AI Technical Summary
Existing golf ball manufacturing methods using injection molds face issues with wear resistance and high processing costs due to the use of thick plating on the inner circumferential surface of the pin receiving hole, leading to deformation and defects in the golf balls.
Applying plasma nitriding treatment to the inner circumferential side of the pin receiving hole in the injection mold, eliminating the need for thick plating and enhancing wear resistance, while allowing for cost-effective production.
The method provides improved wear resistance and reduces processing costs, resulting in higher durability and quality of golf ball production without the drawbacks of thick plating.
Smart Images

Figure 2024151885000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a golf ball, which includes a step of molding a resin material for a cover layer in an injection mold. [Background technology]
[0002] In general, an injection mold is used to manufacture each layer of a golf ball cover. This injection mold often has a plurality of support pins arranged to be movable in a direction perpendicular to the parting line of the mold. That is, when injection molding a cover layer, a molten resin material is poured into a spherical cavity of the mold while a target sphere such as a core or an intermediate layer-coated sphere is supported in the spherical cavity by a plurality of support pins, and injection molding is performed. The support pins are arranged in pin receiving holes located from the inner wall surface of the spherical cavity to the outside, so that the support pins supporting the target sphere are automatically controlled to retract from the spherical cavity to the pin receiving holes during the process of pouring the molten resin material into the spherical cavity.
[0003] However, the core supported by the multiple support pins in the cavity of the mold is made of a rubber material, and the interior of the intermediate layer-coated sphere is also made of a rubber material. When a strong injection pressure is applied to such a core made of a rubber material, the core is significantly deformed into a rugby ball shape in both directions of the mold, and as a result, when the support pin retreats from the spherical cavity into the pin receiving hole, the support pin is pressed by the above-mentioned core deformation and the support pin abuts against the inner peripheral side of the pin receiving hole, especially the outer inner peripheral side, which causes wear on the inner peripheral side of the pin receiving hole. In particular, since the mold is used many times, the pin receiving hole is repeatedly worn each time, causing the pin receiving hole to widen, which not only causes problems with the mold itself but also has a negative effect on the ball product, such as poor ball molding.
[0004] To prevent wear of the pin receiving hole, the inner peripheral side surface of the pin receiving hole is plated with hard chrome plating, electroless nickel plating, etc. However, even if such plating is applied, problems remain in terms of wear resistance, cost, etc. For example, in an injection molding die used to mold a cover made of ionomer resin material, the inner peripheral side surface of the pin receiving hole is plated with a relatively thick hard chrome plating, and jig polishing is also performed to further improve accuracy, resulting in high processing costs and black stains.
[0005] As a technique related to the present case, JP 2000-102630 A discloses a mold treated with boron nitride, chromium nitride, or titanium nitride as a measure to improve the releasability between the inner surface of the cavity and the core material of the golf ball, but does not mention the problem of wear resistance of the pin receiving hole that receives the support pin. JP 2011-67627 A also describes forming a eutectoid plating of nickel and fluororesin on a mold for injection molding a urethane cover material. However, even if such a eutectoid plating is formed, some issues remain with the wear resistance of the pin receiving hole. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] JP 2000-102630 A [Patent Document 2] JP 2011-67627 A Summary of the Invention [Problem to be solved by the invention]
[0007] The present invention has been made in consideration of the above-mentioned circumstances, and has an object to provide a method for manufacturing a golf ball which is inexpensive, does not require thick plating of hard chrome or the like on the inner peripheral surface of the pin receiving hole of the support pin, and which enables the cover material to be molded using an injection molding die which provides good wear resistance for the pin receiving hole. [Means for solving the problem]
[0008] As a result of intensive research into achieving the above object, the inventors discovered that by applying a nitriding treatment, particularly a plasma nitriding treatment, instead of a plating treatment such as hard chrome plating to the inner peripheral side surface of a pin receiving hole that receives a support pin of an injection molding die, the wear resistance of the pin receiving hole can be favorably maintained even when the cover resin material is not only an ionomer resin material but also a urethane resin material, and thus came up with the present invention. Such a nitriding treatment is less expensive than hard chrome plating, and does not cause black stains, etc., and has industrial advantages when using a mold for a golf ball.
[0009] Accordingly, the present invention provides the following method for producing a golf ball. 1. A method for manufacturing a golf ball having a core and at least one cover, the method comprising the step of molding at least one layer of the cover using an injection molding die that is divided into an upper and lower part, the injection molding die having a spherical cavity and three or more support pins that are arranged so as to be able to advance and retreat in a direction perpendicular to the parting line of the die, and at least the inner side surface of the pin hole portion that houses the support pins is nitrided. 2. The method for producing a golf ball according to the above item 1, wherein the nitriding treatment is a plasma nitriding treatment. 3. The method for manufacturing a golf ball according to claim 2, wherein the inner peripheral side surface of the nitriding treated pin hole has a diffusion layer (nitriding layer) having a thickness of 5 to 20 μm, and a layer structure in which no compound layer is present. 4. The method for producing a golf ball according to 1 or 2 above, wherein the injection mold is subjected to a nitriding treatment and then the inner surface of the spherical cavity is machined to form projections and recesses corresponding to dimples. 5. The method for producing a golf ball according to claim 2, further comprising carrying out a plating treatment after the plasma nitriding treatment. 6. The method for producing a golf ball according to 5 above, wherein the plating is a composite plating in which fluororesin particles are dispersed in a nickel-based matrix. 7. The method for producing a golf ball according to 1 or 2 above, wherein the cover layer molded by the injection mold is the outermost layer of the cover. 8. The method for producing a golf ball according to the above 7, wherein the outermost layer has a thickness of 0.2 to 1.5 mm and is formed from a resin material containing polyurethane resin as a main component. 9. The method for producing a golf ball according to the above item 7, wherein the material hardness of the outermost layer is 30 to 55 in Shore D hardness. Effect of the Invention
[0010] The method for manufacturing a golf ball of the present invention includes a step of molding the resin material for the cover layer using an injection molding die, and does not require thick plating of hard chrome or the like on the inner peripheral side surface of the pin receiving hole of the support pin, which is inexpensive and allows the cover material to be molded using an injection molding die which provides good wear resistance for the pin receiving hole. [Brief description of the drawings]
[0011] [Figure 1] 1A is a schematic diagram showing an injection molding die used in the present invention, in which (A) shows the state before injection molding, (B) shows the state during flow of resin material into the die, and (C) shows the state after the resin material has been filled into the die. [Diagram 2] FIG. 2 is a schematic diagram for explaining the arrangement of gates in an injection mold. [Diagram 3] FIG. 4 is a schematic cross-sectional view showing the positions of support pins arranged in an injection molding die. [Figure 4] FIG. 2 is an enlarged view of a pin receiving hole, which is a part of a spherical cavity, and its vicinity. [Diagram 5] FIG. 2 is a photograph showing the main body of an injection molding die. [Figure 6] FIG. 6(A) is a schematic diagram showing how the entire surface of a mold is subjected to a nitriding treatment, and FIG. 6(B) is a schematic diagram showing how the nitride layer in the spherical cavity of the mold is machined. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] The present invention will now be described in further detail. The manufacturing method of the present invention is a method for producing a golf ball having a core and at least one cover layer, which includes a step of molding at least one layer of the cover in an upper and lower two-piece injection mold.
[0013] The cover material is not particularly limited, and various thermoplastic resins used in golf ball cover materials can be used. In particular, it is preferable to use a resin material mainly made of ionomer resin or urethane resin. The cover resin material is heated to a predetermined temperature and injected in a molten state between a target spherical object such as a core or a mid-layer-coated sphere set in an injection mold and a spherical cavity wall surface to form a cover around the target sphere.
[0014] The material hardness of the cover is not particularly limited, but is preferably at least 30, more preferably at least 35, and even more preferably at least 40, in Shore D hardness, with the upper limit being preferably no more than 70, more preferably no more than 62, and even more preferably no more than 55. The cover has a thickness of at least 0.2 mm, preferably no less than 0.5 mm, and more preferably no less than 0.7 mm, with the upper limit being preferably no more than 2.0 mm, preferably no more than 1.8 mm, and even more preferably no more than 1.5 mm.
[0015] The injection molding die used in the present invention (hereinafter, sometimes simply referred to as "die") usually has a spherical cavity, a gate for injecting a resin material for a cover into the spherical cavity, and a support pin arranged so as to be movable in a direction perpendicular to the parting line of the die. For example, as shown in FIG. 1, an injection molding die 10 having a spherical cavity 1, a predetermined number of gates 2, and a predetermined number of support pins 3 is used, and a molten resin material 30, which is a cover material, is injected into the spherical cavity from the gate 2 in a state in which a target sphere 20 such as a core or an intermediate layer-coated sphere is supported by a plurality of support pins 3 in the spherical cavity 1. FIG. 1(A) is a schematic diagram showing the state inside the die before injection molding, showing a state in which the support pins 3 support the target sphere 20. Fig. 1(B) is a schematic diagram of the inside of the mold 10 when the molten resin material 30 is poured into the mold 10, and Fig. 1(C) is a schematic diagram showing the state of the mold 10 after the molten resin material 30 is filled into the mold 10 and injection molding is completed. The operation of the predetermined number of support pins 3 supporting the target spherical object 20 in the spherical cavity 1 in the mold is such that the support pins gradually retreat as the molten resin material 30 fills the spherical cavity 1, and just before the filling of the cavity with the molten resin material is completely completed, the support pins are pulled so as to coincide with the wall surface of the cavity, and then the filling of the resin material is completed. Although not particularly shown, at the position of the parting line of the mold, a runner part for supplying the cover material is arranged so as to surround the spherical cavity, and gates opening radially from the runner part toward the cavity are arranged on the circumference as shown below.
[0016] A plurality of gates are formed along the parting line of the mold. In the example of FIG. 2, six gates 2 are evenly arranged along the parting line PL. If the number of gates is too small, the molten resin material is not sufficiently introduced into the spherical cavity, and after injection molding, the cover thickness near the pole of the spherical cavity becomes thin, and the target spherical object such as the core or the intermediate layer-coated sphere may not be completely covered and may become bald. The gates 2 arranged along the parting line PL of the mold are preferably arranged at equal intervals around the circumference of the parting line PL from the viewpoint of uniformly introducing the molten resin material into the spherical cavity to form a cover of the desired thin thickness.
[0017] A plurality of support pins 3 arranged so as to be movable in a direction perpendicular to the parting line PL of the mold are usually arranged at a predetermined interval of three or more (for example, three at intervals of 120°) along a circle drawn around the pole of the spherical cavity. The support pins are arranged so as to be movable in and out of the holes having a circular cross section of the upper and lower split molds, and as shown in FIG. 1(A), they hold the target sphere 20 when they enter the spherical cavity 1, and retract to the position of the inner wall surface of the spherical cavity 1 when the molten resin material is filled into the spherical cavity 1. It is desirable to optimize the diameter (end diameter) and number of the holes of the support pins in order to suppress deformation of the intermediate layer-coated sphere set in the spherical cavity during the process of filling the spherical cavity with the resin material and to stably position the core in the center of the spherical cavity.
[0018] The number of support pins on one side of the upper or lower mold is preferably 3 or more, more preferably 4 or more, and even more preferably 6 or more. The upper limit of this number is preferably 12 or less, more preferably 10 or less. If the number does not fall within the above range, it may be difficult to hold the target spherical object at the center of the spherical cavity, suppress deformation of the target spherical object, and form the cover resin material with a uniform thickness throughout the space between the target spherical object and the wall surface of the spherical cavity.
[0019] Regarding the position of the support pin, as shown in Fig. 3, it is preferable to arrange the support pin 3 so that the angle θ between the axis X connecting the upper and lower poles of the mold and the normal line from the center O on the axis toward the cavity wall surface 1a from which the support pin 3 exits is 15 to 30°. This angle is more preferably 18° or more, and even more preferably 20° or more, and the upper limit is preferably 30° or less, more preferably 28° or less, and even more preferably 25° or less. If the angle deviates from the above range, it may be difficult to hold the target spherical object 20 at the center O of the cavity, suppress deformation of the target spherical object 20, and form the cover resin material with a uniform thickness overall between the target spherical object and the cavity.
[0020] Here, the mold used in the present invention is characterized in that the inner peripheral side surface of the pin hole portion that houses the support pin is nitrided. Fig. 4 is a partially enlarged view of the pin housing hole in the spherical cavity 1 of the mold and the spherical cavity in its vicinity. As shown in this figure, a nitride layer C1 is formed on the inner peripheral side surface of the pin housing hole 1a that houses the support pin by nitriding. The reference symbol C2 in the figure denotes a plating film that further covers the surface of the nitride layer C1, which will be described later.
[0021] Nitriding is generally a treatment technique in which steel products are heated, nitrogen atoms are diffused and penetrated into the interior, and the surface is hardened. Specific examples include gas nitriding, salt bath nitriding, gas soft nitriding, ion nitriding (plasma nitriding), vacuum nitriding, and active powder nitriding. This nitriding is generally expected to improve wear resistance, fatigue resistance, corrosion resistance, and heat resistance, but in the present invention, it is mainly used for the purpose of improving wear resistance. Among them, the plasma nitriding method does not require an external heating device because the material to be treated is heated by the collision energy of ions, and it uses radicals, nitrogen atoms, and ions in an active plasma state, so it is an economical treatment method with low energy consumption and gas consumption, short treatment time, and low environmental impact. In addition, ion nitriding (plasma nitriding) is preferably adopted in the present invention because it has a high degree of freedom in selecting optimal nitriding conditions depending on the product material and application, and hardening can be achieved without oxidation.
[0022] In addition, in the plasma nitriding method, the passive film is removed by bombardment of the sample surface with fine particles ions by hydrogen or argon plasma for the purpose of activating the sample surface before treatment, and nitriding is possible even for steels with a high chromium content. Next, the target part is heated to the nitriding temperature by plasma energy. Then, in the nitriding process, the type and thickness of the desired compound layer can be determined by various conditions such as the treatment temperature and treatment time. Generally, after nitriding, plating may not be possible due to the precipitation of smut components and the influence of the compound layer, but some plasma nitriding techniques have a small treated surface roughness and are less likely to form a compound layer, making plating easy. For this reason, plasma nitriding is preferably adopted in the present invention from the above points.
[0023] The base material (substrate) of the mold body is not particularly limited as long as it is a metal that can be plated, but for example, a mold formed of a normal metal material such as carbon steel, beryllium-copper alloy, stainless steel, copper, etc. can be used. Among these, it is preferable to use pre-hardened steel that has been heat-treated in advance. Pre-hardened steel has excellent workability and does not require subsequent heat treatment, so that complex dimple shapes can be formed with high precision.
[0024] A composite plating film is formed in the spherical cavity of the mold so as to cover the cavity surface. The composite plating film is not particularly limited, but is preferably one in which fluororesin particles are dispersed in a nickel-based matrix.
[0025] The nickel-based matrix is not particularly limited as long as it is mainly made of nickel, but examples of the nickel-based matrix that can be used include alloys of nickel with other metals or substances, such as nickel-phosphorus alloys, nickel-copper-phosphorus alloys, nickel-boron alloys, cobalt-nickel alloys, and nickel-molybdenum-phosphorus alloys.
[0026] As the fluororesin particles dispersed in the nickel-based matrix, for example, polytetrafluoroethylene (PTFE) particles, tetrafluoroethylene-perfluoroalkylvinylether copolymer (PFA) particles, tetrafluoroethylene-hexafluoropropylene copolymer (FEP) particles, tetrafluoroethylene-ethylene copolymer (ETFE) particles, etc. can be used, among which PTFE particles and FEP particles are particularly preferred. The particle size of the fluororesin particles is not particularly limited, but is preferably 0.05 μm or more, more preferably 0.5 μm or more. In addition, the particle size of the fluororesin particles is preferably 3 μm or less, more preferably 2 μm or less.
[0027] A composite plating film in which fluororesin particles are dispersed in a nickel-based matrix can be formed, for example, by dispersing fluororesin particles in a plating solution of a nickel-based matrix and plating the surface of a substrate while stirring the solution. The plating method can be, for example, an electroplating method or an electroless plating method, but it is preferable to employ the electroless plating method since it is possible to obtain a particularly uniform film.
[0028] The thickness of the composite plating film is not particularly limited, but since this composite plating film can be formed very thin and has sufficient durability even when thin, as well as releasability and wettability with resin materials such as urethane materials, the thickness is preferably 20 μm or less, and more preferably 10 μm or less. On the other hand, the lower limit of the thickness of the composite plating film is preferably 1 μm or more, and more preferably 2 μm or more.
[0029] The blending ratio of the fluororesin particles in the composite plating film is not particularly limited, but is preferably 5 volume % or more, and more preferably 25 volume % or more. On the other hand, in order to obtain a composite plating film 20 having sufficient strength, the blending ratio of the fluororesin particles 22 is preferably 50 volume % or less, and more preferably 40 volume % or less.
[0030] An example of the composite plating film having fluororesin particles dispersed in a nickel-based matrix is "NifGrip," a product name manufactured by ULVAC TECHNO, Inc.
[0031] In addition, the mold used in the present invention, in which a nitride layer is formed on the inner peripheral side surface of the pin receiving hole, is preferably produced by the following procedure. As shown in the photograph of FIG. 5, first, one side (upper or lower) 10 of the mold body having the pin receiving hole 1a and the vent pin 1b is prepared. Then, as shown in the schematic explanatory diagram of FIG. 6(A), a nitride layer is formed on the entire surface of the mold 10 by nitriding treatment such as plasma nitriding. In the figure, the thick black line indicates the nitride layer. Next, as shown in the schematic explanatory diagram of FIG. 6(B), dimple processing is performed inside the spherical cavity 1 of the mold body. Although nitriding is originally a processing method that causes little dimensional change, it is considered that precision can be ensured by performing the precisely designed dimple processing after nitriding. For this reason, the nitride layer formed in the spherical cavity 1 of the mold body is cut away for dimple processing and completely disappears. Although not shown in FIG. 6(B), after dimple processing, the above-mentioned plating process is performed on the entire surface of the mold 10 to improve the durability and releasability of the mold by rust prevention. In that case, the surface without the nitride layer can be plated more advantageously. EXAMPLES
[0032] The present invention will be specifically described below with reference to examples and comparative examples, but the present invention is not limited to the following examples.
[0033] [Example 1, Comparative Example 1] For Example 1 and Comparative Example 1, a 41.1 mm intermediate layer-coated sphere, which was prepared in advance by coating an ionomer resin on a core that was a vulcanized molded product of a rubber composition mainly made of polybutadiene rubber, was set in each injection mold of Example 1 and Comparative Example 1, and a 0.8 mm thick resin material (Shore D hardness "43") for forming a cover mainly made of polyurethane was injection molded. This was repeated, and the number of times it was used repeatedly was determined when wear occurred. Specifically, the number of times that the peripheral side surface of the pin receiving hole (especially its outer part) could be molded without problems without being pushed by the support pin and expanding was confirmed.
[0034] As shown in Fig. 5, the mold used in Example 1 was prepared by preparing a mold body before surface treatment, followed by plasma nitriding (no compound layer / nitriding layer 20μm), and then dimple processing, so that the nitrided layer on the inner surface of the cavity was completely cut off. Finally, the entire mold was subjected to a predetermined plating process (product name "Nifgrip").
[0035] On the other hand, the mold used in Comparative Example 1 was prepared by preparing a mold body before surface treatment, performing dimple processing, and then performing a predetermined plating process over the entire mold, as shown in FIG.
[0036] The specified plating process uses "NifGrip" manufactured by ULVAC TECHNO, and involves co-deposition of electroless nickel and fluororesin in a treatment solution on the mold, uniformly including 30% of the fluororesin by volume in the film, and then heat treatment is performed after film formation to firmly bond the electroless nickel and fluororesin together. This plating process improves mold releasability.
[0037] As a result, both Example 1 and Comparative Example 1 had good demoldability during cover molding, but the abrasion resistance of Example 1 was about 340,000 times of repeated use, while the abrasion resistance of Comparative Example 1 was about 570,000 times of repeated use, meaning that Example 1 had far better abrasion resistance.
[0038] [Example 2, Comparative Example 2] For Example 2 and Comparative Example 2, a core having a diameter of 40.0 mm, which was a vulcanized molded product of a rubber composition mainly made of polybutadiene rubber, was set in each injection mold of Example 2 and Comparative Example 2, and a resin material (Shore D hardness "62") for forming a cover mainly made of ionomer resin was injection molded to a thickness of 1.35 mm. This was repeated, and the number of times that the peripheral side surface of the pin receiving hole (especially the outer part) could be molded without problems without being pushed by the support pin and expanding, as in Example 1, was confirmed.
[0039] As shown in Fig. 5, the mold used in Example 2 is prepared by preparing a mold body before surface treatment, and then performing plasma nitriding (no compound layer / nitriding layer 20μm), followed by dimple processing, so that the nitrided layer on the inner surface of the cavity is completely cut off. Finally, the entire mold is plated. This is the same nitriding process as in Example 1 above.
[0040] On the other hand, as shown in FIG. 5, the mold used in Comparative Example 2 was prepared by preparing a mold body before surface treatment, performing dimple processing, and then performing a slightly thick plating process on the inner peripheral side surface of the pin receiving hole. This thick plating process is a conventional plating process using hard chrome, and the plating thickness is 20 μm. Next, since hard chrome plating is prone to uneven plating thickness depending on the shape of the target object, it is necessary to perform jig polishing to ensure the accuracy of the pin receiving hole (note that jig polishing means a grinding technique that can process the inner diameter of a round hole, a square hole, and the dimensions of an irregular shape at that position in 1 μm units while achieving pitch accuracy). Finally, the entire mold was plated. This is the same plating process as in Example 2 above.
[0041] As a result, both Example 2 and Comparative Example 2 had good demoldability during cover molding. In addition, there was almost no difference in the abrasion resistance between Example 2 and Comparative Example 2 even after repeated use 1 million times, and both had good abrasion resistance. However, Comparative Example 2 used hard chrome plating, which resulted in high processing costs, and when used as a new product, the pin and the thickly plated part rubbed against each other, causing black stains due to metal powder, which often caused defective products. In Example 2, the time and cost required for plating the mold were significantly reduced compared to Comparative Example 2. In addition, black stains were no longer generated. [Explanation of symbols]
[0042] 1. Spherical cavity 2 Gate 3 Support pins 10 Injection mold PL parting line 20 Spherical Objects 30 Molten resin material 1a Pin receiving hole C1 nitride layer C2 plating film
Claims
1. 1. A method for manufacturing a golf ball having a core and at least one cover, the method comprising the step of molding at least one layer of the cover using an injection mold that is two-piece, upper and lower, wherein the injection mold has a spherical cavity and has three or more support pins that are arranged so as to be able to advance and retreat in a direction perpendicular to the parting line of the mold, and at least the inner side surface of the pin hole portion that houses the support pins is nitrided.
2. 2. The method of claim 1, wherein the nitriding treatment is a plasma nitriding treatment.
3. 3. The method for manufacturing a golf ball according to claim 2, wherein the inner peripheral side surface of the nitrided pin hole has a diffusion layer (nitride layer) having a thickness of 5 to 20 μm, and a layer structure in which no compound layer is present is formed.
4. 3. The method for manufacturing a golf ball according to claim 1, wherein the injection mold has an inner surface of a spherical cavity cut to form projections and recesses corresponding to dimples after a nitriding treatment.
5. 3. The method of manufacturing a golf ball according to claim 2, further comprising the step of performing a plating process after said plasma nitriding process.
6. 6. The method for manufacturing a golf ball according to claim 5, wherein the plating is a composite plating in which fluororesin particles are dispersed in a nickel-based matrix.
7. 3. The method for producing a golf ball according to claim 1, wherein the cover layer molded in the injection mold is the outermost layer of the cover.
8. 8. The method for manufacturing a golf ball according to claim 7, wherein the outermost layer has a thickness of 0.2 to 1.5 mm and is made of a resin material mainly composed of a polyurethane resin.
9. 8. The method of manufacturing a golf ball according to claim 7, wherein the material hardness of the outermost layer is 30 to 55 in Shore D hardness.
Citation Information
Patent Citations
Manufacture and metal mold of golf ball and its core