Application of keratin from snail shells in radiocarbon dating
The extraction and purification of keratin from snail shells using specific chemical solutions and purification steps addresses the contamination issues, enabling high-precision radiocarbon-14 dating with reliable F14C values.
Patent Information
- Application Number
- JP2025069353
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2025-04-21
- Publication Date
- 2026-11-02
- Estimated Expiration
- 2045-04-21
AI Technical Summary
The lack of efficient and reliable extraction and preparation methods for snail shells limits their widespread application in radiocarbon-14 dating, particularly due to contamination issues and the need for high-precision materials.
A method involving the extraction of keratin from snail shells using hydrogen peroxide, monophosphate, and diphosphate solutions, followed by recrystallization and purification steps to obtain high-purity snail shell keratin, which is then used in radiocarbon-14 dating.
The method provides high-purity snail shell keratin suitable for high-precision radiocarbon-14 dating, with F14C values close to local plants or the atmosphere, ensuring reliability and applicability in paleoclimate studies.
Smart Images

Figure 2026174830000001_ABST
Abstract
Description
[Technical Field]
[0001] This invention relates to the technical field of radiocarbon dating, and more particularly to the application of keratin from snail shells in radiocarbon-14 dating. [Background technology]
[0002] Radiocarbon-14 ( 14 C) Radiometric dating is a technique that uses the radioactive decay of carbon-14 to determine the age of organic materials.
[0003] traditional 14 The reliability of C dating materials depends on high-precision accelerators. 14 This limits the application of 14C dating to paleoclimate studies. Snail shells from the loess soil of Xinjiang, China, are ideal. 14 Although it is a material used for 14C dating, the lack of efficient and reliable extraction and preparation methods limits its widespread application. [Overview of the project] [Means for solving the problem]
[0004] To solve the above-mentioned problems of the prior art, the present invention provides the application of keratin from snail shells in radiocarbon dating.
[0005] To achieve the above objectives, the main technical solutions adopted by this invention include the following: The application of keratin from snail shells in radiocarbon dating, where, The method for extracting keratin from the snail shell is as follows: The steps involved taking a sample of a snail shell, crushing and washing it, and obtaining the washed snail shell, The steps involved sequentially immersing the washed snail shells in hydrogen peroxide solution and monophosphate solution, then washing them with decarbonized water, freeze-drying them, and obtaining a pre-treated sample. The steps include preparing a diphosphate solution with decarbonated water and orthophosphate, The process includes the step of dissolving a pre-treated sample in a diphosphate solution to obtain an aqueous solution containing snail shell keratin, filtering the residue, separating and purifying it to obtain a snail shell keratin sample.
[0006] Preferably, the mass concentration of the hydrogen peroxide solution is 3% to 7%.
[0007] Preferably, the mass concentration of the first phosphoric acid solution is 1 to 3%.
[0008] Preferably, the method for preparing the decarbonized water is: The steps include: mixing ultrapure water with a supersaturated oxidation solution of potassium peroxodisulfate, performing a water bath reaction, and obtaining the resulting solution; The process includes the step of recrystallizing the reacted solution to obtain decarbonized water.
[0009] Preferably, the method for recrystallization is: The decarbonized water obtained is heated to 35-45°C, and potassium peroxodisulfate is gradually added until saturated. After cooling to room temperature, the crystallization of potassium peroxodisulfate was promoted by cooling to 3-5°C, and crystals were obtained. The process then involves filtering, washing the crystals with cold decarbonated water, repeating the recrystallization process multiple times to achieve purification, and freeze-drying the potassium peroxodisulfate.
[0010] Preferably, the supersaturated oxidation solution of potassium peroxodisulfate comprises potassium peroxodisulfate, ultrapure water, and triphosphate solution, wherein the mass concentration of the triphosphate solution is 80-90%, and the volume ratio of the triphosphate solution to the ultrapure water in the supersaturated oxidation solution of potassium peroxodisulfate is (1.5-2.5):1.
[0011] Preferably, the temperature of the water bath reaction is 100°C.
[0012] Preferably, the mass concentration of the diphosphate solution is 40-60%.
[0013] Preferably, the conditions for performing the decomposition are a water bath condition of 65 to 75°C.
[0014] Preferably, the method for radiocarbon-14 dating using keratin from snail shells comprises: placing the purified snail shell keratin sample in a reactor, adding a supersaturated oxidizing solution of potassium peroxodisulfate, introducing the reactor into a vacuum system, evacuating the system, then performing a water bath reaction, cryogenically collecting CO₂ gas, recording the gas pressure, and calculating the carbon content of the snail shell keratin. [Effects of the Invention]
[0015] The present invention provides the application of snail shell keratin in radiocarbon-14 dating. By adopting the high-efficiency, low-pollution extraction method for snail shell keratin, the present invention is applicable to high-precision radiocarbon-14 dating research, and has important scientific and practical application value. Experimental results show that the F 14 C value of the snail shell keratin extracted by this method is close to the F 14 C value of local plants or the atmosphere, and the difference in F 14 C values of snail shell keratins of different attributes and sizes is small, so the snail shell keratin extracted by this method can be used as a reliable radiocarbon-14 dating material. [Brief Description of the Drawings]
[0016] [Figure 1] is a diagram showing the measurement results of δ13C values of saccharin sodium, sodium sorbate, sugar and oxalic acid. [Figure 2] is a diagram showing the measurement results of F14C values of saccharin sodium, sodium sorbate, sugar and oxalic acid. [Figure 3] is a diagram showing the measurement results of F14C values of snail shell carbonates and shell keratins from different regions. [Mode for Carrying Out the Invention]
[0017] Hereinafter, the technical aspects of embodiments of the present invention will be clearly and completely described in relation to embodiments of the present invention. Clearly, the embodiments described are only some embodiments of the present invention, not all embodiments. All other embodiments obtained by those skilled in the art without creative work based on the embodiments of the present invention are within the scope of the protection of the present invention.
[0018] In one embodiment of the present invention, the application of keratin from snail shells in radiocarbon dating is provided, wherein the method for extracting the keratin from the snail shells is: Step S1 involves collecting snail shell samples, crushing and washing them, and obtaining the washed snail shells. Step S2 involves sequentially immersing the washed snail shells in a 3%-7% hydrogen peroxide solution and a 1%-3% monophosphate solution, then washing them with decarbonized water, freeze-drying them, and obtaining a pre-treated sample. Step S3 involves preparing a 40-60% mass concentration diphosphate solution using decarbonated water and orthophosphate, The process includes the step of placing a pre-treated sample in a diphosphate solution and decomposing it under water bath conditions at 65-75°C to obtain a water-soluble solution containing snail shell keratin, filtering the residue, separating and purifying it to obtain a snail shell keratin sample.
[0019] In the embodiments of the present invention, using phosphoric acid as a raw material can reduce contamination of keratin in snail shells. In contrast, using hydrochloric acid as a raw material is unfavorable for subsequent oxidation with potassium peroxodisulfate, which oxidizes chloride ions to chlorine gas, affecting health. Furthermore, the embodiments of the present invention use decarbonized water as the solvent for the diphosphate solution, thus avoiding interference of trace amounts of keratin in snail shells due to carbon contamination in the water.
[0020] Here, the method for preparing decarbonized water is: Step S21 involves mixing ultrapure water with a supersaturated oxidation solution of potassium peroxodisulfate and performing a water bath reaction at 100°C to obtain a reacted solution, wherein the supersaturated oxidation solution of potassium peroxodisulfate contains potassium peroxodisulfate, ultrapure water, and a triphosphate solution, the mass concentration of the triphosphate solution is 80-90%, and the volume ratio of the triphosphate solution to the ultrapure water in the supersaturated oxidation solution of potassium peroxodisulfate is (1.5-2.5):1. The process includes step S22, in which the reacted solution is recrystallized to obtain decarbonized water. Specifically, the method for recrystallization is as follows: The decarbonized water obtained is heated to 35-45°C, and potassium peroxodisulfate is gradually added until saturated. After cooling to room temperature, the crystallization of potassium peroxodisulfate was promoted by cooling to 3-5°C, and crystals were obtained. The process then involves filtering, washing the crystals with cold decarbonated water, repeating the recrystallization process multiple times to achieve purification, and freeze-drying the potassium peroxodisulfate.
[0021] The above-mentioned monophosphate solution and triphosphate solution can both be prepared using the above-mentioned decarbonized water and orthophosphate.
[0022] In a preferred embodiment of the present invention, a method for performing radiocarbon dating using keratin from a snail shell is: The process includes placing a purified snail shell keratin sample in a reactor, adding a supersaturated potassium peroxodisulfate oxidation solution, immersing the reactor in a vacuum system, evacuating the system, performing a water bath reaction, collecting the CO2 gas by freezing, recording the gas pressure, and calculating the carbon content of the snail shell keratin.
[0023] The following examples illustrate the practical application of the technical means of the present invention, but are not limited thereto. All related reagents and experimental equipment are commercially available.
[0024] (Example 1) This embodiment provides a method for extracting keratin from snail shells, and specifically includes the following steps: (1) To produce decarbonized water, 100 mL of ultrapure water was placed in a 250 mL conical flask, 20 mL of a supersaturated oxidation solution of potassium peroxodisulfate was added, and the mixture was reacted in a 100°C water bath for 6 hours, after which it was cooled to room temperature and stored in a sealed container. Here, the supersaturated oxidation solution of potassium peroxodisulfate was obtained by mixing 100 mL of ultrapure water, 4 g of potassium peroxodisulfate, and 200 mL of a triphosphate solution with a mass concentration of 80-90%. To recrystallize potassium peroxodisulfate, the decarbonized water prepared above is heated to 40°C, potassium peroxodisulfate is gradually added until saturated, and after cooling to room temperature, it is cooled to 4°C to promote the crystallization of potassium peroxodisulfate. Crystals are obtained, then filtered, and the crystals are washed with cold decarbonized water. The recrystallization process is repeated several times to achieve purification, the potassium peroxodisulfate sample is freeze-dried, and placed in a storage container.
[0025] (2) Extracting keratin from snail shells. S1. Snail shell samples were lightly crushed, placed in an ultrasonic cleaner, and washed with deionized water to remove fine particles and some dissolved organic matter adhering to the inner surface. Under a microscope, loose particles or contaminants were lightly removed from the inner and outer surfaces of the shell using a soft brush or fine needle to obtain the cleaned snail shells.
[0026] S2. The washed snail shells were immersed in a 5% hydrogen peroxide solution to remove any attached organic matter, then briefly immersed in a 2% monophosphate solution to remove as much inorganic carbonate contamination as possible and slightly dissociate some of the organic matter. After washing with decarbonized water, the samples were freeze-dried to obtain pre-treated samples.
[0027] S3. A 50% by mass diphosphate solution is prepared using the above carbonless water and orthophosphate, and set aside to decompose the carbonates in the snail shells.
[0028] S4. The above pre-treated sample was placed in a diphosphate solution and decomposed under a 70°C water bath. After 24 hours, if the pH of the solution was 2-3, the decomposition of the carbonates from the snail shell was complete, and the keratin from the snail shell was hydrolyzed into a water-soluble solution, yielding a water-soluble solution containing snail shell keratin. The residue was filtered, then separated and purified to obtain a snail shell keratin sample.
[0029] Of these, the separation and purification methods were selected based on the molecular size of the contaminants, using nanofiltration, ultrafiltration, or high-performance liquid chromatography (HPLC). The purification effect can be evaluated using techniques such as liquid chromatography / mass spectrometry. For the identification and analysis of contaminant molecules, a liquid chromatograph-mass spectrometer can be used to identify and quantitatively analyze water-soluble organic matter, determining the keratin contaminating components and their levels. Sample quality control methods include removing organic matter adhering to glass containers at 550°C and classifying and storing the samples. Quality control is performed throughout the entire experimental procedure using methods such as blank tests to ensure the accuracy and reliability of the experimental results.
[0030] (Example 2) This embodiment provides a method for extracting keratin from snail shells, and specifically includes the following steps: (1) To produce decarbonized water, 100 mL of ultrapure water was placed in a 250 mL conical flask, 20 mL of a supersaturated oxidation solution of potassium peroxodisulfate was added, and the mixture was reacted in a 100°C water bath for 6 hours, after which it was cooled to room temperature and stored in a sealed container. Here, the supersaturated oxidation solution of potassium peroxodisulfate was obtained by mixing 100 mL of ultrapure water, 3.3 g of potassium peroxodisulfate, and 150 mL of an 80% by mass triphosphate solution. To recrystallize potassium peroxodisulfate, the decarbonized water prepared above is heated to 35°C, potassium peroxodisulfate is gradually added until saturated, and after cooling to room temperature, it is cooled to 3°C to promote the crystallization of potassium peroxodisulfate. Crystals are obtained, then filtered, and the crystals are washed with cold decarbonized water. The recrystallization process is repeated several times to achieve purification, the potassium peroxodisulfate sample is freeze-dried, and placed in a storage container.
[0031] (2) Extracting keratin from snail shells. S1. Snail shell samples were lightly crushed, placed in an ultrasonic cleaner, and washed with deionized water to remove fine particles and some dissolved organic matter adhering to the inner surface. Under a microscope, loose particles or contaminants were lightly removed from the inner and outer surfaces of the shell using a soft brush or fine needle to obtain the cleaned snail shells.
[0032] S2. The washed snail shells were immersed in a 3% hydrogen peroxide solution to remove any attached organic matter, then briefly immersed in a 1% monophosphate solution to remove as much inorganic carbonate contamination as possible and slightly dissociate some of the organic matter. After washing with decarbonized water, the samples were freeze-dried to obtain pre-treated samples.
[0033] S3. A 40% by mass diphosphate solution is prepared using the above carbonless water and orthophosphate, and set aside to decompose the carbonates in the snail shells.
[0034] S4. The above pre-treated sample was placed in a diphosphate solution and decomposed under water bath conditions at 65°C. After 24 hours, if the pH of the solution was 2-3, the decomposition of the carbonates from the snail shell was complete, and the keratin from the snail shell was hydrolyzed into a water-soluble solution, yielding a water-soluble solution containing snail shell keratin. The residue was filtered, then separated and purified to obtain a snail shell keratin sample.
[0035] (Example 3) This embodiment provides a method for extracting keratin from snail shells, and specifically includes the following steps: (1) To produce decarbonized water, 100 mL of ultrapure water was placed in a 250 mL conical flask, 20 mL of a supersaturated oxidation solution of potassium peroxodisulfate was added, and the mixture was reacted in a 100°C water bath for 6 hours, after which it was cooled to room temperature and stored in a sealed container. Here, the supersaturated oxidation solution of potassium peroxodisulfate was obtained by mixing 100 mL of ultrapure water, 4.7 g of potassium peroxodisulfate, and 250 mL of a 90% by mass triphosphate solution. To recrystallize potassium peroxodisulfate, the decarbonized water prepared above is heated to 45°C, potassium peroxodisulfate is gradually added until saturated, and after cooling to room temperature, it is cooled to 5°C to promote the crystallization of potassium peroxodisulfate. Crystals are obtained, then filtered, and the crystals are washed with cold decarbonized water. The recrystallization process is repeated several times to achieve purification, the potassium peroxodisulfate sample is freeze-dried, and placed in a storage container.
[0036] (2) Extracting keratin from snail shells. S1. Snail shell samples were lightly crushed, placed in an ultrasonic cleaner, and washed with deionized water to remove fine particles and some dissolved organic matter adhering to the inner surface. Under a microscope, loose particles or contaminants were lightly removed from the inner and outer surfaces of the shell using a soft brush or fine needle to obtain the cleaned snail shells.
[0037] S2. The washed snail shells were immersed in a 7% hydrogen peroxide solution to remove any attached organic matter, then briefly immersed in a 3% monophosphate solution to remove as much inorganic carbonate contamination as possible and slightly dissociate some of the organic matter. After washing with decarbonized water, the samples were freeze-dried to obtain pre-treated samples.
[0038] S3. A 60% mass concentration diphosphate solution is prepared using the above carbon-free water and orthophosphate, and set aside to decompose the carbonates in the snail shells.
[0039] S4. The above pre-treated sample was placed in a diphosphate solution and decomposed under water bath conditions at 75°C. After 24 hours, if the pH of the solution was 2-3, the decomposition of the carbonates from the snail shell was complete, and the keratin from the snail shell was hydrolyzed into a water-soluble solution, yielding a water-soluble solution containing snail shell keratin. The residue was filtered, then separated and purified to obtain a snail shell keratin sample.
[0040] (Example 4) This embodiment provides a method for extracting keratin from snail shells, and specifically includes the following steps: (1) To produce decarbonized water, 100 mL of ultrapure water was placed in a 250 mL conical flask, 15 mL of a supersaturated oxidation solution of potassium peroxodisulfate was added, and the mixture was reacted in a 100°C water bath for 6 hours, after which it was cooled to room temperature and stored in a sealed container. Here, the supersaturated oxidation solution of potassium peroxodisulfate was obtained by mixing 100 mL of ultrapure water, 4 g of potassium peroxodisulfate, and 200 mL of an 82% by mass triphosphate solution. To recrystallize potassium peroxodisulfate, the decarbonized water prepared above is heated to 38°C, potassium peroxodisulfate is gradually added until saturated, and after cooling to room temperature, it is cooled to 4°C to promote the crystallization of potassium peroxodisulfate. Crystals are obtained, then filtered, and the crystals are washed with cold decarbonized water. The recrystallization process is repeated several times to achieve purification, the potassium peroxodisulfate sample is freeze-dried, and placed in a storage container.
[0041] (2) Extracting keratin from snail shells. S1. Snail shell samples were lightly crushed, placed in an ultrasonic cleaner, and washed with deionized water to remove fine particles and some dissolved organic matter adhering to the inner surface. Under a microscope, loose particles or contaminants were lightly removed from the inner and outer surfaces of the shell using a soft brush or fine needle to obtain the cleaned snail shells.
[0042] S2. The washed snail shells were immersed in a 4% hydrogen peroxide solution to remove any attached organic matter, then briefly immersed in a 1.5% monophosphate solution to remove as much inorganic carbonate contamination as possible and slightly dissociate some of the organic matter. After washing with decarbonized water, the samples were freeze-dried to obtain pre-treated samples.
[0043] S3. A 45% mass concentration diphosphate solution is prepared using the above carbonless water and orthophosphate, and set aside to decompose the carbonates in the snail shells.
[0044] S4. The above pre-treated sample was placed in a diphosphate solution and decomposed under water bath conditions at 68°C. After 24 hours, if the pH of the solution was 2-3, the decomposition of the carbonates from the snail shell was complete, and the keratin from the snail shell was hydrolyzed into a water-soluble solution, yielding a water-soluble solution containing snail shell keratin. The residue was filtered, then separated and purified to obtain a snail shell keratin sample.
[0045] (Example 5) This embodiment provides a method for extracting keratin from snail shells, and specifically includes the following steps: (1) To produce decarbonized water, 100 mL of ultrapure water was placed in a 250 mL conical flask, 25 mL of a supersaturated oxidation solution of potassium peroxodisulfate was added, and the mixture was reacted in a 100°C water bath for 6 hours, after which it was cooled to room temperature and stored in a sealed container. Here, the supersaturated oxidation solution of potassium peroxodisulfate was obtained by mixing 100 mL of ultrapure water, 4 g of potassium peroxodisulfate, and 200 mL of an 88% by mass triphosphate solution. To recrystallize potassium peroxodisulfate, the decarbonized water prepared above is heated to 42°C, potassium peroxodisulfate is gradually added until saturated, and after cooling to room temperature, it is cooled to 4°C to promote the crystallization of potassium peroxodisulfate. Crystals are obtained, then filtered, and the crystals are washed with cold decarbonized water. The recrystallization process is repeated several times to achieve purification, the potassium peroxodisulfate sample is freeze-dried, and placed in a storage container.
[0046] (2) Extracting keratin from snail shells. S1. Snail shell samples were lightly crushed, placed in an ultrasonic cleaner, and washed with deionized water to remove fine particles and some dissolved organic matter adhering to the inner surface. Under a microscope, loose particles or contaminants were lightly removed from the inner and outer surfaces of the shell using a soft brush or fine needle to obtain the cleaned snail shells.
[0047] S2. The washed snail shells were immersed in a 6% hydrogen peroxide solution to remove any attached organic matter, then briefly immersed in a 2.5% monophosphate solution to remove as much inorganic carbonate contamination as possible and slightly dissociate some of the organic matter. After washing with decarbonized water, the samples were freeze-dried to obtain pre-treated samples.
[0048] S3. A 55% mass concentration diphosphate solution is prepared using the above carbonless water and orthophosphate, and set aside to decompose the carbonates in the snail shells.
[0049] S4. The above pre-treated sample was placed in a diphosphate solution and decomposed under water bath conditions at 72°C. After 24 hours, if the pH of the solution was 2-3, the decomposition of the carbonates from the snail shell was complete, and the keratin from the snail shell was hydrolyzed into a water-soluble solution, yielding a water-soluble solution containing snail shell keratin. The residue was filtered, then separated and purified to obtain a snail shell keratin sample.
[0050] (Example 6) This embodiment describes a method for performing radiocarbon dating using keratin from snail shells. First, a keratin sample from a snail shell is extracted and purified according to the extraction method provided in Example 1. Then, the purified snail shell keratin sample is placed in a 30 mL reactor, 8 mL of a supersaturated potassium peroxodisulfate oxidizing solution (same as in Example 1) is added, the reactor is placed in a vacuum system, and after vacuuming, the reactor is sealed using a natural gas spray gun. The reactor is then placed in a 100°C water bath container and the water bath reaction is carried out for 1 hour. The CO2 gas is collected by freezing, the gas pressure is recorded, and the carbon content of the snail shell keratin is calculated.
[0051] Specifically, 1.4 mg of Fe2O3 was weighed and placed into a reaction tube, followed by vacuum evacuation, the reaction tube was heated in an electric furnace at 600°C for 10 minutes, and 750 mbar of high-purity H2 was charged to reduce Fe2O3 to iron. After the purification of the Fe2O3 sample was completed, vacuum evacuation was performed to 10 -5 mbar, the collected sample CO2 was transferred into the reaction tube using a -160°C cold trap, CO2 was released, the pressure value thereof was recorded, high-purity hydrogen gas was charged, CO2 was released to mix with H2, the mixture was heated to react at 600°C to synthesize graphite, and 14 C press target preparation was performed for accelerator measurement. In the entire sample preparation process, quality control was carried out using a standard dating substance with a carbon amount equivalent to that of the sample.
[0052] According to the methods provided in Example 1 and Example 6 above, instead of the keratin of snail shells, saccharin sodium, sodium sorbate, sugar and oxalic acid were used to conduct δ 13 C and F 14 C values (the ratio of the sample's 14 C concentration to the local plant or atmospheric 14 C concentration) measurement, to evaluate whether the oxidation method using the supersaturated oxidizing solution of potassium persulfate can oxidize such water-soluble substances, and the specific measurement results are shown in Figure 1 and Figure 2. As can be seen from the results, the potassium persulfate oxidation method was used to separate organic carbon (OC) in the keratin of snail shells, and saccharin sodium, sodium sorbate, sugar and oxalic acid were used as reference materials to conduct strict verification of isotope reliability. Most of the standardized differences in the data are all less than 1, the difference between the test value and the standard value is small, within the allowable error range, and there is no statistical significance.
[0053] In addition, according to the methods provided in Example 1 and Example 6 above, the F values of shell carbonate and keratin of modern living snails with different attributes from different regions in China were 14 The measured C values are shown in Figure 3. Compared with the snail shell carbonate, the F of the snail shell keratin 14 The C value is the F of local plants or the atmosphere 14F values are close to the C value, and represent the F values of keratin in snail shells of different genera and sizes. 14 Because the difference in C values is small, it is highly reliable. 14 It can be used as a material for 14C dating.
[0054] Using the above-described desirable embodiments of the present invention as a hint, those concerned can make various changes and modifications without departing from the technical concept of the present invention as described above. The technical scope of the present invention is not limited to the contents of this specification.
Claims
1. The application of keratin from snail shells in radiocarbon dating, The method for extracting keratin from the snail shell is as follows: The steps involved taking a sample of a snail shell, crushing and washing it, and obtaining the washed snail shell, The steps involved sequentially immersing the washed snail shells in hydrogen peroxide solution and monophosphate solution, then washing them with decarbonized water, freeze-drying them, and obtaining a pre-treated sample. The steps include preparing a diphosphate solution with decarbonated water and orthophosphate, The application of snail shell keratin in radiocarbon dating is characterized by comprising the step of dissolving a pre-treated sample in a diphosphate solution to obtain an aqueous solution containing snail shell keratin, filtering the residue, separating and purifying it to obtain a snail shell keratin sample.
2. The application according to claim 1, characterized in that the mass concentration of the hydrogen peroxide solution is 3% to 7%.
3. The application according to claim 1, characterized in that the mass concentration of the first phosphoric acid solution is 1 to 3%.
4. The method for preparing the decarbonized water is as follows: The steps include: mixing ultrapure water with a supersaturated oxidation solution of potassium peroxodisulfate, performing a water bath reaction, and obtaining the resulting solution; The application according to claim 1, characterized by comprising the step of recrystallizing the reacted solution to obtain decarbonized water.
5. The method for recrystallization is, The decarbonized water obtained is heated to 35-45°C, and potassium peroxodisulfate is gradually added until saturated. After cooling to room temperature, the crystallization of potassium peroxodisulfate was promoted by cooling to 3-5°C, and crystals were obtained. The application according to claim 4, characterized in that it further comprises filtering, washing the crystals with cold decarbonized water, repeating the recrystallization process multiple times to achieve a purification effect, and freeze-drying the potassium peroxodisulfate.
6. The application according to claim 4, characterized in that the supersaturated oxidation solution of potassium peroxodisulfate comprises potassium peroxodisulfate, ultrapure water, and triphosphate solution, the mass concentration of the triphosphate solution being 80-90%, and the volume ratio of the triphosphate solution to the ultrapure water in the supersaturated oxidation solution of potassium peroxodisulfate being (1.5-2.5):
1.
7. The application according to claim 4, characterized in that the temperature of the water bath reaction is 100°C.
8. The application according to claim 1, characterized in that the mass concentration of the diphosphate solution is 40 to 60%.
9. The application according to claim 1, characterized in that the conditions for decomposition are water bath conditions at 65 to 75°C.
10. A method for performing radiocarbon dating using keratin from snail shells is: The purified keratin sample from snail shells is placed in a reactor, a supersaturated oxidation solution of potassium peroxodisulfate is added, the reactor is placed in a vacuum system, and after vacuuming, a water bath reaction is carried out, CO2 2 The application according to claim 1, characterized by comprising the steps of freezing and collecting the gas, recording the gas pressure, and calculating the carbon content of the keratin in the snail shell.