Conductive microneedle patch and preparation method and application thereof
Through the design of conductive microneedle patches, the use of microneedle arrays and conductive microwires of PVA, botulinum toxin type A, graphene and silver nanoparticles, combined with electrical stimulation, solved the adverse penetration reactions of BTX-A in the treatment of blepharospasm. , pain and high frequency of repeated injections, it achieves precise positioning and slow release of drugs, improving treatment effects and patient comfort.
Patent Information
- Application Number
- CN202411016826.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-26
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2044-07-26
AI Technical Summary
The existing BTX-A treatment method for blepharospasm has problems such as drug penetration into surrounding muscles, causing adverse reactions, patient pain, high frequency of repeated injections, and difficulty in injection.
It uses a conductive microneedle patch, which contains PVA, botulinum toxin type A, graphene and silver nanoparticles. It achieves precise positioning and slow release of drugs through microneedle arrays and conductive microwires, and combines electrical stimulation to improve bioavailability and sustainability. time.
It reduces adverse reactions caused by drug penetration into peripheral muscles, reduces the patient's pain, prolongs the treatment effect, simplifies the treatment process, reduces the frequency of repeated treatments, and improves the patient's comfort and treatment effect.
Smart Images

Figure CN118543024B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of biomedical materials, and in particular to a conductive microneedle patch and a preparation method and application thereof. Background Art
[0002] Blepharospasm (BSP) is a focal dystonia characterized by involuntary closure and difficulty in opening the eyelids, usually caused by spasms of the orbicularis oculi muscle. The incidence of this disease varies from region to region, ranging from 20 to 133 cases per 1 million people. It is particularly common in women aged 50 to 70, with a male to female ratio of approximately 1:2.3. The early symptoms of BSP are often mild, and may only manifest as frequent blinking or frequent urges to close the eyes. The disease generally progresses slowly. In the late stage, persistent blepharospasm may even lead to functional blindness. Compared with other types of focal dystonia, BSP is more likely to spread to adjacent areas, and more than 50% of patients may develop dystonia in other parts within 5 years of onset.
[0003] Local injection of botulinum toxin type A (BTX-A) is the preferred method for treating focal dystonia, including BSP. Botulinum toxin can selectively act on peripheral cholinergic neuron terminals, inhibiting the release of acetylcholine to cause transient paralysis of the muscles at the injection site. The effect of BTX-A generally begins to appear 2 to 7 days after injection, and its efficacy can last for 3 to 4 months. About 90% of patients can achieve moderate or above symptom improvement after treatment.
[0004] However, the use of BTX-A in the prior art to treat BSP has the following drawbacks:
[0005] (1) Point injection (such as Figure 1 As shown in Figure 2, point injection relies on drug penetration into the orbicularis oculi muscle (e.g. Figure 2 As shown in Figure 2), point injections usually take a long time to take effect and are easy to penetrate into the surrounding muscles and cause adverse reactions, such as ptosis.
[0006] (2) Subcutaneous injection, which usually causes pain to the patient;
[0007] (3) Most patients require repeated injections to maintain efficacy, but currently, there is no randomized controlled study to provide the optimal treatment interval and dose of BTX-A;
[0008] (4) The injection is difficult and requires high technical skills; only some qualified hospitals can complete it. Summary of the invention
[0009] In view of the above analysis, the present invention aims to provide a conductive microneedle patch and a preparation method and application thereof, so as to solve at least one of the following existing problems: reducing the adverse reactions caused by the penetration of drugs into the muscles surrounding the orbicularis oculi muscle, reducing the pain of patients, and reducing the frequency of repeated treatments.
[0010] The purpose of the present invention is mainly achieved through the following technical solutions:
[0011] In a first aspect, the present invention provides a conductive microneedle patch, comprising a microneedle array and a conductive substrate layer, wherein the microneedle array is arranged on the conductive substrate layer, the microneedle array comprises microneedles and conductive microfilaments, the materials of the microneedles comprise PVA, botulinum toxin type A, graphene and silver nanoparticles; based on the total weight of the microneedles, the mass percentage of PVA is 97-99%; the mass percentage of botulinum toxin type A is 0.5-2%; the mass percentage of graphene is 0.1-1%; the mass percentage of silver nanoparticles is 0.1-1%; the conductive microfilaments are arranged inside the microneedles, and the conductive microfilaments extend from the needle tips of the microneedles to the conductive substrate layer; wherein the conductive microfilaments and the conductive substrate layer are made by curing a PEDOT / PSS aqueous solution, and the mass concentration of PEDOT / PSS in the PEDOT / PSS aqueous solution is 3-5%.
[0012] As a specific embodiment of the present invention, the diameter of the conductive microwire is 4-6 microns.
[0013] As a specific embodiment of the present invention, the microneedle is conical, and the diameter of the cone bottom is 40-60 microns.
[0014] As a specific embodiment of the present invention, the length of the microneedle is 300-500 microns.
[0015] As a specific embodiment of the present invention, the thickness of the conductive base layer is 4-6 microns.
[0016] As a specific embodiment of the present invention, the distance between the centers of the conical bottom surfaces of adjacent microneedles is 0.4-0.6 mm.
[0017] As a specific embodiment of the present invention, the microneedle patch further includes a collagen base layer, which is arranged below the conductive base layer, and the thickness of the collagen base layer is 100-200 microns.
[0018] In a second aspect, the present invention provides a method for preparing the conductive microneedle patch, comprising the following steps:
[0019] S1: preparing a negative mold of the microneedle patch, wherein the negative mold is made of Ecoflex silicone and comprises a base layer negative mold and a microneedle array negative mold;
[0020] S2: adding liquid PVA containing botulinum toxin type A, graphene and silver nanoparticles into the negative mold of the microneedle array, and then heating to form a microneedle array without a substrate layer, and reserving a channel inside each microneedle during the heating process, wherein the diameter of the channel is 4-6 microns;
[0021] S3: After the heating is completed, a PEDOT / PSS aqueous solution is added dropwise into the channel, and ultrasonic vibration is performed to heat and solidify the channel to form conductive microwires and a conductive base layer.
[0022] As a specific implementation of the present invention, S1 includes the following steps:
[0023] S1-1: preparing a mold of the negative mold, and irradiating and heating the mold with ultraviolet light;
[0024] S1-2: placing the mold obtained in step S1-1 into an aqueous solution containing a surfactant, then taking it out and blowing it dry;
[0025] S1-3: Pour liquid Ecoflex into the mold obtained in S1-2, then apply vacuum and heat to form a negative mold of the microneedle patch.
[0026] As a specific embodiment of the present invention, in S1-1, the mold is irradiated with ultraviolet light for 1-3 hours and heated to 100-150° C. for 1-3 hours.
[0027] As a specific embodiment of the present invention, in S1-2, the surfactant is an alkyl sulfonate, and the mass concentration of the surfactant is 1%-2%.
[0028] As a specific embodiment of the present invention, in S1-3, the conditions of applying vacuum and heating include: applying vacuum for 10-15 minutes and heating at 80-85°C for 1-2 hours.
[0029] As a specific embodiment of the present invention, the method further includes step S4: preparing a collagen base layer using a collagen solution.
[0030] As a specific embodiment of the present invention, in S2, heating is performed at 35-40° C. for 1-2 hours to form a microneedle array without a substrate layer.
[0031] As a specific embodiment of the present invention, in S3, the temperature of heating and curing is 30-40°C, preferably 30-35°C.
[0032] In a third aspect, the present invention provides a use of the conductive microneedle patch in the preparation of a drug for treating blepharospasm.
[0033] Compared with the prior art, the present invention can achieve at least one of the following beneficial effects:
[0034] A) The soluble conductive microneedle patch provided by the present invention contains botulinum toxin type A in the microneedle array of the microneedle patch. The microneedle patch can be attached to the orbicularis oculi muscle to achieve precise positioning of the drug, optimize drug delivery, and reduce side effects. The microneedles can directly reach the dermis to ensure the effective release of the drug and enhance the therapeutic effect. The microneedle patch can achieve slow drug release and reduce stimulation to the skin nerves, thereby improving the patient's comfort. The microneedle patch of the present invention combined with electrical stimulation can improve the bioavailability and duration of the drug, reduce the frequency of repeated treatments, and reduce the overall treatment burden on patients.
[0035] B) The soluble conductive microneedle patch provided by the present invention has a conductive structure made of PEDOT / PSS material in the center of the microneedle. PEDOT / PSS material is selected for its excellent biocompatibility and conductivity, and can form a stable potential difference after electrical stimulation. Under the action of electrical stimulation, the PEDOT / PSS conductive structure forms a stable potential difference at the tip of the microneedle, and this potential difference stimulates the cell tissue around the microneedle. BRIEF DESCRIPTION OF THE DRAWINGS
[0036] Figure 1 It is the orbicularis oculi muscle surface injection site for point injection in the prior art.
[0037] Figure 2 It is the range of the orbicularis oculi muscle of the human body.
[0038] Figure 3 This is a schematic structural diagram of the conductive microneedle patch provided by the present invention.
[0039] Figure 4 This is a micrograph of the conductive microneedle patch prepared in Example 1 provided by the present invention.
[0040] Figure 5 This is a microscopic photograph of the microneedles and conductive microwires of the conductive microneedle patch prepared in Example 1 provided by the present invention. DETAILED DESCRIPTION
[0041] Preferred embodiments of the present invention will be described in detail below in conjunction with the accompanying drawings, wherein the accompanying drawings constitute a part of the present invention and are used to explain the principles of the present invention together with the embodiments of the present invention.
[0042] First, as Figure 3As shown, the present invention provides a soluble conductive microneedle patch, comprising a microneedle array 10 and a conductive substrate layer 20, wherein the microneedle array 10 is arranged on the conductive substrate layer 20, wherein the microneedle array 10 comprises a plurality of microneedles 11 and conductive microwires 12, the materials of the microneedles 11 comprise PVA, botulinum toxin type A, graphene and silver nanoparticles; the conductive microwires 12 are arranged inside the microneedles 11, and the conductive microwires 12 extend from the needle tips of the microneedles 11 to the conductive substrate layer 20, the conductive microwires 12 and the conductive substrate layer 20 are made by curing a PEDOT / PSS aqueous solution, and the mass concentration of PEDOT / PSS in the PEDOT / PSS aqueous solution is 3-5%.
[0043] It should be noted that the soluble conductive microneedle patch provided by the present invention contains botulinum toxin type A in the microneedle array of the microneedle patch. The microneedle patch can be fitted with the orbicularis oculi muscle to achieve precise positioning of the drug, optimize drug delivery, and reduce side effects. The microneedles can directly reach the dermis to ensure the effective release of the drug and enhance the therapeutic effect. The microneedle patch can achieve slow drug release and reduce stimulation to the skin nerves, thereby improving the patient's comfort. The microneedle patch of the present invention combined with electrical stimulation can improve the bioavailability and duration of the drug, reduce the frequency of repeated treatments, and reduce the overall treatment burden on patients.
[0044] It should be noted that the center of the microneedle uses an organic guide wire made by curing a PEDOT / PSS aqueous solution, and PEDOT / PSS is a composite material of PEDOT (poly 3,4-ethylenedioxythiophene) and PSS (sodium polystyrene sulfonate). This design can form a stable potential difference along the entire length of the microneedle after electrical stimulation. This electrical stimulation can more effectively activate the voltage-gated channels of the surrounding tissue cells, allowing botulinum toxin to act more effectively on the tissues around the microneedle, thereby enhancing the treatment effect, prolonging the duration of action, and reducing the frequency of repeated treatments.
[0045] As a specific embodiment of the present invention, the diameter of the conductive microwire 12 is 4-6 microns, such as 4.5, 5, 5.5 microns, etc., preferably 5 microns.
[0046] It should be noted that the diameter of the conductive microwire 12 is 4-6 microns. On the one hand, it is necessary to ensure a sufficiently low impedance, and at the same time, it cannot be too thick to reduce the drug loading of the microneedle, ensuring that the impedance of a single conductive microwire is less than 10k ohms, so that the conductive microwire has the ability to conduct electricity.
[0047] It should be noted that the mass concentration of PEDOT / PSS in the PEDOT / PSS aqueous solution is 3-5%. On the one hand, conductivity must be ensured, and on the other hand, too high a content will affect the solubility of the microneedles in the patient's body.
[0048] As a specific embodiment of the present invention, the material of the microneedle 11 is, based on the total weight of the microneedle 11,
[0049] The mass percentage of PVA is 97-99%, preferably 98%;
[0050] The mass percentage of botulinum toxin type A is 0.5-2%, preferably 1%;
[0051] The mass percentage of graphene is 0.1-1%, preferably 0.5%;
[0052] The mass percentage of the silver nanoparticles is 0.1-1%, preferably 0.5%.
[0053] It should be noted that the graphene and silver nanoparticles in the microneedles act as conductors and can be metabolized by the body. The particle size of the silver nanoparticles ranges from 30nm to 60nm.
[0054] As a specific embodiment of the present invention, the thickness of the conductive base layer is 4-6 microns.
[0055] As a specific embodiment of the present invention, the microneedle 11 is conical, the diameter of the cone bottom of the microneedle 11 is 40-60 microns, preferably 50 microns, the spacing between the centers of the cone bottoms of adjacent microneedles 11 is 0.4-0.6 mm, preferably 0.5 mm; the length of the microneedle 11 is 300-500 microns.
[0056] As a specific embodiment of the present invention, the soluble conductive microneedle patch further includes a collagen base layer 30 disposed below the conductive base layer 20, and the thickness of the collagen base layer 30 is 100-200 microns.
[0057] It should be noted that the conductive microwire 12 can be flush with the needle tip of the microneedle 11 or can protrude from the needle tip of the microneedle, but the protrusion cannot be too long and the protrusion length does not exceed 1 micron.
[0058] As a specific embodiment of the present invention, the shapes of the conductive base layer 20 and the collagen base layer 30 are set according to the contour of the orbicularis oculi muscle.
[0059] It should be noted that the conductive microneedle patch provided by the present invention has the following beneficial effects:
[0060] (1) Precise control of the location and distribution of botulinum toxin injection: Traditional injection methods make it difficult to precisely control the distribution of drugs in specific skin areas, which may lead to uneven efficacy or unnecessary side effects. The present invention achieves precise positioning by designing a microneedle arrangement that conforms to the contour of the orbicularis oculi muscle, thereby optimizing drug delivery and reducing side effects.
[0061] (2) Enhance the penetration of botulinum toxin deep into the skin: Traditional epidermal applications make it difficult to ensure that the drug effectively penetrates into the dermis. The soluble microneedle technology of the present invention can directly reach the dermis, ensuring the effective release of the drug and enhancing the therapeutic effect.
[0062] (3) Reduce pain and discomfort during treatment: Traditional injections may cause pain and skin irritation. The present invention reduces stimulation to the skin nerves through the slow release of drugs through microneedles, thereby improving the patient's comfort.
[0063] (4) Simplify the treatment process and improve patient compliance: Traditional treatment methods may be complicated and affect patient compliance. The skin patch-type microneedle design of the present invention is simple and easy to use, which is convenient for patients to use by themselves, improving the convenience of treatment and patient acceptance.
[0064] (5) Prolong drug efficacy and reduce the need for repeated treatment: Traditional treatments require frequent repetitions, which increases the burden on patients. The present invention, combined with electrical stimulation, can improve the bioavailability and duration of drugs, reduce the frequency of repeated treatments, and reduce the overall treatment burden on patients.
[0065] In a second aspect, the present invention provides a method for preparing a soluble conductive microneedle patch, comprising the following steps:
[0066] S1: preparing a negative mold of a microneedle patch, wherein the negative mold is made of Ecoflex silicone and comprises a base layer negative mold and a microneedle array negative mold;
[0067] S2: Liquid polyvinyl acetate (PVA) containing botulinum toxin type A, graphene and silver nanoparticles is dripped into the negative mold of the microneedle array, and the liquid PVA is filled into the negative mold of the microneedle array by vacuum method, the surface of the negative mold is scraped off, and then heated to form a microneedle array without a substrate layer. During the heating process, a channel with a diameter of 4-6 microns is reserved inside each microneedle by using a wire drawing method, and the channel extends from the root of the microneedle to the tip of the microneedle;
[0068] S3: After heating, a PEDOT (poly 3,4-ethylenedioxythiophene) / PSS (sodium polystyrene sulfonate) aqueous solution is added dropwise into the channel of the microneedle, wherein the mass concentration of PEDOT / PSS is 3%-5%, and ultrasonically vibrated and heated to solidify to form conductive microwires and a conductive base layer.
[0069] As a specific embodiment of the present invention, it also includes step S4: using a synthetic type I collagen solution to prepare a collagen basal layer.
[0070] It should be noted that the use of the collagen base layer not only provides the necessary support structure for the microneedle patch, but also ensures the softness and adaptability of the overall structure, enhancing the comfort of patients when using it.
[0071] As a specific implementation of the present invention, step S1 includes the following steps:
[0072] S1-1: using a resin to prepare a negative mold, irradiating the mold with ultraviolet light and heating it;
[0073] S1-2: placing the mold obtained in step S1-1 into an aqueous solution containing a surfactant, then taking it out and blowing it dry;
[0074] S1-3: Pour liquid Ecoflex silicone into the resin mold obtained in S1-2, then apply vacuum and heat, and slowly peel off to form a negative mold of the microneedle patch.
[0075] As a specific embodiment of the present invention, in S1-1, a 3D printing method can be used to prepare a mold using 3D printing materials. It should be noted that the present invention has no limitation on the type of resin of the 3D printing material, and it can be a commercially available resin material.
[0076] As a specific embodiment of the present invention, in S1-1, the mold can be irradiated with ultraviolet light for 1-3 hours and heated to 100-150°C for 1-3 hours. Preferably, the ultraviolet irradiation time can be 1.5, 2, or 2.5 hours, the heating temperature can be 110, 120, 130, or 140°C, and the heating treatment time can be 1.5, 2, or 2.5 hours.
[0077] It should be noted that in S1-1, on the one hand, irradiating the resin with ultraviolet light and heating it can effectively prevent the resin from hindering the curing of the Ecoflex negative mold. Specifically, the chemical composition of the resin is different from that of the Ecoflex silicone, and the chemical properties of the two materials conflict. The resin may cause the Ecoflex negative mold to be incompletely cured or produce poor physical properties. In this case, it is important to ensure that the resin is fully cured and compatible with the Ecoflex material. To achieve complete curing of the resin, the resin (3D printing material) needs to be irradiated with ultraviolet light and heated. On the other hand, irradiating the resin mold with ultraviolet light can further cure the resin and improve the mechanical strength and stability of the resin. Heating treatment (commonly referred to as thermal post-treatment or annealing) can improve the physical properties of the resin, such as improving thermal stability, reducing internal stress, and improving resistance to chemical substances, which is convenient for subsequent demolding of the Ecoflex negative mold.
[0078] As a specific embodiment of the present invention, in S1-2, the mass concentration of the surfactant in water can be 1%-2%, the surfactant can be an alkyl sulfonate, preferably sodium dodecyl sulfate (SDS), and the mold can be placed in the surfactant solution for about 30 minutes. It should be noted that in S1-2, the mold is placed in the surfactant, and the surfactant will be adsorbed on the mold surface, which can reduce the adhesion between the mold and the Ecoflex negative mold.
[0079] As a specific embodiment of the present invention, the conditions for applying vacuum and heating in S1-3 include: applying vacuum for about 10-15 minutes, and heating at 80-85° C. for 1-2 hours to complete curing.
[0080] It should be noted that in S1, polydimethylsiloxane (PDMS) is usually used as the negative mold in the prior art, but due to the large Young's modulus and small tensile limit of PDMS, it is more suitable for the improved dual-mold manufacturing of conical truncated cone-shaped microneedles but not for barbed microneedles. In contrast, the Young's modulus and tensile limit of Ecoflex are more suitable than PDMS, and it also has a certain temperature resistance. When the base thickness of the negative mold is controlled at about 3mm, the Young's modulus and extensibility can be well balanced. Experiments have found that the success rate of using Ecoflex negative molds is much higher than that of PDMS, making it easier to separate Ecoflex negative molds and PVA soluble microneedles. Ecoflex, also known as PBAT, is a copolymer of butylene adipate and butylene terephthalate. Ecoflex is an elastic silicone commonly used in biomedical materials with excellent biocompatibility and mechanical properties.
[0081] As a specific embodiment of the present invention, in S2, heating is performed at 35-40°C for 1-2 hours to form a substrate-free microneedle array. It should be noted that too high a heating temperature may cause the inactivation of botulinum toxin, so the temperature is controlled to be 35-40°C.
[0082] As a specific embodiment of the present invention, in S2, a channel is formed by using a traditional wire drawing process. When the microneedles are not completely solidified, a metal filament with a diameter of 4-6 microns is inserted into the center of each microneedle. After the microneedles are completely solidified, the metal filament is pulled out to form a channel.
[0083] It should be noted that in microneedle technology, especially when designing a composite structure containing soluble microneedles and a conductive matrix (such as PEDOT), the manufacturing order is usually based on the characteristics of the materials and the functional requirements of the final product. In this application, microneedles are first made, and channels are reserved for adding conductive microwires. On the one hand, soluble microneedles may require precise dimensions during manufacturing to ensure that they can properly dissolve and release drugs when used. Making these microneedles first can ensure that they have the required physical and chemical properties. On the other hand, in terms of preparation difficulty, the PEDOT conductive material PEDOT / PSS used is usually in the form of an aqueous solution. If the conductive material is prepared first, its rigidity at the micron level is difficult to guarantee, which greatly increases the difficulty of preparation. At the same time, preparing the conductive microwires first can easily cause the microneedles to break in subsequent operations or fail to ensure that the conductive microwires can extend to the needle tip.
[0084] It should be noted that in S3, ultrasonic oscillation technology is used during the addition process to ensure that the PEDOT / PSS aqueous solution evenly and fully fills the channels in the microneedles. This step is crucial to ensure the uniform distribution and effective conductivity of PEDOT / PSS in the microneedles.
[0085] As a specific embodiment of the present invention, in S3, the temperature of heating and curing is 30-40°C, preferably 30-35°C.
[0086] It should be noted that PEDOT is a high-quality organic conductive material that stands out for its excellent biocompatibility and non-cytotoxicity to the skin, ensuring safety and comfort during long-term skin contact. Compared with traditional metal microneedles, PEDOT is softer and more resistant to pulling, which enhances the durability and reliability of microneedles and reduces the risk of damage during use. At the micron level, PEDOT exhibits a stable conductive effect, providing key support for achieving accurate potential difference and efficient electrical stimulation.
[0087] In a third aspect, the present invention provides an application of a conductive microneedle patch in the preparation of a drug for treating blepharospasm.
[0088] It should be noted that the present invention has the following beneficial effects:
[0089] (1) Precision injection design: The microneedle arrangement is designed according to the contour of the orbicularis oculi muscle, which can achieve precise injection and thus reduce the side effects that may be caused by botulinum toxin injection.
[0090] (2) Microneedle technology: The length of microneedles is 300-500 microns, which is enough to penetrate the stratum corneum and reach the dermis. This design can slowly release drugs, reduce stimulation to skin nerves, and relieve patients’ pain symptoms.
[0091] (3) Skin patch microneedle: The microneedle is designed as a skin patch that fits the shape of the orbicularis oculi muscle. It is simple and convenient to use, making it easy for patients to receive treatment.
[0092] (4) Electrical stimulation enhances drug delivery efficiency: The center of the microneedle uses an organic guide wire made of PEDOT / PSS aqueous solution. This design can form a stable potential difference along the entire length of the microneedle after electrical stimulation. This electrical stimulation can more effectively activate the voltage-gated channels of surrounding tissue cells, allowing botulinum toxin to act more effectively on the tissues around the microneedle, thereby enhancing the therapeutic effect, prolonging the action time, and reducing the frequency of repeated treatments.
[0093] (5) PEDOT microneedles: As an organic conductive material, PEDOT has excellent biocompatibility and is non-cytotoxic to skin tissue. This means that it will not cause adverse reactions when in contact with the skin for a long time, ensuring the safety and comfort of the patient. Flexibility and traction resistance: Compared with traditional metal microneedles, PEDOT material is soft and resistant to traction, which makes the microneedles less likely to be damaged during use, increasing the reliability and durability of the product. Stable conductive effect at the micron level: PEDOT material provides stable conductive properties at the micron scale, which is essential for achieving precise potential difference and effective electrical stimulation.
[0094] The preferred embodiments of the present invention are described in detail below to illustrate the principles of the present invention, but are not intended to limit the scope of the present invention.
[0095] The above raw materials in the present invention can be homemade or commercially available, and the present invention is not particularly limited thereto. Among them, the model of the PEDOT / PSS aqueous solution is CLEVIOS™ P VP AI 4083.
[0096] Example 1
[0097] A soluble conductive microneedle patch, wherein the length of the microneedle 11 is 400 microns, the microneedle 11 comprises PVA (98wt%), botulinum toxin type A (1 wt%), graphene (0.5 wt%) and silver nanoparticles (0.5 wt%), the diameter of the conductive microwire 12 is 5 microns, the thickness of the conductive base layer 20 is 5 microns, and the thickness of the collagen base layer 10 is 100 microns.
[0098] A method for preparing a soluble conductive microneedle patch comprises the following steps:
[0099] S1: Prepare the Ecoflex negative mold of the microneedle patch; the specific steps of S1 are as follows:
[0100] S1-1: Prepare a resin mold using a 3D printing method, irradiate the 3D printed resin mold with ultraviolet light for 2 hours and heat it to 120°C for 2 hours;
[0101] S1-2: Place the resin mold in SDS (sodium dodecyl sulfate) solution for about 30 minutes to reduce the adhesion between the 3D printed mold and the Ecoflex negative mold, and then blow dry with a hair dryer;
[0102] S1-3: The 3D printed mold was placed in a plastic petri dish and liquid Ecoflex was slowly poured in. Then, vacuum was applied to it for about 15 minutes and heated at 85°C for 2 hours to complete the curing. Then, it was slowly peeled off to form a negative mold of the microneedle array.
[0103] S2: Add liquid PVA containing botulinum toxin type A, graphene and silver nanoparticles on the microneedle array of the Ecoflex negative mold, fill the PVA solution to the tip of the Ecoflex negative mold by vacuum, scrape the surface of the Ecoflex negative mold with a spatula, and then heat it at no more than 40°C for 1 hour to form a baseless microneedle (to avoid inactivation of botulinum toxin). During the microneedle preparation process, ensure that a channel with a diameter of about 5 microns is left in the center of each microneedle, extending from the root of the microneedle to the tip of the needle;
[0104] S3: After heating, liquid PEDOT (poly 3,4-ethylenedioxythiophene) solution is added to the shaped microneedles. The mass concentration of PEDOT / PSS is 3%. Ultrasonic oscillation technology is used during the addition process to ensure that the PEDOT solution evenly and fully fills the channels in the microneedles. Heat at 35°C to solidify.
[0105] S4: After microneedle fixation and PEDOT filling, the microneedle base was prepared using synthetic type I collagen solution.
[0106] Example 2
[0107] This embodiment is substantially the same as Embodiment 1, except that the microneedle 11 comprises PVA (97 wt %), botulinum toxin type A (1 wt %), graphene (1 wt %), and silver nanoparticles (1 wt %).
[0108] Example 3
[0109] This embodiment is basically the same as the embodiment 1, except that the diameter of the conductive microwire is 4 microns.
[0110] Example 4
[0111] This embodiment is basically the same as the embodiment 1, except that the diameter of the conductive microwire is 6 microns.
[0112] Comparative Example 1
[0113] This comparative example is substantially the same as Example 1, but differs from Example 1 in that the microneedle does not include conductive microwires.
[0114] Experimental Example 1: Morphological Analysis of Soluble Conductive Microneedle Patch
[0115] The microscopic morphology of the microneedle patch of Example 1 was analyzed using a microscope. Figure 4 As shown in the figure, the microneedle array of the microneedle patch is arranged evenly and neatly. Figure 5 As shown, the microneedle is needle-shaped, and the conductive microwire is flush with the tip of the microneedle.
[0116] Experimental Example 2: Effect of Soluble Conductive Microneedle Patch on Treating Blepharospasm
[0117] The same experiment was performed on the microneedle patches prepared in Examples 1-4 and Comparative Example 1.
[0118] (1) Experimental design
[0119] Healthy adult rabbits (adult New Zealand white rabbits, equal sexes, 6 rabbits in each group, 5 months old, weighing about 5 kg) were selected as experimental subjects and divided into an experimental group and a control group, with 6 rabbits in each group. The rabbit blepharospasm animal model was established by electrical stimulation of the facial nerve.
[0120] The experimental groups used the soluble conductive microneedle patches containing conductive microwires of Examples 1-4, and Examples 1-4 corresponded to Experimental Groups 1-4, respectively. The control group used the microneedle patch without conductive microwires of Comparative Example 1. The sham operation group only established the blepharospasm model but did not receive microneedle patch treatment.
[0121] The patch was applied to the orbicularis oculi muscle of the rabbits and electrical stimulation was performed, and the therapeutic effects of each group of rabbits were recorded.
[0122] (2) Experimental procedures
[0123] Patch application: Apply the microneedle patch to the orbicularis oculi muscle of the rabbit, ensuring that the microneedles are fully inserted into the dermis.
[0124] Electrical stimulation: The experimental group was given 4 mA electrical stimulation to activate the potential difference in the conductive microfilaments and enhance the effect of the drug.
[0125] Observation and Recording: The symptom changes of each rabbit, including the frequency and severity of blepharospasm, were recorded 1 day, 2 days, 7 days, 14 days and 28 days after patch application.
[0126] (3) Experimental results
[0127] (3-1) Symptom improvement
[0128] Experimental Group 1 began to show obvious symptom improvement one day after the application of the patch, and the symptoms of blepharospasm were significantly relieved; Examples 2-4 began to show obvious symptom improvement 2-3 days later (it should be noted that the establishment of a rabbit blepharospasm animal model by electrical stimulation of the facial nerve was carried out after the application of the patch, and the observation time nodes were observed. For example, when the rabbit blepharospasm animal model was established by electrical stimulation of the facial nerve one day after the application of the patch in Experimental Group 1, the experimental subjects did not experience blepharospasm, so it was described as beginning to show obvious symptom improvement. The rest of the situations are similar and will not be repeated).
[0129] During the 7-day and 14-day observations, the therapeutic effects of experimental groups 1-4 continued to be evident, and the symptoms of blepharospasm basically disappeared.
[0130] The control group also showed some improvement in symptoms after 2 days, but the effect was not as significant as that of the experimental group, and the symptoms recurred after 14 days.
[0131] The sham operation group did not show any improvement in symptoms during the observation period.
[0132] (3-2) Comparison of effects
[0133] The therapeutic effects of experimental groups 1-4 were significantly better than those of control group 1 and lasted longer. The blepharospasm symptoms of rabbits in the experimental groups remained well improved after 28 days.
[0134] The symptoms of some rabbits in the control group relapsed after 28 days, indicating that the microneedle patch without conductive microwires was less effective.
[0135] There was no improvement in symptoms in the sham operation group during the observation period.
[0136] (4) Statistical analysis
[0137] The total effective rate of experimental groups 1-4 was 90%, and the total effective rate of the control group was 50%. The data were analyzed using t-test, and the P value was <0.05, indicating that the difference in treatment effect between the experimental group and the control group was statistically significant.
[0138] The results show that the microneedle of Comparative Example 1 does not include conductive microwires inside, and the effect is far inferior to the experimental effects of Examples 1-4.
[0139] Any numerical value mentioned in the present invention, if there is only an interval of two units between any minimum value and any maximum value, includes all values from the minimum value to the maximum value each time increasing by one unit. For example, if the amount of a component, or the value of a process variable such as temperature, pressure, time, etc. is declared to be 50-90, in this specification it means that 51-89, 52-88... and 69-71 and 70-71 are specifically listed. For non-integer values, 0.1, 0.01, 0.001 or 0.0001 can be appropriately considered as a unit. These are just some specially specified examples. In this application, in a similar manner, all possible combinations of numerical values between the listed minimum and maximum values are considered to have been disclosed.
[0140] It should be noted that the embodiments described above are only used to explain the present invention and do not constitute any limitation to the present invention. The present invention has been described with reference to typical embodiments, but it should be understood that the words used therein are descriptive and explanatory words, rather than restrictive words. The present invention may be modified as specified within the scope of the claims of the present invention, and the present invention may be revised without departing from the scope and spirit of the present invention. Although the present invention described therein relates to specific methods, materials and embodiments, it does not mean that the present invention is limited to the specific examples disclosed therein, on the contrary, the present invention can be extended to all other methods and applications with the same functions.
Claims
1. A method for preparing a conductive microneedle patch, characterized in that: The steps include: S1: preparing a negative mold of the conductive microneedle patch, wherein the negative mold is made of Ecoflex silicone and comprises a base layer negative mold and a microneedle array negative mold; S2: adding liquid PVA containing botulinum toxin type A, graphene and silver nanoparticles into the negative mold of the microneedle array, and then heating to form a microneedle array without a substrate layer, and using a wire drawing method to reserve a channel inside each microneedle during the heating process, wherein the diameter of the channel is 4-6 microns; S3: After the heating is completed, a PEDOT / PSS aqueous solution is added dropwise into the channel, and ultrasonic vibration is performed to heat and solidify the channel to form conductive microwires and a conductive base layer.
2. The method according to claim 1, characterized in that: S1 includes the following steps: S1-1: preparing a mold of the negative mold, and irradiating and heating the mold with ultraviolet light; S1-2: placing the mold obtained in step S1-1 into an aqueous solution containing a surfactant, then taking it out and blowing it dry; S1-3: Pour liquid Ecoflex into the mold obtained in S1-2, then apply vacuum and heat to form a negative mold of the conductive microneedle patch.
3. The method according to claim 2, characterized in that In S1-1, the mold is irradiated with ultraviolet light for 1-3 hours and heated to 100-150° C. for 1-3 hours.
4. The method according to claim 2, characterized in that: In S1-2, the surfactant is an alkyl sulfonate, and the mass concentration of the surfactant is 1%-2%. And / or, in S1-3, the conditions of applying vacuum and heating include: applying vacuum for 10-15 minutes, and heating at 80-85°C for 1-2 hours.
5. The method according to any one of claims 1 to 4, characterized in that The method further comprises step S4: preparing a collagen base layer using a collagen solution.
6. The method according to any one of claims 1 to 4, characterized in that In S2, heating at 35-40° C. for 1-2 hours to form a substrate-free microneedle array; And / or, in S3, the temperature of heating and curing is 30-40°C.
7. A conductive microneedle patch prepared by the preparation method according to any one of claims 1 to 6, comprising a microneedle array and a conductive substrate layer, wherein the microneedle array is arranged on the conductive substrate layer, characterized in that: The microneedle array comprises microneedles and conductive microwires. The materials of the microneedle include PVA, botulinum toxin type A, graphene and silver nanoparticles; based on the total weight of the microneedle, the mass percentage of PVA is 97-99%; the mass percentage of botulinum toxin type A is 0.5-2%; the mass percentage of graphene is 0.1-1%; and the mass percentage of silver nanoparticles is 0.1-1%; The conductive microwire is arranged inside the microneedle, and the conductive microwire extends from the needle tip of the microneedle to the conductive base layer; The conductive microwires and the conductive base layer are made by curing a PEDOT / PSS aqueous solution, and the mass concentration of PEDOT / PSS in the PEDOT / PSS aqueous solution is 3-5%.
8. The conductive microneedle patch according to claim 7, characterized in that: The diameter of the conductive microwire is 4-6 microns. And / or, the microneedle is conical, and the diameter of the cone bottom is 40-60 microns; and / or, the length of the microneedle is 300-500 microns, and / or, the thickness of the conductive substrate layer is 4-6 microns, And / or, the distance between the centers of the cone bottom surfaces of adjacent microneedles is 0.4-0.6 mm.
9. The conductive microneedle patch according to claim 7 or 8, characterized in that: The conductive microneedle patch also includes a collagen base layer, which is arranged below the conductive base layer. The thickness of the collagen base layer is 100-200 microns.
10. Use of the conductive microneedle patch according to any one of claims 7 to 9 or the conductive microneedle patch prepared by the method according to any one of claims 1 to 6 in preparing a drug for treating blepharospasm.