Method and device for controlling growth of czochralski silicon and electronic equipment
By calculating the growth rate deviation value and threshold value during the growth process of single crystal silicon and adjusting the heating power of the thermal system, the problem of high interruption rate of straight-pull single crystal silicon growth is solved, and the yield rate is improved.
Patent Information
- Application Number
- CN202411044262.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-31
- Publication Date
- 2024-11-12
AI Technical Summary
In the prior art, the yield rate of straight-pull single crystal silicon is low during the growth process, which cannot prevent the crystal edge breakage, resulting in the fluctuation of the growth rate being uncontrollable.
By obtaining the actual velocity and critical velocity of single crystal silicon in the isometric growth stage, calculating the growth rate deviation value and deviation threshold, adjusting the heating power of the thermal system to control the growth rate, ensuring that it is within the preset range.
The prediction and prevention of edge breaking during single crystal silicon growth is achieved, the edge breaking rate is reduced, and the yield of single crystal silicon is improved.
Smart Images

Figure CN118932480A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of semiconductor technology, and in particular to a method for controlling the growth of Czochralski single crystal silicon, a device for controlling the growth of Czochralski single crystal silicon, a computer-readable storage medium, and an electronic device. Background Art
[0002] Czochralski (CZ) method is a commonly used single crystal silicon growth technology. This process can be roughly divided into the following stages: melting stage, seed crystal contact stage, shoulder release growth stage, shoulder rotation growth stage, equal diameter growth stage, tail growth stage, cooling stage, annealing stage, separation stage and post-processing stage. Among them, the equal diameter growth stage is the main stage in the Czochralski single crystal silicon growth process. In this stage, the crystal growth enters a stable stage and the crystal diameter remains unchanged.
[0003] In the isodiameter growth stage, it is not only necessary to control the diameter of the crystal, but more importantly, to maintain dislocation-free growth of the crystal. The judgment of dislocation-free growth varies depending on the crystal orientation, and can generally be judged by the growth stripes (usually called bracts) or small planes (usually called flat edges or ridges) on the outer surface of the ingot.
[0004] In the prior art, the existence of single crystal silicon edges is usually determined based on the degree of edge protrusion during the equal diameter growth process, and then whether dislocation occurs in the single crystal growth. It can be seen that the above judgment process can only be judged after the crystal breaks, and has no prediction function and cannot help prevent crystal breakage.
[0005] Therefore, a method for preventing crystal edge breakage is urgently needed to improve the yield rate of single crystal silicon growth. Summary of the invention
[0006] The main purpose of the present application is to provide a control method for the growth of direct-pull single-crystal silicon, a control device for the growth of direct-pull single-crystal silicon, a computer-readable storage medium and an electronic device, so as to at least solve the problem of low yield in the process of growing single-crystal silicon in the prior art.
[0007] In order to achieve the above-mentioned purpose, according to one aspect of the present application, a control method for the growth of CZ-type single crystal silicon is provided, comprising: obtaining an actual growth speed and a critical speed of the single crystal silicon in the equal-diameter growth stage, the critical speed being the growth speed when the single crystal silicon has broken edges; determining a growth speed deviation value of the single crystal silicon in the equal-diameter growth stage according to a difference between the actual speed and the target speed; determining a growth speed deviation threshold value of the single crystal silicon in the equal-diameter growth stage according to a difference between the critical speed and the target speed; judging whether the growth speed deviation value is greater than the growth speed deviation threshold value, and obtaining a first judgment result; when the first judgment result indicates yes, adjusting the heating power of the thermal system in which the single crystal silicon is located to a first power according to a first preset program, so that the growth speed of the single crystal silicon is the first speed, and the difference between the first speed and the target speed is less than or equal to the growth speed deviation threshold value, wherein the heating power of the thermal system and the growth speed of the single crystal silicon have a preset mapping relationship.
[0008] Optionally, the control method further includes: when the first judgment result indicates no, adjusting the heating power of the thermal system to a second power according to a second preset program, and the second power and the target speed satisfy a preset mapping relationship.
[0009] Optionally, the single crystal silicon is formed in a silicon liquid pool, and the silicon liquid pool contains silicon melt. The control method further includes: obtaining the supercooling at the growth interface of the silicon melt and the single crystal silicon; determining the target speed according to the supercooling and a first preset formula, and the first preset formula is: ΔT s =αV0, where V0 is the target speed, ΔT s is the degree of supercooling, and α is the growth kinetic coefficient of silicon.
[0010] Optionally, obtaining the degree of supercooling at the interface between the silicon melt and the single crystal silicon growth interface includes: obtaining the temperature gradient of the silicon melt at the growth interface; determining the degree of supercooling according to the temperature gradient of the silicon melt at the growth interface and a second preset formula, the second preset formula being: G i =ΔT s / δ, where G i is the temperature gradient of the silicon melt at the growth interface, and δ is the thickness of the temperature boundary layer.
[0011] Optionally, the single crystal silicon is formed in a silicon liquid pool, the silicon liquid pool contains silicon melt, and obtaining the critical growth speed of the single crystal silicon in the isodiameter growth stage includes: obtaining the temperature gradient of the silicon melt at the growth interface of the silicon melt and the single crystal silicon; determining the critical speed according to the temperature gradient of the silicon melt at the growth interface and a third preset formula, the third preset formula being: V'=K s / 30βLρ-K i G i / Lρ, where V' is the critical speed, K s is the thermal conductivity of single crystal silicon, β is the volume expansion coefficient, L is the latent heat of melting of silicon, ρ is the density of silicon, Ki is the thermal conductivity of silicon melt, G i is the temperature gradient of the silicon melt at the growth interface.
[0012] Optionally, the single crystal silicon is formed in a silicon liquid pool, the silicon liquid pool contains silicon melt, and the silicon melt and the single crystal silicon satisfy the energy conservation equation at the growth interface, wherein the energy conservation equation is: K s G s =K i G i +LV'ρ, where K s is the thermal conductivity of single crystal silicon, G s is the temperature gradient of single crystal silicon at the growth interface, K i is the thermal conductivity of silicon melt, G i is the temperature gradient of silicon melt at the growth interface, L is the latent heat of melting of silicon, ρ is the density of silicon, and V' is the critical growth velocity of single crystal silicon in the isodiameter growth stage.
[0013] Optionally, when the temperature at the growth interface changes instantaneously, the temperature gradient change amount and the growth rate deviation value of the single crystal silicon at the growth interface satisfy a fourth preset relationship, and the fourth preset relationship is: K s ΔG s =LΔVρ, where ΔG s is the temperature gradient change of single crystal silicon at the growth interface, and ΔV is the growth rate deviation.
[0014] According to another aspect of the present application, a control device for the growth of CZ-type single crystal silicon is provided, comprising: a first acquisition module, for acquiring an actual growth speed and a critical speed of the single crystal silicon in the equal-diameter growth stage, wherein the critical speed is the growth speed when the single crystal silicon has broken edges; a first determination module, for determining a growth speed deviation value of the single crystal silicon in the equal-diameter growth stage according to a difference between an actual speed and a target speed; a second determination module, for determining a growth speed deviation threshold value of the single crystal silicon in the equal-diameter growth stage according to a difference between a critical speed and a target speed; a judgment module, for judging whether the growth speed deviation value is greater than the growth speed deviation threshold value, and obtaining a first judgment result; and a first control module, for adjusting the heating power of the thermal system in which the single crystal silicon is located to a first power according to a first preset program when the first judgment result indicates yes, so that the growth speed of the single crystal silicon is the first speed, and the difference between the first speed and the target speed is less than or equal to the growth speed deviation threshold value, wherein the heating power of the thermal system and the growth speed of the single crystal silicon have a preset mapping relationship.
[0015] According to another aspect of the present application, a computer-readable storage medium is provided, the computer-readable storage medium including a stored program, wherein when the program is executed, the device where the computer-readable storage medium is located is controlled to execute any one of the control methods for the growth of CZ single crystal silicon.
[0016] According to another aspect of the present application, an electronic device is provided, comprising: one or more processors, a memory, and one or more programs, wherein the one or more programs are stored in the memory and are configured to be executed by the one or more processors, and the one or more programs include a control method for executing any one of the CZ single crystal silicon growth.
[0017] By applying the technical solution of the present application, after obtaining the actual growth speed and critical speed of the single crystal silicon in the equal-diameter growth stage, the growth speed deviation value of the single crystal silicon in the equal-diameter growth stage can be determined according to the difference between the actual speed and the target speed, and then the growth speed deviation threshold of the single crystal silicon in the equal-diameter growth stage can be determined according to the difference between the critical speed and the target speed. Then, through the first judgment result of whether the growth speed deviation value is greater than the growth speed deviation threshold, the magnitude relationship between the speed fluctuation amplitude and the critical fluctuation amplitude of the single crystal silicon in the equal-diameter growth stage can be obtained. Wherein, when the first judgment result indicates yes, it means that the fluctuation amplitude between the actual speed and the target speed of the single crystal silicon in the equal-diameter growth stage is greater than the critical fluctuation amplitude between the critical speed and the target speed of the single crystal silicon in the equal-diameter growth stage. At this time, if the single crystal silicon continues to grow according to the actual speed at this time, the possibility of single crystal silicon edge breaking is greater. Therefore, in order to avoid the edge breaking phenomenon of single crystal silicon in the equal-diameter growth stage, the present application needs to adjust the growth speed of the single crystal silicon in the equal-diameter growth stage to the first speed after obtaining the above-mentioned first judgment result, so as to limit the fluctuation amplitude of the growth speed of the single crystal silicon. Among them, since the growth rate of single crystal silicon and the heating power of the thermal system in which the single crystal silicon is located have a preset mapping relationship, the first speed of the single crystal silicon in the equal-diameter growth stage and the first power of the thermal system satisfy the above preset mapping relationship, so that the heating power of the thermal system in which the single crystal silicon is located can be adjusted to the above first power according to the first preset program, so as to achieve the purpose of making the growth rate of the single crystal silicon in the equal-diameter growth stage the first speed. It can be seen that through the present application, whether the single crystal silicon will break during the growth of the single crystal silicon can be predicted, and when it is predicted that the single crystal silicon will break, the growth rate of the single crystal silicon is limited by the first preset program, and then the fluctuation range of the growth rate of the single crystal silicon in the equal-diameter growth stage is limited, so as to prevent the single crystal silicon from breaking and reduce the single crystal silicon breaking rate, thereby solving the problem of low yield rate of single crystal silicon grown by the direct-pull single crystal silicon in the prior art. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] The drawings constituting part of the present application are used to provide a further understanding of the present application. The exemplary embodiments and descriptions of the present application are used to explain the present application and do not constitute an improper limitation on the present application. In the drawings:
[0019] Figure 1A hardware structure block diagram of a mobile terminal for executing a control method for CZ single crystal silicon growth provided in an embodiment of the present application is shown;
[0020] Figure 2 A schematic flow chart of a method for controlling the growth of Czochralski single crystal silicon provided in accordance with an embodiment of the present application is shown;
[0021] Figure 3 A comparison diagram of the actual growth rate and the target growth rate of single crystal silicon in the equal-diameter growth stage in a control method for the growth of single crystal silicon by direct pulling provided in an embodiment of the present application is shown;
[0022] Figure 4 A structural block diagram of a control device for growing CZ single crystal silicon provided according to an embodiment of the present application is shown.
[0023] The above drawings include the following reference numerals:
[0024] 102, processor; 104, memory; 106, transmission device; 108, input and output devices. DETAILED DESCRIPTION
[0025] It should be noted that, in the absence of conflict, the embodiments and features in the embodiments of the present application can be combined with each other. The present application will be described in detail below with reference to the accompanying drawings and in combination with the embodiments.
[0026] In order to enable those skilled in the art to better understand the solution of the present application, the technical solution in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the present application.
[0027] It should be noted that the terms "first", "second", etc. in the specification and claims of the present application and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequential order. It should be understood that the data used in this way can be interchanged where appropriate, so that the embodiments of the present application described here. In addition, the terms "including" and "having" and any of their variations are intended to cover non-exclusive inclusions, for example, a process, method, system, product or device comprising a series of steps or units is not necessarily limited to those steps or units clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or devices.
[0028] For the convenience of description, some nouns or terms involved in the embodiments of the present application are explained below:
[0029] Czochralski (CZ) method is a commonly used single crystal silicon growth technology.
[0030] As introduced in the background technology, the isodiametric growth stage is the main stage in the process of growing CZ monocrystalline silicon. In this stage, the crystal growth enters a stable stage and the crystal diameter remains unchanged. In this isodiametric growth stage, it is necessary not only to control the diameter of the crystal, but more importantly to maintain the dislocation-free growth of the crystal. The judgment of dislocation-free growth varies depending on the crystal orientation, and can generally be judged by the growth stripes (usually called bracts) or small planes (usually called flat edges or edges) on the outer surface of the ingot. In the prior art, the existence of the ridges of the single crystal silicon is judged by the degree of protrusion of the ridges during the isodiametric growth process, and then it is judged whether dislocations occur in the growth of the single crystal. It can be seen that the above judgment process can only be judged after the crystal breaks, has no prediction function, and cannot help prevent the crystal from breaking, so there is still a problem of low yield rate of monocrystalline silicon growth.
[0031] In order to solve the problem of low yield rate of single crystal silicon growth during the Czochralski single crystal silicon growth process, the embodiments of the present application provide a control method for Czochralski single crystal silicon growth, a control device for Czochralski single crystal silicon growth, a computer-readable storage medium and an electronic device.
[0032] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the accompanying drawings in the embodiments of the present invention.
[0033] The method embodiments provided in the embodiments of the present application can be executed in a mobile terminal, a computer terminal or a similar computing device. Taking running on a mobile terminal as an example, Figure 1 1 is a hardware structure block diagram of a mobile terminal of a method for controlling the growth of CZ single crystal silicon according to an embodiment of the present invention. Figure 1 As shown, the mobile terminal may include one or more ( Figure 1 Only one is shown in the figure) a processor 102 (the processor 102 may include but is not limited to a processing device such as a microprocessor MCU or a programmable logic device FPGA) and a memory 104 for storing data, wherein the mobile terminal may also include a transmission device 106 and an input / output device 108 for communication functions. It can be understood by those skilled in the art that Figure 1 The structure shown is only for illustration and does not limit the structure of the mobile terminal. Figure 1 More or fewer components as shown, or with Figure 1 Different configurations are shown.
[0034] The memory 104 can be used to store computer programs, for example, software programs and modules of application software, such as the computer program corresponding to the control method for the growth of CZ single crystal silicon in the embodiment of the present invention. The processor 102 executes various functional applications and data processing by running the computer program stored in the memory 104, that is, to implement the above method. The memory 104 may include a high-speed random access memory, and may also include a non-volatile memory, such as one or more magnetic storage devices, flash memory, or other non-volatile solid-state memory. In some examples, the memory 104 may further include a memory remotely arranged relative to the processor 102, and these remote memories can be connected to the mobile terminal via a network. Examples of the above networks include, but are not limited to, the Internet, an intranet, a local area network, a mobile communication network, and combinations thereof. The transmission device 106 is used to receive or send data via a network. The specific examples of the above networks may include a wireless network provided by a communication provider of the mobile terminal. In one example, the transmission device 106 includes a network adapter (Network Interface Controller, referred to as NIC), which can be connected to other network devices through a base station so as to communicate with the Internet. In one example, the transmission device 106 may be a radio frequency (RF) module, which is used to communicate with the Internet wirelessly.
[0035] In this embodiment, a method for controlling the growth of CZ silicon monocrystalline that runs on a mobile terminal, a computer terminal or a similar computing device is provided. It should be noted that the steps shown in the flowchart of the accompanying drawings can be executed in a computer system such as a set of computer executable instructions, and although a logical order is shown in the flowchart, in some cases, the steps shown or described can be executed in an order different from that shown here.
[0036] Figure 2 1 is a flow chart of a method for controlling the growth of Czochralski silicon monocrystalline according to an embodiment of the present application. Figure 2 As shown, the method comprises the following steps:
[0037] Step S201, obtaining the actual growth speed and critical speed of the above-mentioned single crystal silicon in the isodiameter growth stage, wherein the above-mentioned critical speed is the growth speed when the above-mentioned single crystal silicon has broken edges;
[0038] Specifically, the actual growth rate of single crystal silicon in the isodiameter growth stage can be obtained by measuring the size change of the crystal.
[0039] For example, an optical microscope or a scanning electron microscope can be used to observe the growth process of the crystal, and then the actual growth rate of the single crystal silicon in the isodiameter growth stage can be calculated by real-time monitoring and recording the change in crystal size. In addition, X-ray diffraction technology can be used to track the growth process of the crystal, thereby obtaining data on the actual growth rate of the single crystal silicon in the isodiameter growth stage.
[0040] Specifically, the ridges on the surface of the single crystal silicon are caused by the tilted {111} close-packed planes. In addition, the number of ridges on the growth of the single crystal silicon is related to the single crystal orientation of the single crystal silicon. <100> For single crystal silicon, since there are four {111} planes that intersect the cylindrical crystal obliquely, four symmetrically distributed growth edges are formed on the crystal column; <111> For single crystal silicon, since there are three {111} planes that intersect the cylindrical crystal obliquely, three symmetrically distributed growth edges are formed on the crystal column; <110> Single crystal silicon has two {111} faces that intersect with the cylindrical crystal obliquely, so two symmetrically distributed growth edges are formed on the crystal column. If the single crystal silicon breaks during the growth process, it is no longer a single crystal.
[0041] Step S202, determining a growth speed deviation value of the silicon single crystal in the equal-diameter growth stage according to a difference between the actual speed and the target speed;
[0042] Specifically, the target speed is the optimal growth speed that matches the thermal system of the single crystal silicon and the CZ single crystal silicon growth. The actual speed can be adjusted to the target speed through the growth speed deviation value.
[0043] Step S203, determining a growth speed deviation threshold of the silicon single crystal in the equal-diameter growth stage according to a difference between the critical speed and the target speed;
[0044] Specifically, the above growth rate deviation threshold is used to represent the critical fluctuation range of the growth rate of single crystal silicon.
[0045] In order to avoid edge breakage of single crystal silicon during the isodiameter growth stage, the fluctuation range between the actual growth speed and the target growth speed of the single crystal silicon during the isodiameter growth stage can be controlled within the above growth speed deviation threshold range.
[0046] Step S204, determining whether the growth rate deviation value is greater than the growth rate deviation threshold, and obtaining a first determination result;
[0047] Specifically, when the growth speed deviation value is greater than the growth speed deviation threshold, it means that the fluctuation amplitude between the actual speed and the target speed of the single crystal silicon grown in the equal-diameter growth stage is greater than the critical fluctuation amplitude of the single crystal silicon growth speed, and thus the probability of broken edges in the single crystal silicon grown at the actual speed is relatively high; when the growth speed deviation value is less than or equal to the growth speed deviation threshold, it means that the fluctuation amplitude between the actual speed and the target speed of the single crystal silicon grown in the equal-diameter growth stage is less than or equal to the critical fluctuation amplitude of the single crystal silicon growth speed, and thus the probability of broken edges in the single crystal silicon grown at the actual speed is relatively low.
[0048] Step S205, when the above-mentioned first judgment result indicates yes, adjust the heating power of the thermal system in which the above-mentioned single crystal silicon is located to a first power according to a first preset program, so that the growth speed of the above-mentioned single crystal silicon is a first speed, and the difference between the above-mentioned first speed and the above-mentioned target speed is less than or equal to the above-mentioned growth speed deviation threshold, wherein the above-mentioned heating power of the above-mentioned thermal system and the growth speed of the above-mentioned single crystal silicon have a preset mapping relationship.
[0049] Specifically, since the heating power and the growth rate of the single crystal silicon have a preset mapping relationship, when the first judgment result indicates yes, in order to avoid the single crystal silicon from breaking during the growth process, the heating power of the thermal system in which the single crystal silicon is located can be adjusted to the first power according to the first preset program. Since the first power and the first speed satisfy the above preset mapping relationship, the growth rate of the single crystal silicon can be controlled to be the first speed. It should be noted that the difference between the first speed and the target speed after adjustment according to the above first preset program is less than or equal to the above growth rate deviation threshold.
[0050] Through this embodiment, after obtaining the actual growth speed and critical speed of the single crystal silicon in the equal-diameter growth stage, the growth speed deviation value of the single crystal silicon in the equal-diameter growth stage can be determined according to the difference between the actual speed and the target speed, and then the growth speed deviation threshold of the single crystal silicon in the equal-diameter growth stage can be determined according to the difference between the critical speed and the target speed. Then, through the first judgment result of whether the growth speed deviation value is greater than the growth speed deviation threshold, the magnitude relationship between the speed fluctuation amplitude and the critical fluctuation amplitude of the single crystal silicon in the equal-diameter growth stage can be obtained. Wherein, when the first judgment result indicates yes, it means that the fluctuation amplitude between the actual speed and the target speed of the single crystal silicon in the equal-diameter growth stage is greater than the critical fluctuation amplitude, wherein the critical fluctuation amplitude is the above-mentioned growth speed deviation threshold. At this time, if the single crystal silicon continues to be grown according to the actual speed at this time, the possibility of single crystal silicon edge breaking is relatively high. Therefore, in order to avoid the edge breaking phenomenon of single crystal silicon in the equal-diameter growth stage, the present application needs to adjust the growth speed of the single crystal silicon in the equal-diameter growth stage to the first speed after obtaining the above-mentioned first judgment result, so as to limit the fluctuation amplitude of the growth speed of the single crystal silicon. Among them, since the growth rate of single crystal silicon and the heating power of the thermal system in which the single crystal silicon is located have a preset mapping relationship, the first speed of the single crystal silicon in the equal-diameter growth stage and the first power of the above-mentioned thermal system satisfy the above-mentioned preset mapping relationship, so that the heating power of the thermal system in which the single crystal silicon is located can be adjusted to the above-mentioned first power according to the first preset program, so as to achieve the purpose of making the growth rate of the single crystal silicon in the equal-diameter growth stage the first speed. It can be seen that through the present application, whether the single crystal silicon will break during the growth of the single crystal silicon can be predicted, and when it is predicted that the single crystal silicon will break, the growth rate of the single crystal silicon is limited by the first preset program, and then the fluctuation range of the growth rate of the single crystal silicon in the equal-diameter growth stage is limited, so as to prevent the single crystal silicon from breaking and reduce the single crystal silicon breaking rate, thereby solving the problem of low yield rate of single crystal silicon grown by the direct-pull single crystal silicon in the prior art.
[0051] In some optional embodiments, the control method for the CZ-type single crystal silicon growth further includes: when the first judgment result indicates no, adjusting the heating power of the thermal system to a second power according to a second preset program, and the second power and the target speed satisfy the preset mapping relationship.
[0052] Specifically, when the first judgment result indicates no, it means that the fluctuation range between the actual speed and the target speed of the single crystal silicon in the equal-diameter growth stage is less than or equal to the above-mentioned critical fluctuation range. At this time, if the single crystal silicon continues to be grown at the actual speed at this time, the possibility of broken edges of the single crystal silicon is small, that is, the single crystal silicon can continue to be grown at the actual speed at this time. Furthermore, in order to match the growth rate of the single crystal silicon with the above-mentioned thermal system, the heating power of the thermal system in which the single crystal silicon is located can also be adjusted to a second power according to a second preset program, so that the growth rate of the single crystal silicon in the equal-diameter growth stage is the above-mentioned target speed. It should be noted here that the above-mentioned second power and the above-mentioned target speed satisfy the above-mentioned preset mapping relationship.
[0053] Wherein, during the CZ single crystal silicon growth process, the single crystal silicon is formed in a silicon liquid pool, and the silicon liquid pool contains silicon melt.
[0054] In the isodiameter growth stage, in order to obtain the optimal growth rate (i.e., target rate) that matches the thermal system in which the single crystal silicon is located, in some optional embodiments, the control method for the growth of the CZ single crystal silicon further includes: obtaining the degree of supercooling at the growth interface between the silicon melt and the single crystal silicon; determining the target rate according to the degree of supercooling and a first preset formula, wherein the first preset formula is: ΔT s =αV0, where V0 is the target speed, ΔT s is the above-mentioned supercooling, and α is the growth kinetic coefficient of silicon.
[0055] The step of obtaining the degree of supercooling at the interface between the silicon melt and the single crystal silicon growth interface comprises: obtaining the temperature gradient of the silicon melt at the growth interface; determining the degree of supercooling according to the temperature gradient of the silicon melt at the growth interface and a second preset formula, wherein the second preset formula is: G i =ΔT s / δ, where G i is the temperature gradient of the silicon melt at the growth interface, and δ is the thickness of the temperature boundary layer. Specifically, δ = 1.13K I ν -1 / 2 ω -1 / 2 , where K I is the thermal diffusion coefficient of the above silicon melt, ν is the kinematic viscosity coefficient of the silicon melt, and ω is the crystal rotation speed.
[0056] In some optional embodiments, the step of obtaining the critical growth speed of the above-mentioned single crystal silicon in the isodiameter growth stage includes: obtaining the temperature gradient of the above-mentioned silicon melt at the growth interface of the above-mentioned silicon melt and the above-mentioned single crystal silicon; determining the above-mentioned critical speed according to the temperature gradient of the above-mentioned silicon melt at the above-mentioned growth interface and a third preset formula, and the above-mentioned third preset formula is: V'=K s / 30βLρ-K i Gi / Lρ, where V' is the critical speed, K s is the thermal conductivity of the above-mentioned single crystal silicon, β is the volume expansion coefficient, L is the latent heat of melting of silicon, ρ is the density of silicon, K i is the thermal conductivity of the silicon melt, G i is the temperature gradient of the silicon melt at the growth interface.
[0057] Specifically, the silicon melt and the single crystal silicon satisfy the energy conservation equation at the growth interface, wherein the energy conservation equation is: K s G s =K i G i +LV'ρ, where K s is the thermal conductivity of the above-mentioned single crystal silicon, G s is the temperature gradient of the single crystal silicon at the growth interface, K i is the thermal conductivity of the silicon melt, G i is the temperature gradient of the silicon melt at the growth interface, L is the melting latent heat of silicon, ρ is the density of silicon, and V' is the critical growth velocity of the single crystal silicon in the isodiameter growth stage. Thus, the critical growth velocity of the single crystal silicon in the isodiameter growth stage is V'=(K s G s -,K i G i ) / Lρ, where the greater the temperature gradient of the single crystal silicon changes, the greater the thermal stress of the single crystal silicon. The two satisfy the thermal stress of the single crystal silicon σ T =εG s β, ε is the Young's modulus of silicon, and β is the volume expansion coefficient. Therefore, the critical velocity V' of single crystal silicon in the isodiameter growth stage is = (K s σ T / εβ-K i G i ) / Lρ. Since the crystal will produce dislocation after the thermal stress reaches a certain value, the perfect crystal model shows that the critical shear stress produced by the crystal dislocation is about 1 / 30 of the Young's modulus. Therefore, the critical velocity V' of single crystal silicon in the isodiameter growth stage is = (K s / 30β-K i G i ) / Lρ.
[0058] When the target growth rate of the single crystal silicon in the equal diameter growth stage is V0, the growth rate deviation threshold ΔV of the single crystal silicon in the above equal diameter growth stage is cri =K s / 30βLρ-K i G i / Lρ-V0.
[0059] In addition, when the actual growth rate of the single crystal silicon in the equal-diameter growth stage is V, the growth rate deviation value of the single crystal silicon in the above-mentioned equal-diameter growth stage is ΔV=max(V-V0).
[0060] In the case where the temperature at the growth interface of the silicon melt and the single crystal silicon changes instantaneously, due to the fast dynamic process, the growth rate deviation value of the single crystal silicon growth stage changes quickly, and then the temperature gradient of the single crystal silicon changes to meet the energy conservation. Specifically, since the silicon melt is a "heat source", the increase or decrease in heat transfer caused by the change in the growth rate of the single crystal silicon is output or compensated by the change in the thermal diffusion of the single crystal silicon, that is, in some optional embodiments, in the case where the temperature at the above-mentioned growth interface changes instantaneously, the temperature gradient change amount of the above-mentioned single crystal silicon at the above-mentioned growth interface and the above-mentioned growth rate deviation value satisfy the fourth preset relationship, and the above-mentioned fourth preset relationship is: K s ΔG s =LΔVρ, where ΔG s is the temperature gradient change of the single crystal silicon at the growth interface, and ΔV is the growth rate deviation value.
[0061] Under stable conditions for the growth of CZ-grown single crystal silicon, the thermal stress inside the crystal is small, and the single crystal silicon grows without dislocations. However, due to the convection instability in the molten silicon body, the temperature of the crystal growth interface, i.e., the crystal-molten silicon body interface, fluctuates, and this fluctuation further causes the temperature gradient in the crystal to fluctuate. After the crystal temperature field changes, the thermal stress inside the crystal induces the generation of dislocations, causing the crystal edges to disappear. In order to predict the broken edges of the crystal, the present embodiment relates to a specific control method for the growth of CZ-grown single crystal silicon, in which the actual growth rate of the single crystal silicon in the equal-diameter growth stage is compared with the target speed, such as Figure 3 As shown. The horizontal axis represents the time axis of the equal-diameter growth stage (time is h), the vertical axis represents the equal-diameter growth speed of the equal-diameter growth stage (unit is mm / h), the dotted line represents the target speed of the single crystal silicon in the equal-diameter growth stage, the actual speed represents the actual growth speed of the single crystal silicon in the equal-diameter growth stage, and ΔV represents the growth speed deviation value between the actual speed and the target speed.
[0062] The embodiment of the present application also provides a control device for the growth of CZ single crystal silicon. It should be noted that the control device for the growth of CZ single crystal silicon in the embodiment of the present application can be used to execute the control method for the growth of CZ single crystal silicon provided in the embodiment of the present application. The device is used to implement the above-mentioned embodiments and preferred implementation modes, and the descriptions that have been made will not be repeated. As used below, the term "module" can be a combination of software and / or hardware that implements a predetermined function. Although the device described in the following embodiments is preferably implemented in software, the implementation in hardware, or a combination of software and hardware, is also possible and conceivable.
[0063] The following is an introduction to the control device for Czochralski single crystal silicon growth provided in an embodiment of the present application.
[0064] Figure 4 Schematic diagram of a control device for growing Czochralski single crystal silicon according to an embodiment of the present application. Figure 4 As shown, the device comprises:
[0065] A first acquisition module 10 is used to acquire the actual growth speed and critical speed of the above-mentioned single crystal silicon in the isodiameter growth stage, and the above-mentioned critical speed is the growth speed when the above-mentioned single crystal silicon has broken edges;
[0066] Specifically, the actual growth rate of single crystal silicon in the isodiameter growth stage can be obtained by measuring the size change of the crystal.
[0067] For example, an optical microscope or a scanning electron microscope can be used to observe the growth process of the crystal, and then the actual growth rate of the single crystal silicon in the isodiameter growth stage can be calculated by real-time monitoring and recording the change in crystal size. In addition, X-ray diffraction technology can be used to track the growth process of the crystal, thereby obtaining data on the actual growth rate of the single crystal silicon in the isodiameter growth stage.
[0068] Specifically, the ridges on the surface of the single crystal silicon are caused by the tilted {111} close-packed planes. In addition, the number of ridges on the growth of the single crystal silicon is related to the single crystal orientation of the single crystal silicon. <100> For single crystal silicon, since there are four {111} planes that intersect the cylindrical crystal obliquely, four symmetrically distributed growth edges are formed on the crystal column; <111> For single crystal silicon, since there are three {111} planes that intersect the cylindrical crystal obliquely, three symmetrically distributed growth edges are formed on the crystal column; <110> Single crystal silicon has two {111} faces that intersect with the cylindrical crystal obliquely, so two symmetrically distributed growth edges are formed on the crystal column. If the single crystal silicon breaks during the growth process, it is no longer a single crystal.
[0069] A first determination module 20, configured to determine a growth speed deviation value of the single crystal silicon in the equal diameter growth stage according to a difference between the actual speed and the target speed;
[0070] Specifically, the target speed is the optimal growth speed that matches the thermal system of the single crystal silicon and the CZ single crystal silicon growth. The actual speed can be adjusted to the target speed through the growth speed deviation value.
[0071] A second determination module 30 is used to determine a growth speed deviation threshold of the single crystal silicon in the equal diameter growth stage according to a difference between the critical speed and the target speed;
[0072] Specifically, the above growth rate deviation threshold is used to represent the critical fluctuation range of the growth rate of single crystal silicon.
[0073] In order to avoid edge breakage of single crystal silicon during the isodiameter growth stage, the fluctuation range between the actual growth speed and the target growth speed of the single crystal silicon during the isodiameter growth stage can be controlled within the above growth speed deviation threshold range.
[0074] A judgment module 40 is used to judge whether the growth rate deviation value is greater than the growth rate deviation threshold value, and obtain a first judgment result;
[0075] Specifically, when the growth speed deviation value is greater than the growth speed deviation threshold, it means that the fluctuation amplitude between the actual speed and the target speed of the single crystal silicon grown in the equal-diameter growth stage is greater than the critical fluctuation amplitude of the single crystal silicon growth speed, and thus the probability of broken edges in the single crystal silicon grown at the actual speed is relatively high; when the growth speed deviation value is less than or equal to the growth speed deviation threshold, it means that the fluctuation amplitude between the actual speed and the target speed of the single crystal silicon grown in the equal-diameter growth stage is less than or equal to the critical fluctuation amplitude of the single crystal silicon growth speed, and thus the probability of broken edges in the single crystal silicon grown at the actual speed is relatively low.
[0076] The first control module 50 is used to adjust the heating power of the thermal system in which the above-mentioned single crystal silicon is located to a first power according to a first preset program when the above-mentioned first judgment result indicates yes, so that the growth speed of the above-mentioned single crystal silicon is a first speed, and the difference between the above-mentioned first speed and the above-mentioned target speed is less than or equal to the above-mentioned growth speed deviation threshold, wherein the above-mentioned heating power of the above-mentioned thermal system and the growth speed of the above-mentioned single crystal silicon have a preset mapping relationship.
[0077] Specifically, since the heating power and the growth rate of the single crystal silicon have a preset mapping relationship, when the first judgment result indicates yes, in order to avoid the single crystal silicon from breaking during the growth process, the heating power of the thermal system in which the single crystal silicon is located can be adjusted to the first power according to the first preset program. Since the first power and the first speed satisfy the above preset mapping relationship, the growth rate of the single crystal silicon can be controlled to be the first speed. It should be noted that the difference between the first speed and the target speed after adjustment according to the above first preset program is less than or equal to the above growth rate deviation threshold.
[0078] Through this embodiment, after obtaining the actual growth speed and critical speed of the single crystal silicon in the equal-diameter growth stage, the growth speed deviation value of the single crystal silicon in the equal-diameter growth stage can be determined according to the difference between the actual speed and the target speed, and then the growth speed deviation threshold of the single crystal silicon in the equal-diameter growth stage can be determined according to the difference between the critical speed and the target speed. Then, through the first judgment result of whether the growth speed deviation value is greater than the growth speed deviation threshold, the magnitude relationship between the speed fluctuation amplitude and the critical fluctuation amplitude of the single crystal silicon in the equal-diameter growth stage can be obtained. Wherein, when the first judgment result indicates yes, it means that the fluctuation amplitude between the actual speed and the target speed of the single crystal silicon in the equal-diameter growth stage is greater than the critical fluctuation amplitude, wherein the critical fluctuation amplitude is the above-mentioned growth speed deviation threshold. At this time, if the single crystal silicon continues to be grown according to the actual speed at this time, the possibility of single crystal silicon edge breaking is relatively high. Therefore, in order to avoid the edge breaking phenomenon of single crystal silicon in the equal-diameter growth stage, the present application needs to adjust the growth speed of the single crystal silicon in the equal-diameter growth stage to the first speed after obtaining the above-mentioned first judgment result, so as to limit the fluctuation amplitude of the growth speed of the single crystal silicon. Among them, since the growth rate of single crystal silicon and the heating power of the thermal system in which the single crystal silicon is located have a preset mapping relationship, the first speed of the single crystal silicon in the equal-diameter growth stage and the first power of the above-mentioned thermal system satisfy the above-mentioned preset mapping relationship, so that the heating power of the thermal system in which the single crystal silicon is located can be adjusted to the above-mentioned first power according to the first preset program, so as to achieve the purpose of making the growth rate of the single crystal silicon in the equal-diameter growth stage the first speed. It can be seen that through the present application, whether the single crystal silicon will break during the growth of the single crystal silicon can be predicted, and when it is predicted that the single crystal silicon will break, the growth rate of the single crystal silicon is limited by the first preset program, and then the fluctuation range of the growth rate of the single crystal silicon in the equal-diameter growth stage is limited, so as to prevent the single crystal silicon from breaking and reduce the single crystal silicon breaking rate, thereby solving the problem of low yield rate of single crystal silicon grown by the direct-pull single crystal silicon in the prior art.
[0079] In some optional embodiments, the control device for the CZ-type single crystal silicon growth further includes: a second control module for adjusting the heating power of the thermal system to a second power according to a second preset program when the first judgment result indicates no, and the second power and the target speed satisfy the preset mapping relationship.
[0080] Specifically, when the first judgment result indicates no, it means that the fluctuation range between the actual speed and the target speed of the single crystal silicon in the equal-diameter growth stage is less than or equal to the above-mentioned critical fluctuation range. At this time, if the single crystal silicon continues to be grown at the actual speed at this time, the possibility of broken edges of the single crystal silicon is small, that is, the single crystal silicon can continue to be grown at the actual speed at this time. Furthermore, in order to match the growth rate of the single crystal silicon with the above-mentioned thermal system, the heating power of the thermal system in which the single crystal silicon is located can also be adjusted to a second power according to a second preset program, so that the growth rate of the single crystal silicon in the equal-diameter growth stage is the above-mentioned target speed. It should be noted here that the above-mentioned second power and the above-mentioned target speed satisfy the above-mentioned preset mapping relationship.
[0081] Wherein, during the CZ single crystal silicon growth process, the single crystal silicon is formed in a silicon liquid pool, and the silicon liquid pool contains silicon melt.
[0082] In the isodiameter growth stage, in order to obtain the optimal growth rate (i.e., target rate) that matches the thermal system in which the single crystal silicon is located, in some optional embodiments, the control device for the growth of the CZ single crystal silicon further includes: a second acquisition module for obtaining the degree of supercooling at the growth interface between the silicon melt and the single crystal silicon; and a third determination module for determining the target rate according to the degree of supercooling and a first preset formula, wherein the first preset formula is: ΔT s =αV0, where V0 is the target speed, ΔT s is the above-mentioned supercooling, and α is the growth kinetic coefficient of silicon.
[0083] The second acquisition module includes: a first acquisition unit for acquiring the temperature gradient of the silicon melt at the growth interface; a first determination unit for determining the supercooling degree according to the temperature gradient of the silicon melt at the growth interface and a second preset formula, wherein the second preset formula is: G i =ΔT s / δ, where G i is the temperature gradient of the silicon melt at the growth interface, and δ is the thickness of the temperature boundary layer. Specifically, δ = 1.13K I ν -1 / 2 ω -1 / 2 , where K I is the thermal diffusion coefficient of the above silicon melt, ν is the kinematic viscosity coefficient of the silicon melt, and ω is the crystal rotation speed.
[0084] In some optional embodiments, the first acquisition module includes: a second acquisition unit, used to obtain the temperature gradient of the silicon melt at the growth interface of the silicon melt and the single crystal silicon; a second determination unit, used to determine the critical speed according to the temperature gradient of the silicon melt at the growth interface and a third preset formula, wherein the third preset formula is: V'=K s / 30βLρ-K i G i / Lρ, where V' is the critical speed, K s is the thermal conductivity of the above-mentioned single crystal silicon, β is the volume expansion coefficient, L is the latent heat of melting of silicon, ρ is the density of silicon, K i is the thermal conductivity of the silicon melt, G i is the temperature gradient of the silicon melt at the growth interface.
[0085] Specifically, the silicon melt and the single crystal silicon satisfy the energy conservation equation at the growth interface, wherein the energy conservation equation is: K s G s =K i G i +LV'ρ, where K s is the thermal conductivity of the above-mentioned single crystal silicon, G s is the temperature gradient of the single crystal silicon at the growth interface, K i is the thermal conductivity of the silicon melt, G i is the temperature gradient of the silicon melt at the growth interface, L is the melting latent heat of silicon, ρ is the density of silicon, and V' is the critical growth velocity of the single crystal silicon in the isodiameter growth stage. Thus, the critical growth velocity of the single crystal silicon in the isodiameter growth stage is V'=(K s G s -,K i G i ) / Lρ, where the greater the temperature gradient of the single crystal silicon changes, the greater the thermal stress of the single crystal silicon. The two satisfy the thermal stress of the single crystal silicon σ T =εG s β, ε is the Young's modulus of silicon, and β is the volume expansion coefficient. Therefore, the critical velocity V' of single crystal silicon in the isodiameter growth stage is = (K s σ T / εβ-K i G i ) / Lρ. Since the crystal will produce dislocation after the thermal stress reaches a certain value, the perfect crystal model shows that the critical shear stress produced by the crystal dislocation is about 1 / 30 of the Young's modulus. Therefore, the critical velocity V' of single crystal silicon in the isodiameter growth stage is = (K s / 30β-K i G i ) / Lρ.
[0086] When the target growth rate of the single crystal silicon in the equal diameter growth stage is V0, the growth rate deviation threshold ΔV of the single crystal silicon in the above equal diameter growth stage is cri =K s / 30βLρ-K i G i / Lρ-V0.
[0087] In addition, when the actual growth rate of the single crystal silicon in the equal-diameter growth stage is V, the growth rate deviation value of the single crystal silicon in the above-mentioned equal-diameter growth stage is ΔV=max(V-V0).
[0088] In the case where the temperature at the growth interface of the silicon melt and the single crystal silicon changes instantaneously, due to the fast dynamic process, the growth rate deviation value of the single crystal silicon growth stage changes quickly, and then the temperature gradient of the single crystal silicon changes to meet the energy conservation. Specifically, since the silicon melt is a "heat source", the increase or decrease in heat transfer caused by the change in the growth rate of the single crystal silicon is output or compensated by the change in the thermal diffusion of the single crystal silicon, that is, in some optional embodiments, in the case where the temperature at the above-mentioned growth interface changes instantaneously, the temperature gradient change amount of the above-mentioned single crystal silicon at the above-mentioned growth interface and the above-mentioned growth rate deviation value satisfy the fourth preset relationship, and the above-mentioned fourth preset relationship is: K s ΔG s =LΔVρ, where ΔG s is the temperature gradient change of the single crystal silicon at the growth interface, and ΔV is the growth rate deviation value.
[0089] The control device for growing CZ-type single crystal silicon includes a processor and a memory. The first acquisition module 10, the first determination module 20, the second determination module 30, the judgment module 40 and the first control module 50 are all stored in the memory as program units, and the processor executes the program units stored in the memory to implement corresponding functions. The modules are all located in the same processor; or, the modules are located in different processors in any combination.
[0090] The processor includes a kernel, which retrieves the corresponding program unit from the memory. One or more kernels can be set, and the problem of low yield rate in the process of growing single crystal silicon in the prior art can be solved by adjusting kernel parameters.
[0091] The memory may include non-permanent memory in a computer-readable medium, random access memory (RAM) and / or non-volatile memory, such as read-only memory (ROM) or flash RAM, and the memory includes at least one memory chip.
[0092] An embodiment of the present invention provides a computer-readable storage medium, wherein the computer-readable storage medium includes a stored program, wherein when the program is executed, the device where the computer-readable storage medium is located is controlled to execute the control method for the growth of CZ single crystal silicon.
[0093] Specifically, the control method of CZ single crystal silicon growth includes:
[0094] Step S201, obtaining the actual growth speed and critical speed of the above-mentioned single crystal silicon in the isodiameter growth stage, wherein the above-mentioned critical speed is the growth speed when the above-mentioned single crystal silicon has broken edges;
[0095] Specifically, the actual growth rate of single crystal silicon in the isodiameter growth stage can be obtained by measuring the size change of the crystal.
[0096] For example, an optical microscope or a scanning electron microscope can be used to observe the growth process of the crystal, and then the actual growth rate of the single crystal silicon in the isodiameter growth stage can be calculated by real-time monitoring and recording the change in crystal size. In addition, X-ray diffraction technology can be used to track the growth process of the crystal, thereby obtaining data on the actual growth rate of the single crystal silicon in the isodiameter growth stage.
[0097] Specifically, the ridges on the surface of the single crystal silicon are caused by the tilted {111} close-packed planes. In addition, the number of ridges on the growth of the single crystal silicon is related to the single crystal orientation of the single crystal silicon. <100> For single crystal silicon, since there are four {111} planes that intersect the cylindrical crystal obliquely, four symmetrically distributed growth edges are formed on the crystal column; <111> For single crystal silicon, since there are three {111} planes that intersect the cylindrical crystal obliquely, three symmetrically distributed growth edges are formed on the crystal column; <110> Single crystal silicon has two {111} faces that intersect with the cylindrical crystal obliquely, so two symmetrically distributed growth edges are formed on the crystal column. If the single crystal silicon breaks during the growth process, it is no longer a single crystal.
[0098] Step S202, determining a growth speed deviation value of the silicon single crystal in the equal-diameter growth stage according to a difference between the actual speed and the target speed;
[0099] Specifically, the target speed is the optimal growth speed that matches the thermal system of the single crystal silicon and the CZ single crystal silicon growth. The actual speed can be adjusted to the target speed through the growth speed deviation value.
[0100] Step S203, determining a growth speed deviation threshold of the silicon single crystal in the equal-diameter growth stage according to a difference between the critical speed and the target speed;
[0101] Specifically, the above growth rate deviation threshold is used to represent the critical fluctuation range of the growth rate of single crystal silicon.
[0102] In order to avoid edge breakage of single crystal silicon during the isodiameter growth stage, the fluctuation range between the actual growth speed and the target growth speed of the single crystal silicon during the isodiameter growth stage can be controlled within the above growth speed deviation threshold range.
[0103] Step S204, determining whether the growth rate deviation value is greater than the growth rate deviation threshold, and obtaining a first determination result;
[0104] Specifically, when the growth speed deviation value is greater than the growth speed deviation threshold, it means that the fluctuation amplitude between the actual speed and the target speed of the single crystal silicon grown in the equal-diameter growth stage is greater than the critical fluctuation amplitude of the single crystal silicon growth speed, and thus the probability of broken edges in the single crystal silicon grown at the actual speed is relatively high; when the growth speed deviation value is less than or equal to the growth speed deviation threshold, it means that the fluctuation amplitude between the actual speed and the target speed of the single crystal silicon grown in the equal-diameter growth stage is less than or equal to the critical fluctuation amplitude of the single crystal silicon growth speed, and thus the probability of broken edges in the single crystal silicon grown at the actual speed is relatively low.
[0105] Step S205, when the above-mentioned first judgment result indicates yes, adjust the heating power of the thermal system in which the above-mentioned single crystal silicon is located to a first power according to a first preset program, so that the growth speed of the above-mentioned single crystal silicon is a first speed, and the difference between the above-mentioned first speed and the above-mentioned target speed is less than or equal to the above-mentioned growth speed deviation threshold, wherein the above-mentioned heating power of the above-mentioned thermal system and the growth speed of the above-mentioned single crystal silicon have a preset mapping relationship.
[0106] Specifically, since the heating power and the growth rate of the single crystal silicon have a preset mapping relationship, when the first judgment result indicates yes, in order to avoid the single crystal silicon from breaking during the growth process, the heating power of the thermal system in which the single crystal silicon is located can be adjusted to the first power according to the first preset program. Since the first power and the first speed satisfy the above preset mapping relationship, the growth rate of the single crystal silicon can be controlled to be the first speed. It should be noted that the difference between the first speed and the target speed after adjustment according to the above first preset program is less than or equal to the above growth rate deviation threshold.
[0107] Optionally, the control method further includes: when the first judgment result indicates no, adjusting the heating power of the thermal system to a second power according to a second preset program, and the second power and the target speed satisfy a preset mapping relationship.
[0108] Optionally, the single crystal silicon is formed in a silicon liquid pool, and the silicon liquid pool contains silicon melt. The control method further includes: obtaining the supercooling at the growth interface of the silicon melt and the single crystal silicon; determining the target speed according to the supercooling and a first preset formula, and the first preset formula is: ΔT s =αV0, where V0 is the target speed, ΔT s is the degree of supercooling, and α is the growth kinetic coefficient of silicon.
[0109] Optionally, obtaining the degree of supercooling at the interface between the silicon melt and the single crystal silicon growth interface includes: obtaining the temperature gradient of the silicon melt at the growth interface; determining the degree of supercooling according to the temperature gradient of the silicon melt at the growth interface and a second preset formula, the second preset formula being: G i =ΔT s / δ, where G i is the temperature gradient of the silicon melt at the growth interface, and δ is the thickness of the temperature boundary layer.
[0110] Optionally, the single crystal silicon is formed in a silicon liquid pool, the silicon liquid pool contains silicon melt, and obtaining the critical growth speed of the single crystal silicon in the isodiameter growth stage includes: obtaining the temperature gradient of the silicon melt at the growth interface of the silicon melt and the single crystal silicon; determining the critical speed according to the temperature gradient of the silicon melt at the growth interface and a third preset formula, the third preset formula being: V'=K s / 30βLρ-K i G i / Lρ, where V' is the critical speed, K s is the thermal conductivity of single crystal silicon, β is the volume expansion coefficient, L is the latent heat of melting of silicon, ρ is the density of silicon, K i is the thermal conductivity of silicon melt, G i is the temperature gradient of the silicon melt at the growth interface.
[0111] Optionally, the single crystal silicon is formed in a silicon liquid pool, the silicon liquid pool contains silicon melt, and the silicon melt and the single crystal silicon satisfy the energy conservation equation at the growth interface, wherein the energy conservation equation is: K s G s =K i G i +LV'ρ, where K s is the thermal conductivity of single crystal silicon, G s is the temperature gradient of single crystal silicon at the growth interface, K i is the thermal conductivity of silicon melt, G i is the temperature gradient of silicon melt at the growth interface, L is the latent heat of melting of silicon, ρ is the density of silicon, and V' is the critical growth velocity of single crystal silicon in the isodiameter growth stage.
[0112] Optionally, when the temperature at the growth interface changes instantaneously, the temperature gradient change amount and the growth rate deviation value of the single crystal silicon at the growth interface satisfy a fourth preset relationship, and the fourth preset relationship is: K s ΔG s =LΔVρ, where ΔG s is the temperature gradient change of single crystal silicon at the growth interface, and ΔV is the growth rate deviation.
[0113] The embodiment of the present invention provides a device, the device includes a processor, a memory, and a program stored in the memory and can be run on the processor, and the processor implements at least the following steps when executing the program: obtaining the actual growth speed and critical speed of monocrystalline silicon in the equal diameter growth stage, the critical speed is the growth speed when the monocrystalline silicon has broken edges; determining the growth speed deviation value of the monocrystalline silicon in the equal diameter growth stage according to the difference between the actual speed and the target speed; determining the growth speed deviation threshold of the monocrystalline silicon in the equal diameter growth stage according to the difference between the critical speed and the target speed; judging whether the growth speed deviation value is greater than the growth speed deviation threshold, and obtaining a first judgment result; when the first judgment result indicates yes, adjusting the heating power of the thermal system where the monocrystalline silicon is located to the first power according to the first preset program, so that the growth speed of the monocrystalline silicon is the first speed, and the difference between the first speed and the target speed is less than or equal to the growth speed deviation threshold, wherein the heating power of the thermal system and the growth speed of the monocrystalline silicon have a preset mapping relationship. The device in this article can be a server, a PC, a PAD, a mobile phone, etc.
[0114] Optionally, the control method further includes: when the first judgment result indicates no, adjusting the heating power of the thermal system to a second power according to a second preset program, and the second power and the target speed satisfy a preset mapping relationship.
[0115] Optionally, the single crystal silicon is formed in a silicon liquid pool, and the silicon liquid pool contains silicon melt. The control method further includes: obtaining the supercooling at the growth interface of the silicon melt and the single crystal silicon; determining the target speed according to the supercooling and a first preset formula, and the first preset formula is: ΔT s =αV0, where V0 is the target speed, ΔT s is the degree of supercooling, and α is the growth kinetic coefficient of silicon.
[0116] Optionally, obtaining the degree of supercooling at the interface between the silicon melt and the single crystal silicon growth interface includes: obtaining the temperature gradient of the silicon melt at the growth interface; determining the degree of supercooling according to the temperature gradient of the silicon melt at the growth interface and a second preset formula, the second preset formula being: G i =ΔT s / δ, where G i is the temperature gradient of the silicon melt at the growth interface, and δ is the thickness of the temperature boundary layer.
[0117] Optionally, the single crystal silicon is formed in a silicon liquid pool, the silicon liquid pool contains silicon melt, and obtaining the critical growth speed of the single crystal silicon in the isodiameter growth stage includes: obtaining the temperature gradient of the silicon melt at the growth interface of the silicon melt and the single crystal silicon; determining the critical speed according to the temperature gradient of the silicon melt at the growth interface and a third preset formula, the third preset formula being: V'=K s / 30βLρ-K i G i / Lρ, where V' is the critical speed, Ks is the thermal conductivity of single crystal silicon, β is the volume expansion coefficient, L is the latent heat of melting of silicon, ρ is the density of silicon, K i is the thermal conductivity of silicon melt, G i is the temperature gradient of the silicon melt at the growth interface.
[0118] Optionally, the single crystal silicon is formed in a silicon liquid pool, the silicon liquid pool contains silicon melt, and the silicon melt and the single crystal silicon satisfy the energy conservation equation at the growth interface, wherein the energy conservation equation is: K s G s =K i G i +LV'ρ, where K s is the thermal conductivity of single crystal silicon, G s is the temperature gradient of single crystal silicon at the growth interface, K i is the thermal conductivity of silicon melt, G i is the temperature gradient of silicon melt at the growth interface, L is the latent heat of melting of silicon, ρ is the density of silicon, and V' is the critical growth velocity of single crystal silicon in the isodiameter growth stage.
[0119] Optionally, when the temperature at the growth interface changes instantaneously, the temperature gradient change amount and the growth rate deviation value of the single crystal silicon at the growth interface satisfy a fourth preset relationship, and the fourth preset relationship is: K s ΔG s =LΔVρ, where ΔG s is the temperature gradient change of single crystal silicon at the growth interface, and ΔV is the growth rate deviation.
[0120] The present application also provides a computer program product, which, when executed on a data processing device, is suitable for executing a program that is initialized with at least the following method steps: obtaining the actual growth speed and critical speed of single crystal silicon in the equal-diameter growth stage, the critical speed being the growth speed when broken edges appear in the single crystal silicon; determining the growth speed deviation value of the single crystal silicon in the equal-diameter growth stage according to the difference between the actual speed and the target speed; determining the growth speed deviation threshold of the single crystal silicon in the equal-diameter growth stage according to the difference between the critical speed and the target speed; judging whether the growth speed deviation value is greater than the growth speed deviation threshold, and obtaining a first judgment result; when the first judgment result indicates yes, adjusting the heating power of the thermal system in which the single crystal silicon is located to the first power according to the first preset program, so that the growth speed of the single crystal silicon is the first speed, and the difference between the first speed and the target speed is less than or equal to the growth speed deviation threshold, wherein the heating power of the thermal system and the growth speed of the single crystal silicon have a preset mapping relationship.
[0121] Optionally, the control method further includes: when the first judgment result indicates no, adjusting the heating power of the thermal system to a second power according to a second preset program, and the second power and the target speed satisfy a preset mapping relationship.
[0122] Optionally, the single crystal silicon is formed in a silicon liquid pool, and the silicon liquid pool contains silicon melt. The control method further includes: obtaining the supercooling at the growth interface of the silicon melt and the single crystal silicon; determining the target speed according to the supercooling and a first preset formula, and the first preset formula is: ΔT s =αV0, where V0 is the target speed, ΔT s is the degree of supercooling, and α is the growth kinetic coefficient of silicon.
[0123] Optionally, obtaining the degree of supercooling at the interface between the silicon melt and the single crystal silicon growth interface includes: obtaining the temperature gradient of the silicon melt at the growth interface; determining the degree of supercooling according to the temperature gradient of the silicon melt at the growth interface and a second preset formula, the second preset formula being: G i =ΔT s / δ, where G i is the temperature gradient of the silicon melt at the growth interface, and δ is the thickness of the temperature boundary layer.
[0124] Optionally, the single crystal silicon is formed in a silicon liquid pool, the silicon liquid pool contains silicon melt, and obtaining the critical growth speed of the single crystal silicon in the isodiameter growth stage includes: obtaining the temperature gradient of the silicon melt at the growth interface of the silicon melt and the single crystal silicon; determining the critical speed according to the temperature gradient of the silicon melt at the growth interface and a third preset formula, the third preset formula being: V'=K s / 30βLρ-K i G i / Lρ, where V' is the critical speed, K s is the thermal conductivity of single crystal silicon, β is the volume expansion coefficient, L is the latent heat of melting of silicon, ρ is the density of silicon, K i is the thermal conductivity of silicon melt, G i is the temperature gradient of the silicon melt at the growth interface.
[0125] Optionally, the single crystal silicon is formed in a silicon liquid pool, the silicon liquid pool contains silicon melt, and the silicon melt and the single crystal silicon satisfy the energy conservation equation at the growth interface, wherein the energy conservation equation is: K s G s =K i G i +LV'ρ, where K s is the thermal conductivity of single crystal silicon, G s is the temperature gradient of single crystal silicon at the growth interface, K i is the thermal conductivity of silicon melt, G i is the temperature gradient of silicon melt at the growth interface, L is the latent heat of melting of silicon, ρ is the density of silicon, and V' is the critical growth velocity of single crystal silicon in the isodiameter growth stage.
[0126] Optionally, when the temperature at the growth interface changes instantaneously, the temperature gradient change amount and the growth rate deviation value of the single crystal silicon at the growth interface satisfy a fourth preset relationship, and the fourth preset relationship is: K s ΔG s =LΔVρ, where ΔG s is the temperature gradient change of single crystal silicon at the growth interface, and ΔV is the growth rate deviation.
[0127] Obviously, those skilled in the art should understand that the above modules or steps of the present invention can be implemented by a general computing device, they can be concentrated on a single computing device, or distributed on a network composed of multiple computing devices, they can be implemented by a program code executable by a computing device, so that they can be stored in a storage device and executed by the computing device, and in some cases, the steps shown or described can be executed in a different order than here, or they can be made into individual integrated circuit modules, or multiple modules or steps therein can be made into a single integrated circuit module for implementation. Thus, the present invention is not limited to any specific combination of hardware and software.
[0128] Those skilled in the art will appreciate that the embodiments of the present application may be provided as methods, systems, or computer program products. Therefore, the present application may adopt the form of a complete hardware embodiment, a complete software embodiment, or an embodiment in combination with software and hardware. Moreover, the present application may adopt the form of a computer program product implemented in one or more computer-usable storage media (including but not limited to disk storage, CD-ROM, optical storage, etc.) that include computer-usable program code.
[0129] The present application is described with reference to the flowcharts and / or block diagrams of the methods, devices (systems), and computer program products according to the embodiments of the present application. It should be understood that each process and / or box in the flowchart and / or block diagram, as well as the combination of the processes and / or boxes in the flowchart and / or block diagram, can be implemented by computer program instructions. These computer program instructions can be provided to a processor of a general-purpose computer, a special-purpose computer, an embedded processor, or other programmable data processing device to generate a machine, so that the instructions executed by the processor of the computer or other programmable data processing device generate instructions for implementing the processes in the flowchart and / or block diagram. Figure 1 A process or multiple processes and / or boxes Figure 1 A device that provides the functions specified in a block or multiple blocks.
[0130] These computer program instructions may also be stored in a computer-readable memory capable of directing a computer or other programmable data processing device to operate in a specific manner, so that the instructions stored in the computer-readable memory produce an article of manufacture comprising an instruction device, which implements the process Figure 1 A process or multiple processes and / or boxes Figure 1 A function specified in one or more boxes.
[0131] These computer program instructions can also be loaded onto a computer or other programmable data processing device so that a series of operating steps are executed on the computer or other programmable device to produce a computer-implemented process, thereby providing instructions for implementing the process. Figure 1 A process or multiple processes and / or boxes Figure 1 The steps for the functions specified in one or more boxes.
[0132] In a typical configuration, a computing device includes one or more processors (CPU), input / output interfaces, network interfaces, and memory.
[0133] The memory may include non-permanent memory in a computer-readable medium, random access memory (RAM) and / or non-volatile memory in the form of read-only memory (ROM) or flash RAM. The memory is an example of a computer-readable medium.
[0134] Computer readable media include permanent and non-permanent, removable and non-removable media that can be implemented by any method or technology to store information. Information can be computer readable instructions, data structures, program modules or other data. Examples of computer storage media include, but are not limited to, phase change memory (PRAM), static random access memory (SRAM), dynamic random access memory (DRAM), other types of random access memory (RAM), read-only memory (ROM), electrically erasable programmable read-only memory (EEPROM), flash memory or other memory technology, compact disk read-only memory (CD-ROM), digital versatile disk (DVD) or other optical storage, magnetic cassettes, magnetic tape disk storage or other magnetic storage devices or any other non-transmission media that can be used to store information that can be accessed by a computing device. As defined herein, computer readable media does not include temporary computer readable media (transitory media), such as modulated data signals and carrier waves.
[0135] It should also be noted that the terms "include", "comprises" or any other variations thereof are intended to cover non-exclusive inclusion, so that a process, method, commodity or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, commodity or device. In the absence of more restrictions, the elements defined by the sentence "comprises a ..." do not exclude the existence of other identical elements in the process, method, commodity or device including the elements.
[0136] From the above description, it can be seen that the above embodiments of the present application achieve the following technical effects:
[0137] The control method for the growth of CZ-type silicon monocrystalline of the present application, after obtaining the actual growth speed and critical speed of the silicon monocrystalline in the equal-diameter growth stage, can first determine the growth speed deviation value of the silicon monocrystalline in the equal-diameter growth stage according to the difference between the actual speed and the target speed, and then determine the growth speed deviation threshold of the silicon monocrystalline in the equal-diameter growth stage according to the difference between the critical speed and the target speed, and then obtain the magnitude relationship between the speed fluctuation amplitude and the critical fluctuation amplitude of the silicon monocrystalline in the equal-diameter growth stage through the first judgment result of whether the growth speed deviation value is greater than the growth speed deviation threshold. Wherein, when the first judgment result indicates yes, it means that the fluctuation amplitude between the actual speed and the target speed of the silicon monocrystalline in the equal-diameter growth stage is greater than the critical fluctuation amplitude between the critical speed and the target speed of the silicon monocrystalline in the equal-diameter growth stage. At this time, if the silicon monocrystalline continues to grow according to the actual speed at this time, the possibility of the silicon monocrystalline breaking is greater. Therefore, in order to avoid the phenomenon of the silicon monocrystalline breaking in the equal-diameter growth stage, the present application needs to adjust the growth speed of the silicon monocrystalline in the equal-diameter growth stage to the first speed after obtaining the above-mentioned first judgment result, so as to limit the fluctuation amplitude of the growth speed of the silicon monocrystalline. Among them, since the growth rate of single crystal silicon and the heating power of the thermal system in which the single crystal silicon is located have a preset mapping relationship, the first speed of the single crystal silicon in the equal-diameter growth stage and the first power of the above-mentioned thermal system satisfy the above-mentioned preset mapping relationship, so that the heating power of the thermal system in which the single crystal silicon is located can be adjusted to the above-mentioned first power according to the first preset program, so as to achieve the purpose of making the growth rate of the single crystal silicon in the equal-diameter growth stage the first speed. It can be seen that through the present application, whether the single crystal silicon will break during the growth of the single crystal silicon can be predicted, and when it is predicted that the single crystal silicon will break, the growth rate of the single crystal silicon is limited by the first preset program, and then the fluctuation range of the growth rate of the single crystal silicon in the equal-diameter growth stage is limited, so as to prevent the single crystal silicon from breaking and reduce the single crystal silicon breaking rate, thereby solving the problem of low yield rate of single crystal silicon grown by the direct-pull single crystal silicon in the prior art.
[0138] The above description is only the preferred embodiment of the present application and is not intended to limit the present application. For those skilled in the art, the present application may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present application shall be included in the protection scope of the present application.
Claims
1. A method for controlling the growth of CZ single crystal silicon, characterized in that: include: Obtaining an actual growth speed and a critical speed of the silicon single crystal in the isodiameter growth stage, wherein the critical speed is the growth speed when the silicon single crystal has broken edges; Determining a growth speed deviation value of the single crystal silicon in the equal-diameter growth stage according to a difference between the actual speed and the target speed; Determining a growth speed deviation threshold of the single crystal silicon in the isodiameter growth stage according to a difference between the critical speed and the target speed; Determine whether the growth rate deviation value is greater than the growth rate deviation threshold value, and obtain a first determination result; When the first judgment result indicates yes, the heating power of the thermal system in which the single crystal silicon is located is adjusted to a first power according to a first preset procedure so that the growth speed of the single crystal silicon is a first speed, and the difference between the first speed and the target speed is less than or equal to the growth speed deviation threshold, wherein the heating power of the thermal system and the growth speed of the single crystal silicon have a preset mapping relationship.
2. The control method according to claim 1, characterized in that: The control method further comprises: When the first judgment result indicates no, the heating power of the thermal system is adjusted to a second power according to a second preset program, and the second power and the target speed satisfy the preset mapping relationship.
3. The control method according to claim 1 or 2, characterized in that: The silicon monocrystalline is formed in a silicon liquid pool, wherein the silicon liquid pool contains silicon melt, and the control method further comprises: Obtaining the degree of supercooling at the growth interface of the silicon melt and the silicon single crystal; The target speed is determined according to the supercooling degree and a first preset formula, wherein the first preset formula is: ΔT s =αV0, where V0 is the target speed, ΔT s is the undercooling degree, and α is the growth kinetic coefficient of silicon.
4. The control method according to claim 3, characterized in that: Obtain the supercooling degree at the interface between silicon melt and single crystal silicon growth, including: Acquiring a temperature gradient of the silicon melt at the growth interface; The degree of supercooling is determined according to the temperature gradient of the silicon melt at the growth interface and a second preset formula, wherein the second preset formula is: G i =ΔT s / δ, where G i is the temperature gradient of the silicon melt at the growth interface, and δ is the thickness of the temperature boundary layer.
5. The control method according to claim 1 or 2, characterized in that: The silicon single crystal is formed in a silicon liquid pool, wherein the silicon liquid pool contains silicon melt, and obtaining a critical growth rate of the silicon single crystal in an isodiameter growth stage comprises: Acquiring a temperature gradient of the silicon melt at a growth interface between the silicon melt and the silicon single crystal; The critical speed is determined according to the temperature gradient of the silicon melt at the growth interface and a third preset formula, wherein the third preset formula is: V'=K s / 30βLρ-K i G i / Lρ, where V' is the critical speed, K s is the thermal conductivity of the single crystal silicon, β is the volume expansion coefficient, L is the latent heat of melting of silicon, ρ is the density of silicon, K i is the thermal conductivity of the silicon melt, G i is the temperature gradient of the silicon melt at the growth interface.
6. The control method according to claim 1 or 2, characterized in that: The silicon monocrystalline is formed in a silicon liquid pool, wherein the silicon liquid pool contains silicon melt, and the silicon melt and the silicon monocrystalline satisfy the energy conservation equation at the growth interface, wherein the energy conservation equation is: K s G s =K i G i +LV'ρ, where K s is the thermal conductivity of the single crystal silicon, G s is the temperature gradient of the single crystal silicon at the growth interface, K i is the thermal conductivity of the silicon melt, G i is the temperature gradient of the silicon melt at the growth interface, L is the latent heat of melting of silicon, ρ is the density of silicon, and V' is the critical growth velocity of the single crystal silicon in the isodiameter growth stage.
7. The control method according to claim 6, characterized in that: In the case where the temperature at the growth interface changes instantaneously, the temperature gradient change of the single crystal silicon at the growth interface and the growth rate deviation value satisfy a fourth preset relationship, and the fourth preset relationship is: K s ΔG s =LΔVρ, where ΔG s is the temperature gradient change of the single crystal silicon at the growth interface, and ΔV is the growth speed deviation value.
8. A control device for growing CZ single crystal silicon, characterized in that: include: A first acquisition module is used to acquire the actual growth speed and critical speed of the single crystal silicon in the isodiameter growth stage, wherein the critical speed is the growth speed when the single crystal silicon has broken edges; A first determination module, configured to determine a growth speed deviation value of the single crystal silicon in the equal-diameter growth stage according to a difference between the actual speed and the target speed; A second determination module is used to determine a growth speed deviation threshold of the single crystal silicon in the equal-diameter growth stage according to a difference between the critical speed and the target speed; A judgment module, used for judging whether the growth rate deviation value is greater than the growth rate deviation threshold value, and obtaining a first judgment result; A first control module is used to adjust the heating power of the thermal system in which the single crystal silicon is located to a first power according to a first preset program when the first judgment result indicates yes, so that the growth speed of the single crystal silicon is a first speed, and the difference between the first speed and the target speed is less than or equal to the growth speed deviation threshold, wherein the heating power of the thermal system and the growth speed of the single crystal silicon have a preset mapping relationship.
9. A computer-readable storage medium, characterized in that: The computer-readable storage medium includes a stored program, wherein when the program is executed, the device where the computer-readable storage medium is located is controlled to execute the control method for growing CZ single crystal silicon according to any one of claims 1 to 7.
10. An electronic device, characterized in that: include: One or more processors, a memory, and one or more programs, wherein the one or more programs are stored in the memory and are configured to be executed by the one or more processors, and the one or more programs include a control method for executing the CZ single crystal silicon growth described in any one of claims 1 to 7.