A method for synthesizing an antioxidant 1330
By using SO42-/ZrO2-MWCNT solid acid catalyst, the problems of large liquid acid usage and easy catalyst loss were solved, achieving efficient and environmentally friendly preparation of antioxidant 1330, and improving catalyst stability and product purity.
Patent Information
- Application Number
- CN202610342309.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-03-19
- Publication Date
- 2026-06-23
AI Technical Summary
In existing methods for preparing antioxidant 1330, a large amount of liquid acid is used, resulting in serious environmental pollution. Furthermore, the active components of the catalyst are easily lost, the catalyst life is short, it is difficult to reuse the catalyst multiple times, the product yield is low, and the purity is insufficient.
Using SO42-/ZrO2-MWCNT as a solid acid catalyst, antioxidant 1330 was obtained by ultrasonic mixing and low-temperature dropwise addition in the reaction of 3,5-di-tert-butyl-4-hydroxybenzylmethyl ether and mesitylene, followed by purification. The catalyst is easy to separate and recover, and maintains high activity.
It achieves highly efficient catalytic synthesis of antioxidant 1330, reduces environmental pollution, has good catalyst stability, can be reused multiple times, and produces products with high purity and good color, suitable for a variety of polymers and organic materials.
Smart Images

Figure CN122254975A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of synthetic technology, and more specifically, relates to a method for synthesizing the antioxidant 1,3,5-trimethyl-2,4,6-tris(3,5-di-tert-butyl-4-hydroxybenzyl)benzene. Background Technology
[0002] Antioxidants are a general term for a large class of compounds that have anti-aging and antioxidant effects. Adding a small amount to polymer materials can delay or inhibit the aging process of the materials, thereby extending the service life of the polymer materials.
[0003] Currently, there is a wide variety of antioxidants, mainly including hindered phenols, phosphites, thioethers, compound antioxidants, a small amount of metal ion passivators, and some amine oxidants.
[0004] Antioxidant 1330, chemically named 1,3,5-trimethyl-2,4,6-tris(3,5-di-tert-butyl-4-hydroxybenzyl)benzene, is a hindered phenolic antioxidant with special properties. It is suitable for the antioxidant stability of various polymers and organic materials, especially exhibiting good synergistic effects with auxiliary antioxidants such as phosphorus antioxidants, thioesters, and carbon radical scavengers. It is particularly suitable for high-temperature processing and applications requiring high resistance to extraction. Furthermore, due to its non-toxicity, non-polluting nature, and ability to maintain the good color of plastics, it can be used in food packaging. Compared with traditional antioxidants, it is highly efficient, low in toxicity, and non-polluting, making Antioxidant 1330 applicable to a wide range of fields.
[0005] In existing preparation methods, US Patent 3026264A uses concentrated sulfuric acid as a catalyst and 2,6-di-tert-butyl-4-hydroxybenzyl alcohol and mesitylene as raw materials to prepare antioxidant 1330. This method uses a large amount of sulfuric acid, which easily generates a large amount of waste acid. Moreover, the raw material benzyl alcohol is not easy to obtain, and the yield is not high while easily polluting the environment.
[0006] US patents US4754007 and US5292669 describe the synthesis of antioxidant 1330 from mesitylene and 3,5-di-tert-butyl-4-hydroxybenzyl methyl ether using sulfuric acid and methanesulfonic acid as catalysts. However, the yield of this method is still low, the amount of acid used is large, and methanesulfonic acid is expensive, making it unsuitable for production.
[0007] Chinese patent CN201510121181.8 uses a mixture of trifluoromethanesulfonate, 3,4,7,8-tetramethyl-1,10-o-phenanthroline, and CdI-2 as a ternary composite catalyst to prepare antioxidant 1330 using 1,3,5-trichloromethyl-2,4,6-trimethylbenzene and 2,6-di-tert-butylphenol as raw materials. However, the raw material 1,3,5-trichloromethyl-2,4,6-trimethylbenzene used in this method is not easy to obtain, and the synthesis of this raw material also requires a large amount of acid. Although the solid acid catalyst used in this method has good initial catalytic activity, its reactive components are easily lost during the reaction, resulting in a short catalyst life and making it unsuitable for repeated use.
[0008] Chinese patent CN101717326 describes the preparation of antioxidant 1330 using a solid superacid catalyst from 1,3,5-trihalomethyl-2,4,6-trimethylbenzene and 2,6-di-tert-butylphenol. This method is characterized by easy separation, non-corrosiveness to equipment, and simple post-processing. However, the active component SO4 in the solid superacid catalyst used... 2- It is easily lost during the reaction, resulting in a short catalyst life. Summary of the Invention
[0009] To address the aforementioned technical problems, this invention provides a method for synthesizing antioxidant 1330 (1,3,5-trimethyl-2,4,6-tris(3,5-di-tert-butyl-4-hydroxybenzyl)benzene), using 3,5-di-tert-butyl-4-hydroxybenzyl methyl ether and mesitylene as raw materials, under a solid acid catalyst SO4. 2- Antioxidant 1330 was synthesized under the conditions of / ZrO2-MWCNT.
[0010] To achieve the above objectives, the present invention adopts the following technical solution:
[0011] A method for synthesizing antioxidant 1330, the method comprising the following steps:
[0012] Step 1: Add catalyst SO4 2- / ZrO2-MWCNT and mesitylene were added to a solvent and mixed thoroughly to obtain solution A;
[0013] Step 2: Dissolve 3,5-di-tert-butyl-4-hydroxybenzyl methyl ether in dichloromethane and mix thoroughly to obtain solution B;
[0014] Step 3: Add solution B prepared in step 2 dropwise to solution A at 3-8℃, and stir the reaction at 3-8℃ for 2-4 hours to obtain a solid-liquid mixture;
[0015] Step 4: After filtering the solid-liquid mixture obtained in Step 3, collect the solid catalyst and the filtrate separately;
[0016] Step 5: Evaporate the filtrate collected in Step 4 to obtain crude 1330, and purify it to obtain antioxidant 1330 product;
[0017] Among them: SO4 2- The mass ratio of ZrO2-MWCNT to mesitylene is 1:4-8;
[0018] The molar ratio of the mesitylene and 3,5-di-tert-butyl-4-hydroxybenzyl methyl ether is 1:3.2-3.6.
[0019] In the further synthesis method of the antioxidant 1330 described above, the solvent in step one is dichloromethane.
[0020] Furthermore, in the above-mentioned method for synthesizing antioxidant 1330, the mixing in step one is performed using ultrasonic mixing.
[0021] Further, in the above-mentioned method for synthesizing antioxidant 1330, the purification step five involves adding n-heptane to the crude 1330 product, heating and dissolving it, recrystallizing it at 5°C, and then filtering, washing, and drying it to obtain the antioxidant 1330 product.
[0022] Further, in the above-mentioned method for synthesizing antioxidant 1330, the washing in step five is performed by rinsing with n-heptane at 5°C; the drying is performed by vacuum drying at 60°C for 30-90 minutes.
[0023] Further, in the above-mentioned method for synthesizing antioxidant 1330, the catalyst SO4 2- The preparation method of / ZrO2-MWCNT includes the following steps:
[0024] (1) Add sodium hydroxide solution to multi-walled carbon nanotubes and sonicate for 1-3 hours, then wash until the eluent is neutral and dry.
[0025] (2) Add the multi-walled carbon nanotubes from (1) to an aqueous solution of zirconium oxychloride, adjust the pH to 8, continue stirring for 10-60 minutes, then let stand for 8-15 hours, then filter, wash the obtained colloid with deionized water until neutral and dry.
[0026] (3) Grind the solid obtained in (2) into powder and soak it in sulfuric acid solution for 6-12 hours. After soaking, filter, wash and dry the powder. Then put it into a muffle furnace and calcine it at 500-650℃ for 1-5 hours to obtain solid acid catalyst SO4. 2- / ZrO2-MWCNT.
[0027] The mass ratio of the multi-walled carbon nanotubes to zirconium oxychloride octahydrate is 1:0.5-0.8;
[0028] Furthermore, in the above-mentioned method for synthesizing antioxidant 1330, the concentration of the sodium hydroxide solution is 1 mol / L.
[0029] Furthermore, in the above-mentioned method for synthesizing antioxidant 1330, the concentration of the zirconium oxychloride aqueous solution is 0.06-0.1 mol / L.
[0030] Furthermore, in the above-mentioned method for synthesizing antioxidant 1330, the concentration of the sulfuric acid solution is 2 mol / L.
[0031] Furthermore, in the above-mentioned method for synthesizing antioxidant 1330, step (2) involves adjusting the pH using ammonia.
[0032] Compared with existing technologies for preparing antioxidant 1330, the present invention has the following advantages:
[0033] 1. This invention provides a technical solution for preparing SO4. 2- The ZrO2-MWCNT solid acid catalyst features a large specific surface area, high stability, a large number of strong acid centers, and low solubility in solvents. It can effectively catalyze the synthesis of antioxidant 1330, and the active components are not easily lost. It can be recovered and reused while still having good catalytic ability, and can be reused multiple times.
[0034] 2. The method for synthesizing antioxidant 1330 provided by this invention uses SO4. 2- / ZrO2-MWCNT replaces liquid acid catalysts, effectively overcoming the problems of large liquid acid consumption and the inability to recycle, resulting in a large amount of waste acid in existing technologies; reducing environmental pollution.
[0035] 3. The method for synthesizing antioxidant 1330 provided by this invention uses SO4. 2- The ZrO2-MWCNT solid acid catalyst is easy to separate from the system, thus ensuring high purity of the prepared product and avoiding dark color, which is beneficial for its use as an additive in various fields. Attached Figure Description
[0036] Figure 1 This is the 1330 Fourier transform infrared spectrum of antioxidant 1 prepared in Example 1;
[0037] Figure 2 This is the 1H NMR spectrum of antioxidant 1330 prepared in Example 1;
[0038] Figure 3 This is the liquid chromatogram of antioxidant 1330 prepared in Example 1. Detailed Implementation
[0039] The present invention will be further described below with reference to specific embodiments, but the implementation of the present invention is not limited thereto.
[0040] The multi-walled carbon nanotubes were purchased from Shanghai McLean Biochemical Technology Co., Ltd., model number C742308.
[0041] Example 1
[0042] This embodiment provides a method for synthesizing antioxidant 1330, which includes the following steps in sequence:
[0043] 1) Take 0.2g SO4 2- A solution A is obtained by mixing ZrO2-MWCNT solid acid catalyst, 1.2g mesitylene, and 5g dichloromethane and sonicating at 300W for 5 minutes. 8.75g of 3,5-di-tert-butyl-4-hydroxybenzyl methyl ether is dissolved in 26g dichloromethane to obtain solution B.
[0044] 2) Add solution B dropwise to homogeneous solution A at 3℃, completing the addition in half an hour. Continue the reaction for 3 hours. After the reaction is complete, filter the reaction system and collect the filter residue (solid catalyst) for recycling. Heat the filtrate to 80℃ until the dichloromethane is completely evaporated to obtain crude solid 1330.
[0045] 3) Then, n-heptane was added to the crude 1330 solid, and the mixture was heated to 80°C until the solid was completely dissolved. The solid was then crystallized at 5°C for 1 hour. Finally, the mixture was filtered and dried under vacuum at 60°C for 1 hour to obtain antioxidant 1330 as a white solid, with a yield of 86.41%.
[0046] The catalyst used in this embodiment is SO4. 2- / ZrO2-MWCNT powder is prepared by the following steps:
[0047] 4g of multi-walled carbon nanotubes were added to a beaker containing 200mL of 1mol / L sodium hydroxide solution and ultrasonically treated for 2h. The mixture was then washed with a large amount of deionized water until the eluent was neutral. The sodium hydroxide-treated multi-walled carbon nanotubes were mixed with 100mL of 0.08mol / L zirconium oxychloride aqueous solution, and ammonia was added dropwise while stirring to adjust the pH to 8. Stirring was continued for 30 minutes, followed by standing for 12h. After standing, the mixture was filtered and washed with deionized water until the washings were neutral. The powder was dried at 90℃ for 6h, and then soaked in 50mL of 2mol / L sulfuric acid solution for 10h. Finally, it was calcined at 550℃ for 3h to obtain SO4. 2- / ZrO2-MWCNT powder.
[0048] The Fourier transform infrared spectrum of the antioxidant 1330 prepared in this embodiment is shown in the reference document. Figure 1 ,pass Figure 1 It can be seen that 3647cm -1 3614cm -1 The point is the stretching vibration of OH; 3066 cm -1 2997cm -1 The stretching vibration of CH on the benzene ring is located at 2872 cm⁻¹. -1 The vibration is -CH2- symmetric stretching vibration at 1394 cm. -1 1362cm -1 The absorption peak at 1230 cm⁻¹ is due to in-plane bending vibration of the tert-butyl finite; -1 The point is a CO stretching vibration; 870cm -1 The position represents a 1, 2, 3, 5 tetrasubstituted rocking vibration of the benzene ring skeleton.
[0049] The 1H NMR spectrum of antioxidant 1330 prepared in this embodiment is shown in the attached image. Figure 2 ,pass Figure 2 The NMR characterization of the product (500MHz, CDCl3) shows the following peaks: δ=6.89, a single peak with an area representing 6 H atoms (the three H atoms on the benzene ring of 2,6-di-tert-butylphenol); δ=4.98, a single peak with an integrated area representing 3 H atoms (the three phenolic hydroxyl groups, i.e., 3-OH); δ=4.05, a single peak with an integrated area representing 6 H atoms (the three methylene groups, i.e., 3-CH2); δ=2.27, a single peak with an integrated area ratio representing 9 H atoms (the three methyl groups on mesitylene, i.e., 3-CH3); and δ=1.34, a single peak with an integrated area ratio representing 54 H atoms (the H atoms on the tert-butyl group, i.e., 6-C(CH3)3). Therefore, the product can be identified as antioxidant 1330.
[0050] The liquid chromatogram of antioxidant 1330 prepared in this embodiment is shown in the figure. Figure 3 ,pass Figure 3 It can be seen that the product eluted at 10.5 min and had virtually no impurities, indicating high product purity.
[0051] Examples 2-6
[0052] Examples 2 to 6 are basically the same as Example 1 in terms of operation steps and parameters, the only difference being the SO4 used. 2- The ZrO2-MWCNT solid acid catalyst was recovered sequentially in each example and applied directly without treatment to obtain antioxidant 1330 white crystals, as detailed in Table 1.
[0053] Table 1
[0054] Example catalyst Yield % Example 2 <![CDATA[SO4 recovered in Example 1 2- / ZrO2-MWCNT solid acid catalyst]]> 86.21 Example 3 <![CDATA[SO4 recovered in Example 2 2- / ZrO2-MWCNT solid acid catalyst]]> 83.45 Example 4 <![CDATA[SO4 recovered in Example 3 2- / ZrO2-MWCNT solid acid catalyst]]> 82.39 Example 5 <![CDATA[SO4 recovered in Example 4 2- / ZrO2-MWCNT solid acid catalyst]]> 81.95 Example 6 <![CDATA[SO4 recovered in Example 5 2- / ZrO2-MWCNT solid acid catalyst]]> 80.74
[0055] Example 7
[0056] This embodiment provides a method for synthesizing antioxidant 1330, which includes the following steps in sequence:
[0057] 1) Take 0.2g SO4 2- A solution A is obtained by mixing ZrO2-MWCNT solid acid catalyst, 1.2g mesitylene, and 5g dichloromethane and ultrasonicating for 5 minutes at 300W to obtain homogeneous solution A; 8g of 3,5-di-tert-butyl-4-hydroxybenzyl methyl ether is dissolved in 26g dichloromethane to obtain solution B.
[0058] 2) Add solution B dropwise to homogeneous solution A at 8℃, completing the addition in half an hour. Continue the reaction for 3 hours. After the reaction is complete, filter the reaction system and collect the filter residue (solid catalyst) for recycling. Heat the filtrate to 80℃ until the dichloromethane is completely evaporated to obtain crude solid 1330.
[0059] 3) Then, n-heptane was added to the crude 1330 solid, and the mixture was heated to 80°C until the solid was completely dissolved. The solid was then crystallized at 5°C for 1 hour. Finally, the mixture was filtered and dried under vacuum at 60°C for 1 hour to obtain antioxidant 1330 as a white solid, with a yield of 81.73%.
[0060] The catalyst used in this embodiment is SO4. 2- / ZrO2-MWCNT powder is prepared by the following steps:
[0061] 4g of multi-walled carbon nanotubes were added to a beaker containing 200mL of 1mol / L sodium hydroxide solution and ultrasonically treated for 2h. The nanotubes were then washed with a large amount of deionized water until the eluent was neutral. The sodium hydroxide-treated nanotubes were mixed with 100mL of 0.06mol / L zirconium oxychloride aqueous solution, and ammonia was added dropwise while stirring to adjust the pH to 8. Stirring was continued for 30 minutes, followed by standing for 12h. After standing, the nanotubes were filtered, washed, and dried. They were then soaked in 50mL of 2mol / L sulfuric acid solution for 6h, and finally calcined at 500℃ for 2h to obtain SO4. 2- / ZrO2-MWCNT powder.
[0062] Example 8
[0063] This embodiment provides a method for synthesizing antioxidant 1330, which includes the following steps in sequence:
[0064] 1) Take 0.3g SO4 2- ZrO2-MWCNT solid acid catalyst, 1.2g mesitylene and 5g dichloromethane were mixed and sonicated at 300W for 5 minutes to obtain solution A; 8.75g of 3,5-di-tert-butyl-4-hydroxybenzyl methyl ether was dissolved in 26g dichloromethane to obtain solution B;
[0065] 2) Add solution B dropwise to homogeneous solution A at 8℃, completing the addition in half an hour. Continue the reaction for 4 hours. After the reaction is complete, filter the reaction system and collect the filter residue (solid catalyst) for recycling. Heat the filtrate to 80℃ until the dichloromethane is completely evaporated to obtain crude solid 1330.
[0066] 3) Then, n-heptane was added to the crude 1330 solid, and the mixture was heated to 80°C until the solid was completely dissolved. The solid was then crystallized at 5°C for 1 hour. Finally, the mixture was filtered and dried under vacuum at 60°C for 1 hour to obtain antioxidant 1330 as a white solid, with a yield of 83.92%.
[0067] The catalyst used in this embodiment is SO4. 2- / ZrO2-MWCNT powder is prepared by the following steps:
[0068] 4g of multi-walled carbon nanotubes were added to a beaker containing 200mL of 1mol / L sodium hydroxide solution and ultrasonically treated for 2h. The mixture was then washed with a large amount of deionized water until the eluent was neutral. The sodium hydroxide-treated multi-walled carbon nanotubes were mixed with 100mL of 0.08mol / L zirconium oxychloride aqueous solution, and ammonia was added dropwise while stirring to adjust the pH to 8. Stirring was continued for 30 minutes, followed by standing for 12h. After standing, the mixture was filtered and washed with deionized water until the washings were neutral. The powder was dried at 90℃ for 6h, and then soaked in 50mL of 2mol / L sulfuric acid solution for 12h. Finally, the powder was calcined at 600℃ for 2h to obtain SO4. 2- / ZrO2-MWCNT powder.
[0069] Example 9
[0070] This embodiment provides a method for synthesizing antioxidant 1330, which includes the following steps in sequence:
[0071] 1) Take 0.15g SO4 2- ZrO2-MWCNT solid acid catalyst, 1.2g mesitylene and 5g dichloromethane were mixed and sonicated at 300W for 5 minutes to obtain solution A; 8g of 3,5-di-tert-butyl-4-hydroxybenzyl methyl ether was dissolved in 26g of dichloromethane and added to solution B.
[0072] 2) Add solution B dropwise to homogeneous solution A at 8℃, completing the addition in half an hour. Continue the reaction for 2 hours. After the reaction is complete, filter the reaction system and collect the filter residue (solid catalyst) for recycling. Heat the filtrate to 80℃ until the dichloromethane is completely evaporated to obtain crude solid 1330.
[0073] 3) Then, n-heptane was added to the crude 1330 solid, and the mixture was heated to 80°C until the solid was completely dissolved. Then, it was crystallized at 5°C for 1 hour. Finally, it was filtered and dried under vacuum at 60°C for 1 hour to obtain antioxidant 1330 white solid with a yield of 79.89%.
[0074] The catalyst used in this embodiment is SO4. 2- / ZrO2-MWCNT powder is prepared by the following steps:
[0075] 4g of multi-walled carbon nanotubes were added to a beaker containing 200mL of 1mol / L sodium hydroxide solution and ultrasonically treated for 2h. The mixture was then washed with a large amount of deionized water until the eluent was neutral. The sodium hydroxide-treated multi-walled carbon nanotubes were mixed with 100mL of 0.06mol / L zirconium oxychloride aqueous solution. Ammonia was added dropwise while stirring to adjust the pH to 8, and stirring continued for 30 minutes. The mixture was then allowed to stand for 12h. After standing, the mixture was filtered and washed with deionized water until the washings were neutral. The powder was dried at 90℃ for 6h, and then soaked in 50mL of 2mol / L sulfuric acid solution for 8h. Finally, it was calcined at 650℃ for 3h to obtain SO4. 2- / ZrO2-MWCNT powder.
[0076] Example 10
[0077] 1) Take 0.3g SO4 2- A solution A is obtained by mixing ZrO2-MWCNT solid acid catalyst, 1.2g mesitylene, and 5g dichloromethane and ultrasonicating for 5 minutes at 300W to obtain homogeneous solution; 9g of 3,5-di-tert-butyl-4-hydroxybenzyl methyl ether is dissolved in 26g dichloromethane to obtain solution B.
[0078] 2) Add solution B dropwise to homogeneous solution A at 3℃, completing the addition in half an hour. Continue the reaction for 4 hours. After the reaction is complete, filter the reaction system and collect the filter residue (solid catalyst) for recycling. Heat the filtrate to 80℃ until the dichloromethane is completely evaporated to obtain crude solid product 1330.
[0079] 3) Then, n-heptane was added to the crude 1330 solid, and the mixture was heated to 80°C until the solid was completely dissolved. Then, it was crystallized at 5°C for 1 hour. Finally, it was filtered and dried under vacuum at 60°C for 1 hour to obtain antioxidant 1330 white solid with a yield of 87.02%.
[0080] The catalyst used in this embodiment is SO4. 2- / ZrO2-MWCNT powder is prepared by the following steps:
[0081] 4g of multi-walled carbon nanotubes were added to a beaker containing 200mL of 1mol / L sodium hydroxide solution and ultrasonically treated for 2h. The mixture was then washed with a large amount of deionized water until the eluent was neutral. The sodium hydroxide-treated multi-walled carbon nanotubes were mixed with 100mL of 0.1mol / L zirconium oxychloride aqueous solution, and ammonia was added dropwise while stirring to adjust the pH to 8. Stirring was continued for 30 minutes, followed by standing for 12h. After standing, the mixture was filtered and washed with deionized water until the washings were neutral. The powder was dried at 90℃ for 6h, and then soaked in 50mL of 2mol / L sulfuric acid solution for 12h. Finally, it was calcined at 550℃ for 3h to obtain SO4. 2- / ZrO2-MWCNT powder.
[0082] Example 11
[0083] This embodiment provides a method for synthesizing antioxidant 1330, which includes the following steps in sequence:
[0084] 1) Take 0.3g SO4 2- A solution A is obtained by mixing ZrO2-MWCNT solid acid catalyst, 1.2g mesitylene, and 5g dichloromethane and sonicating at 300W for 5 minutes; 8.5g of 3,5-di-tert-butyl-4-hydroxybenzyl methyl ether is dissolved in 26g dichloromethane to obtain solution B.
[0085] 2) Add solution B dropwise to homogeneous solution A at 3℃, completing the addition in half an hour. Continue the reaction for 2 hours. After the reaction is complete, filter the reaction system and collect the filter residue (solid catalyst) for recycling. Heat the filtrate to 80℃ until the dichloromethane is completely evaporated to obtain crude solid product 1330.
[0086] 3) Then, n-heptane was added to the crude 1330 solid, and the mixture was heated to 80°C until the solid was completely dissolved. Then, it was crystallized at 5°C for 1 hour. Finally, it was filtered and dried under vacuum at 60°C for 1 hour to obtain antioxidant 1330 white solid, with a yield of 86.11%.
[0087] The catalyst used in this embodiment is SO4. 2- / ZrO2-MWCNT powder is prepared by the following steps:
[0088] 4g of multi-walled carbon nanotubes were added to a beaker containing 200mL of 1mol / L sodium hydroxide solution and ultrasonically treated for 2h. The mixture was then washed with a large amount of deionized water until the eluent was neutral. The sodium hydroxide-treated multi-walled carbon nanotubes were mixed with 100mL of 0.08mol / L zirconium oxychloride aqueous solution, and ammonia was added dropwise while stirring to adjust the pH to 8. Stirring was continued for 30 minutes, followed by standing for 12h. After standing, the mixture was filtered and washed with deionized water until the washings were neutral. The powder was dried at 90℃ for 6h, and then soaked in 50mL of 2mol / L sulfuric acid solution for 8h. Finally, it was calcined at 550℃ for 5h to obtain SO4. 2- / ZrO2-MWCNT powder.
[0089] Example 12
[0090] This embodiment provides a method for synthesizing antioxidant 1330, which includes the following steps in sequence:
[0091] 1) Take 0.24g SO4 2- ZrO2-MWCNT solid acid catalyst, 1.2g mesitylene and 5g dichloromethane were mixed and sonicated at 300W for 5 minutes to obtain solution A; 9g of 3,5-di-tert-butyl-4-hydroxybenzyl methyl ether was dissolved in 26g dichloromethane to obtain solution B;
[0092] 2) Add solution B dropwise to homogeneous solution A at 3℃, completing the addition in half an hour. Continue the reaction for 2 hours. After the reaction is complete, filter the reaction system and collect the filter residue (solid catalyst) for recycling. Heat the filtrate to 80℃ until the dichloromethane is completely evaporated to obtain crude solid product 1330.
[0093] 3) Then, n-heptane was added to the crude 1330 solid, and the mixture was heated to 80°C until the solid was completely dissolved. Then, it was crystallized at 5°C for 1 hour. Finally, it was filtered and dried under vacuum at 60°C for 1 hour to obtain antioxidant 1330 white solid with a yield of 84.94%.
[0094] The catalyst used in this embodiment is SO4. 2- / ZrO2-MWCNT powder is prepared by the following steps:
[0095] 4g of multi-walled carbon nanotubes were added to a beaker containing 200mL of 1mol / L sodium hydroxide solution and ultrasonically treated for 2h. The mixture was then washed with a large amount of deionized water until the eluent was neutral. The sodium hydroxide-treated multi-walled carbon nanotubes were mixed with 100mL of 0.06mol / L zirconium oxychloride aqueous solution, and ammonia was added dropwise while stirring to adjust the pH to 8. Stirring was continued for 30 minutes, followed by standing for 12h. After standing, the mixture was filtered and washed with deionized water until the washings were neutral. The powder was dried at 90℃ for 6h, and then soaked in 50mL of 2mol / L sulfuric acid solution for 6h. Finally, it was calcined at 550℃ for 4h to obtain SO4. 2- / ZrO2-MWCNT powder.
Claims
1. A method for synthesizing antioxidant 1330, characterized in that, The method includes the following steps: Step 1: Add catalyst SO4 2- / ZrO2-MWCNT and mesitylene were added to a solvent and mixed thoroughly to obtain solution A; Step 2: Dissolve 3,5-di-tert-butyl-4-hydroxybenzyl methyl ether in dichloromethane and mix thoroughly to obtain solution B; Step 3: Add solution B prepared in step 2 dropwise to solution A at 3-8℃, and stir the reaction at 3-8℃ for 2-4 hours to obtain a solid-liquid mixture; Step 4: After filtering the solid-liquid mixture obtained in Step 3, collect the solid catalyst and the filtrate separately; Step 5: Evaporate the filtrate collected in Step 4 to obtain crude 1330, and purify it to obtain antioxidant 1330 product; Among them: SO4 2- The mass ratio of ZrO2-MWCNT to mesitylene is 1:4-8; The molar ratio of the mesitylene and 3,5-di-tert-butyl-4-hydroxybenzyl methyl ether is 1:3.2-3.
6.
2. The method for synthesizing antioxidant 1330 according to claim 1, characterized in that, The solvent mentioned in step one is dichloromethane.
3. The method for synthesizing antioxidant 1330 according to claim 1, characterized in that, The homogenization process described in step one is achieved by ultrasonic mixing.
4. The method for synthesizing antioxidant 1330 according to claim 1, characterized in that, The purification process described in step five involves adding n-heptane to the crude 1330 product, heating to dissolve it, recrystallizing it at 5°C, and then filtering, washing, and drying to obtain the antioxidant 1330 product.
5. The method for synthesizing antioxidant 1330 according to claim 4, characterized in that, The washing described in step five involves rinsing with n-heptane at 5°C; the drying process involves vacuum drying at 60°C for 30-90 minutes.
6. The method for synthesizing antioxidant 1330 according to claim 1, characterized in that, The catalyst SO4 2- The preparation method of / ZrO2-MWCNT includes the following steps: (1) Add sodium hydroxide solution to multi-walled carbon nanotubes and sonicate for 1-3 hours, then wash until the eluent is neutral and dry. (2) Add the multi-walled carbon nanotubes from (1) to an aqueous solution of zirconium oxychloride, adjust the pH to 8, continue stirring for 10-60 minutes, then let stand for 8-15 hours, then filter, wash the obtained colloid with deionized water until neutral and dry. (3) Grind the solid obtained in (2) into powder and soak it in sulfuric acid solution for 6-12 hours. After soaking, filter, wash and dry the powder. Then put it into a muffle furnace and calcine it at 500-650℃ for 1-5 hours to obtain solid acid catalyst SO4. 2- / ZrO2-MWCNT; The mass ratio of the multi-walled carbon nanotubes to zirconium oxychloride octahydrate is 1:0.5-0.
8.
7. The method for synthesizing antioxidant 1330 according to claim 6, characterized in that, The concentration of the sodium hydroxide solution is 1 mol / L.
8. The method for synthesizing antioxidant 1330 according to claim 6, characterized in that, The concentration of the zirconium oxychloride aqueous solution is 0.06-0.1 mol / L.
9. The method for synthesizing antioxidant 1330 according to claim 6, characterized in that, The concentration of the sulfuric acid solution is 2 mol / L.
10. The method for synthesizing antioxidant 1330 according to claim 6, characterized in that, The pH adjustment in step (2) is done using ammonia.
Citation Information
Patent Citations
Synthesis method for hindered phenolic compound antioxidant 330
CN104788292A
Substituted benzenes
US3026264A
Copolymerization of ethylene
US4754007A
Agents for the detection of substrates with hydrolase activity
US5292669A