Method for cyclically preparing halide ions for preparing positive electrode material

Through electrochemical principles and redox reactions, the halide ions are recycled and regenerated in the electrode reactor, which solves the problem of iodine ions being unable to be reused, and efficient production of positive electrode materials is achieved, resource waste and production costs are reduced, and battery performance is improved.

CN119061409APending Publication Date: 2024-12-03NINGBO ZHONGWU NEW MATERIAL IND TECH RES INST CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310649017.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-06-02
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

In the prior art, when synthesizing the positive electrode material, iodine ions cannot be reused, resulting in waste of resources and degradation of battery performance, and the reaction is uncontrollable.

Method used

Using a cycle preparation method based on electrochemical principles and redox reaction, the halide ions are oxidized and reduced in the electrode reactor to return to the initial valence state, and the cyclic regeneration of the halide ions is achieved using a peristaltic pump.

Benefits of technology

It realizes the recycling of halide ions, reduces resource waste, simplifies process flow, improves production efficiency and battery performance, has wide adaptability, and is suitable for large-scale production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119061409A_ABST
    Figure CN119061409A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of secondary batteries, and particularly relates to a method for cyclically preparing halide ions for synthesizing a positive electrode material, which comprises the following steps: dissolving low-valence halide ions in electrolyte in a raw material reaction tank, adding raw materials, and performing oxidation-reduction reaction under the power of a power supply to synthesize the positive electrode material, according to the method, low-valence halide ions are oxidized into high-valence halide ions, electrolyte containing the high-valence halide ions is pumped into an electrode reactor by using a peristaltic pump to carry out oxidation-reduction reaction, the high-valence halide ions are reduced into the low-valence halide ions, and the reduced halide ions are pumped back into a raw material reaction tank by using the peristaltic pump. Based on an electrochemical principle and an oxidation-reduction reaction, a peristaltic pump is used for carrying out a reduction reaction on halide ions oxidized in the synthesis process of the positive electrode material in an electrode reactor, so that the halide ions return to an initial valence state, and cyclic preparation of the halide ions is realized.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of secondary batteries, and in particular relates to a method for cyclically preparing halide ions for synthesizing positive electrode materials. Background Art

[0002] The energy crisis has gradually become a major problem plaguing human society today. The low combustion efficiency and pollution generated by ordinary fossil fuels have put great pressure on the environment. Although renewable energy technologies such as wind power generation, tidal power generation, and nuclear power generation have been deployed on a large scale in my country, the intermittent and unstable nature of such renewable energy sources remains one of the factors limiting the development of these clean energy technologies. Therefore, developing new energy storage and conversion equipment is one of the effective ways to solve these current problems. Currently, the most common new energy conversion technology is lithium-ion battery technology, which has a series of advantages such as green environmental protection, strong continuity, and portability and miniaturization. As an important component of lithium-ion batteries, positive electrode materials play an important role in the development of lithium-ion battery technology.

[0003] In the prior art, when high-performance positive electrode materials are synthesized using chemical methods, iodide ions are used as a reducing agent to reduce and deintercalate materials while simultaneously intercalating metal ions. For example, in the journal (ACS Appl. Mater. Interfaces, 2016, 8(24): 15422-15429), NaI is used to reduce FePO4 in an acetonitrile solvent. The prepared NaFePO4 has an initial discharge capacity of 121 mAh / g at a current density of 10 mA / g, achieving good cycle performance. Although the produced positive electrode materials can achieve continuous, controllable and effective adjustment of electronic properties to optimize activity, and separation and purification are also convenient, the iodide ions cannot be reused after the synthesis of the positive electrode materials. Moreover, as the charge and discharge reactions proceed, the iodide ion concentration decreases, the interfacial reaction rate decreases, and the reaction becomes more uncontrollable, resulting in a low amount of intercalated metal ions, causing a decrease in battery performance. In the existing iodine production method, an appropriate amount of bisulfite is used to reduce iodate to iodide. The iodine recovery process is relatively complicated, and there is a waste of resources. Therefore, it is still urgent to develop high-performance cathode materials to meet the needs of various current electric devices. The repeated recycling of iodide ions is also very critical when preparing high-performance cathode materials on a large scale. Summary of the Invention

[0004] The purpose of the present invention is to provide a method for cyclically preparing halide ions for the synthesis of positive electrode materials in response to the above technical problems. Based on electrochemical principles and redox reactions, the electrochemical regulation of the electrolyte is achieved so that the halide ions, which are important components of the electrolyte, can be cyclically regenerated.

[0005] The method for cyclically preparing halide ions for synthesizing positive electrode materials in the technical solution of the present invention comprises the following steps: dissolving low-valent halide ions in an electrolyte in a raw material reaction tank, adding raw materials to carry out an oxidation-reduction reaction to synthesize the positive electrode material under power of a power source, wherein the low-valent halide ions are oxidized to high-valent halide ions, using a peristaltic pump to pump the electrolyte containing the high-valent halide ions into an electrode reactor for an oxidation-reduction reaction, wherein the high-valent halide ions are reduced to low-valent halide ions, and then using a peristaltic pump to pump the reduced halide ions back to the raw material reaction tank.

[0006] The present invention is based on electrochemical principles and redox reactions. By reducing the oxidized halide ions in an electrode reactor, the halide ions are returned to their final valence state, thereby realizing the recycling of halide ions. The process is simple to operate, has low energy consumption, and is widely adaptable, thus avoiding the waste of resources in traditional recycling processes.

[0007] Furthermore, the halide ion is one or both of iodide ion and bromide ion.

[0008] Furthermore, the concentration of the halide ions after being dissolved in the electrolyte is 0.05 to 2.0 mol / L.

[0009] Furthermore, the electrolyte is an organic solution containing positive electrode material cations. When the positive electrode material to be prepared contains lithium, the electrolyte is an organic solution containing lithium ions, and the solutes of the electrolyte can be listed as LiI, LiBr, LiTFSI, LiFSI, LiPF6, LiAsF6, LiSbF6, LiClO4, LiAlCl4, LiGaCl4, LiB 10 Cl 10 When the positive electrode material to be prepared contains sodium, the electrolyte is an organic solution containing sodium ions, and the solute of the electrolyte can be listed as NaI, NaBr, NaPF6, NaAsF6, NaSbF6, NaClO4, NaAlCl4, NaGaCl4, NaB 10 Cl 10 The solvent of the electrolyte is a carbonate ester, and the carbonate ester can be one or more of dimethyl carbonate, ethylene carbonate, propylene carbonate, propylene carbonate, and methyl ethyl carbonate.

[0010] Furthermore, the raw material reaction tank includes a liquid inlet pipe, a liquid outlet pipe and an air inlet pipe. The liquid inlet pipe and the air inlet pipe are placed at the upper end of the raw material reaction tank, and the liquid outlet pipe is placed at the lower end of the raw material reaction tank. A microporous filter is provided at the end of the liquid outlet pipe close to the liquid surface.

[0011] When the positive electrode material is synthesized in the raw material reaction tank, argon gas is introduced from the air inlet pipe. After the positive electrode material is synthesized, the electrolyte containing high-valent halide ions is pumped into the electrode reactor through the liquid outlet pipe by a peristaltic pump. The microporous filter can only pass the electrolyte to prevent the positive electrode material from flowing into the electrode reactor. The high-valent halide ions are reduced to low-valent halide ions in the electrode reactor, and the electrolyte containing low-valent halide ions is pumped back to the raw material reaction tank through the liquid inlet pipe by the peristaltic pump.

[0012] Furthermore, the raw material is a compound that can be reduced to form a positive electrode material after intercalation of a metal element. For example, if the positive electrode material to be prepared is LiFePO4, the raw material is FePO4, which is reduced to form LiFePO4 after intercalation of lithium; if the positive electrode material to be prepared is Li2Fe2(SO4)3, the raw material is Fe2(SO4)3.

[0013] Furthermore, the positive electrode material is a positive electrode material of a metal ion battery, and the metal elements of the metal ion battery include but are not limited to one or more of lithium, sodium, potassium, magnesium, and zinc.

[0014] Preferably, the positive electrode material is one or more of a transition metal oxide containing the corresponding metal element of the metal ion battery, a phosphate containing the corresponding metal element of the metal ion battery, and a sulfate containing the corresponding metal element of the metal ion battery.

[0015] Lithium-containing transition metal oxides can be listed as LiMn2O4, LiNiO2, LiMnO2, LiV2O5, lithium-containing phosphates can be listed as LiFePO4, Li2FePO4F, LiVPO4F, and lithium-containing sulfates can be listed as Li2Fe(SO4)2, Li2Fe2(SO4)3; sodium-containing transition metal oxides can be listed as NaMn2O4, NaNiO2, NaMnO2, sodium-containing phosphates can be listed as NaFePO4, Na2FePO4F, NaVPO4F, and sodium-containing sulfates can be listed as Na2FeSO4, Na2Fe2(SO4)3.

[0016] Furthermore, the electrode reactor includes, from left to right, a graphite plate, a reducing medium, a diaphragm, a polytetrafluoroethylene ring with a reaction cavity therein, a graphite felt, and a graphite plate.

[0017] Furthermore, the reducing medium is one or more of lithium sheets, sodium sheets, and magnesium sheets.

[0018] Furthermore, the current density during the redox reaction is 0.1 to 50 mA / cm 2 .

[0019] Compared with the prior art, the technical solution of the present invention has the following beneficial effects:

[0020] (1) The present invention is based on electrochemical principles and redox reactions, and uses a peristaltic pump to reduce the halide ions oxidized during the synthesis of the positive electrode material in an electrode reactor, so that the halide ions return to their original valence state, thereby realizing the cyclic preparation of halide ions;

[0021] (2) The method for preparing halide ions by circulation of the present invention improves the applicability of the production line, shortens the process flow, reduces material waste, increases production output, and reduces production costs;

[0022] (3) The present invention can flexibly adjust the regeneration degree at any time according to actual needs to achieve the purpose of regenerating the electrolyte, with high flexibility and wide adaptability. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 Schematic diagram of a reaction device for a cyclic regeneration method of halide ions used in preparing positive electrode materials in a preferred embodiment of the present invention;

[0024] Figure 2 is an enlarged schematic diagram of the electrode reactor;

[0025] Figure 3 It is an enlarged schematic diagram of the raw material reaction tank;

[0026] In the figure, 1-electrode reactor, 11-graphite plate, 12-reducing medium, 13-diaphragm, 14-polytetrafluoroethylene ring with reaction cavity, 15-graphite felt, 16-graphite plate; 2-peristaltic pump; 3-raw material reaction tank, 31-liquid inlet pipe, 32-air inlet pipe, 33-liquid outlet pipe, 34-microporous filter. DETAILED DESCRIPTION

[0027] The technical solution of the present invention will be further described below by means of specific examples and accompanying drawings. It should be understood that the specific embodiments described herein are only used to help understand the present invention and are not intended to be limiting of the present invention. The accompanying drawings used herein are only for the purpose of better illustrating the present invention and do not limit the scope of protection. Unless otherwise specified, the raw materials used in the embodiments of the present invention are all commonly used raw materials in the art, and the methods used in the embodiments are all conventional methods in the art.

[0028] The reaction device of the halogen ion recycling method for preparing positive electrode materials of the present invention is as follows Figure 1 As shown, it includes an electrode reactor 1, a peristaltic pump 2 and a raw material reaction tank 3, and the electrode reactor 1 and the raw material reaction tank 3 are connected through the peristaltic pump 2; the specific structure of the electrode reactor 1 is as shown Figure 2As shown, it includes a graphite plate 11, a reducing medium 12, a diaphragm 13, a polytetrafluoroethylene ring 14 with a reaction cavity, a graphite felt 15, and a graphite plate 16. The electrode reactor 1 is fixed by bolts, and the redox reaction occurs in the cavity of the polytetrafluoroethylene ring 14 with a reaction cavity. The specific structure of the raw material reaction tank 3 is as shown in FIG. Figure 3 As shown, it includes a liquid inlet pipe 31, an air inlet pipe 32, a liquid outlet pipe 33 and a microporous filter 34. The liquid inlet pipe 31 and the air inlet pipe 32 are placed at the upper end of the raw material reaction tank 3, and the liquid outlet pipe 33 is placed at the lower end of the raw material reaction tank 3. A microporous filter 34 is set at the end of the liquid outlet pipe 33 close to the liquid surface. When the positive electrode material is synthesized in the raw material reaction tank 3, argon gas is introduced from the air inlet pipe 32. After the positive electrode material is synthesized, the electrolyte containing high-valent halide ions is pumped into the electrode reactor 1 by the peristaltic pump 2 through the liquid outlet pipe 33. The microporous filter 34 can prevent the positive electrode material from flowing into the electrode reactor 1. The high-valent halide ions are reduced to low-valent halide ions in the electrode reactor 1, and the electrolyte containing low-valent halide ions is pumped back to the raw material reaction tank 3 by the peristaltic pump 2 through the liquid inlet pipe 31.

[0029] Example 1

[0030] The method for cyclically preparing halide ions in this embodiment comprises the following steps:

[0031] (1) LiI was dissolved in an electrolyte (1 mol / L dimethyl carbonate solution containing LiPF6) in a raw material reaction tank and stirred at 300 r / min to fully dissolve LiI (the concentration of LiI was 0.08 mol / L). FePO4 was added, and the molar ratio of FePO4 to LiI was 1:1;

[0032] (2) At 0.5 mA / cm 2 The current density provides power to the reaction device, reducing FePO4 to LiFePO4. - Oxidized to I3 - ;

[0033] (3) Use a peristaltic pump to pump the liquid containing I3 - The electrolyte is pumped into the electrode reactor, and the reducing medium Li sheet in the electrode reactor converts I3 - Oxidized to I - , and then use a peristaltic pump to pump the - The electrolyte is pumped back to the raw material reaction tank, thus achieving I - of recycling.

[0034] Example 2

[0035] The method for cyclically preparing halide ions in this embodiment comprises the following steps:

[0036] (1) Dissolve LiBr in an electrolyte (1 mol / L dimethyl carbonate solution containing LiPF6) in a raw material reaction tank and stir at 300 r / min to fully dissolve LiBr (the concentration of LiBr is 0.10 mol / L). Add FePO4 with a molar ratio of FePO4 to LiBr of 1:1.

[0037] (2) At 0.5 mA / cm 2 The current density provides power to the reaction device, reducing FePO4 to LiFePO4. - Oxidized to Br3 - ;

[0038] (3) Use a peristaltic pump to pump the Br3 - The electrolyte is pumped into the electrode reactor, and the reducing medium Li sheet in the electrode reactor converts Br3 - Oxidized to Br - , and then use a peristaltic pump to pump the Br - The electrolyte is pumped back to the raw material reaction tank, thus achieving Br - of recycling.

[0039] Example 3

[0040] The method for cyclically preparing halide ions in this embodiment comprises the following steps:

[0041] (1) NaI was dissolved in an electrolyte (1 mol / L propylene carbonate solution containing NaPF6) in a raw material reaction tank and stirred at 300 r / min to fully dissolve the NaI (the concentration of NaI was 0.08 mol / L). FePO4 was added, and the molar ratio of FePO4 to NaI was 1:1;

[0042] (2) At 0.8 mA / cm 2 The current density provides power to the reaction device, reducing FePO4 to NaFePO4. - Oxidized to I3 - ;

[0043] (3) Use a peristaltic pump to pump the liquid containing I3 - The electrolyte is pumped into the electrode reactor, and the reducing medium Na sheet in the electrode reactor converts I3 - Oxidized to I - , and then use a peristaltic pump to pump the - The electrolyte is pumped back to the raw material reaction tank, thus achieving I - of recycling.

[0044] Example 4

[0045] The method for cyclically preparing halide ions in this embodiment comprises the following steps:

[0046] (1) In a raw material reaction tank, NaBr was dissolved in an electrolyte (1 mol / L propylene carbonate solution containing NaPF6) and stirred at 300 r / min to fully dissolve the NaBr (the concentration of NaBr was 0.12 mol / L). FePO4 was added, and the molar ratio of FePO4 to NaBr was 1:1;

[0047] (2) At 1.2 mA / cm 2 The current density provides power to the reaction device, reducing FePO4 to NaFePO4. - Oxidized to Br3 - ;

[0048] (3) Use a peristaltic pump to pump the Br3 - The electrolyte is pumped into the electrode reactor, and the reducing medium Na sheet in the electrode reactor converts Br3 - Oxidized to Br - , and then use a peristaltic pump to pump the Br - The electrolyte is pumped back to the raw material reaction tank, thus achieving Br - of recycling.

[0049] Finally, it should be noted that the specific embodiments described herein are merely illustrative of the spirit of the present invention and are not intended to limit the manner in which the present invention is intended to be implemented. Persons skilled in the art may make various modifications, additions, or substitutions to the described embodiments, and it is not necessary or possible to provide a comprehensive list of all possible embodiments. However, any obvious changes or modifications arising from the essential spirit of the present invention remain within the scope of protection of the present invention, and interpreting them as any additional limitations would be contrary to the spirit of the present invention.

Claims

1. A method for cyclically preparing halide ions for synthesis of positive electrode materials, characterized in that: The method comprises the following steps: dissolving low-valent halide ions in an electrolyte in a raw material reaction tank, adding raw materials to carry out redox reaction under power to synthesize positive electrode materials, the low-valent halide ions are oxidized to high-valent halide ions, using a peristaltic pump to pump the electrolyte containing the high-valent halide ions into an electrode reactor for redox reaction, the high-valent halide ions are reduced to low-valent halide ions, and then using a peristaltic pump to pump the reduced halide ions back to the raw material reaction tank.

2. The method according to claim 1, characterized in that The halide ion is one or both of iodide ion and bromide ion.

3. The method according to claim 1, characterized in that The concentration of halide ions after dissolving in the electrolyte is 0.05 to 2.0 mol / L.

4. The method according to claim 1, characterized in that The raw material reaction tank comprises a liquid inlet pipe, a liquid outlet pipe and an air inlet pipe, wherein the liquid inlet pipe and the air inlet pipe are arranged at the upper end of the raw material reaction tank, the liquid outlet pipe is arranged at the lower end of the raw material reaction tank, and a microporous filter is arranged at one end of the liquid outlet pipe close to the liquid surface.

5. The method according to claim 1, characterized in that The electrode reactor includes, from left to right, a graphite plate, a reducing medium, a diaphragm, a polytetrafluoroethylene ring with a reaction cavity inside, a graphite felt and a graphite plate.

6. The method according to claim 5, characterized in that The reducing medium is one or more of lithium flakes, sodium flakes and magnesium flakes.

7. The method according to claim 1, characterized in that The positive electrode material is a positive electrode material of a metal ion battery, and the metal element of the metal ion battery is one or more of lithium, sodium, potassium, magnesium, and zinc.

8. The method according to claim 7, characterized in that The positive electrode material is one or more of transition metal oxides containing metal elements corresponding to metal ion batteries, phosphates containing metal elements corresponding to metal ion batteries, and sulfates containing metal elements corresponding to metal ion batteries.

9. The method according to claim 1, characterized in that: The electrolyte is an organic solution containing cations of the positive electrode material.

10. The method according to claim 1, characterized in that The current density during the redox reaction is 0.1~50mA / cm 2 .