Reduced-pressure multi-layer glass panel

By designing a column structure in the decompression multilayer glass panel, and utilizing the combination of the contact surface and the non-contact part, stress is dispersed and the slope angle is optimized, thus solving the problem of glass panel breakage under external impact and achieving the effect of low heat transfer rate and high impact strength.

CN118908594APending Publication Date: 2024-11-08NIPPON SHEET GLASS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410958435.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2020-03-13
Filing Date
2021-02-24
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

Existing pressure-reducing multilayer glass panels are prone to deformation and breakage when subjected to external impact, and have a high heat transfer rate, making it difficult to simultaneously reduce the heat transfer rate and increase the impact strength.

Method used

The structure adopts a columnar design with a contact surface and a non-contact part. The contact surface is in contact with the glass plate, while the non-contact part is in contact with the deformed glass plate under external force, thus dispersing stress. Furthermore, the heat transfer rate is reduced by optimizing the slope angle and shape design.

Benefits of technology

It effectively inhibits glass breakage, improves impact strength, and reduces heat transfer rate, achieving a glass panel with high thermal insulation and high strength.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118908594A_ABST
    Figure CN118908594A_ABST
Patent Text Reader

Abstract

The present invention relates to a reduced-pressure multilayer glass panel (10) comprising a first glass plate (11), a second glass plate (12), a sealing part for forming a gap part (13) sealed in a reduced-pressure state between the first glass plate (11) and the second glass plate (12), and a plurality of columns (16) disposed between the first glass plate (11) and the second glass plate (12). The column body (16) has an abutting surface (21) which abuts against the facing surfaces (17, 18) of the first glass plate and the second glass plate, and a non-abutting part (23) which is provided around the abutting surface (21) and is separated from the facing surfaces (17, 18) of the first glass plate and the second glass plate. The non-contact section (23) is configured such that at least a portion thereof can come into contact with the first glass plate or the second glass plate which is deformed when the first glass plate or the second glass plate which faces the first glass plate or the second glass plate is deformed by a first external force.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] This application is a divisional application based on the invention with application number 202180020143.7, application date February 24, 2021, applicant being Nippon Sheet Glass Co., Ltd., and invention name being “Pressure-Reducing Multi-Layer Glass Panel”. Technical Field

[0002] The present invention relates to pressure-reducing multi-layer glass panels. Background Art

[0003] The decompression multilayer glass panel includes a pair of glass plates and a plurality of columns arranged between the pair of glass plates. A gap portion sandwiching the columns is provided between the pair of glass plates, and the gap portion is configured to be in a decompression state. When a temperature difference occurs between the pair of glass plates, a portion of the heat moves from one glass plate to the other glass plate via the columns. From the perspective of improving the thermal insulation performance of the decompression multilayer glass panel, such heat movement is preferably as small as possible. That is, in the decompression multilayer glass panel, the heat transfer coefficient (U value) is preferably low. The heat transfer coefficient of the decompression multilayer glass panel is proportional to the contact area between the pair of glass plates and the columns.

[0004] Patent Document 1 discloses a structure of a vacuum multi-layer glass panel using a cylinder with a diameter of 600 μm or less as a column. In this way, a vacuum multi-layer glass panel with a small diameter of the column can reduce the heat transfer rate.

[0005] Prior art literature

[0006] Patent Literature

[0007] Patent Document 1: Japanese Patent Application No. 2016-531081 Summary of the invention

[0008] Problems to be solved by the invention

[0009] When a glass plate is subjected to external forces such as impact, the decompression multi-layer glass panel sometimes deforms toward another glass plate. When the external force is large, the glass plate may be damaged. In order to suppress the deformation of the glass plate caused by the external force, it is considered to increase the area of ​​the column in contact with the glass plate to deal with it, but in this case, as the contact area of ​​a pair of glass plates and the column increases, the heat transfer rate becomes higher. Although the vacuum multi-layer glass panel of patent document 1 can reduce the heat transfer rate by reducing the diameter of the column, there is a possibility of insufficient strength relative to external forces such as impact. In addition, since the vacuum multi-layer glass panel of patent document 1 is a cylinder, when the glass plate is deformed, the deformed glass plate abuts against the corner of the top or bottom surface of the column and the boundary of the side, that is, the periphery. The angle formed by the corner is 90 degrees. When the corner of the column is pressed on the glass plate that has been deformed due to the external force, the stress of the deformed glass plate is concentrated on the part where the corner is pressed, so the deformed glass plate subjected to the external force is easily damaged.

[0010] In view of the above-mentioned actual situation, there is a demand for a decompression multilayer glass panel that can suppress the heat transfer coefficient to be low and suppress the breakage of the glass sheet subjected to external force.

[0011] Means used to solve problems

[0012] The characteristic structure of the pressure-reducing multi-layer glass panel of the present invention is that it includes: a first glass plate; a second glass plate, which is arranged opposite to the first glass plate; a sealing portion, which is arranged around the entire outer edge of the first glass plate and the second glass plate, and forms a gap portion sealed in a pressure-reduced state between the first glass plate and the second glass plate; and a plurality of columns, which are arranged between the first glass plate and the second glass plate, the columns having: abutting surfaces, which abut against the opposing surfaces of the first glass plate and the second glass plate; and a non-contacting portion, which is arranged around the abutting surface and separated from the opposing surface of the first glass plate or the second glass plate, the non-contacting portion being configured so that at least a portion thereof can abut against the first glass plate or the second glass plate that has been deformed when the opposing first glass plate or the second glass plate is deformed by a first external force.

[0013] According to this structure, the column has: a contact surface that contacts the surfaces facing the first glass plate and the second glass plate; and a non-contact portion that is provided around the contact surface. Thus, the contact area between the column and the first glass plate and the second glass plate can be reduced. As a result, the heat transfer rate can be reduced in the decompression multilayer glass panel.

[0014] In addition, the column is configured such that the non-contact portion is separated from the opposing surface of the first glass plate or the second glass plate, and at least a portion thereof can contact the first glass plate or the second glass plate that has been deformed by the first external force. Here, the first external force refers to an external force that causes the first glass plate or the second glass plate to deform so that it can contact the non-contact portion of the column. As a result, the glass plate that has been deformed by the first external force contacts the non-contact portion around the contact surface of the column, so that the applied stress is dispersed. As a result, the decompression multilayer glass panel can improve the impact strength and suppress the breakage of the glass plate.

[0015] Another characteristic structure is that the abutting structure refers to a structure in which the first glass plate or the second glass plate that has been deformed when the first glass plate or the second glass plate is deformed by a second external force abuts against the non-abutting portion before contacting the opposite first glass plate or the second glass plate.

[0016] According to this structure, the first glass plate or the second glass plate that has been deformed by the second external force contacts the non-contacting portion of the column before contacting the first glass plate or the second glass plate opposite to it. Here, the second external force refers to an external force that deforms the first glass plate or the second glass plate so that it can contact the first glass plate or the second glass plate opposite to it. Thus, the glass plate that has been deformed by the second external force reliably contacts the non-contacting portion before contacting the opposite glass plate, thereby dispersing and supporting stress. As a result, the decompression multilayer glass panel can suppress the breakage of the glass plate.

[0017] Another characteristic structure is that the column also has a non-abutment surface, which extends continuously outward from the periphery of the abutment surface, gradually moving away from the opposite surface of the first glass plate or the second glass plate toward the outer periphery, and the non-abutment portion is located on the non-abutment surface.

[0018] According to this structure, the glass sheet deformed by external force abuts against the non-abutting portion on the non-abutting surface extending continuously from the periphery of the abutting surface of the column, thereby dispersing the applied stress. As a result, the decompression multilayer glass panel can improve the impact strength and suppress the breakage of the glass sheet.

[0019] Another characteristic structure is that the column also has a non-abutment surface, which extends continuously outward from the periphery of the abutment surface and gradually moves away from the opposite surface of the first glass plate or the second glass plate toward the outer periphery, and the non-abutment portion is a part of the non-abutment surface.

[0020] According to this configuration, the glass sheet deformed by the external force comes into contact with the non-contact portion which is a part of the non-contact surface extending continuously from the peripheral edge of the contact surface of the pillar, so that the applied stress is dispersed.

[0021] As a result, the reduced-pressure multilayer glass panel can improve the impact strength and suppress breakage of the glass sheet.

[0022] Another characteristic structure is that, in the column, the slope angle formed between the opposing surface of the first glass plate or the second glass plate and the non-contact surface is set to an angle at which at least a portion of the non-contact surface can abut against the first glass plate or the second glass plate that has been deformed when the first glass plate or the second glass plate is deformed by the first external force.

[0023] According to this structure, the slope angle formed between the opposing surface and the non-contact surface of the first glass plate or the second glass plate is set to an angle at which at least a portion of the non-contact surface can abut against the deformed first glass plate or the second glass plate, thereby enabling the deformed glass plate to appropriately abut against the non-contact surface of the column.

[0024] As another characteristic structure, preferably, the slope angle of the column is set to be less than 65 degrees.

[0025] When the first glass plate or the second glass plate is deformed by the first external force, the deformed portion of the glass plate is supported by the column and deforms within the acute angle range from the opposing surface of the glass plate before deformation. Therefore, as in the present structure, in the column, the slope angle formed between the opposing surface of the first glass plate or the second glass plate and the non-contacting surface is made less than 65 degrees, thereby making it possible to make the deformed glass plate contact the non-contacting surface of the column.

[0026] As another characteristic structure, preferably, the slope angle of the column is set to be greater than 0.4 degrees.

[0027] In the column, the minimum angle of the slope angle formed between the opposing surface and the non-contacting surface of the first glass plate or the second glass plate is set based on the slope angle formed in a normal static state between the opposing surface of the glass plate abutting the column and the opposing surface of the glass plates around the column when only atmospheric pressure is applied to the first glass plate or the second glass plate. The initial slope angle is affected by the material and thickness of the glass plate, the material, size, shape, etc. of the column, but is generally less than 0.4 degrees. Therefore, in the present structure, the slope angle formed between the opposing surface and the non-contacting surface of the first glass plate or the second glass plate is set to be greater than 0.4 degrees. As a result, the first glass plate or the second glass plate can abut against the non-contacting surface when deformed by the first external force.

[0028] As another characteristic structure, preferably, the abutment surface of the column is formed into a spherical crown shape.

[0029] When the contact surface of the column is formed into a spherical crown shape as in this configuration, the pressing force of the contact surface on the facing surface of the first glass plate or the second glass plate is increased, thereby suppressing movement of the column from the position provided between the first glass plate and the second glass plate.

[0030] As another characteristic structure, preferably, the abutting surface of the column is formed into a plane shape.

[0031] If the contact surface of the column is formed into a flat surface as in this structure, the contact surface is in even contact with the facing surface of the first glass plate or the second glass plate, so the column is unlikely to fall over between the first glass plate and the second glass plate and can easily maintain its posture.

[0032] As another characteristic structure, preferably, the non-contact portion of the column is formed in a straight line toward the outer periphery.

[0033] If the non-contact portion of the pillar is formed straight toward the outer periphery as in this configuration, the pillar can easily be set to have an inclination (slope angle) for the deformed first glass sheet or second glass sheet to contact the non-contact surface.

[0034] As another characteristic structure, preferably, the abutting surface and the non-abutting portion of the column are integrally formed into a spherical crown shape with the same radius.

[0035] As in this structure, if the contact surface and the non-contact portion of the column are spherical crowns with the same radius as a whole, the contact surface and the non-contact portion are smoothly continuous, so the non-contact portion is easy to contact along the deformed first glass plate or second glass plate. In addition, the spherical crown portion of the column is easy to be separated from the mold when the column is formed using a mold. Therefore, the column can also be formed at a low cost.

[0036] As another characteristic structure, preferably, the curvature radius of the abutting surface and the non-abutting portion is greater than or equal to 0.3 mm and less than or equal to 20 mm.

[0037] According to this configuration, by setting the curvature radii of the abutment surface and the non-abutment portion within a predetermined range, the abutment surface and the non-abutment portion can be easily formed in the column.

[0038] As another characteristic structure, preferably, the first external force refers to the force when the upper limit height of the ball is 100 mm so that the first glass plate will not be broken in the falling ball test, and the falling ball test is a test in which the columns with a diameter of 0.2 mm and a height of 0.2 mm on the abutting surface are scattered between the first glass plate and the second glass plate (both are 350 mm×350 mm and 3.1 mm thick) at intervals of 20 mm, and a 1 kg ball is dropped from the top of the first glass plate to the center position of the first glass plate and the center position between adjacent columns.

[0039] According to this structure, a vacuum multi-layer glass panel with high impact strength can be formed.

[0040] As another characteristic structure, the heat transfer coefficient is preferably 1.5 W / m2K or less.

[0041] By setting the heat conductivity to 1.5 W / m2K or less as in this structure, a vacuum multi-layer glass panel with high heat insulation properties can be obtained.

[0042] As another characteristic structure, preferably, a maximum diameter of a region of the column facing the first glass plate and the second glass plate is greater than or equal to 100 micrometers and less than or equal to 1000 micrometers.

[0043] Even if the contact surface between the column and the first glass plate and the second glass plate is reduced, if the maximum diameter of the area facing the first glass plate and the second glass plate is increased, the amount of heat that can be stored in the column increases, so the heat flow between the glass plates and the column increases. Therefore, in this structure, the maximum diameter of the area facing the first glass plate and the second glass plate of the column is greater than 100 microns and less than 1000 microns. As a result, the column is miniaturized as a whole, so the increase in heat flow between the glass plates and the column can be suppressed.

[0044] As another characteristic structure, it is preferred that the maximum diameter of the abutting surface is greater than 100 microns.

[0045] As in this structure, if the maximum diameter of the contact surface is greater than 100 micrometers, the column can ensure the contact area between the first glass plate and the second glass plate. Thus, the column can be stably held between the first glass plate and the second glass plate.

[0046] As another characteristic structure, preferably, the length of the column in a direction perpendicular to the plate surfaces of the first glass plate and the second glass plate is greater than or equal to 50 micrometers and less than or equal to 500 micrometers.

[0047] As in this configuration, if the length of the pillars in the direction perpendicular to the surfaces of the first and second glass plates is 50 μm to 500 μm, the pillars are miniaturized, thereby suppressing an increase in heat flow between the glass plates and the pillars.

[0048] As another characteristic structure, the compressive strength of the column is preferably above 200 MPa.

[0049] As in this configuration, since the compressive strength of the column is 200 MPa or more, the column will not be compressed and deformed, and the interval between the first glass plate and the second glass plate can be reliably maintained.

[0050] As another characteristic structure, the pillar preferably comprises zirconium oxide.

[0051] As in this structure, when the column contains zirconium oxide, the low thermal conductivity, heat resistance, and strength of the column can be easily improved.

[0052] As another characteristic structure, preferably, the shape of the column when viewed in a direction perpendicular to the surfaces of the first glass plate and the second glass plate is any one of a circle including an ellipse and an oval, a rectangle, a triangle, and a polygon with five or more sides.

[0053] According to this configuration, the pillars can be formed in various shapes, and thus the shape of the pillars can be freely selected in consideration of the type of glass plate, visibility from the outside of the vacuum multilayer glass panel, and the like. BRIEF DESCRIPTION OF THE DRAWINGS

[0054] Figure 1 It is an exploded perspective view showing the pressure-reducing multilayer glass panel according to the first embodiment.

[0055] Figure 2 is a longitudinal cross-sectional view of a decompression multi-layer glass panel.

[0056] Figure 3 It is a top view of the cylinder.

[0057] Figure 4 It is a side view of the cylinder.

[0058] Figure 5 It is a longitudinal cross-sectional view of the main parts of the pressure-reducing multi-layer glass panel.

[0059] Figure 6 This is a longitudinal cross-sectional view of the main parts showing the state of the decompression multilayer glass panel when it is subjected to external force.

[0060] Figure 7 It is a diagram illustrating the slope angle of a column.

[0061] Figure 8 It is a longitudinal cross-sectional view of a column according to the second embodiment.

[0062] Fig. 9 It is a longitudinal sectional view of the main part of the pressure-reduced multilayer glass panel according to the second embodiment.

[0063] Fig.10 It is a partial longitudinal cross-sectional view of a decompression multi-layer glass panel used in a drop ball test.

[0064] Fig.11 It is a partial top view of a decompression multi-layer glass panel used in a drop ball test.

[0065] Fig.12 This is a longitudinal cross-sectional view of a main part of a pressure-reduced multilayer glass panel according to another embodiment.

[0066] Fig.13 is a top view of a column according to another embodiment.

[0067] Fig.14 is a top view of a column according to another embodiment.

[0068] Fig.15 is a top view of a column according to another embodiment.

[0069] Fig.16 is a top view of a column according to another embodiment.

[0070] Fig.17 This is a longitudinal cross-sectional view of a main part of a pressure-reduced multilayer glass panel according to another embodiment.

[0071] Fig.18 This is a longitudinal cross-sectional view of a main part of a pressure-reduced multilayer glass panel according to another embodiment.

[0072] Fig.19 This is a longitudinal cross-sectional view of a main part of a pressure-reduced multilayer glass panel according to another embodiment.

[0073] Fig. 20 This is a longitudinal cross-sectional view of a main part of a pressure-reduced multilayer glass panel according to another embodiment. DETAILED DESCRIPTION

[0074] (First Embodiment)

[0075] Hereinafter, the pressure-reducing multi-layer glass panel of the present invention will be described with reference to the drawings.

[0076] like Figure 1 and Figure 2 As shown, the vacuum multi-layer glass panel 10 includes a first glass plate 11, a second glass plate 12 arranged opposite to the first glass plate 11, a sealing portion 14 arranged around the outer edges of the first glass plate 11 and the second glass plate 12, and a plurality of columns 16 arranged between the first glass plate 11 and the second glass plate 12. The vacuum multi-layer glass panel 10 (hereinafter referred to as "glass panel") is an example of a decompression multi-layer glass panel.

[0077] The glass panel 10 is formed by forming a gap 13 between a first glass plate 11 and a second glass plate 12 at a predetermined interval, and the gap 13 is sealed in a vacuum state by a sealing portion 14. In order to form the gap 13, the sealing portion 14 is formed over the entire periphery of the glass plates 11 and 12 while the opposing surfaces 17 and 18 of the glass plates 11 and 12 are kept at a predetermined interval with a column 16 between them. The sealing portion 14 is composed of a sealing material or the like. In order to make the gap 13 a vacuum state, after the outer periphery is sealed by the sealing portion 14, suction and exhaust are performed, for example, from a suction port (not shown) provided on the first glass plate 11. After suctioning the suction port, the gap 13 is melted and sealed by using a low melting point glass or the like. In addition, the decompression multilayer glass panel is sealed in a state where the gap 13 is decompressed below the atmospheric pressure.

[0078] like Figure 3 as well as Figure 4 As shown, the column 16 has a circular abutment surface 21 centered on the central axis X and an annular non-abutment portion 23 provided around the abutment surface 21 on both sides of the top surface and the bottom surface when viewed along the central axis X. In the present embodiment, the non-abutment portion 23 is composed of a non-abutment surface 22. The abutment surfaces 21, 21 on both sides of the column 16 abut against the respective opposing surfaces 17, 18 of the glass plates 11, 12. The non-abutment surface 22 (non-abutment portion 23) is separated from the opposing surfaces 17, 18 of the first glass plate 11 or the second glass plate 12. The non-abutment surface 22 (non-abutment portion 23) extends continuously outward from the periphery of the abutment surface 21, and gradually separates from the opposing first glass plate 11 or the second glass plate 12 as it approaches the outer periphery 19 of the column 16.

[0079] The non-contact surface 22 is integrally connected to the contact surface 21 over the entire circumference of the column 16 around the central axis X, and the column 16 is formed in a disc shape. In this way, the column 16 has the non-contact surface 22 located at the periphery of the contact surface 21, so that the contact area R1 of the contact surface 21 can be reduced. As a result, the heat transfer rate in the glass panel 10 can be reduced.

[0080] In the present embodiment, the contact surface 21 and the non-contact surface 22 of the column 16 facing the first glass plate 11 and the second glass plate 12 are formed in a spherical crown shape with the same radius as a whole. If the contact surface 21 of the column 16 is formed in a spherical crown shape, the pressing force of the contact surface 21 on the facing surfaces 17 and 18 of the first glass plate 11 and the second glass plate 12 is increased, so that the column 16 can easily maintain its position between the first glass plate 11 and the second glass plate 12. In addition, if the contact surface 21 and the non-contact surface 22 are formed in a spherical crown shape with the same radius as a whole, the non-contact surface 22 can easily contact along the deformed first glass plate 11 or the second glass plate 12. In addition, the spherical crown portion of the column 16 can be easily separated from the mold when the column 16 is formed using a mold. Therefore, the column 16 can also be formed at a low cost. In the column 16, the contact surface 21 and the non-contact surface 22 (non-contact portion 23) are spherical caps with a curvature radius of 0.3 mm or more and 20 mm or less. In this way, by setting the curvature radius of the contact surface 21 and the non-contact surface 22 (non-contact portion 23) within a predetermined range, the contact surface 21 and the non-contact surface 22 (non-contact portion 23) can be easily formed in the column 16.

[0081] The heat transfer coefficient (U value) of the glass panel 10 is 1.5 W / m2K or less. If the heat transfer coefficient of the glass panel 10 is 1.5 W / m2K or less, the glass panel 10 has sufficient heat insulation. Here, the "heat transfer coefficient (U value)" is a value measured according to "ISO 19916-1: 2018 Glass in building-Vacuuminsulating glass-Part 1".

[0082] Figure 5 The glass panel 10 shown is in a normal state, and only the contact surface 21 (contact region R1) of the column 16 contacts the opposing surfaces 17 and 18 of the first glass plate 11 and the second glass plate 12. The Young's modulus of the column 16 is higher than that of the first glass plate 11 and the second glass plate 12, so when the column 16 is pressed, the opposing surfaces 17 and 18 of the first glass plate 11 and the second glass plate 12 are deformed in a concave manner.

[0083] Figure 6The glass panel 10 shown is in a state where the first glass plate 11 is subjected to an external force and the opposing surface 17 abutted by the column 16 is deformed. Thus, when the first glass plate 11 is deformed, the inner side surface 22A of the column 16, which is a part of the non-abutting surface 22, in addition to the abutting surface 21, also abuts against the opposing surface 17, and the abutting region R1 is expanded to the abutting region R2. As a result, only the outer side surface 22B other than the inner side surface 22A of the non-abutting surface 22 does not abut against the opposing surface 17. Specifically, the abutting region R1 is expanded to the abutting region R2, and the deflection generated on the opposing surface 17 of the first glass plate 11 is supported by the abutting surface 21 and the inner side surface 22A of the non-abutting surface 22.

[0084] In this way, the non-contact surface 22 (non-contact portion 23) is configured so that at least a portion can contact the first glass plate 11 or the second glass plate 12 that is deformed when the first glass plate 11 or the second glass plate 12 is deformed by the first external force. Here, the first external force refers to an external force that deforms the first glass plate 11 or the second glass plate 12 so that it can contact the non-contact surface 22 (non-contact portion 23) of the column 16.

[0085] The structure in which at least a portion of the non-contact surface 22 (non-contact portion 23) can contact the deformed first glass plate 11 or second glass plate 12 means that when the first glass plate 11 or second glass plate 12 is deformed by the second external force, the deformed first glass plate 11 or second glass plate 12 contacts the non-contact surface 22 (non-contact portion 23) before contacting the opposing first glass plate 11 or second glass plate 12. Here, the second external force refers to an external force that deforms the first glass plate 11 or second glass plate 12 so that it can contact the opposing first glass plate 11 or second glass plate 12.

[0086] In this way, the first glass plate 11 deformed by the first external force or the second external force abuts against the non-abutting surface 22 extending continuously from the periphery of the abutting surface 21 of the column 16, and the abutting area becomes larger, and there is no situation where the corner is pressed as in the invention of Patent Document 1, so the stress acting on the first glass plate 11 is dispersed. As a result, the glass panel 10 can improve the impact strength and can suppress the breakage of the first glass plate 11 subjected to external forces such as impact.

[0087] In the column 16, a slope angle α1 is set between the facing surfaces 17, 18 of the first glass plate 11 or the second glass plate 12 and the non-contact surface 22. The slope angle α1 is an angle at which at least a portion of the non-contact surface 22 can contact the deformed first glass plate 11 or the second glass plate 12 when the first glass plate 11 or the second glass plate 12 facing the non-contact surface 22 is deformed by the first external force, and is an angle formed by a tangent line passing through the boundary between the contact surface 21 and the non-contact surface 22 and the facing surface 17 or the facing surface 18. By appropriately setting the slope angle α1 in the column 16, the deformed first glass plate 11 or the second glass plate 12 can contact the non-contact surface 22 of the column 16.

[0088] The slope angle α1 is based on Figure 7 The slope angle α is set as shown. Figure 7 In FIG. 1 , a state in which the first glass plate 11 is deformed relative to the cylindrical column 31 is illustrated. In this case, the slope angle α is an angle formed between the opposed surface 17A after deformation and the opposed surface 17B before deformation in the first glass plate 11 when the first glass plate 11 is subjected to the first external force. Figure 7 , the opposing surface 17B before deformation is indicated by a two-dot chain line, and the opposing surface 17A after deformation is indicated by a solid line. The slope angle α can be increased until the first glass plate 11 breaks. The maximum value of the slope angle α varies depending on the material and thickness of the first glass plate 11 and the second glass plate 12, the material, size, shape, etc. of the column 16. For example, when the maximum value of the slope angle α is set to 65 degrees, the slope angle α1 is set to be less than 65 degrees, preferably less than 55 degrees, and more preferably less than 40 degrees. By making the slope angle α1 of the column 16 less than 65 degrees, the deformed glass plates 11 and 12 can be brought into contact with the non-contact surface 22 of the column 16.

[0089] The minimum slope angle α1 is based on Figure 7 The first glass plate 11 shown is set to the slope angle α0 formed between the facing surface 17 of the first glass plate 11 abutting against the column 16 and the facing surface 17 of the first glass plate 11 around the column 16 in a normal static state when only atmospheric pressure is applied to the first glass plate 11. The slope angle α0 is affected by the material and thickness of the first glass plate 11 and the second glass plate 12, the material, size, shape, etc. of the column 16, but is generally less than 0.4 degrees. Therefore, the slope angle α1 can be set to be 0.4 degrees or more. As a result, the glass plates 11 and 12 can abut against the non-abutting surface 22 when deformed by the first external force.

[0090] The column 16 is formed of ceramics such as alumina and zirconia. The column 16 may also contain nanoparticle fillers such as zirconia. The column 16 contains zirconia, which can easily improve the low thermal conductivity, heat resistance and strength of the column 16. The material of the column 16 can include ceramic nanoparticles (Al2O3, SiO2, ZrO2, SiC, Si3N4 and combinations thereof), ceramic precursors such as SSQ and polysilazane, sintered ceramics (Al2O3, SiO2, ZrO2, SiC, Si3N4, zircon, talc, cordierite, aluminum titanate, etc.), glass (silicon dioxide, soda lime, borosilicate, etc.), glass ceramics (crystallized glass), glass frit, glass beads or glass bubbles, metals (SUS304, SUS430, SUS410, iron, nickel, etc.), resins (polyimide, polyamide, PEEK, PTFE, etc.) and combinations thereof. The pillars 16 of this embodiment are formed of a material having a strength greater than that of the glass plates 11 and 12. Therefore, even if the glass plates 11 and 12 are deformed, the pillars 16 can maintain a constant shape.

[0091] The maximum diameter W1 ( Figure 3 ) is set to be greater than 100 microns and less than 1000 microns. Even if the contact surface 21 of the column 16 and the first glass plate 11 and the second glass plate 12 is reduced, if the maximum diameter W1 of the area facing the first glass plate 11 and the second glass plate 12 is increased, the amount of heat that can be stored in the column 16 will increase, so the heat flow between the glass plates 11, 12 and the column 16 will increase. If the maximum diameter W1 of the column 16 is greater than 100 microns and less than 1000 microns, the column 16 is miniaturized as a whole, so the increase in heat flow between the glass plates 11, 12 and the column 16 can be suppressed. However, from the perspective of stably supporting the first glass plate 11 and the second glass plate 12, the maximum diameter W2 of the contact surface 21 is preferably greater than 100 microns.

[0092] In the column 16, the length in the direction perpendicular to the facing surfaces 17 and 18 (plate surfaces) of the first glass plate 11 and the second glass plate 12, i.e., the overall height (thickness) H1 is set to be 50 μm or more and 500 μm or less. The height (thickness) H2 of the outer peripheral edge 19 of the column 16 is appropriately set based on the slope angle α1.

[0093] The compressive strength of the pillars 16 is 200 MPa or more. Therefore, the pillars 16 are not compressed and deformed in the glass panel 10, and the interval between the first glass plate 11 and the second glass plate 12 can be reliably maintained.

[0094] (Second Embodiment)

[0095] based on Figure 8 and Fig. 9A second embodiment of the glass panel 10 will be described. The same components as those of the first embodiment are denoted by the same reference numerals, and description thereof will be omitted.

[0096] In this embodiment, if Figure 8 As shown, the column 16 has a contact surface 21 formed in a planar shape and a non-contact portion 23 extending linearly from the periphery of the contact surface 21 toward the outer periphery 19 of the column 16 .

[0097] In this embodiment, the non-contact portion 23 is composed of the non-contact surface 22. Fig. 9 As shown, in the glass panel 10 , the column 16 is disposed between the first glass plate 11 and the second glass plate 12 .

[0098] If the contact surface 21 of the column 16 is formed in a plane, the contact surface 21 is in even contact with the opposing surfaces 17 and 18 of the first glass plate 11 and the second glass plate 12. Therefore, the column 16 is difficult to fall over between the first glass plate 11 and the second glass plate 12 and is easy to maintain its posture. Moreover, if the non-contact surface 22 (non-contact portion 23) of the column 16 is formed in a straight line toward the outer peripheral edge 19, the column 16 can easily set the slope angle α2. In addition, the boundary portion 24 between the planar contact surface 21 and the linear non-contact surface 22 forms a corner, and there is a possibility that the stress of the deformed glass plates 11 and 12 is concentrated at this corner. Therefore, the boundary portion 24 is preferably formed in an R shape.

[0099] like Figure 8 As shown in FIG. 1 , a predetermined slope angle α2 is set on the column 16. Figure 8 and Fig. 9 In the column 16 shown, the non-contact surface 22 on the first glass plate 11 side and the non-contact surface 22 on the second glass plate 12 side are shaped to intersect at the outer periphery 19. That is, the column 16 does not have a thickness (equivalent to the thickness H2 of the first embodiment) at the outer periphery 19. Therefore, if the maximum diameter W2 of the contact surface 21 is the same as that of the first embodiment, the slope angle α2 is larger than the slope angle α2 of the first embodiment. Fig. 9 In the glass panel 10 shown, when the first glass plate 11 is deformed due to an impact, the pillars 16 can make the deformed first glass plate 11 abut against the non-contact surface 22. Specifically, the non-contact surface 22 can also support the deflection generated by the facing surface 17 of the first glass plate 11. Thus, the non-contact surface 22 can disperse and absorb the impact received by the first glass plate 11. As a result, the impact strength of the glass panel 10 can be improved.

[0100] (Drop ball test)

[0101] The following drop ball test was performed on the glass panels of Examples 1 and 2 and Comparative Examples 1 and 2 shown below to confirm the impact strength. The drop ball test was performed by the following method: between the first glass plate 11 and the second glass plate 12 (both 350 mm×350 mm, 3.1 mm thick), columns 16′ with a height of 0.2 mm were scattered at intervals of 20 mm, so that the first glass plate 11 and the second glass plate 12 were Fig.10 The positional relationship shown in FIG. 1 is to make a 1 kg ball from the top of the first glass plate 11 to the center position of the first glass plate 11 and the center position S between the adjacent columns 16 ′ (refer to FIG. Fig.11 )fall.

[0102] The glass plates 11 and 12 of Examples 1 and 2 are the same as those of Comparative Examples 1 and 2, and only the columns are different. However, the first glass plate 11 of the glass plates 11 and 12 is Low-E glass, and a Low-E film (not shown) is laminated on the entire second surface of the first glass plate 11 (the surface facing the second glass plate 12). Fig.10 and Fig.11 1 is a diagram for explaining the outline of the falling ball test, and shows a cylindrical column 16' as an example of a column. Fig.10 and Fig.11 The columns 16' shown are identical.

[0103] (Example 1)

[0104] The glass panel of Example 1 has the following pillars 16 disposed between the first glass plate 11 and the second glass plate 12. The pillars 16 used in the example are Figure 3 and Figure 4 The column 16 shown has the same shape, the overall diameter (maximum diameter W1) is 0.5 mm, the diameter (maximum diameter W2) of the abutment surface 21 is 0.2 mm, and the non-abutment surface 22 exists around the abutment surface 21 with a width of 0.15 mm. In addition, the height H1 of the column 16 is 0.2 mm, and the height (thickness) H2 of the outer peripheral edge 19 of the column 16 is 0.16 mm. The curvature radius of the abutment surface 21 and the non-abutment surface 22 is 1.2 mm, and the slope angle α1 is 5 degrees.

[0105] (Example 2)

[0106] The glass panel of Example 2 has the following pillars 16 disposed between the first glass plate 11 and the second glass plate 12. The pillars 16 used in Example 2 are Figure 8The column 16 shown in the figure has the same shape, and the overall diameter (maximum diameter W1) is 0.5 mm, and the diameter (maximum diameter W2) of the contact surface 21 is 0.42 mm. In addition, the height (thickness) H1 of the column 16 is 0.2 mm. In the column of Example 2, the slope angle α2 formed between the facing surface 17, 18 of the first glass plate 11 or the second glass plate 12 and the non-contact surface 22 is 52 degrees.

[0107] (Comparative Example 1)

[0108] The glass panel of Comparative Example 1 is provided with the following column between the first glass plate 11 and the second glass plate 12. The column (column 16') used in Comparative Example 1 is a cylinder with a diameter of 0.2 mm and a thickness (height) of 0.2 mm. That is, the contact surface of the column of Comparative Example 1 that contacts the first glass plate 11 and the second glass plate 12 is the same size as that of Example 1. In Comparative Example 1, since the column 16' is a cylinder, the slope angle is 90 degrees.

[0109] (Comparative Example 2)

[0110] The glass panel of Comparative Example 2 has the following columns arranged between the first glass plate 11 and the second glass plate 12. The columns used in Comparative Example 2 are Figure 8 The column 16 shown has the same shape, but its slope angle is different from that of the column of Example 2. In the column of Comparative Example 2, the slope angle α2 is 68 degrees. Therefore, the diameter of the abutment surface of the column of Comparative Example 2 is 0.42 mm, which is the same as that of Example 2, and the overall diameter is also approximately equal to the diameter of the column of Example 2 (about 0.5 mm).

[0111] Furthermore, the height (thickness) of the column 16 is 0.2 mm.

[0112] (Results of the drop ball test 1)

[0113] In the drop ball test, the upper limit height of the ball that does not break the first glass plate 11 is defined as the drop ball clear height (clear height). The drop ball clear heights are compared for Example 1 and Comparative Example 1, both of which have abutment surfaces with diameters of 0.2 mm. Here, the average value of 15 drop ball tests is used as the drop ball clear height for comparison. In Example 1, the maximum value of the drop ball clear height is 203 mm, the minimum value is 109 mm, and the drop ball clear height (average value) is 152 mm. In Example 1, the deviation of the drop ball clear height is close to 100 mm, but the drop ball clear height is more than 100 mm in all drop ball tests. On the other hand, in Comparative Example 1, the maximum value of the drop ball clear height is 58 mm, the minimum value is 32 mm, and the drop ball clear height (average value) is 44 mm. In Comparative Example 1, the deviation of the drop ball clear height is less than 30 mm, but the drop ball clear height is much lower than 100 mm in all drop ball tests.

[0114] Thus, it was confirmed that the glass panel of Example 1 in which the column had the non-contact surface 22 had higher impact strength than the glass panel of Comparative Example 1 in which the column did not have the non-contact surface 22 .

[0115] (Results of the drop ball test 2)

[0116] The clear heights of the falling ball are compared for Example 2 and Comparative Example 2, both of which have abutment surfaces with a diameter of 0.42 mm. Here, the average value of 15 falling ball tests is also used as the clear height of the falling ball for comparison. In Example 2, the maximum value of the clear height of the falling ball is 312 mm, the minimum value is 185 mm, and the clear height of the falling ball (average value) is 230 mm. In Example 2, the deviation of the clear height of the falling ball is close to 130 mm, but the clear height of the falling ball is above 100 mm in all falling ball tests. On the other hand, in Comparative Example 2, the maximum value of the clear height of the ball is 292 mm, the minimum value is 73 mm, and the clear height of the falling ball (average value) is 203 mm. In Comparative Example 2, the deviation of the clear height of the falling ball is relatively large, which is 219 mm. In the falling ball test, the clear height of the falling ball is sometimes lower than 100 mm.

[0117] Thus, it was confirmed that the glass panel of Example 2 in which the slope angle α2 of the pillars was set to less than 65 degrees had higher impact strength than the glass panel of Comparative Example 2 in which the slope angle of the pillars was set to more than 65 degrees.

[0118] Here, when the first external force is set to the force when the net height of the falling ball in the above-mentioned falling ball test is 100 mm, the glass panel 10 of the first embodiment and the second embodiment can make the net height of the falling ball in the above-mentioned falling ball test be greater than 100 mm by setting the slope angles α1 and α2 to appropriate angles. Thus, the glass panel 10 with high impact strength can be formed.

[0119] The heat transfer coefficient (U value) of the glass panels of Examples 1 and 2 and Comparative Examples 1 and 2 was measured. As a result, the U value was 0.5 W / m2K in Example 1 and Comparative Example 1, and the U value was 0.9 W / m2K in Example 2 and Comparative Example 2. Here, in Example 1 and Comparative Example 1, the diameter of the contact surface 21 of the pillars 16 and 16' was 0.2 mm, and in Example 2 and Comparative Example 2, the diameter of the contact surface 21 of the pillars 16 and 16' was 0.42 mm. As can be seen from the above, the heat transfer coefficient (U value) of the glass panel increases in proportion to the diameter (area) of the contact surface 21 of the pillars 16 and 16'.

[0120] (Other embodiments)

[0121] In the glass panel 10 , the pillars 16 are not limited to the shapes shown in the above-mentioned embodiment, and may be in the following shapes.

[0122] (1) Figure 12 to Figure 16 As shown, the column 16 may also be provided with a convex non-contact portion 23 on the non-contact surface 22. Fig.13 As shown in FIG. 2 , the convex non-contact portion 23 may be provided on the non-contact surface 22 over the entire circumference around the central axis X. Figure 14 to Figure 16 As shown, a plurality of convex non-contact portions 23 may be dispersedly arranged around the central axis X of the non-contact surface 22. Fig.14 In the embodiment, four convex non-contacting portions 23 are arranged in four directions. Fig.15 and Fig.16 In the embodiment, eight convex non-contacting portions 23 are arranged in eight directions. The number of convex non-contacting portions 23 arranged on the non-contacting surface 22 is not particularly limited, and may be one or more than two. Fig.14 as well as Fig.15 As shown in the figure, the cylinder 16 is circular in the plane view, and can also be as shown in the figure. Fig.16 As shown in the figure, the column 16 is in a straight line shape extending radially. In this way, by providing the non-contact portion 23 on a part of the non-contact surface 22, the volume of the entire column 16 can be reduced. The heat transfer coefficient (U value) of the column 16 is proportional to the volume of the column 16. Therefore, by setting the column 16 to Figure 12 to Figure 16 The column 16 can suppress the heat transfer coefficient (U value) by the shape shown. In addition, by reducing the volume of the column 16, the material cost of the column 16 can also be suppressed.

[0123] (2) In the first embodiment described above, the contact surface 21 and the non-contact surface 22 of the column 16 are formed in a spherical crown shape, and the side surfaces of the first glass plate 11 and the second glass plate 12 perpendicular to the facing surfaces 17 and 18 are formed of flat surfaces. Fig.17 As shown, the column 16 is not limited to the contact surface 21 and the non-contact surface 22, but may be formed entirely of curved surfaces including the side surfaces. Thus, the column 16 does not have a flat surface on the side surface, and thus will not be held in a posture where the side surface contacts the first glass plate 11 or the second glass plate 12. Therefore, the column 16 is easily arranged on the first glass plate 11 and the second glass plate 12. Fig.17 In the illustrated column 16 , an example is shown in which the non-contact surface 22 is provided with the convex non-contact portion 23 , but the non-contact surface 22 may not have the convex non-contact portion 23 and may be the entire non-contact portion 23 .

[0124] like Fig.18 As shown, the column 16 may have a groove 25 formed on the non-contact surface 22, or may have a shape having the contact surface 21 and the non-contact portion 23 sandwiched by the groove 25. Thus, by providing the groove 25 on the non-contact surface 22, the overall volume of the column 16 can be reduced.

[0125] Thus, the heat transfer rate (U value) of the column 16 can be suppressed, and the material cost of the column 16 can also be suppressed. Fig.19 As shown, in the column 16, the non-contact portion 23 may be formed by a flat surface along the opposing surfaces 17 and 18 of the glass plates 11 and 12 in the non-contact surface 22. If the non-contact portion 23 is a flat surface, the deformed glass plates 11 and 12 are supported by the flat surface of the non-contact portion 23, so that the impact strength of the glass panel 10 can be improved.

[0126] In addition, if Fig. 20 As shown, in the pillar 16 , the non-contact portion 23 may be formed of a protrusion that is disposed on the outer peripheral side of the non-contact surface 22 and protrudes toward the facing surfaces 17 , 18 of the glass plates 11 , 12 .

[0127] (3) In the above-mentioned embodiment, the shapes of the pillars 16 in a plane view (viewed in a direction perpendicular to the plate surfaces (opposing surfaces 17, 18) of the first glass plate 11 and the second glass plate 12) are shown as circles and octagons. The shapes of the pillars 16 in a plane view may be other circles including ellipses and oval, rectangles, triangles, polygons with five or more sides (e.g. Fig.16 Any of the octagons shown).

[0128] (4) In the above embodiment, an example is shown in which the column 16 includes the non-contact surface 22 facing the first glass plate 11 and the second glass plate 12, but the column 16 may be configured such that the contact surface 21 and the non-contact surface 22 face one of the first glass plate 11 and the second glass plate 12, and only the contact surface 21 faces the other of the first glass plate 11 and the second glass plate 12. In addition, in the above embodiment, an example is shown in which the non-contact portion 23 facing the first glass plate 11 and the second glass plate 12 is provided on the non-contact surface 22 or a part of the non-contact surface 22 in the column 16, but the non-contact portion 23 may be provided only on one of the non-contact surfaces 22 facing the first glass plate 11 and the second glass plate 12.

[0129] (5) In the first embodiment, an example is shown in which the outer periphery 19 of the column 16 has a thickness region (thickness H2), and in the second embodiment, an example is shown in which the outer periphery 19 of the column 16 does not have a thickness region. Alternatively, the column 16 of the first embodiment may have a structure in which the outer periphery 19 does not have a thickness region, and the column 16 of the second embodiment may have a structure in which the outer periphery 19 has a thickness region.

[0130] Industrial Applicability

[0131] The present invention can be applied to various pressure-reducing multi-layer glass panels.

[0132] Explanation of symbols

[0133] 10 Vacuum multi-layer glass panel (pressure-reducing multi-layer glass panel)

[0134] 11 First Glass Plate

[0135] 12 Second Glass Plate

[0136] 13 gap

[0137] 14 Sealed part

[0138] 16 columns

[0139] 17, 18 facing surfaces

[0140] 19 Outer periphery

[0141] 21 contact surface

[0142] 22 Non-contact surface

[0143] 22A1 inner side

[0144] 22A2 outer side

[0145] 23 non-contact part

[0146] W1 Maximum diameter of the cylinder

[0147] W2 Maximum diameter of the contact surface

[0148] H1 Overall Height

[0149] H2 outer edge height

[0150] X center axis

[0151] α, α1, α2: slope angle

Claims

1. A pressure-reducing multi-layer glass panel, comprising: First glass plate; a second glass plate disposed opposite to the first glass plate; a sealing portion provided around the entire periphery of the first glass plate and the second glass plate to form a space sealed in a decompressed state between the first glass plate and the second glass plate; and a plurality of columns disposed between the first glass plate and the second glass plate, The column has: a contact surface that contacts the opposing surfaces of the first glass plate and the second glass plate; and a non-contact portion that is disposed around the contact surface and is separated from the opposing surface of the first glass plate or the second glass plate. The abutment surface is a circle centered on the central axis of the cylinder, The non-contact portion is only provided around the contact surface and is formed in a ring shape. The non-contacting portion is configured such that at least a portion thereof can contact the first glass plate or the second glass plate that is deformed when the first glass plate or the second glass plate facing each other is deformed by the first external force. The column further comprises a non-contact surface, the non-contact surface continuously extending outward from the periphery of the contact surface, gradually moving away from the opposing surface of the first glass plate or the second glass plate toward the outer periphery, and at least a portion of the non-contact surface comprises the non-contact portion. In the column, a slope angle formed between the opposing surface of the first glass plate or the second glass plate and the non-contact surface is set to an angle at which at least a portion of the non-contact surface can contact the first glass plate or the second glass plate that is deformed when the first glass plate or the second glass plate is deformed by the first external force, and the slope angle is set to be greater than or equal to 0.4 degrees and less than 65 degrees. The compressive strength of the column is above 200 MPa.

2. The reduced pressure multilayer glass panel according to claim 1, wherein: The contactable structure refers to a structure in which, when the first glass plate or the second glass plate is deformed by a second external force, the deformed first glass plate or the second glass plate contacts the non-contact portion before contacting the opposing first glass plate or the second glass plate.

3. The pressure-reducing multilayer glass panel according to claim 1 or 2, wherein: The non-contact portion is located on the non-contact surface.

4. The pressure-reducing multilayer glass panel according to claim 1 or 2, wherein: The non-contact portion is a portion of the non-contact surface.

5. The pressure-reducing multilayer glass panel according to claim 1 or 2, wherein: The abutting surface of the column is formed in a spherical crown shape.

6. The pressure-reducing multilayer glass panel according to claim 1 or 2, wherein: The abutting surface of the column is formed in a flat surface shape.

7. The pressure-reducing multi-layer glass panel according to claim 1 or 2, wherein: The non-contact portion of the column is formed in a straight line toward the outer peripheral edge.

8. The pressure-reducing multi-layer glass panel according to claim 1 or 2, wherein: The abutting surface and the non-abutting portion of the column are integrally formed into a spherical crown shape with the same radius.

9. The pressure-reducing multi-layer glass panel according to claim 8, wherein: The curvature radius of the abutting surface and the non-abutting portion is greater than or equal to 0.3 mm and less than or equal to 20 mm.

10. The pressure-reducing multi-layer glass panel according to claim 1 or 2, wherein: The first external force refers to the force when the upper limit height of the ball is 100 mm so that the first glass plate will not be broken in the falling ball test. The falling ball test is a test in which the columns with a diameter of 0.2 mm and a height of 0.2 mm on the abutting surface are distributed between the first glass plate and the second glass plate (both are 350 mm×350 mm and 3.1 mm thick) at intervals of 20 mm, and a 1 kg ball is dropped from the top of the first glass plate to the center of the first glass plate and the center between adjacent columns.

11. The pressure-reducing multi-layer glass panel according to claim 1 or 2, wherein: The heat transfer rate of the pressure-reducing multi-layer glass panel is below 1.5 W / m2K.

12. The pressure-reducing multi-layer glass panel according to claim 1 or 2, wherein: A maximum diameter of a region of the column facing the first glass plate and the second glass plate is greater than or equal to 100 micrometers and less than or equal to 1000 micrometers.

13. The pressure-reducing multi-layer glass panel according to claim 1 or 2, wherein: The maximum diameter of the abutment surface of the column is greater than 100 microns.

14. The pressure-reducing multi-layer glass panel according to claim 1 or 2, wherein: The length of the column in a direction perpendicular to the plate surfaces of the first glass plate and the second glass plate is greater than or equal to 50 micrometers and less than or equal to 500 micrometers.

15. The pressure-reducing multi-layer glass panel according to claim 1 or 2, wherein: The cylinder comprises zirconium oxide.

16. The pressure-reducing multi-layer glass panel according to claim 1 or 2, wherein: The shape of the column when viewed in a direction perpendicular to the plate surfaces of the first glass plate and the second glass plate is any one of a circle including an ellipse and an oval, a rectangle, a triangle, and a polygon with five or more sides.