Production process of tencel hemp core-spun weft elastic non-ironing woven fabric
By using Tensil linen blended yarn and blended core-packed spandex yarn in high-heat content fabrics, combined with wool burning and washing processes, the problem of insufficient elasticity of shirts with high-heat content is solved, and high-heat content and comfortable wearing are achieved Fabric production.
Patent Information
- Application Number
- CN202411553844.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-11-04
- Publication Date
- 2024-12-03
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing high-heat content shirts lack elasticity, and the weft direction of the warp hemp yarn does not contain erotic elastic yarn, which leads to a tingling and poor elastic recovery when worn.
Tensil linen blended yarn is used as warp yarn, and Tensil linen blended core spandex yarn is used as weft yarn. It is washed by burning, loose water, drying, overflow, free ironing, baking, water washing, The process of tenting and pre-shrinking rolling is optimized to improve the elasticity and comfort of the fabric.
It has achieved good elasticity and comfortable wearing experience of high-seed fabrics, met the market's demand for spandex elastic fabrics with a linen blended core-packed spandex, and achieved excellent elastic effects of more than 30% of the sesame content, more than 15% of the elastic recovery and less than 6%.
Smart Images

Figure SMS_1
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of textiles, and in particular relates to a production process for a Tencel hemp core-spun weft-elastic wrinkle-free woven fabric. Background Art
[0002] Linen shirts are garments made of natural linen fibers and have many unique characteristics. Linen fabrics are usually light and soft, with a cool texture, giving people a comfortable and relaxed feeling. They have good air permeability and moisture absorption, can regulate body temperature, keep the body dry, and are especially suitable for hot summers. However, due to the rigidity of linen fibers, most of the existing high-linen shirts are non-elastic, and they feel itchy when worn close to the skin. Elastic linen fabrics are also mostly made of linen yarns in the warp direction and non-linen elastic yarns in the weft direction to achieve elasticity. There is a lack of fabrics produced by truly high-linen core-spun yarns.
[0003] Chinese invention patent CN112981665A discloses a method for preparing a linen stretch fabric, wherein the warp yarn is a yarn made of all-linen fiber, and the weft yarn is a fancy yarn made by wrapping linen yarn with T-400 and Lycra, and the weft process is a wrapping process, which is different from the core-spun process, and T-400 is polyester, and the foreign market currently has a high resistance to polyester products; Chinese invention patent CN107177922A discloses a linen stretch fabric, wherein the yarn process is to twist the spun yarn using a fine spinning machine to make fine yarn with a twist coefficient of 1.1, and then dry and wind it into 50Nm yarn, and then Two of the above yarns are taken together with 40D spandex lycra on a covering yarn machine to make linen spandex lycra stretch yarn, which is a two-stage process, and the pure linen has high rigidity, large elastic elongation, and extremely poor elastic recovery and residual; Chinese invention patent CN111560689A discloses a high-elastic linen coated XLA fiber mercerized stretch fabric and a preparation method thereof, wherein the stretch fabric is woven from linen stretch core-spun yarn, including linen fiber, XLA stretch fiber, and an intermediate layer, wherein an intermediate layer is added between the linen yam and the XLA stretch fiber filaments, and the XLA filaments need to be polished, resulting in a decrease in the strength of the stretch yarn and an increase in production costs. Summary of the invention
[0004] The technical problem to be solved by the present invention is to provide a production process of a Tencel hemp core-spun weft-elastic wrinkle-free woven fabric, which has a high hemp content and has good elasticity while having the characteristics of a hemp fabric, thereby improving the itching problem of hemp fabrics.
[0005] The present invention is achieved through the following technical solutions: The production process of the Tencel linen core-spun weft-elastic wrinkle-free woven fabric described in the present invention uses Tencel linen blended yarn as warp yarn and Tencel linen blended core-spun spandex yarn as weft yarn, and the yarn is subjected to spinning, bleaching, dyeing, weaving and finishing steps to obtain the fabric, wherein the finishing step sequentially includes singeing, loose washing, drying, overflow, wrinkle-free, baking, washing, stretching and pre-shrinking and curling processes.
[0006] Preferably, the spinning process: the Tencel and linen blended core-spun spandex yarn is obtained by blending Tencel and linen fibers with core-spun spandex, the average length of the linen fibers is 20~30mm, the blending ratio is linen fiber: Tencel = 20~45%: 55~80%, the spandex drafting multiple is 2.8~3.5 times, the twist is 15~30 / inch, and the yarn count is 16s~30s; the Tencel and linen blended yarn is obtained by blending Tencel and linen fibers, the blending ratio is linen fiber: Tencel = 20~45%: 55~80%, and the yarn count is 16s~30s.
[0007] Preferably, the bleaching and dyeing process: the warp yarn is treated with a pre-treatment process at 115°C to 135°C for 15min to 30min, and then dyed at 60°C to 80°C.
[0008] Preferably, the weaving process: the machine speed is 300~350r / min.
[0009] Preferably, the finishing process: The singeing process: vehicle speed 110~130m / min, flame intensity 8~13; The loose-type water washing process: vehicle speed 30-60 m / min, water washing temperature 90-95°C, steamer temperature 90-100°C, desizing vehicle speed 85-95°C, trough temperature 35-40°C; the auxiliary agents used include: high-temperature desizing enzyme 5-10 g / L, refining agent 5-10 g / L, and penetrant 1-5 g / L; wherein the high-temperature desizing enzyme is preferably DS-HT, a product of Zibo Lurui Fine Chemical Co., Ltd., the refining agent is preferably XC-J, a product of Zibo Lurui Fine Chemical Co., Ltd., and the penetrant is preferably WR-03, a product of Qingdao Onosi Industry and Trade Co., Ltd.; The drying process: speed 50~70m / min, temperature 100~120℃; The overflow process: the temperature is 50-70°C, and the auxiliary agent used includes 1-3g / L cellulase CR, preferably produced by Novozymes; The non-ironing process: the vehicle speed is 60-80m / min, the drying room temperature is 90-110℃, and the auxiliary agents used include: 1-5g / L acid-base stabilizer PH-X, 40-160g / L non-ironing resin ERF-N, 40-150g / L resin catalyst 530, 20-40g / L formaldehyde scavenger FDS, 5-30g / L fiber protection agent SF-P, 5-30g / L hydrophilic softener SEH-02; the components of the auxiliary agents are preferably produced by Zibo Lurui Fine Chemical Co., Ltd.; The baking process: vehicle speed 20~50m / min, drying room temperature 150~170℃; The water washing process: temperature 50-70°C, vehicle speed 50-70m / min, acid tank pH 3-5; The tentering process: pressure 1.1-2 bar, vehicle speed 50-70 m / min, drying room temperature 100-120°C, the auxiliary agent used is 1-5 g / L acid-base stabilizer PH-X, preferably produced by Zibo Lurui Fine Chemical Co., Ltd.; The pre-shrinking and rolling process: the vehicle speed is 50-70 m / min.
[0010] Compared with the prior art, the present invention has the following beneficial effects: The present invention effectively solves the pain points of low hemp content and inability to directly core-spun hemp fabrics under conventional weaving processes, and meets the market demand for hemp blended core-spun spandex stretch fabrics. The fabric can achieve a hemp content of more than 30%, and an elasticity of more than 15% and an elastic recovery of more than 55% under the ASTMD3107-07 (2019) standard, with excellent residual elasticity of less than 6%, achieving the effect of high hemp content in hemp fabrics and being comfortable and not tight to wear, while also improving the itchiness of the linen fabric.
[0011] The production process of the Tencel hemp core-spun weft-elastic wrinkle-free woven fabric proposed in the present invention combines the spinning technology with high hemp content and the finishing technology adapted thereto, optimizes the entire process from raw material selection to specific procedures, and finally realizes the combination of the natural texture and elasticity of the hemp fiber in the fabric.
[0012] In the spinning process, the present invention adopts the spandex processing technology of blending Tencel and hemp fiber, and improves the spinnability of the yarn by controlling the length of hemp fiber (average length 20-30 mm), blending ratio (hemp fiber: Tencel = 20-45%: 55-80%), the drafting multiple of spandex (2.8-3.5 times), the twist of the yarn (15-30 / inch) and the yarn count (16s-30s), so as to ensure that the yarn has both the air permeability and moisture absorption of the hemp fiber and good elasticity and strength. This blended yarn, as the warp yarn, provides a solid foundation for the fabric; and in the selection of the weft yarn, the present invention adopts the Tencel-hemp blended core-spun spandex yarn, which further enhances the elasticity and comfort of the fabric. The introduction of this yarn enables the fabric to better adapt to the curve of the human body while maintaining the characteristics of the hemp fiber, providing a more fitting wearing experience. In the bleaching and dyeing process, a yarn setting process of 115℃~135℃ and 15min~30min is adopted.
[0013] In the finishing process, multiple processes such as singeing, loose washing, drying, overflow, free ironing, baking, washing, stretching and pre-shrinking and curling were optimized to further improve the quality and feel of the fabric. In the singeing process, the fluff on the surface of the fabric is effectively removed by controlling the speed and flame intensity, thereby improving the neatness and glossiness of the fabric. The loose washing process completely removes the sizing and impurities on the fabric and protects the original properties of the fiber by precisely controlling the washing temperature, steamer temperature, desizing speed and trough temperature, as well as using specific auxiliaries. The drying process ensures the stability and consistency of the fabric in subsequent processing. The overflow process uses specific auxiliaries to give the fabric a soft feel and improve the itchy feeling. The iron-free process uses a specific combination of auxiliaries to make the fabric have good wrinkle resistance while maintaining elasticity and softness. The baking process further consolidates the color and shape stability of the fabric. The washing process removes excess auxiliaries on the fabric and adjusts the pH value of the fabric to make it more in line with the physiological needs of human skin. The tentering process achieves the expected width and stability of the fabric by precisely controlling the pressure and drying room temperature. Finally, the pre-shrinking and rolling process ensures the dimensional stability of the fabric in subsequent processing and use. Through this series of fine finishing processes, the fabric not only maintains the natural texture of the hemp fiber, but also has good elasticity, wrinkle resistance and dimensional stability, thus achieving the technical effect of containing both hemp and elasticity. DETAILED DESCRIPTION
[0014] In order to make the purpose, technical method, application scope, product effect and advantages of the present invention clearer, the following will be described clearly and completely in conjunction with the implementation case of the present invention. All raw materials used in the examples are commercially available unless otherwise specified.
[0015] Example 1 The production process of the Tencel linen core-spun weft-elastic wrinkle-free woven fabric uses Tencel linen blended yarn as warp yarn and Tencel linen blended core-spun spandex yarn as weft yarn, and the yarn is subjected to spinning, bleaching, dyeing, weaving and finishing processes to obtain the fabric, wherein the finishing process sequentially includes singeing, loose washing, drying, overflow, wrinkle-free, baking, washing, stretching and pre-shrinking and rolling processes.
[0016] Spinning process: Tencel and linen blended core-spun spandex yarn is obtained by blending tencel and linen fibers with core-spun spandex. The average length of the linen fiber is 20 mm, the blending ratio is linen fiber: tencel = 20%: 80%, the spandex drafting multiple is 2.8 times, the twist is 15 / inch, and the yarn count is 16s; Tencel and linen blended yarn is obtained by blending tencel and linen fibers, the blending ratio is linen fiber: tencel = 20%: 80%, and the yarn count is 16s.
[0017] Bleaching and dyeing process: The warp yarn is treated with a pre-treatment process at 115°C for 30 minutes, and then dyed at 60°C.
[0018] Weaving process: speed 300r / min.
[0019] Finishing process: The singeing process: vehicle speed 110m / min, flame intensity 8mbar; The loose-type water washing process: vehicle speed 30m / min, water washing temperature 90°C, steamer temperature 90°C, desizing vehicle speed 85°C, trough temperature 35°C; the auxiliary agents used include: high-temperature desizing enzyme 5g / L, refining agent 5g / L, and penetrant 1g / L; wherein the high-temperature desizing enzyme is DS-HT, a product of Zibo Lurui Fine Chemical Co., Ltd., the refining agent is XC-J, a product of Zibo Lurui Fine Chemical Co., Ltd., and the penetrant is WR-03, a product of Qingdao Onosi Industry and Trade Co., Ltd.; The drying process: speed 50m / min, temperature 100°C; The overflow process: the temperature is 50°C, and the additives used include 1g / L cellulase CR, preferably produced by Novozymes; The non-ironing process: the vehicle speed is 60m / min, the drying room temperature is 90℃, and the additives used include: 1g / L acid-base stabilizer PH-X, 40g / L non-ironing resin ERF-N, 40g / L resin catalyst 530, 20g / L formaldehyde scavenger FDS, 5g / L fiber protector SF-P, 5g / L hydrophilic softener SEH-02; all the components of the additives are produced by Zibo Lurui Fine Chemical Co., Ltd.; The baking process: vehicle speed 20m / min, drying room temperature 150°C; The water washing process: temperature 50°C, vehicle speed 50m / min, acid tank pH 3; The tentering process: pressure 1.1 bar, vehicle speed 50 m / min, drying room temperature 100°C, the auxiliary agent used is 1g / L acid-base stabilizer PH-X, produced by Zibo Lurui Fine Chemical Co., Ltd.; The pre-shrinking and rolling process: the vehicle speed is 50m / min.
[0020] Example 2 The production process of the Tencel linen core-spun weft-elastic wrinkle-free woven fabric uses Tencel linen blended yarn as warp yarn and Tencel linen blended core-spun spandex yarn as weft yarn, and the yarn is subjected to spinning, bleaching, dyeing, weaving and finishing processes to obtain the fabric, wherein the finishing process sequentially includes singeing, loose washing, drying, overflow, wrinkle-free, baking, washing, stretching and pre-shrinking and rolling processes.
[0021] Spinning process: Tencel and linen blended core-spun spandex yarn is obtained by blending tencel and linen fibers with core-spun spandex. The average length of the linen fiber is 25 mm, the blending ratio is linen fiber: tencel = 30%: 70%, the spandex drafting multiple is 3.0 times, the twist is 20 / inch, and the yarn count is 21s; Tencel and linen blended yarn is obtained by blending tencel and linen fibers, the blending ratio is linen fiber: tencel = 30%: 70%, and the yarn count is 21s.
[0022] Bleaching and dyeing process: The warp yarn is treated with a pre-treatment process at 125°C for 20 minutes, and then dyed at 70°C.
[0023] Weaving process: speed 330r / min.
[0024] Finishing process: The singeing process: vehicle speed 120m / min, flame intensity 10mbar; The loose-type water washing process: vehicle speed 45m / min, water washing temperature 92°C, steamer temperature 95°C, desizing vehicle speed 90°C, trough temperature 38°C; the auxiliary agents used include: high-temperature desizing enzyme 8g / L, refining agent 8g / L, and penetrant 3g / L; wherein the high-temperature desizing enzyme is DS-HT, a product of Zibo Lurui Fine Chemical Co., Ltd., the refining agent is XC-J, a product of Zibo Lurui Fine Chemical Co., Ltd., and the penetrant is WR-03, a product of Qingdao Onosi Industry and Trade Co., Ltd.; The drying process: speed 60m / min, temperature 110°C; The overflow process: the temperature is 60°C, and the additives used include 2g / L cellulase CR, preferably produced by Novozymes; The non-ironing process: the vehicle speed is 70m / min, the drying room temperature is 100℃, and the additives used include: 3g / L acid-base stabilizer PH-X, 100g / L non-ironing resin ERF-N, 80g / L resin catalyst 530, 30g / L formaldehyde scavenger FDS, 25g / L fiber protection agent SF-P, 25g / L hydrophilic softener SEH-02; all the components of the additives are produced by Zibo Lurui Fine Chemical Co., Ltd.; The baking process: vehicle speed 35m / min, drying room temperature 160°C; The water washing process: temperature 60°C, vehicle speed 60m / min, acid tank pH 4; The tentering process: pressure 1.5 bar, vehicle speed 60 m / min, drying room temperature 110°C, the auxiliary agent used is 3g / L acid-base stabilizer PH-X, produced by Zibo Lurui Fine Chemical Co., Ltd.; The pre-shrinking and rolling process: the vehicle speed is 60m / min.
[0025] Example 3 The production process of the Tencel linen core-spun weft-elastic wrinkle-free woven fabric uses Tencel linen blended yarn as warp yarn and Tencel linen blended core-spun spandex yarn as weft yarn, and the yarn is subjected to spinning, bleaching, dyeing, weaving and finishing processes to obtain the fabric, wherein the finishing process sequentially includes singeing, loose washing, drying, overflow, wrinkle-free, baking, washing, stretching and pre-shrinking and rolling processes.
[0026] Spinning process: Tencel and linen blended core-spun spandex yarn is obtained by blending tencel and linen fibers with core-spun spandex. The average length of the linen fiber is 30 mm, the blending ratio is linen fiber: tencel = 45%: 55%, the spandex drafting multiple is 3.5 times, the twist is 30 / inch, and the yarn count is 30s; Tencel and linen blended yarn is obtained by blending tencel and linen fibers, the blending ratio is linen fiber: tencel = 45%: 55%, and the yarn count is 30s.
[0027] Bleaching and dyeing process: The warp yarn is treated with a pre-treatment process at 135°C for 15 minutes, and then dyed at 80°C.
[0028] Weaving process: speed 350r / min.
[0029] Finishing process: The singeing process: vehicle speed 130m / min, flame intensity 13mbar; The loose-type water washing process: vehicle speed 60m / min, water washing temperature 95°C, steamer temperature 100°C, desizing vehicle speed 95°C, trough temperature 40°C; the auxiliary agents used include: high-temperature desizing enzyme 10g / L, refining agent 10g / L, and penetrant 5g / L; wherein, the high-temperature desizing enzyme is DS-HT, a product of Zibo Lurui Fine Chemical Co., Ltd., the refining agent is XC-J, a product of Zibo Lurui Fine Chemical Co., Ltd., and the penetrant is WR-03, a product of Qingdao Onosi Industry and Trade Co., Ltd.; The drying process: speed 70m / min, temperature 120°C; The overflow process: the temperature is 70°C, and the additives used include 3g / L cellulase CR, preferably produced by Novozymes; The non-ironing process: the vehicle speed is 80m / min, the drying room temperature is 110℃, and the additives used include: 5g / L acid-base stabilizer PH-X, 160g / L non-ironing resin ERF-N, 150g / L resin catalyst 530, 40g / L formaldehyde scavenger FDS, 30g / L fiber protector SF-P, 30g / L hydrophilic softener SEH-02; all the components of the additives are produced by Zibo Lurui Fine Chemical Co., Ltd.; The baking process: vehicle speed 50m / min, drying room temperature 170°C; The water washing process: temperature 70°C, vehicle speed 70m / min, acid tank pH 5; The tentering process: pressure 2 bar, vehicle speed 70 m / min, drying room temperature 120°C, the auxiliary agent used is 5 g / L acid-base stabilizer PH-X, produced by Zibo Lurui Fine Chemical Co., Ltd.; The pre-shrinking and rolling process: the vehicle speed is 70m / min.
[0030] The fabrics obtained in Examples 1 to 3 were tested, and the results are shown in Table 1. The elasticity index is in accordance with the ASTM D3107-07 (2019) standard.
[0031] Table 1 Performance of Tencel hemp core-spun weft-elastic non-ironing woven fabrics in Examples 1 to 3
[0032] It can be seen from the data in Table 1 that the Tencel hemp core-spun weft-elastic wrinkle-free woven fabric produced by the process of the present invention has a high hemp content and good elastic properties, achieving the effect of a hemp fabric with a high hemp content and being comfortable and not tight to wear.
Claims
1. A production process for Tencel hemp core-spun weft-elastic non-ironing woven fabric, characterized in that: The fabric is obtained by taking Tencel and linen blended yarn as warp yarn and Tencel and linen blended core-spun spandex yarn as weft yarn through the processes of spinning, bleaching and dyeing, weaving and finishing. The finishing process sequentially includes singeing, loose washing, drying, overflowing, ironing-free, baking, washing, stretching and pre-shrinking and curling.
2. The production process of the Tencel hemp core-spun weft-elastic non-ironing woven fabric according to claim 1, characterized in that: Spinning process: Tencel and linen blended core-spun spandex yarn is obtained by blending tencel and linen fibers through core-spun spandex treatment. The average length of linen fiber is 20~30mm, and the blending ratio is linen fiber: tencel = 20~45%: 55~80%. The spandex drafting multiple is 2.8~3.5 times, the twist is 15~30 / inch, and the yarn count is 16s~30s.
3. The production process of the Tencel hemp core-spun weft elastic non-ironing woven fabric according to claim 1, characterized in that: Bleaching and dyeing process: use 115℃~135℃, 15min~30min pre-treatment process to treat the warp yarn, and then dye it at 60~80℃; weaving process: machine speed 300~350r / min.
4. The production process of the Tencel hemp core-spun weft-elastic non-ironing woven fabric according to claim 1, characterized in that: The singeing process: vehicle speed 110~130m / min, flame intensity 8~13mbar.
5. The production process of the Tencel hemp core-spun weft elastic non-ironing woven fabric according to claim 1, characterized in that: The loose water washing process: vehicle speed 30~60m / min, water washing temperature 90~95℃, steamer temperature 90~100℃, desizing vehicle speed 85~95℃, trough temperature 35~40℃; the auxiliary agents used include: high temperature desizing enzyme 5~10g / L, refining agent 5~10g / L, penetrant 1~5g / L.
6. The production process of the Tencel hemp core-spun weft elastic non-ironing woven fabric according to claim 1, characterized in that: The drying process: vehicle speed 50~70m / min, temperature 100~120℃.
7. The production process of the Tencel hemp core-spun weft-elastic non-ironing woven fabric according to claim 1, characterized in that: The overflow process: the temperature is 50-70°C, and the auxiliary agents used include 1-3 g / L of cellulase CR.
8. The production process of the Tencel hemp core-spun weft elastic non-ironing woven fabric according to claim 1, characterized in that: The non-ironing process: the vehicle speed is 60~80m / min, the drying room temperature is 90~110℃, and the additives used include: 1~5g / L acid-base stabilizer PH-X, 40-160g / L non-ironing resin ERF-N, 40-150g / L resin catalyst 530, 20~40g / L formaldehyde scavenger FDS, 5-30g / L fiber protection agent SF-P, and 5~30g / L hydrophilic softener SEH-02.
9. The production process of the Tencel hemp core-spun weft elastic non-ironing woven fabric according to claim 1, characterized in that: The baking process: the vehicle speed is 20-50 m / min, the drying room temperature is 150-170° C.; the washing process: the temperature is 50-70° C., the vehicle speed is 50-70 m / min, and the acid tank pH is 3-5.
10. The production process of the Tencel hemp core-spun weft elastic non-ironing woven fabric according to claim 1, characterized in that: The tentering process: pressure 1.1~2bar, vehicle speed 50~70m / min, drying room temperature 100~120℃, the auxiliary agent used is 1~5g / L acid-base stabilizer PH-X; the pre-shrinking and rolling process: vehicle speed 50~70m / min.
Citation Information
Patent Citations
Method for preparing elastic linen fabric
CN107177922A
High-elasticity flax and XLA fiber coated mercerized elastic fabric and preparation method thereof
CN111560689A
Preparation method of linen elastic fabric
CN112981665A
Preparation method of linen flat-strip fabric
CN107419403A
Flax tencel weft elastic fabric production process
CN118292166A