A low leakage GaN Schottky diode and its preparation method
By arranging a P-type GaN layer on the sidewalls and boss sidewalls of the GaN Schottky diode to form a depletion region, the reverse leakage current problem of the quasi-vertical GaN Schottky diode is solved and the effect of low leakage is achieved .
Patent Information
- Application Number
- CN202410674491.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-05-29
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2044-05-29
AI Technical Summary
Quasi-vertical structure GaN Schottky diodes have a large reverse leakage current problem, mainly due to leakage channels caused by conductive ions on the side walls.
A P-type GaN layer is provided on the sidewalls of the N-GaN layer and the sidewalls of the boss of the GaN Schottky diode to form a depletion region, ensuring that the P-type GaN layer does not contact the Schottky electrode and the ohmic electrode to prevent sidewall depletion. Leakage channel.
The reverse leakage current is effectively reduced, and a depletion region is formed in the sidewall area to ensure that the charge is in a balanced state, avoiding the flow of electrons, thereby preventing the formation of leakage channels.
Smart Images

Figure CN118248746B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of Schottky diodes, and in particular relates to a low leakage GaN Schottky diode and a preparation method thereof. Background Art
[0002] The characteristics of Si-based power electronic devices have approached the theoretical limit that Si materials can reach. The third-generation semiconductors represented by GaN have become the preferred materials for the next generation of semiconductor power devices. GaN has a large bandgap, high electron mobility, and low dielectric constant, which allows GaN power devices to be used in high-frequency and high-voltage applications. At the same time, GaN materials have very stable chemical properties and radiation resistance, and can work stably in more harsh environments.
[0003] Schottky diodes (SBDs) made of GaN materials have the characteristics of large current, high reverse withstand voltage, and low recovery time, and have become a hot spot in power device research. GaN SBD has lateral structure, quasi-vertical structure, and vertical structure. The lateral structure has the characteristics of large current and high withstand voltage, but due to the existence of surface states, the device has the problem of current collapse. The vertical structure does not have current collapse and has high withstand voltage, but the cost is very high, and the process technology is not easy to industrialize. The quasi-vertical structure GaN SBD has the advantages of low cost, small on-resistance, no current collapse, and easy industrialization, but the reverse leakage of the device is large. The reverse leakage of the quasi-vertical structure GaN SBD, part of it flows from the cathode to the anode through the heavily doped n-type GaN layer (N+GaN layer) and the lightly doped n-type GaN layer (N-GaN layer), and the other part flows from the cathode to the anode through the surface of N+GaN and N-GaN. Summary of the invention
[0004] The object of the present invention is to provide a low leakage GaN Schottky diode and a preparation method thereof. The low leakage GaN Schottky diode provided by the present invention can effectively block the leakage channel of the side wall, thereby effectively reducing the reverse leakage current.
[0005] In order to achieve the above object, the present invention provides the following technical solutions:
[0006] The present invention provides a low leakage GaN Schottky diode, comprising: a substrate; an N+GaN layer arranged on the upper surface of the substrate, the N+GaN layer consisting of a planar layer and a boss integrally arranged on the planar layer; an N-GaN layer covering the upper surface of the boss; a P-type GaN layer arranged on a partial upper surface of the N-GaN layer, a side wall of the N-GaN layer, a side wall of the boss, and a partial upper surface of the planar layer; a Schottky electrode arranged on the remaining upper surface of the N-GaN layer; an ohmic electrode arranged on the remaining upper surface of the planar layer; and the P-type GaN layer is not in contact with the Schottky electrode and the ohmic electrode.
[0007] Preferably, the gap between the P-type GaN layer and the Schottky electrode is ≥5 μm;
[0008] The gap between the P-type GaN layer and the ohmic electrode is ≥5 μm.
[0009] Preferably, the material of the P-type GaN layer is Mg-doped GaN, and the doping concentration of the Mg element in the Mg-doped GaN is greater than 1×10 18 cm -3 .
[0010] Preferably, the doping concentration of the N+GaN layer is greater than 1×10 19 cm -3 ; The thickness of the planar layer is 2~3μm and is not equal to 3μm; the thickness of the boss is ≤1μm.
[0011] Preferably, the doping concentration of the N-GaN layer is less than 1×10 19 cm -3 ; The thickness of the N-GaN layer is 5μm.
[0012] Preferably, the Schottky electrode comprises a contact layer and a metal layer arranged on the upper surface of the contact layer; the material of the contact layer of the Schottky electrode is Ni, with a thickness of 100 nm; the material of the metal layer of the Schottky electrode is Au, with a thickness of 1000 nm.
[0013] Preferably, the ohmic electrode includes a contact layer and a metal layer arranged on the upper surface of the contact layer; the material of the contact layer of the ohmic electrode is Ni, with a thickness of 20nm; the material of the metal layer of the ohmic electrode is Al, with a thickness of 1000nm.
[0014] Preferably, the substrate is a sapphire substrate.
[0015] The present invention provides a method for preparing the low leakage GaN Schottky diode described in the above technical solution, comprising the following steps:
[0016] Epitaxially growing an initial N+GaN layer and an initial N-GaN layer in sequence on the upper surface of the substrate; etching the initial N+GaN layer and the initial N-GaN layer according to the shape and structure of the N+GaN layer and the N-GaN layer to obtain the N+GaN layer and the N-GaN layer; preparing a hard mask template on a portion of the upper surface of the N-GaN layer and a portion of the upper surface of the planar layer, and then performing ion implantation on the remaining upper surface of the N-GaN layer, the side wall of the N-GaN layer, the side wall of the boss, and the remaining upper surface of the planar layer to obtain a first semi-finished product;
[0017] Annealing the first semi-finished product in a protective gas atmosphere to obtain a P-type GaN layer, thereby obtaining a second semi-finished product;
[0018] After removing the hard mask from the second semi-finished product, a Schottky electrode and an ohmic electrode are prepared to obtain the low leakage GaN Schottky diode.
[0019] Preferably, the annealing treatment is carried out at a temperature of 1250° C., for 30 min, at a pressure of normal pressure; and the protective gas is nitrogen.
[0020] The present invention provides a low leakage GaN Schottky diode (GaN SBD), comprising: a substrate; an N+GaN layer arranged on the upper surface of the substrate, the N+GaN layer consisting of a plane layer and a boss integrally arranged on the plane layer; an N-GaN layer covering the upper surface of the boss; a P-type GaN layer arranged on the upper surface of part of the N-GaN layer, the side wall of the N-GaN layer, the side wall of the boss, and the upper surface of part of the plane layer; a Schottky electrode arranged on the remaining upper surface of the N-GaN layer; an ohmic electrode arranged on the remaining upper surface of the plane layer; and the P-type GaN layer is not in contact with the Schottky electrode and the ohmic electrode. The present invention finds that due to the etching damage on the side wall of the N-GaN layer and the side wall of the boss, conductive ions will be generated on the side wall region, and some exogenous conductive ions will also adhere to the side wall. Due to the above conductive ions on the side wall, when the device is reversely voltageed (high voltage is applied to the ohmic electrode), a reverse leakage current will be formed. In the present invention, a P-type GaN layer is disposed on the side wall of the N-GaN layer and the side wall of the boss. Since the P-type GaN is in contact with the N-type GaN (N+GaN layer and N-GaN layer), a depletion region is formed. Figure 7As shown. In the depletion region, the charge is in a state of equilibrium, so the sidewall region of the GaN Schottky diode provided by the present invention will not form a leakage channel. At the same time, the present invention also arranges a P-type GaN layer on the upper surface of the N-GaN layer portion and the upper surface of the planar layer portion, and the P-type GaN layer is not in contact with the Schottky electrode and the ohmic electrode, which can well maintain the potential of the P-GaN layer (that is, when the GaN SBD is forward biased or negatively biased, the potential of the P-GaN layer does not change), and keeps the width of the depletion region from shrinking. In summary, the low-leakage GaN Schottky diode proposed by the present invention forms a depletion region in the sidewall region through structural improvement, and the depletion effect of the P-type GaN layer on the N-type GaN, and no electrons flow in the depletion region, thereby preventing the leakage channel on the side wall of the device and reducing the reverse leakage current of the device. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 A schematic diagram of the structure of a low leakage GaN Schottky diode provided by the present invention;
[0022] Figure 2 This is a schematic diagram of the structure of preparing an initial N+GaN layer and an initial N-GaN layer on the substrate surface in Example 1 of the present invention;
[0023] Figure 3 A schematic diagram of the structure of an N+GaN layer and an N-GaN layer obtained by etching according to an embodiment of the present invention;
[0024] Figure 4 This is a schematic diagram of the structure of preparing a hard mask template according to Example 1 of the present invention;
[0025] Figure 5 This is a schematic diagram of the structure of ion implantation in Example 1 of the present invention;
[0026] Figure 6 This is a schematic diagram of the structure of a P-type GaN layer obtained after annealing in Example 1 of the present invention;
[0027] Figure 7 A schematic diagram of the structure of a depletion region formed by the contact between a P-type GaN layer and an N-type GaN (N+GaN layer and N-GaN layer) obtained after annealing in Example 1 of the present invention;
[0028] In the figure: 1 is the substrate, 2 is the N+GaN layer, 3 is the N-GaN layer, 4 is the ohmic electrode, 5 is the Schottky electrode, 6 is the P-type GaN layer, 7 is the initial N+GaN layer, 8 is the initial N-GaN layer, 9 is the hard mask, and 10 is the depletion region. DETAILED DESCRIPTION
[0029] The present invention provides a low leakage GaN Schottky diode, comprising: a substrate; an N+GaN layer arranged on the upper surface of the substrate, the N+GaN layer consisting of a planar layer and a boss integrally arranged on the planar layer; an N-GaN layer covering the upper surface of the boss; a P-type GaN layer arranged on a partial upper surface of the N-GaN layer, a side wall of the N-GaN layer, a side wall of the boss, and a partial upper surface of the planar layer; a Schottky electrode arranged on the remaining upper surface of the N-GaN layer; an ohmic electrode arranged on the remaining upper surface of the planar layer; and the P-type GaN layer is not in contact with the Schottky electrode and the ohmic electrode.
[0030] In the present invention, unless otherwise specified, all preparation raw materials / components are commercially available products well known to those skilled in the art.
[0031] The low leakage GaN Schottky diode provided by the present invention comprises a substrate. In the present invention, the substrate is preferably a sapphire substrate.
[0032] The low leakage GaN Schottky diode provided by the present invention comprises an N+GaN layer disposed on the upper surface of the substrate, wherein the N+GaN layer is composed of a planar layer and a boss integrally disposed on the planar layer. In the present invention, the doping concentration of the N+GaN layer is preferably >1×10 19 cm -3 The boss is preferably located near the center of the N+GaN layer. The thickness of the boss is preferably ≤ the thickness of the planar layer. The thickness of the planar layer is preferably 2~3μm, and is not equal to 3μm, more preferably 2~2.8μm. The thickness of the boss is preferably ≤1μm, more preferably 200nm~1μm. The total thickness of the planar layer and the boss is preferably 3μm.
[0033] The low leakage GaN Schottky diode provided by the present invention comprises an N-GaN layer covering the upper surface of the boss. In the present invention, the doping concentration of the N-GaN layer is preferably <1×10 19 cm -3 ; The thickness of the N-GaN layer is preferably 5μm.
[0034] The low leakage GaN Schottky diode provided by the present invention comprises a P-type GaN layer arranged on the upper surface of the N-GaN layer, the side wall of the N-GaN layer, the side wall of the boss, and the upper surface of the planar layer. In the present invention, the P-type GaN layer is continuous. The material of the P-type GaN layer is preferably Mg-doped GaN, and the doping concentration of the Mg element in the Mg-doped GaN is preferably >1×10 18 cm -3 .
[0035] The low leakage GaN Schottky diode provided by the present invention comprises a Schottky electrode arranged on the remaining upper surface of the N-GaN layer. In the present invention, the Schottky electrode preferably comprises a contact layer and a metal layer arranged on the upper surface of the contact layer; the material of the contact layer of the Schottky electrode is preferably Ni, and the thickness is preferably 100nm; the material of the metal layer of the Schottky electrode is preferably Au, and the thickness is preferably 1000nm.
[0036] The low leakage GaN Schottky diode provided by the present invention comprises an ohmic electrode arranged on the remaining upper surface of the planar layer. In the present invention, the ohmic electrode preferably comprises a contact layer and a metal layer arranged on the upper surface of the contact layer; the material of the contact layer of the ohmic electrode is preferably Ni, and the thickness is preferably 20nm; the material of the metal layer of the ohmic electrode is preferably Al, and the thickness is preferably 1000nm.
[0037] In the low leakage GaN Schottky diode provided by the present invention, the P-type GaN layer is not in contact with the Schottky electrode and the ohmic electrode. In the present invention, the gap between the P-type GaN layer and the Schottky electrode is preferably ≥5 μm. The gap between the P-type GaN layer and the ohmic electrode is preferably ≥5 μm.
[0038] The present invention provides a method for preparing the low leakage GaN Schottky diode described in the above technical solution, comprising the following steps:
[0039] Epitaxially growing an initial N+GaN layer and an initial N-GaN layer in sequence on the upper surface of the substrate; etching the initial N+GaN layer and the initial N-GaN layer according to the shape and structure of the N+GaN layer and the N-GaN layer to obtain the N+GaN layer and the N-GaN layer; preparing a hard mask template on a portion of the upper surface of the N-GaN layer and a portion of the upper surface of the planar layer, and then performing ion implantation on the remaining upper surface of the N-GaN layer, the side wall of the N-GaN layer, the side wall of the boss, and the remaining upper surface of the planar layer to obtain a first semi-finished product;
[0040] Annealing the first semi-finished product in a protective gas atmosphere to obtain a P-type GaN layer, thereby obtaining a second semi-finished product;
[0041] After removing the hard mask from the second semi-finished product, a Schottky electrode and an ohmic electrode are prepared to obtain the low leakage GaN Schottky diode.
[0042] The present invention sequentially epitaxially grows an initial N+GaN layer and an initial N-GaN layer on the upper surface of the substrate; etches the initial N+GaN layer and the initial N-GaN layer according to their shapes and structures to obtain the N+GaN layer and the N-GaN layer; prepares a hard mask template on a portion of the upper surface of the N-GaN layer and a portion of the upper surface of the planar layer, and then performs ion implantation on the remaining upper surface of the N-GaN layer, the sidewall of the N-GaN layer, the sidewall of the boss, and the remaining upper surface of the planar layer to obtain a first semi-finished product. In the present invention, the epitaxial growth is preferably carried out in an MOCVD device, and the present invention has no special requirements for the specific implementation of the epitaxial growth. In the present invention, the thickness of the initial N+GaN layer is preferably 3μm. The thickness of the initial N-GaN layer is preferably 5μm. The present invention preferably etches the initial N-GaN layer and the initial N+GaN layer in sequence, and when etching the initial N-GaN layer, until the initial N+GaN layer underneath is exposed; then the initial N+GaN is continuously etched. The present invention has no special requirements for the etching method of the initial N+GaN layer and the initial N-GaN layer. The hard mask is preferably SiO2. The ion implantation is preferably Mg ion implantation. The energy of the Mg ion implantation is preferably 360Kev. The present invention has no special requirements for the specific implementation of the ion implantation.
[0043] After obtaining the first semi-finished product, the present invention anneals the first semi-finished product in a protective gas atmosphere to obtain a P-type GaN layer, thereby obtaining a second semi-finished product. In the present invention, the temperature of the annealing treatment is preferably 1250°C, the time is preferably 30 minutes, and the pressure is preferably normal pressure; the protective gas is preferably nitrogen. In the present invention, the annealing of the annealing treatment has the following effects: one is to repair the material damage caused during the injection process, and the other is that because the activation energy of Mg in GaN is large, high-temperature annealing is required to activate Mg to form P-type GaN.
[0044] After obtaining the second semi-finished product, the present invention removes the hard mask from the second semi-finished product to prepare a Schottky electrode and an ohmic electrode to obtain the low leakage GaN Schottky diode. The present invention has no special requirements for the preparation method of the Schottky electrode and the ohmic electrode.
[0045] In order to further illustrate the present invention, the technical solutions provided by the present invention are described in detail below in conjunction with embodiments, but they should not be construed as limiting the protection scope of the present invention.
[0046] Example 1
[0047] Step 1: Place the substrate 1 into the MOCVD device, wherein the substrate 1 is sapphire, and sequentially epitaxially grow the initial N+GaN layer 7 and the initial N-GaN layer 8 (such as Figure 2 As shown). The initial N-GaN layer 8 is a lightly doped n-type GaN layer with a thickness of 5 μm and a doping concentration of less than 1×10 18 / cm 3 The initial N+GaN layer 7 is a heavily doped n-type GaN layer with a thickness of 3 μm and a doping concentration greater than 1×10 19 / cm 3 .
[0048] Step 2: Etching the initial N-GaN layer 8 until the initial N+GaN layer 7 underneath is exposed to obtain the N-GaN layer 3; continuing to etch the initial N+GaN layer 7, etching the initial N+GaN layer 7 downward by 1 μm using the N-GaN layer 3 as a template to obtain a boss structure with a thickness of 1 μm, thereby obtaining the N+GaN layer 2 (such as Figure 3 As shown). During the etching process, the obtained N-GaN layer 3 and the sidewalls of the 1μm thick platform structure will be damaged by etching, thereby generating conductive ions on the sidewalls, and during the wafer fabrication process, some contamination or conductive ions will also adhere to the sidewalls. Due to the presence of these conductive ions, when the reverse voltage of the device is applied (high voltage is applied to the ohmic electrode), a reverse leakage current will be formed.
[0049] Step 3: SiO2 is prepared as a hard mask 9 on the upper surface of part of the N-GaN layer 3 and the upper surface of part of the planar layer, and then ion implantation is performed on the remaining upper surface of the N-GaN layer 3, the side wall of the N-GaN layer 3, the side wall of the boss, and the remaining upper surface of the planar layer (the energy of the ion implantation is 360 KeV, and the total Mg ion concentration is greater than 1×10 18 / cm 3 ),like Figure 5 As shown. Then, annealing treatment was performed for 30 minutes at normal pressure, 1250°C, and nitrogen atmosphere. The purpose of annealing is twofold. One is to repair the material damage caused by the implantation process. The other is that because the activation energy of Mg in GaN is large, high-temperature annealing is required to activate Mg to form P-type GaN.
[0050] Step 4: After annealing, remove the SiO2 hard mask 9 to form Figure 6 The structure shown. Figure 6 In the injected area, P-type GaN is formed. Since P-type GaN contacts N-type GaN, a depletion region is formed, such as Figure 7 In the depletion region, the charges are in equilibrium, so no leakage channel will form in the sidewall region.
[0051] Step 5: Finally, Schottky electrodes (Ni / Au 100nm / 1000nm) and ohmic electrodes (Ti / Al20nm / 1000nm) are made respectively. During the production process, neither the Schottky electrode nor the ohmic electrode is connected to the injection region, and a certain distance (>5μm) is maintained. The purpose of this is to maintain the potential of the P-GaN layer (that is, when the GaN SBD is forward biased or negatively biased, the potential of the P-GaN layer does not change) and keep the width of the depletion region from shrinking.
[0052] It can be seen from the above embodiments that the present invention provides a method for preparing a low-leakage GaN Schottky diode: First, an initial N+GaN layer and an initial N-GaN layer are grown in sequence on a sapphire substrate. Then the initial N+GaN layer and the initial N-GaN layer are etched. Next, Mg ions are implanted into the side walls and part of the surface of the N-GaN, as well as the side walls of the bosses and part of the surface of the planar layer of the N+GaN. After the implantation is completed, high-temperature annealing is performed to form a depletion region. Finally, Schottky electrodes and ohmic electrodes are made. The Schottky electrodes and ohmic electrodes should not be connected to the implanted area and should be kept at a certain distance. The low leakage GaN Schottky diode provided by the present invention performs Mg ion implantation on the upper surface of the N-GaN layer portion, the side wall of the N-GaN layer, the side wall of the boss, and the upper surface area of the planar layer portion, and then performs high-temperature annealing to convert the implanted layer into P-GaN, and utilizes the depletion effect of P-type GaN on N-type GaN to form a depletion region in the side wall region, in which no electrons flow, thereby preventing the leakage channel of the side wall and reducing the reverse leakage current.
[0053] Although the above embodiment describes the present invention in detail, it is only a part of the embodiments of the present invention, not all of the embodiments. Other embodiments can be obtained based on this embodiment without creativity, and these embodiments all fall within the protection scope of the present invention.
Claims
1. A low leakage GaN Schottky diode, It is characterized in that include: substrate; An N+GaN layer is arranged on the upper surface of the substrate, and the N+GaN layer is composed of a planar layer and a boss integrally arranged on the planar layer; an N-GaN layer covering the upper surface of the boss; a P-type GaN layer is arranged on the upper surface of part of the N-GaN layer, the side wall of the N-GaN layer, the side wall of the boss, and the upper surface of part of the planar layer; a Schottky electrode is arranged on the remaining upper surface of the N-GaN layer; an ohmic electrode is arranged on the remaining upper surface of the planar layer; and the P-type GaN layer is not in contact with the Schottky electrode and the ohmic electrode; the gap between the P-type GaN layer and the Schottky electrode is ≥5μm; the gap between the P-type GaN layer and the ohmic electrode is ≥5μm; the material of the P-type GaN layer is Mg-doped GaN, and the doping concentration of the Mg element in the Mg-doped GaN is greater than 1×10 18 cm -3 ; The method for preparing the low leakage GaN Schottky diode comprises the following steps: Epitaxially growing an initial N+GaN layer and an initial N-GaN layer in sequence on the upper surface of the substrate; etching the initial N+GaN layer and the initial N-GaN layer according to the shape and structure of the N+GaN layer and the N-GaN layer to obtain the N+GaN layer and the N-GaN layer; preparing a hard mask template on a portion of the upper surface of the N-GaN layer and a portion of the upper surface of the planar layer, and then performing ion implantation on the remaining upper surface of the N-GaN layer, the side wall of the N-GaN layer, the side wall of the boss, and the remaining upper surface of the planar layer to obtain a first semi-finished product; Annealing the first semi-finished product in a protective gas atmosphere to obtain a P-type GaN layer, thereby obtaining a second semi-finished product; After removing the hard mask from the second semi-finished product, a Schottky electrode and an ohmic electrode are prepared to obtain the low leakage GaN Schottky diode.
2. The low leakage GaN Schottky diode according to claim 1, It is characterized in that The doping concentration of the N+GaN layer is greater than 1×10 19 cm -3 ; The thickness of the planar layer is 2~3μm and is not equal to 3μm; the thickness of the boss is ≤1μm.
3. The low leakage GaN Schottky diode according to claim 1, It is characterized in that The doping concentration of the N-GaN layer is less than 1×10 19 cm -3 ; The thickness of the N-GaN layer is 5μm.
4. The low leakage GaN Schottky diode according to claim 1, It is characterized in that The Schottky electrode comprises a contact layer and a metal layer arranged on the upper surface of the contact layer; the material of the contact layer of the Schottky electrode is Ni, with a thickness of 100 nm; the material of the metal layer of the Schottky electrode is Au, with a thickness of 1000 nm.
5. The low leakage GaN Schottky diode according to claim 1, It is characterized in that The ohmic electrode includes a contact layer and a metal layer arranged on the upper surface of the contact layer; the material of the contact layer of the ohmic electrode is Ni, with a thickness of 20nm; the material of the metal layer of the ohmic electrode is Al, with a thickness of 1000nm.
6. The low leakage GaN Schottky diode according to claim 1, It is characterized in that The substrate is a sapphire substrate.
7. A method for preparing a low leakage GaN Schottky diode according to any one of claims 1 to 6, It is characterized in that The following steps are involved: Epitaxially growing an initial N+GaN layer and an initial N-GaN layer in sequence on the upper surface of the substrate; etching the initial N+GaN layer and the initial N-GaN layer according to the shape and structure of the N+GaN layer and the N-GaN layer to obtain the N+GaN layer and the N-GaN layer; preparing a hard mask template on a portion of the upper surface of the N-GaN layer and a portion of the upper surface of the planar layer, and then performing ion implantation on the remaining upper surface of the N-GaN layer, the side wall of the N-GaN layer, the side wall of the boss, and the remaining upper surface of the planar layer to obtain a first semi-finished product; Annealing the first semi-finished product in a protective gas atmosphere to obtain a P-type GaN layer, thereby obtaining a second semi-finished product; After removing the hard mask from the second semi-finished product, a Schottky electrode and an ohmic electrode are prepared to obtain the low leakage GaN Schottky diode.
8. The preparation method according to claim 7, It is characterized in that The annealing treatment was performed at a temperature of 1250° C., for 30 minutes, at a pressure of normal pressure; and the protective gas was nitrogen.
Citation Information
Patent Citations
SBD structure and manufacturing method thereof
CN110190115A
PN junction base coupled gallium nitride Schottky diode and production method thereof
CN113964181A
Quasi-vertical structure GaN Schottky barrier diode and preparation method thereof
CN115763247A
Low-damage gallium nitride Schottky diode and preparation method thereof
CN116387152A
Schottky barrier diode and method for manufacturing schottky barrier diode
US20150069412A1