Method for evaluating long-term safety of degraded structure of tunnel support system
By calculating the corrosion rate and mechanical parameters of the steel frame, it determines its safety in the tunnel support system, establishes a three-dimensional structural mechanical model, solves the safety assessment problem caused by deterioration in tunnel operation, and realizes the tunnel support system The long-term safety evaluation ensures operational safety.
Patent Information
- Application Number
- CN202411201283.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-29
- Publication Date
- 2024-12-03
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
During the operation of the existing tunnel support system, due to environmental erosion and other factors, it is difficult to effectively evaluate its long-term safety. The existing evaluation methods are mainly applicable to the design and construction stages and cannot meet the safety needs of operating tunnels.
By calculating the corrosion rate of the steel frame, determining its mechanical parameters and the combined structural interface bonding structure, establishing the initial support-secondary lining three-dimensional solid load structure mechanical model of the steel frame after corrosion, extracting internal forces and conducting safety evaluation , including corrosion rate determination, mechanical parameter calculation, interface bond structure determination and three-dimensional model simulation.
Accurate safety evaluation of tunnel support system after deterioration, ensure long-term operation safety of tunnel, fill the gap in the theory of bonding and slip of rust steel frame-concrete interface, and provide bonding and slip of rust steel frame-concrete interface The constitutive relationship is shifted to ensure the safety assessment of the structure.
Smart Images

Figure CN119066871A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of tunnel engineering, and in particular to a method for evaluating the long-term safety of a tunnel support system after the system has deteriorated. Background Art
[0002] After tunnel excavation and secondary lining construction, the surrounding rock is in a tertiary stress state. After a period of dynamic adjustment, the surrounding rock-primary support-secondary lining is in a mechanical equilibrium state. As time goes by, the support system is affected by factors such as surrounding rock characteristics, geological structure, environmental erosion, construction disturbance, and operating vehicle disturbance, and the surrounding rock, primary support, and secondary lining components may deteriorate. For example, the erosion caused by groundwater flow and seepage will cause surrounding rock deterioration; in a groundwater environment rich in chloride ions and sulfate ions, shotcrete will deteriorate, and anchor rods, steel frames, and steel bars will rust. After the support system deteriorates, on the one hand, the material mechanical parameters of the surrounding rock, primary support, and secondary lining are constantly changing; on the other hand, the mechanical constitutive relationship of the interface of the support system components will change; these two aspects lead to nonlinear stress transfer between the tunnel surrounding rock-primary support-secondary lining, thereby changing the stress state of the support structure system, thereby affecting the long-term safety of the tunnel support system. Therefore, it is urgent to establish a set of long-term safety evaluation methods for the structure after the tunnel support system deteriorates.
[0003] The existing tunnel safety evaluation generally uses the damage stage method to evaluate the safety of initial support and secondary lining according to the "Highway Tunnel Design Code Volume 1 Civil Engineering" (JTG3370.1) and the "Railway Tunnel Design Code" (TB10003-2016). This method is mainly applicable to the design and construction stages. For operating tunnels, the support system will deteriorate due to the influence of the engineering environment, so the safety evaluation of operating tunnels needs to consider material degradation. Summary of the invention
[0004] The purpose of the present invention is to provide a method for evaluating the long-term safety of a tunnel support system after the system has deteriorated, thereby ensuring the long-term operation safety of the tunnel.
[0005] To achieve the above object, the present invention provides a method for evaluating the long-term safety of a tunnel support system after degradation, comprising the following steps:
[0006] S1. Calculate the corrosion rate of the steel frame, and determine the mechanical parameters of the steel frame after corrosion based on the corrosion rate;
[0007] S2. Determine the interface bonding constitutive property of the composite structure after the steel frame is corroded;
[0008] S3. Establish a three-dimensional solid load structural mechanics model of initial support-secondary lining after corrosion of steel frame;
[0009] S4, extract the internal forces of initial support and secondary lining, and calculate the structural bending moment and axial force;
[0010] S5. Evaluate the safety of initial support and secondary lining.
[0011] Preferably, in step S1, the corrosion rate of the steel frame is calculated, and the specific operation is as follows:
[0012] Cut off a section of rusted steel frame in the tunnel, remove the rust products of the rusted steel frame with hydrochloric acid solution, then neutralize it with 3% sodium carbonate solution, finally wash it with clean water, and put it into an oven for drying;
[0013] Weigh the steel frame after rust removal to obtain the mass m of the steel frame after rusting. c , and compared with the mass m of the non-corroded steel frame of the same specification and length, the actual corrosion loss mass Δm is further obtained;
[0014] Finally, the corrosion rate of the steel frame is calculated. The calculation formula of the corrosion rate is as follows:
[0015]
[0016] Among them, ρ is the actual corrosion rate.
[0017] Preferably, in step S1, the mechanical parameters of the corroded steel frame include yield strength, ultimate strength and ultimate strain, and the calculation formulas are as follows:
[0018]
[0019] ε suc =e -3.789ρ ε su0 (4)
[0020] Among them, f yc 、f uc , ε suc are the yield strength, ultimate strength and ultimate strain of the corroded steel frame; f y0 、f u0 , ε su0 are the yield strength, ultimate strength and ultimate strain of the corresponding non-corroded steel frame, respectively.
[0021] Preferably, in step S2, the interface bonding constitutive property of the combined structure after the steel frame is corroded is determined, and the specific operation is as follows:
[0022] S21, determining the size of the steel frame concrete component, manufacturing the steel frame concrete component, and then obtaining the steel frame concrete components with different corrosion rates through electrical acceleration test;
[0023] S22. The bond strength-slip curves of the steel frame-concrete interface with different corrosion rates were obtained through push-out tests;
[0024] S23. Based on the bond strength-slip curve, the bond-slip constitutive model between the steel frame and concrete interface under different corrosion rates was fitted using statistical theory. The calculation formula is as follows:
[0025]
[0026] Among them, τ is the bond strength of the corroded steel frame-concrete interface; S is the bond slip of the corroded steel frame-concrete interface; Parameters for considering the effect of steel frame corrosion on interface strength.
[0027] Preferably, in step S3, a three-dimensional solid load structural mechanics model of the initial support-secondary lining after the corrosion of the steel frame is established, and the calculation model is a three-dimensional solid load-structure model, and the steel frame, the initial support concrete, and the secondary lining are simulated by solid units, and the surrounding rock constraints are simulated by spring units;
[0028] Among them, contact units are used between the initial support and the secondary lining to simulate the force transfer between the two; nonlinear springs are used between the initial support concrete and the steel frame to achieve the bond slip between the two; for the corrosion simulation of the steel frame, the mechanical parameters of the steel frame itself are modified by formulas (2) to (4), and the force F-displacement D curve is converted by formula (5), further defining the nonlinear spring force properties between the initial support concrete and the steel frame.
[0029] Preferably, the force F-displacement D curve is converted by formula (5), and the specific operation is as follows:
[0030] There are three directions of stress on the interface between the steel frame and the concrete, namely, longitudinal tangential stress τ z , transverse tangential stress τ x , normal stress τ y ;
[0031] When establishing the interface spring connection, the stress-displacement relationship calculated by formula (5) is only assigned to the longitudinal tangential spring unit, and the transverse tangential stiffness and normal stiffness are assigned infinite values;
[0032] Any spring unit force F i :
[0033] F i =τS i (6)
[0034] Among them, S i is the stress action area; i=1,2,3;
[0035] The stress action area of the spring nodes in the middle, one-side boundary and corner of the three-dimensional solid load-structure model is expressed as:
[0036]
[0037] Among them, S1 is the stress action area of the middle spring node; S2 is the stress action area of the unilateral boundary spring node; S3 is the stress action area of the spring node at the corner point; A is the length of the grid unit in the three-dimensional solid load-structure model; B is the width of the grid unit in the three-dimensional solid load-structure model.
[0038] Preferably, in step S4, the unit stresses at the vault, arch waist, side wall, wall foot and invert under different corrosion rates are extracted through calculation by a three-dimensional solid load-structure model, and then the coordinate transformation method of elastic mechanics is used to transform the node stress in the rectangular coordinate system into the tangential stress of the support structure, and then the bending moment M and axial force N of the section are calculated.
[0039] Preferably, in step S5, the initial support safety evaluation is as follows:
[0040] The safety factor of initial support is the safety factor K of concrete compression control. c , Safety factor K for tensile control t The minimum value in ;
[0041] The compressive strength is calculated as follows:
[0042]
[0043] Among them, R a is the ultimate compressive strength of concrete; b is the section width; h is the section thickness; is the longitudinal bending coefficient of the steel frame concrete member; α is the eccentric influence coefficient of the axial force;
[0044] Based on the crack resistance requirement, the tensile strength of the plain concrete rectangular section eccentrically compressed member is calculated as follows:
[0045]
[0046] Among them, R1 is the tensile strength of concrete; e0 is the cross-sectional eccentricity;
[0047] The safety evaluation of secondary lining is as follows:
[0048] The strength safety factor of the secondary lining structure is checked and calculated according to the damage stage. The cross-sectional safety factor K of the reinforced concrete bending member is calculated as follows:
[0049] KM≤R w bx(h0-x / 2)+R g Ag ′(h0-a′) (10)
[0050] The position of the neutral axis is determined by the following formula:
[0051] R g (A g -A g ′)=R w bx (11)
[0052] Where x is the height of the compression zone of concrete; R w is the ultimate compressive strength of concrete; R g A is the calculated tensile or compressive strength of the steel bar; g ' is the cross-sectional area of the steel bar in the compression zone; A g is the cross-sectional area of the steel bar in the tension zone; h0 is the effective height of the cross section; a′ is the steel bar A g The distance from the centroid of ′ to the nearest edge of the cross section;
[0053] The safety factor K obtained by the above formulas (8), (9) and (10) is c , K t , K are compared with the limit values in tunnel specifications to determine the safety of the corroded steel frame structure of the tunnel section.
[0054] Therefore, the present invention adopts the above-mentioned method for evaluating the long-term safety of the structure after the tunnel support system is deteriorated, and the beneficial technical effects are as follows:
[0055] (1) The present invention provides a method for determining the corrosion rate of a steel frame, thereby solving the problem of difficulty in obtaining the corrosion rate on site;
[0056] (2) The present invention designs an experiment to obtain the bond-slip at the interface between steel frame and concrete with different corrosion rates, and based on this, establishes the bond-slip constitutive model of the interface between corroded steel frame and concrete, filling the gap in the bond-slip theory of the interface between corroded steel frame and concrete;
[0057] (3) The present invention uses the spring unit in the three-dimensional solid load-structure model to realize the bond slip between the corroded steel frame and the concrete interface. Based on this, a three-dimensional solid load-structure model of initial support-secondary lining considering the corrosion of the steel frame is established, which realizes the accurate and detailed simulation considering the corrosion of the steel frame;
[0058] (4) The present invention extracts the bending moment and axial force of the initial support and secondary lining, and provides a safety evaluation method for the initial support and secondary lining based on the bending moment and axial force, which can provide guarantee for the long-term safe service of the tunnel. BRIEF DESCRIPTION OF THE DRAWINGS
[0059] Figure 1It is a flow chart of the method for evaluating the long-term safety of the structure of the tunnel support system after degradation according to the present invention;
[0060] Figure 2 is the size of the steel frame concrete member;
[0061] Figure 3 This is the electrical accelerated corrosion test diagram;
[0062] Figure 4 To launch the test chart;
[0063] Figure 5 is the bond-slip curve;
[0064] Figure 6 It is a three-dimensional solid load-structure model;
[0065] Figure 7 It is the contact unit between the primary support and the secondary lining;
[0066] Figure 8 It is the spring between the steel frame and the concrete;
[0067] Fig. 9 It is a schematic diagram of spring unit F calculation; among them, Fig. 9 (a) is a schematic diagram of the three-dimensional stress at the steel frame-concrete interface; Fig. 9 (b) in the figure is a schematic diagram of the stress action area. DETAILED DESCRIPTION
[0068] The technical solution of the present invention is further described below through the accompanying drawings and embodiments.
[0069] Unless otherwise defined, technical or scientific terms used in the present invention shall have the common meanings understood by one having ordinary skills in the field to which the present invention belongs.
[0070] Embodiment 1
[0071] The support system in the present invention mainly includes anchor rods, steel frames, shotcrete in the initial support and cast concrete and steel bars in the secondary lining. The following description will be made taking the steel frames in the initial support as an example.
[0072] like Figure 1 FIG. 1 is a flow chart of a method for evaluating the long-term safety of a tunnel support system after degradation according to the present invention, which specifically includes the following steps:
[0073] S1. Calculate the corrosion rate of the steel frame, and determine the mechanical parameters of the steel frame after corrosion based on the corrosion rate;
[0074] The corrosion rate is calculated as follows:
[0075] Cut off a section of rusted steel frame in the tunnel, remove the rust products of the rusted steel frame with hydrochloric acid solution, then neutralize it with 3% sodium carbonate solution, finally wash it with clean water, and put it into an oven for drying;
[0076] Weigh the steel frame after rust removal to obtain the mass m of the steel frame after rusting. c , and compared with the mass m of the non-corroded steel frame of the same specification and length, the actual corrosion loss mass Δm is further obtained;
[0077] Finally, the corrosion rate of the steel frame is calculated. The calculation formula of the corrosion rate is as follows:
[0078]
[0079] Among them, ρ is the actual corrosion rate.
[0080] The mechanical parameters of the corroded steel frame include yield strength, ultimate strength and ultimate strain, and the calculation formulas are as follows:
[0081]
[0082]
[0083] ε suc =e -3.789ρ ε su0 (4)
[0084] Among them, f yc 、f uc , ε suc are the yield strength, ultimate strength and ultimate strain of the corroded steel frame; f y0 、f u0 , ε su0 are the yield strength, ultimate strength and ultimate strain of the corresponding non-corroded steel frame, respectively.
[0085] S2. Determine the interface bonding constitutive property of the composite structure after the steel frame is corroded. The specific operation is as follows:
[0086] S21. Determine the size of steel frame concrete components (such as Figure 2 As shown), steel frame concrete components are manufactured, and then steel frame concrete components with different corrosion rates are obtained through electrical acceleration tests;
[0087] According to Faraday's law, the accelerated electrolysis test is used to control the constant current, and the steel frame with different corrosion rates is obtained by controlling the power-on time. The accelerated test mainly uses an electrolytic cell composed of a DC power supply, an ammeter, a wire, a 5% NaCl solution, a copper sheet, a plastic water tank, and a wooden pad, such as Figure 3 shown.
[0088] S22, through the push test (such as Figure 4 As shown in the figure, the push-out device mainly includes a hydraulic servo jack, a steel pad, a digital displacement meter, a force support, and a fixed end) to obtain the bond strength-slip curve of the steel frame-concrete interface with different corrosion rates (such as Figure 5 shown);
[0089] Figure 5 In the equation, τ0 is the maximum bonding strength in the linear elastic stage, S0 is the corresponding slip value when the bonding strength is the maximum in the linear elastic stage; τ u is the ultimate bonding strength, S u is the slip value corresponding to the ultimate bonding strength; τ r is the residual bond strength, S r is the slip value corresponding to the residual bonding strength; OA represents the τ-S straight rising section; AB represents the τ-S curve rising section; BC represents the τ-S steep falling section; CD represents the τ-S residual section.
[0090] S23. Based on the bond strength-slip curve, the bond-slip constitutive model between the steel frame and concrete interface under different corrosion rates was fitted using statistical theory. The calculation formula is as follows:
[0091]
[0092] Among them, τ is the bond strength of the corroded steel frame-concrete interface; S is the bond slip of the corroded steel frame-concrete interface; Parameters for considering the effect of steel frame corrosion on interface strength.
[0093] S3. Establish a three-dimensional solid load structural mechanics model of initial support-secondary lining after corrosion of steel frame;
[0094] The calculation model is a three-dimensional solid load-structure model (such as Figure 6 As shown in the figure, the steel frame, initial support concrete and secondary lining are simulated with solid units, and the surrounding rock constraints are simulated with spring units;
[0095] Among them, the contact unit is used between the initial support and the secondary lining to simulate the force transfer between the two (such as Figure 7 nonlinear springs are used between the initial support concrete and the steel frame to achieve the bond slip between the two (as shown in Figure 8 As shown in the figure, for the corrosion simulation of the steel frame, the mechanical parameters of the steel frame are modified by formulas (2) to (4), and the force F-displacement D curve is transformed by formula (5) to further define the nonlinear spring force properties between the initial support concrete and the steel frame.
[0096] The force F-displacement D curve is converted by formula (5), and the specific operation is as follows:
[0097] There are stresses in three directions on the interface between the steel frame and the concrete (such as Fig. 9 As shown), the longitudinal tangential stress τ z , transverse tangential stress τ x , normal stress τ y ;
[0098] When establishing the interface spring connection, the stress-displacement relationship calculated by formula (5) is only assigned to the longitudinal tangential spring unit (z direction), and the transverse tangential stiffness and normal stiffness (x, y directions) are assigned infinite values;
[0099] Any spring unit force F i :
[0100] F i =τS i (6)
[0101] Among them, S i is the stress action area; i=1,2,3;
[0102] The stress action area of the spring nodes in the middle, one-side boundary and corner of the three-dimensional solid load-structure model is expressed as:
[0103]
[0104] Among them, S1 is the stress action area of the middle spring node; S2 is the stress action area of the unilateral boundary spring node; S3 is the stress action area of the spring node at the corner point; A is the length of the grid unit in the three-dimensional solid load-structure model; B is the width of the grid unit in the three-dimensional solid load-structure model.
[0105] S4, extract the internal forces of initial support and secondary lining, and calculate the structural bending moment and axial force;
[0106] Through the calculation of the three-dimensional solid load-structure model, the unit stresses at the arch crown, arch waist, side wall, wall foot and invert under different corrosion rates are extracted. Then, the coordinate transformation method of elastic mechanics is used to transform the node stress in the rectangular coordinate system into the tangential stress of the supporting structure, and then the bending moment M and axial force N of the section are calculated.
[0107] The safety factor of initial support is the safety factor K of concrete compression control. c , Safety factor K for tensile control t The minimum value in ;
[0108] The compressive strength is calculated as follows:
[0109]
[0110] Among them, R ais the ultimate compressive strength of concrete; b is the section width; h is the section thickness; is the longitudinal bending coefficient of the component; α is the eccentric influence coefficient of the axial force;
[0111] Based on the crack resistance requirement, the tensile strength of the plain concrete rectangular section eccentrically compressed member is calculated as follows:
[0112]
[0113] Among them, R1 is the tensile strength of concrete; e0 is the cross-sectional eccentricity;
[0114] The safety evaluation of secondary lining is as follows:
[0115] The strength safety factor of the secondary lining structure is checked and calculated according to the damage stage. The cross-sectional safety factor K of the reinforced concrete bending member is calculated as follows:
[0116] KM≤R w bx(h0-x / 2)+R g A g ′(h0-a′) (10)
[0117] The position of the neutral axis is determined by the following formula:
[0118] R g (A g -A g ′)=R w bx (11)
[0119] Where x is the height of the compression zone of concrete; R w is the ultimate compressive strength of concrete; R g A is the calculated tensile or compressive strength of the steel bar; g ' is the cross-sectional area of the steel bar in the compression zone; A g is the cross-sectional area of the steel bar in the tension zone; h0 is the effective height of the cross section; a′ is the steel bar A g The distance from the centroid of ′ to the nearest edge of the cross section;
[0120] The safety factor K obtained by the above formulas (8), (9) and (10) is c , K t , K are compared with the limit values in tunnel specifications to determine the safety of the corroded steel frame structure of the tunnel section.
[0121] Therefore, the present invention adopts the above-mentioned method for evaluating the long-term safety of the structure after the tunnel support system is deteriorated, which can ensure the long-term operation safety of the tunnel.
[0122] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that they can still modify or replace the technical solution of the present invention with equivalents, and these modifications or equivalent replacements cannot cause the modified technical solution to deviate from the spirit and scope of the technical solution of the present invention.
Claims
1. A method for evaluating the long-term structural safety of a tunnel support system after degradation, characterized in that: The following steps are involved: S1. Calculate the corrosion rate of the steel frame, and determine the mechanical parameters of the steel frame after corrosion based on the corrosion rate; S2. Determine the interface bonding constitutive property of the composite structure after the steel frame is corroded; S3. Establish a three-dimensional solid load structural mechanics model of initial support-secondary lining after corrosion of steel frame; S4, extract the internal forces of initial support and secondary lining, and calculate the structural bending moment and axial force; S5. Evaluate the safety of initial support and secondary lining.
2. The method for evaluating the long-term safety of a tunnel support system after degradation according to claim 1 is characterized in that: In step S1, the corrosion rate of the steel frame is calculated, and the specific operation is as follows: Cut off a section of rusted steel frame in the tunnel, remove the rust products of the rusted steel frame with hydrochloric acid solution, then neutralize it with 3% sodium carbonate solution, finally wash it with clean water, and put it into an oven for drying; Weigh the steel frame after rust removal to obtain the mass m of the steel frame after rusting. c , and compared with the mass m of the non-corroded steel frame of the same specification and length, the actual corrosion loss mass Δm is further obtained; Finally, the corrosion rate of the steel frame is calculated. The calculation formula of the corrosion rate is as follows: Among them, ρ is the actual corrosion rate.
3. The method for evaluating the long-term safety of a tunnel support system after degradation according to claim 2, characterized in that: In step S1, the mechanical parameters of the corroded steel frame include yield strength, ultimate strength and ultimate strain, and the calculation formulas are as follows: e suc =e -3.789ρ e su0 (4) Among them, f yc 、f uc , ε suc are the yield strength, ultimate strength and ultimate strain of the corroded steel frame; f y0 、f u0 , ε su0 are the yield strength, ultimate strength and ultimate strain of the corresponding non-corroded steel frame, respectively.
4. The method for evaluating the long-term safety of a tunnel support system after degradation according to claim 3 is characterized in that: In step S2, the interface bonding constitutive model of the composite structure after the steel frame is corroded is determined, and the specific operation is as follows: S21, determining the size of the steel frame concrete component, manufacturing the steel frame concrete component, and then obtaining the steel frame concrete components with different corrosion rates through electrical acceleration test; S22. The bond strength-slip curves of the steel frame-concrete interface with different corrosion rates were obtained through push-out tests; S23. Based on the bond strength-slip curve, the bond-slip constitutive model between the steel frame and concrete interface under different corrosion rates was fitted using statistical theory. The calculation formula is as follows: Among them, τ is the bond strength of the corroded steel frame-concrete interface; S is the bond slip of the corroded steel frame-concrete interface; Parameters for considering the effect of steel frame corrosion on interface strength.
5. The method for evaluating the long-term safety of a tunnel support system after degradation according to claim 4, characterized in that: In step S3, a three-dimensional solid load structural mechanics model of the initial support-secondary lining after the corrosion of the steel frame is established. The calculation model is a three-dimensional solid load-structure model. The steel frame, initial support concrete, and secondary lining are simulated by solid units, and the surrounding rock constraints are simulated by spring units. Among them, contact units are used between the initial support and the secondary lining to simulate the force transfer between the two; nonlinear springs are used between the initial support concrete and the steel frame to achieve the bond slip between the two; for the corrosion simulation of the steel frame, the mechanical parameters of the steel frame itself are modified by formulas (2) to (4), and the force F-displacement D curve is converted by formula (5), further defining the nonlinear spring force properties between the initial support concrete and the steel frame.
6. The method for evaluating the long-term safety of a tunnel support system after degradation according to claim 5, characterized in that: The force F-displacement D curve is converted by formula (5), and the specific operation is as follows: There are three directions of stress on the interface between the steel frame and the concrete, namely, longitudinal tangential stress τ z , transverse tangential stress τ x , normal stress τ y ; When establishing the interface spring connection, the stress-displacement relationship calculated by formula (5) is only assigned to the longitudinal tangential spring unit, and the transverse tangential stiffness and normal stiffness are assigned infinite values; Any spring unit force F i : F i =τS i (6) Among them, S i is the stress action area; i=1,2,3; The stress action area of the spring nodes in the middle, one-side boundary and corner of the three-dimensional solid load-structure model is expressed as: Among them, S1 is the stress action area of the middle spring node; S2 is the stress action area of the unilateral boundary spring node; S3 is the stress action area of the spring node at the corner point; A is the length of the grid unit in the three-dimensional solid load-structure model; B is the width of the grid unit in the three-dimensional solid load-structure model.
7. The method for evaluating the long-term safety of a tunnel support system after degradation according to claim 6, characterized in that: In step S4, the unit stresses at the arch crown, arch waist, side wall, wall foot and invert under different corrosion rates are extracted through calculation by a three-dimensional solid load-structure model. Then, the coordinate transformation method of elastic mechanics is used to transform the node stress in the rectangular coordinate system into the tangential stress of the support structure, and then the bending moment M and axial force N of the section are calculated.
8. The method for evaluating the long-term safety of a tunnel support system after degradation according to claim 7, characterized in that: In step S5, the initial support safety evaluation is as follows: The safety factor of initial support is the safety factor K of concrete compression control. c , Safety factor K for tensile control t The minimum value in ; The compressive strength is calculated as follows: Among them, R a is the ultimate compressive strength of concrete; b is the section width; h is the section thickness; is the longitudinal bending coefficient of the steel frame concrete member; α is the eccentric influence coefficient of the axial force; Based on the crack resistance requirement, the tensile strength of the plain concrete rectangular section eccentrically compressed member is calculated as follows: Among them, R1 is the tensile strength of concrete; e0 is the cross-sectional eccentricity; The safety evaluation of secondary lining is as follows: The strength safety factor of the secondary lining structure is checked and calculated according to the damage stage. The cross-sectional safety factor K of the reinforced concrete bending member is calculated as follows: KM≤R w bx(h0-x / 2)+R g A g ′(h0-a′) (10) The position of the neutral axis is determined by the following formula: R g (A g -A g ′)=R w bx (11) Where x is the height of the compression zone of concrete; R w is the ultimate compressive strength of concrete; R g A is the calculated tensile or compressive strength of the steel bar; g ' is the cross-sectional area of the steel bar in the compression zone; A g is the cross-sectional area of the steel bar in the tension zone; h0 is the effective height of the cross section; a′ is the steel bar A g The distance from the centroid of ′ to the nearest edge of the cross section; The safety factor K obtained by the above formulas (8), (9) and (10) is c , K t , K are compared with the limit values in tunnel specifications to determine the safety of the corroded steel frame structure of the tunnel section.
Citation Information
Patent Citations
Tunnel fabricated prestressed lining design method
CN111550262A
Method for evaluating degradation degree of bidirectional bending bearing capacity of corroded bridge pier
CN113656955A
Safety checking and calculating method for arch wall assembly type tunnel structure excavated through mining method
CN115203781A
Connection structure of Hollow reinforced concrete column with internal steeltube by using coupler
KR1020120067699A
Energy harvesting methods and devices, and applications thereof
US20130033130A1
Cited By
Method for predicting long-term rigidity of hogging moment area of steel-concrete composite beam bridge
CN119918159A
Tunnel structure mechanical property test method and system aiming at gradual deterioration of primary support
CN119935751A
Yield support optimization method under influence of local weakening of hard rock mining section
CN120654500A
A water gate safety evaluation method based on material degradation