Epitaxial film growth state detection method and detection system
By using a combination method of optical detection device and main control device on semiconductor growth equipment, the crystal form of the epitaxial film is monitored in real time, and the defect problem caused by mismatch of the crystal lattice and thermal expansion coefficient during heteroepitaxial film growth is solved, and the epitaxial film is improved quality and production efficiency.
Patent Information
- Application Number
- CN202410907219.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-08
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2044-07-08
AI Technical Summary
During the growth of heteroepitaxial membranes, due to the mismatch between the lattice and thermal expansion coefficients between the substrate material and the epitaxial membrane material, the epitaxial membrane structure is prone to high-density defects, and it is difficult for the prior art to realize real-time monitoring of the epitaxial membrane surface. Evaluate.
By combining an optical detection device and a main control device, optical detection of light in a specific wavelength range is performed on the epitaxial film on the semiconductor growth device, light intensity information is obtained, and calculation is performed based on the relationship data between the pre-stored crystal form and the absorption coefficient. Monitor the crystal form of the epitaxial film surface in real time.
Real-time crystal form monitoring and evaluation during epitaxial film growth process, can promptly detect abnormal crystal form, uneven thickness and growth rate problems, improve the deposition quality of epitaxial film, reduce trial and error and waiting time, and is suitable for high frequency and large Manufacturing of power devices.
Smart Images

Figure CN119092420A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of semiconductor material growth, and in particular to an epitaxial film growth state detection method and detection system. Background Art
[0002] Some semiconductor materials, such as aluminum gallium nitride (AlGaN), are suitable for manufacturing high-frequency and high-power devices with high temperature resistance due to their wider bandgap, higher thermal conductivity and dielectric constant. However, some of these semiconductor materials have high bond energy and are difficult to form high-quality substrates through crystal pulling or cutting.
[0003] The epitaxial process is a technology that grows an epitaxial film along a specific crystal direction on a crystal-oriented substrate, and the device manufacturing continues on the epitaxial film. The epitaxial film can be a homoepitaxial film, that is, the substrate and the epitaxial film have the same material, or a heteroepitaxial film, that is, the substrate and the epitaxial film have different composition materials. It can be seen that the epitaxial process can form a high-quality heteroepitaxial film of high-bond energy semiconductor material on the substrate, which is conducive to the manufacture of high-frequency and high-power devices.
[0004] However, for heteroepitaxial films, due to the mismatch in lattice and thermal expansion coefficient between the substrate material and the epitaxial film material, the epitaxial film structure is prone to high-density defects. Therefore, high requirements are placed on the heteroepitaxial process, and it is necessary to monitor and evaluate the crystal type of the epitaxial film surface in real time during the heteroepitaxial process. Summary of the invention
[0005] The present application provides an epitaxial film growth state detection method and a detection system for executing the growth state detection method, so as to achieve real-time monitoring and evaluation of the crystal state of the film surface during the epitaxial film growth process.
[0006] The epitaxial film growth state detection method of the present application at least comprises the following steps:
[0007] S0: providing a semiconductor growth device, an optical detection device and a main control device, wherein the semiconductor growth device carries a substrate, the optical detection device is arranged in the semiconductor growth device, the main control device is in communication connection with the optical detection device, and the main control device pre-stores crystal form correspondence data of crystal forms of semiconductor materials at different wavelengths and corresponding absorption coefficients, and each of the absorption coefficients is different;
[0008] S1: controlling the semiconductor growth device to perform an epitaxial process on the substrate, so that an epitaxial film composed of the semiconductor material and having a composition material different from that of the substrate is formed on the exposed surface of the substrate;
[0009] S2: During the execution of the epitaxial process, controlling the optical detection device to emit light in a specific wavelength range to the epitaxial film for optical detection, and acquiring and sending light intensity information of the epitaxial film to the main control device;
[0010] S3: The main control device calculates according to the light intensity information of the epitaxial film, the specific wavelength and the crystal type correspondence data to obtain the real-time crystal type information of the surface of the epitaxial film.
[0011] The detection system of the present application is used to execute the epitaxial film growth state detection method, and the detection system includes an optical detection device for being set on a semiconductor growth device, and a main control device communicatively connected to the optical detection device. The semiconductor growth device is configured to perform an epitaxial process on a substrate to form an epitaxial film whose composition material is different from that of the substrate.
[0012] The beneficial effects of the epitaxial film growth status detection method and the detection system described in the present application are: by controlling the optical detection device to emit light in a specific wavelength range to the epitaxial film for optical detection during the execution of the epitaxial process, and obtaining and sending the light intensity information of the epitaxial film to the main control device, and the main control device performs calculations based on the light intensity information of the epitaxial film, the specific wavelength and the crystal type correspondence data, so as to realize real-time monitoring and evaluation of the crystal type condition of the film surface during the epitaxial film growth process.
[0013] Optionally, the main control device also pre-stores empirical reflectivity correspondence data with the reflectivity, thickness, phase difference, absorption coefficient and refractive index of the semiconductor material. In step S3, the main control device performs calculations according to the light intensity information, the specific wavelength and the crystal form correspondence data, including:
[0014] S31: the main control device obtains real-time reflectivity correspondence data between the real-time reflectivity of the epitaxial film and the growth time according to the light intensity information of the epitaxial film;
[0015] S32: The main control device calculates the real-time absorption coefficient of the epitaxial film according to the real-time reflectivity correspondence data and the empirical reflectivity correspondence data, and obtains the real-time crystal type information of the epitaxial film surface according to the real-time absorption coefficient, the specific wavelength and the crystal type correspondence data.
[0016] Optionally, the empirical reflectivity correspondence data includes:
[0017]
[0018] in:
[0019] R is the empirical reflectivity, ni is the refractive index of the reaction space medium above the epitaxial film, n j is the refractive index of the semiconductor material, n k is the refractive index of the substrate material, a is the absorption coefficient of a specific crystal plane of the semiconductor material at the specific wavelength, γ is the phase difference, d is the optical thickness of the epitaxial film;
[0020] λ is the specific wavelength, i is the incident angle of the light in the specific wavelength range from the reaction space medium to the epitaxial film, j is the refraction angle of the outgoing light emitted from the bottom surface of the epitaxial film, and k is the refraction angle of the outgoing light emitted from the bottom surface of the substrate.
[0021] Optionally, the real-time reflectivity correspondence data is periodic oscillation curve data of the real-time reflectivity and growth time of the epitaxial film.
[0022] Optionally, the real-time reflectivity of the epitaxial film tends to decay as the growth time increases.
[0023] Optionally, before executing step S1, the step of acquiring the specific wavelength is further included:
[0024] Obtaining single crystal samples of different crystal forms of the semiconductor material;
[0025] Performing optical testing and analysis on each of the single crystal samples under light of different wavelength ranges to obtain absorption spectrum group data;
[0026] Acquire the wavelength corresponding to the maximum value of the absorption coefficient of each single crystal sample in the absorption spectrum data to form a wavelength data group, and acquire the crystal form corresponding relationship data;
[0027] Any wavelength in the wavelength data group is selected as the specific wavelength.
[0028] Optionally, the step of obtaining single crystal samples of different crystal forms of the semiconductor material includes:
[0029] Obtaining a single crystal sample of the semiconductor material to be cut;
[0030] The single crystal samples to be cut are subjected to crystal plane cutting to form the single crystal samples.
[0031] Optionally, the semiconductor growth equipment includes a carrying device to carry the substrate;
[0032] The process of executing the step S1 includes controlling the carrying device to drive the substrate to rotate;
[0033] The process of executing step S2 further includes controlling the optical detection device to emit the light in the specific wavelength range to the carrier device, so as to obtain and send the received light intensity information of the carrier device to the main control device;
[0034] In step S3, the main control device performs subtraction processing based on the light intensity information of the epitaxial film and the light intensity information of the carrier device to deduct background information including thermal radiation information, and then performs calculation based on the obtained light intensity information, the specific wavelength and the crystal type correspondence data.
[0035] Optionally, after the step S32 is executed, the following steps are further performed:
[0036] S33: the main control device calculates the real-time optical thickness increment of the epitaxial film according to the empirical reflectivity correspondence data, the real-time reflectivity correspondence data and the real-time crystal type information;
[0037] S34: The main control device obtains the growth rate change data of the epitaxial film according to the real-time optical thickness increment.
[0038] Optionally, step S33 includes:
[0039] S331: The main control device obtains the reflectivity value in the ith period of the periodic oscillation curve, the empirical reflectivity correspondence value and the real-time crystal type information. i The real-time optical thickness increment Δd of the epitaxial film within a time period i ;
[0040] S332: The main control device obtains the reflectivity value at Δt according to the real-time reflectivity values in the (i+n)th period of the periodic oscillation curve, the empirical reflectivity correspondence value and the real-time crystal type information. (i+n) The real-time optical thickness increment Δd of the epitaxial film within a time period (i+n) ;
[0041] S333: Repeat step S332 until the epitaxial process is completed or until the
[0042] in:
[0043] i is a positive integer greater than or equal to 1, n is a positive integer greater than or equal to 1 and the values are taken sequentially.
[0044] Optionally, the energy of light in the specific wavelength range is greater than the bandgap width of the semiconductor material.
[0045] Optionally, the epitaxial film is an epitaxial doped film. BRIEF DESCRIPTION OF THE DRAWINGS
[0046] Figure 1 A flow chart of a method for detecting epitaxial film growth status provided by an embodiment of the present invention;
[0047] Figure 2 A schematic diagram of the working state of the detection device provided by an embodiment of the present invention;
[0048] Figure 3 A schematic diagram of the structure of a detection device provided in an embodiment of the present invention;
[0049] Figure 4 A schematic diagram of a light path formed by light incident on a thin film on a substrate provided by an embodiment of the present invention;
[0050] Figure 5 A schematic diagram of the periodic oscillation of reflectivity with optical thickness provided by an embodiment of the present invention;
[0051] Figure 6 A schematic diagram of the periodic attenuation oscillation of reflectivity with optical thickness provided by an embodiment of the present invention;
[0052] Figure 7 A graph showing the relationship between the absorption coefficient and wavelength of different doped epitaxial films provided in an embodiment of the present invention.
[0053] Description of reference numerals:
[0054] 1.500 substrates
[0055] 2 films
[0056] 3 Medium
[0057] 100 Reaction chamber
[0058] 200 Master control device
[0059] 300 Detection Device
[0060] 310 light emitter
[0061] 320 light emitter adjustment unit
[0062] 330 Connector
[0063] 340 Light Transmission Department
[0064] 400 Carrier DETAILED DESCRIPTION
[0065] For semiconductor materials with very high bond energy that are difficult to form high-quality substrates through crystal pulling or cutting, a corresponding heteroepitaxial film can be grown on a heterogeneous substrate through a heteroepitaxial process. Since the substrate used in the epitaxial process has a specific crystal orientation feature (the crystal orientation feature is determined according to the requirements of semiconductor device manufacturing), the epitaxial process requires the control of the epitaxial film to follow the crystal orientation feature of the substrate for extension growth, thereby ensuring that the crystal orientation is highly consistent with the substrate and the lattice structure is highly complete. However, due to the different constituent materials of the substrate and the epitaxial film, the mismatch between the lattice and thermal expansion coefficient between the two makes the epitaxial film structure prone to high-density defects. Therefore, it is necessary to monitor and evaluate the crystal form of the epitaxial film surface in real time during the epitaxial process.
[0066] It can be understood that the technical solution provided in this embodiment is also applicable to the thin film deposition process in which the substrate and the epitaxial layer are made of the same material or the material deposition process in the preparation of other semiconductor functional layers. No excessive restrictions are made here to expand the scope of application of the technical solution provided in this embodiment.
[0067] The embodiment of the present invention provides a method for detecting the growth state of an epitaxial film and a detection system for executing the growth detection method, so as to monitor and evaluate the lattice growth condition of the epitaxial film during its growth process non-destructively, rapidly and in real time through a non-contact optical detection method, and at the same time obtain the optical thickness of the heteroepitaxial film and the change in the growth rate.
[0068] The detection system provided by the embodiment of the present invention comprises an optical detection device and a main control device which are communicatively connected to each other, and the optical detection device is arranged in the semiconductor growth equipment.
[0069] The epitaxial film growth state detection method of the embodiment of the present invention refers to Figure 1 ,include:
[0070] S1: controlling the semiconductor growth device to perform an epitaxial process on the substrate, so that an epitaxial film composed of the semiconductor material and having a composition material different from that of the substrate is formed on the exposed surface of the substrate;
[0071] S2: During the execution of the epitaxial process, controlling the optical detection device to emit light in a specific wavelength range to the epitaxial film for optical detection, and acquiring and sending the received light intensity information of the epitaxial film to the main control device;
[0072] S3: The main control device calculates according to the light intensity information, the specific wavelength and the crystal type correspondence data to obtain real-time crystal type information of the epitaxial film surface.
[0073] The following will be combined with the drawings in the embodiments of the present invention, and the technical solution of the present application will be described in detail through Examples 1 to 5. Those skilled in the art can understand other advantages and effects of the present application from the contents disclosed in this specification. The present application can also be implemented or applied through other different specific implementation methods, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present application.
[0074] Embodiment 1:
[0075] The semiconductor growth equipment for performing the epitaxial process provided in this embodiment is a MOCVD equipment, see Figure 2 , including a reaction chamber 100, the reaction chamber 100 has a built-in carrier 400, the top surface of the carrier 400 carries a substrate 500, and a gas injection device (not shown in the figure) opposite to the top surface of the carrier 400 is arranged on the top of the reaction chamber 100 to provide process gas toward the substrate 500.
[0076] In step S1, the semiconductor growth device is controlled to perform an epitaxial process on the substrate, so that an epitaxial film composed of the semiconductor material and having a composition material different from that of the substrate is formed on the exposed surface of the substrate. Specifically:
[0077] In the semiconductor growth device provided in this embodiment, a heating device is further provided under the carrier device 400 to adjust the temperature in the reaction chamber 100. Specifically, the heating device transfers heat to the substrate 500 via the carrier device 400. In the semiconductor growth device provided in this embodiment, a pressure control system including an exhaust system and an exhaust system is further provided to adjust the pressure in the process chamber. The specific implementation methods of the heating device and the pressure control system are conventional technical means of those skilled in the art.
[0078] In this embodiment, the semiconductor growth equipment is controlled to perform an epitaxial process on the substrate. Specifically, the heating device is controlled to make the reaction chamber 100 meet the process temperature conditions required by the epitaxial process, and the pressure control system is controlled to make the pressure in the reaction chamber 100 meet the process pressure conditions required by the epitaxial process. Then, the carrier 400 is controlled to drive the substrate 500 to rotate around the axis of the reaction chamber 100 at a certain rate, and the gas injection device is controlled to provide the process gas for the epitaxial process to the top surface of the carrier 400, so that the process gas is epitaxially grown on the surface of the substrate 500 to form an epitaxial film composed of semiconductor materials and different from the composition material of the substrate 500, that is, a heteroepitaxial film. The rotation of the carrier 400 enables the process gas above the top surface of the carrier 400 to be evenly mixed, which is conducive to improving the quality of the epitaxial film.
[0079] In some embodiments, it may be selected whether to adjust the rotation of the carrier device 400 according to the requirements of the epitaxial process.
[0080] In some embodiments, the heteroepitaxial film is aluminum gallium nitride (Al (1-x) Ga x As) epitaxial film. The semiconductor growth equipment is a MOCVD equipment, the carrier device 400 is a graphite base, and the corresponding substrate 500 is a silicon substrate. Specifically, the growth temperature is controlled at 1100 degrees Celsius, the process pressure is controlled at 50 Torr, the source gas used is trimethylaluminum, trimethylgallium and ammonia, and the specific epitaxial process is a conventional technical means in the art.
[0081] In some embodiments, the epitaxial process includes any one of epitaxial film preparation processes such as metal organic chemical vapor deposition (MOCVD), molecular beam epitaxy (MBE), pulsed laser deposition (PLD) or atomic layer deposition (ALD), and the epitaxial film in this embodiment is obtained by metal organic chemical vapor deposition (MOCVD) process.
[0082] In order to facilitate the optical detection of the epitaxial film formed on the substrate, refer to Figure 2 A transparent window (not shown) is disposed on the top of the reaction chamber 100 , and the optical detection device 300 is disposed above the transparent window. The optical detection device 300 is electrically connected to the main control device 200 to transmit the light intensity information of the reflected light.
[0083] Furthermore, the specific configuration of the transparent window and the optical detection device 300 must not affect the normal operation of the gas injection device and the pressure in the reaction chamber 100 .
[0084] The optical detection device 300 is arranged at the top of the reaction chamber 100. During the execution of the epitaxial process, the optical detection device 300 emits light in a specific wavelength range to the area where the substrate is located in the reaction chamber 100, can receive reflected light in the specific wavelength range, and transmit the acquired light intensity information to the main control device 200.
[0085] The main control device 200 is used to receive the light intensity information from the optical detection device 300 and perform data processing on the light intensity information, so as to obtain the growth state of the heterogeneous epitaxial film in the reaction chamber 100 in real time, such as the surface crystal form, optical thickness, and growth rate change of the epitaxial film. The provision of the above information enables the process personnel to know the process growth of the epitaxial film in time, so as to be used as a reference for optimizing and adjusting the growth process of the epitaxial film, and to find abnormal conditions in the growth process at the first time, such as abnormal crystal form, uneven thickness, too fast or too slow growth rate, etc., so as to adjust the process parameters in time to ensure that the deposition quality of the epitaxial film meets the requirements, and also helps to reduce the trial and error and waiting time in the epitaxial process, and provide valuable reference for subsequent large-scale production.
[0086] In one embodiment, see Figure 3 , the detection device 300 at least comprises:
[0087] Light extractor 310;
[0088] The light emitter adjustment unit 320 is connected to the light emitter 310 and is used to drive the light emitter 310 to move so as to adjust the position and direction of the light emitter 310;
[0089] The connection base 330 is connected to the light emitter adjustment part 320. The connection base 330 is provided with a light through hole (not shown in the figure). The light through hole is used for passing the light emitted by the light emitter 310 and the light reflected by the epitaxial film;
[0090] The light propagation unit 340 is located between the light emitter 310 and the light hole of the connection base 330, and is used to transmit and / or focus the light emitted by the light emitter 310 to the surface of the film to be tested, and receive the light reflected by the epitaxial film and passing through the light hole. Further, the light propagation unit 340 includes a photodetector, which receives the reflected light to obtain optical information and sends the optical information to the main control device 200.
[0091] In step S2, during the execution of the epitaxial process, the optical detection device is controlled to emit light in a specific wavelength range to the epitaxial film for optical detection, and the received light intensity information is obtained and sent to the main control device. Specifically:
[0092] The optical detection device 300 is disposed on the top of the transparent window of the reaction chamber 100 through the connection seat 330. Before detection, the light emitter adjustment part 320 is adjusted so that the light emitted by the light emitter 310 is processed by the light propagation part 340, and then incident on the substrate or epitaxial film through the light hole of the connection seat 330 and the transparent window of the reaction chamber 100, and then the light is reflected by the substrate or epitaxial film and transmitted back to the light propagation part 340 of the detection device 300, and is processed into optical information by the light propagation part 340 and sent to the main control device 200 for calculation and analysis.
[0093] In one embodiment, the main control device 200 pre-stores crystal form correspondence data of the semiconductor material at different wavelengths and the corresponding absorption coefficient.
[0094] In one embodiment, the main control device 200 pre-stores empirical reflectivity correspondence data between the reflectivity, thickness, phase difference, absorption coefficient and refractive index of the semiconductor material.
[0095] Embodiment 2:
[0096] This embodiment provides a method for obtaining a specific wavelength λ.
[0097] In step S3, the main control device performs calculations based on the light intensity information, the specific wavelength and the crystal type correspondence data to obtain real-time crystal type information of the epitaxial film surface.
[0098] In this embodiment, step S3 includes:
[0099] S31: The main control device obtains real-time reflectivity correspondence data between the real-time reflectivity of the epitaxial film and the growth time according to the light intensity information.
[0100] See also Figure 4 , a heterogeneous epitaxial film 2 is covered on the substrate 1. When light is incident from the medium to the epitaxial film 2, it is reflected and refracted once at the medium / epitaxial film interface. The refracted light is further reflected twice at the substrate / epitaxial film interface. After the epitaxial film begins to grow, as its optical thickness increases, the reflectivity and refractive index change. For example, under vertical incidence, the reflectivity increases with the optical thickness. Figure 5 The periodic oscillation characteristics shown in the figure show that the maximum and minimum values of the reflectivity appear at the point where the optical thickness of the film is an integer multiple of 1 / 4 of the incident wavelength. Therefore, it is possible to determine whether the optical thickness of the film has reached 1 / 4 of the incident wavelength thickness by judging the maximum and minimum values of the reflectivity. More importantly, due to the increase in thickness of the film growth during the epitaxial process, the reflectivity presents a periodic oscillation characteristic as the optical thickness increases, which is also the theoretical basis for the application to monitor the real-time crystal information on the surface of the epitaxial film.
[0101] However, since the epitaxial film absorbs certain wavelengths of light, its reflectivity R will also show a decay trend over time. Figure 6 The real-time reflectivity correspondence data of the embodiment shown is a periodic attenuation oscillation curve of the real-time reflectivity of the epitaxial film and the growth time. If the incident wavelength is not properly selected, the attenuation of R is so significant that its periodic change over time is not significant or even presents a linear trend. Therefore, it is necessary to select a suitable light with a specific wavelength λ so that the real-time reflectivity correspondence data between the real-time reflectivity R and the growth time obtained by the main control device according to the light intensity information has a significant periodic change.
[0102] In some embodiments, the energy of a specific wavelength is greater than the bandgap width of the semiconductor material. If the energy of the specific wavelength is lower than the bandgap width, the incident light emitted to the epitaxial film will be completely absorbed by the semiconductor material, or fluorescence excitation will occur so that the optical detection device cannot detect the corresponding reflected light.
[0103] In this embodiment, before executing step S1, the step of acquiring the specific wavelength includes:
[0104] S01: Obtaining single crystal samples of different crystal forms of the semiconductor material;
[0105] S02: performing optical testing and analysis on each of the single crystal samples under light of different wavelength ranges to obtain absorption spectrum group data;
[0106] S03: in the absorption spectrum group data, obtaining the wavelength corresponding to the maximum absorption coefficient of each single crystal sample to form a wavelength data group, and obtaining the crystal form corresponding relationship data;
[0107] S04: Select any wavelength in the wavelength data group as the specific wavelength.
[0108] In step S01 of this embodiment, the epitaxial film is an epitaxial doped film, and the corresponding composition is Al(1-x)GaxAs. Different values of x correspond to epitaxial films of different crystal forms. The epitaxial film of the required composition is designed according to the functional requirements of the semiconductor device, and then the corresponding epitaxial process is selected. In addition, the crystal form needs to be monitored during the epitaxial process to determine whether the composition of the epitaxial film meets the device requirements.
[0109] In some embodiments, the step of obtaining single crystal samples of different crystal forms of the semiconductor material includes: obtaining single crystal samples of the semiconductor material to be cut; performing crystal face cutting on the single crystal samples to be cut to form each single crystal sample. This method requires that the single crystal sample is suitable for crystal face cleavage by crystal face cutting, and it is necessary to select a suitable crystal orientation deviation angle and ensure that the cutting process does not destroy the cutting crystal face characteristics as much as possible. For example, taking silicon carbide as an example, its (0001) and (11-20) direction crystal faces are cut from 4H-SiC single crystal samples grown along (000-1)C, and the cutting inclination angle is 4 degrees away from the [11-20] crystal direction. (11-22) and (11-2-2) oriented wafers are cut from 4H-SiC of the same orientation. The (11-22) oriented 4H-SiC crystal is cut from the (000-1)C crystal plane at an angle of 73° relative to the basal plane.
[0110] In step S02 of this embodiment, the instrument used for optical testing and analysis is a VERTEX 80 Fourier transform infrared (FTIR) spectrometer, and the sample to be tested is placed on the measuring platform of the instrument for measurement and analysis at room temperature. Transmission and reflection measurements are performed at the same point of the sample, and the light incident angle is selected to be close to the normal of the corresponding sample. The probe beam is polarized by a linear polarizer, and the sample under study is rotated to change the angle between the optical axis of the crystal c and the electric field vector of the incident electromagnetic wave e. The specific test and analysis implementation method is a routine operation of those skilled in the art.
[0111] In step S03 of this embodiment, the Figure 7 The corresponding relationship between the absorption coefficient and wavelength of each single crystal sample is shown in the figure. Figure 7It can be seen that the wavelengths corresponding to the maximum absorption coefficients of the single crystal samples all fall within a narrow range of 0.23 μm to 0.26 μm. This narrow range is the wavelength data set of the light in this specific wavelength range, that is, ultraviolet light can be used as the specific wavelength light.
[0112] Embodiment three:
[0113] This embodiment provides a step of performing background information subtraction including thermal radiation information by using the optical detection device 300 during the epitaxial process to ensure accurate detection results.
[0114] Since the epitaxial process reaction space is filled with hot medium (hot process gas atmosphere), such as Al (1-x) Ga x The process temperature of the As epitaxial process reaches 1100 degrees Celsius, and the epitaxial film itself will generate significant thermal radiation. This part of the thermal radiation enters the optical detection device along with the reflected light, so that its radiation information is included in the light intensity information, and this part of the radiation information needs to be deducted.
[0115] Since the carrier device drives the carrier substrate of the epitaxial film to rotate synchronously, and the carrier device and the epitaxial film are in the same process environment, it can be considered that the temperature of the two is the same, so in the process of executing the step S2, it also includes controlling the optical detection device to emit the light in the specific wavelength range to the carrier device, so as to obtain and send the light intensity information of the carrier device to the main control device. In this embodiment, the carrier device absorbs most or even all of the light in the specific wavelength range significantly, and the real-time reflectivity of the carrier device does not change substantially with the growth time. The light intensity information of the carrier device is the information reflected to the optical detection device due to thermal radiation. Specifically, the constituent material of the carrier device in this embodiment is different from the epitaxial film material, and is a light absorbing material that absorbs light in the specific wavelength range, for example, graphite. More specifically, the optical detection device in a fixed position can collect the light intensity information of the epitaxial film and the light intensity information of the carrier device when detecting the rotating carrier device. The main control device can distinguish and process these two types of information, and the specific processing method is a conventional technical means of those skilled in the art.
[0116] In some embodiments, the carrier device has a certain reflectivity to light within a specific wavelength range, and the light intensity information of the carrier device includes not only thermal radiation information but also real-time reflection information of the carrier device. The main control device further deducts the real-time reflection information of the carrier device, and the specific processing method is a conventional technical means of those skilled in the art.
[0117] Furthermore, in step S3, the main control device performs a subtraction process on the received light intensity information to deduct background information including thermal radiation information, and then performs calculation based on the obtained light intensity information, the specific wavelength and the crystal form correspondence data.
[0118] Embodiment 4:
[0119] This embodiment provides a method for obtaining the real-time crystal structure of an epitaxial film.
[0120] After step S31 of Example 2 is completed, S32 is executed: the main control device calculates the real-time absorption coefficient of the epitaxial film according to the real-time reflectivity correspondence data and the empirical reflectivity correspondence data, and obtains the real-time crystal type information of the epitaxial film surface according to the real-time absorption coefficient, the specific wavelength and the crystal type correspondence data.
[0121] The main control device pre-stores empirical reflectivity corresponding relationship data related to the reflectivity, thickness, phase difference, absorption coefficient and refractive index of the semiconductor material. The empirical reflectivity is R.
[0122] Specifically,
[0123]
[0124] in:
[0125] n i is the refractive index of the reaction space medium above the epitaxial film, n j is the refractive index of the semiconductor material, n k is the refractive index of the substrate material, which are constants pre-stored in the main control device.
[0126] a is the absorption coefficient of a specific crystal plane of the semiconductor material at the specific wavelength, γ is the phase difference, d is the optical thickness of the epitaxial film, λ is the specific wavelength, i is the incident angle of the light in the specific wavelength range from the reaction space medium to the epitaxial film, j is the refraction angle of the outgoing light emitted from the bottom surface of the epitaxial film, and k is the refraction angle of the outgoing light emitted from the bottom surface of the substrate.
[0127] Perform epitaxial process to prepare Al (1-x) Ga x During the As epitaxial film growth process, the optical detection device emits light vertically to the epitaxial film, so that the values of cosi, cosj, and cosk can all be approximately 1. The main control device obtains the light intensity information of the epitaxial film obtained and sent by the optical detection device. Figure 6The real-time reflectivity and growth time periodic oscillation decay curve is shown. The real-time reflectivity corresponding to the adjacent d sampling growth time of the curve is R1 and R2 respectively. Solving the following equation can calculate the real-time absorption coefficient a, and then refer to Figure 7 According to the absorption coefficient a, Al (1-x) Ga x The value of x in As can be used to obtain the value of Al (1-x) Ga x The crystal form corresponding to the As composition.
[0128]
[0129] Embodiment five:
[0130] This embodiment provides a method for obtaining real-time optical thickness and growth rate variation data of an epitaxial film.
[0131] After S32 of the fifth embodiment is completed, S33 is executed: the main control device calculates the real-time optical thickness of the epitaxial film according to the empirical reflectivity correspondence data, the real-time reflectivity correspondence data and the real-time crystal type information, specifically:
[0132] S331: The main control device obtains the value of the adjacent real-time reflectivity in the ith period of the periodic oscillation curve, the empirical reflectivity correspondence value and the real-time crystal type information at Δt i The real-time optical thickness d of the epitaxial film during the time period i .
[0133] Specifically, since the time of one cycle is very short, the absorption coefficient a can be taken as the value determined in step S32, referring to Figure 6 In the Δt1 time period from t1 to t2 (the first cycle), the absorption coefficient a can be calculated at adjacent time nodes according to the adjacent real-time reflectivity peak value R max1 and R max2 The optical thickness increment Δd1=d2-d1 within the Δt1 time period is calculated:
[0134]
[0135] After step S331 is completed, step S332 is executed: the main control device obtains the value of the adjacent real-time reflectivity in the (i+n)th period of the periodic oscillation curve, the corresponding relationship value of the theoretical reflectivity and the real-time crystal type information at Δt (i+n) The real-time optical thickness increment Δd of the epitaxial film within a time period (i+n) .
[0136] Specifically, refer to Figure 6, in the Δt2 time period from t2 to t3 (the second cycle), according to the adjacent real-time reflectivity peak value R max3 and R max4 The average optical thickness increment Δd2=d3-d4 within the Δt2 time period is calculated:
[0137]
[0138] Similarly, in step S333, the average optical thickness increment Δd3 in the Δt3 time period of the next cycle can be calculated based on the adjacent real-time reflectivity peak values. Similarly, the average optical thickness increments Δd1, Δd2, ... Δd3 in each of the n cycles are obtained. n Until the epitaxial process is completed, or until the real-time reflectivity meets exist In this case, it indicates that the attenuation oscillation trend of the real-time reflectivity R with the growth time has tended to a linear relationship.
[0139] Further, according to the average optical thickness increments Δd1, Δd2, ... Δd in each of the n periods, n And the corresponding time periods Δt1, Δt2, ....Δt n , can be obtained by The change of the growth rate of the epitaxial film in each cycle was calculated.
[0140] In some embodiments, the corresponding optical thickness increment may also be calculated based on adjacent real-time reflectivity trough values within a period.
[0141] The technical solution provided in the present application is particularly suitable for an online optical detection method for heteroepitaxial film growth, which can not only measure the growth rate and the change of optical thickness over time, but also evaluate the crystal characteristics of the epitaxial film. Under the guidance of the real-time detection data of the heteroepitaxial growth, the epitaxial process can be further adjusted to accurately control the growth parameters of the epitaxial layer, which is of great significance for manufacturing semiconductor devices with excellent performance.
[0142] The above embodiments are merely illustrative of the principles and effects of the present application and are not intended to limit the present application. Anyone familiar with the technology may modify or change the above embodiments without violating the spirit and scope of the present application. Therefore, all equivalent modifications or changes made by a person of ordinary skill in the art without departing from the spirit and technical ideas disclosed in the present application shall still be covered by the claims of the present application.
Claims
1. A method for detecting the growth state of an epitaxial film, characterized in that: At least the following steps are included: S0: Providing a semiconductor growth device, an optical detection device, and a main control device, wherein the semiconductor growth device carries a substrate, the optical detection device is disposed in the semiconductor growth device, and the main control device is in communication with the optical detection device. The main control device pre-stores data on a correspondence between crystal forms of semiconductor materials at different wavelengths and corresponding absorption coefficients, wherein the absorption coefficients are different. S1: controlling the semiconductor growth device to perform an epitaxial process on the substrate, so that an epitaxial film composed of the semiconductor material and having a composition material different from that of the substrate is formed on the exposed surface of the substrate; S2: During the epitaxial growth process, controlling the optical detection device to emit light within a specific wavelength range toward the epitaxial film for optical detection, and acquiring and sending light intensity information of the epitaxial film to the main control device; S3: The main control device performs calculations based on the light intensity information of the epitaxial film, the specific wavelength, and the crystal type correspondence data to obtain real-time crystal type information of the surface of the epitaxial film.
2. The epitaxial film growth state detection method according to claim 1, characterized in that: The main control device also pre-stores empirical reflectivity correspondence data with the reflectivity, thickness, phase difference, absorption coefficient and refractive index of the semiconductor material. In step S3, the main control device performs calculations based on the light intensity information, the specific wavelength and the crystal form correspondence data, including: S31: The main control device obtains real-time reflectivity correspondence data between the real-time reflectivity of the epitaxial film and the growth time according to the light intensity information of the epitaxial film; S32: The main control device calculates the real-time absorption coefficient of the epitaxial film based on the real-time reflectivity correspondence data and the empirical reflectivity correspondence data, and obtains the real-time crystal type information of the epitaxial film surface based on the real-time absorption coefficient, the specific wavelength and the crystal type correspondence data.
3. The epitaxial film growth state detection method according to claim 2, characterized in that: The empirical reflectivity correspondence data includes: in: R is the empirical reflectivity, n i is the refractive index of the reaction space medium above the epitaxial film, n j is the refractive index of the semiconductor material, n k is the refractive index of the substrate material, a is the absorption coefficient of a specific crystal plane of the semiconductor material at the specific wavelength, γ is the phase difference, d is the optical thickness of the epitaxial film; λ is the specific wavelength, i is the incident angle of the light in the specific wavelength range from the reaction space medium to the epitaxial film, j is the refraction angle of the outgoing light emitted from the bottom surface of the epitaxial film, and k is the refraction angle of the outgoing light emitted from the bottom surface of the substrate.
4. The epitaxial film growth state detection method according to claim 2, characterized in that: The real-time reflectivity correspondence data is periodic oscillation curve data of the real-time reflectivity and growth time of the epitaxial film.
5. The epitaxial film growth state detection method according to claim 4, characterized in that: The real-time reflectivity of the epitaxial film shows a decaying trend as the growth time increases.
6. The epitaxial film growth state detection method according to claim 5, characterized in that: Before executing step S1, the method further includes executing the step of obtaining the specific wavelength: Obtaining single crystal samples of different crystal forms of the semiconductor material; Performing optical testing and analysis on each of the single crystal samples under light of different wavelength ranges to obtain absorption spectrum group data; Obtaining the wavelength corresponding to the maximum absorption coefficient of each single crystal sample in the absorption spectrum data to form a wavelength data group, and obtaining the crystal form corresponding relationship data; Any wavelength in the wavelength data set is selected as the specific wavelength.
7. The epitaxial film growth state detection method according to claim 6, characterized in that: The steps of obtaining single crystal samples of different crystal forms of the semiconductor material include: Obtaining a single crystal sample of the semiconductor material to be cut; The single crystal samples to be cut are subjected to crystal plane cutting to form the single crystal samples.
8. The epitaxial film growth state detection method according to claim 1, characterized in that: The semiconductor growth equipment includes a carrying device for carrying the substrate; The process of executing the step S1 includes controlling the carrying device to drive the substrate to rotate; The process of executing step S2 further includes controlling the optical detection device to emit light in the specific wavelength range toward the carrier device to obtain and send the received light intensity information of the carrier device to the main control device; In step S3, the main control device performs subtraction processing based on the light intensity information of the epitaxial film and the light intensity information of the carrier to deduct background information including thermal radiation information, and then performs calculation based on the obtained light intensity information, the specific wavelength and the crystal form correspondence data.
9. The epitaxial film growth state detection method according to claim 2, characterized in that: After step S32 is completed, the following steps are further performed: S33: The main control device calculates the real-time optical thickness increment of the epitaxial film according to the empirical reflectivity correspondence data, the real-time reflectivity correspondence data, and the real-time crystal type information; S34: The main control device obtains the growth rate change data of the epitaxial film according to the real-time optical thickness increment.
10. The epitaxial film growth state detection method according to claim 9, characterized in that: The step S33 includes: S331: The main control device obtains the real-time reflectivity value in the ith period of the periodic oscillation curve, the empirical reflectivity correspondence value and the real-time crystal type information at Δt i The real-time optical thickness increment Δd of the epitaxial film within the time period i ; S332: The main control device obtains the reflectivity value in the (i+n)th period of the periodic oscillation curve, the empirical reflectivity correspondence value and the real-time crystal type information. (i+n) The real-time optical thickness increment Δd of the epitaxial film within the time period (i+n) ; S333: Repeat step S332 until the epitaxial process is completed or until the condition is satisfied. in: i is a positive integer greater than or equal to 1, n is a positive integer greater than or equal to 1 and is taken sequentially.
11. The epitaxial film growth state detection method according to claim 1, characterized in that: The energy of the light in the specific wavelength range is greater than the band gap width of the semiconductor material.
12. The epitaxial film growth state detection method according to claim 1, characterized in that: The epitaxial film is an epitaxial doped film.
13. A detection system, characterized in that: For executing the epitaxial film growth state detection method according to any one of claims 1 to 12, the detection system comprises an optical detection device for being arranged in a semiconductor growth device, and A main control device is communicatively connected to the optical detection device, and the semiconductor growth equipment is configured to perform an epitaxial process on a substrate to form an epitaxial film whose composition material is different from that of the substrate.
Citation Information
Patent Citations
Microwave plasma chemical vapor deposition equipment capable of realizing on-line / in-situ monitoring
CN111349914A
Crystal orientation testing device and method for two-dimensional material
CN113884471A
Method of calculating and determining composition of oxide single crystal
JP2001322896A
Cited By
Method and system for optimizing process environment in epitaxial growth reaction cavity
CN121093859A
Method for optimizing process environment in epitaxial growth reaction chamber and system thereof
CN121093859B
Epitaxial film growth state detection method, and detection system
WO2026012110A1