Method for identifying individual fiber-reinforced plastics
The method uses unique appearance information of fiber-reinforced plastics to identify and track products without expensive marking devices, addressing the limitations of existing methods.
Patent Information
- Application Number
- JP2023516446
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2021-04-20
- Filing Date
- 2022-04-08
- Publication Date
- 2024-11-20
- Estimated Expiration
- 2042-04-08
AI Technical Summary
Existing methods for identifying fiber-reinforced plastics require expensive dedicated marking devices and cannot effectively track products after shipment, especially those with good appearance or same-type differentiation.
A method for recognizing individual fiber-reinforced plastics using unique appearance information, such as randomly arranged discontinuous fibers, without the need for expensive marking devices, by creating a database of identification information images and comparing them with acquired images.
Enables individual identification of fiber-reinforced plastics without dedicated marking equipment, allowing tracking even after shipment, based on unique patterns.
Smart Images

Figure 0007587690000001 
Figure 0007587690000002 
Figure 0007587690000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for recognizing individual pieces of fiber-reinforced plastic based on a captured image of the fiber-reinforced plastic. [Background technology]
[0002] Conventionally, fiber reinforced plastics have been individually authenticated by printing a QR code (registered trademark) on the surface of the fiber reinforced plastic using laser marking, and reading this with a scanner, as in the invention described in Patent Document 1. The QR code (registered trademark) contains product information held by the fiber reinforced plastic.
[0003] On the other hand, as a method for authenticating an individual object, for example, Patent Document 2 describes an invention relating to an object identification device equipped with an image processing means that captures images of two or more objects placed on the same plane by an imaging means in order to identify the objects, and identifies the type of the objects by performing image recognition on the images.
[0004] Patent Document 3 provides a medical materials recognition system that can easily and quickly recognize medical materials and can be used for accurate counting and management.
[0005] In Patent Document 4, individual sintered products are identified in order to understand the manufacturing conditions and to facilitate investigation of the cause of defects. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] International Publication No. 2015 / 137093 [Patent Document 2] Japanese Patent Publication No. 2012-198848 [Patent Document 3] Japanese Patent Application Publication No. 2019-168765 [Patent Document 4] Japanese Patent Application Publication No. 2013-232069 Summary of the Invention [Problem to be solved by the invention]
[0007] However, the laser marking described in Patent Document 1 requires an expensive dedicated marking device. In addition, since marking processing traces (e.g., QR code (registered trademark)) are left on part of the product, it is difficult to apply this method to products where appearance is important.
[0008] The individual authentication described in Patent Document 2 can recognize different types of bread, but cannot distinguish between bread of the same type, and therefore cannot be used for tracking products after they are shipped.
[0009] The medical material recognition system described in Patent Document 3 identifies the type of medical material from characteristics such as characters and figures intentionally and explicitly given to the packaging material, but cannot identify the product itself without packaging. In addition, since it cannot distinguish between medical materials of the same type, it cannot be used to track products after they are shipped.
[0010] The individual identification method described in Patent Document 4 does not use fiber-reinforced plastics, and consideration of individual recognition of fiber-reinforced plastics is insufficient.
[0011] In view of the problems associated with the prior art, the present invention aims to provide a method for identifying individual fiber-reinforced plastics that does not require expensive dedicated marking equipment or other processing for identification, and that does not require such equipment. [Means for solving the problem]
[0012] As a result of extensive investigations, the present inventors have found that the above problems can be solved by the means described below, and have arrived at the present invention.
[0013] 1. A method for identifying individual fiber-reinforced plastics, comprising the following steps: Step 101: A step of obtaining identification information of a fiber reinforced plastic in advance, obtaining an identification information image P1, and creating a database in which product information of the fiber reinforced plastic is associated and stored; Step 201. After step 101, acquiring identification information of the fiber-reinforced plastic to acquire an identification information image P2; Step 301: A step of performing individual recognition of fiber reinforced plastics by comparing the acquired identification information image P2 with the identification information image P1 stored in the database; However, the resin M1 contained in the fiber reinforced plastic product of step 101 has a larger number average molecular weight than the resin M2 contained in the fiber reinforced plastic product of step 201.
[0014] 2. The method for identifying individual fiber-reinforced plastics described in 1 above, wherein the product information includes at least one of fiber length, fiber volume fraction, fiber brand, resin brand, manufacturing date, manufacturing time, or product serial number. 3. The fiber-reinforced plastic in step 101 is a molding material, The fiber-reinforced plastic in step 201 is a molded body, and the molded body is obtained by compression molding a molding material; 3. A method for identifying individual fiber-reinforced plastics according to any one of 1 and 2 above. 4. The compression molding is cold press molding using a mold having an upper mold and a lower mold, The identification information is a surface image of the fiber-reinforced plastic on the side that contacts the lower die. 4. The individual recognition method according to claim 3. 5. The individual recognition method according to 4, A method for identifying an individual, wherein identification information is present in a non-flowing or low-flowing area.
[0015] 6. The surface of the fiber-reinforced plastic has discontinuous fibers arranged randomly, 6. The method for identifying individual fiber-reinforced plastics according to any one of 1 to 5, wherein the randomly arranged discontinuous fibers are acquired as the identification information. 7. The discontinuous fibers include discontinuous fiber bundles A1, and the identification information image P1 indicates that the area of the discontinuous fiber bundles A1 is 2000 mm 2 The method for identifying individual fiber-reinforced plastics according to 6 above, further comprising the steps of: 8. A method for identifying individual fiber-reinforced plastics as described in any one of claims 1 to 7, wherein the identification information image is non-destructive testing data. 9. A method for recognizing individual fiber-reinforced plastics described in any one of claims 1 to 8, wherein line scan lighting or dome lighting is used when imaging the identification information of the fiber-reinforced plastic. 10. A method for evaluating the degree of deterioration of a resin contained in a fiber-reinforced plastic, after performing individual recognition using the method for recognizing individual fiber-reinforced plastics described in any one of 1 to 9 above. Effect of the Invention
[0016] The method for identifying individual fiber-reinforced plastics of the present invention is based on the unique appearance information possessed by fiber-reinforced plastics, so there is no need for expensive dedicated marking equipment or processing and equipment for identification.
[0017] Furthermore, the present invention recognizes the unique patterns possessed by fiber-reinforced plastics, even for products of the same brand, making it possible to identify individual products and track products after shipment. [Brief description of the drawings]
[0018] [Figure 1] Schematic diagram of fiber-reinforced plastic in which the reinforcing fibers are discontinuous and randomly arranged in two dimensions. [Diagram 2] FIG. 3 is a schematic diagram showing the molding material turned into a molded body. [Diagram 3] Schematic diagram showing a molded product before and after distribution. [Figure 4] A schematic diagram showing that when cold-pressed, the inside of the molding material flows and the molding material flows out to the periphery of the molding material that was initially placed. [Diagram 5](a) Schematic diagram showing the molding material placed in the mold and the upper die being lowered (no pressure is being applied). (b) Schematic diagram showing the upper die being closed and pressure being applied to the molding material. [Figure 6] (a) Image of the surface of a fiber-reinforced plastic using ring lighting. (b) Image of the surface of a fiber-reinforced plastic using dome lighting. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0019] Hereinafter, embodiments of the present invention will be described with reference to the drawings, but the present invention is not limited to these.
[0020] [Reinforced fiber] 1. Types The fiber reinforced plastic of the present invention contains reinforcing fibers. Although there is no particular limitation on the reinforcing fibers, the reinforcing fibers are preferably one or more reinforcing fibers selected from the group consisting of carbon fibers, glass fibers, aramid fibers, boron fibers, and basalt fibers.
[0021] When PAN-based carbon fibers are used as reinforcing fibers, their tensile modulus is preferably within the range of 100 to 600 GPa, more preferably within the range of 200 to 500 GPa, and even more preferably within the range of 230 to 450 GPa, and their tensile strength is preferably within the range of 2000 to 6000 MPa, and more preferably within the range of 3000 to 6000 MPa.
[0022] 2. Discontinuous Fibers The reinforcing fibers preferably contain discontinuous fibers. When discontinuous fibers are used, the formability is improved compared to fiber-reinforced plastics using only continuous fibers, and it becomes easier to produce complex molded articles.
[0023] 3. Weight average fiber length of reinforcing fibers The reinforcing fibers used in the present invention are discontinuous reinforcing fibers, and may have a weight-average fiber length of 1 to 100 mm. The weight-average fiber length of the discontinuous reinforcing fibers is more preferably 3 to 80 mm, and even more preferably 5 to 60 mm. If the weight-average fiber length is 100 mm or less, when the fiber-reinforced plastic is used as a molding material, the fluidity of the molding material is improved, and it is easy to obtain a desired molded shape by, for example, compression molding. On the other hand, if the weight-average fiber length is 1 mm or more, the mechanical strength of the fiber-reinforced plastic is improved.
[0024] In the present invention, reinforcing fibers having different fiber lengths may be used in combination. In other words, the reinforcing fibers used in the present invention may have a single peak in the weight average fiber length, or may have multiple peaks.
[0025] The average fiber length of the reinforcing fibers can be calculated, for example, by measuring the fiber lengths of 100 fibers randomly extracted from a fiber-reinforced plastic to the nearest 1 mm using a vernier caliper or the like, and then calculating the average fiber length based on the following formula. The average fiber length is measured as the weight-average fiber length (Lw). If the fiber length of each reinforcing fiber is Li and the number of fibers measured is j, the number-average fiber length (Ln) and weight-average fiber length (Lw) can be calculated by the following formulas (c) and (d). Ln = ΣLi / j···Eq. (c) Lw = (ΣLi 2 ) / (ΣLi)···Eq. (d) When the fiber length is constant, the number average fiber length and the weight average fiber length have the same value.
[0026] Reinforcing fibers can be extracted from fiber-reinforced plastics, for example, by subjecting the fiber-reinforced plastic to a heat treatment at 500° C. for about 1 hour and removing the resin in a furnace.
[0027] 4. Fiber volume fraction The fiber volume fraction Vf of the reinforcing fibers is not particularly limited, but is preferably 20 to 70%, more preferably 25 to 60%, and even more preferably 30 to 55%. The fiber volume ratio (Vf unit: volume %) is the ratio of the volume of the reinforcing fibers to the total volume including not only the reinforcing fibers and matrix resin but also other additives.
[0028] 5. Fiber diameter When the reinforcing fiber used in the present invention is a carbon fiber, the fiber diameter of the carbon fiber is preferably in the range of 3 to 50 μm, more preferably in the range of 4 to 12 μm, and further preferably in the range of 5 to 8 μm, as the average fiber diameter. Here, the average fiber diameter refers to the diameter of a single fiber of the carbon fiber. Therefore, when the carbon fiber is in the form of a fiber bundle, it refers to the diameter of the carbon fiber (single fiber) constituting the fiber bundle, not the diameter of the fiber bundle. The average fiber diameter of the carbon fiber can be measured, for example, by the method described in JIS R-7607:2000.
[0029] When glass fibers are used as reinforcing fibers, the average fiber diameter of the glass fibers is preferably 1 μm to 50 μm, more preferably 5 μm to 20 μm. If the average fiber diameter is large, the resin can easily be impregnated into the fibers, and if it is equal to or less than the upper limit, the moldability and processability are good.
[0030] 6. Fiber bundle When the reinforcing fibers are discontinuous fibers and the fiber bundles are used by opening them, the reinforcing fibers contained in the fiber reinforced plastic may be only monofilament-like, only fiber bundle-like, or both may be mixed. When the reinforcing fibers used in the present invention are in the form of fiber bundles, the number of single fibers (also called monofilaments) constituting each fiber bundle is not particularly limited, but is usually within the range of 1,000 to 100,000. When carbon fibers are used as reinforcing fibers, they are generally in the form of fiber bundles in which several thousand to several tens of thousands of single fibers are assembled. If the carbon fibers are used as they are, the entangled portions of the fiber bundles may become locally thick, making it difficult to obtain a thin-walled impact absorbing member. For this reason, when carbon fibers are used as reinforcing fibers, the fiber bundles are usually used by widening or opening them.
[0031] More specifically, it is preferable that the reinforcing fiber bundle (A) is composed of a critical single fiber number or more defined by the following formula (a), and other opened reinforcing fibers (B), i.e., a fiber bundle composed of single fibers or less than the critical single fiber number. Critical single yarn number = 600 / D Equation (a) (where D is the average fiber diameter of the reinforcing fibers (μm))
[0032] The degree of opening of the reinforcing fibers can be controlled within a desired range by adjusting the conditions for opening the fiber bundle, such as adjusting the pressure of the air blown in the opening step.
[0033] In the present invention, when the reinforcing fibers are discontinuous fibers and the discontinuous fibers include discontinuous fiber bundles A1, the average number of fibers (N) of the discontinuous fiber bundles A1 can be appropriately determined within a range that does not impair the object of the present invention, and is not particularly limited, but it is preferable that the average number of fibers (N) satisfies the following formula (b). 0.6×10 4 / D 2 <N<6×10 5 / D 2 Formula (b) (where D is the average fiber diameter of the reinforcing fibers (μm))
[0034] Specifically, when the reinforcing fibers contained in the fiber reinforced plastic are carbon fibers and the average fiber diameter is 5 to 7 μm, the critical single fiber number is 86 to 120. When the average fiber diameter of the carbon fibers is 5 μm, the average number of fibers (N) in the carbon fiber bundle is 240 to 24,000, more preferably 300 to 10,000, and even more preferably 500 to 5,000. When the average fiber diameter of the carbon fibers is 7 μm, the average number of fibers (N) in the carbon fiber bundle is 122 to 12,200, more preferably 200 to 5,000, and even more preferably 300 to 3,000. When the average fiber diameter of the carbon fibers is 0.6×10 4 / D 2 In the above cases, it becomes easy to increase the carbon fiber volume fraction (Vf) of the fiber-reinforced plastic, and as a result, it becomes easier to obtain the desired mechanical properties. On the other hand, if the average number of fibers (N) in the carbon fiber bundle is 6 × 105 / D 2 In the following cases, locally thick portions are less likely to occur and voids are less likely to occur in the fiber reinforced plastic.
[0035] 7. Reinforcement fiber orientation The orientation state of the reinforcing fibers contained in fiber-reinforced plastics can be, for example, a unidirectional orientation in which the long axis directions of the reinforcing fibers are aligned in one direction, or a two-dimensional random orientation in which the long axis directions are aligned randomly in the in-plane direction of the molding material.
[0036] The orientation state of the reinforcing fibers in the present invention may be either the above-mentioned unidirectional arrangement or two-dimensional random arrangement. It may also be an irregular arrangement between the above-mentioned unidirectional arrangement and two-dimensional random arrangement (an arrangement state in which the long axis direction of the reinforcing fibers is not completely aligned in one direction and is not completely random). Furthermore, depending on the fiber length of the reinforcing fibers, the long axis direction of the reinforcing fibers may be aligned at an angle to the in-plane direction of the fiber-reinforced plastic, the fibers may be aligned so as to be entangled in a cotton-like manner, and further the fibers may be aligned like a bidirectional fabric such as a plain weave or twill weave, a multiaxial fabric, a nonwoven fabric, a mat, a knit, a braid, or a paper made from reinforcing fibers.
[0037] The reinforcing fibers in the present invention may be in the form of a reinforcing fiber mat. The reinforcing fiber mat refers to a mat-like shape formed by stacking or entangling reinforcing fibers. Examples of the reinforcing fiber mat include a two-dimensional random reinforcing fiber mat in which the long axis direction of the reinforcing fibers is randomly arranged in the in-plane direction of the fiber-reinforced plastic, and a three-dimensional random reinforcing fiber mat in which the long axis direction of the reinforcing fibers is randomly arranged in each of the X, Y, and Z directions by entangling the reinforcing fibers in a flocculent manner.
[0038] The orientation of the two-dimensional random arrangement of reinforcing fibers in fiber-reinforced plastics can be confirmed, for example, by performing a tensile test based on an arbitrary direction of the fiber-reinforced plastic and a direction perpendicular thereto, measuring the tensile modulus, and then measuring the ratio (Eδ) obtained by dividing the larger of the measured tensile modulus values by the smaller one. The closer the ratio of modulus of elasticity is to 1, the more the reinforcing fibers can be evaluated as being two-dimensionally randomly arranged. When the ratio obtained by dividing the larger of the modulus of elasticity values in two perpendicular directions by the smaller one does not exceed 2, the material is considered to be isotropic, and when this ratio does not exceed 1.3, the material is evaluated to have excellent isotropy.
[0039] There are no particular limitations on the method for controlling the direction of arrangement of reinforcing fibers, but specific examples include a method of using fiber bundles in the shape of the reinforcing fibers, and using an airlaid method, carding method, or papermaking method when manufacturing fiber-reinforced plastics.
[0040] [resin] In the present invention, the type of resin is not particularly limited, and a thermosetting resin or a thermoplastic resin is used. When a thermosetting resin is used, it is preferable that the resin is an unsaturated polyester resin, a vinyl ester resin, an epoxy resin, or a phenol resin. The resin may be used alone or in combination of two or more kinds.
[0041] [Sheet molding compound] The fiber reinforced plastic of the present invention may be a product obtained by molding a sheet molding compound (sometimes called SMC) using reinforcing fibers. Because of its high moldability, a sheet molding compound can be easily molded even into complicated shapes such as battery trays and battery covers.
[0042] As a fiber reinforced plastic using sheet molding compound (SMC), a sheet molding compound manufactured by Continental Structural Plastics (sometimes abbreviated as CSP) can be used.
[0043] [Other agents] The fiber reinforced resin used in the present invention may contain additives such as various fibrous or non-fibrous fillers of organic or inorganic fibers, inorganic fillers, flame retardants, UV resistance agents, stabilizers, release agents, pigments, softeners, plasticizers, surfactants, etc., within the scope of the present invention. In addition, when a thermosetting resin is used, it may contain a thickener, a curing agent, a polymerization initiator, a polymerization inhibitor, etc. As the additive, one type may be used alone, or two or more types may be used in combination.
[0044] [Individual recognition method] The method for identifying individual fiber-reinforced plastics according to the present invention includes the following steps 101, 201, and 301. Step 101: A step of obtaining identification information of a fiber reinforced plastic in advance, obtaining an identification information image P1, and creating a database in which product information of the fiber reinforced plastic is associated and stored; Step 201. After step 101, acquiring identification information of the fiber-reinforced plastic to acquire an identification information image P2; Step 301: A step of performing individual recognition of fiber reinforced plastics by comparing the acquired identification information image P2 with the identification information image P1 stored in the database; However, the resin M1 contained in the fiber reinforced plastic product of step 101 has a larger number average molecular weight than the resin M2 contained in the fiber reinforced plastic product of step 201.
[0045] Step 101 is a step of obtaining identification information of a fiber reinforced plastic in advance, obtaining an identification information image P1, and creating a database in which product information of the fiber reinforced plastic is associated and stored, but preferably, it is a step of capturing an image of identification information of a fiber reinforced plastic in advance, obtaining an identification information image P1, and creating a database in which product information of the fiber reinforced plastic is associated and stored. The identification information of the fiber reinforced plastic is preferably a surface image of the fiber reinforced plastic. The identification information of the fiber reinforced plastic is preferably an image obtained by imaging the surface of the fiber reinforced plastic. In step 101, identification information of the fiber-reinforced plastic is obtained in advance, but if the identification information is a surface image of the fiber-reinforced plastic obtained by imaging the surface of the fiber-reinforced plastic, the imaging itself may be performed by the person performing step 101 or by someone other than the person performing step 101.
[0046] Step 101 is also a stage for creating a database including n sets of data {Lot. 1...n; P1...Pn} that link fiber reinforced plastics with identification information of a certain lot and images of the identification information. In step 101, the product information of the fiber reinforced plastics is clear.
[0047] On the other hand, the identification information of the fiber reinforced plastic in step 201 is unknown. This is because it has been distributed on the market, etc. In step 201, an identification information image P2 is obtained by capturing an image of the identification information of the unknown fiber reinforced plastic, and in step 301, the identification information image P2 is compared with an identification information image in a database. If it is registered in the database, the product information of the unknown fiber reinforced plastic can be checked.
[0048] [Individual recognition method: Step 101] 1. The identification information image P1 is obtained by capturing an image of the identification information of the fiber reinforced plastic itself that is the recognition target. The imaging device for capturing images is not particularly limited, but may be, for example, a digital camera equipped with a lens, which captures the identification information of the captured fiber-reinforced plastic as electronic data of a digital image and sends the identification information image data to a computer. For example, the imaging device is set to face the identification information of the fiber-reinforced plastic and capture the entire identification information. In order to reduce extraneous light reflected or reflected by the surface of the fiber-reinforced plastic, the positions of the product, the surrounding light source, and the camera can be adjusted, or a polarizing filter that linearly polarizes the light entering the lens can be installed at the tip of the lens of the imaging device, for example, to accurately capture the identification information of the fiber-reinforced plastic. Any known computer can be used.
[0049] Illumination may be used when imaging the identification information of the fiber reinforced plastic. Examples of lighting include line scan lighting, natural light (sunlight), dome lighting (diffused light), ring lighting, and multi-angle lighting (composite of ring light shining from various directions), but line scan lighting or dome lighting is preferred, and dome lighting is particularly preferred. Line scan lighting may be used from only one direction, and images may be captured from the position of regular reflection, or may be captured slightly shifted from the position of regular reflection. For example, in the case of ring lighting or multi-angle lighting, if it is not possible to capture an image due to strong reflection, photos may be composited. Since the image obtained may differ when the fiber-reinforced plastic is rotated, it is preferable to capture the image from the same direction each time.
[0050] 2. Identification information and identification image Preferably, the identification information of the fiber-reinforced plastic is, for example, a pattern of reinforcing fibers observed on the surface of the fiber-reinforced plastic itself, as shown in Fig. 1. In other words, the surface image of the fiber-reinforced plastic itself can be used as the identification information image P1. The individual authentication of the present invention can be said to be an industrial version of fingerprint authentication, so obtaining a surface image of the fiber-reinforced plastic can be said to be equivalent to a fingerprint.
[0051] The surface of the fiber-reinforced plastic has discontinuous fibers arranged randomly, and it is preferable to image the randomly arranged discontinuous fibers as the identification information. For example, in the fiber-reinforced plastic depicted in FIG. 1, the reinforcing fibers are discontinuous and arranged randomly in two dimensions. Such fiber morphology differs from product to product, even for products of the same brand. Specifically, the characteristics of the arranged fiber bundles, such as the position, direction, thickness, and length, differ from product to product, and therefore can be used as identification information.
[0052] The discontinuous fibers include discontinuous fiber bundles A1, and the area of the discontinuous fiber bundles A1 is captured in the identification information image P1. 2 More than 4000mm is preferable. 2 More preferably, 8000mm or more. 2 It is even more preferable that the above is included.
[0053] For the identification information of the fiber reinforced plastic, it is preferable to use an image of an area of 400 mm x 400 mm as the identification information data. In this area, the area of identifiable discontinuous fiber bundles A1 is included in more than the required amount. This information may be processed and stored in a database.
[0054] In addition, the identification information image may be non-destructive inspection data and is not necessarily limited to surface observation patterns. Specifically, it includes images obtained by X-ray devices, gamma ray devices, ultrasonic devices, millimeter wave devices, microwave devices, eddy current devices, thermography, etc. Furthermore, the non-destructive inspection data is not limited to two-dimensional images, and may be configured as three-dimensional data.
[0055] 3.Product Information The product information preferably includes at least one of the following: fiber length, fiber volume ratio, fiber brand, resin brand, manufacturing date, manufacturing time, or product serial number. The manufacturing date and time and product serial number are associated with separately stored product production process data, inspection, transportation, and sales history data, and are preferably used as a traceability system that can extract all data related to each product.
[0056] 4. Database The database is created by acquiring the identification information image P1, and storing the product information of the fiber reinforced plastic corresponding to the acquired image in association with it. The database is a database that stores the identification information of a plurality of fiber reinforced plastics and the corresponding product information in association with each other, and may be stored in a storage unit of a computer.
[0057] 5. Fiber-reinforced plastics as molding materials The fiber-reinforced plastic in step 101 is preferably a molding material. The molding material is preferably one that can be compression molded to form a molded body, and the compression molding is more preferably cold press molding using a mold having an upper mold and a lower mold.
[0058] [Individual recognition method: step 201] 1. Acquisition of identification information image P2 Step 201 is a stage in which identification information of the fiber reinforced plastic is obtained again to obtain an identification information image P2 after step 101. The imaging device used may be the same as that used in step 101. In step 102, identification information of the fiber-reinforced plastic is obtained, but if the identification information is a surface image of the fiber-reinforced plastic obtained by imaging the surface of the fiber-reinforced plastic, the imaging itself may be performed by the person performing step 102 or by someone other than the person performing step 102.
[0059] 2. Fiber-reinforced plastics as molded bodies The fiber reinforced plastic in step 201 is a molded body, and the molded body is preferably obtained by compression molding a molding material.
[0060] 3. Identification information on fiber-reinforced plastics The compression molding is cold press molding using a mold having an upper mold and a lower mold, and the identification information is preferably a surface image of the fiber reinforced plastic on the side that contacts the lower mold. However, it is not necessary to image the entire fiber reinforced plastic on the side that contacts the lower mold.
[0061] In the case of cold press molding, the surface of the fiber reinforced plastic that comes into contact with the lower mold has low fluidity or is non-flowing during molding. This tendency is particularly evident when the resin of the fiber reinforced plastic is a thermoplastic resin. When cold pressing a fiber reinforced plastic (molding material) whose resin is a thermoplastic resin, the molding mold is below the plasticization temperature, so the moment the heated molding material comes into contact with the lower mold, the thermoplastic resin on the molding material surface solidifies and becomes a non-flowing region. When the fiber reinforced plastic is placed in the lower mold, the surface that first comes into contact with the lower mold is shown, for example, as 403 in FIG. 4. 401 in FIG. 4 is the lower mold, and 402 in FIG. 4 is the upper mold. The inside of the molding material remains at or above the plasticization temperature even after being placed in the lower mold, and when the upper mold descends and press pressure is applied, the inside of the fiber reinforced plastic flows and flows out to the outside of the molding material (for example, 404 in FIG. 4). Due to this outflow, a flowing region is formed in the outer peripheral region of the surface where the molding material first comes into contact with the lower mold.
[0062] A similar state is shown in Figure 5. Figure 5(a) shows the state in which the molding material is placed in the mold, and Figure 5(b) shows the state in which press pressure is being applied to the molding material. Therefore, in step 201, if the surface image of the fiber reinforced plastic on the side that contacts the lower mold is used as the identification information, it is preferable that the identification information exists in a non-flow area or a low-flow area. It is more preferable that the surface image of the fiber reinforced plastic on the side that contacts the lower mold exists in a non-flow area. If the identification information exists in this area, the fiber morphology in the identification information image P1 and the identification information image P2 will be approximately the same, making it easier to compare them in step 301.
[0063] 4. Identification during the manufacturing process The fiber reinforced plastic imaged in step 201 is preferably a molded body that has been compression molded after being manufactured in step 101. That is, the molding material 201 in Fig. 2 may be the object of image capture in step 101, and the molded body 202 after molding may be the object of image capture in step 201. Images of steps 101 and 201 may be captured at the manufacturing site of the molding material and the manufacturing site of the molded body, respectively, thereby enabling individual authentication of the fiber reinforced plastic as the molding material and the fiber reinforced plastic as the molded body.
[0064] Conventionally, fiber-reinforced plastics have been individually authenticated by printing a QR code (registered trademark) on the surface of the fiber-reinforced plastic by laser marking, as in the invention described in Patent Document 1, and reading the QR code with a scanner. The QR code (registered trademark) contains product information possessed by the fiber-reinforced plastic. However, to use the laser marking described in Patent Document 1, an expensive dedicated marking device is required. In addition, since the marking processing trace (e.g., QR code (registered trademark)) is left on a part of the product, it is difficult to apply to products where appearance is required. Furthermore, when a molding material containing a thermoplastic resin is used for the fiber-reinforced plastic, the resin is heated in the molding process and the marking disappears. In other words, it becomes necessary to re-apply the product information associated at the manufacturing site of the molding material at the manufacturing site of the molded body. If the individual recognition method of fiber-reinforced plastic of the present invention is used, it is based on the unique identification information possessed by the fiber-reinforced plastic, so there is no need for an expensive dedicated marking device, or processing for identification and the device for that purpose. In addition, there is no need to re-apply the product information associated with the molding material in the manufacturing process of the molded body.
[0065] 5. Distribution of fiber reinforced plastics The fiber reinforced plastic imaged in step 201 may be one that has been manufactured in step 101, shipped, and distributed on the market. The fiber reinforced plastic of the present invention is used in automobile parts, etc. That is, the molded product 301 in FIG. 3 may be the object of image capture in step 101, and the molded product 302 after distribution may be the object of image capture in step 201.
[0066] When distributing fiber-reinforced plastics on the market, it is preferable to provide identification information at a specific location that is not damaged by rubbing or colliding with other components during use. If damage to the surface can be avoided as much as possible, the identification information can be clearly secured for a long period of time, for example, until the product is discarded.
[0067] [Individual recognition method: Step 301] Step 301 is a stage in which the acquired identification information image P2 is compared with the identification information image P1 stored in the database to perform individual recognition of the fiber reinforced plastic.
[0068] 1. Matching The identification information image P2 and the identification information P1 stored in the database can be collated by, for example, a computer. The computer has, for example, a known computer configuration, a central processing unit, a memory, and a storage unit, and operates based on a program previously stored in the storage unit. The computer is connected to an imaging device, an input unit for a user to perform input operations, and an output unit for displaying images captured by the imaging device and a user interface of the system on a screen so as to be capable of data communication. For input to the computer, for example, a pointing device such as a mouse or a keyboard may be used. In addition, the output unit may be, for example, a device having only a screen display function such as a display, or may be a transmitting device for transmitting recognition results to other computers, peripheral devices such as a printer, etc.
[0069] The matching is a means for recognizing and identifying the fiber-reinforced plastic captured by the imaging device by matching the identification information image P2 captured by the imaging device with the identification information image P1 stored in the database. The image matching means uses a well-known image recognition technology such as feature-based matching, which performs pre-processing such as luminance averaging, hue conversion, edge detection, various filters such as Gaussian, opening, and closing, and semantic segmentation using a method such as Convolutional Neural Network to remove image noise and emphasize image features, extracts features unique to each product by a feature point extraction process such as Oriented-BRIEF, Accelerated KAZE, and Feature from Accelerated Segment Test, and identifies the pair of images with the highest degree of match, and searches for the identification information image P1 stored in the database that completely or approximately matches the identification information image P2 from the imaging device to identify the fiber-reinforced plastic.
[0070] For example, the identification information of fiber-reinforced plastics includes the shape and arrangement of fiber bundles observed on the surface of fiber-reinforced plastics. From the difference image between the identification image and the image after applying a Gaussian filter or a nonlinear diffusion filter with different smoothing scales to the identification image, the contour information (length, thickness, angle, curvature) of each fiber bundle expressed as a brightness gradient is extracted as a feature point. Furthermore, from the brightness gradient information of the pixels around each feature point, a dominant direction vector specific to each feature point and a 64-dimensional brightness gradient vector are calculated, and these are described as feature values for each feature point. After correcting the effects of image rotation, illumination, and scale changes using the feature values, the positional relationship of each feature point is compared and the degree of match of the images is calculated. For this reason, in order to perform highly accurate identification, fiber bundles of a certain area or more are required as identification information.
[0071] When there are multiple pieces of identification image information P1 with similar degrees of matching to the identification image information P1 with the highest degree of matching, multiple candidates for fiber reinforced plastics are determined as recognition results in the first stage. Next, although an auxiliary recognition means for auxiliary identification of fiber reinforced plastics using different elements may be provided, it is preferable that the matching is basically configured to match image data that more completely matches the identification information image of the fiber reinforced plastic.
[0072] However, if there is image data that is similar to the highest degree of match, the identification image information P2 may be configured to use multiple candidates from the first stage as recognition results, and then an auxiliary recognition means may be used to auxiliary identify the candidate using other elements such as user input.
[0073] [Fiber-reinforced plastics: molding materials and molded bodies] In both steps 101 and 201, the fiber-reinforced plastic to be the subject of individual recognition may be a material before it is molded to form a three-dimensional shape (hereinafter, may be referred to as a molding material), or a molded body having a three-dimensional shape obtained by molding the molding material. The molding material is a material for creating a molded body, and the molding material is molded to become a molded body. Therefore, it is preferable that the molding material has a flat plate shape. On the other hand, it is preferable that the molded body is shaped and has a three-dimensional shape. The molding is preferably compression molding, which will be described later.
[0074] However, more preferably, in step 101, the fiber-reinforced plastic imaged in advance is a molding material. Even more preferably, in step 201, the fiber-reinforced plastic imaged later is a molded body, and the molded body is obtained by compression molding the molding material.
[0075] [Compression molding] The molding material can be molded by various molding methods, preferably by applying heat and pressure, and preferably by compression molding methods such as cold press molding and hot press molding.
[0076] 1.Cold press molding When the resin contained in the fiber reinforced plastic is a thermoplastic resin, compression molding using a cold press is particularly preferable. In cold press molding, for example, a molding material heated to a first predetermined temperature is placed in a mold set to a second predetermined temperature, and then pressurized and cooled.
[0077] Specifically, when the resin constituting the molding material is a thermoplastic resin and the thermoplastic resin is crystalline, the first predetermined temperature is equal to or higher than the melting point, and the second set temperature is lower than the melting point. When the thermoplastic resin is amorphous, the first predetermined temperature is equal to or higher than the glass transition temperature, and the second set temperature is lower than the glass transition temperature. That is, the cold press molding includes at least the following steps A-1) to A-2).
[0078] A-1) A process of heating the molding material to a temperature above the melting point and below the decomposition temperature if the thermoplastic resin is crystalline, or to a temperature above the glass transition temperature and below the decomposition temperature if the thermoplastic resin is amorphous. A-2) The molding material heated in A-1) above is placed in a mold whose temperature is adjusted to below the melting point if the thermoplastic resin is crystalline, or below the glass transition temperature if the thermoplastic resin is amorphous, and then pressurized.
[0079] By carrying out these steps, the molding of the molding material can be completed. When the molding material is poured into the mold, a single sheet (one sheet) or multiple sheets are used according to the plate thickness of the target molded body. When multiple sheets are used, multiple sheets may be stacked and heated in advance, or heated molding materials may be stacked and then poured into the mold, or heated molding materials may be stacked in sequence in the mold. When stacked, the temperature difference between the molding material of the bottom layer and the molding material of the top layer is preferably small, and from this viewpoint, it is preferable to stack them before putting them into the mold. In addition, the pressurization in the above A-1) can be performed using, for example, a molding die or a nip roller. The above steps need to be performed in the above order, but other steps may be included between each step. The other steps include, for example, a shaping step in which, before A-2), a molding die other than the molding die used in A-2) is used to pre-shape the mold into the shape of the cavity of the mold.
[0080] 2.Hot press molding In hot press molding, for example, a molding material is put into a mold, pressure is applied while the temperature of the mold is raised to a first predetermined temperature, and the mold is cooled to a second predetermined temperature. Specifically, when the thermoplastic resin constituting the molding material is crystalline, the first predetermined temperature is equal to or higher than the melting point, and the second predetermined temperature is lower than the melting point. When the thermoplastic resin constituting the molding material is amorphous, the first predetermined temperature is equal to or higher than the glass transition temperature, and the second predetermined temperature is lower than the glass transition temperature. The hot press molding preferably includes at least the following steps B-1) to B-4).
[0081] B-1) A process in which the molding material is placed into the mold (lower mold). B-2) A process of applying pressure while heating the mold to a temperature above the melting point and below the thermal decomposition temperature of the thermoplastic resin if the thermoplastic resin is crystalline, or to a temperature above the glass transition temperature and below the thermal decomposition temperature of the thermoplastic resin if the thermoplastic resin is amorphous (first pressing process). B-3) A process of applying pressure in one or more stages so that the pressure in the final stage is 1.2 to 100 times the pressure in the first press process (second press process). B-4) A process for adjusting the mold temperature to below the melting point if the thermoplastic resin is crystalline, or below the glass transition temperature if the thermoplastic resin is amorphous. By carrying out these steps, the molding of the molding material can be completed.
[0082] 3.Common matters Steps A-2) and B-3) are steps in which pressure is applied to the molding material to obtain a molded body of a desired shape. The molding pressure at this time is not particularly limited, but is preferably as low as possible within a range in which the desired molded body shape can be obtained. Specifically, the molding pressure is preferably less than 30 MPa relative to the mold cavity projected area, more preferably 20 MPa or less, and even more preferably 10 MPa or less. When the molding pressure is less than 30 MPa, it is preferable because it does not require capital investment or maintenance costs for a press machine. In addition, it is natural that various processes may be inserted between the above processes during compression molding, and for example, vacuum compression molding in which compression molding is performed while being evacuated may be used.
[0083] [Number average molecular weight of resin M1 and resin M2] In the present invention, Resin M1 contained in the fiber-reinforced plastic product imaged in step 101 has a larger number average molecular weight than resin M2 contained in the fiber-reinforced plastic product imaged in step 201. The number average molecular weights of resin M1 and resin M2 in the present invention are preferably measured in the surface layer region of the fiber reinforced plastic, and the surface layer region is a region less than 50 μm deep from the surface of the fiber reinforced plastic.
[0084] 1. Measurement of number average molecular weight The sample to be measured is prepared by cutting the surface area (or the central area) of the molded body after cold pressing with a flat knife. In the case of a painted fiber-reinforced plastic, the paint is removed. The number average molecular weight can be determined by gel permeation chromatography (GPC).
[0085] 2. Molecular weight reduction during the manufacturing process When the fiber reinforced plastic imaged in step 101 is used as a molding material, and is molded into a molded body, and then the fiber reinforced plastic is imaged in step 201, the molecular weight contained in the fiber reinforced plastic decreases.
[0086] In particular, when using carbon fibers as reinforcing fibers and a molding material containing discontinuous carbon fibers with a weight-average fiber length of 1 mm or more and 100 mm or less, it is necessary to heat the material in a high temperature range (275 to 330°C if the resin is nylon 6) in order to improve the fluidity during molding.
[0087] Under such severe heating conditions, the molecular weight of the polyamide resin present in the surface layer region in particular is significantly reduced.
[0088] 3. Molecular weight reduction during distribution The fiber reinforced plastic imaged in step 201 may be one that has been manufactured in step 101, shipped, and distributed on the market. The fiber reinforced plastic of the present invention is used for automobile parts and the like. When fiber reinforced plastic is distributed on the market, it is exposed to rain and wind over time, and the number average molecular weight contained in the fiber reinforced plastic decreases. Therefore, the resin M1 contained in the fiber reinforced plastic product imaged in advance has a larger number average molecular weight than the resin M2 contained in the fiber reinforced plastic product to be imaged and subsequently subjected to individual recognition.
[0089] 4. Evaluation of the degree of resin deterioration After performing individual recognition using the individual recognition method for fiber reinforced plastics, the degree of deterioration of the resin contained in the fiber reinforced plastic may be evaluated. The deterioration of the resin is evaluated by measuring the number average molecular weights contained in the resins M1 and M2. EXAMPLES
[0090] The present invention will be specifically described below using examples, but the present invention is not limited to these.
[0091] 1.Material 1.1 Carbon fiber Teijin's carbon fiber "Tenax" (registered trademark) STS40-24K (average fiber diameter 7 μm, 24,000 single fibers) 1.2 Thermoplastic resin Polyamide 6 (A1030 manufactured by Unitika Ltd., sometimes abbreviated as PA6).
[0092] 2.Various measurements The values in the present examples were determined according to the following methods. (1) Measurement of fiber volume fraction (Vf) A sample of 100 mm x 100 mm was cut out from the fiber-reinforced plastic, and the sample was heated to 550°C in an electric furnace (FP410 manufactured by Yamato Scientific Co., Ltd.) in a nitrogen atmosphere for 1 hour to burn off organic matter such as the matrix resin. The weights of the fibers and resin were calculated by weighing the samples before and after burn-off, and the volume fraction of the fibers was then calculated using the specific gravity of each component. Fiber volume fraction (Vf) = 100 × fiber volume / (fiber volume + resin volume) Equation (1)
[0093] 3. Measurement of number average molecular weight The samples for measurement were obtained by cutting the surface layer of the fiber-reinforced plastic (molding material, molded body) before and after cold pressing with a flat knife. The entire area of a 135 mm x 65 mm test piece was cut with a flat knife to obtain a measurement sample of about 80 to 120 mg.
[0094] The molecular weight was determined by gel permeation chromatography (GPC). The instrument was a Tosoh HLC-8220GPC, the detector was a differential refractometer (RI), and the solvent was hexafluoroisopropanol (HFIP) to which CF3COONa was added to make the concentration 10 mM (mol / l). One Shodex HFIP-LG column and two HFIP-806M columns were used. The solvent flow rate was 0.8 ml / min, and the sample concentration was approximately 0.1 wt / vol%. The sample was filtered to remove insoluble matter and used as a measurement sample. Based on the obtained elution curve, the number average molecular weight (Mn) was calculated in terms of polymethyl methacrylate (PMMA).
[0095] [Example 1] 1. Preparing the Fiber-reinforced Plastic for Imaging The carbon fibers used were Teijin's "Tenax" (registered trademark) STS40-24K carbon fibers (average fiber diameter 7 μm, number of single fibers 24,000) cut to a fiber length of 20 mm, and Unitika's nylon 6 resin A1030 was used as the resin, to prepare a molding material of carbon fibers and nylon 6 resin in which the carbon fibers are oriented two-dimensionally randomly based on the method described in U.S. Patent No. 8,946,342. The obtained molding material was heated at 2.0 MPa for 5 minutes in a press machine heated to 270°C, to obtain a flat fiber-reinforced plastic with a width of 400 mm, length of 400 mm, and average thickness of 2.6 mm.
[0096] Analysis of the carbon fibers contained in the flat fiber-reinforced plastic revealed that the carbon fiber volume fraction (Vf) was 35%, the fiber length of the carbon fibers was constant, and the weight average fiber length was 20 mm.
[0097] This flat fiber-reinforced plastic was used as a molding material to be molded into a molded product later. The surface of the fiber-reinforced plastic had a two-dimensional random orientation as shown in Figure 1.
[0098] A total of 100 sheets of fiber-reinforced plastic, the molding material, were prepared and proceeded to step 101. In addition, in order to measure the number average molecular weight, two additional pieces of fiber-reinforced plastic were prepared to measure the number average molecular weight of resin M1 contained in the fiber-reinforced plastic product imaged in step 101, and resin M2 contained in the fiber-reinforced plastic product imaged in step 201.
[0099] 2.Process 101 The surface of the fiber reinforced plastic prepared in 1 was used as identification information, and images of this were taken with a Sony RX100V, and a database was created on a computer by linking the images with the corresponding product information. Images were similarly taken of the 100 sheets of fiber reinforced plastic used as the molding material prepared in 1, and a database was created. The product information included the serial number, manufacturing date, and manufacturing time.
[0100] 3.Compression molding The fiber-reinforced plastic (molding material) whose surface identification information was obtained in step 101 was heated to 290°C, which is above the plasticization temperature of polyamide 6 (thermoplastic resin), using a resin sheet heating device (model H7GS-73408) manufactured by NGK Kiln Tech Co., Ltd.
[0101] The heated fiber-reinforced plastic (molding material) was placed in the lower die of a molding die with a clearance of 400 mm × 400 mm × 2.5 mm and set at 150° C. At this time, the surface having the identification information (imaging surface) was the surface of the fiber-reinforced plastic that came into contact with the lower die.
[0102] The upper die of the mold was lowered to apply pressure and cold pressed at 20 MPa for 1 minute. The upper die of the mold was raised to completely open the mold, after which the molded body was released from the lower die and taken out.
[0103] A total of 100 sheets of fiber-reinforced plastic molding material prepared in step 1 were all cold pressed and extracted as molded bodies.
[0104] 4.Process 201 The identification information of the fiber-reinforced plastic (molded body) produced by cold pressing was imaged to obtain an identification information image P2. The identification information is the surface of the fiber-reinforced plastic (molded body) that was in contact with the lower die.
[0105] 5.Process 301 The obtained identification information image P2 was compared with the identification information image P1 stored in the database, and individual fiber reinforced plastics were recognized.
[0106] By identifying feature points such as the position, orientation, thickness, and length of fiber bundles observed on the surface of fiber-reinforced plastic, classification was performed using only the images with the highest degree of match, and as a result, 90 out of 100 images were correctly recognized. In other words, when classification was performed using the system alone, one identification information image P1 could be extracted based on the identification information image P1 with 90% accuracy (TOP-1 ACCURACY was 90%).
[0107] Furthermore, five identification information images P1 were presented in descending order of the degree of matching with the identification information image P2, and as a result, the correct identification information image P1 was included with a 100% probability. In other words, when a human being assisted in selecting from the top five images extracted by the system, it was possible to extract one identification information image P1 based on the identification information image P1 with 100% accuracy (TOP-5 ACCURACY was 100%).
[0108] [Number average molecular weight of resin M1 and resin M2] The number average molecular weight of resin M1 was 17,000, and the number average molecular weight of resin M2 was 11,500. Resin M1 contained in the fiber-reinforced plastic product to be imaged in advance had a larger number average molecular weight than resin M2 contained in the fiber-reinforced plastic product to be imaged later for individual recognition. [Industrial Applicability]
[0109] The method for identifying individual fiber-reinforced plastics of the present invention is based on the unique appearance information possessed by fiber-reinforced plastics, and therefore does not require expensive dedicated marking equipment or processing and equipment for identification. Furthermore, the present invention recognizes the unique patterns possessed by fiber-reinforced plastics, even for products of the same brand, making it possible to identify individual products and track products after shipment.
[0110] Although the present invention has been described in detail and with reference to specific embodiments, it will be apparent to those skilled in the art that various changes and modifications can be made therein without departing from the spirit and scope of the invention. This application is based on a Japanese patent application (Patent Application No. 2021-071135) filed on April 20, 2021, the contents of which are incorporated herein by reference. [Explanation of symbols]
[0111] 101: Fiber reinforced plastic 102: Carbon fiber bundle 201: Molding material (fiber-reinforced plastic imaged in step 101) 202: Molded body (fiber-reinforced plastic imaged in step 201) 301: Molded body (fiber-reinforced plastic imaged in step 101) 302: Molded body (fiber-reinforced plastic imaged in step 201) 401: Lower mold 402: Upper mold 403: When fiber-reinforced plastic is placed in the lower die, the surface that first comes into contact with the lower die 404: Flow, part where molding material flows out to the periphery of the initially placed molding material 405: Molding material
Claims
1. A method for identifying individual fiber-reinforced plastics, comprising: a surface of the fiber-reinforced plastic having discontinuous fibers randomly arranged thereon; the discontinuous fibers including discontinuous fiber bundles A1; A method for recognizing individual fiber-reinforced plastics, comprising the following steps: Step 101. A step of acquiring discontinuous fibers randomly arranged on the surface of a fiber-reinforced plastic as identification information in advance, acquiring an identification information image P1 including discontinuous fiber bundles A1 with an area of 2000 mm2 or more, and creating a database in which the product information of the fiber-reinforced plastic is associated and stored; Step 201. After step 101, acquiring identification information of the fiber-reinforced plastic to acquire an identification information image P2; Step 301. A step of performing individual recognition of fiber reinforced plastics by comparing the acquired identification information image P2 with the identification information image P1 stored in the database; However, the resin M1 contained in the fiber reinforced plastic product of step 101 has a larger number average molecular weight than the resin M2 contained in the fiber reinforced plastic product of step 201.
2. The method for identifying individual fiber-reinforced plastics according to claim 1 , wherein the product information includes at least one of fiber length, fiber volume fraction, fiber brand, resin brand, manufacturing date, manufacturing time, and product serial number.
3. The fiber reinforced plastic in step 101 is a molding material, The fiber-reinforced plastic in step 201 is a molded body, and the molded body is obtained by compression molding a molding material. A method for identifying individual fiber-reinforced plastics according to claim 1.
4. The compression molding is cold press molding using a mold having an upper mold and a lower mold, The identification information is a surface image of the fiber-reinforced plastic on the side that contacts the lower die. The method for identifying an individual according to claim 3.
5. The method for identifying an individual according to claim 4, A method for identifying an individual, wherein identification information is present in a non-flowing or low-flowing area.
6. The method for identifying individual fiber-reinforced plastics according to claim 1 , wherein the identification information image is non-destructive inspection data.
7. The method for recognizing individual fiber-reinforced plastics according to claim 1 , wherein line scan lighting or dome lighting is used when imaging the identification information of the fiber-reinforced plastic.
8. A method for evaluating a degree of deterioration of a resin contained in a fiber-reinforced plastic after performing individual recognition using the method for recognizing individual fiber-reinforced plastics according to any one of claims 1 to 5.
Citation Information
Patent Citations
Parts made of resin, and device and method for treating waste
JP2001038733A
Object identification device
JP2012198848A
Individual identification method for sintered product
JP2013232069A
Medical material recognition system
JP2019168765A
Marked composite material and method for producing same
WO2015137093A1