Manufacturing method and manufacturing device for resin container

A two-step injection molding process for resin containers forms a multilayer preform, enabling precise three-dimensional patterns on the thick bottom with reduced deformation and cooling defects, enhancing the aesthetic and luxury feel.

JP7566133B2Active Publication Date: 2024-10-11NISSEI ASB MASCH CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2023507117
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-03-15
Filing Date
2022-03-14
Publication Date
2024-10-11
Estimated Expiration
2042-03-14

AI Technical Summary

Technical Problem

Existing methods struggle to form a three-dimensional pattern on the thick bottom of resin containers with high precision, as the thick bottom is prone to deformation and uneven cooling during the blow molding process.

Method used

A two-step injection molding process is employed to create a multilayer preform, where a first layer is formed with a thicker bottom, followed by a second layer, allowing for precise transfer of a three-dimensional pattern onto the thick bottom during blow molding, and enhanced cooling efficiency.

Benefits of technology

The method enables accurate formation of a three-dimensional pattern on the thick bottom of resin containers with reduced deformation and cooling defects, improving the aesthetic appearance and luxury feel.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007566133000001
    Figure 0007566133000001
  • Figure 0007566133000002
    Figure 0007566133000002
  • Figure 0007566133000003
    Figure 0007566133000003
Patent Text Reader

Abstract

This resin container manufacturing method comprises: a first injection molding step in which a bottomed cylindrical intermediate molded body made of a resin is injection-molded; a second injection molding step in which a resin material is injection-molded on the intermediate molded body to manufacture a multilayer preform in which a resin layer is layered on the intermediate molded body; and a blow molding step in which the multilayer preform is blow-molded, while the residual heat from the time of injection molding is retained, to produce a resin container. The multilayer preform is formed such that the bottom is thicker than a trunk section. In the blow molding step, at least one surface of the bottom of the multilayer preform is pressed by a mold, and a three-dimensional pattern corresponding to the mold is transferred to the thick bottom section of the resin container.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method and an apparatus for manufacturing a resin container. [Background technology]

[0002] Containers for cosmetics, lotions, etc., are required to have an aesthetically pleasing appearance in order to increase consumer purchasing power. Glass bottles, which have a heavy and luxurious feel and can maintain their beauty even after repeated use, are preferred for containers for storing this type of cosmetics. However, glass bottles are heavy and breakable, and the costs of transportation and manufacturing are high. For this reason, the replacement of glass bottles with plastic containers for storing cosmetics, etc., is being considered.

[0003] Here, a hot parison type blow molding method has been conventionally known as one of the methods for manufacturing a resin container. In the hot parison type blow molding method, a resin container is blow molded by utilizing the heat retained during injection molding of a preform. In the hot parison type blow molding method, the injection molded preform is blow molded without being removed from the machine, so scratches are unlikely to form on the exterior of the container, and it is easy to design and adjust the shape of the preform to match the shape of the container. Therefore, compared to the cold parison type, it is advantageous in that it can manufacture a variety of resin containers with excellent aesthetic appearance.

[0004] Furthermore, in the case of resin containers for storing cosmetics and the like, it has been proposed to form a three-dimensional pattern on the inner surface of the bottom for the purposes of improving the aesthetic appearance of the container and preventing the contents from rotating. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] Japanese Patent Application Publication No. 5-169521 [Patent Document 2] Patent No. 5035676 Summary of the Invention [Problem to be solved by the invention]

[0006] When a resin container is used as a container for storing cosmetics, etc., it is desirable to mold the resin container into a shape in which the bottom is thick and the body is thin and uniformly thick in order to emphasize a sense of luxury and weight. However, when forming a three-dimensional pattern on the bottom of a thick-walled container, a preform with a thick bottom and a large amount of heat retention at the bottom is blow molded, so it has been difficult to accurately form a three-dimensional pattern while ensuring a predetermined thickness on the easily deformed bottom. [Means for solving the problem]

[0007] A method for producing a resin container according to one embodiment of the present invention includes the steps of: Using the first injection mold a first injection molding step of injection molding a bottomed cylindrical intermediate molded body made of resin; Using a second injection mold that is different from the first injection mold A resin material is injected into the intermediate molded body; The bottom is thicker than the body, and the bottom is thicker than the intermediate molded body due to the lamination of the resin layers. The method includes a second injection molding step of producing a multi-layer preform, and a blow molding step of blow molding the multi-layer preform while retaining the heat generated during injection molding to produce a resin container. B In the row molding process, at least one surface of the bottom of the multi-layer preform is pressed with a metal mold, and a three-dimensional pattern corresponding to the metal mold is transferred to the thick-walled bottom of the resin container. At the same time, the three-dimensional patterned protrusions on the mold promote cooling within the thick bottom wall. . Effect of the Invention

[0008] According to one aspect of the present invention, a three-dimensional pattern can be formed with high precision on the thick-walled bottom portion of a resin container. [Brief description of the drawings]

[0009] [Figure 1] FIG. 2 is a perspective view of the container according to the first embodiment. [Diagram 2] FIG. 2(a) is a front view of the container of the first embodiment, and FIG. 2(b) is a vertical sectional view of the container of FIG. 2(a). [Diagram 3] FIG. 2 is a longitudinal sectional view of the preform of the first embodiment. [Figure 4] FIG. 1 is a diagram illustrating a schematic configuration of a blow molding device according to a first embodiment. [Diagram 5] 3A to 3C are diagrams illustrating an example of a manufacturing process for the preform of the first embodiment. [Figure 6] 3A to 3C are diagrams illustrating a blow molding process according to the first embodiment. [Figure 7] 4 is a flow chart showing steps of a method for manufacturing a container. [Figure 8] FIG. 11 is a perspective view of a container according to a second embodiment. [Figure 9] 9(a) is a front view of a container according to a second embodiment, and FIG. 9(b) is a vertical cross-sectional view of the container of FIG. 9(a). [Figure 10] 11A to 11C are diagrams illustrating a blow molding process according to a second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In the embodiments, in order to make the description easier to understand, structures and elements other than the main parts of the present invention will be described in a simplified or omitted manner. In addition, in the drawings, the same elements are given the same reference numerals. Note that the shapes, dimensions, etc. of each element shown in the drawings are shown only for illustrative purposes, and do not represent the actual shapes, dimensions, etc.

[0011] First Embodiment (Example of resin container configuration) First, with reference to Figs. 1 and 2, a configuration example of a resin container (hereinafter also simply referred to as a container) 10 according to a first embodiment will be described. Figures 1(a) and (b) are perspective views of a container 10 according to a first embodiment. Figure 2(a) is a front view of the container 10 according to the first embodiment, and Figure 2(b) is a vertical cross-sectional view of the container 10 of Figure 2(a).

[0012] Container 10 shown in Figures 1 and 2 has an overall shape of a short cylinder with an opening on the top side. Container 10 is formed of a resin material such as PET, and contains lotion, milky lotion, etc. Container 10 has a neck 12 with a mouth 11 at the top end, a short cylindrical body 13 continuing from neck 12, and a bottom 14 continuing from body 13.

[0013] 2(b), the thickness t2 of the bottom 14 of the container 10 is formed to be thicker than the thickness t1 of the body 13. That is, the thickness t1 of the body 13 is formed to be significantly thinner than the bottom 14, and the body 13 is uniformly thick. Although not particularly limited, the thickness t2 of the bottom 14 of the container 10 is set to be 6 mm or more (6 mm to 15 mm), preferably, for example, 10 mm or more (10 mm to 15 mm).

[0014] By giving the container 10 a shape with the above thickness distribution, the sense of luxury and weight is emphasized, and the container 10 can be made closer to the image of a cosmetic container that consumers have. In other words, the aesthetic appearance of the container 10 can be improved, and the container 10 can be used as a cosmetic container where appearance is important.

[0015] 2(b), the body 13 and the bottom 14 of the container 10 have a structure in which a first layer 15 facing the inner surface of the container and a second layer 16 facing the outer surface of the container are laminated together. This structure is formed by blow molding a preform 20, which will be described later.

[0016] In the first embodiment, as shown in Fig. 1(b) and Fig. 2(b), a three-dimensional pattern 17 is applied to the inner surface of the bottom 14 of the container 10. The three-dimensional pattern 17 is a depression that is concave downward from the inner surface of the container of the bottom 14 toward the inside of the bottom 14, and is formed, for example, in a diamond shape (a group of polyhedrons) or a flower crown shape. By forming the three-dimensional pattern 17 on the bottom 14 of the container 10, the aesthetic appearance of the container 10 can be further improved, and the desire to purchase the product can be further increased.

[0017] 1 and 2, when the container 10 (and further the contents of the container 10) is translucent, the three-dimensional pattern 17, such as a diamond shape or a flower crown shape, also serves to enhance the luxury of the container 10 by scattering incident light at the site of the three-dimensional pattern 17. The shape of the three-dimensional pattern 17 is not limited to the examples shown in Figs. 1 and 2, and can be modified as appropriate.

[0018] (Example of preform configuration) FIG. 3 is a vertical cross-sectional view of a preform (multilayer preform, two-layer preform) 20 used in the manufacture of the container 10 of the first embodiment. The overall shape of the preform 20 is a bottomed cylindrical shape that is open at a mouth 21 on one end side and closed at the other end side. The preform 20 includes a cylindrical body portion 23, a bottom portion 24 that closes the other end side of the body portion 23, and a neck portion 22 that is formed at one end side of the body portion 23 and has the mouth portion 21. In the preform 20 of Fig. 3, the axial length of the body portion 23 is set to be short so as to correspond to the container 10 having a short cylindrical shape.

[0019] The preform 20 has a structure in which a first layer 15 located on the inner periphery side and a second layer 16 located on the outer periphery side are laminated. The neck portion 22 is made of the material of the first layer 15, but the body portion 23 and the bottom portion 24 are configured by laminating the second layer 16 on the outer periphery of the first layer 15.

[0020] The preform 20 in Fig. 3 is formed as follows. First, an intermediate molded body 20A having a neck portion 22, a body portion 23, and a bottom portion 24 is injection molded with the material of the first layer 15. Then, the material of the second layer 16 is further injection molded onto the outer periphery of the body portion 23 and the bottom portion 24 of the intermediate molded body 20A, thereby forming the preform 20.

[0021] Here, the composition of the material of the first layer 15 and the second layer 16 may be the same or different. For example, the same resin material may be used for the first layer 15 and the second layer 16, or different materials may be used. Also, for example, the amount of coloring material (shade of color) or the type of coloring material (type of color) may be changed in each material of the first layer 15 and the second layer 16. At least one of the first layer 15 and the second layer 16 (preferably both the first layer 15 and the second layer 16) may have a property of transmitting light (translucency or transparency).

[0022] In the example of Fig. 3, in order to form a container 10 with a thick bottom, a preform 20 is applied in which the thickness t12 of the bottom 24 is at least twice the thickness t11 of the body 23. The dimensions and specifications of the preform 20, for example, the thicknesses of the first layer 15 and the second layer 16, can be appropriately changed according to the shape of the container 10 to be manufactured. It is preferable that the axial length of the entire preform 20 (the length from the upper end of the neck 22 to the lower end of the second layer 16 of the bottom 24) is set longer than that of the container 10. The gate portion (the mark where the material of the second layer 16 is introduced) extending downward from the bottom 24 may be removed before blow molding.

[0023] (Explanation of container manufacturing equipment) 4 is a diagram showing a schematic configuration of the blow molding apparatus 30 of the first embodiment. The blow molding apparatus 30 of the first embodiment is an example of a container manufacturing apparatus, and employs a hot parison method (also called a one-stage method) in which the container is blow-molded by utilizing the heat (internal heat) retained during injection molding without cooling the preform 20 to room temperature.

[0024] The blow molding apparatus 30 includes a first injection molding section 31, a first temperature adjustment section 32, a second injection molding section 33, a second temperature adjustment section 34, a blow molding section 35, a take-out section 36, and a conveying mechanism 37. The first injection molding section 31, the first temperature adjustment section 32, the second injection molding section 33, the second temperature adjustment section 34, the blow molding section 35, and the take-out section 36 are disposed at positions rotated by a predetermined angle (for example, 60 degrees) around the conveying mechanism 37. The blow molding apparatus 30 may be configured so as to omit the first temperature adjustment section 32.

[0025] (Transport mechanism 37) The transport mechanism 37 includes a transfer plate 37a that moves so as to rotate about an axis perpendicular to the plane of the drawing in Fig. 4. At least one neck mold 37b (not shown in Fig. 1) that holds the neck portion 22 of the preform 20 (or the neck portion 12 of the container 10) is disposed at each predetermined angle on the transfer plate 37a. The transport mechanism 37 moves the transfer plate 37a by 60 degrees at a time, thereby transporting the preform 20 (or the container 10) with the neck portion 22 held by the neck mold 37b to the first injection molding section 31, the first temperature adjustment section 32, the second injection molding section 33, the second temperature adjustment section 34, the blow molding section 35, and the removal section 36 in that order. When the first temperature adjustment section 32 is omitted from the blow molding apparatus 30, the conveying mechanism 37 moves the transfer plate 37a by 72 degrees at a time to convey the preform 20 (or container 10) through the first injection molding section 31, the second injection molding section 33, the second temperature adjustment section 34, the blow molding section 35, and the removal section 36 in that order. In addition, the conveying mechanism 37 further includes a lifting mechanism (vertical mold opening and closing mechanism) and a mold opening mechanism for the neck mold 37b, and performs operations related to raising and lowering the transport plate 37a, as well as operations related to mold closing and mold opening (mold release) in the injection molding section 31, etc.

[0026] (First injection molding section 31) The first injection molding section 31 includes an injection cavity mold 40, an injection core mold 41, and a hot runner mold 42, and produces an intermediate molded body 20A of the preform 20. As shown in Fig. 4, the first injection molding section 31 is connected to a first injection device 38 that supplies a resin material (first resin material) for forming the first layer 15 to the hot runner mold 42.

[0027] 5(a) shows the injection molding process in the first injection molding section 31. In the first injection molding section 31, the injection cavity mold 40, the injection core mold 41, and the neck mold 37b of the transport mechanism 37 are closed to form a mold space for the first layer 15. Then, a first resin material is poured into the mold space from the first injection device 38 via a hot runner mold 42, whereby an intermediate molded body (single-layer preform) 20A corresponding to the first layer 15 is manufactured in the first injection molding section 31.

[0028] Here, the first resin material is a thermoplastic synthetic resin, and can be appropriately selected according to the specifications of the container 10. Specific types of materials include, for example, PET (polyethylene terephthalate), PEN (polyethylene naphthalate), PCTA (polycyclohexane dimethylene terephthalate), Tritan (Tritan (registered trademark): a copolyester manufactured by Eastman Chemical Co.), PP (polypropylene), PE (polyethylene), PC (polycarbonate), PES (polyethersulfone), PPSU (polyphenylsulfone), PS (polystyrene), COP / COC (cyclic olefin polymer), PMMA (polymethyl methacrylate: acrylic), and PLA (polylactic acid). In addition, additives such as coloring agents may be added to the first resin material. Although not particularly limited, in consideration of the translucency and low material cost, it is preferable to apply PET as the first resin material.

[0029] Incidentally, even when the first injection molding section 31 is opened, the neck mold 37b of the transport mechanism 37 is not opened and continues to hold and transport the intermediate molded body 20A. The number of intermediate molded bodies 20A that are molded simultaneously in the first injection molding section 31 (i.e., the number of containers 10 that can be molded simultaneously by the blow molding device 30) can be set appropriately.

[0030] (First temperature adjustment section 32) The first temperature adjustment section 32 is equipped with a temperature adjustment mold (a heating pot or temperature adjustment pot (temperature adjustment pot) that adjusts the temperature of the intermediate molded body 20A from the outside, and a heating rod, temperature adjustment rod (temperature adjustment rod) or air introduction rod that adjusts the temperature of the preform 20 from the inside) not shown. The first temperature adjustment section 32 cools (or heats) the intermediate molded body 20A, which is in a high temperature state after injection molding, by placing it in a temperature adjustment mold that is kept at a predetermined temperature. The first temperature adjustment section 32 also has the function of adjusting the temperature distribution of the intermediate molded body 20A to a predetermined state before it is transported to the second injection molding section 33.

[0031] (Second injection molding section 33) The second injection molding section 33 includes an injection cavity mold 50, an injection core mold 51, and a hot runner mold 52, and injection molds the second layer 16 onto the outer periphery of the first layer 15. As shown in Fig. 4, the second injection molding section 33 is connected to a second injection device 39 that supplies a resin material (second resin material) for forming the second layer 16 to the hot runner mold 52.

[0032] FIG. 5( b ) shows the injection molding process in the second injection molding section 33 . The injection cavity mold 50 of the second injection molding section 33 accommodates the intermediate molded body 20A injection molded in the first injection molding section 31. When the second injection molding section 33 is in a closed state, a mold space is formed between the inner surface of the injection cavity mold 50 and the body part of the intermediate molded body 20A, which is the first layer 15, from the outer periphery side of the body to the bottom. The second resin material is filled into the mold space from the second injection device 39 via the hot runner mold 52, so that the second layer 16 is molded on the outer periphery of the intermediate molded body 20A, which is the first layer 15. As a result, the second layer 16 is laminated on the outer periphery side of the first layer 15, and the preform (multilayer preform, two-layer preform) 20 of FIG. 3 is manufactured.

[0033] The second resin material is a thermoplastic synthetic resin, and the specific type of material is the same as that of the first resin material. The composition of the second resin material may be the same as or different from that of the first resin material. For example, the first layer 15 and the second layer 16 may use the same resin material, or different materials. In addition, for example, the amount and type of coloring material may be changed in each material of the first layer 15 and the second layer 16. Although not particularly limited, it is preferable to use PET as the second resin material in consideration of the translucency and low material cost.

[0034] (Second temperature adjustment section 34) The second temperature adjustment section 34 is equipped with a temperature adjustment mold (a heating pot or temperature adjustment pot (temperature adjustment pot) for adjusting the temperature of the preform 20 from the outside, and a heating rod, temperature adjustment rod (temperature adjustment rod) or air introduction rod for adjusting the temperature of the preform 20 from the inside) not shown. The second temperature adjustment section 34 uses the temperature adjustment mold to equalize the temperature of the injection-molded preform 20 and remove any temperature deviations, and adjusts the temperature of the preform 20 to a temperature suitable for blow molding (for example, about 90°C to 105°C) and to a temperature distribution suitable for the container shape to be formed. The second temperature adjustment section 34 also has the function of cooling the preform 20 in a high-temperature state after injection molding.

[0035] (Blow molding section 35) The blow molding section 35 performs blow molding on the preform 20 whose temperature has been adjusted in the second temperature adjustment section 34, to manufacture the container 10. Fig. 6 shows the blow molding process in the blow molding section 35. The blow molding section 35 includes a blow cavity mold 60, a bottom mold 61, a stretch rod 62, and an air introduction member (blow core) 63.

[0036] The blow cavity mold 60 is a pair of split molds that determine the shape of the container 10 excluding the bottom surface. The blow cavity mold 60 is divided by a parting surface (not shown) along the vertical direction in FIG. 6, and is configured to be openable and closable in the left-right direction in FIG. 6. The bottom mold 61 is disposed below the blow cavity mold 60, and is a molding material that determines the shape of the bottom surface of the container 10. The blow cavity mold 60 and the bottom mold 61 are closed to form a mold space that determines the shape of the container 10.

[0037] The stretch rod 62 and the air introduction member (blow core) 63 are configured to be movable axially forward and backward relative to the neck mold 37b that holds the preform 20. The stretch rod 62 presses the bottom 24 of the preform 20 from the inside, and performs longitudinal stretching of the preform 20 as necessary.

[0038] A pressing piece 64 is attached to the tip of the stretching rod 62, which has a convex portion having a shape corresponding to the three-dimensional pattern 17 and transfers the shape of the three-dimensional pattern 17 to the bottom 14 of the container 10. In order to insert the pressing piece 64 into the preform 20, the outer diameter of the pressing piece 64 is set smaller than the inner diameter of the mouth 21 (or the body 23 or the bottom 24) of the preform 20. From the viewpoints of forming the three-dimensional pattern 17 over a wide range on the inner surface of the preform 20 and mitigating stress concentration due to the pressing of the pressing piece 64, it is preferable that the outer diameter of the pressing piece 64 be 2 / 3 or more and 4 / 5 or less of the inner diameter of the mouth 21 (or the body 23 or the bottom 24) of the preform 20.

[0039] In addition, in order to avoid interference between the air introduction member (blow core) 63 and the pressing piece 64 when the stretch rod 62 is raised and then retreated after blow molding, it is preferable that the diameter of the pressing piece 64 be set smaller than the inner diameter of the air introduction member (blow core) 63.

[0040] When inserted into the neck mold 37b, the air introduction member 63 comes into close contact with the inner periphery of the neck portion 22 of the preform 20, and keeps the preform 20 (or the container 10) airtight. The air introduction member 63 also introduces blow air supplied from a compressor (not shown) into the preform 20 during blow molding.

[0041] In the blow molding section 35, the preform 20 is accommodated in a mold space formed by a blow cavity mold 60 and a bottom mold 61. In the blow molding section 35, the preform 20 is stretched by a stretch rod 62 while blow air from an air introduction member 63 is introduced into the preform 20. In this way, the blow molding section 35 can shape the preform 20 to the shape of the mold space to manufacture the container 10. The shape of the three-dimensional pattern 17 is transferred to the inner surface side of the bottom 14 of the container 10 by the pressing piece 64 of the stretch rod 62.

[0042] There are cases where the length of the container 10 is approximately the same as the length of the preform 20 or is shorter than the length of the preform 20 (when the longitudinal axis stretch ratio of the preform to the container is 0.8 to 1.2 (especially when it is 0.9 to 1.1)). In the above case, it does not matter which of the pressing piece 64 descends and the bottom mold 61 ascends. In other words, either the pressing piece 64 or the bottom mold 61 may come into contact with the preform 20 first. The bottom 24 of the preform 20 is sandwiched and pressed between the bottom mold 61 and the pressing piece 64, thereby forming a container. 10 A three-dimensional pattern is transferred to the inner bottom surface (or the outer bottom surface, as described below) of the container.

[0043] (Removal part 36) The removal section 36 is configured to release the neck portion 12 of the container 10 manufactured in the blow molding section 35 from the neck mold 37 b , and remove the container 10 to the outside of the blow molding apparatus 30 .

[0044] (Explanation of container manufacturing method) Next, a method for manufacturing a container using the blow molding apparatus 30 of this embodiment will be described. Fig. 7 is a flow chart showing the steps of the method for manufacturing a container.

[0045] (Step S101: First injection molding process) First, the first injection molding section 31 injects a resin material from the first injection device 38 into a mold space of the intermediate molded body 20A formed by the injection cavity mold 40, the injection core mold 41, and the neck mold 37b of the transport mechanism 37. This produces the intermediate molded body 20A corresponding to the first layer 15 of the preform 20, as shown in Fig. 5(a).

[0046] When the injection molding of the first layer 15 is completed, the first injection molding section 31 is opened and the intermediate molded body 20A is released from the injection cavity mold 40 and the injection core mold 41. Next, the transfer plate 37a of the transport mechanism 37 moves so as to rotate by a predetermined angle.

[0047] As a result, the intermediate molded body 20A held in the neck mold 37b is transported to the first temperature adjustment section 32 while containing the heat retained during injection molding. At this time, the intermediate molded body 20A is exposed to air while being transported from the first injection molding section 31 to the first temperature adjustment section 32. As a result, the intermediate molded body 20A is slightly cooled from the outer surface, and temperature equalization progresses due to heat exchange (thermal conduction) between the skin layer (surface layer in a solidified state) and the core layer (internal layer in a softened or molten state).

[0048] (Step S102: First temperature adjustment process) Next, in the first temperature adjustment section 32, the intermediate molded body 20A is placed in a temperature adjustment mold, and the first layer 15 The first temperature adjustment step is for cooling the intermediate molded body 20A and adjusting the temperature distribution (uniform temperature and removal of uneven temperature). The first temperature adjustment step is for uniform temperature by heat exchange (thermal conduction) between the skin layer and the core layer. The first temperature adjustment step may be omitted.

[0049] After the first temperature adjustment step (or the first injection molding step), the transfer plate 37a of the transport mechanism 37 moves so as to rotate by a predetermined angle, and the temperature-adjusted intermediate molded body 20A held in the neck mold 37b is transported to the second injection molding section 33. The intermediate molded body 20A is exposed to air while being transported from the first temperature adjustment section 32 to the second injection molding section 33, so that the outer surface is cooled slightly and the temperature is uniformed by heat exchange (thermal conduction) between the skin layer and the core layer.

[0050] (Step S103: Second injection molding process) Next, in the second injection molding section 33, the intermediate molded body 20A is accommodated inside the injection cavity mold 50, and then a resin material is injected from the second injection device 39 between the outer periphery of the intermediate molded body 20A and the injection cavity mold 50. As a result, a second layer 16 is formed on the outer periphery of the intermediate molded body 20A as shown in Fig. 5(b), and the preform 20 is manufactured.

[0051] When the injection molding of the second layer 16 is completed, the second injection molding section 33 is opened and the preform 20 is released from the injection cavity mold 50 and the injection core mold 51. Next, the transfer plate 37a of the transport mechanism 37 moves so as to rotate by a predetermined angle. As a result, the preform 20 held by the neck mold 37b is transported to the second temperature adjustment section 34 while retaining the heat retained during the injection molding.

[0052] (Step S104: Second temperature adjustment process) Next, in the second temperature adjustment section 34, the preform 20 is housed in a temperature adjustment mold, and temperature adjustment is performed to bring the temperature of the preform 20 close to a temperature suitable for the final blow.

[0053] After the second temperature adjustment step, the transfer plate 37a of the transport mechanism 37 moves so as to rotate by a predetermined angle, and the preform 20 after temperature adjustment held by the neck mold 37b is transported to the blow molding section .

[0054] (Step S105: Blow molding process) Next, in the blow molding section 35, the container 10 is blow molded. First, the blow cavity mold 60 is closed to accommodate the preform 20 in the mold space, and the air introduction member 63 is lowered to abut against the neck portion 22 of the preform 20. Then, the stretch rod 62 is lowered to press the bottom portion 24 of the preform 20 from the inside, and vertical axis stretching is performed as necessary (FIG. 6(a)).

[0055] Then, the preform 20 is horizontally stretched by supplying blow air from the air introduction member 63 (FIG. 6(b)). As a result, the preform 20 is bulged and shaped so as to fit closely into the mold space of the blow cavity mold 60, and is blow molded into the container 10. If the preform 20 is longer than the container 10, the bottom mold 61 may be made to wait at a lower position where it does not come into contact with the bottom 24 of the preform 20 before the blow cavity mold 60 is closed, and then quickly raised to the molding position after the mold is closed.

[0056] During blow molding, the pressing piece 64 of the stretch rod 62 comes into contact with the bottom 24 of the preform 20 , so that the shape of the three-dimensional pattern 17 is transferred to the inner surface side of the bottom 14 of the container 10 .

[0057] As described above, the bottom mold 61 may be brought into contact with the preform 20 and then the stretch rod 62 may be lowered to press the pressing piece 64 against the preform 20 .

[0058] (Step S106: container removal process) When the blow molding is completed, the blow cavity mold 60 and the bottom mold 61 are opened, thereby making it possible to remove the container 10 from the blow molding section 35. Next, the transfer plate 37a of the conveying mechanism 37 moves so as to rotate a predetermined angle, and the container 10 is conveyed to the removal section 36. In the removal section 36, the neck portion 12 of the container 10 is released from the neck mold 37b, and the container 10 is removed to the outside of the blow molding apparatus 30.

[0059] This completes one cycle in the method for manufacturing a container. Thereafter, the transfer plate 37a of the conveying mechanism 37 is moved so as to rotate by a predetermined angle, and the above steps S101 to S105 are repeated. During operation of the blow molding apparatus 30, six sets of containers (five sets when the first temperature adjustment step is omitted) are manufactured in parallel, with a time difference between each step.

[0060] In addition, due to the structure of the blow molding apparatus 30, the times for the first injection molding process, the second injection molding process, the temperature adjustment process, the blow molding process, and the container removal process are all the same. Similarly, the transport times between each process are also the same.

[0061] The effects of the first embodiment will be described below. In the first embodiment, in order to blow mold a thick-walled container 10 suitable for a cosmetic container or the like, a preform 20 having a thick bottom 24 is manufactured in two injection molding steps. Then, in the blow molding step, a three-dimensional pattern 17 is formed on the inner surface of the bottom 14 of the container 10 by the pressing piece 64 of the stretching rod 62.

[0062] Generally, the heat capacity of a preform increases in proportion to its thickness, so the thicker the part, the more likely the preform is to deform. Therefore, when a preform with a thick part is molded in one injection molding and a three-dimensional pattern is transferred to the thick part, when the thick part is stretched by blow molding, for example, the thick part is likely to be unable to maintain a predetermined thickness or the inner surface of the thick part is likely to become uneven. Furthermore, since the thick part is likely to suffer from insufficient cooling, molding defects such as sink marks, bubbles, and whitening (crystallization) may occur in the three-dimensional pattern (or the thick part where the three-dimensional pattern is formed).

[0063] For example, when the material is PET, the maximum thickness of the preform that can suppress defects such as whitening is limited to about 9 mm. Therefore, when a container is molded from the preform, the preform is stretched slightly (at least in the horizontal direction), so the thickness of the bottom of the container will be at most a value below the maximum thickness mentioned above (for example, about 5 mm).

[0064] In contrast, in the first embodiment, the preform 20 is injection molded in two separate steps as described above, and the second layer 16 is laminated on the intermediate molded body 20A that is exposed to air during transportation and has its temperature adjusted. As a result, the preform 20 of the first embodiment can reduce the internal heat retention, even though the bottom 24 is thick, compared to a preform manufactured in a single injection molding process. This makes it easier to adjust the amount of deformation of the thick bottom 24 in the blow molding process, and the three-dimensional pattern 17 can be formed accurately on the bottom 14 of the container 10.

[0065] Furthermore, part of the thick bottom of the container (specifically, the central region of the bottom) is recessed and made thin by the length of the three-dimensional pattern of the pressing piece 64. Since the distance between the inside (core layer) of the central region of the thick bottom, which has the most heat and is the most difficult to cool during blow molding, and the bottom mold surface is shortened, the cooling efficiency of the bottom of the container can be improved and whitening of the bottom of the container can be easily suppressed.

[0066] In addition, in the first embodiment, the preforms injected in the first and second injection molding steps are thinner than when a thick preform is molded in a single injection molding step, and the difficulty of injection molding is reduced. Furthermore, parameters such as the cooling time in each injection molding step can be adjusted separately. Therefore, in the first embodiment, a thick preform 20 suitable for the specifications of the container 10 can be easily molded, and the quality of the container 10 can be improved.

[0067] For example, even if the thicknesses of the first and second layers formed in the first and second injection molding processes are each 8 mm, the bottom thickness of the preform can be formed to 16 mm while suppressing whitening, and the bottom of the container can be easily formed to a thickness of about 10 mm (excluding the portion where the three-dimensional pattern is formed).

[0068] Furthermore, in the first embodiment, the injection and cooling times of the first and second injection molding steps are both shorter than the injection and cooling times required to mold a thick-walled preform in a single injection molding step. This shortens the injection and cooling times of the preform, which are the rate-limiting steps, and therefore shortens the molding cycle when manufacturing a thick-walled container 10 suitable for cosmetic containers and the like.

[0069] In this embodiment, since the preform 20 is manufactured by two injection molding steps, it is possible to make the first layer 15 and the second layer 16 of the preform 20 have different colors. By providing the container 10 with a three-dimensional pattern 17, the design of the container 10 can be further improved.

[0070] <Second embodiment> Next, a second embodiment will be described. Figures 8 and 9 are diagrams showing a container 10A according to the second embodiment. In the following description, the same elements as those in the first embodiment are designated by the same reference numerals, and duplicated description will be omitted.

[0071] As shown in Figures 8 and 9, in the second embodiment, a three-dimensional pattern 17A, which is an example of a three-dimensional pattern, is applied to the outer surface of the bottom 14 of the container 10A. The three-dimensional pattern 17A is a depression that is concave upward from the outer surface of the container of the bottom 14 toward the inside of the bottom 14, and is formed in a shape that imitates the appearance of a mountain, for example. The other configurations of the container 10A are the same as those of the first embodiment.

[0072] The method of manufacturing the container 10A of the second embodiment is the same as that of the first embodiment, except for the blow molding step. Fig. 10 shows the blow molding step in the blow molding section 35 of the second embodiment.

[0073] In the second embodiment, a convex portion 65 having a shape corresponding to the three-dimensional pattern 17A is formed on the upper surface of the bottom mold 61 facing the preform 20. The stretch rod 62 shown in Fig. 10 has a tip piece 64a with a flat tip attached to its tip. Unlike the pressing piece 64 described above, the tip piece 64a does not transfer the shape of the three-dimensional pattern. However, if it is desired to add a three-dimensional pattern to the inner surface side of the bottom 14 as well, the pressing piece 64 that transfers the shape of the three-dimensional pattern may be attached to the stretch rod 62.

[0074] In the blow molding section 35 of the second embodiment, after the air introduction member 63 is brought into contact with the neck portion 22 of the preform 20, the stretch rod 62 descends and the bottom mold 61 rises (FIG. 10(a)). As a result, the bottom portion 24 of the preform 20 is pressed against the bottom mold 61 having a convex portion 65 on the upper surface side.

[0075] When the blow air from the air introduction member 63 is introduced into the preform 20, the preform 20 is bulged and shaped so as to fit closely into the mold space of the blow cavity mold 60, and is blow molded into the container 10A. The shape of the three-dimensional pattern 17A is transferred to the outer surface side of the bottom 14 of the container 10A by the convex portion 65 of the bottom mold 61. In the second embodiment described above, substantially the same effects as in the first embodiment can be obtained.

[0076] The present invention is not limited to the above-described embodiment, and various improvements and design changes may be made without departing from the spirit of the present invention.

[0077] In the above embodiment, an example has been described in which a three-dimensional pattern is formed on either the inner surface side or the outer surface side of the thick-walled bottom of the container. However, in the present invention, a three-dimensional pattern may be formed on both the inner surface side and the outer surface side of the thick-walled bottom of the container.

[0078] In the above embodiment, an example was described in which the second layer was laminated on the outside of the first layer in the second injection molding step to manufacture a preform. However, in the present invention, the second layer may be laminated on the inside of the first layer in the second injection molding step to manufacture a preform. In this case, in the first injection molding step, a thin film portion is formed in the center of the bottom of the intermediate molded body by pressing with a pin or the like. Then, in the second injection molding step, the thin film portion is broken by injecting resin, and the resin is introduced into the inside of the intermediate molded body.

[0079] In addition, the embodiments disclosed herein should be considered to be illustrative and not restrictive in all respects. The scope of the present invention is defined by the claims, not the above description, and is intended to include all modifications within the meaning and scope of the claims. [Explanation of symbols]

[0080] Reference Signs List 10, 10A...container, 12...neck, 13...body, 14...bottom, 15...first layer, 16...second layer, 17, 17A...three-dimensional pattern, 20...preform, 20A...intermediate molded body, 22...neck, 23...body, 24...bottom, 30...blow molding device, 31...first injection molding section, 32...first temperature adjustment section, 33...second injection molding section, 34...second temperature adjustment section, 35...blow molding section, 38...first injection device, 39...second injection device, 61...bottom mold, 62...stretching rod, 64...pressure piece, 65...projection

Claims

1. A first injection molding process for injection molding a bottomed cylindrical resin intermediate molded body using a first injection mold; a second injection molding step of injection-molding a resin material into the intermediate molded body using a second injection mold different from the first injection mold to produce a multi-layer preform having a bottom portion thicker than a body portion and having a bottom portion thicker than the intermediate molded body by laminating resin layers; and a blow molding step of blow molding the multilayer preform while the multilayer preform has the heat retained during injection molding to produce a resin container, In the blow molding process, at least one surface of the bottom of the multilayer preform is pressed with a metal mold, a three-dimensional pattern corresponding to the metal mold is transferred to the thick-walled bottom of the resin container, and a protrusion of the three-dimensional pattern provided on the metal mold promotes cooling within the wall surface of the thick-walled bottom. A method for manufacturing a resin container.

2. The die is attached to the tip of a stretch rod, The three-dimensional pattern is transferred to the inner surface of the thick bottom of the container. The method for producing the resin container according to claim 1.

3. The outer diameter of the mold is at least 2 / 3 of the inner diameter of the multilayer preform. The method for producing the resin container according to claim 2.

4. The mold is a bottom mold facing the bottom outer periphery of the multilayer preform, The three-dimensional pattern is transferred to the outer surface of the thick bottom of the container. The method for producing a resin container according to any one of claims 1 to 3.

5. The thickness of the bottom of the resin container is 10 mm or more. The method for producing a resin container according to any one of claims 1 to 4.

6. A first injection molding section that uses a first injection mold to injection mold a bottomed cylindrical resin intermediate molded body; a second injection molding section that uses a second injection mold different from the first injection mold to injection mold a resin material into the intermediate molded body, and produces a multi-layer preform having a bottom portion thicker than a body portion by laminating resin layers, the bottom portion being thicker than the intermediate molded body; a blow molding section for blow molding the multilayer preform while the multilayer preform has the heat retained during injection molding to manufacture a resin container, The blow molding section presses at least one surface of the bottom of the multilayer preform with a metal mold, transfers a three-dimensional pattern corresponding to the metal mold to the thick-walled bottom of the resin container, and promotes cooling within the wall surface of the thick-walled bottom with a protrusion of the three-dimensional pattern provided on the metal mold. Plastic container manufacturing equipment.

Citation Information

Patent Citations

  • JP1975035676A

  • Forming method for vessel in polyethylene terephthalate

    JP1981166027A

  • Manufacture of hollow molded article

    JP1993169521A

  • Temperature control apparatus for preforms, temperature control method for preforms, resin container and method for producing resin container

    WO2013012067A1

  • Preform, resin-made container, and manufacturing method therefor

    WO2020251035A1