Reproduction process of fitness equipment

By using a combination of sand and gravel, iron powder, super-heavy metal materials and water-absorbent resin or hydraulic coagulant, the problems of high cost, low efficiency and environmental pollution in the production of fitness equipment weight devices are solved, achieving cost reduction, efficiency improvement and environmental protection. Effect.

CN118744537APending Publication Date: 2024-10-08JINHUA LETU SPORTS GOODS CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411002206.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-25
Publication Date
2024-10-08

AI Technical Summary

Technical Problem

The existing production process of fitness equipment counterweight devices has problems of high cost, low efficiency and environmental pollution. Traditional processes such as steel smelting and cement canning lead to high material costs, high transportation costs, low production efficiency and serious environmental pollution.

Method used

Sand, iron powder, and super-heavy metal materials are used as counterweight materials, combined with water-absorbent resin or hydraulic coagulant, mixed and solidified through mechanical stirring, pressing or vibration, and water is injected to adjust the density and shape to achieve flexible counterweight adjustment.

Benefits of technology

It significantly reduces production and transportation costs, improves production efficiency, reduces environmental pollution, enriches product usage scenarios and adaptability, and meets market demand.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118744537A_ABST
    Figure CN118744537A_ABST
Patent Text Reader

Abstract

The invention provides a fitness equipment re-production process which is particularly suitable for production of dumbbell, kettle-bell and barbell weight-bearing fitness equipment. By optimizing the production materials and adjusting the production process, the purposes of increasing the yield, reducing the cost, diversifying forms and reducing the transportation size are achieved, by optimizing the production process and the material ratio, the production efficiency of the fitness equipment balance weight can be remarkably improved, and therefore the ever-increasing requirements of the market for fitness equipment are met. The water-absorbent resin or the hydrogel is adopted as the additive, so that the volume of the counterweight product can be flexibly adjusted through water injection after the counterweight product is cured, the counterweight product can form various forms such as a liquid, a semi-liquid, a semi-solidified state or a solid state according to needs, and the use scene and the adaptability of the product are greatly enriched. According to the technical scheme, low-cost materials such as gravel, iron powder and overweight metal materials are selected as the balance weight materials, and the production cost is effectively reduced by combining the additives.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of fitness equipment weight production, and in particular to a new production process of fitness equipment weights. Background Art

[0002] With the rapid development of the fitness industry, the demand for fitness equipment is increasing. As an important part of fitness equipment, the production process and cost control of weight devices are of great significance to improving product quality, reducing production costs and protecting the environment. Before this innovation, the production of fitness equipment weight devices mainly used two processes: steel smelting and cement canning.

[0003] Steel smelting production process: Steel smelting production process is the traditional production method of fitness equipment weight devices, which mainly includes steel smelting, cutting, electroplating, rubber coating and other steps. Although this production method can produce weight devices with certain strength and durability, it has the following shortcomings in the production process: High temperature smelting: Steel smelting requires a high temperature environment, which not only consumes a lot of energy, but also produces waste gas and waste slag that pollute the environment. Material cost: Steel, as a 100% filling material, is expensive and heavy, increasing transportation costs. Production efficiency: Smelting, cutting, electroplating and other processes are complicated, the production cycle is long, and the efficiency is low.

[0004] Cement canning production process: Cement canning production process is another common way to produce weight devices for fitness equipment, including preparation of raw materials, calcination of cement clinker, grinding, canning and other steps. This production method also has the following problems: Labor cost: Cement canning requires manual operation, high labor cost and low production efficiency. Environmental pollution: Dust particles generated during cement canning pose a threat to the environment and workers' health. Transportation cost: Cement, as a 100% filling material, is heavy, resulting in increased transportation costs.

[0005] In summary, the existing fitness equipment weight device production process has the following deficiencies in the production process: High cost: Whether it is steel smelting or cement canning, the material cost is high, and due to the heavy weight, the transportation cost is also relatively high. Low efficiency: The production processes of steel smelting and cement canning are both complicated and have low production efficiency. Environmental pollution: The waste gas, waste slag and dust particles generated during high-temperature smelting and cement canning pollute the environment and do not meet modern environmental protection requirements. Therefore, we propose a new production process for fitness equipment. Summary of the invention

[0006] The purpose of the present invention is to solve the problems in the existing background technology. In order to achieve the above invention purpose, the present invention provides the following technical solutions: a new production process of fitness equipment accessories, including the following production process steps: S1. Material preparation: select sand, stone, iron powder and super heavy metal materials as counterweight materials and mix them according to the proportion; S11, Proportion: sand and gravel account for 40%, iron powder accounts for 30%, and super heavy metal materials account for 30%; S12, mixing method: use a batching machine to mix the proportions, and mix evenly with a mechanical stirrer, and the stirring time is set to 10 minutes; S2. Additive mixing: add water-absorbing resin or hydrocoagulant into the weight material and stir evenly; S21, water-absorbing resin or hydrogelling agent addition amount: add 1-5% water-absorbing resin or hydrogelling agent to 10-50% or more of the weight material; S22. Stirring method: Use a high-speed stirrer to stir, ensuring that the water-absorbing resin or hydrocoagulant is evenly distributed in the weight material, and the stirring time is set to 5 minutes; S3, Punching: Put the mixed material into the mold and punch it by pressing or vibrating. S31. Mould type: Select the corresponding mould according to the product design and shape; S32, pressing or vibration method: if the pressing method is adopted, the pressure is set to 10 MPa and the pressure holding time is 30 seconds; if the vibration method is adopted, the vibration frequency is set to 50 Hz and the vibration time is 60 seconds; S33, Punching density: The density of the weight material after punching is between 2.5-3.0g / cm³, which makes the product strong and stable; S4, water injection: inject water through the water injection port to make the water-absorbing resin inside the product absorb water and expand, so as to flexibly adjust the counterweight; S41. Water inlet location: Set the water inlet at the bottom or side of the fitness equipment to ensure that the water inlet is easy to operate and not prone to leakage; S42, water injection amount: according to the product size and the required weight, calculate and inject the appropriate amount of water; every 100g of water-absorbent resin can absorb about 200-300ml of water; S43, water injection speed: control the water injection speed between 10-20ml / s; S44, water absorption and swelling time: after water injection, the water-absorbing resin is allowed to naturally absorb water and swell for about 30 minutes to ensure that it fully absorbs water; S5, curing: curing the product after punching to make it have certain strength and stability; S51, curing temperature: set the curing temperature to 60-80°C, and adjust it according to the properties of specific materials and additives; S52, curing time: according to the size and thickness of the product, set the curing time to 2-4 hours; S53. Curing method: natural curing or heating curing. When using heating curing, it is necessary to ensure that the temperature is evenly distributed to avoid deformation or cracking of the product.

[0007] As a preferred technical solution of the present invention, S2, during the additive mixing process, the density of the product is controlled by adjusting the ratio of sand, iron powder and super heavy metal materials in the weight mixture so that the product density ranges from 1000kg to 6000kg / m³.

[0008] As a preferred technical solution of the present invention, in S5, during the water injection process, 5% iron sand and 1% coagulant are used to produce and transport a weight of 1.5KG, and the product weight after water injection is 6-7kg.

[0009] As a preferred technical solution of the present invention, in S5, during the water injection process, 10% iron sand and 1% coagulant are used to produce and transport a weight of 2.7KG, and the product weight after water injection is 7-8kg.

[0010] As a preferred technical solution of the present invention, in S5, during the water injection process, 15% iron sand and 1% coagulant are used to produce and transport a weight of 3.8KG, and the weight of the product after water injection is 8-9KG.

[0011] As a preferred technical solution of the present invention, in S5, during the water injection process, 30% iron sand and 1% coagulant are used to produce and transport a weight of 7.8KG, and the product weight after water injection is 11-12KG.

[0012] As a preferred technical solution of the present invention, after water injection using 5% iron sand and 1% coagulant, the product state is a semi-wave fluid.

[0013] As a preferred technical solution of the present invention, after water injection using 5% iron sand + 2% coagulant, the product state is a semi-solidified Newtonian body.

[0014] As a preferred technical solution of the present invention, after water injection using 5% iron sand and 3%-5% coagulant, the product is in a solidified flexible body.

[0015] As a preferred technical solution of the present invention, after injecting water using 5% iron sand and more than 5% solidifying agent, the product is in a solidified state; the weight of the product is in a powdery state.

[0016] Compared with the prior art, the beneficial effects of the present invention are as follows: In the scheme of the present invention: by optimizing the production process and material ratio, the technical scheme can significantly improve the production efficiency of fitness equipment weights, thereby meeting the market's growing demand for fitness equipment.

[0017] By using absorbent resin or hydrogel as additives, the volume of the counterweight product can be flexibly adjusted by water injection after solidification, and it can be formed into various forms such as liquid, semi-liquid, semi-solid or solid as needed, greatly enriching the product's usage scenarios and adaptability.

[0018] This technical solution uses low-cost materials such as sand, iron powder, and super-heavy metal materials as counterweight materials, and combines the use of additives to effectively reduce production costs. It is estimated that compared with traditional processes, this technical solution can reduce production costs by more than 30%, bringing significant economic benefits to enterprises.

[0019] Since the counterweight products produced by this technical solution are in a smaller volume and lighter weight state before transportation, the volume and weight during transportation can be significantly reduced, thereby reducing transportation costs. It is estimated that this technical solution can reduce transportation costs in this field by more than 30%, bringing great convenience to the logistics and distribution of enterprises.

[0020] This technical solution does not require high-temperature smelting and a large amount of manpower in the production process, reducing environmental pollution and energy consumption. At the same time, by flexibly adjusting the product shape and volume, it can reduce unnecessary material waste, further embodying the concept of environmental protection and energy saving.

[0021] By injecting water to adjust the water absorption and expansion degree of the water-absorbent resin inside the product, users can flexibly adjust the weight according to actual needs, thereby improving the practicality and convenience of the product. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 A process flow chart provided by the present invention; Figure 2 A schematic diagram of experimental data provided by the present invention; Figure 3 This is a schematic diagram of experimental data provided by the present invention. DETAILED DESCRIPTION

[0023] To make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be described clearly and completely in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them.

[0024] Therefore, the following detailed description of the embodiments of the present invention is not intended to limit the scope of the invention claimed for protection, but only represents some embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention. It should be noted that, in the absence of conflict, the embodiments of the present invention and the features and technical solutions in the embodiments are combined with each other. It should be noted that similar numbers and letters represent similar items in the following drawings. Therefore, once an item is defined in one drawing, it does not need to be further defined and explained in subsequent drawings.

[0025] Example 1: Please refer to Figure 1-Figure 3 , a fitness equipment re-production process, including the following production process steps: S1. Material preparation: select sand, stone, iron powder and super heavy metal materials as counterweight materials and mix them according to the proportion; S11, Proportion: sand and gravel account for 40%, iron powder accounts for 30%, and super heavy metal materials account for 30%; S12, mixing method: use a batching machine to mix the proportions, and mix evenly with a mechanical stirrer, and the stirring time is set to 10 minutes; S2. Additive mixing: add water-absorbing resin or hydrocoagulant into the weight material and stir evenly; S21, water-absorbing resin or hydrogelling agent addition amount: add 1-5% water-absorbing resin or hydrogelling agent to 10-50% or more of the weight material; S22. Stirring method: Use a high-speed stirrer to stir, ensuring that the water-absorbing resin or hydrocoagulant is evenly distributed in the weight material, and the stirring time is set to 5 minutes; S3, Punching: Put the mixed material into the mold and punch it by pressing or vibrating. S31. Mould type: Select the corresponding mould according to the product design and shape; S32, pressing or vibration method: if the pressing method is adopted, the pressure is set to 10 MPa and the pressure holding time is 30 seconds; if the vibration method is adopted, the vibration frequency is set to 50 Hz and the vibration time is 60 seconds; S33, Punching density: The density of the weight material after punching is between 2.5-3.0g / cm³, which makes the product strong and stable; S4, water injection: inject water through the water injection port to make the water-absorbing resin inside the product absorb water and expand, so as to flexibly adjust the counterweight; S41. Water inlet location: Set the water inlet at the bottom or side of the fitness equipment to ensure that the water inlet is easy to operate and not prone to leakage; S42, water injection amount: according to the product size and the required weight, calculate and inject the appropriate amount of water; every 100g of water-absorbent resin can absorb about 200-300ml of water; S43, water injection speed: control the water injection speed between 10-20ml / s; S44, water absorption and swelling time: after water injection, the water-absorbing resin is allowed to naturally absorb water and swell for about 30 minutes to ensure that it fully absorbs water; S5, curing: curing the product after punching to make it have certain strength and stability; S51, curing temperature: set the curing temperature to 60-80°C, and adjust it according to the properties of specific materials and additives; S52, curing time: according to the size and thickness of the product, set the curing time to 2-4 hours; S53. Curing method: natural curing or heating curing. When using heating curing, it is necessary to ensure that the temperature is evenly distributed to avoid deformation or cracking of the product.

[0026] S2. During the additive mixing process, the density of the product is controlled by adjusting the ratio of sand, iron powder and super heavy metal materials in the weight mixture, so that the product density range is 1000kg-6000kg / m³.

[0027] S5. During the water injection process, 5% iron sand and 1% coagulant are used to produce and transport 1.5KG of product weight after water injection, and the product weight is 6-7kg.

[0028] S5. During the water injection process, 10% iron sand and 1% coagulant are used to produce and transport 2.7KG. The product weight after water injection is 7-8kg.

[0029] S5. During the water injection process, 15% iron sand and 1% coagulant are used to produce and transport a weight of 3.8KG. The product weight after water injection is 8-9KG.

[0030] S5. During the water injection process, 30% iron sand and 1% coagulant are used to produce and transport 7.8KG of product weight after water injection, and the product weight is 11-12KG.

[0031] After water injection using 5% iron sand and 1% solidifying agent, the product state is a semi-wavy fluid.

[0032] After using 5% iron sand + 2% coagulant and injecting water, the product state is a semi-solidified Newtonian body.

[0033] After using 5% iron sand and 3%-5% solidifying agent and injecting water, the product state is a solidified flexible body.

[0034] After using 5% iron sand and more than 5% solidifying agent and injecting water, the product is in a solidified state; the product is in a powdery state.

[0035] By optimizing the production process and material ratio, this technical solution can significantly improve the production efficiency of fitness equipment weights, thereby meeting the market's growing demand for fitness equipment.

[0036] By using absorbent resin or hydrogel as additives, the volume of the counterweight product can be flexibly adjusted by water injection after solidification, and it can be formed into various forms such as liquid, semi-liquid, semi-solid or solid as needed, greatly enriching the product's usage scenarios and adaptability.

[0037] This technical solution uses low-cost materials such as sand, iron powder, and super-heavy metal materials as counterweight materials, and combines the use of additives to effectively reduce production costs. It is estimated that compared with traditional processes, this technical solution can reduce production costs by more than 30%, bringing significant economic benefits to enterprises.

[0038] Since the counterweight products produced by this technical solution are in a smaller volume and lighter weight state before transportation, the volume and weight during transportation can be significantly reduced, thereby reducing transportation costs. It is estimated that this technical solution can reduce transportation costs in this field by more than 30%, bringing great convenience to the logistics and distribution of enterprises.

[0039] This technical solution does not require high-temperature smelting and a large amount of manpower in the production process, reducing environmental pollution and energy consumption. At the same time, by flexibly adjusting the product shape and volume, it can reduce unnecessary material waste, further embodying the concept of environmental protection and energy saving.

[0040] By injecting water to adjust the water absorption and expansion degree of the water-absorbent resin inside the product, users can flexibly adjust the weight according to actual needs, thereby improving the practicality and convenience of the product.

[0041] During the use of the present invention, the specific workflow of the fitness equipment re-production process is as follows: Material preparation (S1): Select sand, gravel, iron powder, and super heavy metal materials as counterweight materials. Determine the proportion of various materials according to the density requirements of the product and mix them evenly.

[0042] Additive mixing (S2): Add 1-5% of water-absorbing resin or hydrogel to the weight material with good proportion. Use stirring equipment to ensure that the additive and weight material are mixed evenly.

[0043] Punching (S3): Put the mixed material into the pre-designed mold. Use pressing or vibration equipment to punch the material to ensure that the shape and size of the product meet the design requirements.

[0044] Curing (S4): After punching, the product enters the curing stage, which is cured naturally or by heating. During the curing process, the product gradually acquires a certain strength and stability.

[0045] Water injection (S5): A water injection port is set at a specific position of the fitness equipment. Water is injected into the product through the water injection port to make the water-absorbing resin absorb water and expand, thereby achieving flexible adjustment of the weight.

[0046] Working principle: Material ratio: By adjusting the ratio of sand, iron powder and super heavy metal materials, the density of the product can be controlled to meet the weight requirements of different fitness equipment.

[0047] Function of additives: Water-absorbent resin swells when it comes into contact with water, allowing flexible adjustment of the weight; hydrogel helps solidify the product, enhancing its stability and durability.

[0048] Punching and curing: Punching and curing processes ensure that the product has a fixed shape and size while obtaining sufficient strength and stability.

[0049] Water injection adjustment: The water injection process adjusts the weight of the product according to actual needs to meet the personalized needs of different users.

[0050] Experimental Example 1 1. Purpose of the experiment To verify a new fitness equipment re-production process, which reduces product production costs, improves production efficiency, saves materials, and allows flexible adjustment of product volume and density by adjusting the ratio of sand, iron powder, super-heavy metal materials, water-absorbing resin or hydrocoagulant.

[0051] 2. Experimental Materials Sand, stone, iron powder, heavy metal material, water-absorbing resin, hydrogel, water injection mold 3. Experimental steps 1. Material preparation: Prepare sand, gravel, iron powder, super heavy metal materials, absorbent resin or hydraulic agent according to the preset ratio.

[0052] 2. Mixing and stirring: Mix sand, iron powder and super heavy metal materials evenly according to the preset proportion to form the basic counterweight material.

[0053] 3. Formula adjustment: According to experimental requirements, add an appropriate amount of water-absorbing resin or hydrocoagulant to the basic weight material to adjust the volume and weight of the product.

[0054] 4. Water injection molding: Pour the adjusted weight material into the water injection mold, and inject an appropriate amount of water through the water injection port to form it into the desired shape.

[0055] 5. Curing treatment: Leave the product in the mold for a period of time to cure to the required hardness and strength.

[0056] 6. Measurement records: Weigh the cured product and record its weight and status.

[0057] IV. Experimental Results The following are the experimental results obtained according to different ratios and water injection conditions: Experiment number Ratio (iron sand / coagulant) Shipping weight (kg) Weight range after water injection (kg) Product Status 1 5% / 1% 1.5 6-7 Half-wave fluid 2 10% / 1% 2.7 7-8 Semi-solidified Newtonian body 3 15% / 1% 3.8 8-9 Solidification Flexible Body 4 30% / 1% 7.8 11-12 Solid Experimental data analysis From the experimental data, it can be seen that by adjusting the ratio and water injection volume, the transportation weight of the product and the weight range after water injection can be effectively controlled, and the product state can be diversified. Specifically: When the ratio of iron sand to coagulant is 5% / 1%, the product has a lighter transportation weight and presents a semi-wave fluid state after water injection, which is suitable for occasions that require flexible weight adjustment.

[0058] As the ratio of iron sand to coagulant increases, the transportation weight of the product also increases accordingly, and the weight range and state after water injection also change. For example, when the ratio is 10% / 1%, the product presents a semi-solidified Newtonian state after water injection, with higher stability and load-bearing capacity.

[0059] When the ratio reaches 30% / 1%, the transportation weight of the product increases significantly, and it presents a solidified state after water injection, which is suitable for occasions requiring high density and high load-bearing capacity.

[0060] In summary, the fitness equipment re-production process of the present invention achieves reduced product production costs, improved production efficiency, material savings, and flexible adjustment of product volume and density by flexibly adjusting the mixing ratio and water injection volume, thereby meeting the needs of different users and occasions.

[0061] Experimental Example 2: Take the production and transportation of a dumbbell weighing 1.5KG using 5% iron sand and 1% coagulant as an example: 1. Material preparation and mixing: According to the proportion, mix sand, gravel, iron powder and super heavy metal materials evenly.

[0062] Add 5% iron sand and 1% coagulant to the mixed materials and mix well again.

[0063] 2. Punching and curing: Put the mixed materials into the dumbbell mold and punch it.

[0064] After the punching is completed, a curing process is carried out to ensure that the dumbbells have sufficient strength and stability.

[0065] 3. Water injection: A water injection port is provided at a specific position of the dumbbell.

[0066] Water is injected into the dumbbell through the water injection port to make the water-absorbent resin absorb water and expand.

[0067] The weight of the dumbbells after water filling should be between 67kg.

[0068] 4. Product status and testing: After being filled with water, the dumbbell is in a semi-wave fluid state, with good flexibility and adaptability.

[0069] The dumbbells are tested for strength, stability, etc. to ensure that the products meet quality requirements.

[0070] 5. Experimental Data Product density under different ratios: Ratio A (50% sand and gravel, 30% iron powder, 20% super heavy metal material): product density is about 2500kg / m³. Ratio B (40% sand and gravel, 40% iron powder, 20% super heavy metal material): product density is about 3500kg / m³. Ratio C (30% sand and gravel, 50% iron powder, 20% super heavy metal material): product density is about 4500kg / m³. Comparison of product weights before and after water injection: Dumbbells weighing 1.5KG produced and transported using 5% iron sand and 1% coagulant: Weight before water injection: 1.5KG Weight after water injection: 6.5KG (range 67kg) Barbell plates weighing 2.7KG produced and transported using 10% iron sand and 1% coagulant: Weight before water injection: 2.7KG Weight after water injection: 7.8KG (range 78kg) Kettlebells weighing 3.8KG produced and transported using 15% iron sand and 1% coagulant: Weight before water injection: 3.8KG Weight after water injection: 8.7KG (range 89kg) Rubber-coated weight plates weighing 7.8KG produced and transported using 30% iron sand and 1% coagulant: Weight before water injection: 7.8KG Weight after water injection: 11.5KG (range 1112kg) Product status description: The product after water injection using 5% iron sand and 1% coagulant is in a semi-wavy fluid state, soft and easy to flush.

[0071] The product after water injection using 5% iron sand + 2% coagulant is in a semi-solidified Newtonian state with a certain hardness and stability.

[0072] The product after water injection using 5% iron sand and 3%5% coagulant is in a solidified flexible body state, which has a certain hardness and maintains good flexibility.

[0073] The product after water injection using 5% iron sand and more than 5% solidifying agent is in a solidified state with high hardness and good stability.

[0074] Conclusion: The above experimental data show that by adjusting the material ratio and the amount of water injection, fitness equipment weight products with different densities, weights and states can be produced. These products not only meet the demand for weights for fitness equipment, but also have good flexibility and adaptability, and can be adjusted according to the personalized needs of users. At the same time, the experimental data also verifies the feasibility and effectiveness of this production process.

[0075] The above embodiments are only used to illustrate the present invention and are not intended to limit the technical solutions described in the present invention. Although the present invention has been described in detail with reference to the above embodiments, the present invention is not limited to the above specific implementation methods. Therefore, any modification or replacement of the present invention; and all technical solutions and improvements thereof that do not depart from the spirit and scope of the invention are included in the scope of the claims of the present invention.

Claims

1. A fitness equipment re-production process, characterized in that: The production process includes the following steps: S1. Material preparation: select sand, stone, iron powder and super heavy metal materials as counterweight materials and mix them according to the proportion; S11, Proportion: sand and gravel account for 40%, iron powder accounts for 30%, and super heavy metal materials account for 30%; S12, mixing method: use a batching machine to mix the proportions, and mix evenly with a mechanical stirrer, and the stirring time is set to 10 minutes; S2. Additive mixing: add water-absorbing resin or hydrocoagulant to the weight material and stir evenly; S21, water-absorbing resin or hydrogelling agent addition amount: add 1-5% water-absorbing resin or hydrogelling agent to 10-50% or more of the weight material; S22. Stirring method: Use a high-speed stirrer to stir, ensuring that the water-absorbing resin or hydrocoagulant is evenly distributed in the weight material, and the stirring time is set to 5 minutes; S3, punching and packing: put the mixed materials into the mold and punch them by pressing or vibrating; S31. Mould type: Select the corresponding mould according to the product design and shape; S32, pressing or vibration method: if the pressing method is adopted, the pressure is set to 10 MPa and the pressure holding time is 30 seconds; if the vibration method is adopted, the vibration frequency is set to 50 Hz and the vibration time is 60 seconds; S33, Punching density: The density of the weight material after punching is between 2.5-3.0g / cm³, which makes the product strong and stable; S4, water injection: set a water injection port at a specific position of the fitness equipment, including dumbbells, kettlebells, barbells and weight-bearing fitness equipment, and inject water through the water injection port to make the water-absorbing resin inside the product absorb water and expand, so as to flexibly adjust the weight; S41. Water inlet location: Set the water inlet at the bottom or side of the fitness equipment to ensure that the water inlet is easy to operate and not prone to leakage; S42, water injection amount: according to the product size and the required weight, calculate and inject the appropriate amount of water; every 100g of water-absorbent resin can absorb about 200-300ml of water; S43, water injection speed: control the water injection speed between 10-20ml / s; S44, water absorption and swelling time: after water injection, the water-absorbing resin is allowed to naturally absorb water and swell for about 30 minutes to ensure that it fully absorbs water; S5, curing: curing the product after punching to make it have certain strength and stability; S51, curing temperature: set the curing temperature to 60-80°C, and adjust it according to the properties of specific materials and additives; S52, curing time: according to the size and thickness of the product, set the curing time to 2-4 hours; S53. Curing method: natural curing or heating curing. When using heating curing, it is necessary to ensure that the temperature is evenly distributed to avoid deformation or cracking of the product.

2. A fitness equipment re-production process according to claim 1, characterized in that: S2. During the additive mixing process, the density of the product is controlled by adjusting the ratio of sand, iron powder and super heavy metal materials in the weight mixture, so that the product density range is 1000kg-6000kg / m³.

3. A fitness equipment re-production process according to claim 2, characterized in that: S5. During the water injection process, 5% iron sand and 1% coagulant are used to produce and transport 1.5KG of product weight after water injection, and the product weight is 6-7kg.

4. A fitness equipment re-production process according to claim 3, characterized in that: S5. During the water injection process, 10% iron sand and 1% coagulant are used to produce and transport 2.7KG. The product weight after water injection is 7-8kg.

5. A fitness equipment re-production process according to claim 4, characterized in that: S5. During the water injection process, 15% iron sand and 1% coagulant are used to produce and transport a weight of 3.8KG. The product weight after water injection is 8-9KG.

6. A fitness equipment re-production process according to claim 5, characterized in that: S5. During the water injection process, 30% iron sand and 1% coagulant are used to produce and transport 7.8KG of product weight after water injection, and the product weight is 11-12KG.

7. A fitness equipment re-production process according to claim 3, characterized in that: After water injection using 5% iron sand and 1% solidifying agent, the product state is a semi-wavy fluid.

8. A fitness equipment re-production process according to claim 7, characterized in that: After using 5% iron sand + 2% coagulant and injecting water, the product state is a semi-solidified Newtonian body.

9. A fitness equipment re-production process according to claim 8, characterized in that: After using 5% iron sand and 3%-5% solidifying agent and injecting water, the product state is a solidified flexible body.

10. A fitness equipment re-production process according to claim 9, characterized in that: After using 5% iron sand and more than 5% solidifying agent and injecting water, the product is in a solidified state; the product is in a powdery state.

Citation Information

Patent Citations

  • Novel ball or dumb bells and producing method thereof

    CN101297995A

  • Manufacturing method for fitness equipment and accessories thereof

    CN102100958A

  • Dumbbell and barbell products manufactured from composite material and manufacturing method of dumbbell and barbell products

    CN102746579A

  • Manufacturing method of rotationally molded dumbbell or barbell plate

    CN111716611A