Chip sealing ring structure and preparation method thereof, semiconductor chip and preparation method thereof
By forming a multi-layer structure on the chip, including the bottom protective layer, sealed metal ring and moisture-proof layer, the chip sealing ring has insufficient ability to erode water vapor or gas-liquid, and the gas-liquid barrier capability and reliability of the chip are significantly improved.
Patent Information
- Application Number
- CN201811102067.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2018-09-20
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2038-09-20
AI Technical Summary
The existing chip sealing ring structure has poor resistance to water vapor or other gas and liquids, which affects the chip electrical performance and reliability.
The bottom protective layer is formed on the active surface of the chip, and a first and second sealing metal ring are established thereon, combining the insulating dielectric layer and the moisture-proof layer, exposing the second sealing metal ring through the isolation ring groove, forming a moisture-proof layer to enhance the gas Liquid blocking capability.
It effectively avoids oxidation or erosion of the metal layer during the process, enhances its resistance to water vapor or other gas and liquids, maintains the electrical performance and reliability of the chip, and does not reduce the ability to expand and rupture the barrier stress.
Smart Images

Figure CN110931436B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a chip sealing ring structure and a preparation method thereof, a semiconductor chip and a preparation method thereof. Background Art
[0002] Since silicon materials are brittle, when the wafer is cut, the cutting method of the cutting knife will generate certain mechanical stress on the front and back of the wafer, which may cause chipping at the edge of the chip. The chipping problem will reduce the mechanical strength of the chip. The initial chip edge cracks will further spread in the subsequent packaging process or in the use of the chip product, which is likely to cause the chip to break, resulting in failure of the chip's electrical performance. In order to protect the internal circuit of the chip, prevent dicing damage, and improve chip reliability, a chip seal ring (SR) structure is usually designed around the chip. Figure 1 As shown, the chip sealing ring structure includes a sealing ring metal layer pattern 12 between the scribe lane (SL) 20 of the wafer and the periphery region (PR) of the chip 10. When the wafer cutting process is performed along the scribe lane, the chip sealing ring structure can block the unwanted stress expansion and cracking from the scribe lane to the chip caused by the above-mentioned wafer cutting process. In addition, the chip sealing ring structure also has the ability to resist gas and liquid erosion, and can prevent the penetration and damage of water vapor or other chemical pollution sources. In today's semiconductor technology, the size of semiconductor components is miniaturized, which puts higher requirements on the crack blocking ability and gas and liquid shielding ability of the chip sealing ring. In the existing process, the metal layer is directly exposed to the air during the process and will be oxidized or corroded by oxygen, water vapor or other gas and liquid. The existing chip sealing ring structure mainly blocks oxygen to prevent the metal layer from being oxidized, but has poor resistance to corrosion by water vapor or other gas and liquid, so that the internal devices of the chip are also oxidized or corroded by gas and liquid, and the electrical performance and reliability of the chip are affected. Therefore, how to enhance the gas-liquid barrier capability of the chip sealing ring structure without reducing the ability to block stress expansion is an urgent problem to be solved. Summary of the invention
[0003] In view of the shortcomings of the prior art described above, the object of the present invention is to provide a chip sealing ring structure and a preparation method thereof, a semiconductor chip and a preparation method thereof, so as to solve the problem that the chip sealing ring structure in the prior art has poor resistance to gas and liquid corrosion, resulting in the electrical performance and reliability of the chip being affected.
[0004] To achieve the above-mentioned object and other related objects, the present invention provides a method for preparing a chip sealing ring structure, comprising the following steps:
[0005] Providing a chip, wherein a bottom protection layer is formed on an active surface of the chip;
[0006] forming a first sealing metal ring and a second sealing metal ring on the bottom protection layer, wherein the first sealing metal ring is located around the active surface of the chip, and the second sealing metal ring is disposed on the first sealing metal ring in a stacked manner;
[0007] forming an insulating dielectric layer on the bottom protective layer, wherein the insulating dielectric layer has an isolation ring groove exposing the second sealing metal ring, and the bottom of the isolation ring groove does not expose the bottom protective layer;
[0008] forming a moisture-proof layer on the insulating dielectric layer and in the isolation ring groove, wherein the moisture-proof layer covers the first exposed portion of the second sealing metal ring and the second exposed portion of the insulating dielectric layer in the isolation ring groove;
[0009] Among them, the moisture-proof layer on the insulating dielectric layer and in the isolation ring groove, the first sealing metal ring and the second sealing metal ring isolate the insulating dielectric layer into a peripheral layer portion and a central layer portion, and the chip sealing ring structure enhances the gas-liquid blocking capability through the combination of the first sealing metal ring, the second sealing metal ring and the moisture-proof layer, thereby preventing the internal components of the chip in the central layer portion from being oxidized or corroded by gas and liquid.
[0010] Preferably, the step of forming an insulating dielectric layer on the bottom protective layer comprises:
[0011] Forming an insulating dielectric material on the bottom protective layer to cover the first sealing metal ring, the second sealing metal ring and the bottom protective layer;
[0012] Disposing a first photomask on the insulating dielectric material, wherein the first photomask has a photomask opening aligned with the first sealing metal ring and the second sealing metal ring region; and
[0013] The insulating dielectric material is etched using the mask opening until the isolation ring groove corresponding to the mask opening is formed, thereby exposing the second sealing metal ring.
[0014] Preferably, the isolation ring groove exposes an upper portion or a top portion of the second sealing metal ring.
[0015] Preferably, in the process of etching the insulating dielectric material, the etching stops at the metal portion of the second sealing metal ring.
[0016] Preferably, in the process of etching the insulating dielectric material, the etching stops at the metal side surface of the middle portion of the second sealing metal ring or the metal top surface of the second sealing metal ring.
[0017] Preferably, the width of the isolation ring groove is greater than or equal to the width of the second sealing metal ring, so that the isolation ring groove completely exposes the upper part or top of the second sealing metal ring, and the first sealing metal ring is embedded in the insulating dielectric layer.
[0018] Preferably, the width of the isolation ring groove is smaller than the width of the second sealing metal ring, so that the isolation ring groove partially exposes the upper part or top of the second sealing metal ring, and the first sealing metal ring is embedded in the insulating dielectric layer.
[0019] Preferably, the first sealing metal ring and the second sealing metal ring each include at least one continuous metal ring structure, the continuous metal ring structure is formed by stacking a barrier layer, a metal layer and a plug portion, and the plug portion in the second sealing metal ring is formed as a whole by extending downward from the metal layer in the second sealing metal ring, and metal interconnection is achieved through the barrier layer in the second sealing metal ring and the metal layer in the first sealing metal ring.
[0020] Preferably, the material of the moisture-proof layer includes nitride or oxynitride, the material of the bottom protection layer includes silicon carbon nitride, and the material of the insulating dielectric layer includes oxide.
[0021] Preferably, the method for preparing the chip sealing ring structure further comprises:
[0022] A top covering layer is formed on the moisture-proof layer.
[0023] To achieve the above-mentioned object and other related objects, the present invention provides a method for preparing a semiconductor chip, wherein the method for preparing a semiconductor chip at least comprises: preparing a chip sealing ring structure by adopting the method for preparing a chip sealing ring structure as described above.
[0024] To achieve the above-mentioned object and other related objects, the present invention provides a method for preparing a semiconductor chip, wherein the method for preparing a semiconductor chip at least comprises:
[0025] Providing a wafer, wherein the wafer includes a plurality of chips and dicing lanes between adjacent chips;
[0026] The chip sealing ring structure is prepared by the method for preparing the chip sealing ring structure as described above, in the peripheral area of the chip and along the cutting path; wherein a pad metal layer pattern is formed while forming the first sealing metal ring and the second sealing metal ring, the pad metal layer pattern is located in the peripheral area of the chip, and the pad metal layer pattern is partially wrapped in the insulating dielectric layer;
[0027] A pad opening is formed above the pad metal layer pattern to expose the pad region of the chip.
[0028] Preferably, the step of forming a pad opening above the pad metal layer pattern comprises:
[0029] forming a top covering layer on the moisture-proof layer;
[0030] Disposing a second photomask on the top covering layer;
[0031] The top cover layer is patterned using the second photomask, and the moisture-proof layer and the insulating dielectric layer are etched until the pad opening is formed above the pad metal layer pattern, and the portion of the pad metal layer pattern exposed within the pad opening serves as a chip pad, thereby exposing the pad area of the chip.
[0032] Preferably, the method for preparing the semiconductor chip further comprises:
[0033] The wafer is cut along the cutting paths to obtain a plurality of semiconductor chips.
[0034] To achieve the above objectives and other related objectives, the present invention provides a chip sealing ring structure, which at least includes:
[0035] chip;
[0036] A bottom protection layer, located on the active surface of the chip;
[0037] A first sealing metal ring is located on the bottom protection layer and around the active surface of the chip;
[0038] a second sealing metal ring, located on the first sealing metal ring;
[0039] an insulating dielectric layer, located on the bottom protective layer, the insulating dielectric layer having an isolation ring groove exposing the second sealing metal ring, the bottom of the isolation ring groove not exposing the bottom protective layer; and
[0040] a moisture-proof layer, located on the insulating medium layer and in the isolation ring groove, the moisture-proof layer covering a first exposed portion of the second sealing metal ring and a second exposed portion of the insulating medium layer in the isolation ring groove;
[0041] Among them, the moisture-proof layer, the first sealing metal ring and the second sealing metal ring isolate the insulating medium layer into a peripheral layer portion and a central layer portion, and the chip sealing ring structure enhances the gas-liquid blocking capability through the combination of the first sealing metal ring, the second sealing metal ring and the moisture-proof layer, thereby preventing the internal components of the chip in the central layer portion from being oxidized or corroded by gas and liquid.
[0042] Preferably, the bottom surface of the portion of the moisture-proof layer located in the isolation ring groove is connected to and covers the upper portion or top of the second sealing metal ring.
[0043] Preferably, the width of the isolation ring groove is greater than or equal to the width of the second sealing metal ring, so that the upper part or top of the second sealing metal ring is completely exposed in the isolation ring groove, and the first sealing metal ring is embedded in the insulating dielectric layer.
[0044] Preferably, the width of the isolation ring groove is smaller than the width of the second sealing metal ring, so that the upper part or top portion of the second sealing metal ring is exposed in the isolation ring groove, and the first sealing metal ring is embedded in the insulating medium layer.
[0045] Preferably, the first sealing metal ring and the second sealing metal ring each include at least one continuous metal ring structure, the continuous metal ring structure is formed by stacking a barrier layer, a metal layer and a plug portion, and the plug portion in the second sealing metal ring is formed as a whole by extending downward from the metal layer in the second sealing metal ring, and metal interconnection is achieved through the barrier layer in the second sealing metal ring and the metal layer in the first sealing metal ring.
[0046] Preferably, the isolation ring groove at least exposes the metal top surface of the continuous metal ring structure of the second sealing metal ring.
[0047] Preferably, the material of the moisture-proof layer includes nitride or oxynitride, the material of the bottom protection layer includes silicon carbon nitride, and the material of the insulating dielectric layer includes oxide.
[0048] Preferably, the chip sealing ring structure further includes:
[0049] The top covering layer is located on the moisture-proof layer.
[0050] To achieve the above object and other related objects, the present invention provides a semiconductor chip, which at least includes: the chip sealing ring structure as described above.
[0051] To achieve the above objectives and other related objectives, the present invention provides a semiconductor device structure, wherein the semiconductor device structure at least includes:
[0052] A wafer, wherein the wafer comprises a plurality of chips and dicing lanes between adjacent chips; wherein the chip at least comprises the chip sealing ring structure as described above; and
[0053] A pad metal layer pattern is located in a peripheral area of the chip, and the pad metal layer pattern is partially wrapped in the insulating dielectric layer;
[0054] The insulating dielectric layer has a pad opening located above the pad metal layer pattern, the pad opening also passes through the moisture-proof layer, and the exposed portion of the pad metal layer pattern serves as a chip pad, thereby exposing the pad area of the chip.
[0055] As described above, the chip sealing ring structure and the manufacturing method thereof, the semiconductor chip and the manufacturing method thereof of the present invention have the following beneficial effects:
[0056] The chip sealing ring structure and preparation method thereof of the present invention utilize the chip circuit area manufacturing process to form a moisture-proof layer on the surface of the second sealing metal ring without increasing the process flow, and the moisture-proof layer wraps part of the metal layer in the second sealing metal ring. The combination of the first sealing metal ring, the second sealing metal ring and the moisture-proof layer can effectively prevent the metal layer from being directly exposed to the air during the process and being oxidized or corroded by oxygen, water vapor or other gases and liquids, and also prevent the internal devices of the chip in the central layer from being oxidized or corroded by gas and liquids, greatly enhancing the gas-liquid blocking ability without reducing the stress expansion and rupture blocking ability; compared with the prior art that mainly blocks oxygen, the ability to resist corrosion to water vapor or other gases and liquids is also enhanced, thereby preventing the electrical performance and reliability of the chip from being affected.
[0057] The semiconductor chip and the preparation method thereof of the present invention adopt the chip sealing ring structure and the preparation method thereof of the present invention. On a wafer with a plurality of chips, a chip sealing ring structure is simultaneously prepared between the surrounding area of each chip and the cutting path, and a chip circuit area manufacturing process is utilized to form a pad metal layer pattern while forming a first sealing metal ring and a second sealing metal ring, and a pad opening is formed above the pad metal layer pattern to open the pad area of each chip, and finally the wafer is cut along the cutting path to obtain a plurality of semiconductor chips. When the wafer cutting process is performed along the cutting path, the chip sealing ring structure can effectively block stress expansion and rupture capabilities, and at the same time has a strong gas-liquid blocking capability, and can effectively resist the erosion of water vapor or other gas-liquids. Therefore, the semiconductor chip obtained by the above method has excellent electrical performance and reliability. BRIEF DESCRIPTION OF THE DRAWINGS
[0058] Figure 1 A top view of a chip sealing ring structure in the prior art of the present invention is shown.
[0059] Figure 2 Display as Figure 1 An exemplary structural cross-sectional view along the AA direction.
[0060] Figure 3 It is a schematic flow chart of a method for preparing a chip sealing ring structure in a first embodiment of the present invention.
[0061] Figures 4 to 12 The schematic diagram shows the specific steps of the method for preparing the chip sealing ring structure according to the first embodiment of the present invention. Figure 7 (a) is a top view showing a first mask disposed on an insulating dielectric material, wherein the width of the mask opening is greater than the width of the second sealing metal ring.
[0062] Fig.12 Also shown is a schematic diagram of a chip sealing ring structure in the case where the second sealing metal ring includes a continuous metal ring structure in the method for preparing the chip sealing ring structure according to the first embodiment of the present invention.
[0063] Figure 13 to Figure 16 The structure schematic diagram shows a specific step of an example of a method for preparing a chip sealing ring structure according to the first embodiment of the present invention.
[0064] Fig.17 (a) shows a top view of a method for preparing a chip sealing ring structure according to the first embodiment of the present invention, in which the second sealing metal ring includes two continuous metal ring structures, a first mask is set on the insulating dielectric material, and the width of the mask opening is greater than or equal to the width of the second sealing metal ring.
[0065] Fig.17 (b) is a schematic diagram of the chip sealing ring structure in which the second sealing metal ring includes two continuous metal ring structures, the width of the isolation ring groove is greater than or equal to the width of the second sealing metal ring, and the isolation ring groove completely exposes the upper part of the second sealing metal ring in the preparation method of the chip sealing ring structure of the first embodiment of the present invention.
[0066] Fig.17 (c) is a schematic diagram of the chip sealing ring structure in which the second sealing metal ring includes two continuous metal ring structures, the width of the isolation ring groove is greater than or equal to the width of the second sealing metal ring, and the isolation ring groove completely exposes the top of the second sealing metal ring in the preparation method of the chip sealing ring structure of the first embodiment of the present invention.
[0067] Fig.18 (a) shows a top view of a method for preparing a chip sealing ring structure according to the first embodiment of the present invention, in which the second sealing metal ring includes three continuous metal ring structures, a first mask is set on the insulating dielectric material, and the width of the mask opening is greater than the width of the second sealing metal ring.
[0068] Fig.18 (b) is a schematic diagram of the chip sealing ring structure in which the second sealing metal ring includes three continuous metal ring structures, the width of the isolation ring groove is greater than or equal to the width of the second sealing metal ring, and the isolation ring groove completely exposes the middle part of the second sealing metal ring in the preparation method of the chip sealing ring structure of the first embodiment of the present invention.
[0069] Fig.18 (c) is a schematic diagram of the chip sealing ring structure in which the second sealing metal ring includes three continuous metal ring structures, the width of the isolation ring groove is greater than or equal to the width of the second sealing metal ring, and the isolation ring groove completely exposes the top of the second sealing metal ring in the preparation method of the chip sealing ring structure of the first embodiment of the present invention.
[0070] Figure 19 to Figure 23 The structure schematic diagram shows a specific step of an example of a method for preparing a chip sealing ring structure in the first embodiment of the present invention. Fig.19 (a) shows a top view of a method for preparing a chip sealing ring structure according to the first embodiment of the present invention, in which the second sealing metal ring includes a continuous metal ring structure, a first mask is set on the insulating dielectric material, and the width of the mask opening is smaller than the width of the second sealing metal ring.
[0071] Fig.24 (a) shows a top view of a method for preparing a chip sealing ring structure according to the first embodiment of the present invention, in which the second sealing metal ring includes two continuous metal ring structures, a first mask is set on the insulating dielectric material, and the width of the mask opening is smaller than the width of the second sealing metal ring.
[0072] Fig.24 (b) is a schematic diagram of the chip sealing ring structure in which the second sealing metal ring includes two continuous metal ring structures, the width of the isolation ring groove is smaller than the width of the second sealing metal ring, and the isolation ring groove partially exposes the middle part of the second sealing metal ring in the preparation method of the chip sealing ring structure of the first embodiment of the present invention.
[0073] Fig.24 (c) is a schematic diagram of the chip sealing ring structure showing a method for preparing a chip sealing ring structure according to the first embodiment of the present invention, in which the second sealing metal ring includes two continuous metal ring structures, the width of the isolation ring groove is smaller than the width of the second sealing metal ring, and the isolation ring groove partially exposes the top of the second sealing metal ring.
[0074] Fig.25 (a) shows a top view of a method for preparing a chip sealing ring structure according to the first embodiment of the present invention, in which the second sealing metal ring includes three continuous metal ring structures, a first mask is set on the insulating dielectric material, and the width of the mask opening is smaller than the width of the second sealing metal ring.
[0075] Fig.25(b) is a schematic diagram of the chip sealing ring structure in which the second sealing metal ring includes three continuous metal ring structures, the width of the isolation ring groove is smaller than the width of the second sealing metal ring, and the isolation ring groove partially exposes the middle part of the second sealing metal ring in the preparation method of the chip sealing ring structure of the first embodiment of the present invention.
[0076] Fig.25 (c) is a schematic diagram of a chip sealing ring structure in which the second sealing metal ring includes three continuous metal ring structures, the width of the isolation ring groove is smaller than the width of the second sealing metal ring, and the isolation ring groove partially exposes the top of the second sealing metal ring in the preparation method of the chip sealing ring structure according to the first embodiment of the present invention.
[0077] Fig.26 (a) is a top view showing a first photomask having a spacer pattern disposed on an insulating dielectric material when the second sealing metal ring includes three continuous metal ring structures in the method for preparing a chip sealing ring structure according to the first embodiment of the present invention.
[0078] Fig.26 (b) and Fig.26 (c) Displayed as per Fig.17 (a) Schematic diagram of the two chip sealing ring structures finally obtained.
[0079] Fig. 27 and Fig.28 The diagram shows a top view of a method for manufacturing a chip sealing ring structure according to the first embodiment of the present invention, in which a mask opening is aligned with a selected area of a second sealing metal ring.
[0080] Fig.29 It is a schematic diagram of a wafer having a chip, a dicing street and a chip sealing ring structure prepared in a method for preparing a semiconductor chip according to a third embodiment of the present invention.
[0081] Figure 30 to Figure 33 The schematic diagram shows the specific steps of preparing the pad in the method for preparing the semiconductor chip according to the third embodiment of the present invention. Fig.31 A mask image showing the locations of the pads covered.
[0082] Fig.29 Also shown is a schematic diagram of a wafer including a chip, a dicing street and a chip seal ring structure in a semiconductor device structure according to a sixth embodiment of the present invention.
[0083] Fig.33 Also shown is a schematic structural diagram of a semiconductor device structure according to a sixth embodiment of the present invention.
[0084] Component number description
[0085] 10 Chip
[0086] 11 Bottom protective layer
[0087] 12 Sealing ring metal layer pattern
[0088] 12A First sealing metal ring
[0089] 12B Second sealing metal ring
[0090] 12a First exposure site
[0091] 121 Metal Layer
[0092] 121A Metal layer in the first sealing metal ring
[0093] 121B Metal layer in the second sealing metal ring
[0094] 122 Barrier layer
[0095] 122A Barrier layer in the first sealing metal ring
[0096] 122B Barrier layer in the second sealing metal ring
[0097] 123 Plug
[0098] 123A Plug portion in the first sealing metal ring
[0099] 123B Plug portion in the second sealing metal ring
[0100] 13 Insulation dielectric layer
[0101] 13a Second exposure site
[0102] 131 Insulating dielectric materials
[0103] 132 Isolation ring groove
[0104] 133 Photoresist
[0105] 14 First mask
[0106] 141 Mask opening
[0107] 15 Moisture-proof layer
[0108] 16 Top cover layer
[0109] 17 Pad metal layer pattern
[0110] 171 Pad opening
[0111] 18 Second mask
[0112] 20 Cutting Lanes
[0113] Steps S1 to S5 DETAILED DESCRIPTION
[0114] See also Figure 1 and Figure 2 In the prior art, the chip sealing ring structure at least includes: a chip 10, on which a bottom protection layer 11 is formed; a sealing ring metal layer pattern 12, formed on the bottom protection layer 11, and located at the periphery of the chip 10; an insulating dielectric layer 13, formed on the bottom protection layer 11, and the sealing ring metal layer pattern 12 is wrapped in the insulating dielectric layer 13; a moisture-proof layer 15, formed on the insulating dielectric layer 13; and a top cover layer 16, formed on the moisture-proof layer 15. The sealing ring metal layer pattern 12 includes at least one continuous metal ring structure, which is formed by alternately stacking a plurality of barrier layers 122, metal layers 121, and plugs 123, and the metal layers 121 are interconnected by forming a plug 123 integrally from the metal layers 121 on the barrier layers 122.
[0115] After long-term practice, the inventor found that, since the moisture-proof layer 15 in the prior art only covers the insulating dielectric layer 13, and the sealing ring metal layer pattern 12 is wrapped in the insulating dielectric layer 13, the moisture-proof layer 15 has limited gas-liquid barrier capability for the sealing ring metal layer pattern 12 located in the insulating dielectric layer 13; and since the insulating dielectric layer 13 is usually made of oxide material, it mainly blocks oxygen to prevent the metal layer in the sealing ring metal layer pattern 12 from being oxidized, but has poor resistance to corrosion by water vapor or other gas and liquid. The metal layer is directly exposed to the air during the manufacturing process and is easily corroded by water vapor or other gas and liquid, so that the internal devices of the chip are also oxidized or corroded by gas and liquid, and the electrical performance and reliability of the chip 10 are affected. In order to solve the problems of the prior art, after long-term experiments and research, the inventor has achieved the purpose of enhancing the gas-liquid barrier capability of the chip sealing ring structure without reducing the ability to block stress expansion.
[0116] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.
[0117] See also Figure 3 to Figure 28The first embodiment of the present invention relates to a method for preparing a chip sealing ring structure. It should be noted that the illustrations provided in this embodiment are only schematic illustrations of the basic concept of the present invention, and the drawings only show components related to the present invention rather than the number, shape and size of components in actual implementation. In actual implementation, the type, quantity and proportion of each component may be changed arbitrarily, and the component layout may also be more complicated.
[0118] like Figure 3 As shown, the method for preparing the chip sealing ring structure of this embodiment at least includes the following steps:
[0119] Step S1 : providing a chip 10 , wherein a bottom protection layer 11 is formed on an active surface of the chip 10 .
[0120] Step S2 , forming a first sealing metal ring 12A and a second sealing metal ring 12B on the bottom protection layer 11 , wherein the first sealing metal ring 12A is located around the active surface of the chip 10 , and the second sealing metal ring 12B is disposed on the first sealing metal ring 12A in a stacked manner.
[0121] In step S3 , an insulating dielectric layer 13 is formed on the bottom protection layer 11 . The insulating dielectric layer 13 has an isolation ring groove 132 that exposes the second sealing metal ring 12B. The bottom of the isolation ring groove 132 does not expose the bottom protection layer 11 .
[0122] Step S4 , forming a moisture-proof layer 15 on the insulating dielectric layer 13 and in the isolation ring groove 132 , wherein the moisture-proof layer 15 covers the first exposed portion 12 a of the second sealing metal ring 12B and the second exposed portion 13 a of the insulating dielectric layer 13 in the isolation ring groove 132 .
[0123] Among them, the moisture-proof layer 15, the first sealing metal ring 12A and the second sealing metal ring 12B on the insulating dielectric layer 13 and in the isolation ring groove 132 isolate the insulating dielectric layer 13 into a peripheral layer and a central layer. The chip sealing ring structure enhances the gas-liquid blocking capability through the combination of the first sealing metal ring 12A, the second sealing metal ring 12B and the moisture-proof layer 15, thereby preventing the internal devices of the chip 10 from being oxidized or corroded by gas and liquid.
[0124] like Figure 4 to Figure 28 As shown, each step in the method for preparing the chip sealing ring structure of this embodiment is specifically described below.
[0125] First, step S1 is performed to provide a chip 10, and a bottom protection layer 11 is formed on the active surface of the chip 10. Figure 4 shown.
[0126] It should be noted that, in the present embodiment, the active surface of the chip 10 is the surface provided with the device pattern, and a bottom protective layer 11 is formed on the active surface of the chip 10, and the material of the bottom protective layer 11 includes silicon carbon nitride SiCN. It is worth mentioning that the bottom protective layer 11 can be used as an etching stop layer in subsequent steps. In addition, the bottom protective layer 11 also has the function of protecting the bottom metal layer in the sealing ring metal layer pattern 12 above it and protecting the device layer under the ILD (Inter Layer Dielectric) layer of the active surface of the chip 10 below it. Of course, in other embodiments, the bottom protective layer 11 may also include other materials with protective functions, and is not limited to the examples in the present embodiment.
[0127] Next, step S2 is performed to form a first sealing metal ring 12A and a second sealing metal ring 12B on the bottom protection layer 11. The first sealing metal ring 12A is located around the active surface of the chip 10, and the second sealing metal ring 12B is stacked on the first sealing metal ring 12A. Figure 5 shown.
[0128] In this embodiment, the first sealing metal ring 12A and the second sealing metal ring 12B each include at least one continuous metal ring structure, the continuous metal ring structure is formed by stacking the barrier layer 122, the metal layer 121 and the plug portion 123, and the plug portion 123B in the second sealing metal ring 12B is formed by extending downward from the metal layer 121B in the second sealing metal ring 12B, and metal interconnection is achieved through the barrier layer 122B in the second sealing metal ring 12B and the metal layer 121A in the first sealing metal ring 12A, so as to ensure the reliability of the chip sealing ring structure as an electrostatic protection device for grounding and the ability to conduct static electricity during wafer cutting, such as Figure 5 As shown. The metal layer 121, the barrier layer 122 and the plug portion 123 are formed by physical vapor deposition (PVD) or other methods of metal film growth that can be thought of by those skilled in the art. Of course, the plug portion 123B in the second sealing metal ring 12B can also be formed by filling with other metal filling plugs. In addition, the plug portion 123A in the first sealing metal ring 12A is metal-interconnected with the chip 10 through the barrier layer 122A in the first sealing metal ring 12A, wherein the plug portion 123A in the first sealing metal ring 12A can be formed integrally by extending downward from the metal layer 121A in the first sealing metal ring 12A using a dual damascene process, or can be formed by filling with other metal filling plugs. As an example, the material of the metal layer 121 includes metal copper or aluminum, the material of the barrier layer 122 includes titanium nitride or titanium, and the material of the plug portion 123 includes metal copper or aluminum or tungsten.
[0129] In addition, the number of continuous metal ring structures can be designed according to actual needs, taking into account the balance between sealing effect and occupied space layout. Figure 5 As shown, as an example, the first sealing metal ring 12A and the second sealing metal ring 12B each include a continuous metal ring structure.
[0130] In addition, it is worth mentioning that in this embodiment, the second sealing metal ring 12B is stacked on the first sealing metal ring 12A, that is, the area of the second sealing metal ring 12B on the first sealing metal ring 12A accounts for more than 80% of the overall top surface area of the second sealing metal ring 12B.
[0131] Next, step S3 is performed to form an insulating dielectric layer 13 on the bottom protection layer 11. The insulating dielectric layer 13 has an isolation ring groove 132 that exposes the second sealing metal ring 12B. The bottom of the isolation ring groove 132 does not expose the bottom protection layer 11. Figure 6 to Figure 10 shown.
[0132] The process of executing step S3 includes:
[0133] An insulating dielectric material 131 is formed on the bottom protection layer 11 to cover the first sealing metal ring 12A, the second sealing metal ring 12B and the bottom protection layer 11. Figure 6 shown.
[0134] A first mask 14 is disposed on the insulating dielectric material 131, wherein the first mask 14 has a mask opening 141 aligned with the first sealing metal ring 12A and the second sealing metal ring 12B. Figure 7 (a) and Figure 7 In the process of setting the first photomask 14 on the insulating dielectric material 131, a photoresist 133 is first formed on the insulating dielectric material 131, and then the first photomask 14 is placed above the photoresist 133, and the photomask opening 141 is aligned with the first sealing metal ring 12A and the second sealing metal ring 12B area, as shown in FIG. Figure 7 (a) and 7 (b). The pattern of the mask opening 141 enables the subsequently formed isolation ring groove 132 to fully or partially expose the upper part or top of the second sealing metal ring 12B. As a preferred embodiment, the pattern of the mask opening 141 enables the subsequently formed isolation ring groove 132 to expose the upper part or top of at least one continuous metal ring structure of the second sealing metal ring 12B.
[0135] The insulating dielectric material 131 is etched by using the mask opening 141 until an isolation ring groove 132 corresponding to the mask opening 141 is formed, thereby exposing the second sealing metal ring 12B while protecting the chip 10 area. Figure 7 (b) Figure 8 , Fig. 9 and Fig.10 As shown, the insulating dielectric layer 13 is obtained. In the process of etching the insulating dielectric material 131, specifically, as Figure 7 As shown in (b), the mask opening 141 of the first mask 14 is first aligned with the first sealing metal ring 12A and the second sealing metal ring 12B and focused, and then the photoresist 133 is exposed to ultraviolet light to copy the pattern of the mask opening 141 of the first mask 14 onto the photoresist 133 to obtain a patterned photoresist 133, as shown in FIG. Figure 8 As shown, the first photomask 14 is then removed, and the insulating dielectric material 131 is then dry-etched or wet-etched using the patterned photoresist 133 as a mask, or an etching method that can be thought of by a person skilled in the art, until the isolation ring groove 132 is formed, and the etching stops at the metal part of the second sealing metal ring 12B, wherein the metal part of the second sealing metal ring 12B includes the metal side of the middle part of the second sealing metal ring 12B and the metal top surface of the second sealing metal ring 12B, as well as other metal parts. As a preferred embodiment, the etching stops at the metal side of the middle part of the second sealing metal ring 12B or the metal top surface of the second sealing metal ring 12B, and more preferably, the etching stops at the metal side of the middle part of the second sealing metal ring 12B, as shown in FIG. Fig. 9 As shown, the upper part of the continuous metal ring structure of the second sealing metal ring 12B is exposed, and finally the patterned photoresist 133 is removed to obtain the following Fig.10 The structure shown.
[0136] In this embodiment, the material of the insulating dielectric layer 13 includes oxide. As an example, the material of the insulating dielectric layer 13 includes silicon oxide. Of course, in other embodiments, the insulating dielectric layer 13 may also include other materials with insulating isolation functions, and is not limited to the examples in this embodiment.
[0137] In addition, in this embodiment, the width of the isolation ring groove 132 is greater than or equal to the width of the second sealing metal ring 12B, so that the isolation ring groove 132 completely exposes the upper part or top of the second sealing metal ring 12B, and the first sealing metal ring 12A is embedded in the insulating dielectric layer 13. As an example, Figure 7 As shown in (a), the width d1 of the mask opening 141 is greater than or equal to the width d2 of the second sealing metal ring 12B, that is, d1≥d2, so that the width d3 of the isolation ring groove 132 formed subsequently is greater than or equal to the width d2 of the second sealing metal ring 12B, that is, d3≥d2, so that the isolation ring groove 132 formed subsequently completely exposes the upper part of the second sealing metal ring 12B, and the first sealing metal ring 12A is embedded in the insulating dielectric layer 13, as shown in FIG. Fig.10It should be noted that when the width d1 of the mask opening 141 is greater than or equal to the width d2 of the second sealing metal ring 12B, the isolation ring groove 132 can completely expose the upper part or top of the second sealing metal ring 12B, so that the moisture-proof layer 15 formed subsequently can cover and wrap the second sealing metal ring 12B with a larger area, thereby enhancing the sealing effect of the chip sealing ring structure of this embodiment.
[0138] In addition, it should be noted that, since the isolation ring groove 132 can completely expose the upper part or top of the second sealing metal ring 12B, and its bottom does not expose the bottom protection layer 11, in this embodiment, the part of the second sealing metal ring 12B exposed by the isolation ring groove 132 is called the first exposure part 12a, and the part of the insulating dielectric layer 13 exposed by the isolation ring groove 132 is called the second exposure part 13a. Due to the different patterns of the mask opening 141 and the different etching depths of the insulating dielectric material 131, the isolation ring groove 132 is also different accordingly, so the positions of the first exposure part 12a and the second exposure part 13a will also change accordingly. As a preferred solution, since the pattern of the mask opening 141 enables the subsequently formed isolation ring groove 132 to expose the upper part of at least one continuous metal ring structure of the second sealing metal ring 12B, the first exposed portion 12a of the second sealing metal ring 12B at least includes the upper sidewall and top of the exposed continuous metal ring structure; and since the etching stops at the middle of the insulating dielectric layer 13 when etching the insulating dielectric material 131, the second exposed portion 13a of the insulating dielectric layer 13 in the isolation ring groove 132 at least includes the surface of the insulating dielectric layer 13 located on both sides of the exposed continuous metal ring structure and at the bottom and sidewalls of the isolation ring groove 132. As an example, if Fig.10 As shown, since the second sealing metal ring 12B only includes a continuous metal ring structure, the isolation ring groove 132 completely exposes the upper part of the continuous metal ring structure. Therefore, the first exposed part 12a of the second sealing metal ring 12B is the upper side wall and top of the exposed continuous metal ring structure, and the second exposed part 13a of the insulating dielectric layer 13 in the isolation ring groove 132 is the surface of the insulating dielectric layer 13 located on both sides of the exposed continuous metal ring structure and at the bottom and side walls of the isolation ring groove 132. Therefore, the moisture-proof layer 15 formed subsequently covers the first exposed part 12a of the second sealing metal ring 12B, that is, covers the upper side wall and top of the exposed continuous metal ring structure, and the moisture-proof layer 15 formed subsequently covers the second exposed part 11a of the insulating dielectric layer 13 in the isolation ring groove 132, that is, covers the surface of the insulating dielectric layer 13 located on both sides of the exposed continuous metal ring structure and at the bottom and side walls of the isolation ring groove 132.
[0139] Next, step S4 is performed to form a moisture-proof layer 15 on the insulating dielectric layer 13 and in the isolation ring groove 132. The moisture-proof layer 15 covers the first exposed portion 12a of the second sealing metal ring 12B and the second exposed portion 13a of the insulating dielectric layer 13 in the isolation ring groove 132. Fig.10 and Fig.11 shown.
[0140] Furthermore, in this embodiment, the moisture-proof layer 15 on the insulating dielectric layer 13 and in the isolation ring groove 132, the first sealing metal ring 12A and the second sealing metal ring 12B isolate the insulating dielectric layer 13 into a peripheral layer portion and a central layer portion, such as Figure 7 In the top view shown in (a), the peripheral layer of the insulating dielectric layer 13 is located between the periphery of the first sealing metal ring 12A and the second sealing metal ring 12B and the cutting path 20, while the central layer of the insulating dielectric layer 13 is located on the active surface of the chip 10 surrounded by the first sealing metal ring 12A and the second sealing metal ring 12B. The chip sealing ring structure enhances the gas-liquid blocking capability through the combination of the first sealing metal ring 12A, the second sealing metal ring 12B and the moisture-proof layer 15, thereby preventing the internal components of the chip 10 in the central layer from being oxidized or corroded by gas and liquid.
[0141] In this embodiment, the material of the moisture-proof layer 15 includes nitride or oxynitride. As an example, the material of the moisture-proof layer 15 includes silicon nitride. It should be explained that the silicon nitride layer located in the isolation ring groove 132 covers the first exposed portion 12a of the second sealing metal ring 12B to form a silicon nitride support protective film (spacer nitride), which can effectively prevent the metal layer 121B in the second sealing metal ring 12B from being directly exposed to the air during the process and being oxidized or corroded by oxygen, water vapor or other gas and liquid. At the same time, the combination of the first sealing metal ring 12A, the second sealing metal ring 12B and the moisture-proof layer 15 can also effectively prevent the internal devices of the chip 10 in the central layer from being oxidized or corroded by gas and liquid. Compared with the existing process that mainly blocks oxygen, the ability to block gas and liquid to prevent corrosion will be better. Of course, in other embodiments, the moisture-proof layer 15 can also include other materials that have gas and liquid blocking capabilities and can effectively protect the metal layer.
[0142] In addition, the method for preparing the chip sealing ring structure of this embodiment further includes:
[0143] Step S5, forming a top cover layer 16 on the moisture-proof layer 15, such as Fig.12 shown.
[0144] In this embodiment, the material of the top cover layer 16 includes photoresist. The top cover layer 16 can be used as a mask layer to facilitate subsequent photolithography and etching processes.
[0145] The above steps finally produce Fig.12 The chip seal ring structure is shown.
[0146] In addition, in step S3 of the present embodiment, the insulating dielectric material 131 is dry-etched or wet-etched using the patterned photoresist 133 as a mask until the isolation ring groove 132 is formed, and the etching stops at the metal portion of the second sealing metal ring 12B. As another preferred embodiment, the etching stops at the metal top of the second sealing metal ring 12B. Fig.13 As shown, the metal top surface of the second sealing metal ring 12B is completely exposed, and finally the patterned photoresist 133 is removed to obtain Fig.14 Then, step S4 is performed to form a moisture-proof layer 15 on the insulating dielectric layer 13 and in the isolation ring groove 132. The moisture-proof layer 15 covers the first exposed portion 12a of the second sealing metal ring 12B and the second exposed portion 13a of the insulating dielectric layer 13 in the isolation ring groove 132. Fig.15 Finally, step S5 is performed to form a top covering layer 16 on the moisture-proof layer 15, and finally the Fig.16 The chip seal ring structure is shown.
[0147] It is worth mentioning that Fig.12 and Fig.16 The chip sealing ring structure shown is only an example of a case where the second sealing metal ring 12B includes a continuous metal ring structure; in this case, a first mask 14 is disposed on the insulating dielectric material 131, and the width d1 of the mask opening 141 is greater than or equal to the width d2 of the second sealing metal ring 12B. Figure 7 (a), that is, d1≥d2, so that the width d3 of the isolation ring groove 132 formed subsequently is greater than or equal to the width d2 of the second sealing metal ring 12B, that is, d3≥d2. Therefore, if the isolation ring groove 132 completely exposes the upper part of the second sealing metal ring 12B, the final result is as follows Fig.12 If the isolation ring groove 132 completely exposes the top of the second sealing metal ring 12B, the final result is as follows Fig.16 The chip seal ring structure is shown.
[0148] As another example, the second sealing metal ring 12B includes two continuous metal ring structures; in this case, a first mask 14 is disposed on the insulating dielectric material 131, and the width d1 of the mask opening 141 is greater than or equal to the width d2 of the second sealing metal ring 12B. Fig.17 (a), that is, d1≥d2, so that the width d3 of the isolation ring groove 132 formed subsequently is greater than or equal to the width d2 of the second sealing metal ring 12B, that is, d3≥d2. Therefore, if the isolation ring groove 132 completely exposes the upper part of the second sealing metal ring 12B, the final result is as follows Fig.17 (b) shows the chip sealing ring structure; if the isolation ring groove 132 completely exposes the top of the second sealing metal ring 12B, the final result is as follows Fig.17 (c) shows the chip sealing ring structure.
[0149] As a third example, the second sealing metal ring 12B includes three continuous metal ring structures; in this case, a first mask 14 is disposed on the insulating dielectric material 131, and the width d1 of the mask opening 141 is greater than or equal to the width d2 of the second sealing metal ring 12B. Figure 8 (a), that is, d1≥d2, so that the width d3 of the isolation ring groove 132 formed subsequently is greater than or equal to the width d2 of the second sealing metal ring 12B, that is, d3≥d2. Therefore, if the isolation ring groove 132 completely exposes the upper part of the second sealing metal ring 12B, the final result is as follows Fig.18 (b) shows the chip sealing ring structure; if the isolation ring groove 132 completely exposes the top of the second sealing metal ring 12B, the final result is as follows Fig.18 (c) shows the chip sealing ring structure.
[0150] In addition, in this embodiment, the width of the isolation ring groove 132 may also be smaller than the width of the second sealing metal ring 12B, so that the isolation ring groove 132 partially exposes the upper part or top of the second sealing metal ring 12B, and the first sealing metal ring 12A is embedded in the insulating dielectric layer 13. Therefore, in the process of performing step S3, the pattern of the mask opening 141 can make the isolation ring groove 132 formed subsequently partially expose the upper part or top of the second sealing metal ring 12B. As an example, Fig.19 (a) and Fig.19 As shown in (b), a first mask 14 is disposed on the insulating dielectric isolation material 131; then, the insulating dielectric material 131 is etched using the pattern of the mask opening 141 of the first mask 14 until an isolation ring groove 132 having a pattern corresponding to the mask opening 141 is formed, and the etching stops at the metal top surface of the second sealing metal ring 12B, thereby partially exposing the top of the second sealing metal ring 12B while protecting the chip 10 area, as shown in FIG. Fig. 20 and Fig.21 Then, step S4 is performed to form a moisture-proof layer 15 on the insulating dielectric layer 13 and in the isolation ring groove 132. The moisture-proof layer 15 covers the first exposed portion 12a of the second sealing metal ring 12B and the second exposed portion 13a of the insulating dielectric layer 13 in the isolation ring groove 132. Fig. 22 Finally, step S5 is performed to form a top covering layer 16 on the moisture-proof layer 15, and finally the Fig.23 The chip seal ring structure is shown.
[0151] Among them, the first mask 14 has a mask opening 141 positioned to be aligned with the first sealing metal ring 12A and the second sealing metal ring 12B, and the width d1 of the mask opening 141 is smaller than the width d2 of the second sealing metal ring 12B, that is, d1<d2, so that the subsequently formed isolation ring groove 132 partially exposes the top of the second sealing metal ring 12B, so that the subsequently formed moisture-proof layer 15 can cover a portion of the top surface of the metal layer 121B in the second sealing metal ring 12B. The gas-liquid blocking capability is enhanced by the combination of the first sealing metal ring 12A, the second sealing metal ring 12B and the moisture-proof layer 15, and the sealing effect of the chip sealing ring structure of this embodiment is enhanced while occupying a smaller space layout.
[0152] It needs to be explained that Fig.23 The chip sealing ring structure shown is only an example of a case where the second sealing metal ring 12B includes a continuous metal ring structure; in this case, a first mask 14 is disposed on the insulating dielectric isolation material 131, and the width d1 of the mask opening 141 is smaller than the width d2 of the second sealing metal ring 12B. Fig.19 As shown in (a), i.e., d1<d2, so that the width d3 of the subsequently formed isolation ring groove 132 is smaller than the width d2 of the second sealing metal ring 12B, i.e., d3<d2, so that the subsequently formed isolation ring groove 132 partially exposes the top of the second sealing metal ring 12B, and finally obtains the following Fig.23 The chip seal ring structure is shown.
[0153] As another example, the second sealing metal ring 12B includes two continuous metal ring structures; in this case, the first mask 14 is disposed on the insulating dielectric material 131, and the width d1 of the mask opening 141 is smaller than the width d2 of the second sealing metal ring 12B. Fig.24 (a), that is, d1<d2, so that the width d3 of the isolation ring groove 132 formed subsequently is less than or equal to the width d2 of the second sealing metal ring 12B, that is, d3<d2. Therefore, if the isolation ring groove 132 partially exposes the upper part of the second sealing metal ring 12B, the final result is as follows Fig.24 (b) shows the chip sealing ring structure; if the isolation ring groove 132 partially exposes the top of the second sealing metal ring 12B, the final result is as follows Fig.24 (c) shows the chip sealing ring structure.
[0154] As a third example, the second sealing metal ring 12B includes three continuous metal ring structures; in this case, a first mask 14 is disposed on the insulating dielectric material 131, and the width d1 of the mask opening 141 is smaller than the width d2 of the second sealing metal ring 12B. Fig.25(a), that is, d1<d2, so that the width d3 of the isolation ring groove 132 formed subsequently is less than or equal to the width d2 of the second sealing metal ring 12B, that is, d3<d2. Therefore, if the isolation ring groove 132 partially exposes the upper part of the second sealing metal ring 12B, the final result is as follows Fig.25 (b) shows the chip sealing ring structure; if the isolation ring groove 132 partially exposes the top of the second sealing metal ring 12B, the final result is as follows Fig.24 (c) shows the chip sealing ring structure.
[0155] In addition, in this embodiment, when the first mask 14 is provided, the mask opening 141 pattern is designed as an interval pattern according to actual needs, so that the isolation ring groove 132 formed subsequently exposes the continuous metal ring structure in the sealing ring metal layer pattern at intervals. As an example, the second sealing metal ring 12B includes three continuous metal ring structures. The mask opening 141 pattern of the first mask 14 provided on the insulating dielectric material 131 is as follows: Fig.26 As shown in (a), the pattern of the mask opening 141 can make the isolation ring groove 132 formed subsequently expose the upper part or top of the inner continuous metal ring structure and the upper part or top of the outer continuous metal ring structure in the second sealing metal ring 12B, while the insulating dielectric layer 13 is still retained on the middle continuous metal ring structure, and the width of the isolation ring groove 132 is greater than or equal to the width of any continuous metal ring structure in the second sealing metal ring 12B, so that the final result is as shown in FIG. Fig.26 (b) or Fig.26 (c) shows the chip sealing ring structure. Of course, the pattern of the mask opening 141 can also be designed according to actual needs, taking into account the balance between the sealing effect and the occupied space layout.
[0156] In addition, in this embodiment, when setting the first mask 14, the mask opening 141 is designed according to actual needs, so that the mask opening 141 is aligned with the selected area of the second sealing metal ring 12B, so that the isolation ring groove 132 formed subsequently exposes the selected area of the second sealing metal ring 12B. It should be noted that the isolation ring groove 132 exposes the selected area of the second sealing metal ring 12B, so that the moisture-proof layer 15 formed in the subsequent process can wrap the surface of the second sealing metal ring 12B covering the selected area; by covering the moisture-proof layer 15 in the selected area, the circuit or device accessories that are more easily corroded by gas and liquid or need to be protected can be sealed and protected. As an example, Fig. 27 and Fig.28As shown, the right parts of the two continuous metal ring structures are used together as the selected area of the second sealing metal ring 12B, and the width of the mask opening 141 is designed to be larger and smaller than the width of the second sealing metal ring 12B, respectively. Then, the mask opening 141 is aligned with the selected area of the second sealing metal ring 12B, and finally, a moisture-proof layer 15 is formed in the selected area to wrap and cover the surface of the second sealing metal ring 12B, which can effectively enhance the sealing effect of the selected area.
[0157] The preparation method of the chip sealing ring structure of the present embodiment forms a moisture-proof layer 15 on the surface of the second sealing metal ring 12B by utilizing the manufacturing process of the circuit area of the chip 10 without increasing the process flow. The moisture-proof layer 15 wraps a part of the metal layer 121 in the second sealing metal ring 12B. The combination of the first sealing metal ring 12A, the second sealing metal ring 12B and the moisture-proof layer 15 can effectively prevent the metal layer 121 from being directly exposed to the air during the manufacturing process and being oxidized or corroded by oxygen, water vapor or other gases and liquids. At the same time, it also prevents the internal devices in the central layer of the chip 10 from being oxidized or corroded by gases and liquids, greatly enhancing the gas-liquid blocking ability without reducing the ability to block stress expansion and rupture. Compared with the prior art that mainly blocks oxygen, it also enhances the ability to resist corrosion to water vapor or other gases and liquids, thereby preventing the electrical performance and reliability of the chip 10 from being affected.
[0158] The step division of the above methods is only for the purpose of clear description. When implemented, they can be combined into one step or some steps can be split and decomposed into multiple steps. As long as they contain the same logical relationship, they are all within the scope of protection of this patent; adding insignificant modifications to the algorithm or process or introducing insignificant designs without changing the core design of the algorithm and process are all within the scope of protection of this patent.
[0159] A second embodiment of the present invention relates to a method for preparing a semiconductor chip, which at least comprises: preparing a chip sealing ring structure by using the method for preparing a chip sealing ring structure as described in the first embodiment of the present invention.
[0160] It is not difficult to find that this embodiment needs to be implemented in conjunction with the first embodiment, so the relevant technical details mentioned in the first embodiment are still valid in this embodiment, and in order to reduce repetition, they are not repeated here. Accordingly, the relevant technical details mentioned in this embodiment can also be applied in the first embodiment.
[0161] The method for preparing a semiconductor chip of this embodiment adopts the method for preparing a chip sealing ring structure of the first embodiment of the present invention to prepare a chip sealing ring structure. The prepared chip sealing ring structure can effectively block stress expansion and cracking, and has strong gas-liquid blocking ability, and can effectively resist the erosion of water vapor or other gas and liquid, thereby protecting the internal devices of the chip. Therefore, the semiconductor chip obtained by the above method has excellent electrical performance and reliability.
[0162] A third embodiment of the present invention relates to a method for preparing a semiconductor chip, such as Figure 29 to Figure 33 As shown, it at least includes:
[0163] A wafer is provided, on which a plurality of chips 10 and dicing lanes 20 between adjacent chips 10 are prepared. Fig.29 shown.
[0164] By adopting the method for preparing the chip sealing ring structure according to the first embodiment of the present invention, a chip sealing ring structure is prepared in the surrounding area of the chip 10 and along the cutting road 20, as shown in FIG. Fig.29 As shown, Fig.17 (a) Fig.29 A partial enlarged view of a in the figure. A pad metal layer pattern 17 is formed while forming the first sealing metal ring 12A and the second sealing metal ring 12B. The pad metal layer pattern 17 is located in the surrounding area of the chip 10, and the pad metal layer pattern 17 is wrapped in the central layer of the insulating dielectric layer 13, as shown in FIG. Fig.30 It is worth mentioning that, in this embodiment, without increasing the process flow, the first sealing metal ring 12A, the second sealing metal ring 12B and the pad metal layer pattern 17 are simultaneously prepared by using the chip 10 circuit area manufacturing process.
[0165] A pad opening 171 is formed above the pad metal layer pattern 17 to expose the pad region of the chip 10 .
[0166] In addition, in this embodiment, the step of forming the pad opening 171 above the pad metal layer pattern 17 is as follows: Figure 30 to Figure 33 As shown, including:
[0167] A top covering layer 16 is formed on the moisture-proof layer 15, such as Fig.30 shown.
[0168] A second mask 18 is disposed on the top cover layer 16, such as Fig.31 and Fig.32 As shown, Fig.31 It is a top view of the second mask 18 disposed on the top cover layer 16, that is, a mask image covering the pad position.
[0169] The top cover layer 16 is patterned by using the opening pattern of the second photomask 18, and the moisture-proof layer 15 and the insulating dielectric layer 13 are etched until a pad opening 171 is formed above the pad metal layer pattern 17, and the pad metal layer pattern 17 is exposed in the pad metal layer pattern 17 as a chip pad, thereby exposing the pad area of the chip 10, such as Fig.32 and Fig.33 shown.
[0170] In addition, in this embodiment, the method for preparing the semiconductor chip further includes:
[0171] The wafer is cut along the dicing streets 20 to obtain a plurality of semiconductor chips 10 .
[0172] It is not difficult to find that this embodiment needs to be implemented in conjunction with the first embodiment, so the relevant technical details mentioned in the first embodiment are still valid in this embodiment, and in order to reduce repetition, they are not repeated here. Accordingly, the relevant technical details mentioned in this embodiment can also be applied in the first embodiment.
[0173] The method for preparing the semiconductor chip of the present embodiment adopts the method for preparing the chip sealing ring structure of the first embodiment of the present invention. On a wafer with a plurality of chips 10, a chip sealing ring structure is simultaneously prepared in the surrounding area of each chip 10 and along the cutting path 20, and the chip 10 circuit area manufacturing process is used to form a pad metal layer pattern 17 while forming the first sealing metal ring 12A and the second sealing metal ring 12B, and a pad opening 171 is formed above the pad metal layer pattern 17 to open the pad area of each chip 10, and finally the wafer is cut along the cutting path 20 to obtain a plurality of semiconductor chips 10; when the wafer cutting process is performed along the cutting path 20, the chip sealing ring structure can effectively block stress expansion and rupture, and at the same time has a strong gas-liquid blocking ability, and can effectively resist the erosion of water vapor or other gas-liquids. Therefore, the semiconductor chip 10 obtained by the above method has excellent electrical performance and reliability.
[0174] A fourth embodiment of the present invention relates to a chip sealing ring structure, such as Fig.12 As shown, it at least includes:
[0175] Chip 10.
[0176] The bottom protection layer 11 is located on the active surface of the chip 10 .
[0177] The first sealing metal ring 12A is located on the bottom protection layer 11 and around the active surface of the chip 10.
[0178] The second sealing metal ring 12B is located on the first sealing metal ring 12A.
[0179] The insulating dielectric layer 13 is located on the bottom protection layer 11, and the insulating dielectric layer 13 has an isolation ring groove 132 that exposes the second sealing metal ring 12B, and the bottom of the isolation ring groove 132 does not expose the bottom protection layer 11. And,
[0180] The moisture-proof layer 15 is located on the insulating medium layer 13 and in the isolation ring groove 132 . The moisture-proof layer 15 covers the first exposed portion 12 a of the second sealing metal ring 12B and the second exposed portion 13 a of the insulating medium layer 13 in the isolation ring groove 132 .
[0181] Among them, the moisture-proof layer 15, the first sealing metal ring 12A and the second sealing metal ring 12B on the insulating dielectric layer 13 and in the isolation ring groove 132 isolate the insulating dielectric layer 13 into a peripheral layer and a central layer. The chip sealing ring structure enhances the gas-liquid blocking capability through the combination of the first sealing metal ring 12A, the second sealing metal ring 12B and the moisture-proof layer 15, thereby preventing the internal devices of the chip 10 in the central layer from being oxidized or corroded by gas and liquid.
[0182] In addition, in the present embodiment, the bottom surface of the moisture-proof layer 15 located in the isolation ring groove 132 is connected to and covers the upper portion or the top portion of the second sealing metal ring 12B.
[0183] In addition, in the present embodiment, the width of the isolation ring groove 132 is greater than or equal to the width of the second sealing metal ring 12B, so that the upper part or the top of the second sealing metal ring 12B is completely exposed in the isolation ring groove 132, the first sealing metal ring 12A is embedded in the insulating dielectric layer 13, and the upper surface or the top surface of the second sealing metal ring 12B is covered with a moisture-proof layer 15. The moisture-proof layer 15 can cover and wrap the second sealing metal ring 12B with a larger area, thereby enhancing the sealing effect of the chip sealing ring structure of the present embodiment.
[0184] In addition, in the present embodiment, the first sealing metal ring 12A and the second sealing metal ring 12B each include at least one continuous metal ring structure, the continuous metal ring structure is formed by staggered stacking of the barrier layer 122 and the metal layer 121, and the plug portion 123B in the second sealing metal ring 12B is formed by extending downward from the metal layer 121B in the second sealing metal ring 12B, and metal interconnection is achieved through the barrier layer 122 of the second sealing metal ring 12B and the metal layer 121A in the first sealing metal ring 12A, such as Fig.11 As an example, the material of the metal layer 121 includes metal aluminum, the material of the barrier layer 122 includes titanium nitride or titanium, and the material of the plug portion 123 includes metal tungsten.
[0185] Furthermore, in this embodiment, the isolation ring groove 132 at least exposes the metal top of the continuous metal ring structure of the second sealing metal ring 12B.
[0186] As an example, the second sealing metal ring 12B includes a continuous metal ring structure. If the isolation ring groove 132 completely exposes the upper portion of the second sealing metal ring 12B, the following structure is formed: Fig.12 If the isolation ring groove 132 completely exposes the top of the second sealing metal ring 12B, the chip sealing ring structure shown in FIG. Fig.16 The chip seal ring structure is shown.
[0187] As another example, the second sealing metal ring 12B includes two continuous metal ring structures. If the isolation ring groove 132 completely exposes the upper portion of the second sealing metal ring 12B, a structure such as Fig.17 (b) shows the chip sealing ring structure; if the isolation ring groove 132 completely exposes the top of the second sealing metal ring 12B, a structure such as Fig.17 (c) shows the chip sealing ring structure.
[0188] As a third example, the second sealing metal ring 12B includes three continuous metal ring structures. If the isolation ring groove 132 completely exposes the upper portion of the second sealing metal ring 12B, the following structure is formed: Fig.18 (b) shows the chip sealing ring structure; if the isolation ring groove 132 completely exposes the top of the second sealing metal ring 12B, a structure such as Fig.18 (c) shows the chip sealing ring structure.
[0189] In addition, in this embodiment, the width of the isolation ring groove 132 can also be smaller than the width of the second sealing metal ring 12B, so that the upper part or the top part of the second sealing metal ring 12B is exposed in the isolation ring groove 132, and the first sealing metal ring 12A is embedded in the insulating dielectric layer 13. The subsequently formed moisture-proof layer 15 can cover and wrap the first exposed part 12a of the second sealing metal ring 12B and the second exposed part 13a of the insulating dielectric layer 13 in the isolation ring groove 132, thereby enhancing the sealing effect of the chip sealing ring structure of this embodiment while occupying a smaller space layout.
[0190] As an example, the second sealing metal ring 12B includes a continuous metal ring structure, and the isolation ring groove 132 partially exposes the top of the second sealing metal ring 12B, forming a Fig.23 The chip seal ring structure is shown.
[0191] As another example, the second sealing metal ring 12B includes two continuous metal ring structures. If the isolation ring groove 132 partially exposes the upper portion of the second sealing metal ring 12B, the following structure is formed: Fig.24 (b) shows the chip sealing ring structure; if the isolation ring groove 132 partially exposes the top of the second sealing metal ring 12B, a structure such as Fig.24 (c) shows the chip sealing ring structure.
[0192] As a third example, the second sealing metal ring 12B includes three continuous metal ring structures. If the isolation ring groove 132 partially exposes the upper portion of the second sealing metal ring 12B, the following structure is formed: Fig.25 (b) shows the chip sealing ring structure; if the isolation ring groove 132 partially exposes the top of the second sealing metal ring 12B, a structure such as Fig.24 (c) shows the chip sealing ring structure.
[0193] As a fourth example, the second sealing metal ring 12B includes three continuous metal ring structures, the isolation ring groove 132 exposes the upper part or top of the inner ring continuous metal ring structure and the upper part or top of the outer ring continuous metal ring structure in the second sealing metal ring 12B, and the insulating dielectric layer 13 is still retained on the middle continuous metal ring structure, forming Fig.26 (b) or Fig.26 (c) shows the chip sealing ring structure.
[0194] In addition, in this embodiment, the position of the isolation ring groove 132 is designed according to actual needs, so that the isolation ring groove 132 exposes the selected area of the second sealing metal ring 12B. It should be noted that the isolation ring groove 132 exposes the selected area of the second sealing metal ring 12B, so that the moisture-proof layer 15 formed in the subsequent process can wrap the surface of the second sealing metal ring 12B covered in the selected area; by covering the moisture-proof layer 15 in the selected area, the circuit or device accessories that are more easily corroded by gas and liquid or need to be protected can be sealed and protected, effectively enhancing the sealing effect of the selected area.
[0195] In this embodiment, the material of the moisture-proof layer 15 includes nitride or nitride oxide.
[0196] In this embodiment, the material of the bottom protection layer 11 includes silicon carbon nitride.
[0197] In this embodiment, the material of the insulating dielectric layer 13 includes oxide.
[0198] In addition, the chip sealing ring structure of this embodiment further includes:
[0199] The top covering layer 16 is located on the moisture-proof layer 15 .
[0200] In this embodiment, the material of the top cover layer 16 includes polyimide or benzoylcyclobutene (BCB). The top cover layer 16 has a passivation effect, which can protect the moisture-proof layer 15 below it, and provide a protective passivation effect for other subsequent processes. Of course, in other embodiments, the top cover layer 16 can also include other materials with a protective passivation effect, and is not limited to the examples in this embodiment.
[0201] It is not difficult to find that this embodiment is a product implementation method corresponding to the first embodiment, and this embodiment can be implemented in conjunction with the first embodiment. The relevant technical details mentioned in the first embodiment are still valid in this embodiment, and in order to reduce repetition, they are not repeated here. Accordingly, the relevant technical details mentioned in this embodiment can also be applied in the first embodiment.
[0202] In the chip sealing ring structure of the present embodiment, a moisture-proof layer 15 is formed on the surface of the second sealing metal ring 12B, and the moisture-proof layer 15 is wrapped on the metal layer. The combination of the first sealing metal ring 12A, the second sealing metal ring 12B and the moisture-proof layer 15 can effectively prevent the metal layer from being directly exposed to the air during the manufacturing process and being oxidized or corroded by oxygen, water vapor or other gases and liquids, and also prevent the internal components of the chip in the central layer from being oxidized or corroded by gas and liquids, thereby greatly enhancing the gas-liquid blocking ability without reducing the ability to block stress expansion and rupture. Compared with the prior art that mainly blocks oxygen, the ability to resist corrosion from water vapor or other gases and liquids is also enhanced, thereby preventing the electrical performance and reliability of the chip 10 from being affected.
[0203] A fifth embodiment of the present invention relates to a semiconductor chip, which at least includes: the chip sealing ring structure as described in the fourth embodiment of the present invention.
[0204] It is not difficult to find that the semiconductor chip involved in this embodiment adopts the chip sealing ring structure involved in the fourth embodiment, so the relevant technical details mentioned in the fourth embodiment are still valid in this embodiment, and in order to reduce repetition, they are not repeated here. Correspondingly, the relevant technical details mentioned in this embodiment can also be applied to the fourth embodiment.
[0205] The semiconductor chip of this embodiment, due to the chip sealing ring structure involved in the fourth embodiment of the present invention, can effectively prevent the metal layer from being directly exposed to the air during the manufacturing process and being oxidized or corroded by oxygen, water vapor or other gases and liquids, thereby greatly enhancing the gas-liquid barrier capability, effectively protecting the internal devices of the chip in the central layer, and not reducing the ability to block stress expansion and rupture; compared with the prior art that mainly blocks oxygen, it also enhances the ability to resist corrosion by water vapor or other gases and liquids, thereby avoiding the impact on the electrical performance and reliability of the chip.
[0206] A sixth embodiment of the present invention relates to a semiconductor device structure, such as Fig.29 and Fig.33 As shown, it at least includes:
[0207] The wafer includes a plurality of chips 10 and dicing lanes 20 between adjacent chips 10 ; wherein the chip 10 includes the chip sealing ring structure involved in the fourth embodiment of the present invention.
[0208] The pad metal layer pattern 17 is located in the peripheral area of the chip 10 , and the pad metal layer pattern 17 is wrapped in the central layer portion of the insulating dielectric layer 13 .
[0209] The insulating dielectric layer 13 also has a pad opening 171 located above the pad metal layer pattern 17 . The pad opening 171 also passes through the moisture-proof layer 15 , and the exposed portion of the pad metal layer pattern 17 serves as a chip pad, thereby exposing the pad area of the chip 10 .
[0210] It is not difficult to find that the semiconductor device structure involved in this embodiment includes the chip sealing ring structure involved in the fourth embodiment, so the relevant technical details mentioned in the fourth embodiment are still valid in this embodiment, and in order to reduce repetition, they are not repeated here. Correspondingly, the relevant technical details mentioned in this embodiment can also be applied to the fourth embodiment.
[0211] The semiconductor device structure of this embodiment adopts the chip sealing ring structure of the fourth embodiment of the present invention, and forms a chip sealing ring structure between the surrounding area of each chip 10 on the wafer and the cutting path 20 at the same time, and forms a pad metal layer pattern 17 while forming the second sealing metal ring 12B, and forms a pad opening 171 above the pad metal layer pattern 17 to open the pad area of each chip 10; when the wafer is cut along the cutting path 20, the chip sealing ring structure can effectively block the stress expansion and rupture ability, and at the same time has a strong gas-liquid blocking ability, and can effectively resist the erosion of water vapor or other gas-liquids. Therefore, the semiconductor chip obtained by cutting the wafer has excellent electrical performance and reliability.
[0212] In summary, the chip sealing ring structure and the manufacturing method thereof, the semiconductor chip and the manufacturing method thereof of the present invention have the following beneficial effects:
[0213] The chip sealing ring structure and preparation method thereof of the present invention utilize the chip circuit area manufacturing process to form a moisture-proof layer on the surface of the second sealing metal ring without increasing the process flow, and the moisture-proof layer wraps part of the metal layer in the second sealing metal ring. The combination of the first sealing metal ring, the second sealing metal ring and the moisture-proof layer can effectively prevent the metal layer from being directly exposed to the air during the process and being oxidized or corroded by oxygen, water vapor or other gases and liquids, and also prevent the internal devices of the chip in the central layer from being oxidized or corroded by gas and liquids, greatly enhancing the gas-liquid blocking ability without reducing the stress expansion and rupture blocking ability; compared with the prior art that mainly blocks oxygen, the ability to resist corrosion to water vapor or other gases and liquids is also enhanced, thereby preventing the electrical performance and reliability of the chip from being affected.
[0214] The semiconductor chip and the preparation method thereof of the present invention adopt the chip sealing ring structure and the preparation method thereof of the present invention. On a wafer with a plurality of chips, a chip sealing ring structure is simultaneously prepared between the surrounding area of each chip and the cutting path, and a chip circuit area manufacturing process is utilized to form a pad metal layer pattern while forming a first sealing metal ring and a second sealing metal ring, and a pad opening is formed above the pad metal layer pattern to open the pad area of each chip, and finally the wafer is cut along the cutting path to obtain a plurality of semiconductor chips. When the wafer cutting process is performed along the cutting path, the chip sealing ring structure can effectively block stress expansion and rupture capabilities, and at the same time has a strong gas-liquid blocking capability, and can effectively resist the erosion of water vapor or other gas-liquids. Therefore, the semiconductor chip obtained by the above method has excellent electrical performance and reliability.
[0215] Therefore, the present invention effectively overcomes various shortcomings in the prior art and has high industrial utilization value.
[0216] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the technology may modify or change the above embodiments without violating the spirit and scope of the present invention. Therefore, all equivalent modifications or changes made by a person of ordinary skill in the art without departing from the spirit and technical ideas disclosed by the present invention shall still be covered by the claims of the present invention.
Claims
1. A method for preparing a chip sealing ring structure, characterized in that: The steps include: Providing a chip (10), wherein a bottom protection layer (11) is formed on an active surface of the chip (10); A first sealing metal ring (12A) and a second sealing metal ring (12B) are formed on the bottom protection layer (11), wherein the first sealing metal ring (12A) is located around the active surface of the chip (10), and the second sealing metal ring (12B) is disposed on the first sealing metal ring (12A) in a stacked manner; An insulating dielectric layer (13) is formed on the bottom protective layer (11), the insulating dielectric layer (13) having an isolation ring groove (132) exposing the second sealing metal ring (12B), the top surface of the second sealing metal ring (12B) being higher than the bottom surface of the isolation ring groove (132), and the bottom of the isolation ring groove (132) does not expose the bottom protective layer (11); A moisture-proof layer (15) is formed on the insulating dielectric layer (13) and in the isolation ring groove (132), wherein the moisture-proof layer (15) covers a first exposed portion (12a) of the second sealing metal ring (12B) and a second exposed portion (13a) of the insulating dielectric layer (13) in the isolation ring groove (132); The moisture-proof layer (15), the first sealing metal ring (12A) and the second sealing metal ring (12B) on the insulating dielectric layer (13) and in the isolation ring groove (132) isolate the insulating dielectric layer (13) into a peripheral layer portion and a central layer portion. The chip sealing ring structure enhances the gas-liquid blocking capability through the combination of the first sealing metal ring (12A), the second sealing metal ring (12B) and the moisture-proof layer (15), thereby preventing the internal components of the chip (10) in the central layer portion from being oxidized or corroded by gas and liquid.
2. The method for preparing a chip sealing ring structure according to claim 1, characterized in that: The step of forming the insulating dielectric layer (13) on the bottom protective layer (11) comprises: forming an insulating dielectric material (131) on the bottom protective layer (11) to cover the first sealing metal ring (12A), the second sealing metal ring (12B) and the bottom protective layer (11); A first mask (14) is arranged on the insulating dielectric material (131), wherein the first mask (14) has a mask opening (141) aligned with the first sealing metal ring (12A) and the second sealing metal ring (12B) regions; and The insulating dielectric material (131) is etched using the mask opening (141) until the isolation ring groove (132) corresponding to the mask opening (141) is formed, thereby exposing the second sealing metal ring (12B).
3. The method for preparing a chip sealing ring structure according to claim 1, characterized in that: The isolation ring groove (132) exposes the upper part or top of the second sealing metal ring (12B).
4. The method for preparing a chip sealing ring structure according to claim 2, characterized in that: During the process of etching the insulating dielectric material (131), the etching stops at the metal portion of the second sealing metal ring (12B).
5. The method for preparing a chip sealing ring structure according to claim 4, characterized in that: In the process of etching the insulating dielectric material (131), the etching stops at the metal side surface of the middle part of the second sealing metal ring (12B) or the metal top surface of the second sealing metal ring (12B).
6. The method for preparing a chip sealing ring structure according to claim 1, characterized in that: The width of the isolation ring groove (132) is greater than or equal to the width of the second sealing metal ring (12B), so that the isolation ring groove (132) completely exposes the upper part or top of the second sealing metal ring (12B), and the first sealing metal ring (12A) is embedded in the insulating dielectric layer (13).
7. The method for preparing a chip sealing ring structure according to claim 1, characterized in that: The width of the isolation ring groove (132) is smaller than the width of the second sealing metal ring (12B), so that the isolation ring groove (132) partially exposes the upper part or top of the second sealing metal ring (12B), and the first sealing metal ring (12A) is embedded in the insulating dielectric layer (13).
8. The method for preparing a chip sealing ring structure according to claim 1, characterized in that: The first sealing metal ring (12A) and the second sealing metal ring (12B) each comprise at least one continuous metal ring structure, wherein the continuous metal ring structure is formed by stacking a barrier layer (122), a metal layer (121) and a plug portion (123), and the plug portion (123B) in the second sealing metal ring (12B) is formed integrally by extending downward from the metal layer (121B) in the second sealing metal ring (12B), and metal interconnection is achieved through the barrier layer (122B) in the second sealing metal ring (12B) and the metal layer (121A) in the first sealing metal ring (12A).
9. The method for preparing a chip sealing ring structure according to claim 1, characterized in that: The material of the moisture-proof layer (15) comprises nitride or oxynitride, the material of the bottom protection layer (11) comprises silicon carbon nitride, and the material of the insulating dielectric layer (13) comprises oxide.
10. The method for preparing a chip sealing ring structure according to claim 1, characterized in that: Also includes: A top covering layer (16) is formed on the moisture-proof layer (15).
11. A method for preparing a semiconductor chip, characterized in that: The method for preparing the semiconductor chip at least comprises: preparing a chip sealing ring structure by using the method for preparing a chip sealing ring structure according to any one of claims 1 to 10.
12. A method for preparing a semiconductor chip, characterized in that: include: Providing a wafer, on which a plurality of chips (10) and dicing lanes (20) located between adjacent chips (10) are prepared; The chip sealing ring structure is prepared in the peripheral area of the chip (10) and along the cutting path (20) by using the method for preparing the chip sealing ring structure as claimed in claim 1; wherein a pad metal layer pattern (17) is formed while forming the first sealing metal ring (12A) and the second sealing metal ring (12B); the pad metal layer pattern (17) is located in the peripheral area of the chip (10), and the pad metal layer pattern (17) is partially wrapped in the insulating dielectric layer (13); A pad opening (171) is formed above the pad metal layer pattern (17) to expose the pad region of the chip (10).
13. The method for preparing a semiconductor chip according to claim 12, characterized in that: The step of forming the pad opening (171) above the pad metal layer pattern (17) comprises: forming a top covering layer (16) on the moisture-proof layer (15); A second light mask (18) is arranged on the top covering layer (16); The top cover layer (16) is patterned using the second photomask (18), and the moisture-proof layer (15) and the insulating dielectric layer (13) are etched until the pad opening (171) is formed above the pad metal layer pattern (17), and the portion of the pad metal layer pattern (17) exposed in the pad opening (171) serves as a chip pad, thereby exposing the pad area of the chip (10).
14. The method for preparing a semiconductor chip according to claim 12, characterized in that: Also includes: The wafer is cut along the cutting path (20) to obtain a plurality of semiconductor chips.
15. A chip sealing ring structure, characterized in that: include: Chip (10); A bottom protective layer (11) located on the active surface of the chip (10); A first sealing metal ring (12A) is located on the bottom protection layer (11) and is located around the active surface of the chip (10); A second sealing metal ring (12B) is arranged on the first sealing metal ring (12A) in a stacked manner; an insulating dielectric layer (13) located on the bottom protective layer (11), the insulating dielectric layer (13) having an isolation ring groove (132) exposing the second sealing metal ring (12B), the top surface of the second sealing metal ring (12B) being higher than the bottom surface of the isolation ring groove (132), and the bottom of the isolation ring groove (132) not exposing the bottom protective layer (11); and a moisture-proof layer (15) located on the insulating dielectric layer (13) and in the isolation ring groove (132), the moisture-proof layer (15) covering a first exposed portion (12a) of the second sealing metal ring (12B) and a second exposed portion (13a) of the insulating dielectric layer (13) in the isolation ring groove (132); The moisture-proof layer (15), the first sealing metal ring (12A) and the second sealing metal ring (12B) isolate the insulating medium layer (13) into a peripheral layer portion and a central layer portion, and the chip sealing ring structure enhances the gas-liquid blocking capability through the combination of the first sealing metal ring (12A), the second sealing metal ring (12B) and the moisture-proof layer (15), thereby preventing the internal components of the chip (10) in the central layer portion from being oxidized or corroded by gas and liquid.
16. The chip sealing ring structure according to claim 15, characterized in that: The moisture-proof layer (15) is located in the isolation ring groove (132), and its bottom surface is connected to and covers the upper part or top of the second sealing metal ring (12B).
17. The chip sealing ring structure according to claim 15, characterized in that: The width of the isolation ring groove (132) is greater than or equal to the width of the second sealing metal ring (12B), so that the upper part or top of the second sealing metal ring (12B) is completely exposed in the isolation ring groove (132), and the first sealing metal ring (12A) is embedded in the insulating dielectric layer (13).
18. The chip sealing ring structure according to claim 15, characterized in that: The width of the isolation ring groove (132) is smaller than the width of the second sealing metal ring (12B), so that the upper part or the top part of the second sealing metal ring (12B) is exposed in the isolation ring groove (132), and the first sealing metal ring (12A) is embedded in the insulating medium layer (13).
19. The chip sealing ring structure according to claim 15, characterized in that: The first sealing metal ring (12A) and the second sealing metal ring (12B) each comprise at least one continuous metal ring structure, wherein the continuous metal ring structure is formed by stacking a barrier layer (122), a metal layer (121) and a plug portion (123), and the plug portion (123B) in the second sealing metal ring (12B) is formed integrally by extending downward from the metal layer (121B) in the second sealing metal ring (12B), and metal interconnection is achieved through the barrier layer (122B) in the second sealing metal ring (12B) and the metal layer (121A) in the first sealing metal ring (12A).
20. The chip sealing ring structure according to claim 19, characterized in that: The isolation ring groove (132) at least exposes the metal top surface of the continuous metal ring structure of the second sealing metal ring (12B).
21. The chip sealing ring structure according to claim 15, characterized in that: The material of the moisture-proof layer (15) comprises nitride or oxynitride, the material of the bottom protection layer (11) comprises silicon carbon nitride, and the material of the insulating dielectric layer (13) comprises oxide.
22. The chip sealing ring structure according to claim 15, characterized in that: Also includes: A top covering layer (16) is located on the moisture-proof layer (15).
23. A semiconductor chip, characterized in that: At least: The chip sealing ring structure according to any one of claims 15 to 22.
24. A semiconductor device structure, characterized in that: include: A wafer, comprising a plurality of chips (10) and a dicing road (20) between adjacent chips (10); wherein the chip (10) comprises at least the chip sealing ring structure according to any one of claims 15 to 22; and A pad metal layer pattern (17) is located in a peripheral area of the chip (10), and the pad metal layer pattern (17) is wrapped in the insulating dielectric layer (13); The insulating dielectric layer (13) further comprises a pad opening (171) located above the pad metal layer pattern (17); the pad opening (171) also penetrates the moisture-proof layer (15); and the portion of the pad metal layer pattern (17) exposed thereby serves as a chip pad, thereby exposing a pad area of the chip (10).