IGBT (Insulated Gate Bipolar Translator) chip structure preparation method and IGBT chip structure
By forming a contact structure of the silicide region and P well region in the IGBT chip, replacing the traditional NPNP structure, the problem of latch effect is solved, the natural anti-latch characteristics and stability of the chip are realized, and the manufacturing process is simplified.
Patent Information
- Application Number
- CN202411582952.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-11-07
- Publication Date
- 2024-12-06
AI Technical Summary
The NPNP structure in traditional IGBT chips is prone to cause latch effect, resulting in current runaway and chip burning.
By forming a contact structure of the silicide region and the P well region in the IGBT chip as Schottky contact, replacing the traditional NPNP structure, natural latch-resistant characteristics are achieved.
Eliminates the latch effect, enhances the robustness and stability of IGBT chips in extreme environments, simplifies the manufacturing process and reduces production costs.
Smart Images

Figure CN119092408A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of semiconductor devices, and in particular to a method for preparing an IGBT chip structure and an IGBT chip structure. Background Art
[0002] IGBT (Insulated Gate Bipolar Transistor) is a high-power semiconductor device that combines the high switching frequency and easy controllability of MOS devices with the high current handling capability of BJT (bipolar junction transistor) devices. It is widely used in industrial frequency conversion, consumer electronics, rail transportation, new energy, aerospace and other fields. In traditional trench gate IGBT chips, the N+ source is usually formed based on high-dose P or As ion implantation to provide electrons when the channel is turned on. This, together with the gate, the P well region below and the N-type drift layer, forms a positive MOSFET structure, thereby controlling the switching state of the chip.
[0003] In this way, in the area far away from the gate, the N-type heavily doped source forms an N+P junction with the P-well area below. In the vertical direction of this area, the N-type drift layer and the P-type anode further form an NPNP structure. In this way, when the potential of the P-well area increases, the N+P junction between the N+ source and the P-well area may be triggered, resulting in a latch effect. At this time, the current will lose control and increase sharply, which may eventually cause the chip to burn out.
[0004] The above contents are only used to assist in understanding the technical solution of the present application and do not constitute an admission that the above contents are prior art. Summary of the invention
[0005] The main purpose of the present application is to provide a method for preparing an IGBT chip structure and an IGBT chip structure, aiming to enable the IGBT chip to have a natural anti-latch characteristic to eliminate the corresponding latch effect.
[0006] To achieve the above object, the present application provides a method for preparing an IGBT chip structure, comprising the following steps: forming an oxide layer over a substrate front side of the wafer; The oxide layer is selectively etched, and a field limiting ring and a reserved area are formed at the etched portion of the terminal area, and two reserved areas are formed at the etched portion of the cell area; After forming an oxide layer in the reserved area, polysilicon filling growth is performed, and a Poly gate is formed in the reserved area of the cell area, and a field stop ring is formed in the reserved area of the terminal area; A P-well region is formed at other etched locations of the oxide layer in the cell region except for the reserved region; An oxide layer is formed covering the polysilicon, and a silicide region is formed on the upper surface of the P-well region between the two Poly gates; Forming a dielectric layer on the oxide layer and the silicide region, and etching the dielectric layer to form a front metal layer penetrating the dielectric layer and contacting the silicide region; A buffer layer, a P-type doping layer and a back metal layer are sequentially formed under the back side of the substrate.
[0007] Optionally, after the step of forming a dielectric layer on the oxide layer and the silicide region, and etching the dielectric layer to form a front metal layer penetrating the dielectric layer and contacting the silicide region, the method further includes: forming a passivation layer on the dielectric layer and the front metal layer; The passivation layer in the cell region is subjected to photolithography patterning to remove the middle portion of the passivation layer and to divide the remaining passivation layer into a left passivation layer and a right passivation layer.
[0008] Optionally, the method for preparing the IGBT chip structure further includes: In the process of forming the oxide layer on the front side of the substrate, a wet oxygen process is used, and the process temperature is 800~1050℃; And / or, in the process of forming the oxide layer in the reserved area, a sacrificial oxide layer is first grown, and after the sacrificial oxide layer is removed, gate oxide is grown.
[0009] Optionally, before the step of forming a P-well region at other etching locations of the oxide layer in the cell region except the reserved region, the step further includes: Etching the polysilicon on the front side of the substrate to form a Poly gate in a reserved area of the cell region; The polysilicon on the back side of the substrate is removed and a cleaning process is performed.
[0010] Optionally, the method for preparing the IGBT chip structure further includes: In the process of forming the field limiting ring, a dose of 8E13~5E14 B+ ions is injected, and the injection energy is 80~140keV; And / or, in the process of forming the P-well region, B+ ions with a dosage of 1E13-1E14 and an implantation energy of 80-140 keV are implanted.
[0011] Optionally, the step of forming a silicide region on the upper surface of the P-well region between the two Poly gates includes: Based on photolithography, a source contact window is formed above the P-well region between the two Poly gates; Etching the oxide layer of the source contact window to remove the oxide layer of the source contact window; Metal titanium sputtering is performed on the source contact window to form a silicide region on the upper surface of the P-well region between the two Poly gates.
[0012] Optionally, the step of performing metal titanium sputtering on the source contact window to form a silicide region on the upper surface of the P-well region between the two Poly gates includes: After metal titanium is sputtered on the source contact window, a stripping process is used to remove the photoresist and the metal titanium on the photoresist; A rapid thermal processing annealing process is performed to make the metal titanium react with the underlying silicon alloy to generate silicide, so as to form a silicide region on the upper surface of the P-well region between the two Poly gates.
[0013] Optionally, before the step of sequentially forming a buffer layer, a P-type doping layer and a back metal layer under the back side of the substrate, the method further includes: The back of the wafer is ground to remove the silicon oxide on the back of the substrate and thin the wafer to 60~150um.
[0014] Optionally, the method for preparing the IGBT chip structure further includes: In the process of forming the buffer layer, P+ ions with a dose of 2E11~1E13 and an injection energy of 200~900keV are injected; And / or, in the process of forming the P-type doping layer, B+ ions with a dosage of 1E12-8E13 and an implantation energy of 20-50 keV are implanted.
[0015] To achieve the above objectives, the present application also provides an IGBT chip structure, which is prepared by the preparation method of the IGBT chip structure as described above.
[0016] The preparation method of the IGBT chip structure and the IGBT chip structure provided in the present application form contact structures of the silicide region and the P-well region in the IGBT chip structure as Schottky contacts to replace the NPNP structure in the traditional IGBT chip, so that the IGBT chip has a natural anti-latch characteristic and eliminates the latch effect, thereby enhancing the robustness and stability of the IGBT chip working in extreme environments. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 This is a schematic diagram of the steps of a method for preparing an IGBT chip structure in an embodiment of the present application; Figure 2 A schematic diagram of a preparation process of an IGBT chip structure in an embodiment of the present application; Figure 3 Another schematic diagram of the preparation process of the IGBT chip structure in one embodiment of the present application; Figure 4 A schematic diagram of forming a P-well region during the preparation of an IGBT chip structure in an embodiment of the present application; Figure 5 A schematic diagram of forming a silicide region in the preparation of an IGBT chip structure in an embodiment of the present application; Figure 6 It is another schematic diagram of the preparation process of the IGBT chip structure in one embodiment of the present application; Figure 7 A schematic diagram of an IGBT chip structure in an embodiment of the present application; Figure 8 This is a schematic diagram of the steps of a method for preparing an IGBT chip structure in another embodiment of the present application; Fig. 9 FIG. 4 is another schematic diagram of the structure of the IGBT chip in one embodiment of the present application.
[0018] Description of reference numerals: 1. Substrate; 2. Oxide layer; 3. Field limiting ring; 4. Poly gate; 5. Field stop ring; 6. Busbar routing; 7. P-well region; 8. Silicide region; 9. Dielectric layer; 10. Front metal layer; 11. Buffer layer; 12. P-type doped layer; 13. Back metal layer; 14. Passivation layer.
[0019] The realization of the purpose, functional features and advantages of this application will be further explained in conjunction with embodiments and with reference to the accompanying drawings. DETAILED DESCRIPTION
[0020] The embodiments of the present application are described in detail below, and examples of the embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are intended to be used to explain the present application, and should not be construed as limiting the present application. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in the field without creative work are within the scope of protection of the present application.
[0021] In addition, if the descriptions of "first", "second", etc. are involved in this application, they are only used for descriptive purposes (such as for distinguishing the same or similar features), and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In addition, the technical solutions between the various embodiments can be combined with each other, but they must be based on the ability of ordinary technicians in this field to implement them. When the combination of technical solutions is contradictory or cannot be implemented, it should be deemed that such combination of technical solutions does not exist and is not within the scope of protection required by this application.
[0022] Reference Figure 1 In one embodiment, a method for preparing an IGBT chip structure includes: Step S10, forming an oxide layer on the front side of the substrate of the wafer; Step S20, selectively etching the oxide layer, and forming a field limiting ring and a reserved area at the etching position of the terminal area, and forming two reserved areas at the etching position of the cell area; Step S30, after forming an oxide layer in the reserved area, performing polysilicon filling growth, forming a Poly gate in the reserved area of the cell area, and forming a field stop ring in the reserved area of the terminal area; Step S40, forming a P-well region at other etched locations of the oxide layer in the cell region except the reserved region; Step S50, forming an oxide layer covering the polysilicon, and forming a silicide region on the upper surface of the P well region between the two Poly gates; Step S60, forming a dielectric layer on the oxide layer and the silicide region, and etching the dielectric layer to form a front metal layer penetrating the dielectric layer and contacting the silicide region; Step S70: forming a buffer layer, a P-type doping layer and a back metal layer in sequence under the back side of the substrate.
[0023] In this embodiment, in the preparation process of the IGBT chip structure with a Schottky barrier structure, processes including ion implantation, furnace oxidation and impurity pushing, trench etching, sacrificial oxide layer and gate oxide layer growth, polysilicon deposition and dry etching, metal sputtering and stripping, silicide formation, wafer back thinning, furnace annealing, etc. can be used.
[0024] As described in step S10, a FZ single crystal substrate is used, which is N-type and can be provided based on a 4-8 inch wafer, the wafer surface is a (100) crystal plane, and the resistivity is 30-90 Ωcm.
[0025] Reference Figure 2 A field oxide layer 2 is grown on the front surface of the provided substrate 1 to form an oxide layer 2 with a thickness of 1 to 3 um.
[0026] As described in step S20, the oxide layer 2 is selectively etched in the terminal region to leave a window for making the field limit ring 3. Photoresist can be used to protect the oxide layer portion that does not need to be etched.
[0027] Then, ion implantation is performed into the window of the field limiting ring 3. After debonding (i.e., removing the solidified photoresist), impurity push is performed at a temperature of 1000-1200°C for 300-600 minutes. In this way, the impurities that have been injected are diffused in the semiconductor material through high temperature treatment, thereby achieving the desired doping characteristics. Impurity push helps stabilize its electrical properties.
[0028] The oxide layer 2 is selectively etched again in the cell region and the terminal region to form reserved area manufacturing windows in the cell region and the terminal region.
[0029] Then, etching is performed in the fabrication window of the reserved area to etch out the reserved area, wherein two reserved areas are formed in the cell area and one reserved area is formed in the terminal area.
[0030] Optionally, the reserved area may be etched by first using plasma enhanced chemical vapor deposition (PECVD) technology to deposit and grow a SiO2 etching hard mask layer (the thickness may be 5000-10000Å), and then performing trench etching in a production window of the reserved area, the depth of which may be 4-7um, thereby forming a corresponding reserved area.
[0031] It should be noted that the cell region is the main working area of the IGBT structure, which includes the actual channel and gate structure and is responsible for realizing the switching function of the device. The terminal region is the peripheral structure of the IGBT, which is usually used to provide additional electrical protection to ensure the safety and stability of the device in high voltage and high current applications to prevent damage to the cell region under extreme working conditions.
[0032] In the design of IGBT, the cell area and the terminal area complement each other. The cell area is responsible for load control and regulation, while the terminal area ensures the stability and reliability of the IGBT under high voltage conditions. A well-designed structure can effectively improve device performance, reduce the risk of failures such as latch-up, and enable IGBT to exhibit good characteristics in many application fields (such as power conversion, drive control, etc.).
[0033] As described in step S30, refer to Figure 3 After the reserved area is made, an oxide layer 2 is grown again on the front side of the substrate 1 so that the oxide layer 2 can cover the newly formed reserved area and perform protection isolation.
[0034] Then, polysilicon is filled and grown on the reserved areas in the cell region and the terminal region and covered with the oxide layer 2 .
[0035] Among them, polysilicon filling growth can adopt Low Pressure Chemical Vapor Deposition (LPCVD) process to form polysilicon with a thickness of 8000~12000Å. LPCVD can achieve uniform thin film deposition and is suitable for large-area substrate surfaces.
[0036] Then, the polysilicon is dry-etched, and corresponding Poly gates 4 are formed in two reserved areas of the cell region, and a field stop ring 5 is formed in the reserved area of the terminal region.
[0037] In addition, other polysilicon in the terminal region can be used to make a busbar trace 6, which is used to connect the poly gate 4 to the metal gate of the IGBT chip. It should be noted that the role of the busbar trace in the semiconductor mainly includes current transmission and current distribution.
[0038] Among them, dry etching (such as reactive ion etching, RIE) can be used to achieve highly selective polysilicon removal, which can effectively leave polysilicon in a specific area without causing damage to the surrounding oxide layer 2 or other areas.
[0039] It should be noted that the field limiting ring 3 (also known as the fast front region (FFR)) in the terminal region is a specific structure used to limit the electric field strength and ensure that the electric field is not overly concentrated at the edge of the device; the field stop ring 5 in the terminal region is used to further ensure the smooth termination of the electric field and reduce the field strength.
[0040] As described in step S40, in the process of etching the oxide layer 2 to form the window for the reserved area of the cell area, the window for the P-well area 7 of the cell area can also be simultaneously formed. That is, among the etching locations of the oxide layer 2 in the cell area, other etching locations except the reserved area are used as the window for the P-well area 7, so that the efficiency of forming the P-well area 7 can be improved.
[0041] If the thickness of the oxide layer at the manufacturing window of the P-well region 7 is increased during the subsequent process of forming the oxide layer in the reserved area, the oxide layer at the manufacturing window of the P-well region 7 can be removed or thinned again after the polysilicon is filled.
[0042] Reference Figure 4 , B+ ions are implanted at the manufacturing window of the P-well region 7 (other areas that do not require ion implantation can be protected based on photoresist), and impurity advancement is performed after debonding (Poly oxidation is performed at the same time), and the doped B+ ions are diffused in the crystal through heat treatment to form the P-well region 7, and the thickness of the formed P-well region 7 is made smaller than the thickness of the Poly gate 4, so that the two Poly gates 4 are equivalent to penetrating the P-well region 7. Among them, the heat treatment temperature is 1000~1150℃, which can effectively promote the diffusion and distribution of impurities and avoid material annealing caused by excessively high temperature; the time is 90~150min to ensure that the P-well is fully formed.
[0043] It should be understood that the purpose of implanting B+ ions in the fabrication window of the P-well region 7 is to introduce an appropriate concentration of doping so that the P-well region 7 forms the desired electrical characteristics. The implantation of B+ ions can provide a good doping layer for the P-well region 7 of the cell region, thereby improving the performance and stability of the device.
[0044] As described in step S50, after forming the P-well region 7, an oxide layer 2 covering the polysilicon (including the Poly gate 4, the field stop ring 5 and the Busbar trace 6) is formed on the upper surface of the polysilicon to isolate the polysilicon from other structures or media to protect the polysilicon from oxidation. In addition, the oxide layer 2 may also cover the upper surface of the P-well region 7 and the field limit ring 3.
[0045] Reference Figure 5 , a silicide region 8 is formed on the upper surface of the P-well region 7 between the two Poly gates 4 by sputtering metal titanium (if there is an excess oxide layer on the upper surface of the P-well region 7 between the two Poly gates 4, it can be thinned or etched away first); wherein the silicide region 8 can be a silicide (Silicide, the main component of which is SiTi) alloy region.
[0046] As described in step S60, refer to Figure 6 , a dielectric layer 9 is formed on the oxide layer 2 and the silicide region 8.
[0047] Among them, ILD (InterLayer Dielectric) dielectric layer deposition is used to form a dielectric layer 9 with a double-layer structure of USG+BPSG. The USG and BPSG layers can effectively isolate signals and prevent cross interference. The optional thickness range of the dielectric layer 9 is 9000~12000Å to ensure that the device can still exert good electrical characteristics under high temperature and high pressure conditions.
[0048] After the dielectric layer 9 is formed, the dielectric layer 9 is selectively etched (photolithography technology may be used to form an etching mask through exposure and development to ensure that only the cell region and the terminal region to be etched are exposed). The dielectric layer 9 in the cell region is selectively etched to form a contact window of the silicide region 8 (i.e., a window that can expose the silicide region 8); and contact windows corresponding to the polysilicon and the field limiting ring 3 are formed in the terminal region.
[0049] Among them, the contact window is used for subsequent metal deposition.
[0050] Metal deposition is performed at the contact windows to form a front metal layer 10 that fills each contact window and partially covers the dielectric layer 9 above the dielectric layer 9; wherein, the excess metal layer formed by deposition can be removed by dry etching in a graphical manner, which will not be described in detail here.
[0051] In this way, a front metal layer 10 penetrating through the dielectric layer 9 and contacting the silicide region 8 can be formed.
[0052] The thickness of the front metal layer 10 can be selected to be in the range of 4 to 8 μm.
[0053] As described in step S70, refer to Figure 7 A buffer layer 11 , a P-type doping layer 12 and a back metal layer 13 are sequentially formed under the back side of the substrate 1 .
[0054] When manufacturing the back side of the substrate 1 , the wafer may be turned over first so that the back side of the substrate 1 faces upward.
[0055] The buffer layer 11 refers to a thin film first formed on the back side of the substrate 1 , wherein the buffer layer 11 may be an N-type doped layer.
[0056] The buffer layer 11 is usually designed to provide electrical isolation between different materials of the IGBT, prevent current leakage between different regions, and ensure the stability of device performance. The N-type doped layer can help optimize the distribution of carriers, enhance device performance, improve conductivity, and reduce switching losses.
[0057] Furthermore, a P-type dopant (such as boron) is introduced onto the buffer layer 11 (or the lower surface if the back side of the substrate 1 faces downward) by ion implantation or diffusion process to form a P-type doping layer 12. The implantation dose and energy are controlled to ensure the required doping depth and concentration.
[0058] Furthermore, a back metal layer 13 is deposited on the lower surface of the P-type doping layer 12 (the lower surface if the back surface of the substrate 1 faces downward) by physical vapor deposition or chemical vapor deposition.
[0059] The thickness of the back metal layer 13 can be selected to be in the range of 1 to 2 μm.
[0060] The front metal layer 10 is used as the front cathode metal, and the back metal layer 13 is used as the back anode metal.
[0061] Reference Figure 7 Since the silicide region 8 is in contact with the front metal layer 10 (forming an electrical connection), and the P-type doped layer 12 is in contact with the back metal layer 13 as the back anode (forming an electrical connection), in the state where the channel is turned on, the silicide region 8 can provide electrons and play the same role as the N+ source in the traditional IGBT chip. At the same time, the contact with the P-well region 7 below is a Schottky contact, thereby replacing the N-type doped source in the traditional IGBT chip. Since there is no complete NPNP structure in the longitudinal direction of the IGBT chip, the meta-cell structure of this IGBT chip has a natural anti-latch characteristic, and latch failure will not occur under any circumstances, thereby enhancing the robustness and stability of the chip in extreme environments. In addition, since the front cathode metal (i.e., the front metal layer 10) is directly in contact with the P-well region 7 through the silicide region 8, the process steps of dry etching and B+ ion implantation after N+ ion doping in the traditional IGBT chip are also omitted, which can shorten the manufacturing cycle and production cost of the IGBT chip.
[0062] In one embodiment, by forming a contact structure of a silicide region and a P-well region in the IGBT chip structure as a Schottky contact to replace the NPNP structure in a traditional IGBT chip, the IGBT chip has a natural anti-latch characteristic, eliminating the latch effect, thereby enhancing the robustness and stability of the IGBT chip working in extreme environments.
[0063] In one embodiment, based on the above embodiment, referring to Figure 8 After the step of forming a dielectric layer on the oxide layer and the silicide region, and etching the dielectric layer to form a front metal layer penetrating the dielectric layer and contacting the silicide region, the method further includes: Step S61, forming a passivation layer on the dielectric layer and the front metal layer; Step S62: Photolithography is performed on the passivation layer in the cell region to remove the middle portion of the passivation layer, and the remaining passivation layer is divided into a left passivation layer and a right passivation layer.
[0064] In this embodiment, after forming the front metal layer 10, a passivation layer 14 is first formed on the dielectric layer 9 and the front metal layer 10. The passivation layer 14 can be formed by PI coating, and the thickness of the formed passivation layer 14 can be selected to be in the range of 8-12 um.
[0065] After the passivation layer 14 is formed, the passivation layer 14 in the cell area is patterned using photolithography technology, and the middle portion of the passivation layer 14 is removed, leaving the left and right passivation layers 14. Finally, two independent passivation regions can be formed on the dielectric layer 9 and the front metal layer 10: the left passivation layer 14 and the right passivation layer 14. The region without the passivation layer 14 in the middle exposes the front metal layer 10 below.
[0066] After the passivation layer 14 is made, step S70 is performed to finally form Fig. 9 The IGBT chip structure with a passivation layer 14 is shown.
[0067] The passivation layer 14 serves as an electrical insulation layer, which can protect the front metal layer 10 and the dielectric layer 9, prevent unnecessary current leakage, and ensure the stability of the electrical performance inside the device.
[0068] At the same time, the passivation layer 14 can provide environmental protection, prevent oxygen, moisture and other harmful substances from damaging the device, and increase the durability and service life of the device.
[0069] In addition, the formation of the left and right passivation layers can help improve the distribution of the electric field, reduce the local electric field strength, and help reduce the risk of electrical breakdown and failure. The lateral spacing design of the left and right passivation layers can promote the effective dissipation of heat and help avoid excessive local heating. The spacing between the passivation layers can effectively reduce parasitic capacitance, reduce the impact on device performance, and increase switching speed.
[0070] It should be noted that after executing step S60 to form the front metal layer 10, first executing steps S61-S62 to form the passivation layer 14, and then executing step S70, can improve the efficiency of the preparation process flow of the IGBT chip structure; of course, without considering the process efficiency, the present application does not exclude that after executing step S60 to form the front metal layer 10, step S70 may be first executed, and then steps S61-S62 may be executed to form the passivation layer 14, so as to form the corresponding IGBT chip structure in this process flow order.
[0071] In one embodiment, based on the above embodiment, the method for preparing the IGBT chip structure further includes: In the process of forming the oxide layer on the front side of the substrate, a wet oxygen process is used, and the process temperature is 800~1050℃; And / or, in the process of forming the oxide layer in the reserved area, a sacrificial oxide layer is first grown, and after the sacrificial oxide layer is removed, gate oxide is grown.
[0072] In this embodiment, in the process of forming the oxide layer 2 on the front surface of the substrate 1, the wet oxygen process is used, which means that an oxygen environment containing water vapor is used to promote an oxidation reaction at a specific temperature.
[0073] Optionally, a temperature of 800-1050° C. can promote the penetration of oxygen atoms on the surface of the substrate 1 and form a high-quality oxide layer 2. This temperature range is very effective for growing a thick and dense oxide layer 2.
[0074] The use of wet oxygen process can achieve a higher oxidation rate and better oxide layer quality, reduce defects and impurities, and improve electrical properties.
[0075] And / or, when the oxide layer 2 is formed in the reserved area, a sacrificial oxide layer is first grown. This oxide layer 2 is usually thin (optionally 800-1200Å) and serves as a protective layer or buffer layer 11 in subsequent processes. The purpose of this is to balance the surface charge and improve the growth environment of the subsequent oxide layer 2 through a preliminary oxidation reaction.
[0076] After the sacrificial oxide layer is grown, it is removed by chemical or dry etching. This process usually removes the excess oxide layer without affecting the subsequent gate oxide growth.
[0077] After removing the sacrificial oxide layer, gate oxide growth is performed (thickness can be selected from 1000 to 1200 Å). At this time, the oxide layer 2 will have better electrical properties, which can effectively improve the stability and switching performance of the device.
[0078] In one embodiment, based on the above embodiment, before the step of forming a P-well region at other etching locations of the oxide layer in the cell region except the reserved region, the step further includes: Etching the polysilicon on the front side of the substrate to form a Poly gate in a reserved area of the cell region; The polysilicon on the back side of the substrate is removed and a cleaning process is performed.
[0079] In this embodiment, after polysilicon deposition, the polysilicon on the front side of the substrate 1 is etched. Polysilicon etching refers to etching away the polysilicon material on the front side of the substrate 1 by chemical or dry etching to form a structure of a specific shape (eg, Poly gate 4).
[0080] The purpose of this step is to form a Poly gate 4 of a desired shape in the reserved area of the cell region for subsequent processing. As a gate electrode, the Poly gate 4 has good conductivity and control ability, and will regulate the flow of current.
[0081] If, during the polysilicon deposition process, redundant polysilicon is inevitably formed on the back side of the substrate 1, a corresponding acid or solution may be used to selectively remove only the polysilicon on the back side of the substrate 1, ensuring that the polysilicon structure on the front side is not affected.
[0082] After removing the polysilicon, a cleaning agent (such as deionized water, ammonia, hydrogen peroxide, etc.) is used for thorough cleaning to remove the remaining chemicals and impurities to ensure the cleanliness of the wafer surface. The cleaning process can prevent cross contamination of substances in subsequent processes and ensure that the surface structure of the substrate 1 is good, thereby improving the manufacturing yield and performance of the device.
[0083] In the preparation process of the IGBT chip structure, etching the polysilicon on the front side of the substrate 1 and removing and cleaning the polysilicon on the back side are key steps to ensure the success of subsequent processing. These steps lay the foundation for forming an effective Poly gate 4 and optimizing the formation of the P well region 7. At the same time, the cleaning process ensures the cleanliness of the substrate 1, reduces defects, and improves the electrical performance and manufacturing yield of the device.
[0084] In one embodiment, based on the above embodiment, the method for preparing the IGBT chip structure further includes: In the process of forming the field limiting ring, a dose of 8E13~5E14 B+ ions is injected, and the injection energy is 80~140keV; And / or, in the process of forming the P-well region, B+ ions with a dosage of 1E13-1E14 and an implantation energy of 80-140 keV are implanted.
[0085] In this embodiment, during the process of forming the field limiting ring 3, B+ ions with a dose of 8E13-5E14 are injected into the manufacturing window corresponding to the field limiting ring 3 in the terminal area (photoresist can be used to protect other areas during the process), and the injection energy is 80-140keV.
[0086] After degumming, impurity advancement is carried out at a temperature of 1000~1200℃ (this relatively high temperature helps to accelerate the diffusion rate of impurities) and the time is maintained for 300~600min (through long-term high-temperature treatment, a more uniform and deep doping distribution can be achieved).
[0087] And / or, in the process of forming the P-well region 7, a window is made into the P-well region 7 of the cell region, and B+ ions with a dose of 1E13-1E14 are injected (photoresist may be used to protect other areas during the process), and the injection energy is 80-140 keV.
[0088] Then after stripping, impurity pushing is carried out at a temperature of 1000~1150℃ (this temperature range helps to increase the diffusion rate of B+ ions and promotes the redistribution of ions in the substrate 1), and the time is maintained for 90~150min (the appropriate time extension allows the impurities to have enough time to diffuse and achieve the desired doping depth and concentration).
[0089] The high temperature and long driving process can make the doping more evenly distributed in the substrate 1, reduce the defect density and improve the electrical performance.
[0090] In one embodiment, based on the above embodiment, the step of forming a silicide region on the upper surface of the P-well region between the two Poly gates includes: Based on photolithography, a source contact window is formed above the P-well region between the two Poly gates; Etching the oxide layer of the source contact window to remove the oxide layer of the source contact window; Metal titanium sputtering is performed on the source contact window to form a silicide region on the upper surface of the P-well region between the two Poly gates.
[0091] In this embodiment, during the process of making the silicide region 8, a photoresist layer is first formed on the upper layer, and then the photoresist above the P well region 7 between the two Poly gates 4 is exposed (using a mask to protect other photoresists), and a source contact window (i.e., a window for making the silicide region 8) is etched. The thickness of the photoresist is 1-5 um, and the inclination angle of the side wall of the photoresist is 90°-135°.
[0092] Then, the oxide layer 2 at the source contact window is etched to remove the oxide layer 2 at the source contact window. The oxide layer etching can be performed by wet etching, dry etching, or the like.
[0093] Metal titanium sputtering is performed on the source contact window, and the sputtering thickness can be 500-2000Å, so as to form a silicide region 8 on the upper surface of the P-well region 7 between the two Poly gates 4.
[0094] Through the above steps, the source contact window formed on the P-well region 7 lays a foundation for the production of the silicide region 8. The good coating of the photoresist layer, the clear exposure profile and the window formed by etching ensure the accurate formation of the silicide region 8.
[0095] In one embodiment, based on the above embodiment, the step of performing metal titanium sputtering on the source contact window to form a silicide region on the upper surface of the P-well region between the two Poly gates includes: After metal titanium is sputtered on the source contact window, a stripping process is used to remove the photoresist and the metal titanium on the photoresist; A rapid thermal processing annealing process is performed to make the metal titanium react with the underlying silicon alloy to generate silicide, so as to form a silicide region on the upper surface of the P-well region between the two Poly gates.
[0096] In this embodiment, for the source contact window, a titanium film is formed on the upper surface of the P-well region 7 between the two Poly gates 4 by sputtering a titanium target material, so as to facilitate the subsequent silicide formation. The thickness of the titanium film is set to 500Å to 2000Å to ensure the uniformity of the metal film and good contact performance.
[0097] After the metal titanium is sputtered, a lift-off process is used to remove the photoresist and the metal titanium on the upper layer of the photoresist.
[0098] Then, a rapid thermal processing annealing process is performed at a temperature of 500-1000° C. for 0.5-10 minutes, so that the metal silicon reacts with the underlying silicon alloy to generate silicide, thereby forming a silicide region 8 on the upper surface of the P-well region 7 between the two Poly gates 4 .
[0099] Among them, the rapid thermal processing promotes the interaction between the titanium layer and the silicon crystal, and the generated titanium silicide improves the conductivity of the source and forms a good electrical contact.
[0100] In this way, by stripping off the photoresist and excess metal titanium to ensure the cleanliness of the wafer surface, and by rapid heat treatment, the metal titanium reacts with the underlying silicon to form a silicide region 8. These processes work together to provide a foundation for the electrical performance and stability of the IGBT chip structure.
[0101] In one embodiment, based on the above embodiment, before the step of sequentially forming a buffer layer, a P-type doping layer and a back metal layer under the back side of the substrate, the step further includes: The back of the wafer is ground to remove the silicon oxide on the back of the substrate and thin the wafer to 60~150um.
[0102] In this embodiment, in the aforementioned multiple times of growing the oxide layer 2 on the front side of the substrate 1, it is inevitable that unnecessary silicon oxide will also grow on the back side of the substrate 1. Therefore, before the steps of sequentially forming the buffer layer 11, the P-type doping layer 12 and the back metal layer 13 under the back side of the substrate 1, the back side of the wafer can be ground to remove the silicon oxide on the back side of the substrate 1 and reduce the wafer thickness to 60~150um.
[0103] By grinding the back side of the substrate 1, unnecessary silicon oxide layers are removed and the wafer thickness is reduced, thus creating a good foundation for the subsequent formation of the buffer layer 11, the P-type doping layer 12 and the back metal layer 13. This process ensures the success of the subsequent manufacturing process and improves the performance and reliability of the IGBT device.
[0104] In one embodiment, based on the above embodiment, the method for preparing the IGBT chip structure further includes: In the process of forming the buffer layer, P+ ions with a dose of 2E11~1E13 and an injection energy of 200~900keV are injected; And / or, in the process of forming the P-type doping layer, B+ ions with a dosage of 1E12-8E13 and an implantation energy of 20-50 keV are implanted.
[0105] In this embodiment, when executing step S70, in the process of forming the buffer layer 11, P+ ions with a dose of 2E11~1E13 and an injection energy of 200~900keV can be first implanted on the surface of the back side of the substrate 1 to form an N-type doped layer as the buffer layer 11.
[0106] Then, B+ ions with an implantation dose of 1E12-8E13 and an implantation energy of 20-50 keV are implanted into the other side (non-substrate contact side) of the buffer layer 11 to form a P-type doping layer 12 .
[0107] Then, furnace tube annealing is used to activate the impurities (the wafer can be placed in a furnace tube and annealed according to the set temperature and time), the temperature is 300~500°C, and the time is maintained for 20~80 minutes to form a buffer layer 11 and a P-type doping layer 12 under the back side of the substrate 1 in sequence.
[0108] Then, metal deposition is performed on the other side (non-buffer layer 11 contact side) of the P-type doping layer 12 to form a back metal layer 13 .
[0109] Through the above steps, a buffer layer 11 and a P-type doping layer 12 are sequentially formed on the back of the substrate 1, and then metal deposition is performed to finally realize the preparation of the IGBT chip structure. This series of processing steps ensures the electrical performance and structural stability of the device.
[0110] In addition, the present application also proposes an IGBT chip structure, which is prepared by using the preparation method of the IGBT chip structure described in the above embodiment.
[0111] Since the present IGBT chip structure adopts all the technical solutions of all the above embodiments, it at least has all the technical effects brought by the technical solutions of the above embodiments, which will not be described one by one here.
[0112] To sum up, the preparation method of the IGBT chip structure and the IGBT chip structure provided in the embodiments of the present application form contact structures of the silicide region and the P-well region in the IGBT chip structure as Schottky contacts to replace the NPNP structure in the traditional IGBT chip, so that the IGBT chip has a natural anti-latch characteristic, eliminates the latch effect, and thus enhances the robustness and stability of the IGBT chip working in extreme environments.
[0113] It should be noted that, in this article, the terms "include", "comprises" or any other variations thereof are intended to cover non-exclusive inclusion, so that a process, device, article or method including a series of elements includes not only those elements, but also includes other elements not explicitly listed, or also includes elements inherent to such process, device, article or method. In the absence of further restrictions, an element defined by the sentence "includes a ..." does not exclude the presence of other identical elements in the process, device, article or method including the element.
[0114] The above description is only a preferred embodiment of the present application, and does not limit the patent scope of the present application. Any equivalent structure or equivalent process transformation made using the contents of the present application specification and drawings, or directly or indirectly used in other related technical fields, are also included in the patent protection scope of the present application.
Claims
1. A method for preparing an IGBT chip structure, It is characterized in that include: forming an oxide layer over a substrate front side of the wafer; The oxide layer is selectively etched, and a field limiting ring and a reserved area are formed at the etched portion of the terminal area, and two reserved areas are formed at the etched portion of the cell area; After forming an oxide layer in the reserved area, polysilicon filling growth is performed, and a Poly gate is formed in the reserved area of the cell area, and a field stop ring is formed in the reserved area of the terminal area; A P-well region is formed at other etched locations of the oxide layer in the cell region except for the reserved region; An oxide layer is formed covering the polysilicon, and a silicide region is formed on the upper surface of the P-well region between the two Poly gates; Forming a dielectric layer on the oxide layer and the silicide region, and etching the dielectric layer to form a front metal layer penetrating the dielectric layer and contacting the silicide region; A buffer layer, a P-type doping layer and a back metal layer are sequentially formed under the back side of the substrate.
2. The method for preparing the IGBT chip structure according to claim 1, It is characterized in that After the steps of forming a dielectric layer on the oxide layer and the silicide region, and etching the dielectric layer to form a front metal layer penetrating the dielectric layer and contacting the silicide region, the method further includes: forming a passivation layer on the dielectric layer and the front metal layer; The passivation layer in the cell region is subjected to photolithography patterning to remove the middle portion of the passivation layer and to divide the remaining passivation layer into a left passivation layer and a right passivation layer.
3. The method for preparing the IGBT chip structure according to claim 1, It is characterized in that The method for preparing the IGBT chip structure further includes: In the process of forming the oxide layer on the front side of the substrate, a wet oxygen process is used, and the process temperature is 800~1050℃; And / or, in the process of forming the oxide layer in the reserved area, a sacrificial oxide layer is first grown, and after the sacrificial oxide layer is removed, gate oxide is grown.
4. The method for preparing the IGBT chip structure according to claim 1, It is characterized in that Before the step of forming a P-well region at other etching locations of the oxide layer in the cell region except the reserved region, the method further includes: Etching the polysilicon on the front side of the substrate to form a Poly gate in a reserved area of the cell region; The polysilicon on the back side of the substrate is removed and a cleaning process is performed.
5. The method for preparing the IGBT chip structure according to claim 1, It is characterized in that The method for preparing the IGBT chip structure further includes: In the process of forming the field limiting ring, a dose of 8E13~5E14 B+ ions is injected, and the injection energy is 80~140keV; And / or, in the process of forming the P-well region, B+ ions with a dosage of 1E13-1E14 and an implantation energy of 80-140 keV are implanted.
6. The method for preparing the IGBT chip structure according to claim 1, It is characterized in that The step of forming a silicide region on the upper surface of the P-well region between the two Poly gates comprises: Based on photolithography, a source contact window is formed above the P-well region between the two Poly gates; Etching the oxide layer of the source contact window to remove the oxide layer of the source contact window; Metal titanium sputtering is performed on the source contact window to form a silicide region on the upper surface of the P-well region between the two Poly gates.
7. The method for preparing the IGBT chip structure according to claim 6, It is characterized in that The step of performing metal titanium sputtering on the source contact window to form a silicide region on the upper surface of the P-well region between the two Poly gates includes: After metal titanium is sputtered on the source contact window, a stripping process is used to remove the photoresist and the metal titanium on the photoresist; A rapid thermal processing annealing process is performed to make the metal titanium react with the underlying silicon alloy to generate silicide, so as to form a silicide region on the upper surface of the P-well region between the two Poly gates.
8. The method for preparing the IGBT chip structure according to claim 1, It is characterized in that Before the step of sequentially forming a buffer layer, a P-type doping layer and a back metal layer under the back side of the substrate, the method further includes: The back of the wafer is ground to remove the silicon oxide on the back of the substrate and thin the wafer to 60~150um.
9. The method for preparing the IGBT chip structure according to claim 1, It is characterized in that The method for preparing the IGBT chip structure further includes: In the process of forming the buffer layer, P+ ions with a dose of 2E11~1E13 and an injection energy of 200~900keV are injected; And / or, in the process of forming the P-type doping layer, B+ ions with a dosage of 1E12-8E13 and an implantation energy of 20-50 keV are implanted.
10. An IGBT chip structure, It is characterized in that The IGBT chip structure is prepared by the method for preparing an IGBT chip structure according to any one of claims 1 to 9.
Citation Information
Patent Citations
Novel source Schottky contact IGBT structure
CN113013239A
High-reliability IGBT (Insulated Gate Bipolar Translator) chip and manufacturing method thereof
CN114975602A
IGBT (Insulated Gate Bipolar Translator) chip with trench field cut-off structure and manufacturing method thereof
CN116646384A
Devices and methods for a power transistor having a schottky or schottky-like contact
US20170323970A1