Resist composition and pattern forming method

JP7593438B2Active Publication Date: 2024-12-03SHIN ETSU CHEMICAL CO LTD
View PDF 12 Cites 0 Cited by

Patent Information

Application Number
JP2023082693
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2023-05-19
Publication Date
2024-12-03
Estimated Expiration
2038-09-11

AI Technical Summary

Benefits of technology

【0011】 本発明のヨードニウム塩をクエンチャーとして含むレジスト組成物を用いて、KrF又はArFエキシマレーザー光、EB、EUV等の高エネルギー線、特にArFエキシマレーザー光、EUVを露光光として用いるフォトリソグラフィーによってパターン形成を行った場合、高度に酸拡散が抑制され、矩形性に優れ、MEF、LWR、CDU等が改善されたパターンを形成することが可能となる。

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007593438000001
    Figure 0007593438000001
  • Figure 0007593438000002
    Figure 0007593438000002
  • Figure 0007593438000003
    Figure 0007593438000003
Patent Text Reader

Abstract

To provide a carboxylic acid iodonium salt that gives a resist composition, used as a quencher in photolithography with high energy rays such as KrF or ArF excimer laser beams, EB, EUV as a light source, excelling in rectangularity, and also excelling in MEF, LWR, and CDU, a resist composition comprising the iodonium salt, and a patterning method using the resist composition.SOLUTION: A resist composition comprises a quencher composed of an iodonium salt represented by the formula (1), a base resin that comprises a polymer comprising a repeat unit of a specific structure (excluding repeat units having an oxirane ring), and an organic solvent. The base resin also serves as a photoacid generator, and other photoacid generators are not comprised.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a resist composition and a pattern forming method using the resist composition. [Background technology]

[0002] In recent years, as the integration and speed of LSIs increases, there is a demand for finer pattern rules, and far-ultraviolet lithography and extreme ultraviolet (EUV) lithography are seen as promising next-generation microfabrication technologies. Among these, photolithography using an ArF excimer laser as a light source is an essential technology for ultra-fine processing of 0.13 μm or less.

[0003] In order to achieve the demands for finer patterning, it is important not only to optimize the base resin of the resist composition, but also to improve the performance of additives such as photoacid generators. In particular, in chemically amplified resist compositions, controlling the diffusion of strong acids generated upon exposure is a critical issue.

[0004] As a photoacid generator, sulfonium salts such as triphenylsulfonium nonafluorobutanesulfonate, which have excellent stability in a resist composition, have been generally used. However, when this is used in a resist composition, the generated acid diffuses widely, making it difficult to achieve high resolution. In response to this problem, various partially fluorinated alkanesulfonic acids and their salts have been developed, and photoacid generators that have an acid diffusion suppressing effect by introducing a bulky substituent or a polar group have been studied. For example, triphenylsulfonium 2-(1-adamantanecarbonyloxy)-1,1,3,3,3-pentafluoropropane-1-sulfonate is a photoacid generator that has an acid diffusion suppressing effect by having a bulky substituent. However, even in resist compositions using this, the high level control of acid diffusion is still insufficient, and the lithography performance is not satisfactory when the line width roughness (LWR) and resolution, which are indicators of pattern roughness, are considered comprehensively.

[0005] In addition to the structural modification of the photoacid generator, various quenchers (acid diffusion control agents) have also been studied. As the quencher, amines and weak acid onium salts are generally used. Patent Document 1 describes that the addition of triphenylsulfonium acetate can form a good resist pattern without the formation of a T-top, the difference in line width between isolated patterns and dense patterns, and standing waves. Patent Document 2 describes that the addition of ammonium sulfonate or ammonium carboxylate improves sensitivity, resolution, and exposure margin. Patent Document 3 describes that a resist composition for KrF or electron beam (EB) containing a photoacid generator that generates a fluorine-containing carboxylic acid has excellent resolution and improved process tolerance such as exposure margin and depth of focus. Furthermore, Patent Document 4 also describes that a resist composition for F2 laser light containing a photoacid generator that generates a fluorine-containing carboxylic acid has excellent line edge roughness and improved footing problems. These are used in KrF, EB, and F2 lithography, but Patent Document 5 describes a positive-type photosensitive composition for ArF excimer laser exposure that contains a carboxylate onium salt. These compositions are produced by exposing a strong acid (sulfonic acid) generated from another photoacid generator to light, and ion exchange occurs with a weak acid onium salt to form a weak acid and a strong acid onium salt, thereby replacing a strong acid (sulfonic acid) with a weak acid (carboxylic acid), thereby suppressing the acid decomposition reaction of acid labile groups and reducing (controlling) the acid diffusion distance.

[0006] However, even when these weak acid onium salts are used, pattern collapse may occur, resulting in no improvement in resolution, or the solubility in an alkaline developer may be low, causing defects after development, and various lithography performances such as LWR may not be satisfactory. As a means for solving these problems, Patent Document 6 describes a resist composition containing a sulfonium salt of a fluorine-containing carboxylic acid, but there is still a problem that satisfactory results cannot be obtained in terms of pattern shape and lithography performance. [Prior art documents] [Patent documents]

[0007] [Patent Document 1] Japanese Patent Application Publication No. 11-295887 [Patent Document 2] Japanese Patent Application Publication No. 11-327143 [Patent Document 3] Patent No. 4231622 [Patent Document 4] Patent No. 4116340 [Patent Document 5] Patent No. 4226803 [Patent Document 6] Patent No. 5556765 Summary of the Invention [Problem to be solved by the invention]

[0008] The present invention has been made in view of the above-mentioned circumstances, and has an object to provide an iodonium carboxylate salt that is used as a quencher in photolithography using a high-energy ray such as KrF or ArF excimer laser light, EB, or EUV as a light source, and that provides a resist composition that is excellent in rectangularity, mask error factor (MEF), LWR, and dimensional uniformity (CDU); a resist composition that contains the iodonium salt; and a pattern formation method that uses the resist composition. [Means for solving the problem]

[0009] As a result of intensive investigations in order to achieve the above-mentioned object, the inventors have discovered that a resist composition containing an iodonium salt having a specific structure is excellent in rectangular shape and in lithography performance such as MEF, CDU, and LWR, and is extremely effective as a resist composition for precise microfabrication, which has led to the completion of the present invention.

[0010] That is, the present invention provides the following resist composition and pattern forming method. 1. A quencher comprising an iodonium salt represented by the following formula (1): A base resin containing a polymer containing at least one repeating unit selected from the group consisting of a repeating unit represented by the following formula (a), a repeating unit represented by the following formula (b), and repeating units represented by the following formulas (c1) to (c4) (however, the base resin does not contain a repeating unit having an oxirane ring), and Organic Solvents wherein the base resin is also a photoacid generator, and no other photoacid generator is contained. [ka] (In the formula, R f1 and R f2 are each independently a hydrogen atom, a fluorine atom, or a linear or branched monovalent hydrocarbon group having 1 to 4 carbon atoms which may contain a fluorine atom, but at least one of them is a fluorine atom, or a linear or branched monovalent hydrocarbon group having 1 to 4 carbon atoms which contains a fluorine atom. Ar 1 and Ar 2 are each independently an aryl group having 6 to 40 carbon atoms which may contain a heteroatom. 1 and Ar 2 may be bonded to each other to form a ring together with the iodine atom to which they are attached. [ka] (In the formula, R A is a hydrogen atom, a fluorine atom, a methyl group or a trifluoromethyl group. Z A is a single bond, a phenylene group, a naphthylene group, or (main chain) -C(=O)-O-Z'-, where Z' is an alkanediyl group having 1 to 10 carbon atoms which may contain a hydroxy group, an ether bond, an ester bond, or a lactone ring, or a phenylene group or a naphthylene group. A is an acid labile group. Y Ais a hydrogen atom, or a polar group containing at least one structure selected from a hydroxyl group, a cyano group, a carbonyl group, a carboxyl group, an ether bond, an ester bond, a sulfonate ester bond, a carbonate bond, a lactone ring, a sultone ring, and a carboxylic acid anhydride. [ka] (In the formula, R A is a hydrogen atom, a fluorine atom, a methyl group or a trifluoromethyl group. L 1 is a single bond, a phenylene group, -OL 11 -, -C(=O)-OL 11 - or -C(=O)-NH-L 11 - represents L 11 is an alkanediyl group having 1 to 20 carbon atoms, an alkenediyl group having 2 to 20 carbon atoms, or a phenylene group, which may contain a heteroatom. L 2 and L 3 are each independently a single bond or a divalent hydrocarbon group having 1 to 20 carbon atoms which may contain a heteroatom. L 4 is a single bond, a methylene group, an ethylene group, a phenylene group, a fluorinated phenylene group, -OL 41 -, -C(=O)-OL 41 or -C(=O)-NH-L 41 -It is. 41 is an optionally substituted phenylene group. R 11 ~R 21 are each independently a monovalent hydrocarbon group having 1 to 20 carbon atoms which may contain a heteroatom. 1 , R 11 and R 12 Any two of R may be bonded to each other to form a ring together with the sulfur atom to which they are attached; 13 , R 14 and R 15 Any two of R 16 , R 17 and R 18 Any two of the above, or R 19, R 20 and R 21 Any two of may be bonded to each other to form a ring together with the sulfur atom to which they are attached. Xc - represents a non-nucleophilic counter ion. A 1 is a hydrogen atom or a trifluoromethyl group. n 1 is 0 or 1, but L 2 When is a single bond, it is 0. 2 is 0 or 1, but L 3 is a single bond, it is 0.) 2. The resist composition of 1 further comprising an amine compound. 3. The resist composition of 1 or 2, further comprising a surfactant that is insoluble or poorly soluble in water but soluble in an alkaline developer, and / or a surfactant that is insoluble or poorly soluble in water and an alkaline developer. 4. A pattern forming method comprising the steps of: forming a resist film on a substrate using the resist composition according to any one of 1 to 3; exposing the resist film to KrF excimer laser light, ArF excimer laser light, an electron beam or extreme ultraviolet light; and developing the exposed resist film using a developer. 5. The pattern formation method of 4, in which an alkaline aqueous solution is used as a developer to dissolve the exposed areas and obtain a positive pattern in which the unexposed areas do not dissolve. 6. The pattern formation method of 4, in which an organic solvent is used as a developer to dissolve the unexposed areas and obtain a negative pattern in which the exposed areas do not dissolve. 7. The organic solvent is 2-octanone, 2-nonanone, 2-heptanone, 3-heptanone, 4-heptanone, 2-hexanone, 3-hexanone, diisobutyl ketone, methylcyclohexanone, acetophenone, methylacetophenone, propyl acetate, butyl acetate, isobutyl acetate, pentyl acetate, butenyl acetate, isopentyl acetate, propyl formate, butyl formate, isobutyl formate, pentyl formate, isopentyl formate, methyl valerate, methyl pentenoate, methyl crotonate, ethyl crotonate, methyl propionate, propionate and 6. a pattern forming method in which the lactate is at least one selected from the group consisting of ethyl 3-ethoxypropionate, methyl lactate, ethyl lactate, propyl lactate, butyl lactate, isobutyl lactate, pentyl lactate, isopentyl lactate, methyl 2-hydroxyisobutyrate, ethyl 2-hydroxyisobutyrate, methyl benzoate, ethyl benzoate, phenyl acetate, benzyl acetate, methyl phenylacetate, benzyl formate, phenylethyl formate, methyl 3-phenylpropionate, benzyl propionate, ethyl phenylacetate and 2-phenylethyl acetate. 8. The pattern forming method according to any one of 4 to 7, wherein the exposure is immersion exposure performed by interposing a liquid having a refractive index of 1.0 or more between the resist film and a projection lens. 9. The pattern formation method according to claim 8, further comprising coating a protective film on the resist film, and carrying out immersion exposure by placing the liquid between the protective film and a projection lens. Effect of the Invention

[0011] When a resist composition containing the iodonium salt of the present invention as a quencher is used to form a pattern by photolithography using high-energy rays such as KrF or ArF excimer laser light, EB, or EUV, particularly ArF excimer laser light or EUV, as exposure light, it becomes possible to form a pattern in which acid diffusion is highly suppressed, rectangularity is excellent, and MEF, LWR, CDU, etc. are improved. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] The present invention will be described in detail below. In the following description, some structures represented by chemical formulas may have asymmetric carbons and may have enantiomers or diastereomers, but in such cases, one formula will be used to represent these isomers. These isomers may be used alone or in combination of two or more.

[0013] [Iodonium salts] The iodonium salt of the present invention is represented by the following formula (1). [ka]

[0014] In formula (1), R f1 and R f2 are each independently a hydrogen atom, a fluorine atom, or a linear or branched monovalent hydrocarbon group having 1 to 4 carbon atoms which may contain a fluorine atom. f1 and R f2 At least one of the groups is a fluorine atom, or a linear or branched monovalent hydrocarbon group having 1 to 4 carbon atoms which may contain a fluorine atom.

[0015] Examples of the monovalent hydrocarbon group include a methyl group, an ethyl group, an n-propyl group, an isopropyl group, an n-butyl group, a monofluoromethyl group, a difluoromethyl group, a trifluoromethyl group, a 2,2,2-trifluoromethyl group, a pentafluoroethyl group, a heptafluoropropyl group, a nonafluorobutyl group, a 2,2,2-trifluoroethyl group, and a 1-trifluoromethyl-2,2,2-trifluoroethyl group. f1 and R f2 is preferably a hydrogen atom, a methyl group, a fluorine atom, or a trifluoromethyl group, and particularly preferably a trifluoromethyl group. f1 and R f2When both are trifluoromethyl groups, the acidity of the conjugate acid of the carboxylate anion is moderately high, and the nucleophilic site is sterically bulky, suppressing the nucleophilicity to a moderate degree, which is expected to improve the stability of the resist composition. In addition, the presence of fluoroalcohol units improves compatibility, and the uniform dispersion in the resist film is expected to improve lithography performance such as LWR and CDU.

[0016] In formula (1), Ar 1 and Ar 2 are each independently an aryl group having 6 to 40 carbon atoms which may contain a heteroatom. 1 and Ar 2 may be bonded to each other to form a ring together with the iodine atom to which they are bonded.

[0017] The aryl group may be a phenyl group, a naphthyl group, or a substituent may be substituted at any position. Examples of the aryl group include, but are not limited to, a tolyl group, a xylyl group, a trimethylphenyl group, an ethylphenyl group, an isopropylphenyl group, a tert-butylphenyl group, a 1-adamantylphenyl group, a triisopropylphenyl group, a tricyclohexylphenyl group, a methoxyphenyl group, an ethoxyphenyl group, a butoxyphenyl group, a hydroxyphenyl group, a dihydroxyphenyl group, a trimethoxyphenyl group, a methylthiophenyl group, a biphenyl group, a fluorophenyl group, a difluorophenyl group, a bromophenyl group, an iodophenyl group, an N,N-diphenylaminophenyl group, an acetoxyphenyl group, an acetylaminophenyl group, a 2,2,2-trifluoroethoxyphenyl group, a (2-methoxyethoxy)phenyl group, a hydroxynaphthyl group, a dihydroxynaphthyl group, a 2,2,2-trifluoroethoxynaphthyl group, and a (2-methoxyethoxy)naphthyl group.

[0018] The aryl group further includes an aryl group having a polymerizable substituent such as an acryloyloxy group or a methacryloyloxy group. Specific examples thereof include a 4-acryloyloxyphenyl group, a 4-methacryloyloxyphenyl group, a 4-acryloyloxy-3,5-dimethylphenyl group, a 4-methacryloyloxy-3,5-dimethylphenyl group, a 4-vinyloxyphenyl group, a 4-(2-acryloyloxyethoxy)phenyl group, and a 4-(2-methacryloyloxyethoxy)phenyl group.

[0019] Ar 1 and Ar 2 As the aryl group, an unsubstituted phenyl group or a phenyl group having a substituent selected from a halogen atom, an alkyl group and an alkoxy group at the para-position of the iodine atom is preferred, with a phenyl group, a 4-tert-butylphenyl group, a 4-fluorophenyl group and the like being particularly preferred.

[0020] Also, Ar 1 and Ar 2 are bonded to each other to form a ring together with the iodine atom to which they are attached, Ar 1 and Ar 2 may be bonded directly or via an oxygen atom, a methylene group, a sulfone group, a carbonyl group, etc. Examples of the ring structure formed in this case include, but are not limited to, those shown below. In addition, in the following formula, a substituent may be present at any position on the aromatic ring. [ka]

[0021] Examples of the anion of the iodonium salt represented by formula (1) include, but are not limited to, those shown below. [ka]

[0022] Examples of the cation of the iodonium salt compound represented by formula (1) include, but are not limited to, those shown below: In the following formula, tBu is a tert-butyl group, and Ph is a phenyl group. [ka]

[0023] [ka]

[0024] Specific structures of the iodonium salt of the present invention include, but are not limited to, any combination of the specific cations and the specific anions described above. Particularly preferred structures include the following. In the following formula, tBu is a tert-butyl group. [ka]

[0025] The resist composition of the present invention containing the iodonium salt as a quencher has excellent rectangularity and excellent lithography performance such as MEF, LWR, CDU, etc. Although the exact reason why such effects are obtained is unclear, it can be considered as follows.

[0026] The iodonium salt of the present invention has a fluoroalcohol unit in the anion skeleton, and therefore has high compatibility, and is uniformly dispersed in the resist film, which is believed to improve lithography performance such as LWR and CDU. In addition, since the iodonium cation has a higher dissolution inhibition ability than the sulfonium cation, it is believed that, for example, in an alkali development type resist composition, the dissolution of the upper part of the pattern by the developer is suppressed, thereby improving rectangularity.

[0027] In addition, when comparing the iodonium salt of the present invention with a triarylsulfonium salt having the same anion, the iodonium salt of the present invention has superior thermal stability. Although the exact reason for this result is unclear, it can be considered as follows. The anion of the present invention has a structure having a hydroxyl group and a carboxyl group via a methylene, and the oxygen atoms on these two functional groups and the cation moiety (M + ) and is believed to be stabilized by forming a ring structure as shown in the following formula (1'). When forming this ring structure, the iodonium cation has a large atomic radius of the central iodine atom and is bound to two aryl groups, so there is little steric hindrance and it is easy to form a ring structure, but the triarylsulfonium cation has a large steric hindrance because the central sulfur atom is bound to three aryl groups and the atomic radius of the sulfur atom is small, so it is difficult to form a stable structure and it is believed that the thermal stability is reduced. [ka] (In the formula, R f1 and R f2 is the same as above. M is an iodine atom or a sulfur atom.

[0028] Furthermore, the iodonium salt of the present invention is likely to easily assume the above-mentioned stable structure, which enhances its ability to inhibit dissolution in an alkaline developer, thereby helping to improve rectangularity.

[0029] The iodonium salt of the present invention can be synthesized, for example, according to the following scheme, but is not limited thereto. [ka] (In the formula, R f1 , R f2 , Ar 1 and Ar 2 is the same as above. R is a hydrogen atom or an alkyl group. B is a base. X - is an anion.)

[0030] The raw material compounds can be synthesized by various methods, for example, by adding hydrogen cyanide to the corresponding carbonyl compound and then hydrolyzing it. However, hydrogen cyanide is highly toxic, and some carbonyl compounds, such as hexafluoroacetone, are also highly toxic, so they must be handled with care. 3,3,3-trifluoro-2-hydroxy-2-(trifluoromethyl)propionic acid derivatives, especially their methyl esters, can be obtained from octafluoroisobutylene, a by-product produced when synthesizing hexafluoropropene, and are therefore fluorine compounds that can be obtained in large quantities at relatively low cost because their supply source is a by-product of industrial products.

[0031] The hydrolysis reaction in the first step will be described in detail. The raw material α-hydroxycarboxylic acid or its ester may be a commercially available product, or may be synthesized by the above-mentioned method. Examples of the base to be used include lithium hydroxide, sodium hydroxide, potassium hydroxide, calcium hydroxide, tetramethylammonium hydroxide, tetraethylammonium hydroxide, tetrabutylammonium hydroxide, and ammonium hydroxide, and sodium hydroxide and tetramethylammonium hydroxide are particularly preferred.

[0032] The number of equivalents of the base used is preferably 0.8 to 3 equivalents, more preferably 0.9 to 1.2 equivalents, relative to the α-hydroxycarboxylic acid or its ester. Examples of the solvent include water, water-methanol, water-ethanol, water-tetrahydrofuran, etc., and water is preferred. The reaction temperature and reaction time are optional, but a temperature of about room temperature to 40°C is preferred in order to accelerate the disappearance of the raw material. The reaction solution may be used as it is as a carboxylate solution in the next step of ion exchange reaction, or may be taken out as crude crystals (carboxylate) after concentrating the solvent. An acid such as hydrochloric acid may be added to neutralize the basicity. The reaction solution may also be used after washing with an organic solvent that is hydrophobic and insoluble in carboxylate, such as hexane, toluene, diethyl ether, or diisopropyl ether.

[0033] Next, the ion exchange reaction in the second step will be specifically described. The ion exchange reaction can be carried out by a known method, and can be carried out by using an organic solvent such as dichloroethane, chloroform, ethyl acetate, methyl isobutyl ketone, methanol, ethanol, acetonitrile, 1-pentanol, or the like, or a combination of an organic solvent and water. It is also possible to use a mixture of two or more organic solvents. After removing the by-product salt components, the product can be purified by a standard method such as recrystallization or chromatography.

[0034] The anion of the iodonium salt used in the ion exchange reaction is not particularly limited, and examples thereof include chloride ion, bromide ion, methanesulfonate ion, p-toluenesulfonate ion, nitrate ion, sulfate ion, carbonate ion, hydrogencarbonate ion, methylsulfate ion, acetate ion, etc. Among these, chloride ion, p-toluenesulfonate ion, and acetate ion are preferred.

[0035] [Resist composition] The resist composition of the present invention contains (A) the quencher composed of the iodonium salt as an essential component, and optionally contains other components, such as: (B) a base resin, and (C) Organic solvent Includes.

[0036] Furthermore, the resist composition of the present invention may contain, if necessary, one or more components selected from the following (D) to (G). (D) a photoacid generator, (E) a surfactant, and (F) a quencher other than component (A), and (G) Other Ingredients

[0037] [(A) Iodonium salt] The iodonium salt of component (A) used in the resist composition of the present invention is the iodonium salt of the present invention, and is added as a photoacid generator or quencher. The amount of the sulfonium salt of component (A) is preferably 0.1 to 20 parts by mass, more preferably 0.5 to 10 parts by mass, per 100 parts by mass of the base resin of component (B). If the amount is equal to or greater than the lower limit, it functions satisfactorily as a quencher, and if it is equal to or less than the upper limit, there is no risk of performance degradation such as the generation of foreign matter due to insufficient solubility.

[0038] The iodonium salt represented by formula (1) may be used alone or in combination of two or more. In addition, since the iodonium salt of the present invention mainly acts as a photodecomposable quencher, it is preferable to use it in combination with a photoacid generator that generates a strong acid, such as a sulfonic acid fluorinated at the α-position, and in this case, the photoacid generator that generates the strong acid may be a base resin having a repeating unit having an acid generating site introduced therein, or may be added to the resist composition separately from the base resin.

[0039] By using the iodonium salt of the present invention as a quencher, it is possible to provide a resist composition that has excellent rectangularity and excellent lithography performance such as LWR and CDU in photolithography using a high-energy ray such as KrF or ArF excimer laser light, EB, or EUV as a light source.

[0040] [(B) Base resin] The base resin of the component (B) is preferably a polymer containing a repeating unit represented by the following formula (a) and a repeating unit represented by the following general formula (b). [ka]

[0041] In formulas (a) and (b), R A is a hydrogen atom, a fluorine atom, a methyl group or a trifluoromethyl group. Ais a single bond, a phenylene group, a naphthylene group, or (main chain) -C(=O)-O-Z'-, where Z' is an alkanediyl group having 1 to 10 carbon atoms which may contain a hydroxy group, an ether bond, an ester bond, or a lactone ring, or a phenylene group or a naphthylene group. A is an acid labile group. Y A is a hydrogen atom, or a polar group containing at least one structure selected from a hydroxy group, a cyano group, a carbonyl group, a carboxyl group, an ether bond, an ester bond, a sulfonate ester bond, a carbonate bond, a lactone ring, a sultone ring, and a carboxylic anhydride (-C(=O)-OC(=O)-).

[0042] The alkanediyl group may be linear, branched, or cyclic. Specific examples thereof include a methylene group, an ethane-1,1-diyl group, an ethane-1,2-diyl group, a propane-1,2-diyl group, a propane-2,2-diyl group, a propane-1,3-diyl group, a 2-methylpropane-1,3-diyl group, a butane-1,3-diyl group, a butane-2,3-diyl group, a butane-1,4-diyl group, a pentane-1,3-diyl group, a pentane-1,4-diyl group, a 2,2-dimethylpropane-1,3-diyl group, a pentane-1,5-diyl group, a hexane-1,6-diyl group, a cyclopentane-1,2-diyl group, a cyclopentane-1,3-diyl group, and a cyclohexane-1,6-diyl group.

[0043] Z in formula (a) A Examples of structures in which R is changed include, but are not limited to, those shown below. A and X A is the same as above. do. [ka] (In the formula, R A and X A is the same as above.)

[0044] X AThe acid labile group represented by the formula (I) is not particularly limited, but examples thereof include a tertiary alkyl group having 4 to 20 carbon atoms, a trialkylsilyl group in which each alkyl group has 1 to 6 carbon atoms, and an oxoalkyl group having 4 to 20 carbon atoms. For detailed explanations of the specific structures of these acid labile groups, see paragraphs

[0016] to

[0035] of JP2014-225005A.

[0045] The acid labile group is particularly preferably one represented by the following formula (xa), (xb) or (xc). [ka] (In the formula, R x is a monovalent hydrocarbon group having 1 to 10 carbon atoms which may contain a heteroatom. k is 1 or 2. The dashed lines represent bonds.

[0046] When a tertiary alicyclic hydrocarbon group represented by formula (xa), (xb) or (xc) is bonded to an ester oxygen, the acid decomposition ability is higher than that of other tertiary alkyl groups, such as a tert-butyl group or a tert-pentyl group, due to steric repulsion. When the tertiary alicyclic hydrocarbon group is used as a polarity changing unit of a resist composition, the dissolution contrast between the exposed and unexposed areas increases, which is thought to result in a pattern with excellent lithography performance such as LWR and CDU and excellent rectangularity.

[0047] Examples of the repeating unit represented by formula (a) include, but are not limited to, those shown below. In the following formula, R A is the same as above. [ka]

[0048] [ka]

[0049] [ka]

[0050] The above specific examples are Z A is a single bond, but Z A Even when Z is other than a single bond, it can be combined with a similar acid labile group. A Specific examples of when is other than a single bond are as described above.

[0051] Examples of the repeating unit represented by formula (b) include, but are not limited to, those shown below. In the following formula, R A is the same as above. [ka]

[0052] [ka]

[0053] [ka]

[0054] The polymer may further contain at least one repeating unit selected from the repeating units represented by the following formulas (c1) to (c4). [ka]

[0055] In formulas (c1) to (c4), R A is a hydrogen atom, a fluorine atom, a methyl group or a trifluoromethyl group. 1 is a single bond, a phenylene group, -OL 11 -, -C(=O)-OL 11 - or -C(=O)-NH-L 11 - stands for L 11 L is an alkanediyl group having 1 to 20 carbon atoms, an alkenediyl group having 2 to 20 carbon atoms, or a phenylene group, which may contain a heteroatom.2 and L 3 are each independently a single bond or a divalent hydrocarbon group having 1 to 20 carbon atoms which may contain a heteroatom. 4 is a single bond, a methylene group, an ethylene group, a phenylene group, a fluorinated phenylene group, -OL 41 -, -C(=O)-OL 41 or -C(=O)-NH-L 41 -It is. 41 is an optionally substituted phenylene group.

[0056] L 11 The alkanediyl group represented by the formula (I) may be linear, branched or cyclic, and specific examples thereof include a methylene group, an ethane-1,1-diyl group, an ethane-1,2-diyl group, a propane-1,2-diyl group, a propane-2,2-diyl group, a propane-1,3-diyl group, a 2-methylpropane-1,3-diyl group, a butane-1,3-diyl group, a butane-2,3-diyl group, a butane-1,4-diyl group, a pentane-1,3-diyl group, a pentane-1,4-diyl group, a 2,2-dimethylpropane-1,3-diyl group, a pentane-1,5-diyl group, a hexane-1,6-diyl group, a cyclopentane-1,2-diyl group, a cyclopentane-1,3-diyl group, and a cyclohexane-1,6-diyl group. 11 The alkene diyl group represented by the formula (I) may be linear, branched, or cyclic, and specific examples thereof include an ethene-1,2-diyl group, a 1-propene-1,3-diyl group, a 2-butene-1,4-diyl group, a 1-methyl-1-butene-1,4-diyl group, and a 2-cyclohexene-1,4-diyl group.

[0057] L 2 and L 3 The divalent hydrocarbon group represented by the formula (I) may be linear, branched, or cyclic, and specific examples thereof include the above-mentioned alkanediyl group and alkenediyl group.

[0058] In formulas (c1) to (c4), R 11 ~R 21are each independently a monovalent hydrocarbon group having 1 to 20 carbon atoms which may contain a heteroatom. The monovalent hydrocarbon group may be linear, branched or cyclic, and specific examples thereof include alkyl groups such as methyl, ethyl, n-propyl, isopropyl, n-butyl and tert-butyl; monovalent saturated cyclic aliphatic hydrocarbon groups such as cyclopropyl, cyclopentyl, cyclohexyl, cyclopropylmethyl, 4-methylcyclohexyl, cyclohexylmethyl, norbornyl and adamantyl; alkenyl groups such as vinyl, allyl, propenyl, butenyl and hexenyl; monovalent unsaturated cyclic aliphatic hydrocarbon groups such as cyclohexenyl, aryl groups such as phenyl and naphthyl, heteroaryl groups such as thienyl, and aralkyl groups such as benzyl, 1-phenylethyl and 2-phenylethyl. Among these, aryl groups are preferred. In addition, a portion of the hydrogen atoms of these groups may be substituted with a heteroatom-containing group such as an oxygen atom, a sulfur atom, a nitrogen atom or a halogen atom, and a portion of the carbon atoms of these groups may be substituted with a heteroatom-containing group such as an oxygen atom, a sulfur atom or a nitrogen atom, and as a result, these groups may contain a hydroxy group, a cyano group, a carbonyl group, an ether bond, an ester bond, a sulfonate ester bond, a carbonate bond, a lactone ring, a sultone ring, a carboxylic acid anhydride, a haloalkyl group, or the like.

[0059] L 1 , R 11 and R 12 Any two of R may be bonded to each other to form a ring together with the sulfur atom to which they are attached; 13 , R 14 and R 15 Any two of R 16 , R 17 and R 18 Any two of the above, or R 19 , R 20 and R 21 Any two of may be bonded to each other to form a ring together with the sulfur atom to which they are attached.

[0060] In formula (c1), Xc -is a non-nucleophilic counter ion. Examples of the non-nucleophilic counter ion include halide ions such as chloride ion and bromide ion; fluoroalkyl sulfonates such as triflate, 1,1,1-trifluoroethanesulfonate, and nonafluorobutanesulfonate; aryl sulfonates such as tosylate, benzenesulfonate, 4-fluorobenzenesulfonate, and 1,2,3,4,5-pentafluorobenzenesulfonate; alkyl sulfonates such as mesylate and butanesulfonate; imide acids such as bis(trifluoromethylsulfonyl)imide, bis(perfluoroethylsulfonyl)imide, and bis(perfluorobutylsulfonyl)imide; and methide acids such as tris(trifluoromethylsulfonyl)methide and tris(perfluoroethylsulfonyl)methide.

[0061] Furthermore, Xc - Examples of the non-nucleophilic counter ion represented by the formula (c5) or (c6) include anions represented by the following formula (c5) or (c6). [ka] (In the formula, R 31 and R 32 A is each independently a monovalent hydrocarbon group having 1 to 40 carbon atoms which may contain a heteroatom. 2 is a hydrogen atom or a trifluoromethyl group.

[0062] In formula (c2), specific examples of the structure of the anion moiety include those described in paragraphs

[0021] to

[0026] of JP 2014-177407 A. 1 Specific examples of the anion moiety when A is a hydrogen atom include those described in paragraphs

[0021] to

[0028] of JP2010-116550A, 1 Specific examples of the structure of the anion moiety when is a trifluoromethyl group include those described in paragraphs

[0021] to

[0027] of JP2010-77404A.

[0063] Specific examples of the anion moiety in formula (c3) include -CH(A1 )CF2SO3 - -C(CF3)2CH2SO3 - Examples of structures include those in which

[0064] Preferred examples of the anion moiety in formula (c2) include, but are not limited to, those shown below. 1 is the same as above. [ka]

[0065] Preferred examples of the anion in formula (c3) include, but are not limited to, those shown below. [ka]

[0066] Examples of the sulfonium cation in the formulas (c2) to (c4) include, but are not limited to, those shown below. In the following formulas, Me is a methyl group, nBu is an n-butyl group, and tBu is a tert-butyl group. [ka]

[0067] The polymer may further include a repeating unit having a structure in which a hydroxyl group is protected by an acid labile group. The repeating unit having a structure in which a hydroxyl group is protected by an acid labile group is not particularly limited as long as it has one or more structures in which a hydroxyl group is protected, and the protecting group is decomposed by the action of an acid to generate a hydroxyl group. Specific examples of such a repeating unit include those described in paragraphs

[0055] to

[0065] of JP 2014-225005 A and those described in paragraphs

[0110] to

[0115] of JP 2015-214634 A.

[0068] The polymer may further contain other repeating units other than those described above. Examples of the other repeating units include repeating units having an oxirane ring or an oxetane ring. By including a repeating unit having an oxirane ring or an oxetane ring, the exposed portion is crosslinked, improving the residual film properties and etching resistance of the exposed portion.

[0069] The polymer may further include, as other repeating units, substituted acrylic esters such as methyl methacrylate, methyl crotonate, dimethyl maleate, and dimethyl itaconate, unsaturated carboxylic acids such as maleic acid, fumaric acid, and itaconic acid, norbornene, norbornene derivatives, tetracyclo[6.2.1.1 3,6 .0 2,7 ] It may contain repeating units derived from cyclic olefins such as dodecene derivatives, unsaturated acid anhydrides such as itaconic anhydride, vinyl aromatics such as styrene, vinyl naphthalene, hydroxystyrene, hydroxyvinyl naphthalene, 4-tert-butoxystyrene, and other monomers. Specific examples of the other repeating units include, but are not limited to, those described in paragraphs

[0120] to

[0132] of JP 2015-214634 A. In particular, when using the resist composition of the present invention for EUV lithography, it is preferable to contain repeating units derived from hydroxystyrene and its derivatives, such as o-hydroxystyrene, m-hydroxystyrene, p-hydroxystyrene, and their tertiary etherified products, and it is particularly preferable to contain repeating units derived from m-hydroxystyrene and p-hydroxystyrene.

[0070] The weight average molecular weight (Mw) of the polymer is preferably 1,000 to 500,000, more preferably 3,000 to 100,000. If Mw is within the above range, there is no risk of the etching resistance being extremely decreased, or the difference in dissolution rate before and after exposure being unable to be secured, resulting in a decrease in resolution. In the present invention, Mw is a value measured in terms of polystyrene by gel permeation chromatography (GPC). The dispersity (Mw / Mn) is preferably 1.2 to 2.5, particularly preferably 1.3 to 1.8.

[0071] The polymer can be synthesized, for example, by polymerizing one or more desired monomers among monomers that provide various repeating units in an organic solvent with the addition of a radical polymerization initiator and heating. Such a polymerization method is described in detail in paragraphs

[0134] to

[0137] of JP 2015-214634 A. In addition, the acid labile group introduced into the monomer may be used as it is, or may be protected or partially protected after polymerization.

[0072] In the polymer, the preferred content ratio of each repeating unit obtained from each monomer can be, for example, within the ranges (mol %) shown below, but is not limited thereto. (I) 1 to 80 mol %, preferably 5 to 70 mol %, more preferably 10 to 60 mol %, of one or more types of structural units represented by formula (a); (II) 20 to 99 mol %, preferably 30 to 95 mol %, more preferably 40 to 90 mol %, of one or more structural units represented by formula (b); (III) 0 to 30 mol %, preferably 0 to 20 mol %, and more preferably 0 to 15 mol % of one or more structural units selected from those represented by formulas (c1) to (c4), and (IV) One or more types of structural units derived from other monomers: 0 to 80 mol %, preferably 0 to 70 mol %, more preferably 0 to 60 mol %.

[0073] The base resin of the component (B) may contain, in addition to the above polymer, a hydrogenated ring-opening metathesis polymer, such as those described in JP-A-2003-66612.

[0074] [(C) Organic solvent] There are no particular limitations on the organic solvent of component (C), so long as it is an organic solvent in which the components described above and the components described below can be dissolved. Examples of such organic solvents include ketones such as cyclohexanone and methyl-2-n-pentyl ketone, alcohols such as 3-methoxybutanol, 3-methyl-3-methoxybutanol, 1-methoxy-2-propanol, 1-ethoxy-2-propanol, and diacetone alcohol, propylene glycol monomethyl ether, ethylene glycol monomethyl ether, propylene glycol monoethyl ether, ethylene glycol monoethyl ether, and propylene glycol monoethyl ether, as described in paragraphs

[0144] and

[0145] of JP-A-2008-111103. Examples of suitable solvents include ethers such as ethylene glycol dimethyl ether and diethylene glycol dimethyl ether, propylene glycol monomethyl ether acetate (PGMEA), propylene glycol monoethyl ether acetate, ethyl lactate, ethyl pyruvate, butyl acetate, methyl 3-methoxypropionate, ethyl 3-ethoxypropionate, tert-butyl acetate, tert-butyl propionate, propylene glycol monotert-butyl ether acetate, and other esters, lactones such as γ-butyrolactone, and mixed solvents thereof. When an acetal-based acid labile group is used, a high-boiling alcohol solvent, specifically diethylene glycol, propylene glycol, glycerin, 1,4-butanediol, 1,3-butanediol, or the like, may be added to accelerate the deprotection reaction of the acetal.

[0075] Of these organic solvents, 1-ethoxy-2-propanol, PGMEA, diacetone alcohol, cyclohexanone, γ-butyrolactone, and mixed solvents thereof are preferably used in the present invention because they have particularly excellent solubility for the photoacid generator in the resist component.

[0076] The amount of the organic solvent, component (C), added is preferably 100 to 8,000 parts by mass, and more preferably 400 to 5,000 parts by mass, per 100 parts by mass of the base resin, component (B).

[0077] [(D) Photoacid generator] The resist composition of the present invention may contain a photoacid generator that generates a strong acid as component (D). In the present invention, a strong acid refers to an acid having a higher acidity than the acid generated by the iodonium salt represented by formula (1). In addition, when the base resin of component (B) has a solubility that changes due to the action of an acid and contains a repeating unit represented by any one of formulas (c1) to (c4), the photoacid generator of component (D) may or may not be contained.

[0078] The photoacid generator is not particularly limited as long as it is a compound that generates an acid when irradiated with high-energy rays. Suitable photoacid generators include sulfonium salts, iodonium salts, sulfonyldiazomethane, N-sulfonyloxydicarboximide, O-arylsulfonyloxime, O-alkylsulfonyloxime, etc. Specifically, for example, the compounds described in paragraphs

[0102] to

[0113] of JP 2007-145797 A, the compounds described in paragraphs

[0122] to

[0142] of JP 2008-111103 A, the compounds described in paragraphs

[0081] to

[0092] of JP 2014-001259 A, the compounds described in JP 2012-041320 A, the compounds described in JP 2012-153644 A, the compounds described in JP 2012-106986 A, the compounds described in JP 2016-018007 A, etc. can be mentioned. The partially fluorinated sulfonic acid generating photoacid generators described in these publications have moderate strength and diffusion length of the generated acid, particularly in EUV lithography and ArF lithography, and can be preferably used. When an iodonium salt is combined, the cation is preferably a diphenyliodonium cation, a p-fluorophenylphenyliodonium cation, a tert-butylphenylphenyliodonium cation or a di-tert-butylphenyliodonium cation.

[0079] Preferred examples of the photoacid generator (D) include sulfonium salts represented by the following formula (2). [ka]

[0080] In formula (2), R 101 , R 102 and R 103 are each independently a monovalent hydrocarbon group having 1 to 20 carbon atoms which may contain a heteroatom. 101 , R 102 and R 103 Any two of the above may be bonded to each other to form a ring together with the sulfur atom to which they are bonded. 11 ~R 21 The same as those described in the explanation of R 101 , R 102 and R 103 At least one of these is preferably an aryl group.

[0081] The sulfonium cation in formula (2) is described in paragraph 2 of JP-A-2014-001259.

[0082] To

[0085] , for details. Specific examples include the cations described in paragraphs

[0027] to

[0033] of JP 2007-145797 A, the cations described in paragraphs

[0059] of JP 2010-113209 A, the cations described in JP 2012-041320 A, the cations described in JP 2012-153644 A, and the cations described in JP 2012-106986 A. Particularly preferred examples of the cation in formula (2) include the same as those exemplified as the sulfonium cation in formulas (c2) to (c4).

[0082] In formula (2), X - is an anion selected from the following formulas (2A) to (2D). [ka]

[0083] In formula (2A), R fais a monovalent hydrocarbon group having 1 to 40 carbon atoms which may contain a fluorine atom or a heteroatom. As the anion represented by formula (2A), one represented by the following formula (2A') is particularly preferable. [ka]

[0084] In formula (2A'), R 111 R is a hydrogen atom or a trifluoromethyl group, preferably a trifluoromethyl group. 112is a monovalent hydrocarbon group having 1 to 35 carbon atoms which may contain a heteroatom. The heteroatom is preferably an oxygen atom, a nitrogen atom, a sulfur atom, a halogen atom, or the like, and more preferably an oxygen atom. In order to obtain high resolution in the formation of a fine pattern, the monovalent hydrocarbon group is preferably one having 6 to 30 carbon atoms. The monovalent hydrocarbon group may be linear, branched, or cyclic. Specific examples thereof include linear or branched alkyl groups such as methyl, ethyl, propyl, isopropyl, butyl, isobutyl, sec-butyl, tert-butyl, pentyl, neopentyl, cyclopentyl, hexyl, heptyl, 2-ethylhexyl, nonyl, undecyl, tridecyl, pentadecyl, heptadecyl, and icosanyl groups; monovalent saturated cyclic aliphatic hydrocarbon groups such as cyclohexyl, 1-adamantyl, 2-adamantyl, 1-adamantylmethyl, norbornyl, norbornylmethyl, tricyclodecanyl, tetracyclododecanyl, tetracyclododecanylmethyl, and dicyclohexylmethyl groups; monovalent unsaturated aliphatic hydrocarbon groups such as allyl and 3-cyclohexenyl groups; and aralkyl groups such as benzyl and diphenylmethyl groups. Examples of monovalent hydrocarbon groups containing heteroatoms include tetrahydrofuryl, methoxymethyl, ethoxymethyl, methylthiomethyl, acetamidomethyl, trifluoroethyl, (2-methoxyethoxy)methyl, acetoxymethyl, 2-carboxy-1-cyclohexyl, 2-oxopropyl, 4-oxo-1-adamantyl, and 3-oxocyclohexyl groups. Some of the hydrogen atoms in these groups may be substituted with heteroatom-containing groups such as oxygen, sulfur, nitrogen, and halogen atoms, or some of the carbon atoms in these groups may be substituted with heteroatom-containing groups such as oxygen, sulfur, and nitrogen atoms, and as a result, they may contain hydroxy groups, cyano groups, carbonyl groups, ether bonds, ester bonds, sulfonate ester bonds, carbonate bonds, lactone rings, sultone rings, carboxylic anhydrides, and haloalkyl groups.

[0085] The anion represented by formula (2A') is described in detail in JP-A-2007-145797, JP-A-2008-106045, JP-A-2009-007327, JP-A-2009-258695, and JP-A-2012-181306.

[0086] In formula (2B), R fb1 and R fb2 are each independently a monovalent hydrocarbon group having 1 to 40 carbon atoms which may contain a fluorine atom or a heteroatom. The monovalent hydrocarbon group may be linear, branched, or cyclic. Specific examples thereof include the R 112 Examples of the same as those given in the explanation of R fb1 and R fb2 is preferably a fluorine atom or a linear fluorinated alkyl group having 1 to 4 carbon atoms. fb1 and R fb2 means that the groups (-CF2-SO2-N - -SO2-CF2-) may form a ring, in which case R fb1 and R fb2 The group obtained by bonding together is preferably a fluorinated ethylene group or a fluorinated propylene group.

[0087] In formula (2C), R fc1 , R fc2 and R fc3 are each independently a monovalent hydrocarbon group having 1 to 40 carbon atoms which may contain a fluorine atom or a heteroatom. The monovalent hydrocarbon group may be linear, branched, or cyclic. Specific examples thereof include the R 112 Examples of the same as those given in the explanation of R fc1 , R fc2 and R fc3 is preferably a fluorine atom or a linear fluorinated alkyl group having 1 to 4 carbon atoms. fc1 and R fc2 means that the groups (-CF2-SO2-C - -SO2-CF2-) may form a ring, in which case R fc1 and Rfc2 The group obtained by bonding together is preferably a fluorinated ethylene group or a fluorinated propylene group.

[0088] In formula (2D), R fd is a monovalent hydrocarbon group having 1 to 40 carbon atoms which may contain a heteroatom. The monovalent hydrocarbon group may be linear, branched, or cyclic. Specific examples thereof include the above-mentioned R 112 Examples of the anion represented by formula (2D) include those exemplified in the description of . The anion represented by formula (2D) is described in detail in JP 2010-215608 A and JP 2014-133723 A. Note that, although the photoacid generator having the anion represented by formula (2D) does not have fluorine at the α-position of the sulfo group, it has two trifluoromethyl groups at the β-position and therefore has sufficient acidity to cleave the acid labile group in the base resin. Therefore, it can be used as a photoacid generator.

[0089] X - Examples of the anion represented by the formula (I) include, but are not limited to, those shown below: In the formula (I), A is a hydrogen atom or a trifluoromethyl group, and Ac is an acetyl group. [ka]

[0090] [ka]

[0091] Specific structures of the sulfonium salt represented by formula (2) include any combination of the specific anions and the specific cations described above, but are not limited thereto.

[0092] Other preferred examples of the photoacid generator (D) include the compounds represented by the following formula (3). [ka]

[0093] In formula (3), R 201 and R 202 R is each independently a monovalent hydrocarbon group having 1 to 30 carbon atoms which may contain a heteroatom. 203 is a divalent hydrocarbon group having 1 to 30 carbon atoms which may contain a heteroatom. 201 , R 202 and R 203 Any two of may be bonded to each other to form a ring together with the sulfur atom to which they are attached. A X is a single bond, an ether bond, or a divalent hydrocarbon group having 1 to 20 carbon atoms which may contain a heteroatom. 1 , X 2 , X 3 and X 4 each independently represents a hydrogen atom, a fluorine atom or a trifluoromethyl group, 1 , X 2 , X 3 and X 4 At least one of these is a fluorine atom or a trifluoromethyl group.

[0094] As the compound represented by formula (3), the compound represented by the following formula (3') is particularly preferred. [ka]

[0095] In formula (3'), L A is the same as above. 2 R is a hydrogen atom or a trifluoromethyl group, preferably a trifluoromethyl group. 211 , R 212 and R 213 are each independently a hydrogen atom or a linear, branched or cyclic monovalent hydrocarbon group having 1 to 20 carbon atoms which may contain a heteroatom. p and q are each independently an integer of 0 to 5. r is an integer of 0 to 4.

[0096] In formulas (3) and (3'), L Ais preferably an ether bond, or Q X -OL A '-OQ Y Q X represents a bond to a benzene ring, and Q Y -CH(A 2 )-CF2-SO3 - It represents a bond with L A ' is a divalent hydrocarbon group having 1 to 10 carbon atoms which may contain a heteroatom.

[0097] Photoacid generators represented by formula (3) or (3') are described in detail in JP2011-016746A. Specific examples include the sulfonium compounds described in the above publication and the sulfonium compounds described in paragraphs

[0149] to

[0150] of JP2015-214634A.

[0098] Examples of photoacid generators represented by formula (3) include, but are not limited to, those shown below. 2 is the same as above, Me is a methyl group, nBu is an n-butyl group, and tBu is a tert-butyl group. [ka]

[0099] Among the photoacid generators, those having an anion represented by formula (2A') or (2D) are particularly preferred because of their small acid diffusion and excellent solubility in solvents. Also, those having a structure represented by formula (3') are particularly preferred because of their extremely small acid diffusion.

[0100] The amount of the photoacid generator (D) added is preferably 0 to 40 parts by mass, and when added, is preferably 0.5 to 30 parts by mass, and more preferably 0.5 to 20 parts by mass, relative to 100 parts by mass of the base resin (B). Within this range, there is no risk of degradation of resolution or problems with foreign matter occurring after resist development or during peeling.

[0101] [(E) Surfactant] The resist composition of the present invention may further contain a surfactant commonly used as component (E) to improve coating properties. The content of the surfactant may be a normal amount. Specifically, reference may be made to those described in JP-A-2010-215608 and JP-A-2011-016746.

[0102] The surfactant of the component (E) is preferably a surfactant that is insoluble or slightly soluble in water but soluble in an alkaline developer, or a surfactant (hydrophobic resin) that is insoluble or slightly soluble in water and an alkaline developer.

[0103] Among the surfactants described in the above publication, preferred surfactants that are insoluble or poorly soluble in water and alkaline developers include FC-4430 (manufactured by 3M), Surflon (registered trademark) S-381, Olfine (registered trademark) E1004 (manufactured by Nissin Chemical Industry Co., Ltd.), KH-20, KH-30 (manufactured by AGC Seimi Chemical Co., Ltd.), and an oxetane ring-opening polymer represented by the following formula (surf-1). [ka]

[0104] Here, R, Rf, A, B, C, m, and n apply only to formula (surf-1), regardless of the above description. R is a divalent to tetravalent aliphatic group having 2 to 5 carbon atoms. Examples of the aliphatic group include divalent ones such as ethylene group, 1,4-butylene group, 1,2-propylene group, 2,2-dimethyl-1,3-propylene group, and 1,5-pentylene group, and examples of trivalent or tetravalent ones include the following: [ka] (In the formula, the dashed lines represent bonds, and are partial structures derived from glycerol, trimethylolethane, trimethylolpropane, and pentaerythritol, respectively.)

[0105] Among these, a 1,4-butylene group, a 2,2-dimethyl-1,3-propylene group, and the like are preferable.

[0106] Rf is a trifluoromethyl group or a pentafluoroethyl group, preferably a trifluoromethyl group. m is an integer of 0 to 3, n is an integer of 1 to 4, and the sum of n and m is the valence of R, which is an integer of 2 to 4. A is 1. B is an integer of 2 to 25, preferably an integer of 4 to 20. C is an integer of 0 to 10, preferably 0 or 1. The order of each constitutional unit in the formula (surf-1) is not specified, and they may be bonded in blocks or randomly. The production of a partially fluorinated oxetane ring-opening polymer surfactant is described in detail in the specification of U.S. Pat. No. 5,650,483.

[0107] Surfactants that are insoluble or poorly soluble in water and soluble in an alkaline developer have the function of reducing water penetration and leaching by orienting on the resist surface after spin coating when no resist protective film is used in ArF immersion exposure. Therefore, they are useful for suppressing the elution of water-soluble components from the resist film and reducing damage to the exposure device, and are also useful because they are soluble during alkaline development after exposure and post-exposure bake (PEB), making them less likely to become foreign matter that causes defects. Such surfactants are insoluble or poorly soluble in water and soluble in an alkaline developer, and are polymer-type surfactants, also called hydrophobic resins, and are particularly preferred for their high water repellency and improved water slippage.

[0108] The polymer surfactant is preferably one containing repeating units represented by the following formulas (4) to (6). [ka]

[0109] In formulas (4) to (6), R B R is a hydrogen atom, a fluorine atom, or an alkyl group or a fluorinated alkyl group having 1 to 4 carbon atoms. 301 is a hydrogen atom, -R 301A -COH or -R 301A -OH and R 301Ais a divalent organic group which may contain a fluorine atom. R 302 is a fluorinated alkyl group having 2 to 20 carbon atoms. R 303 is a hydrogen atom, a methyl group or a trifluoromethyl group. R 304 is a methylene group or an ether bond. R 305 is a fluorinated alkyl group having 2 to 20 carbon atoms.

[0110] R B The alkyl group or fluorinated alkyl group having 1 to 4 carbon atoms represented by R is preferably linear or branched. R 301A The divalent organic group represented by R is preferably an alkanediyl group having 1 to 20 carbon atoms which may contain an oxygen atom. R 302 Or R 305 The fluorinated alkyl group represented by R may be linear, branched or cyclic.

[0111] The Mw of the polymer surfactant is preferably 1,000 to 500,000, more preferably 2,000 to 30,000.

[0112] In the polymer surfactant, the content ratio of the repeating unit represented by formula (4) is x (mol%), the content ratio of the repeating unit represented by formula (5) is y (mol%), and the content ratio of the repeating unit represented by formula (6) is z (mol%), and it is preferable to satisfy 0 ≦ x < 1, 0 < y < 1, 0 ≦ z < 1, and 0 < x + y + z ≦ 1.

[0113] Also, for these surfactants which are insoluble or hardly soluble in water and soluble in an alkali developer, reference can also be made to JP-A-2007-297590, JP-A-2008-088343, JP-A-2008-122932, JP-A-2010-134012, JP-A-2010-107695, JP-A-2009-276363, JP-A-2009-192784, JP-A-2009-191151, JP-A-2009-098638, JP-A-2010-250105, JP-A-2011-042789.

[0114] The content of the polymeric surfactant is preferably from 0.001 to 20 parts by mass, and more preferably from 0.01 to 10 parts by mass, per 100 parts by mass of the base resin of the component (B).

[0115] [(F) Quencher other than component (A)] The resist composition of the present invention may contain a quencher other than the component (A) (i.e., a quencher other than the iodonium salt represented by formula (1)) as the component (F) as necessary. In the present invention, a quencher refers to a compound that can suppress the diffusion rate of the acid generated from the photoacid generator when it diffuses into the resist film.

[0116] The quencher of the component (F) may be, for example, an amine compound. The primary, secondary or tertiary amine compounds described in paragraphs

[0146] to

[0164] of JP-A-2008-111103, particularly amine compounds having any of a hydroxyl group, an ether bond, an ester bond, a lactone ring, a cyano group, a sulfonate ester bond, etc., are preferred quenchers. In addition, primary or secondary amine compounds having a carbamate group, such as the compounds described in JP-A-3790649, may also be used. Such protected amine compounds are effective when the resist composition contains a component that is unstable to bases.

[0117] In addition, as the quencher of the component (F), a compound represented by the following formula (7) (onium salt of a sulfonic acid not fluorinated at the α-position) or a compound represented by the following formula (8) (onium salt of a carboxylic acid) can also be used. [ka]

[0118] In formula (7), R 401is a hydrogen atom or a monovalent hydrocarbon group having 1 to 40 carbon atoms which may contain a heteroatom, except for those in which the hydrogen atom bonded to the carbon atom at the α-position of the sulfo group is substituted with a fluorine atom or a fluoroalkyl group. Examples of the monovalent hydrocarbon group include an alkyl group, an alkenyl group, an aryl group, an aralkyl group, and an aryloxoalkyl group. Specifically, examples of the alkyl group include a methyl group, an ethyl group, a propyl group, an isopropyl group, an n-butyl group, a sec-butyl group, a tert-butyl group, a tert-pentyl group, an n-pentyl group, an n-hexyl group, an n-octyl group, an n-nonyl group, an n-decyl group, a cyclopentyl group, a cyclohexyl group, a 2-ethylhexyl group, a cyclopentylmethyl group, a cyclopentylethyl group, a cyclopentylbutyl group, a cyclohexylmethyl group, a cyclohexylethyl group, a cyclohexylbutyl group, a norbornyl group, a tricyclo[5.2.1.0 2,6]decanyl group, adamantyl group, adamantylmethyl group, etc. Examples of the alkenyl group include vinyl group, allyl group, propenyl group, butenyl group, hexenyl group, cyclohexenyl group, etc. Examples of the aryl group include a phenyl group, a naphthyl group, a thienyl group, and the like; alkoxyphenyl groups such as a 4-hydroxyphenyl group, a 4-methoxyphenyl group, a 3-methoxyphenyl group, a 2-methoxyphenyl group, a 4-ethoxyphenyl group, a 4-tert-butoxyphenyl group, and a 3-tert-butoxyphenyl group; alkylphenyl groups such as a 2-methylphenyl group, a 3-methylphenyl group, a 4-methylphenyl group, a 4-ethylphenyl group, a 4-tert-butylphenyl group, a 4-n-butylphenyl group, a 2,4-dimethylphenyl group, and a 2,4,6-triisopropylphenyl group; alkylnaphthyl groups such as a methylnaphthyl group and an ethylnaphthyl group; alkoxynaphthyl groups such as a methoxynaphthyl group, an ethoxynaphthyl group, an n-propoxynaphthyl group, and an n-butoxynaphthyl group; dialkylnaphthyl groups such as a dimethylnaphthyl group and a diethylnaphthyl group; and dialkoxynaphthyl groups such as a dimethoxynaphthyl group and a diethoxynaphthyl group. Examples of the aralkyl group include a benzyl group, a 1-phenylethyl group, and a 2-phenylethyl group. Examples of the aryloxoalkyl group include a 2-aryl-2-oxoethyl group, such as a 2-phenyl-2-oxoethyl group, a 2-(1-naphthyl)-2-oxoethyl group, and a 2-(2-naphthyl)-2-oxoethyl group. In addition, a part of the hydrogen atoms of these groups may be substituted with a heteroatom-containing group such as an oxygen atom, a sulfur atom, a nitrogen atom, or a halogen atom, and a part of the carbon atoms of these groups may be substituted with a heteroatom-containing group such as an oxygen atom, a sulfur atom, or a nitrogen atom, and as a result, the group may contain a hydroxy group, a cyano group, a carbonyl group, an ether bond, an ester bond, a sulfonate ester bond, a carbonate bond, a lactone ring, a sultone ring, a carboxylic acid anhydride, a haloalkyl group, or the like.

[0119] In formula (8), R 402 R is a monovalent hydrocarbon group having 1 to 40 carbon atoms which may contain a heteroatom. 402 The monovalent hydrocarbon group represented by the formula: 401Examples of the monovalent hydrocarbon group include the same as those exemplified above. Other specific examples include fluorine-containing alkyl groups such as a trifluoromethyl group, a trifluoroethyl group, a 2,2,2-trifluoro-1-methyl-1-hydroxyethyl group, and a 2,2,2-trifluoro-1-(trifluoromethyl)-1-hydroxyethyl group, aryl groups such as a phenyl group, a tolyl group, a xylyl group, a 4-tert-butylphenyl group, and a naphthyl group, and fluorine-containing aryl groups such as a pentafluorophenyl group and a 4-trifluoromethylphenyl group.

[0120] The onium sulfonate represented by formula (7) and the onium carboxylate represented by formula (8) are described in detail in JP-A-2008-158339 and JP-A-2010-155824.

[0121] Preferred examples of the anion in formula (7) include, but are not limited to, those shown below. [ka]

[0122] Furthermore, preferred examples of the anion in formula (8) include, but are not limited to, those shown below. [ka]

[0123] In formulas (7) and (8), Mq + is an onium cation. The onium cation is preferably one represented by any one of the following formulas (9) to (11). [ka]

[0124] In formulas (9) to (11), R 411 ~R 419 are each independently a monovalent hydrocarbon group having 1 to 40 carbon atoms which may contain a heteroatom.411 and R 412 and, or R 416 and R 417 and may be bonded to each other to form a ring together with the sulfur atom or nitrogen atom to which they are attached.

[0125] Specific examples of the sulfonium cation represented by formula (9) include the same as those exemplified as the cations in formulas (c2) to (c4). Specific examples of the iodonium cation represented by formula (10) include the same as those exemplified as the cations of the iodonium salt represented by formula (1). Specific examples of the ammonium cation represented by formula (11) include, but are not limited to, the following: [ka]

[0126] Specific examples of the onium salt represented by formula (7) or (8) include any combination of the specific anions and the specific cations described above. These onium salts can be easily prepared by ion exchange reaction using known organic chemical techniques. For the ion exchange reaction, see, for example, JP-A-2007-145797.

[0127] The anion in formula (7) or (8) is a conjugate base of a weak acid. The term "weak acid" as used herein refers to an acidity that cannot deprotect the acid labile group of the acid labile group-containing unit used in the base resin. The onium salt represented by formula (7) or (8) functions as a quencher when used in combination with an onium salt-type photoacid generator having a conjugate base of a strong acid such as sulfonic acid fluorinated at the α-position as a counter anion. That is, when an onium salt that generates a strong acid such as sulfonic acid substituted with a fluorine atom at the α-position is mixed with an onium salt that generates a weak acid such as sulfonic acid or carboxylic acid not substituted with a fluorine atom, when the strong acid generated from the photoacid generator by irradiation with high energy rays collides with an onium salt having an unreacted weak acid anion, the weak acid is released by salt exchange to generate an onium salt having a strong acid anion. In this process, the strong acid is exchanged for a weak acid with a lower catalytic ability, and the acid is apparently deactivated, thereby controlling acid diffusion.

[0128] In particular, in the onium salt compound represented by formula (7) or (8), Mq + In the case where the photosensitive layer is a sulfonium cation represented by formula (9) or an iodonium cation represented by formula (10), the photosensitive layer is photodecomposable, and therefore the quenching ability of the photosensitive layer where the light intensity is strong is reduced, and the concentration of the strong acid derived from the photoacid generator is increased. This improves the contrast of the exposed area, and enables the formation of a pattern with good dimensional control and further improved DOF (Depth of Focus).

[0129] Here, when the photoacid generator that generates a strong acid is an onium salt, the strong acid generated by irradiation with high-energy rays can be exchanged for a weak acid as described above, but it is considered that the weak acid generated by irradiation with high-energy rays collides with the onium salt that generates the unreacted strong acid, making it difficult to carry out salt exchange. This is due to the phenomenon that the onium cation is more likely to form an ion pair with the anion of the strong acid.

[0130] The iodonium salt of the present invention also acts mainly as a quencher, and due to the above-mentioned effects, can improve various lithography performances.

[0131] When the acid labile group is an acetal that is particularly sensitive to acid, the acid for removing the protecting group does not necessarily have to be a sulfonic acid, an imide acid, or a methide acid whose α-position is fluorinated, and the deprotection reaction may proceed even with a sulfonic acid whose α-position is not fluorinated. In this case, it is preferable to use an onium salt of a carboxylic acid as represented by formula (8) as the quencher.

[0132] As the quencher of the component (F), in addition to the onium salt type quenchers described above, betaine type quenchers, for example, diphenyliodonium-2-carboxylate, which is a known compound, can also be used.

[0133] In addition, a photodegradable onium salt having a nitrogen-containing substituent may be used as the quencher of the component (F). Such a compound functions as a quencher in the unexposed area, and functions as a so-called photodegradable base in the exposed area, which loses its quenching ability by neutralization with the acid generated from itself. By using a photodegradable base, the contrast between the exposed area and the unexposed area can be further enhanced. For example, JP-A-2009-109595, JP-A-2012-46501, JP-A-2013-209360, etc. can be referred to for the photodegradable base.

[0134] The content of the (F) component is preferably 0 to 40 parts by mass, and when it is blended, it is preferably 0.1 to 40 parts by mass, and more preferably 0.5 to 20 parts by mass. If it is 40 parts by mass or less, there is no risk of deterioration of resolution or problems with foreign matter occurring after resist development or during peeling. In addition, blending a quencher within the above range makes it easy to adjust the resist sensitivity, suppresses the diffusion rate of acid in the resist film, improves resolution, suppresses sensitivity changes after exposure, reduces substrate and environmental dependency, and improves exposure margin and pattern profile. Furthermore, the addition of a quencher can also improve substrate adhesion. The (F) component quencher can be used alone or in combination of two or more types.

[0135] [(G) Other ingredients] The resist composition of the present invention may further contain, as other components (G), compounds that decompose with an acid to generate an acid (acid multiplying compounds), organic acid derivatives, fluorine-substituted alcohols, crosslinking agents, compounds with Mw of 3,000 or less (dissolution inhibitors) whose solubility in a developer changes due to the action of an acid, acetylene alcohols, etc. Specifically, the acid multiplying compounds are described in detail in JP-A-2009-269953 and JP-A-2010-215608, and the blending amount is preferably 0 to 5 parts by mass, more preferably 0 to 3 parts by mass, relative to 100 parts by mass of the base resin of the component (B). If it is 3 parts by mass or less, acid diffusion control is easy, and there is no risk of deterioration of resolution or pattern shape. For details of other additives, see paragraphs

[0155] to

[0182] of JP2008-122932A, JP2009-269953A, and JP2010-215608A.

[0136] [Pattern formation method] The present invention further provides a pattern forming method using the resist composition described above. A known lithography technique can be employed to form a pattern using the resist composition of the present invention. More specifically, the method includes the steps of applying the resist composition of the present invention onto a substrate to form a resist film, exposing the resist film to KrF excimer laser light, ArF excimer laser light, EB or EUV, and developing the exposed resist film using a developer. Some further steps may be added as necessary.

[0137] The substrate may be, for example, a substrate for integrated circuit manufacturing (Si, SiO2, SiN, SiON, TiN, WSi, BPSG, SOG, organic anti-reflective film, etc.) or a substrate for mask circuit manufacturing (Cr, CrO, CrON, MoSi2, SiO2, etc.).

[0138] The resist film can be formed, for example, by applying a resist composition onto a substrate by a method such as spin coating so that the film thickness is preferably 10 to 2000 nm, and more preferably 20 to 500 nm, and then pre-baking the composition on a hot plate at 60 to 180° C. for 10 to 600 seconds, and preferably at 70 to 150° C. for 15 to 300 seconds.

[0139] When KrF excimer laser light, ArF excimer laser light, or EUV light with a wavelength of 13.5 nm is used for exposure of the resist film, a mask for forming a desired pattern is used, and the exposure amount is preferably 1 to 200 mJ / cm. 2 , more preferably 10 to 100 mJ / cm 2 Alternatively, when EB is used, the exposure amount is preferably 1 to 300 μC / cm 2 using a mask for forming a desired pattern or directly. 2 , more preferably 10 to 200 μC / cm 2 Irradiate so that

[0140] In addition to the usual exposure method, the exposure may be performed by an immersion method (liquid immersion exposure) in which the space between the mask and the resist film is immersed in liquid. In this case, a water-insoluble protective film may be used. When performing immersion exposure, it is preferable to interpose a liquid having a refractive index of 1.0 or more between the resist coating film and the projection lens. In this case, the liquid is preferably water. When water is used, a water-insoluble protective film may be formed on the resist film.

[0141] Water-insoluble protective films are used to prevent elution from the resist film and to increase the water sliding property of the film surface, and are roughly divided into two types. One is an organic solvent stripping type that needs to be stripped before alkaline development using an organic solvent that does not dissolve the resist film, and the other is an alkali-soluble type that is soluble in an alkaline developer and removes the protective film together with removing the soluble part of the resist film. The latter is based on a polymer having a 1,1,1,3,3,3-hexafluoro-2-propanol residue that is insoluble in water and soluble in an alkaline developer, and is preferably a material dissolved in an alcohol-based solvent having 4 or more carbon atoms, an ether-based solvent having 8 to 12 carbon atoms, or a mixed solvent thereof. The above-mentioned water-insoluble and alkaline developer-soluble surfactant can also be dissolved in an alcohol-based solvent having 4 or more carbon atoms, an ether-based solvent having 8 to 12 carbon atoms, or a mixed solvent thereof.

[0142] After the exposure, PEB may be performed, for example, by heating on a hot plate at preferably 60 to 150° C. for 1 to 5 minutes, more preferably 80 to 140° C. for 1 to 3 minutes.

[0143] Development can be carried out by a conventional method such as a dip method, a puddle method or a spray method using, for example, a developer such as an alkaline aqueous solution of 0.1 to 5 mass %, preferably 2 to 3 mass %, tetramethylammonium hydroxide (TMAH) or the like, or an organic solvent developer, for 0.1 to 3 minutes, preferably 0.5 to 2 minutes.

[0144] Regarding the developer in the pattern formation method of the present invention, examples of the alkaline aqueous developer include the above-mentioned TMAH and the alkaline aqueous solutions described in paragraphs

[0148] to

[0149] of JP-A-2015-180748. Preferably, it is 2 to 3 mass % tetramethylammonium hydroxide (TMAH).

[0145] Examples of the developer for organic solvent development include 2-octanone, 2-nonanone, 2-heptanone, 3-heptanone, 4-heptanone, 2-hexanone, 3-hexanone, diisobutyl ketone, methylcyclohexanone, acetophenone, methylacetophenone, propyl acetate, butyl acetate, isobutyl acetate, pentyl acetate, butenyl acetate, isopentyl acetate, propyl formate, butyl formate, isobutyl formate, pentyl formate, isopentyl formate, methyl valerate, methyl pentenoate, methyl crotonate, ethyl crotonate, propyl cyclohexanone, ethyl cyclohexanone, propyl ... Examples of the organic solvent that can be used include methyl propionate, ethyl propionate, ethyl 3-ethoxypropionate, methyl lactate, ethyl lactate, propyl lactate, butyl lactate, isobutyl lactate, pentyl lactate, isopentyl lactate, methyl 2-hydroxyisobutyrate, ethyl 2-hydroxyisobutyrate, methyl benzoate, ethyl benzoate, phenyl acetate, benzyl acetate, methyl phenylacetate, benzyl formate, phenylethyl formate, methyl 3-phenylpropionate, benzyl propionate, ethyl phenylacetate, 2-phenylethyl acetate, etc. These organic solvents can be used alone or in combination of two or more.

[0146] As a means for forming a pattern, after forming a resist film, a pure water rinse (post soak) may be performed to extract an acid generator and the like from the film surface or to wash away particles, or a rinse (post soak) may be performed to remove water remaining on the film after exposure.

[0147] Furthermore, a pattern can also be formed by a double patterning method. Examples of double patterning methods include a trench method in which a 1:3 trench pattern is processed by a first exposure and etching, and a 1:3 trench pattern is formed by a second exposure with a shifted position to form a 1:1 pattern, and a line method in which a first base of a 1:3 isolated leave pattern is processed by a first exposure and etching, and a 1:3 isolated leave pattern is processed by a second exposure with a shifted position to form a 1:1 pattern with half the pitch.

[0148] When forming a hole pattern by negative tone development using an organic solvent as a developer, light with the highest contrast can be used by performing exposure using dipole illumination with two line patterns in the X-axis and Y-axis directions. In addition, contrast can be further increased by adding s-polarized illumination to the dipole illumination with two line patterns in the X-axis and Y-axis directions. These pattern formation methods are described in detail in JP 2011-221513 A.

[0149] The developed hole pattern or trench pattern can also be shrunk by thermal flow, RELACS (Resolution Enhancement Lithography Assisted by CHEMICAL Shrink) technology, DSA (Directed Self-Assembly) technology, etc. A shrink agent is applied onto the hole pattern, and crosslinking of the shrink agent occurs on the surface of the resist due to diffusion of an acid catalyst from the resist layer during baking, and the shrink agent adheres to the sidewall of the hole pattern. The bake temperature is preferably 70 to 180°C, more preferably 80 to 170°C, and the bake time is preferably 10 to 300 seconds. Finally, excess shrink agent is removed to shrink the hole pattern.

[0150] According to the pattern forming method of the present invention, by using a resist composition containing the iodonium salt of the present invention, it is possible to easily form a fine pattern that has excellent rectangularity and excellent lithography performance such as MEF, CDU, and LWR. EXAMPLES

[0151] The present invention will be specifically described below with reference to Synthesis Examples, Examples, and Comparative Examples, but the present invention is not limited to the following Examples, etc. In the following Examples, Mw is a polystyrene-equivalent value measured by GPC using tetrahydrofuran (THF) as a solvent.

[0152] [1] Synthesis of intermediates [Synthesis Example 1] Synthesis of anion intermediate (C-1) [ka]

[0153] In a flask, 260.8 g of a 25% by mass aqueous solution of tetramethylammonium hydroxide was added and stirred, and 154.0 g of methyl 3,3,3-trifluoro-2-hydroxy-2-(trifluoromethyl)propionate was added dropwise at room temperature. After the dropwise addition, the mixture was heated to 40° C. and stirred and aged at the same temperature overnight. 19 After confirming the progress of the reaction by F-NMR, 80 g of toluene was added and stirred, and the aqueous layer was separated. The obtained aqueous layer was washed with 80 g of toluene to obtain the desired anion intermediate (C-1) as an aqueous solution (concentration 1.48 mmol / g).

[0154] [2] Synthesis of iodonium salts [Example 1-1] Synthesis of iodonium salt (I-1) [ka]

[0155] 6.3g of diphenyliodonium chloride, 16.2g of an aqueous solution of anion intermediate (C-1), 60g of methylene chloride, 8g of methanol, 12g of 1-pentanol and 16g of pure water were mixed and stirred for 1 hour, and then the organic layer was separated. 1.4g of an aqueous solution of anion intermediate (C-1) and 20g of pure water were added to the obtained organic layer and stirred, and then the organic layer was separated, and the organic layer was washed once with 20g of pure water, three times with 25g of 25% by mass aqueous methanol solution, and once with 20g of pure water. The obtained organic layer was concentrated under reduced pressure to remove methylene chloride, and then 56g of diisopropyl ether was added and stirred to perform crystallization. The obtained solid was filtered, rinsed with diisopropyl ether, and dried under reduced pressure at 40°C to obtain 5.5g of the desired iodonium salt (I-1) (yield: 56%). 1 H-NMR (500MHz, DMSO-d6): δ= 6.34(1H, s), 7.52(4H, m), 7.66(2H, m), 8.24(4H, m) ppm. 19 F-NMR (500MHz, DMSO-d6): δ= -74.6(6F, s) ppm. Time-of-flight mass spectrometry (TOFMS; MALDI) POSITIVE M + 281(C 12 H 10 I + equivalent) NEGATIVE M - 211(C4HF6O3 - equivalent)

[0156] [Example 1-2] Synthesis of iodonium salt (I-2) [ka]

[0157] 8.3 g of a known compound (4-fluorophenyl)phenyliodonium p-toluenesulfonate, 16.8 g of an aqueous solution of anion intermediate (C-1), 63 g of 1-pentanol, 20 g of methanol and 20 g of pure water were mixed and stirred for 4 hours, and then the organic layer was separated. 1.8 g of an aqueous solution of anion intermediate (C-1) and 10 g of pure water were added to the organic layer and stirred, and the organic layer was separated and separated five times, and the organic layer was washed five times with 10 g of pure water. The obtained organic layer was concentrated under reduced pressure to remove the solvent, and then 68 g of diisopropyl ether was added to perform crystallization. The solid was filtered off, rinsed with diisopropyl ether, and then heated and dried under reduced pressure at 40°C to obtain 5.7 g of the desired iodonium salt (I-2) (yield: 61%). 1 H-NMR (500MHz, DMSO-d6): δ= 6.36(1H, s), 7.40(2H, m), 7.52(2H, m), 7.65(1H, m), 8.24(2H, m), 8.31(2H, m) ppm. 19 F-NMR (500MHz, DMSO-d6): δ= -108.3(1F, m), -74.6(6F, s) ppm. Time-of-flight mass spectrometry (TOFMS; MALDI) POSITIVE M + 299(C 12 H9FI + equivalent) NEGATIVE M - 211(C4HF6O3 - equivalent)

[0158] [Example 1-3] Synthesis of iodonium salt (I-3) [ka] 4.3 g of bis(4-tert-butylphenyl)iodonium chloride, 8.1 g of an aqueous solution of anion intermediate (C-1), 50 g of methylene chloride, and 20 g of pure water were mixed and stirred for 1 hour, and then the organic layer was separated. 0.67 g of an aqueous solution of anion intermediate (C-1) and 10 g of pure water were added to the organic layer and stirred, and the organic layer was separated three times, and the organic layer was washed five times with 10 g of pure water. The obtained organic layer was concentrated under reduced pressure to remove the solvent, and then 60 g of diisopropyl ether was added to perform crystallization. The solid was filtered off, rinsed with diisopropyl ether, and then heated and dried under reduced pressure at 45°C, obtaining 5.9 g of the desired iodonium salt (I-3) (yield: 97%). 1 H-NMR (500MHz, DMSO-d6): δ= 1.25(18H, s), 6.34(1H, s), 7.53(4H, m), 8.14(4H, m) ppm. 19 F-NMR (500MHz, DMSO-d6): δ= -74.6(6F, s) ppm. Time-of-flight mass spectrometry (TOFMS; MALDI) POSITIVE M + 393(C 20 H 26 I + equivalent) NEGATIVE M - 211(C4HF6O3 - equivalent)

[0159] [Example 1-4] Synthesis of iodonium salt (I-4) [ka]

[0160] 8.7 g of phenyl[2,4,6-tris(1-methylethyl)phenyl]iodonium p-toluenesulfonate, a known compound, 11.1 g of an aqueous solution of anion intermediate (C-1), 40 g of methylene chloride, and 10 g of pure water were mixed and stirred for 1 hour, after which the organic layer was separated. 1.0 g of an aqueous solution of anion intermediate (C-1) and 20 g of pure water were added to the organic layer and stirred, and the organic layer was separated and separated 7 times, and the organic layer was washed 5 times with 20 g of pure water. The obtained organic layer was concentrated under reduced pressure to remove the solvent, and then 60 g of tert-butyl methyl ether was added to perform crystallization. The solid was filtered off, rinsed with tert-butyl methyl ether, and then heated and dried under reduced pressure at 50°C to obtain 4.9 g of the desired iodonium salt (I-4) (yield: 52%). 1 H-NMR (500MHz, DMSO-d6): δ= 1.20(6H, d), 1.21(12H, d), 2.96(1H, m), 3.37(2H, m), 6.38(1H, s), 7.30(2H, s), 7.52(2H, m), 7.62(1H, m), 7.91(2H, m) ppm. 19 F-NMR (500MHz, DMSO-d6): δ= -74.6(6F, s) ppm. Time-of-flight mass spectrometry (TOFMS; MALDI) POSITIVE M + 407(C 21 H 28 I + equivalent) NEGATIVE M - 211(C4HF6O3 - equivalent)

[0161] [Example 1-5] Synthesis of iodonium salt (I-5) [ka]

[0162] 7.9 g of 3,3,3-trifluoro-2-hydroxy-2-methylpropionic acid and 34.1 g of pure water were added to a flask and stirred, and 8.0 g of 25% by mass aqueous sodium hydroxide solution was added dropwise under ice cooling. After the dropwise addition, the mixture was stirred at room temperature for 20 minutes to obtain an aqueous solution of sodium 3,3,3-trifluoro-2-hydroxy-2-methylpropionate (concentration: 1 mmol / g, hereinafter referred to as aqueous solution A). 4.3 g of bis(4-tert-butylphenyl)iodonium chloride, 40 g of methylene chloride, and 30 g of aqueous solution A were mixed and stirred for 30 minutes, after which the organic layer was separated. 10 g of aqueous solution A was added to the obtained organic layer, and the mixture was stirred and then the organic layer was separated. The organic layer was washed four times with 15 g of pure water. The obtained organic layer was concentrated under reduced pressure, and the methylene chloride was removed to precipitate a solid. The precipitated solid was dispersed in 30 g of diisopropyl ether, stirred for 1 hour, filtered, and rinsed with diisopropyl ether. The solid was heated and dried under reduced pressure at 50°C to obtain 4.9 g of the desired iodonium salt (I-5) (yield: 88%). 1 H-NMR (500MHz, DMSO-d6): δ= 1.19(3H,s), 1.24(18H, s), 5.59(1H, s), 7.51(4H, m), 8.13(4H, m) ppm. 19 F-NMR (500MHz, DMSO-d6): δ= -78.5(3F, s) ppm. Time-of-flight mass spectrometry (TOFMS; MALDI) POSITIVE M + 393(C 20 H 26 I + equivalent) NEGATIVE M - 157(C4H4F3O3 - equivalent)

[0163] [Examples 1-6 to 1-12] Synthesis of iodonium salts (I-6) to (I-12) Instead of the raw material ester (methyl 3,3,3-trifluoro-2-hydroxy-2-(trifluoromethyl)propionate) or raw material carboxylic acid (3,3,3-trifluoro-2-hydroxy-2-methylpropionic acid), the corresponding raw material ester or raw material carboxylic acid was used, and the corresponding iodonium cation was used to obtain the following iodonium salts (I-6) to (I-12) in the same manner as in the above-mentioned Examples. The anion raw material and the cation raw material can be commercially available products, or can be synthesized by known methods. [ka]

[0164] [3] Synthesis of base resin [Synthesis Example 2-1] Synthesis of Polymer P-1 Under a nitrogen atmosphere, 22 g of 1-tert-butylcyclopentyl methacrylate, 17 g of 2-oxotetrahydrofuran-3-yl methacrylate, 0.48 g of V-601 (manufactured by Wako Pure Chemical Industries, Ltd.), 0.41 g of 2-mercaptoethanol, and 50 g of methyl ethyl ketone were placed in a flask to prepare a monomer-polymerization initiator solution. 23 g of methyl ethyl ketone was placed in another flask under a nitrogen atmosphere, and the mixture was heated to 80° C. with stirring, and the monomer-polymerization initiator solution was then dropped over 4 hours. After the dropwise addition, the temperature of the polymerization liquid was kept at 80° C. and the mixture was stirred for 2 hours, and then cooled to room temperature. The obtained polymerization liquid was dropped into 640 g of vigorously stirred methanol, and the precipitated polymer was filtered off. The polymer was washed twice with 240 g of methanol, and then vacuum dried at 50° C. for 20 hours to obtain 36 g of white powdery polymer P-1 (yield 90%). Analysis by GPC revealed that Mw was 8,200 and Mw / Mw was 1.63. [ka]

[0165] [Synthesis Examples 2-2 to 2-10] Synthesis of Polymers P-2 to P-10 The following polymers P-2 to P-10 were produced in the same manner as in Synthesis Example 2-1, except that the types and compounding ratios of the respective monomers were changed.

[0166] The compositions of the produced polymers P-1 to P-10 are shown in the following Table 1. In Table 1, the introduction ratio indicates a molar ratio. The structures of the units in Table 1 are shown in the following Tables 2, 3, and 4.

[0167] [Table 1]

[0168] [Table 2]

[0169] [Table 3]

[0170] [Table 4]

[0171] [4] Preparation of resist composition [Examples 2-1 to 2-24, Comparative Examples 1-1 to 1-12] Iodonium salts I-1 to I-12, polymers P-1 to P-10, photoacid generators PAG-A to PAG-C, quenchers Q-1 to Q-8, and alkali-soluble surfactant SF-1 were dissolved in a solvent containing 0.01% by mass of surfactant A (manufactured by Omnova), and the resulting solution was filtered through a 0.2 μm Teflon (registered trademark) filter to prepare resist compositions. The compositions of the prepared resist compositions are shown in Tables 5 and 6 below.

[0172] In Tables 5 and 6, the quenchers Q-1 to Q-8, the solvents, the photoacid generators PAG-A to PAG-C, and the alkali-soluble surfactant SF-1 are as follows.

[0173] Quencher Q-1: 1-(tert-butoxycarbonyl)-4-hydroxypiperidine [ka]

[0174] Q-2: 2,6-diisopropylaniline [ka]

[0175] Q-3: Triphenylsulfonium 2-[(adamantane-1-carbonyl)oxy]-ethylsulfonate [ka]

[0176] Q-4: Diphenyliodonium-2-carboxylate [ka]

[0177] Q-5: Triphenylsulfonium 3,3,3-trifluoro-2-hydroxy-2-trifluoromethylpropiolate [ka]

[0178] Q-6: Bis(4-tert-butylphenyl)phenylsulfonium 3,3,3-trifluoro-2-hydroxy-2-trifluoromethylpropiolate [ka]

[0179] Q-7: Triphenylsulfonium adamantanecarboxylate [ka]

[0180] Q-8: Triphenylsulfonium salicylate [ka]

[0181] ·solvent PGMEA: Propylene glycol monomethyl ether acetate GBL: gamma-butyrolactone

[0182] Photoacid generator PAG-A: Triphenylsulfonium 2-[(adamantane-1-carbonyl)oxy]-1,1,3,3,3-pentafluoropropane-1-sulfonate [ka]

[0183] PAG-B: Triphenylsulfonium 2-[(adamantane-1-carbonyl)oxy]-2-trifluoromethyl-3,3,3-trifluoropropane-1-sulfonate [ka]

[0184] PAG-C: 4-[(2-methoxyethoxy)naphthalene]-1-tetrahydrothiophenium 2-[(adamantane-1-carbonyl)oxy]-1,1-difluoroethanesulfonate [ka]

[0185] Alkaline-soluble surfactant SF-1: Poly(2,2,3,3,4,4,4-heptafluoro-1-isobutyl-1-butyl methacrylate, 9-(2,2,2-trifluoro-1-trifluoroethyloxycarbonyl)-4-oxatricyclo[4.2.1.0 3,7]nonane-5-on-2-yl) Mw=7,700 Mw / Mn=1.82 [ka]

[0186] Surfactant A: 3-methyl-3-(2,2,2-trifluoroethoxymethyl)oxetane-tetrahydrofuran-2,2-dimethyl-1,3-propanediol copolymer (Omnova) (see formula below) [ka] a:(b+b'):(c+c')=1:4-7:0.01-1 (molar ratio) Mw=1,500

[0187] [Table 5]

[0188] [Table 6]

[0189] [5] ArF Exposure Patterning Evaluation (1) - Hole Pattern Evaluation [Examples 3-1 to 3-18, Comparative Examples 2-1 to 2-7] The resist compositions of the present invention (R-1 to R-7, R-11 to R-21) and the resist compositions for comparative examples (R-25 to R-31) were spin-coated onto a substrate for a trilayer process having a 200 nm spin-on carbon film ODL-101 manufactured by Shin-Etsu Chemical Co., Ltd. and a 35 nm thick silicon-containing spin-on hard mask SHB-A940 (silicon content of 43% by mass) formed thereon, and baked at 100° C. for 60 seconds using a hot plate to form a resist film with a thickness of 100 nm. In response to this, an ArF immersion excimer laser stepper (Nikon Corporation, NSR-610C, NA1.30, σ0.98 / 0.78, dipole aperture 20°, azimuthally polarized illumination, 6% halftone phase shift mask, dipole illumination) was used to perform a first exposure using a mask with lines arranged in the X direction with a pitch of 80 nm and a line width of 40 nm on the wafer, followed by a second exposure using a mask with lines arranged in the Y direction with a pitch of 80 nm and a line width of 40 nm on the wafer, and then PEB was applied for 60 seconds after exposure, after which butyl acetate was ejected from the development nozzle while rotating at 30 rpm for 3 seconds, followed by static paddle development for 27 seconds. Water was used as the immersion liquid.

[0190] [Sensitivity evaluation] The resist pattern was observed with a CD-SEM (CG-5000) manufactured by Hitachi High-Technologies Corporation, and the optimal exposure dose Eop (mJ / cm) was determined as the exposure dose that results in a hole diameter of 40 nm at a pitch of 80 nm. 2 ) was decided.

[0191] [Mask Error Factor (MEF) evaluation] While keeping the mask pitch fixed, the line width of the mask was changed and irradiated with the optimum exposure (Eop) in the sensitivity evaluation to form a pattern. From the changes in the mask line width and the pattern space width, the MEF value was calculated using the following formula. The closer this value is to 1, the better the performance. MEF = (pattern space width / mask line width) - b (b: constant)

[0192] [Dimensional Uniformity (CDU) Evaluation] The obtained hole pattern was observed with a Hitachi High-Technologies Corporation CD-SEM (CG-5000), and the hole diameter was measured at 125 points. The standard deviation (σ) calculated from the results was tripled (3σ) to obtain CDU. The smaller the CDU value, the better the dimensional uniformity.

[0193] The evaluation results are shown in Table 7.

[0194] [Table 7]

[0195] From the results shown in Table 7, it was found that when a hole pattern was formed by organic solvent development using the resist composition of the present invention, it was found to be excellent in MEF and CDU. From the above, it was made clear that the resist composition of the present invention is useful in an organic solvent development process.

[0196] [6] ArF Exposure Patterning Evaluation (2) - Line and Space Evaluation [Examples 4-1 to 4-24, Comparative Examples 3-1 to 3-12] The resist compositions of the present invention (R-1 to R-24) and the resist compositions for comparative examples (R-25 to R-36) were spin-coated onto a substrate for a trilayer process having a 200 nm spin-on carbon film ODL-101 manufactured by Shin-Etsu Chemical Co., Ltd. and a 35 nm thick silicon-containing spin-on hard mask SHB-A940 (silicon content of 43% by mass) formed thereon, and baked at 100° C. for 60 seconds using a hot plate to form a resist film with a thickness of 100 nm. This was subjected to pattern exposure using an ArF immersion excimer laser scanner (Nikon Corporation, NSR-610C, NA1.30, σ0.98 / 0.78, 4 / 5 annular illumination) using a 6% halftone phase shift mask with a wafer-on-wafer dimension of pitch 100 nm and space width 50 nm, and PEB was applied for 60 seconds after exposure, after which a 2.38 mass % TMAH aqueous solution was ejected from the development nozzle while rotating at 30 rpm for 3 seconds, and then static paddle development was performed for 27 seconds. As a result, the exposed portion was dissolved in the developer, and a line and space pattern (hereinafter referred to as LS pattern) with a space width of 50 nm and a pitch of 100 nm was obtained. Water was used as the immersion liquid.

[0197] [Sensitivity evaluation] The obtained LS pattern was observed with a CD-SEM (CG-5000) manufactured by Hitachi High-Technologies Corporation, and the exposure dose that gave an LS pattern with a space width of 50 nm and a pitch of 100 nm was determined as the optimal exposure dose Eop (mJ / cm 2 ) was decided.

[0198] [MEF Rating] While keeping the mask pitch fixed, the line width of the mask was changed and irradiated with the optimum exposure (Eop) in the sensitivity evaluation to form a pattern. From the changes in the mask line width and the pattern space width, the MEF value was calculated using the following formula. The closer this value is to 1, the better the performance. MEF = (pattern space width / mask line width) - b (b: constant)

[0199] [LWR rating] The LS pattern obtained by irradiating with the optimal exposure dose Eop was measured at 10 points in the longitudinal direction of the space width using a CD-SEM (CG-5000) manufactured by Hitachi High-Technologies Corporation, and the LWR was calculated as three times the standard deviation (σ). The smaller this value, the less roughness and the more uniform the space width pattern.

[0200] [Shape evaluation] The LS pattern shape obtained by irradiation at the optimum exposure dose Eop was observed with a CD-SEM (CG-5000) manufactured by Hitachi High-Technologies Corporation, and judged as good or bad according to the following criteria. Good: The pattern shape is rectangular and the side walls are highly perpendicular. Defective: A tapered shape with a large inclination of the pattern sidewall, or a top rounding shape due to top loss.

[0201] The evaluation results are shown in Table 8.

[0202] [Table 8]

[0203] The results shown in Table 8 indicate that the resist composition of the present invention is excellent in shape (rectangularity) and also in MEF and LWR in positive pattern formation by alkaline aqueous solution development. These results suggest that the resist composition of the present invention is useful in an alkaline aqueous solution development process.

[0204] [7] EB exposure patterning evaluation - Line and space evaluation [Examples 5-1 to 5-7, Comparative Examples 4-1 to 4-5] The resist compositions of the present invention (R-7 to R-10, R-22 to R-24) and the resist compositions for comparative examples (R-32 to R-36) were spin-coated on a Si substrate on which a 60-nm-thick anti-reflective film DUV-42 manufactured by Nissan Chemical Industries, Ltd. had been formed, and the substrate was pre-baked at 105°C for 60 seconds using a hot plate to prepare a resist film with a thickness of 50 nm. The resist film was exposed to light using an EB lithography device manufactured by Elionix (ELS-F125, accelerating voltage 125 kV), and PEB was performed on a hot plate at the temperature shown in Table 9 for 60 seconds. The resist film was developed with a 2.38 mass% TMAH aqueous solution for 30 seconds to form a positive resist pattern. As a result, the exposed portion was dissolved in the developer to obtain an LS pattern with a space width of 45 nm and a pitch of 90 nm.

[0205] [Sensitivity evaluation] The obtained LS pattern was observed with a CD-SEM (S-9380) manufactured by Hitachi High-Technologies Corporation, and the optimal exposure dose Eop (μC / cm) was determined as the exposure dose that would give an LS pattern with a space width of 45 nm and a pitch of 90 nm. 2 ) was decided.

[0206] [LWR rating] The LS pattern obtained by irradiating with the optimal exposure dose Eop was measured at 10 points in the longitudinal direction of the space width using a CD-SEM (S-9380) manufactured by Hitachi High-Technologies Corporation, and the LWR was calculated as three times the standard deviation (σ). The smaller this value, the less roughness and the more uniform the space width pattern.

[0207] [Shape evaluation] The LS pattern shape obtained by irradiation at the optimum exposure dose Eop was observed with a CD-SEM (S-9380) manufactured by Hitachi High-Technologies Corporation, and judged as good or bad according to the following criteria. Good: The pattern shape is rectangular and the side walls are highly perpendicular. Defective: A tapered shape with a large inclination of the pattern sidewall, or a top loss due to top loss Bonding shape.

[0208] The evaluation results are shown in Table 9.

[0209] [Table 9]

[0210] From the results shown in Table 9, it was found that the resist composition of the present invention is excellent in sensitivity, shape (rectangularity), and LWR in positive pattern formation by alkaline aqueous solution development using EB lithography. In Examples 5-1 to 5-7, EB is used for exposing the resist film, but even when short-wavelength radiation such as EUV is used, the basic resist characteristics are similar, and it is also known that there is a correlation between EB exposure evaluation and EUV exposure evaluation. Therefore, it can be inferred that the resist composition of the present invention is excellent in sensitivity, shape, and LWR even in the case of EUV exposure.

Claims

1. A quencher consisting of an iodonium salt represented by the following formula (1): A base resin containing a polymer containing a repeating unit represented by the following formula (a), a repeating unit derived from hydroxystyrene, and at least one repeating unit selected from the repeating units represented by the following formulas (c1) to (c4) (however, the base resin does not contain a repeating unit having an oxirane ring); and Organic Solvents wherein the base resin is also a photoacid generator, and no other photoacid generator is contained. 【Chemistry 1】 (In the formula, R f1 and R f2 are each independently a hydrogen atom, a fluorine atom, or a linear or branched monovalent hydrocarbon group having 1 to 4 carbon atoms which may contain a fluorine atom, and at least one of them is a fluorine atom, or a linear or branched monovalent hydrocarbon group having 1 to 4 carbon atoms which contains a fluorine atom. Ar 1 and Ar 2 are each independently an aryl group having 6 to 40 carbon atoms which may contain a heteroatom. 1 and Ar 2 may be bonded to each other to form a ring together with the iodine atom to which they are bonded.) 【Chemistry 2】 (In the formula, R A is a hydrogen atom, a fluorine atom, a methyl group or a trifluoromethyl group. Z A is a single bond, a phenylene group, a naphthylene group, or (main chain)-C(=O)-O-Z'-, where Z' is an alkanediyl group having 1 to 10 carbon atoms which may contain a hydroxy group, an ether bond, an ester bond, or a lactone ring, or a phenylene group or a naphthylene group. A is an acid labile group. 【Chemistry 3】 (In the formula, R A is a hydrogen atom, a fluorine atom, a methyl group or a trifluoromethyl group. L 1 represents a single bond, a phenylene group, -O-L 11 -, -C(=O)-OL 11 - or -C(=O)-NH-L 11 - represents L 11 represents an alkanediyl group having 1 to 20 carbon atoms, an alkenediyl group having 2 to 20 carbon atoms, or a phenylene group, which may contain a heteroatom. L 2 and L 3 are each independently a single bond or a divalent hydrocarbon group having 1 to 20 carbon atoms which may contain a heteroatom. L 4 represents a single bond, a methylene group, an ethylene group, a phenylene group, a fluorinated phenylene group, -O-L 41 -, -C(=O)-OL 41 Or -C(=O)-NH-L 41 - is. 41 is an optionally substituted phenylene group. R 11 ~R 21 are each independently a monovalent hydrocarbon group having 1 to 20 carbon atoms which may contain a heteroatom. 1 , R 11 and R 12 Any two of R may be bonded to each other to form a ring together with the sulfur atom to which they are attached, 13 , R 14 and R 15 Any two of R 16 , R 17 and R 18 Any two of the above, or R 19 , R 20 and R 21 Any two of may be bonded to each other to form a ring together with the sulfur atom to which they are attached. Xc - represents a non-nucleophilic counter ion. A 1 is a hydrogen atom or a trifluoromethyl group. n 1 is 0 or 1, but L 2 When n is a single bond, it is 0. 2 is 0 or 1, but L 3 is a single bond, the value is 0.)

2. The resist composition according to claim 1, wherein the polymer comprises at least one repeating unit selected from the following formulae A-1 to A-3, a repeating unit derived from hydroxystyrene, and at least one repeating unit selected from the following formulae C-1 to C-3: 【Chemistry 4】

3. 3. The resist composition according to claim 1, further comprising an amine compound.

4. 4. The resist composition according to claim 1, further comprising a surfactant that is insoluble or slightly soluble in water but soluble in an alkaline developer, and / or a surfactant that is insoluble or slightly soluble in water and an alkaline developer.

5. A pattern forming method comprising the steps of: forming a resist film on a substrate using the resist composition according to any one of claims 1 to 4; exposing the resist film to KrF excimer laser light, ArF excimer laser light, an electron beam or extreme ultraviolet light; and developing the exposed resist film using a developer.

6. 6. The method for forming a pattern according to claim 5, wherein an aqueous alkaline solution is used as a developer to dissolve the exposed areas and to obtain a positive pattern in which the unexposed areas do not dissolve.

7. 6. The method for forming a pattern according to claim 5, wherein an organic solvent is used as a developer to dissolve the unexposed areas and to obtain a negative pattern in which the exposed areas do not dissolve.

8. The organic solvent is 2-octanone, 2-nonanone, 2-heptanone, 3-heptanone, 4-heptanone, 2-hexanone, 3-hexanone, diisobutyl ketone, methylcyclohexanone, acetophenone, methylacetophenone, propyl acetate, butyl acetate, isobutyl acetate, pentyl acetate, butenyl acetate, isopentyl acetate, propyl formate, butyl formate, isobutyl formate, pentyl formate, isopentyl formate, methyl valerate, methyl pentenoate, methyl crotonate, ethyl crotonate, methyl propionate, ethyl propionate, or ethyl methacrylate.

8. The pattern forming method according to claim 7, wherein the lactate is at least one selected from the group consisting of ethyl, ethyl 3-ethoxypropionate, methyl lactate, ethyl lactate, propyl lactate, butyl lactate, isobutyl lactate, pentyl lactate, isopentyl lactate, methyl 2-hydroxyisobutyrate, ethyl 2-hydroxyisobutyrate, methyl benzoate, ethyl benzoate, phenyl acetate, benzyl acetate, methyl phenylacetate, benzyl formate, phenylethyl formate, methyl 3-phenylpropionate, benzyl propionate, ethyl phenylacetate and 2-phenylethyl acetate.

9. 9. The method for forming a pattern according to claim 5, wherein the exposure is an immersion exposure performed by interposing a liquid having a refractive index of 1.0 or more between the resist film and a projection lens.

10. 10. The pattern forming method according to claim 9, further comprising the step of coating a protective film on the resist film, and carrying out immersion exposure by placing the liquid between the protective film and a projection lens.

Citation Information

Patent Citations

  • Noise elimination method for picture process

    JP1980056765A

  • Chemically amplifying resist composition

    JP1999295887A

  • Resist and method for forming resist pattern

    JP1999327143A

  • Pattern forming method and resist composition

    JP2013076990A

  • Pattern forming method and resist composition

    JP2014145809A