Method for controlling bending of rod during cooling after rolling
Through the control and control of the cooling process, the cold bed step distance, the lead coefficient of the double-sized shear and the accuracy of the cold bed equipment, the cooling bending problem of rods after rolling is solved, and the processing efficiency and material yield are significantly improved.
Patent Information
- Application Number
- CN202411349408.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-26
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2044-09-26
AI Technical Summary
The bars are prone to bending the head, middle and tail during the post-rolling cooling process, which affects subsequent processing and production efficiency.
By controlling the cooling process, cold bed step distance, double-slicing lead coefficient and cold bed equipment accuracy, it specifically includes setting the appropriate cold bed temperature, cold bed step distance, lead coefficient and precision control of the cold bed equipment to ensure the moving beam The elevation, rack height and roller wear are within the appropriate range.
It effectively reduces the cooling bending phenomenon of rods after rolling, and improves the processing efficiency and material yield of the next process.
Smart Images

Figure CN119076644A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of iron and steel metallurgy production and manufacturing, and in particular to a method for controlling the bending of a bar during cooling after rolling. Background Art
[0002] In the process of bar production, the phenomenon of bending after cooling after rolling is very common, causing the head, middle and tail of the bar to bend, affecting the processing of the bar in subsequent steps and reducing production efficiency. Summary of the invention
[0003] In order to solve the above problems, the present invention provides a method for controlling the bending of a bar during cooling after rolling, which effectively solves the problem of the bending of the bar during cooling after rolling.
[0004] The technical solution adopted by the present invention is: a method for controlling the bending of a bar during cooling after rolling, characterized in that: according to the rolling specifications and steel types, the cooling process, the cooling bed step, the multiple shear advance coefficient and the cooling bed equipment are controlled, specifically comprising the following steps:
[0005] S1. Controlled cooling process: the temperature of the cooling bed on the rolled piece is ≤1000℃;
[0006] S2, cooling bed step selection:
[0007] Rolling specifications Φ12~28, steel type HRB400E, cooling bed step 60~70mm; rolling specifications Φ32~40, steel type HRB400E, cooling bed step 125~135mm; rolling specifications Φ12~22, steel type HRB500E, cooling bed step 60~70mm; rolling specifications Φ25~40, steel type HRB500E, cooling bed step 125~135mm; rolling specifications Φ12~22, steel type HRB600E and above, cooling bed step 60~70mm; rolling specifications Φ25~40, steel type HRB600E and above, cooling bed step 125~135mm;
[0008] S3, multiple length shear advance coefficient setting:
[0009] Rolling specification Φ12, leading coefficient 1.03 ~ 1.05; rolling specification Φ14, leading coefficient 1.04 ~ 1.06; rolling specification Φ16 ~ 20, leading coefficient 1.05 ~ 1.07; rolling specification Φ22, leading coefficient 1.06 ~ 1.08; rolling specification Φ25, leading coefficient 1.26 ~ 1.27; rolling specification Φ28, leading coefficient 1.265 ~ 1.275; rolling specification Φ32 ~ 40, leading coefficient 1.275 ~ 1.285;
[0010] S4. Precision control of cooling bed equipment: control the elevation deviation of the moving beam and the height deviation of the moving rack, the wear of the eccentric wheel and roller, and the wear of the rack end.
[0011] Preferably, in step S1, the cooling bed temperature of rolled pieces made of HRB400E material is ≤880°C, the cooling bed temperature of rolled pieces made of HRB500E material is ≤950°C, and the cooling bed temperature of rolled pieces made of HRB600E and above series is ≤1000°C.
[0012] Preferably, in step S4, the elevation of the moving beam is measured, and measures such as adding pads or reducing pads are taken for moving beams that are not within the standard range to ensure that the elevation deviation of the moving beam and the height deviation of the moving rack are ≤3 mm.
[0013] Preferably, in step S4, the height deviation of the moving beam and the height deviation of the moving rack are ≤3 mm.
[0014] Preferably, the wear of the eccentric wheel and the roller is ≤2mm.
[0015] Preferably, in step S4, the wear on the rack end is ≤3 mm.
[0016] The beneficial effects achieved by the present invention are as follows: the present invention effectively controls the cooling control process, cooling bed step distance, multiple shear advance coefficient and cooling bed equipment according to the rolling specifications and steel types, solves the problem of bar bending after cooling and rolling, greatly improves the bending phenomenon of the bar after cooling and rolling, and improves the processing efficiency and yield rate of the next process. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 It is a schematic diagram of the main structure of the walking cooling bed;
[0018] Figure 2 It is the height difference of the cooling bed moving beam base (positive value is high, negative value is low);
[0019] Among them: 1. Input roller; 2. Brake plate; 3. Straightening plate; 4. Stationary rack; 5. Moving rack; 6. Roller seat; 7. Roller; 8. Eccentric wheel; 9. Moving rack frame; 10. Rack seat. DETAILED DESCRIPTION
[0020] The technical solution of the present invention will be described clearly and completely below in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0021] A method for controlling the bending of a bar during cooling after rolling of the present invention controls the cooling process, the cooling bed step, the multiple-length shear advance coefficient and the cooling bed equipment according to the rolling specifications and the steel type, and specifically comprises the following steps:
[0022] S1. Controlled cooling process: The upper cooling bed temperature of HRB400E rolled pieces is ≤880℃, the upper cooling bed temperature of HRB500E rolled pieces is ≤950℃, the upper cooling bed temperature of HRB600E and above rolled pieces is ≤1000℃;
[0023] Considering that as the strength of rolled pieces increases, the use of a lower upper cooling bed controlled cooling process will result in the strength-to-yield ratio of rolled pieces not meeting the standard, while the use of a higher upper cooling bed controlled cooling process can solve the problem of the strength-to-yield ratio not meeting the standard caused by high-strength rebar, but due to the high temperature, it is very easy to cause bending in the subsequent cooling process. Through process adjustment, the above controlled cooling process can solve the problem of the strength-to-yield ratio not meeting the standard and the bending not being able to be achieved at the same time;
[0024] S2, cooling bed step selection:
[0025] Rolling specifications Φ12~28, steel type HRB400E, cooling bed step 60~70mm; rolling specifications Φ32~40, steel type HRB400E, cooling bed step 125~135mm; rolling specifications Φ12~22, steel type HRB500E, cooling bed step 60~70mm; rolling specifications Φ25~40, steel type HRB500E, cooling bed step 125~135mm; rolling specifications Φ12~22, steel type HRB600E and above, cooling bed step 60~70mm; rolling specifications Φ25~40, steel type HRB600E and above, cooling bed step 125~135mm;
[0026] The larger the size of the rolled piece, the slower the heat dissipation. If the step size is too small, the heat dissipation will be slow and uneven, which may cause bending. Similarly, the higher the strength of the rolled piece, the higher the temperature of the upper cooling bed. If the step size is too small, the heat dissipation will be slow and uneven, which may cause bending.
[0027] S3, multiple length shear advance coefficient setting:
[0028] Rolling specification Φ12, leading coefficient 1.03 ~ 1.05; rolling specification Φ14, leading coefficient 1.04 ~ 1.06; rolling specification Φ16 ~ 20, leading coefficient 1.05 ~ 1.07; rolling specification Φ22, leading coefficient 1.06 ~ 1.08; rolling specification Φ25, leading coefficient 1.26 ~ 1.27; rolling specification Φ28, leading coefficient 1.265 ~ 1.275; rolling specification Φ32 ~ 40, leading coefficient 1.275 ~ 1.285;
[0029] The smaller the size of the rolled piece, the faster the rolling speed, and the smaller the shear force required for the rolled piece, the smaller the shear speed drop during the shearing process. Therefore, setting a smaller advance coefficient can ensure that the shear speed after shearing is greater than the speed of the rolled piece, so as not to cause the elbow at the end after shearing. Similarly, the larger the size of the rolled piece, the slower the rolling speed, and the greater the shear force required for shearing, the greater the shear speed drop during the shearing process. Therefore, a larger advance coefficient is required to ensure that the shear speed after shearing is greater than the speed of the rolled piece.
[0030] S4. Precision control of cooling bed equipment: Control the deviation of the height of the moving beam and the height of the moving rack, the wear of the eccentric wheel and roller, and the wear of the rack end; the deviation of the height of the moving beam and the height of the moving rack is ≤3mm, the wear of the eccentric wheel and roller is ≤2mm, and the wear of the rack end is ≤3mm; for the measurement of the height of the moving beam, take measures such as adding or reducing pads for the moving beam that is not within the standard range to ensure that the deviation of the height of the moving beam and the height of the moving rack is ≤3mm;
[0031] After rolling, the rolled piece is put on the cooling bed. The precision control of the cooling bed equipment does not meet the requirements, causing bending when it is put on the cooling bed; the deviation of the movable beam elevation and the movable rack height exceeds the standard. The rack in some parts cannot transport the steel backward, which will cause inconsistent steel support and failure to synchronously put on the straightening plate, resulting in bending. The wear of the eccentric wheel and the supporting wheel exceeds the standard, causing the rack frame height to be low, and some racks cannot support the rolled piece and synchronously transport it forward, causing the rolled piece to bend.
[0032] like Figure 1 As shown, it is a conventional step-type cooling bed, including an input roller 1, a brake plate 2, a straightening plate 3, a movable rack 5, a static rack 4, an eccentric wheel 8 and a roller 7. The cooling bed is generally driven synchronously by four volute reducers to ensure that the cooling bed can continuously perform the four actions of rising-forward-falling-backward.
[0033] The elevation of the cooling bed moving beam base is measured during regular maintenance and long-term shutdown, and the data are as follows:
[0034] Measured from north to south, the mean of all measuring points is taken as zero point, values above the mean are positive, and values below the mean are negative, in mm:
[0035]
[0036]
[0037] By measuring the elevation of the moving beam, measures such as adding or reducing pads are taken for moving beams that are not within the standard range: for example, if the elevation of moving beam No. 8 is higher than 4mm, subtract a 1mm pad to ensure that its height deviation is ≤3mm.
[0038] On-site results:
[0039] From May 1 to May 30, 2024, the rolling specifications include Φ12, Φ14, Φ16, Φ18, Φ25, etc., and the products include HRB400E and HRB500E.
[0040] Effect 1: From May 5 to 12, 2024, Φ14 specification and steel grade HRB400E were produced. The temperature of the cooling bed on the rolled piece was controlled at 860℃±5℃, the cooling bed step was 60mm, the multiple shear advance coefficient was 1.03, and there was steel bending during the cooling bed production process; when the cooling bed step was adjusted to 63mm and the multiple shear advance coefficient was adjusted to 1.04, the phenomenon of steel bending on the cooling bed was significantly improved.
[0041] Effect 2: From May 23 to 27, 2024, the Φ20 specification was produced, the steel grade was HRB500E, the upper cooling bed temperature was controlled at 920℃±5℃, the cooling bed step was 68mm, the multiple shear advance coefficient was 1.07, and bent steel rarely occurred during the production process. In the production of Φ22 specifications, the step was 68mm, and the multiple shear advance coefficient was 1.07. Previously, after 2 hours of continuous rolling, bent steel would appear near 50 meters and 90 meters of the cooling bed. The downtime was used to add 2mm pads to the moving beam base here, and there was no bent steel in the subsequent production process.
[0042] Effect 3: From May 3rd to 4th and 13th to 14th, 2024, the Φ25 specification and steel grade HRB400E were rolled. The temperature of the cooling bed on the rolled piece was controlled at 870℃±5℃, the cooling bed step was 130mm, and the multiple shear advance coefficient was 1.265. The cooling bed had steel bending during the production process. When the cooling bed step was adjusted to 133 and the multiple shear advance coefficient was adjusted to 1.268, the elbow at the tail of the rolled piece was reduced and the bending phenomenon of the cooling bed was reduced.
[0043] It should be noted that the description of the above technical solutions is exemplary, and this specification can be embodied in different forms and should not be interpreted as being limited to the technical solutions set forth herein. On the contrary, providing these descriptions will make the disclosure of the present invention thorough and complete, and will fully convey the scope disclosed in this specification to those skilled in the art. In addition, the technical solutions of the present invention are limited only by the scope of the claims.
[0044] Finally, it should be pointed out that the above embodiments are only representative examples of the present invention. Obviously, the present invention is not limited to the above embodiments, and there are many variations. Any simple modification, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention should be considered to belong to the protection scope of the present invention.
Claims
1. A method for controlling the bending of a bar during cooling after rolling, characterized in that: According to the rolling specifications and steel types, the cooling process, cooling bed step, multiple shear advance coefficient and cooling bed equipment are controlled, including the following steps: S1. Controlled cooling process: the temperature of the cooling bed on the rolled piece is ≤1000℃; S2, cooling bed step selection: Rolling specifications Φ12~28, steel type HRB400E, cooling bed step 60~70mm; rolling specifications Φ32~40, steel type HRB400E, cooling bed step 125~135mm; rolling specifications Φ12~22, steel type HRB500E, cooling bed step 60~70mm; rolling specifications Φ25~40, steel type HRB500E, cooling bed step 125~135mm; rolling specifications Φ12~22, steel type HRB600E and above, cooling bed step 60~70mm; rolling specifications Φ25~40, steel type HRB600E and above, cooling bed step 125~135mm; S3, multiple length shear advance coefficient setting: Rolling specification Φ12, leading coefficient 1.03 ~ 1.05; rolling specification Φ14, leading coefficient 1.04 ~ 1.06; rolling specification Φ16 ~ 20, leading coefficient 1.05 ~ 1.07; rolling specification Φ22, leading coefficient 1.06 ~ 1.08; rolling specification Φ25, leading coefficient 1.26 ~ 1.27; rolling specification Φ28, leading coefficient 1.265 ~ 1.275; rolling specification Φ32 ~ 40, leading coefficient 1.275 ~ 1.285; S4. Precision control of cooling bed equipment: control the elevation deviation of the moving beam and the height deviation of the moving rack, the wear of the eccentric wheel and roller, and the wear of the rack end.
2. The method for controlling the bending of a bar during cooling after rolling according to claim 1, characterized in that: In step S1, the cooling bed temperature of the rolled piece made of HRB400E material is ≤880°C, the cooling bed temperature of the rolled piece made of HRB500E material is ≤950°C, and the cooling bed temperature of the rolled piece made of HRB600E and above series is ≤1000°C.
3. The method for controlling the bending of a bar during cooling after rolling according to claim 1, characterized in that: In step S4, the elevation of the moving beam is measured, and measures such as adding pads or reducing pads are taken for moving beams that are not within the standard range to ensure that the deviation of the moving beam elevation and the height deviation of the moving rack are ≤3mm.
4. The method for controlling the bending of a bar during cooling after rolling according to claim 1, characterized in that: In step S4, the height deviation of the moving beam and the height deviation of the moving rack are ≤3 mm.
5. The method for controlling the bending of a bar during cooling after rolling according to claim 4, characterized in that: The wear of eccentric wheel and roller is ≤2mm.
6. The method for controlling the bending of a bar during cooling after rolling according to claim 1, characterized in that: In step S4, the rack end wear is ≤3 mm.
Citation Information
Patent Citations
On-line control method of banded structure and hardness of gear steel and post-rolling on-line controlled cooling bed device
CN103589843A
Low-cost red-rust-free high-strength anti-knock deformed steel bar production method and system
CN111360066A
Method for improving flying shear head shearing precision and improving multi-length sectional bending and rolling technology
CN117483434A
Hardness control method for small-specification 50CrVA bar
CN117619878A
Double-length reinforcing steel bar head-picking device for bar stepping type cooling bed