air cathode ink, the aluminum anode ink, the silicone rubber ink and the electrolyte ink into the syringe;

[0013] S4, using an extrusion 3D printer to drive a syringe to print the air cathode and the aluminum anode on the PET film respectively, forming a structure in which the comb teeth of the aluminum anode and the comb teeth of the air cathode are interlaced and do not intersect with each other, and putting the prepared electrodes into a vacuum dryer for drying;

[0014] S5. Put the dried electrode back into the extrusion 3D printer, and use the extrusion 3D printer to build a battery outer frame of silicone rubber on the outside of the electrode. After the battery outer frame is built, let it solidify at room temperature to form a stable structure;

[0015] S6, filling the gaps between the comb teeth and between the electrode and the outer frame of the battery with hydrogel electrolyte, and setting the upper surface of the hydrogel electrolyte lower than the upper surfaces of the air cathode and the aluminum anode, and then placing the battery filled with electrolyte in an environment of -35°C to gel;

[0016] S7. After solidification is completed, a solid-state aluminum-air battery is obtained.

[0017] The present invention also provides a method for manufacturing a solid-state aluminum-air battery array, comprising the following steps:

[0018] fabricating a plurality of individual aluminum-air cells at specific locations on a substrate;

[0019] Connect the positive and negative tabs of different aluminum-air battery cells using conductive silver paste on the substrate;

[0020] The solid-state aluminum-air battery array was prepared by drying in the open air at room temperature.

[0021] Compared with the prior art, the advantages of the present invention are: 1. The present invention uses a hydrogel quasi-solid electrolyte and does not require the support of a peristaltic pump, an electrolyte storage device, or a delivery pipeline; 2. The battery anode, cathode, and electrolyte of the present invention are all manufactured using 3D printing technology (extrusion 3D), which can achieve customized, refined, and rapid production and manufacturing of the shape; 3. The battery cathode and anode of the present invention are both comb-tooth structures, and the gaps in the middle are filled with hydrogel electrolytes, and the upper surface of the air cathode is exposed to the air to ensure that oxygen has sufficient diffusion windows; 4. The battery of the present invention has a three-dimensional spatial geometric structure, and its thickness is changed by changing the number of layers of extruded microfilaments, and the manufacturing accuracy directly depends on the performance of the 3D printer used; 5. All components of the battery of the present invention are constructed using 3D printing technology, and its structure is compact and small, with a size of millimeters and a weight of grams; 6. The battery of the present invention can form an array in series, parallel, or mixed to provide electrical energy for electrical appliances with different needs. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0023] Figure 1 This is a geometric parameter diagram of the fully printed 3D micro solid-state aluminum-air battery of the present invention.

[0024] Figure 2 It is a structural schematic diagram of the fully printed 3D micro solid-state aluminum-air battery of the present invention.

[0025] In the figure: battery outer frame 1, air cathode 2, quasi-solid hydrogel electrolyte 3, aluminum anode 4. DETAILED DESCRIPTION

[0026] The preferred embodiments of the present invention are described in detail below in conjunction with the accompanying drawings so that the advantages and features of the present invention can be more easily understood by those skilled in the art, thereby making a clearer and more definite definition of the protection scope of the present invention.

[0027] Embodiment 1

[0028] See also Figure 1 and Figure 2As shown, this embodiment discloses a fully printed 3D micro solid-state aluminum-air battery, including a battery outer frame 1, an air cathode 2, a quasi-solid hydrogel electrolyte 3 and an aluminum anode 4, wherein the air cathode 2 and the aluminum anode 4 are both comb-tooth structures and the tooth gap L is greater than the comb width D (satisfying the following formulas 1-3), the comb teeth of the air cathode 2 and the comb teeth of the aluminum anode 4 are staggered and non-intersecting (mirror images of each other) in the battery outer frame 1, and the quasi-solid hydrogel electrolyte 3 is filled in the gaps between the air cathode 2 and the aluminum anode 4, between the air cathode 2 and the battery outer frame 1, and between the aluminum anode 4 and the battery outer frame 1.

[0029] L1=L2=…=L n (1)

[0030] D1=D2=…=D n+1 (2)

[0031] L i >D j ,i=1,2,…n,j=1,2,…n+1 (3)

[0032] In this embodiment, the air cathode 2 and the aluminum anode 4 are stacked layer by layer using 3D printing technology.

[0033] In this embodiment, the upper surface of the quasi-solid hydrogel electrolyte 3 is lower than the upper surfaces of the air cathode 2 and the aluminum anode 4, ensuring that the electrolyte air diffuses smoothly to the air cathode.

[0034] Embodiment 2

[0035] This embodiment provides a method for manufacturing the fully printed 3D micro solid-state aluminum-air battery described in Embodiment 1, comprising the following steps:

[0036] Step S1, designing the electrode structure to be a comb tooth structure in which the tooth gap L is larger than the comb width D, and the electrode cathode and anode are mirror images of each other.

[0037] Step S2: adding MnO2, aluminum powder, and electrolyte powder to corresponding adhesives or aqueous solutions respectively to prepare quasi-solid air cathode ink, aluminum anode ink, and electrolyte ink.

[0038] Step S3, respectively loading the air cathode ink, the aluminum anode ink, the silicone rubber ink and the electrolyte ink into the syringes.

[0039] Step S4, write G code according to the designed structure and download it to the extrusion 3D printer. Use the extrusion 3D printer to drive the syringe to print the air cathode and the aluminum anode on the PET film respectively, forming a structure in which the comb teeth of the aluminum anode and the comb teeth of the air cathode are interlaced and do not intersect, and put the prepared electrode into a vacuum dryer for drying.

[0040] Step S5, putting the dried electrode back into the extrusion 3D printer, and using the extrusion 3D printer to build a battery outer frame 1 of silicone rubber on the outside of the electrode. After the battery outer frame 1 is built, let it solidify at room temperature to form a stable structure.

[0041] Step S6, filling the gaps between the comb teeth and between the electrodes and the outer frame of the battery with hydrogel electrolyte, and setting the upper surface of the hydrogel electrolyte lower than the upper surfaces of the air cathode 2 and the aluminum anode 4, and then placing the battery filled with electrolyte in an environment of -35°C to gel.

[0042] Step S7: After solidification is completed, a solid aluminum-air battery is obtained. Figure 2 shown.

[0043] This embodiment is different from the traditional aluminum-air battery electrodes and electrolytes that adopt a planar structure. The designed battery electrodes and electrolytes are stacked layer by layer using 3D printing technology to form a spatial three-dimensional structure that is convenient for air diffusion.

[0044] The battery electrode structure proposed in this embodiment is a comb-tooth structure: the cathode and anode comb teeth are staggered and do not touch each other, and are mirror images of each other, and the spaces between the comb teeth and the electrodes and the silicone rubber frame are filled with hydrogel electrolyte.

[0045] The air cathode and aluminum electrode, gel electrolyte, and packaging frame size of this embodiment can all be customized according to specific application requirements.

[0046] This embodiment is easy to miniaturize: a micro-battery with a three-dimensional spatial geometric structure with a size of millimeters and a mass of grams can be manufactured by controlling the number of microwire stacking layers using high-precision 3D printing equipment.

[0047] Embodiment 3

[0048] This embodiment provides a method for manufacturing a solid-state aluminum-air battery array, comprising the following steps:

[0049] Fabricating a plurality of individual aluminum-air batteries according to embodiment 2 at specific locations on the substrate;

[0050] Connect the positive and negative tabs of different aluminum-air battery cells using conductive silver paste on the substrate;

[0051] The solid-state aluminum-air battery array was prepared by drying in the open air at room temperature.

[0052] This embodiment has excellent scalability: according to the power consumption requirements of the electrical equipment, several battery cells can be connected in series, parallel or mixed using conductive silver paste to quickly build a battery array.

[0053] Although the embodiments of the present invention are described in conjunction with the accompanying drawings, the patent owner may make various variations or modifications within the scope of the appended claims. As long as they do not exceed the protection scope described in the claims of the present invention, they should be within the protection scope of the present invention.

Claims

1. A fully printed 3D micro solid-state aluminum-air battery, characterized in that: The invention comprises a battery outer frame, an air cathode, a quasi-solid hydrogel electrolyte and an aluminum anode, wherein the air cathode and the aluminum anode are both comb-tooth structures and the tooth gap L is greater than the comb width D, the comb teeth of the air cathode and the comb teeth of the aluminum anode are staggered and non-intersectingly arranged in the battery outer frame, and the quasi-solid hydrogel electrolyte is filled in the gaps between the air cathode and the aluminum anode, between the air cathode and the battery outer frame, and between the aluminum anode and the battery outer frame.

2. The fully printed 3D micro solid-state aluminum-air battery according to claim 1, characterized in that: The air cathode and the aluminum anode are stacked layer by layer using 3D printing technology.

3. The fully printed 3D micro solid-state aluminum-air battery according to claim 1, characterized in that: The upper surface of the quasi-solid hydrogel electrolyte is lower than the upper surfaces of the air cathode and the aluminum anode.

4. A method for manufacturing a fully printed 3D micro solid-state aluminum-air battery according to any one of claims 1 to 3, characterized in that: The following steps are involved: S1. Design the electrode structure to be a comb structure in which the tooth gap L is larger than the comb width D, and the electrode cathode and anode are mirror images of each other; S2, adding MnO2, aluminum powder, and electrolyte powder to corresponding binders or aqueous solutions to prepare quasi-solid air cathode ink, aluminum anode ink, and electrolyte ink; S3, respectively loading the air cathode ink, the aluminum anode ink, the silicone rubber ink and the electrolyte ink into the syringe; S4, using an extrusion 3D printer to drive a syringe to print the air cathode and the aluminum anode on the PET film respectively, forming a structure in which the comb teeth of the aluminum anode and the comb teeth of the air cathode are interlaced and do not intersect with each other, and putting the prepared electrodes into a vacuum dryer for drying; S5. Put the dried electrode back into the extrusion 3D printer, and use the extrusion 3D printer to build a battery outer frame of silicone rubber on the outside of the electrode. After the battery outer frame is built, let it solidify at room temperature to form a stable structure; S6, filling the gaps between the comb teeth and between the electrode and the outer frame of the battery with hydrogel electrolyte, and setting the upper surface of the hydrogel electrolyte lower than the upper surfaces of the air cathode and the aluminum anode, and then placing the battery filled with electrolyte in an environment of -35°C to gel; S7. After solidification is completed, a solid-state aluminum-air battery is obtained.

5. A method for manufacturing a solid-state aluminum-air battery array, characterized in that: The following steps are involved: Manufacturing a plurality of individual aluminum-air batteries according to the manufacturing method of claim 4 at specific locations on the substrate; Connect the positive and negative tabs of different aluminum-air battery cells using conductive silver paste on the substrate; The solid-state aluminum-air battery array was prepared by drying in the open air at room temperature.