Urea derivatives and their use as curatives and curative accelerators for resin systems
Bisfunctional orthohydroxy aromatic urones address the challenges of storage stability and high Tg retention in epoxy resin systems, enabling low-temperature curing and controlled heat management for enhanced mechanical properties in composite materials.
Patent Information
- Application Number
- GB2020012669
- Authority / Receiving Office
- GB · GB
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-08-13
- Publication Date
- 2024-11-27
- Estimated Expiration
- 2040-08-13
AI Technical Summary
Current epoxy resin curatives fail to provide storage stability, low-temperature curing, and high glass transition temperature (Tg) retention, especially in thick composite materials used in aerospace and wind turbine applications, while also risking thermal degradation and stress in large-scale components.
Bisfunctional orthohydroxy aromatic urones are used as curatives or accelerators in epoxy resin formulations, allowing for lower temperature curing, improved Tg retention, and controlled heat generation, reducing the risk of thermal damage and enhancing mechanical properties.
The use of bisfunctional orthohydroxy aromatic urones enables epoxy resin systems to maintain high Tg values over time, even at elevated temperatures, and provides excellent storage stability and mechanical properties, suitable for large-scale composite materials without excessive heat generation.
Smart Images

Figure 00000001_0000 
Figure 00000001_0001 
Figure 00000002_0000
Abstract
Description
The present invention relates to derivatives of urea, their use as curatives or curative 5 accelerators for resin systems particularly epoxy resins, epoxy resin formulations containing the derivatives of urea and prepregs and moulded articles employing such epoxy resin formulations. Accordingly the invention provides urea based compounds, a curative system, a resin formulation, a cured resin, a use, a composite and a moulding material. 10 Adipic acid dihydrazide and isophthalic acid dihydrazide are known as curatives for epoxy resin formulations. It has been suggested that they may be used together with accelerators such as urea based materials as is disclosed in US Patents 4404356 and 4507445. However there remains a need for curatives, which enable the combination of storage stability of the resin formulation prior to cure, low temperature cure, fast cure to produce a cured resin having 15 a high glass transition temperature (Tg) and which also retains the Tg over a period of time particularly when subjected to moisture particularly at elevated temperatures. One object of the present invention is therefore to provide a curable epoxy resin composition having excellent storage stability, enhanced curing characteristics including low temperature and faster cure and which provides a cured product having excellent mechanical properties. 20 A curative is a compound which is adapted to initiate or advance a polymerisation reaction of a polymerisable resin. An accelerator is a compound which enhances the polymerisation reaction (or “curing”) caused by a curative. 25 The curing of epoxy resins is usually an exothermic reaction and it is important that the reaction is controlled to avoid excess temperatures that can degrade the epoxy material and can cause stress and deformation such as cracking in articles and components created from the epoxy containing formulation. There is however an ongoing need to increase the Tg of cured epoxy resins particularly to provide sufficient strength to the articles and components particularly 30 when the resins are being used in resin impregnated fibre reinforcements sometimes known as prepregs that are used to produce larger and larger articles and particularly thicker articles made from stacks of prepregs such as stacks of more than 40, sometimes more than 60 up to 80 prepregs especially in the production of components for the aerospace and wind turbine industries. A prepreg comprises a fibrous reinforcement impregnated with a curable resin 35 ready for curing within a mould or vacuum bag. To date a higher Tg has been obtained using higher curing temperatures and / or longer curing cycles and employing hardeners such as 30 08 24 dicyandiamide which require higher curing temperatures; however, this increases the risk of high temperature degradation of the resin. It has been proposed that the use of urones as curatives can enable higher Tgs to be obtained 5 using lower cure temperatures and shorter cure cycles. Derivatives of urea are known as is their use as curatives for epoxy resins and such derivatives are sometimes known as urones. United States Patent 4,404,356 relates to hydroxy phenyl ureas of formula r2 NHCON—R3 OH rm (R% 10 and to their use as accelerators for heat curing of epoxy resins and also to their use as primary curing agents for epoxy resins. 15 United States Patent 9,663,609 relates to the use of bis or multifunctional N,N’-(Dimethyl) urones and a method for curing epoxy resin compositions using such urones. The use of these materials is said to provide a method for the controlled curing of epoxy resins particularly for solid components having large layer thickness of epoxy resins to avoid internal stresses or other thermal damage in mouldings or components that are produced therefrom. The bis- or 20 multi-functional N,N’-(dimethyl) urones are of the general formula R-(NH-CO-N(CH3)2)n where R is a linear or branched aliphatic radical or an unsubstituted, halo substituted 25 and / or alkyl substituted aromatic radical and n is a number from 2 to 20. However, United States Patent 9,663,609 does not envisage that when R is an aromatic radical it can be hydroxy substituted. The use of the bis- or multifunctional orthohydroxy aromatic urones according to this invention as curatives or curative accelerators provides a 30 further improvement in the control of the curing of epoxy resins particularly in prepregs. We have now produced bisfunctional orthohydroxy aromatic urones and we have found that when used as curatives for epoxy resins, the resin can be cured at lower temperatures, such as an externally applied temperature from 80°C to 150°C to produce a cured epoxy resin 5 having a higher Tg at complete cure than is produced from the non-hydroxy substituted aromatic bisfunctional urones such as those described in United States Patent 9,663,609. The urones of this invention may also be used as accelerators for other epoxy curatives when the curing temperature may be higher for example up to 180°C. 10 In one embodiment the invention therefore provides the use of bisfunctional and multifunctional orthohydroxy aromatic urones, as a curative for epoxy resins, their use as accelerators for other curatives for epoxy resins, epoxy resin formulations containing the bisfunctional and multifunctional orthohydroxy nurones, the use of such formulations as a resin matrix for reinforcing fibres particularly in prepregs and fibre reinforced materials made 15 therefrom. 30 08 24 The invention therefore provides a resin formulation comprising one or more bis orthohydroxy aromatic urones of the formulae selected from 20 Where Ri = S, SO2, SO, P, PX, N, NH, NX, P=O(OX or OH), C=O, a linear or branched aliphatic radical (substituted or unsubstituted), or an unsubstituted, halo substituted and / or 25 alkyl substituted aromatic radical and n is a number from 2 to 20. 30 08 24 Where X = a linear or branched aliphatic radical (substituted or unsubstituted), or an unsubstituted, halo substituted and / or alkyl substituted aromatic radical R2 and R3— at each occurrence, independently of one another, selected from an alkyl, 5 cycloalkyl, alkenyl, cycloalkenyl, or aralkyl group, which may be substituted by a halogen atom (preferably a chlorine atom) or by a hydroxyl or cyano group, with the proviso that R may alternatively denote a hydrogen atom, or R2 and R3 together with the indicated attached nitrogen atom denote a heterocyclic ring containing 3 to 5 carbon atoms, and optionally one oxygen atom. 10 R4 = at each occurrence, independently of one or another, is selected from H, NH2, NO2, nitrile, a halogen, linear or branched aliphatic radical, or an unsubstituted, halo substituted and / or alkyl substituted aromatic radical, and Y = 1 to 3 and at least one resin component selected from an epoxy, a polyisocyanate and a phenolic resin. 15 The compounds used in this invention may be used as curatives or accelerators for other curatives or they can perform both of these functions particularly with epoxy resins and the invention also provides an epoxy resin formulation containing one or more of the compounds of this invention optionally together with one or more other curatives. 20 Where the urea derivatives of this invention are used as the primary or sole curative for the resin we prefer to use from 2 to 20 wt % of the urea derivative based on the weight of the resin more preferably 5 to 15 wt %. 25 The use of the urea derivatives according to this invention as primary or sole curatives in thermosetting resin systems has produced a material which can be stored for several weeks without significant cure (known as the outlife of the system) and which produces a cured resin having a desirable Tg for applications such as prepregs used to make components for the aerospace and wind energy industries particularly when the components are thick and made 30 from a stack of several layers of the prepreg. Typically, at least 40 layers and sometimes 60 or more layers. The use of the curative also allows improved control of the heat generated during the curing reaction to avoid the risk of reaction run away which can cause degradation of the resin and damage to the cured article. 35 The compounds according to this invention may also be used as accelerators for other curatives for epoxy resins. Examples of curative whose performance can be accelerated by 30 08 24 the compounds of this invention are primary or secondary amines. The amines may be aliphatic, cycloaliphatic, aromatic, or aromatic structures having one or more amino moieties. Exemplary amine curing agents include ethylenediamine, diethylenediamine, 5 diethylenetriamine, triethylenetetramine, propylene diamine, tetraethylenepentamine, hexaethyleneheptamine, hexamethylenediamine, cyanoguanidine, 2-methyl-1,5-pentamethylene-diamine, 4,7,10-trioxatridecan-1,13-diamine, aminoethylpiperazine, and the like. Exemplary curing agents include dicyanopolyamides, most preferably (DICY). 4,4’-diaminodiphenyl sulfone (4,4’-DDS) or 3,3’-diaminodiphenyl sulfone (3,3’-DDS) can also be 10 beneficially employed as a latent amine curing agent, as well as mixtures of DICY and DDS. Dyhadrazides such and ADH, IDH and polyamines such as Ancamine (RTM) 2441 and BF3-MEA complexes such as Anchor (RTM) 1040 (Air Products) are also suitable as a latent curing agent. 15 In some embodiments, the amine curing agent is a polyether amine having one or more amine moieties, including those polyether amines that can be derived from polypropylene oxide or polyethylene oxide. Commercially available polyether amines include the polyether polyamines (available under the trade designation “JEFFAMINE” (RTM) from Huntsman Corporation and 4,7, 10-trioaxatridencane- 1,13- diamine (TTD) (available from BASF). A 20 preferred latent amine curing agent is Dyhard (RTM) 100E from AlzChem. Preferred other curatives are amino sulfones such as 4,4 diaminodiphenyl sulfone (sometimes known as 4,4-DDS) and 3,3 diaminodiphenyl sulfone (sometimes known as 3,3-DDS) which are typically used as curatives in resin formulations used in the production of aerospace 25 components. When the compounds according to this invention are used as accelerators for other curatives a smaller amount based on the weight of epoxy resin may be used than when the compound is the primary or sole curative. For this use we prefer to use from 0.1 to 1.5 wt % more 30 preferably 0.2 to 1 wt % based on the weight of epoxy resin. The resin formulation comprising the bisorthohydroxy aromatic urone in combination with at least one resin component such as an epoxy, polyisocyante and a phenolic resin particularly an epoxy resinis preferably in the form of a one-component resin formulation which does not 35 require any further mixing of components before its use. 30 08 24 In a further embodiment there is provided a resin formulation comprising a curable resin such as an epoxy, polyisocyante and a phenolic resin containing a curative other than a bisorthohydroxy aromatic urone of this invention together with a bisorthohydroxy aromatic urone of this invention which acts as an accelerator for the curative. 5 In a further embodiment the invention provides the use of a resin formulation of this invention as a matrix in fibre reinforced composites which may be a prepreg or may be obtained by resin infusion of dry fibrous material laid up in a mould with the resin formulation. The invention further provides a fibre reinforced composite obtained by the thermal curing of such a resin 10 matrix which can be accomplished in a press or in a vacuum bag. The cured Tg of a resin is measured in accordance with ASTM D7028 (Glass Transition Temperature (DMA Tg) of Polymer Matrix Composites by Dynamic Mechanical Analysis (DMA)). 15 The heat released during the curing reaction is related to the total heat for fully curing and can be measured using Digital Scanning Calorimetry as follows. A reference resin sample is heated from 10°C to 350°C. at 10°C / min rate to full cure (100%) and the generated heat AHi is recorded. The degree of cure of a particular resin sample of the same composition as the 20 reference resin sample can then be measured by curing the sample to the desired temperature and at the desired rate and for the desired time by heating the sample at these conditions and measuring the heat AHe generated by this cure reaction. The degree of cure (Cure %) is then defined by: 25 Cure %=[(AHi-AHe) / AHi]x100 [%] where AHi is the heat generated by the uncured resin heated from 10°C up to fully cured at 350°C. and AHe the heat generated by the certain degree cured resin heated up to a desired temperature and rate. 30 In another embodiment of the invention there is provided a moulding material comprising the thermosetting resin formulation of this invention in combination with a fibrous reinforcement material. The fibrous reinforcement material may be provided: as a woven fabric or a multi-axial fabric to form a prepreg, as individual fibre tows for impregnation with the resin composition to form towpregs, or as chopped fibres, short fibres or filaments to form a 35 moulding compound. The preferred fibrous material is selected from carbon fibre, glass fibre, aramid and mixtures thereof. The moulding material may be constructed from a cast resin film which contains the resin formulation and which is combined with a fibrous reinforcement 30 08 24 layer. Preferably the resin film impregnates the fibrous reinforcement which may be accomplished by pressing a layer of resin onto the fibrous material or by infusion of the resin into fibrous material within a mould. 5 Ina further embodiment of the invention there is provided an adhesive comprising a resin formulation of this invention in combination with at least one filler. The compositions of this invention are storage stable at ambient temperature prior to curing and are capable of fast curing at relatively low temperatures, such as 80°C to 150°C whilst the 10 Tg, the retained Tg and the mechanical properties of the cured resin enable use of the cured resin formulation in Industrial structural applications particularly as fibre reinforced materials which are useful as automotive and aerospace structural components as well as sporting goods and wind turbine components. 15 Where the resin is an epoxy resin it may be mono-functional or multifunctional, preferably at least difunctional. In an embodiment, the epoxy resin component (A) may be selected from various conventionally-known polyepoxy compounds. Examples thereof include: aromatic glycidyl ether compounds such as bis(4-hydroxyphenyl)propane diglycidyl ether, bis(4-hydroxy-3,5-dibromophenyl)propane diglycidyl ether, bis(4-hydroxyphenyl)ethane diglycidyl 20 ether, bis(4-hydroxyphenyl)methane diglycidyl ether, resorcinol diglycidyl ether, phloroglucinol triglycidyl ether, trihydroxy biphenyl triglycidyl ether, tetraglycidyl benzophenone, bisresorcinol tetraglycidyl ether, tetramethyl bisphenol A diglycidyl ether, bisphenol C diglycidyl ether, bisphenol hexafluoropropane diglycidyl ether, 1,3-bis[1-(2,3-epoxypropoxy)-1-trifluoromethyl-2,2,2-trifluoroethyl]benzene, 1,4-bis[1 -(2,3-epoxypropoxy)-1-trifluoromethyl-2,2,2- 25 trifluoromethyl]benzene, 4,4'-bis(2,3-epoxypropoxy)octafluorobiphenyl, and phenolic novolac type bisepoxy compounds; alicyclic polyepoxy compounds such as alicyclic diepoxy acetal, alicyclic diepoxy adipate, alicyclic diepoxy carboxylate, and vinylcyclohexene dioxide; glycidyl ester compounds such as diglycidyl phthalate, diglycidyl tetrahydrophthalate, diglycidyl hexahydrophthalate, dimethylglycidyl phthalate, dimethylglycidyl hexahydrophthalate, 30 diglycidyl-p-oxybenzoate, diglycidylcyclopentane-1,3-dicarboxylate, and dimer acid glycidyl ester; glycidyl amine compounds such as diglycidyl aniline, diglycidyl toluidine, triglycidyl aminophenol, tetraglycidyl diaminodiphenyl methane, and diglycidyl tribromoaniline; and heterocyclic epoxy compounds such as diglycidylhydantoin, glycidyl glycidoxyalkylhydantoin, and triglycidyl isocyanurate; and oligomer compounds thereof. 35 Examples of the liquid epoxy resin include polyalkylene ether type epoxy compounds such as (poly)ethylene glycol diglycidyl ether, (poly)propylene glycol diglycidyl ether, and 30 08 24 trimethylolpropane triglycidyl ether; glycidyl ester type epoxy compounds such as dimer acid diglycidyl ester, phthalic acid diglycidyl ester, and tetrahydrophtalic acid diglycidyl ester; and homopolymers of glycidyl (meth)acrylate, allyl glycidyl ether and the like or copolymers of these monomers with other soft unsaturated monomers. In this context, soft unsaturated 5 monomer refers to a monomer which contains a homopolymer which has a glass transition temperature of less than 60°C. Examples of soft unsaturated monomers include methyl acrylate, ethyl acrylate, butyl(meth)acrylate, isobutyl(meth)acrylate, 2-ethylhexyl(meth)acrylate, and lauryl methacrylate. 10 A liquid curable epoxy resin composition of the present invention is particularly useful as a one-component liquid epoxy resin prepreg matrix resin formulation which is excellent in both storage stability and curing characteristics and provides a cured product having excellent characteristics, particularly organic solvent resistance. 15 When the epoxy resin composition of the present invention is used as a prepreg resin formulation, known additives such as fillers, viscosity modifiers, tougheners, pigments, thixotropic agents, and fire retardants, or the like can be optionally mixed into the formulation to enhance its mechanical performance and flow behaviour during cure. 20 The compositions of this invention may include other typical additives used in thermosetting resin formulations such as impact modifiers, fillers, antioxidants and the like. The preferred urone of this invention is N,N’-[propylene(4-hydroxy-3,1-phenylene)]bis(N,N-dimethyl)urea. When used as the primary or sole curative for the resins the urones of this 25 invention are preferably present in the epoxy resin composition of the invention in an amount relative to the total weight to 2 to 20 wt % and more preferably 3 to 12 weight %, most preferably in an amount of the total weight of the composition with respect to 4 to 8 wt %. The bisfunctional orthohydroxy aromatic urones of this invention may be prepared from a 30 precursor obtained by the reaction of 2,2-bis(3-amino-4-hydroxyphenyl)propane and 1,1'-carbonyldiimidazole to produce the bisbenxozolinone precursor of formula This precursor may be reacted with dimethylamine to produce N,N’-[propylene(4-hydroxy-3,1-phenylene)]bis(N,N-dimethyl)urea of formula Hereinafter known as PBOHFLI. The bis- or multi-functional orthohydroxy aromatic urone used in this invention has the 10 structure represented by formulae 30 08 24 15 Where Ri = S, SO2, SO, P, PX, N, NH, NX, P=O(OX or OH), C=O, a linear or branched aliphatic radical (substituted or unsubstituted), or an unsubstituted, halo substituted and / or alkyl substituted aromatic radical and n is a number from 2 to 20. Where X = a linear or branched aliphatic radical (substituted or unsubstituted), or an 20 unsubstituted, halo substituted and / or alkyl substituted aromatic radical R2 and R3 = at each occurrence, independently of one another, selected from an alkyl, cycloalkyl, alkenyl, cycloalkenyl, or aralkyl group, which may be substituted by a halogen atom 30 08 24 (preferably a chlorine atom) or by a hydroxyl or cyano group, with the proviso that R2 may alternatively denote a hydrogen atom, or R2 and R3 together with the indicated attached nitrogen atom denote a heterocyclic ring containing 3 to 5 carbon atoms, and optionally one oxygen atom, in the ring. 5 R4 = at each occurrence, independently of one or another, selected from H, NH2, NO2, nitrile, a halogen, linear or ranched aliphatic radical, or an unsubstituted, halo substituted and / or alkyl substituted aromatic radical, and Y = 1 to 3. 10 The functionality is determined solely by the number of urea substituents or radicals. Furthermore, a urea substituent or radical is a radical or substituent according to formula -(NH-CO-N(R)2) The radical Ri in compounds of formula (i) is a bridging unit selected from S, SO2, SO, P, 15 PX, N, NH, NX, P=O(OX or OH), C=O, a linear or branched aliphatic radical (substituted or unsubstituted), or an unsubstituted, halo substituted and / or alkyl substituted aromatic radical. Where X = a linear or branched aliphatic radical (substituted or unsubstituted), or an unsubstituted, halo substituted and / or alkyl substituted aromatic radical. 20 According to the present invention, n in formula (i) can denote a number from 2 to 20, that is to say compounds having from 2 to 20 urea radicals can be used according to the invention. Preferably n is an integer from 2 to 10 and more preferably n is an integer from 2 to 8, and yet more preferably n is 2 or 3. Accordingly, there can be used according to the present invention in particular diurones, triurones or oligourones of the general formula (i), or mixtures thereof, 25 having two, three or up to 20 dimethylurea radicals. Particular preference is given to diurones where n=2 and triurones where n=3. Moreover, preference is also given to oligourones where n=from 4 to 20, wherein n can be a number from 4 to 20. It is to be emphasised that the choice of the basic structure is of lesser importance. 30 In another embodiment of the invention as shown by the compounds of formulae (ii) and (iii) the bisfunctional orthohydroxy aromatic urone may comprise a single aromatic moiety to which are attached two urea substitutes having hydroxyl groups in the ortho position to the urea substituents. 35 It has been found according to the invention in particular that urones of the general formula can be used as the sole curing agents in epoxy resin compositions. Accordingly, in this 30 08 24 embodiment these epoxy resin compositions can be free of further curing agents, co-curing agents, curing accelerators and / or catalysts for the curing of epoxy resins. The amount of the compounds of this invention that is used in the resin formulation depends 5 upon the required function of the compound and depending upon whether it is used as the primary or sole curative or as an accelerator for another curative. The amount can range from 0.01 to 20 parts of the urone of this invention or mixtures thereof per 100 parts of resin, preferably from 0.1 to 15 parts, preferably from 1 to 15 parts and most particularly preferably from 2 to 15 parts per 100 parts of resin. Also preferred are amounts in which there are used, 10 per 100 parts of resin, from 1 to 12 parts, in particular from 2 to 12 parts, more preferably from 3 to 12 parts, particularly preferably from 4 to 12 parts and most particularly preferably from 5 to 12 parts of the urone of the invention. With these amounts it is possible according to the invention to generate, at a temperature of 15 from 60 to 180°C, a maximum heat flow in the epoxy resin composition of from 0.05 to 0.99 W / g (based on the mass of epoxy resin), so that the epoxy resin composition cures fully. We have found that the use of the compounds as primary curatives for epoxy resin compositions enables curing at a temperature of from 60 to 190°C in particular 60°C to 180°C, 20 in particular from 60 to 160°C and most particularly preferably from 60 to 150°C, and that the curing reaction is controlled so that the epoxy resin composition cures fully without the generation of excess heat that can damage the resin and articles made therefrom. Where the compounds are used as accelerators for other curatives the curing temperature may be at the higher end of the range such as from 150 to 190°C particularly 60°C to 180°C. 25 An epoxy resin composition is considered to be fully cured if the epoxy resin composition cures to the extent Of ^80% , preferably 230% , more preferably =35% , yet more preferably =38% , in particular ^99% and most preferably 100% . Accordingly, the epoxy groups in the cured epoxy resin composition have reacted to the extent of in particular ^80% , preferably 2$0% , 30 more preferably ^95% , yet more preferably =38% , in particular =39% and most preferably 100%. The compositions of this invention can contain other components conventionally used in epoxy resin formulations such as impact modifiers and fillers as set out below. 35 30 08 24 Impact modifiers The composition may comprise an impact modifier. Impact modifiers are widely used to improve the impact strength of cured resin compositions with the aim to compensate their inherent brittleness and crack propagation. Impact modifier may comprise rubber particles 5 such as CTBN rubbers (carboxyl-terminated butadiene-acrylonitrile) or core shell particles which contain a rubber or other elastomeric compound encased in a polymer shell. The advantage of core shell particles over rubber particles is that they have a controlled particle size of the rubber core for effective toughening and the grafted polymer shell ensures adhesion and compatibility with the epoxy resin composition. Examples of such core shell rubbers are 10 disclosed in EP0985692 and in WO 2014062531. Alternative impact modifiers may include methylacrylate based polymers, polyamides, acrylics, polyacrylates, acrylate copolymers, phenoxy based polymers, and polyethersulphones. 15 Fillers In addition the composition may comprise one or more fillers to enhance the flow properties of the composition. Suitable fillers may comprise talc, microballoons, flock, glass beads, silica, fumed silica, carbon black, fibres, filaments and recycled derivatives, and titanium dioxide. 20 A prepreg resin formulation of the present invention can be prepared by uniformly mixing the curative of the invention, the resin and other additives using a pot mill, a ball mill, a bead mill, a roll mill, a homogenizer, Supermill, Homodisper, a universal mixer, Banbury mixer, a kneader, or the like. 25 Since the prepreg resin formulation of the present invention can be a one-component type that has both high storage stability and excellent thermosetting properties, it can be suitably used for applications which require long term storage or storage in unconditioned facilities at room temperature. 30 The resin formulations of this invention are particularly useful as the curable matrix for the production of fibre reinforced articles such as in prepregs that are used for the production of components for wind turbines and components for the aerospace industry such as aircraft wings and fuselages. The formulations may also be used in the production of automobile 35 components and components used in shipping and in the production of sporting goods such as skis. 30 08 24 The invention is illustrated by the following Examples in which the following materials were used. 2,2-bis(3-amino-4-hydroxyphenyl)propane and 2,2-bis(3-amino-4-hydroxyphenyl), hexa-5 fluoro-propane were purchased from Tokyo chemicals Industry 3,3-diamino-4,4-dihydroxydipheynlsulfone (44-DDS) prepared as described in the literature 1,1-carbonyldiimidazole was supplied by Apollo Scientific Dyhard (RTM) UR500 (3,3’-(4-methyl-1,3-phenylene)bis(1,1-dimethylurea) purchased from Alzchem (see US patent 9,663,609) 10 U52 (4,4’ methylene diphenylene bis (N,N dimethylurea) from Emerald Performance Materials Company Orthohydroxyfenuron (OHFU) and N-(2-hydroxy-5-nitrophenyl)-N,N’-dimethylurea (5-NOHFU) were prepared as described in US4404356A MY721, a tetraglycidyldiaminodiphenylmethane epoxy resin, LY3581, a bisphenol F epoxy 15 resin, MY0610 an epoxy resin based on triglycidyl-m-aminophenol and 4,4’-diphenyldiaminosulphone from Huntsman Advanced Materials Bisphenol A epoxy, Epikote (RTM) 828 were obtained from Brenntag LY1556 an Araldite (RTM) Epoxy resin from Huntsman 5003P a polyethersulfone thermoplastic supplied by Sumitomo 20 polyamide particle supplied by Arkema All other reagents and solvents were supplied by Sigma-Aldrich The following test methods were used on the materials of the Examples. 25 Dynamic differential scanning calorimetry (DSC) was performed using a TA Q100 instrument to determine the uncured Tgs, of the resin and the onset and peak temperatures using a heating rate of 10°C / min, from -50 to 350°C. Dynamic DSC was also use to determine residual enthalpy in cured formulations for determination of % cure. 30 Isothermal differential scanning calorimetry (DSC) was performed using a DSC 1 from Mettler Toledo instruments to determine the time taken to reach the peak temperature reached during curing at various externally applied temperatures. Dynamic mechanical analysis (DMA) was performed using a Q800 instrument on cured resin 35 to determine glass transition temperatures at a heating rate of 5°C / min and at a frequency of 1 Hz, and at an amplitude of 30 pm. 30 08 24 Thermogravimetric analysis (TGA-DSC) was performed using a TGA / DSC 1 from Mettler Toledo to determine the melting point / decomposition temperature using a heating rate of 10°C / min, from 25 to 350°C in air. 5 Dynamic and Isothermal rheology was performed using a MCR92 from Anton Paar. Dynamic rheology was performed with a heating rate of 2°C / min. Outlifes were measured by monitoring the uncured Tg of the mixtures over time. The mixtures 10 were stored in a temperature controlled incubator set at 23°C. The following abbreviations are used. PBOHFLI - N,N’-[propylene(4-hydroxy3,1-phenylene)]bis(N,N-dimethyl)urea 15 FPBOHFU - N,N’-[hexafluoropropylene(4-hydroxy3,1-phenylene)]bis(N,N-dimethyl)urea SBOHFLI - N,N’-[sulfonyl(4-hydroxy-3,1-phenylene)]bis(N,N-dimethyl)urea DOHFLI - 3,3’-(4,6-dihydroxy-1,3-phenylene)bis(1,1-dimethylurea) OHFII - orthohydroxyfenuron 5-NOHFU - N-(2-hydroxy-5-nitrophenyl)-N,N’-dimethylurea 20 44-DDS 4,4-diaminodiphenyl sulfone The results of the tests employed in the Examples are shown in Figures 1 to 4 hereof. Example 1 The production of N,N’-[propylene(4-hydroxy3,1-phenylene)]bis(N,N-dimethyl)urea, PBOHFLI 25 The bisbenxoazolinone precursor of this formula was first prepared as follows to a 500 ml round bottom flask was added 25.2 g of 2,2-bis(3-amino-4-hydroxyphenyl)propane and 300 30 ml of dimethylacetamide. To the stirred solution was added 57.0 g of 1,1-carbonyldiimidazole portion-wise over 1 hour. The solution was heated to 60°C and stirred at this temperature for 6 hours before cooling to room temperature. The solution was then poured in to 1 litre of deionised water to precipitate to the product. To the mixture was added 4M hydrochloric acid until the solution had become slightly acidic. The precipitate was collected by vacuum filtration and washed with deionised water before drying in a vacuum oven at 60°C overnight to give 29.7 g of a white powder, 98.0 % yield, with a melting point of 278°C. 1H NMR (DMSO-d6): 5 (ppm) 11.45 (bs, 2H, NH); 7.17 (d, 2H, Ar H); 6.96 (dd, 2H, Ar H); 6.82 5 (d, 2H,ArH); 1.63 (s, 6H, CH3). The PBOHFU of formula 30 08 24 Was prepared from the precursor as follows to a 250 ml round bottom flask was added 29.7 g of 2,2-bis(3H-1,3-benzoxazol-2-one)propane precursor and 85 ml of 40 wt. % aqueous dimethylamine. The mixture was heated to 50°C and stirred at this temperature for a total of 15 hours before cooling to room temperature. During this time, 80 ml of deionised water was 15 added to dilute the solids content and aid stirring. The mixture was then transferred to a one neck round bottom flask and the excess dimethylamine removed on a rotary evaporator. The mixture was then acidified slightly using 4M hydrochloric acid. The precipitate was collected by filtration and washed with deionised water before drying in a vacuum oven at 60°C overnight to give 36.1 g of a white powder, 94.3 % yield, with a melting point of 189°C (dec.). The formula was confirmed by 1H NMR (DMSO-d6): 5 (ppm) 9.62 (s, 2H, OH); 7.88 (s, 2H, NH); 7.29 (d, 2H, Ar H); 6.74 (dd, 2H, Ar H); 6.70 (d, 2H, Ar H); 2.93 (s, 12H, NCH3); 1.53 (s, 6H, CCH3); 25 Example 2 Production of N,N-[hexafluoropropylene(4-hydroxy3,1-phenylene)]bis(N,N-dimethyl)urea, FPBOHFU The above benxoazolinone precursor was first prepared using 25.0 g of 2,2-bis(3-amino-4-hydroxyphenyl)hexafluoropropane, 175 ml of dimethylacetamide and 36.2 g of 1,1-carbonyldiimidazole in the same procedure set out in example 1 using a reaction time of 2.5 hours to give 26.2 g of a white powder, 91.8 % yield, with a melting point of 322°C. 5 1H NMR (Methanol-d4): 5 (ppm) 7.26 (d, 2H, Ar H); 7.15 (d, 2H, Ar H); 7.09 (s, 2H, Ar H). The urone was prepared using 26.2 g of 2,2-bis(3H-1,3-benzoxazol-2-one)hexafluoropropane, and 50 ml of 40 wt. % aqueous dimethylamine in the same procedure set out in example 1 10 using a reaction time of 2.5 hours to give 17.7 g of a white powder, 55.6 % yield, with a melting point of 202°C (dec.) to yield a product of the formula 30 08 24 15 as confirmed by 1H NMR (DMSO-d6): 5 (ppm) 10.29 (s, 2H, OH); 7.76 (s, 2H, NH); 7.72 (s, 2H, Ar H); 6.86 (d, 2H, Ar H); 6.81 (d, 2H, Ar H); 2.93 (s, 12H, NCH3); Example 3 Production of N,N’-fsulfonyl(4-hydroxy-3,1-phenylene)1bis(N,N-dimethyl)urea, SBOHFU 20 The benxoazolinone precursor was first prepared using 5.6 g of 3,3-diamino-4,4-dihydroxydipheynlsulfone, 50 ml of dimethylacetamide and 10.3 g of 1,1-carbonyldiimidazole in the same procedure set out in example 1 using a reaction time of 4 hours to give 6.2 g of a white powder, 91.2 % yield, with a melting point of >350 °C. 1H NMR (DMSO-d6): 5 (ppm) 12.13 (bs, 2H, NH); 7.74 (dd, 2H, Ar H); 7.57 (d, 2H, Ar H); 7.49 25 (d, 2H,ArH); The urone was prepared using 6.2 g of 2,2-bis(3H-1,3-benzoxazol-2-one)sulfone, and 15 ml of 40 wt. % aqueous dimethylamine in the same procedure set out in example 1 using a reaction time of 7 hours to give 6.2 g of a tan coloured powder, 79.5 % yield, with a melting 5 point of 220 °C (dec.). Example 4 Production of 3,3’-(4,6-dihydroxy-1,3-phenylene)bis(1,1-dimethylurea), DOHFLI 30 08 24 10 The bisbenxoazolinone precursor was first prepared. To a 500 ml round bottom flask was added 25.0 g of 4,6-diaminoresorcinol dihydrochloride and the flask placed under an inert atmosphere of nitrogen. 300 ml of dimethylacetamide was then added. To the stirred suspension was added 16.0 ml of triethylamine drop-wise followed by 63.4 g of 1,1-carbonyldiimidazole portion-wise over 1 hour. The suspension was heated to 60 °C and stirred 15 at this temperature for 2 hours before cooling to room temperature. The mixture was then poured in to 1 L of deionised water to precipitate to the product. To the mixture was added 4M hydrochloric acid until the solution had become slightly acidic. The precipitate was collected by vacuum filtration and washed with deionised water before drying in a vacuum oven at 60 °C overnight to give 21.8 g of an off-white powder, 96.9 % yield, with a melting >350 °C. 20 1H NMR (DMSO-d6): 5 (ppm) 11.25 (bs, 2H, NH); 7.44 (s, 2H, Ar H); 6.76 (s, 2H, Ar H); The urone was prepared using 10.1 g of [1,3]-oxazolo[4,5-F][1,3]benzoxazole-2,6-(3H,5H)-dione, and 40 ml of 40 wt. % aqueous dimethylamine in the same procedure set out in example 1 using a reaction time of 2.5 hours. The product was purified by dissolving in 100 ml of hot 25 dimethylacetamide and filtering. The filtrate was then poured in to 250 ml of deionized water. The precipitate was collected by filtration and washed with deionized water before drying in a vacuum oven at 60 °C overnight to give 11.4 g of a burgundy powder, 77.0 % yield, with a melting point of 233 °C (dec.). 1H NMR (DMSO-d6): 5 (ppm) 9.47 (s, 2H, OH); 7.70 (s, 2H, NH); 7.28 (s, 1H, Ar H); 6.32 (d, 1H, Ar H); 2.94 (s, 12H, NCH3); 5 Example 5 The products of Examples 1 and 2 were used as curatives for an Epoxy resin and compared with standard bisfunctional urones UR500 and U52, and with OHFU and NOHFU as monofunctional orthohydroxyfenurons. The urones were dispersed in the epoxy resin Epikote 10 (RTM) 828 so that there is an equivalent ratio of urone functionalities to epoxy resin groups = 5.6 mol % of urone groups to epoxy groups. Table 1 30 08 24 Epoxy weight (g) Urone Urone weight (g) 11.40 UR500 0.44 11.40 U52 0.57 11.40 OHFU 0.60 11.40 5-NOHFU 0.75 11.40 PBOHFU 0.68 11.40 FPBOHFU 0.87 15 The mixtures were cured in a fan oven at 150°C for 1 hour with 1 °C / min temperature increase to reach 150°C. The samples were also postcured at 180°C to for 2 hours to achieve full cure. The results in Table 2 show that the use of the urones of this invention show improved ultimate Tg compared the standard urones and the monofunctional OHFUs. 20 Table 2 Urone Tg 150°C cure Tg 180°C postcure lljllllllllll UR500 94 96 U52 94 96 OHFU 97 98 5-NOHFU 79 98 PBOHFU 109 110 FPBOHFU 83 100 The reactivity was measured at various cure temperatures by the time to peak from isothermal DSC and as Table 3 shows the PBOHFLI of the invention performs in a similar manner if not slightly better than the non-hydroxy phenyl bisfunctional U52. Table 3 Time to peak at T = (mins) Urone 80°C 90°C 110°C 130°C U52 244 118 36 14 PBOHFU 230 99 28 11 30 08 24 The outlifes of the mixtures was tracked by monitoring the uncured Tg of the mixtures when held at 23°C over time. The graph which is Figure 1 hereof shows the outlife performance is 10 similar to both that of the standard bisfunctional urones and the monofunctional OHFUs. Furthermore, as Table 4 shows increasing the content of the bis OHFUs of this invention in the epoxy resin from 5.6 to 10 mol % of urone groups to epoxy groups improves the Tg to a greater extent than when using the monofunctional OHFUs. Table 4 Epoxy weight (g) Urone Urone weight (g) Tg 150°C cure Tg 180°C postcure llllllllllll 11.40 OHFU 1.06 101 104 11.40 5-NOHFU 1.37 101 106 11.40 PBOHFU 1.22 116 121 11.40 FPBOHFU 1.55 101 108 As shown the PBOHFU exhibited an improved Tg compared the monofunctional OHFU. OHFU shows an increase of only 6°C in ultimate Tg when added a 10 mol % compared to 5.6 20 mol % whereas PBOHFU shows and 11°C increase at 10 mol % compared to 5.6 mol %. Example 6 The product of Example 1 was used as curatives for an Epoxy resin and compared with standard bisfunctional urones UR500 and U52 and with OHFII as a monofunctional orthohydroxyfenuron. The urones were dispersed in the epoxy resin MY721 so that there is 5 an equivalent ratio of urone functionalities to epoxy resin groups = 5.6 mol % of urone groups to epoxy groups. Table 5 MY721 (g) Urone Urone weight (g) 11.40 UR500 0.74 11.40 U52 0.95 11.40 OHFU 1.01 11.40 PBOHFU 1.12 30 08 24 10 The mixtures were cured in a fan oven at 180°C for 2 hours with 1 °C / min temperature increase to reach 180°C. The results in Table 6 show that the use of the urones of this invention show improved ultimate Tg postcure compared the standard urones and the monofunctional OHFU. Table 6 Urone Tg 180 °C cure UR500 175 U52 168 OHFU 185 PBOHFU 190 The outlifes of the mixtures of Table 5 were tracked by monitoring the uncured Tg of the mixtures when held at 23°C over time. The graph which is Figure 2 hereof shows the outlife performance is similar for the products of the invention to both that of the standard bisfunctional urones and slightly better than the monofunctional OHFUs. 20 The latency of the mixtures at 80 °C was monitored by isothermal rheology over a 3-hour time frame. The graph which is Figure 3 hereof shows the PBOHFLI of the invention shows the latency performance at 80 °C is better than the monofunctional OHFII and approaches that of the standard bisfunctional urones UR500 and U52. Example 7 5 The products of Examples 1 and 2 were used as accelerators for a 4,4-DDS curing system as shown in Table 7 compared with standard bisfunctional urones UR200 and U52 and with OHFII as a monofunctional orthohydroxyfenuron. Table 7 30 08 24 10 Component Composition (wt. %) MY0610 27.64 LY1556 24.45 5003P 15.00 Polyamide particle 13.50 4,4-DDS 18.40 Urone 1.00 The mixtures were cured in a fan oven at 180 °C for 45, 75 and 120 minutes, 1 °C / min temperature increase to reach 180°C. The results in Tables 8 and 9 show, whilst the PBOHFLI and FPBOHFU of the invention show similar effects of cure acceleration in terms of % cure, they exhibit improved Tgs across all cure cycle times compared to the standard urones and 15 the monofunctional OHFII. Table 8 Tg (°C) after 180 °C cure for Accelerator 45 minutes 75 minutes 120 minutes UR500 130 n / a 136 U52 131 n / a 143 OHFU 138 n / a 145 PBOHFU 151 149 151 FPBOHFU 156 162 167 Table 9 % cure after 180 °C cure for Accelerator 45 minutes 75 minutes 120 minutes UR500 96.1 n / a 97.5 U52 94.6 n / a 98.5 OHFU 96.1 n / a 98.4 PBOHFU 97.4 97.8 97.8 FPBOHFU 96.4 97.5 99.0 No accelerator 81.1 85.1 91.8 30 08 24 as the composition of the formulation was modified by reducing the urone content to that 5 shown in Table 10 and Tables 11 and 12 show how decreasing the content of the bis OHFUs of this invention in the DDS curing system lead to a further improvement in Tg whilst still offering good acceleration across all cure cycle times. Table 10 Component Composition (wt. %) MY0610 27.84 LY1556 24.63 5003P 15.00 Polyamide particle 13.50 4,4-DDS 18.53 Urone 0.50 Table 11 Tg (°C) after 180 °C cure for Accelerator 45 minutes 75 minutes 120 minutes PBOHFU 160 166 176 FPBOHFU 163 173 180 Table 12 % cure after 180 °C cure for Accelerator 45 minutes 75 minutes 120 minutes PBOHFU 96.8 97.8 99.0 FPBOHFU 94.1 96.0 97.6 No accelerator 81.1 85.1 91.8 The latency of the mixtures at 100 °C was monitored by isothermal rheology over a 3-hour 5 time frame. The graph which is Figure 4 hereof shows that the FBOHFLI and PBOHFLI of the invention show the latency performance at 100 °C that is unchanged for FBOHFLI, at both the 1% and 0.50%loadings, compared to the unaccelerated formulation. 30 08 24
Claims
1. A resin formulation comprising one or more Bisorthohydroxy aromatic urones of formulae selected from30 05 2410 where Ri = S, SO2, SO, P, PX, N, NH, NX, P=O(OX or OH), C=O, a linear or branched aliphatic radical (substituted or unsubstituted), or an unsubstituted, halo substituted and / or alkyl substituted aromatic radical and n is a number from 2 to 20where X = a linear or branched aliphatic radical (substituted or unsubstituted), or an 15 unsubstituted, halo substituted and / or alkyl substituted aromatic radicalR2 and R3 = at each occurrence, independently of one another, selected from an alkyl, cycloalkyl, alkenyl, cycloalkenyl, or aralkyl group, which may be substituted by a halogen atom (preferably a chlorine atom) or by a hydroxyl or cyano group, with the proviso that20 R2 may alternatively denote a hydrogen atom, or R2 and R3 together with the indicated attached nitrogen atom denote a heterocyclic ring containing 3 to 5 carbon atoms, and optionally one oxygen atom, in the ringR4 = at each occurrence, independently of one or another, selected from H, NH2, NO2, 25 nitrile, a halogen, linear or ranched aliphatic radical, or an unsubstituted, halo substitutedand / or alkyl substituted aromatic radical, and Y = 1 to 330 05 24and at least one resin component selected from an epoxy, a polyisocyanate and a phenolic resin.
2. A resin formulation according to Claim 1 in which the bisorthohydroxy aromatic urone comprises N, N’-[propylene(4-hydroxy3,1 -phenylene)]bis(N,N-dimethyl)urea.
3. A moulding material comprising a resin formulation according to Claim 1 of Claim 2 in combination with a fibrous reinforcement material.
4. A moulding material according to Claim 3 in which the fibrous reinforcement material is selected from a woven fabric, a multi-axial fabric, individual fibre tows, chopped fibres, short fibres and I or filaments and mixtures thereof.
5. A moulding material according to Claim 4 in which the fibrous material is selected from carbon fibre, glass fibre and aramid.
6. A prepreg comprising fibre reinforcement and a resin formulation according to Claim 1 or Claim 2.
7. A stack of prepregs according to Claim 6.
8. A stack according to Claim 7 containing at least 40 prepregs.
9. A process for the production of an article comprising curing a prepreg according to Claim 6 or a stack of prepregs according to Claim 7 or Claim 8.
10. A process according to Claim 9 in which the curing is caused by an externally applied temperature of 60°C to 190°C.
11. A process according to Claim 9 or Claim 10 performed in a vacuum bag.
12. A process according to Claim 9 or Claim 10 wherein cure is performed in a press.
13. A process according to any of Claims 9 to 12 for the production of wind turbine components.
14. A process according to any of Claims 9 to 12 for the production of aerospace components.
15. A resin formulation according to Claim 1 or Claim 2 comprising an epoxy resin and from 2 to 20 wt % of the bisorthohydroxy aromatic urone.30 05 2416. A resin formulation according to Claim 1 or Claim 2 comprising an epoxy resin and a curing agent other than a bisorthohydroxy aromatic urone according to Claim 1 and from 0.1 to 2 wt % of a bisorthohydroxy aromatic urone according to Claim 1 or Claim 2.
517. A composition according to Claim 16 in which the curing agent other than a bisorthohydroxy aromatic urone according to Claim 1 is a primary or secondary amine.
18. A composition according to Claim 17 in which the primary or secondary amine is selected 10 from ethylenediamine, diethylenediamine, diethylenetriamine, triethylenetetramine, propylene diamine, tetraethylenepentamine, hexaethyleneheptamine, hexamethylenediamine, cyanoguanidine, 2-methyl-1,5-pentamethylene-diamine, 4,7,10-trioxatridecan-1,13-diamine, aminoethylpiperazine,dicyanopolyamides, 4,4’-diaminodiphenyl sulfone or 3,3’-diaminodiphenyl sulfone, bisanilines, dihydrazides, 15 polyamines, polyether amines having one or more amine moieties, and mixtures thereof.
19. A wind turbine component made from a moulding material according to any of Claims 3 to 5 or a composition according to any of Claims 15 to 18.20 20. An aerospace component made from a moulding material according to any of Claims 3 to5 or a composition according to any of Claims 15 to 18.
21. The use of bisorthohydroxy aromatic urones as defined in Claim 1 or Claim 2 as a curative for epoxy resins.2522. The use of bisorthohydroxy aromatic urones as defined in Claim 1 or Claim 2 as an accelerator or curative for epoxy resins.
23. The use according to Claim 21 or Claim 22 in a prepreg.30
Citation Information
Patent Citations
Heat developable photosensitive material
JP2005084469A
Heat developable photosensitive material
JP2005241691A
Use of n,n'-(dimethyl) urones and method for curing epoxy resin compositions
US20140357762A1
Heat-curable epoxide resin compositions
US4404356A
Silver halide color photographic material
US5294530A