Surge protection device and its manufacturing method

The surge protection element with dielectric film-covered and uncovered regions, combined with an oxide film removal process, stabilizes discharge starting voltage, addressing individual differences and temporal changes, ensuring consistent surge protection.

JP7608883B2Active Publication Date: 2025-01-07MITSUBISHI MATERIALS CORP
View PDF 13 Cites 0 Cited by

Patent Information

Application Number
JP2021038863
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-03-11
Publication Date
2025-01-07
Estimated Expiration
2041-03-11

AI Technical Summary

Technical Problem

Conventional surge protection elements exhibit significant individual differences in discharge starting voltage and temporal changes in this voltage, leading to instability.

Method used

The surge protection element features a configuration with opposing discharge electrodes having regions covered and uncovered by a dielectric film, along with an oxide film removal section, and a manufacturing method involving application of a dielectric material and aging process to stabilize the discharge starting voltage.

Benefits of technology

This configuration and method result in a stable discharge starting voltage by concentrating the electric field and reducing variations, enhancing the element's responsiveness to surges.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007608883000001
    Figure 0007608883000001
  • Figure 0007608883000002
    Figure 0007608883000002
  • Figure 0007608883000003
    Figure 0007608883000003
Patent Text Reader

Abstract

To provide a surge protection element capable of suppressing individual differences in discharge start voltages and changes in discharge start voltages over time, and a method for manufacturing the same.SOLUTION: A surge protection element includes a pair of discharge electrodes spaced apart from each other and facing each other, and an insulating tube in which the pair of discharge electrodes are arranged at both ends and at least the mutually facing surfaces of the pair of discharge electrodes are sealed inside together with discharge control gas, and the discharge electrode includes an electrode body 4 made of metal and having the facing surface, and a region A covered with a dielectric film 5 and a region B not covered with the dielectric film 5 are provided on the facing surface.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a surge protection element used to protect various devices from surges generated by lightning strikes and the like, and to a method for manufacturing the same. [Background technology]

[0002] Surge protection elements are connected to parts of electronic equipment for communication devices such as telephones, facsimiles, and modems that are susceptible to electric shock from abnormal voltages (surge voltages) such as lightning surges and static electricity, in order to prevent destruction by heat damage or fire of the electronic equipment or the printed circuit board on which this equipment is mounted, caused by abnormal voltages, such as connections to communication lines, power lines, antennas, and CRT drive circuits.

[0003] Conventionally, as a surge protection element with good responsiveness, a surge protection element using a surge absorption element having a so-called microgap has been proposed, as shown in Patent Document 1, for example. This surge protection element is a surge absorber in which a microgap is formed on the peripheral surface of a ceramic member, which is a cylindrical insulating member covered with a conductive coating, and a surge absorption element having a pair of cap electrodes on both ends of the ceramic member is housed in a glass tube together with a discharge control gas, and sealing electrodes (so-called slug leads) having lead wires are sealed to both ends of the cylindrical glass tube by high-temperature heating. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] Patent No. 3265874 Summary of the Invention [Problem to be solved by the invention]

[0005] The above conventional techniques still have the following problems. The above-mentioned conventional surge protection elements have the disadvantage that the discharge start voltage varies greatly from one element to another and also changes over time.

[0006] The present invention has been made in consideration of the above-mentioned problems, and has an object to provide a surge protection element capable of suppressing individual differences in discharge start voltage and changes in discharge start voltage over time, and a manufacturing method thereof. [Means for solving the problem]

[0007] In order to solve the above problems, the present invention employs the following configuration: That is, a surge protection element of a first invention includes a pair of discharge electrodes arranged facing each other with a gap therebetween, and an insulating tube having the pair of discharge electrodes at both ends and sealing at least the opposing surfaces of the pair of discharge electrodes together with a discharge control gas inside, the discharge electrodes include an electrode body formed of a metal and having the opposing surfaces, and the opposing surfaces are provided with an area covered with a dielectric film and an area not covered with the dielectric film.

[0008] In this surge protection element, the opposing surfaces of the electrode body are provided with a region covered with a dielectric film and a region not covered with the dielectric film. Therefore, in the region partially covered with the dielectric film, the metal of the opposing surface is less likely to oxidize, and the dielectric film Outer periphery The electric field is concentrated in the vicinity due to the lines of electric force gathering, making it easier to discharge, and a stable discharge start voltage can be obtained.

[0009] A surge protection element according to a second aspect of the present invention is the surge protection element according to the first aspect of the present invention, In an area not covered with the dielectric film, an oxide film of a metal constituting the inside of the electrode body is formed on the opposing surface and exposed, the oxide film of the metal of the opposing surface is diffused and contained in the outer peripheral edge of the dielectric film, and an oxide film removal portion where the oxide film of the metal of the opposing surface has been removed is formed on the opposing surface side of the outer peripheral edge of the dielectric film. It is characterized by: That is, in this surge protection device, An oxide film removal portion is formed on the opposing surface side of the outer periphery of the dielectric film by removing the oxide film of the metal on the opposing surface. Therefore, the electric field is further concentrated at the oxide film-removed portion where the oxide film on the opposing surface has been removed, and a more stable discharge start voltage can be obtained.

[0010] A surge protection element according to a third invention is the surge protection element according to the first or second invention, characterized in that the dielectric material of the dielectric film is sodium silicate or potassium silicate.

[0011] A manufacturing method of a surge protection element according to the fourth invention is a manufacturing method of a surge protection element according to any one of the first to third inventions, characterized in that it includes a dielectric film formation step of applying an aqueous solution containing a dielectric material to opposing surfaces of a pair of discharge electrodes arranged opposite each other with a gap therebetween and drying the aqueous solution, thereby providing an area on the opposing surfaces that is covered with a dielectric film and an area that is not covered with the dielectric film. In other words, the manufacturing method of this surge protection element includes a dielectric film formation process in which an aqueous solution containing a dielectric material is applied to the opposing surfaces of a pair of discharge electrodes arranged opposite each other with a gap between them, and then dried, to provide areas on the opposing surfaces that are covered with a dielectric film and areas that are not covered with the dielectric film.Therefore, by applying and drying the aqueous solution containing the dielectric, it is possible to easily provide areas that are covered with a dielectric film and areas that are not covered with a dielectric film.

[0012] The manufacturing method of a surge protection element according to the fifth invention is characterized in that, in the fourth invention, after the dielectric film forming process, it includes a sealing process in which the pair of discharge electrodes are arranged on both ends and at least the opposing surfaces of the pair of discharge electrodes are sealed inside an insulating tube together with a discharge control gas, and an aging process in which a DC voltage or an AC voltage is applied between the pair of discharge electrodes after the sealing process. That is, the manufacturing method of this surge protection element includes an aging step in which a DC or AC voltage is applied between a pair of discharge electrodes, so that aging causes electrons to impinge on the metal oxide film on the opposing surface, accelerating the removal of the oxide film, and also aging the dielectric film on the opposing surface. Outer periphery Directly below (Opposite surface of outer periphery) The metal in the insulating tube is activated, and an oxide film-removed portion is formed where the oxide film is removed. Furthermore, excess oxygen in the insulating tube is included in the dielectric film by aging, so that a more stable discharge starting voltage can be obtained.

[0013] The sixth invention relates to a method for manufacturing a surge protection element according to the fourth or fifth invention, and is characterized in that the aqueous solution is an aqueous solution of water glass containing sodium silicate or potassium silicate as the dielectric material. That is, in the manufacturing method of this surge protection element, since the aqueous solution is an aqueous solution of water glass containing sodium silicate or potassium silicate as a dielectric material, it is easy to apply and dry, and a dielectric film of sodium silicate or potassium silicate can be obtained. Effect of the Invention

[0014] According to the present invention, the following effects are obtained. That is, in the surge protection element according to the present invention, the opposing surfaces of the electrode body are provided with a region covered with a dielectric film and a region not covered with the dielectric film, so that the metal of the opposing surface is less likely to oxidize in the region covered with the dielectric film, and the dielectric film Outer periphery The electric field is concentrated in the vicinity due to the lines of electric force gathering, making it easier to discharge, and a stable discharge start voltage can be obtained. Furthermore, the manufacturing method of the surge protection element of the present invention includes a dielectric film formation process in which an aqueous solution containing a dielectric material is applied to the opposing surfaces of a pair of discharge electrodes arranged opposite each other with a gap therebetween and then dried, thereby providing an area on the opposing surfaces that is covered with a dielectric film and an area that is not covered with the dielectric film.Therefore, the application and drying of the aqueous solution containing the dielectric makes it possible to easily provide an area covered with a dielectric film and an area not covered with a dielectric film. [Brief description of the drawings]

[0015] [Figure 1] 1 is a front view of a surge protection element with an insulating tube cut away, showing the surge protection element in a first embodiment of the surge protection element and the manufacturing method thereof according to the present invention. [Diagram 2] FIG. 2 is a plan view showing a schematic view of opposing surfaces of an electrode body in the first embodiment. [Diagram 3] FIG. 2 is a perspective view illustrating a dielectric film forming step in the method for manufacturing the surge protection element in the first embodiment. [Figure 4] FIG. 11 is a front view of a surge protection element with an insulating tube cut away, showing the surge protection element in a second embodiment of the surge protection element and the manufacturing method thereof according to the present invention. [Diagram 5]4 is a SEM composition image showing the opposing surfaces of electrode bodies in an embodiment of a surge protection element and a manufacturing method thereof according to the present invention. [Figure 6] 1 is a graph showing the change over time in discharge start voltage Vs of a comparative example (a) and an example of the present invention (b) after aging. [Figure 7] 4 is a graph showing insulation resistance (IR) of a comparative example (a) and an example (b) of a surge protection element and a manufacturing method thereof according to the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0016] A first embodiment of a surge protection element and a manufacturing method thereof according to the present invention will be described below with reference to Fig. 1 to Fig. 3. Note that in each drawing used in the following description, the scale is appropriately changed so that each component is sized to be recognizable or easily recognizable.

[0017] As shown in Figures 1 and 2, the surge protection element 1 of this embodiment includes a pair of discharge electrodes 2 arranged opposite each other with a gap between them, and an insulating tube 3 having the pair of discharge electrodes 2 at both ends and sealing at least the opposing surfaces 4a of the pair of discharge electrodes 2 together with a discharge control gas inside. The discharge electrode 2 includes an electrode body 4 made of metal and having an opposing surface 4a.

[0018] As shown in FIG. 2, the opposing surface 4a has an area A covered with the dielectric film 5 and an area B not covered with the dielectric film 5. That is, in the region B not covered with the dielectric film 5, the metal constituting the inside of the electrode body 4, the metal film formed on the opposing surface 4a, and the oxide film thereof are exposed. In this embodiment, a copper (Cu) film is formed on the opposing surface 4a of the electrode body 4, and a copper oxide film (Cu 2 O, CuO) is formed thinly.

[0019] The dielectric film 5 Outer periphery The metal oxide film (Cu 2O, CuO), and the dielectric film 5 on the opposing surface 4a Outer periphery Directly below (Opposite surface of outer periphery) The metal oxide film (Cu 2 Oxide film-removed portion 5a is formed from the oxide film (O, CuO) removed. The dielectric material of the dielectric film 5 is sodium silicate. Potassium silicate may also be used as the dielectric material.

[0020] The surge protection element 1 of this embodiment also includes a columnar or cylindrical insulating member 6 having a conductive coating 6a formed on its peripheral surface in parts separated by a discharge gap G at the axial center. The discharge electrodes 2 are disposed on both ends of an insulating member 6 so as to face each other via metal caps 7, which are conductive members. The insulating member 6 is made of a ceramic material such as a mullite sintered body, and has a conductive coating 6a formed on its surface by a thin film formation technique such as physical vapor deposition (PVD) or chemical vapor deposition (CVD). 2 etc. are being formed.

[0021] The discharge gap G is formed by irradiating the axial center of the conductive coating 6a with laser light from a YAG laser along the peripheral surface of the insulating member 6, thereby dividing the conductive coating 6a. The pair of metal caps 7 are formed from a metal such as copper or stainless steel that has a lower hardness and is plastically deformable than the insulating member 6. The pair of metal caps 7 are engaged with both ends of the insulating member 6, respectively, and their opposing surfaces, together with the inner surface of the discharge electrode 2, form the main discharge surfaces.

[0022] The electrode body 4 of the discharge electrode 2 is a sealed electrode having a metal surface of an Fe (iron)-Ni (nickel) alloy or the like coated with copper and copper oxide, and is disk-shaped or cylindrical. One surface of the electrode body 4 is in contact with a metal cap 7, and a lead wire 8 is welded to the other surface. The lead wire 8 is made of a copper-clad steel wire or the like. That is, the discharge electrode 2 having the lead wire 8 attached to the electrode body 4 is a so-called slug lead.

[0023] The insulating tube 3 is made of soft glass such as lead glass or soda-lime glass and has a cylindrical shape. The outer circumferential surface of the discharge electrode 2 is fused to the inner circumferential surface of the insulating tube 3 near both ends of the insulating tube 3. The discharge control gas is a sealing gas whose composition is adjusted so that electrical characteristics such as the discharge start voltage are set to desired values, and is selected from the group consisting of He, Ar, Ne, Xe, and SF. 6 , CO 2 , C 3 F 8 , C 2 F 6 , C.F. 4 , H 2 and inert gases such as mixtures of these. In this embodiment, Ar is used as the discharge control gas.

[0024] Next, a method for manufacturing the surge protection device 1 of this embodiment will be described. The manufacturing method of the surge protection element 1 of this embodiment includes a dielectric film formation step of applying an aqueous solution L containing a dielectric material to opposing surfaces 4a of a pair of discharge electrodes 2 arranged opposite each other with a gap therebetween, as shown in FIG. 3, and drying the aqueous solution L, thereby providing an area A covered with a dielectric film 5 and an area B not covered with the dielectric film 5 on the opposing surfaces 4a. In addition, the manufacturing method of the surge protection element of this embodiment includes, after the dielectric film forming process, a sealing process in which a pair of discharge electrodes 2 are arranged on both ends and at least the opposing surfaces 4 a of the pair of discharge electrodes 2 are sealed inside the insulating tube 3 together with a discharge control gas, and an aging process in which a DC voltage or an AC voltage is applied between the pair of discharge electrodes 2 after the sealing process.

[0025] The aqueous solution L is an aqueous solution of water glass containing sodium silicate as a dielectric material. Note that the aqueous solution L may be an aqueous solution of potassium water glass containing potassium silicate as a dielectric material. In this embodiment, a dilute solution having a weight of, for example, 5 to 50 times that of water glass is used as the aqueous solution L. Since water glass is used as the dilute solution, water droplets can be applied and attached to the opposing surface 4a in almost the same manner as handling water. When applying the aqueous solution L to the facing surface 4a, a dropper or the like is used, but a dispenser or the like may also be used.

[0026] The applied aqueous solution L is dried, for example, at 150° C. for 10 minutes. As shown in FIG. 2, the applied aqueous solution L partially gathers at one or more locations on the opposing surface 4a when it dries, forming the dielectric film 5 in a scattered state. In the sealing step, the insulating tube 3 is heated to, for example, 700° C. to seal the discharge control gas of Ar (800 torr) and also to join the outer circumferential surface of the electrode body 4 and the inner circumferential surface of the insulating tube 3 . Furthermore, in the aging process, aging is performed at AC 100 mA, 2 sec: 2 kV, 20 kΩ, for example.

[0027] In this manner, in the surge protection element 1 of the present embodiment, the opposing surface 4a of the electrode body 4 is provided with the region A covered with the dielectric film 5 and the region B not covered with the dielectric film 5. Therefore, in the region A partially covered with the dielectric film 5, the metal of the opposing surface 4a is less likely to oxidize, and the dielectric film 5 is less likely to oxidize. Outer periphery The electric field is concentrated in the vicinity due to the lines of electric force gathering, making it easier to discharge, and a stable discharge start voltage can be obtained. In addition, the dielectric film 5 on the opposing surface 4a Outer periphery Directly below (Opposite surface of outer periphery) Since an oxide film-removed portion 5a is formed on the opposing surface 4a where the oxide film of the metal on the opposing surface 4a has been removed, the electric field is further concentrated by the oxide film-removed portion 5a where the oxide film has been removed, thereby obtaining a more stable discharge start voltage.

[0028] The manufacturing method of the surge protection element 1 of this embodiment includes a dielectric film formation process in which an aqueous solution L containing a dielectric material is applied to the opposing surfaces 4a of a pair of discharge electrodes 2 arranged opposite each other with a gap therebetween and then dried to provide an area A covered with a dielectric film 5 and an area B not covered with the dielectric film 5 on the opposing surfaces 4a. Therefore, the area A covered with the dielectric film 5 and the area B not covered with the dielectric film 5 can be easily provided by applying and drying the aqueous solution L containing the dielectric.

[0029] In addition, since the aging process includes applying a DC or AC voltage between the pair of discharge electrodes 2, the electrons impinge on the metal oxide film on the opposing surface 4a by aging, and the effect of removing the oxide film is promoted. Outer periphery Directly below (Opposite surface of outer periphery) The metal is activated, and the oxide film is removed to form an oxide film-removed portion 5a. Furthermore, excess oxygen in the insulating tube 3 is enclosed in the dielectric film 5 by aging, so that a more stable discharge starting voltage can be obtained. Furthermore, since the aqueous solution L is an aqueous solution of water glass containing sodium silicate or potassium silicate as a dielectric material, it is easy to apply and dry, and a dielectric film 5 of sodium silicate or potassium silicate can be obtained.

[0030] Next, a second embodiment of the surge protection element and its manufacturing method according to the present invention will be described below with reference to Fig. 4. In the following description of the embodiment, the same components as those described in the above embodiment are denoted by the same reference numerals, and the description thereof will be omitted.

[0031] The difference between the first and second embodiments is that the first embodiment includes a columnar or cylindrical insulating member 6 having a conductive coating 6a formed thereon in a divided manner via a discharge gap portion G, and a pair of discharge electrodes 2 are disposed opposite each other at both ends of the insulating member 6 via metal caps 7, which are conductive members, whereas the surge protection element 21 of the second embodiment is disposed opposite each other with electrode bodies 24 of a pair of discharge electrodes 22 directly sandwiching a plate-shaped insulating member 26 between their opposing surfaces 4a, as shown in FIG. 4.

[0032] The plate-like insulating member 26 is made of, for example, SiO 2 It is formed by: In this way, in the second embodiment, the insulating tube 23 can be made shorter than in the first embodiment, allowing for miniaturization. In the surge protection element 21 of the second embodiment, similarly to the first embodiment, the opposing surface 4a of the electrode body 24 is provided with an area A covered with the dielectric film 5 and an area B not covered with the dielectric film 5, so that a stable discharge starting voltage can be obtained. EXAMPLES

[0033] Next, in an example in which the surge protection element of the second embodiment was produced by the above-mentioned manufacturing method, an SEM composition image showing the opposing surface 4a of the electrode body 24 is shown in FIG. In this SEM composition image, the brighter (whiter) the image, the more elements with larger atomic numbers are present. In this embodiment, the white parts are copper (including copper oxide). The black parts represent the dielectric film 5 formed by coating water glass containing sodium silicate. Furthermore, the dielectric film 5 Outer periphery The blurred, shadow-like portions are areas where copper oxide on the surface of opposing surface 4a has diffused into dielectric film 5 and has been removed from the surface of opposing surface 4a.

[0034] As can be seen from this image, the opposing surface 4a of the electrode body 24 is provided with a region A covered with the dielectric film 5 and a region B not covered with the dielectric film 5. In addition, the dielectric film 5 on the opposing surface 4a Outer periphery Directly below (Opposite surface of outer periphery) An oxide film-removed portion 5a is formed on the opposing surface 4a by removing the oxide film of the metal (copper) on the opposing surface 4a.

[0035] Next, for the above-mentioned embodiment of the present invention, the change over time in the discharge starting voltage Vs when AC aging was performed under the above-mentioned aging conditions was measured, and the result is shown in Fig. 6(b). For comparison, for a comparative example in which the aqueous solution L was not applied to the facing surface 4a and there was no region A covered with the dielectric film 5, the change over time in the discharge starting voltage Vs when aging was performed in the same manner was also measured, and the result is shown in Fig. 6(a). As can be seen from these results, in the comparative example, which does not have the region A covered with dielectric film 5 on the opposing surface 4a, some individuals did not show the aging effect even after aging, and the variation in discharge start voltage was large, whereas in the examples of the present invention, which have the region A covered with dielectric film 5 on the opposing surface 4a, the aging effect was large in all individuals, and the variation in discharge start voltage was small.

[0036] Next, the results of measuring the change in insulation resistance (IR) for the above-mentioned embodiment of the present invention are shown in Fig. 7(b). For comparison, the results of measuring the change in insulation resistance for a comparative example in which the aqueous solution L was not applied to the opposing surface 4a and there was no region A covered with the dielectric film 5 are also shown in Fig. 7(a). As can be seen from these results, in the comparative example, many specimens exhibited a decrease in insulation resistance, whereas in the examples of the present invention, the insulation resistance was stable.

[0037] The technical scope of the present invention is not limited to the above-described embodiments and examples, and various modifications can be made without departing from the spirit of the present invention. [Explanation of symbols]

[0038] 1, 21... surge protection element, 2, 22... discharge electrode, 3, 23... insulating tube, 4, 24... electrode body, 4a... opposing surface, 5... dielectric film, 5a... oxide film removal portion, A... area covered with dielectric film, B... area not covered with dielectric film, L... aqueous solution

Claims

1. A pair of discharge electrodes arranged opposite each other with a gap therebetween; an insulating tube having the pair of discharge electrodes disposed at both ends thereof and sealing at least the mutually facing surfaces of the pair of discharge electrodes together with a discharge control gas therein; The discharge electrode includes an electrode body formed of a metal and having the opposing surface, The opposing surface is provided with a region covered with a dielectric film and a region not covered with the dielectric film, an oxide film of a metal constituting the inside of the electrode body is formed on the opposing surface and exposed in a region not covered with the dielectric film; A surge protection element characterized in that an oxide film of the metal of the opposing surface is diffused and contained in the outer peripheral edge portion of the dielectric film, and an oxide film removal portion in which the oxide film of the metal of the opposing surface has been removed is formed on the opposing surface side of the outer peripheral edge portion of the dielectric film.

2. 2. The surge protection device according to claim 1, 4. A surge protection element, wherein the dielectric material of the dielectric film is sodium silicate or potassium silicate.

3. A method for manufacturing the surge protection element according to claim 1 or 2, comprising the steps of: A method for manufacturing a surge protection element, comprising the steps of: applying an aqueous solution containing a dielectric material to the opposing surfaces of a pair of discharge electrodes arranged opposite each other with a gap therebetween; and drying the aqueous solution, the aqueous solution containing a dielectric material, to provide an area on the opposing surfaces that is covered with a dielectric film and an area that is not covered with the dielectric film.

4. 4. The method for manufacturing a surge protection element according to claim 3, a sealing step of disposing the pair of discharge electrodes on both ends and sealing at least the mutually facing surfaces of the pair of discharge electrodes together with a discharge control gas inside an insulating tube after the dielectric film forming step; The method for manufacturing a surge protection element further comprises, after the sealing step, an aging step of applying a DC voltage or an AC voltage between the pair of discharge electrodes.

5. The method for manufacturing a surge protection element according to claim 3 or 4, 2. A method for manufacturing a surge protection element, wherein the aqueous solution is an aqueous solution of water glass containing sodium silicate or potassium silicate as the dielectric material.

Citation Information

Patent Citations

  • JP1981005392U

  • Discharge tube and its manufacture

    JP1998312877A

  • Gas-filled discharge path

    JP2001516943A

  • Arrester for low voltage power system

    JP2003077617A

  • Discharge tube and its manufacturing method

    JP2004079230A